Zero stress region and controlled fracture region in passivation layer of semiconductor device
By forming passivation layer grooves and controlled fracture zones in the passivation layer of semiconductor devices, the problem of cracks caused by thermomechanical stress is solved, and the mechanical stability and life of the device are significantly improved.
Patent Information
- Application Number
- CN202410348634.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-03-29
- Filing Date
- 2024-03-26
- Publication Date
- 2024-10-01
AI Technical Summary
The thermomechanical stress caused by the difference in thermal expansion coefficient during the assembly process of semiconductor devices, especially the ratchet effect plastic deformation, leads to the uncontrolled formation of cracks in the passivation layer, affecting the device life.
A passivation layer groove is formed in the passivation layer of the semiconductor device, divided into multiple areas, and a controlled fracture zone is formed therein to reduce tensile stress and control the formation of cracks. Passivation layer grooves can be continuous, discontinuous, serpentine, honeycomb, crisscross or zigzag, positioned on the metal layer or its edge to reduce stress concentration.
By introducing passivation layer grooves and controlled fracture zones, the tensile stress in the passivation layer is significantly reduced, uncontrolled crack formation is avoided, and the mechanical stability and life of the device are improved.
Smart Images

Figure CN118737846A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to methods of manufacturing semiconductor devices and semiconductor devices manufactured using the methods. More particularly, the present disclosure relates to reducing thermomechanical stress in a passivation layer of a semiconductor device. Background Art
[0002] Semiconductor devices, especially power devices, can be encapsulated with epoxy molding compound (EMC) at a high temperature of about 180°C during the assembly process. EMC is molded onto the device passivation layer, power metal, bonding wires or clips, silicon substrate, and package lead frame. It is known that the materials that make up the final whole have various thermal expansion coefficients (CTE), which sometimes differ by as much as an order of magnitude. For the most commonly used EMC, the CTE is in the range of 10ppm / °C to 20ppm / °C, which makes EMC one of the main materials that cause thermomechanical stress in the passivation layer of MOSFET.
[0003] Figure 1 A schematic cross-sectional view of an exemplary power MOSFET is shown in FIG. The following materials are shown with the following corresponding CTEs: CTE CU =17ppm / ℃Cu lead frame 102; CTE Si =2.6ppm / ℃ Si epitaxial body 104; CTE AlCu =23ppm / ℃ AlCu metal layer 106; CTE SiO2 = 0.55ppm / ℃ SiO2 oxide 108; CTE SiNx =2.5ppm / ℃SiN x Passivation layer 110; and CTE EMC = 12 ppm / °C EMC 112. Also shown are trenches 114 forming, for example, gate trenches. Movement of each material due to thermal expansion is depicted by arrows, where the length of the arrows indicates the amount of relative movement.
[0004] from Figure 1 It can be clearly seen in Figure 1 that upon cooling from the mold-cure temperature, the EMC will shrink more than the material that makes up the passivation layer (e.g., SiO2 or Si3N4). In an unconstrained situation where the materials are not bonded to each other, this would not be a problem, but because the EMC is bonded to the passivation layer, shear stress is generated at the passivation layer / EMC interface, which accumulates with each thermal cycle.
[0005] Figure 2 An exemplary simulation result of the stress state in the passivation film due to temperature cycling to -55°C is shown in FIG. Figure 2, a 3-dimensional view of a quarter of a die 200 is shown, with a die corner 202 and a die middle 204 indicated at two corners of the quarter. Stress levels 206 are visualized, increasing from the middle 204 to the corner 202, as depicted by contour 206. The following observations are made: (i) there is a point near the middle 204 of the die 200 where the shear stress is close to zero; (ii) the direction of the dominant shear stress τ0 is toward the center 204 of the die; (iii) the maximum shear stress is concentrated at the device corner 202; and (iv) the device edge experiences different levels of stress, which decreases as it moves away from the device corner 202.
[0006] The stress levels can cause cracks in the passivation layer. It has been found that the most severe cracks occur near the edges of the metal layer, especially in the corners of the device. The orientation of cracks and tears is usually towards the middle of the device at right angles to the main forces. The problem with passivation layer cracks is their uncontrolled nature, unpredictable propagation direction and range, large time variability and poor correlation with device life. The mechanism that causes passivation layer cracks is called "plastic deformation by ratcheting". Summary of the invention
[0007] The following describes a summary of aspects of some examples disclosed herein. It should be understood that these aspects are presented to provide the reader with a brief summary of these specific embodiments only, and these aspects are not intended to limit the scope of the disclosure of the present invention. In fact, the disclosure of the present invention may encompass various aspects and / or combinations of aspects that may not be described.
[0008] The present disclosure aims to overcome the drawbacks pointed out in the background section. In particular, the present disclosure aims to provide a solution to limit cracks formed in passivation layers of semiconductor devices due to plastic deformation, such as thermomechanical stress or ratcheting effect.
[0009] According to one aspect of the disclosure of the present invention, a method for manufacturing a semiconductor device is provided. The method may include forming a metal layer. The metal layer may include an edge at which the metal layer ends. The method may further include forming a passivation layer that at least partially covers the metal layer. The method may further include forming a passivation layer groove in the passivation layer. The passivation layer groove may be at least partially positioned above the metal layer. The passivation layer groove may divide the passivation layer into a plurality of regions. Each region is subjected to a reduced tensile stress σ due to the passivation layer groove. SiNx .
[0010] There may be one or more passivation layer trenches.
[0011] In an embodiment, the passivation layer groove can be positioned above the metal layer to form a first region in the passivation layer and a second region in the passivation layer. In this embodiment, the first region does not have an anchor point with the edge of the metal layer, and the second region has an anchor point with the edge of the metal layer.
[0012] In an embodiment, the second region may have an average width L measured from the passivation layer groove to the anchor point. B The anchor point may be located at a distance L0 from the middle of the die. B It can be in the range of L0 / 10 to L0 / 10000.
[0013] In an embodiment, the passivation layer groove may be positioned over an edge of the metal layer to form a first region in the passivation layer and a second region in the passivation layer. In this embodiment, neither the first region nor the second region has an anchor point to the edge of the metal layer.
[0014] In an embodiment, one edge of the passivation layer trench may be positioned above the metal layer, while another edge of the passivation layer trench may be positioned outside of the metal layer but still on top of the barrier base.
[0015] In an embodiment, the passivation layer groove may be formed as a continuous passivation layer groove.
[0016] In an embodiment, the passivation layer groove may be in a polygonal shape.
[0017] In an embodiment, the passivation layer groove may be formed as a serpentine-shaped passivation layer groove.
[0018] In an embodiment, the passivation layer grooves may be formed as honeycomb-shaped passivation layer grooves.
[0019] In an embodiment, the passivation layer groove may be formed as a cross-shaped passivation layer groove.
[0020] In an embodiment, the passivation layer groove may be formed as a zigzag-shaped passivation layer groove.
[0021] In an embodiment, the passivation layer groove may be formed as a discontinuous passivation layer groove.
[0022] In an embodiment, the passivation layer grooves may be formed as a series of perforations.
[0023] In an embodiment, the passivation layer groove may follow one or more edges of the metal layer.
[0024] In an embodiment, the method may further include forming a controlled-fracturing zone in the passivation layer. The controlled-fracturing zone may be a portion of the passivation layer where no passivation layer groove is formed. The controlled-fracturing zone may enable tensile stress to be concentrated in the controlled-fracturing zone. Thus, the formation of cracks may be controlled and limited to the controlled-fracturing zone. There may be one or more controlled-fracturing zones.
[0025] In an embodiment, a controlled fracture zone may be formed between the passivation layer trenches.
[0026] According to one aspect of the disclosure of the present invention, a semiconductor device is provided, which is manufactured using a method having one or more of the above-mentioned features.
[0027] In an embodiment, the semiconductor device may be a power MOSFET. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Disclosed embodiments of the present invention will now be described, by way of example only, with reference to the accompanying schematic drawings in which corresponding reference numerals indicate corresponding parts, and in which:
[0029] Figure 1 shows a schematic cross-sectional view of a power MOSFET;
[0030] Figure 2 is a 3D model of a quarter of a semiconductor device, showing stress levels;
[0031] Figure 3 shows a 3-dimensional schematic cross-sectional view of a portion of an exemplary power MOSFET;
[0032] Figure 4 shows a 3-dimensional schematic cross-sectional view of a portion of an exemplary power MOSFET including a continuous passivation slot;
[0033] Figure 5 shows a 3-dimensional schematic cross-sectional view of a portion of an exemplary power MOSFET including a discontinuous passivation layer trench;
[0034] Fig. 6A , Figure 6B , Fig. 7A , Figure 7B , Figure 7C , Fig.7D , Figure 8 , Fig. 9A , Fig. 9B and Fig. 9C Different variations of the passivation layer grooves are shown;
[0035] Fig.10shows a cross-sectional view of a power MOSFET including a passivation layer trench; and
[0036] Fig.11 Steps of a method of manufacturing a semiconductor device including a passivation layer trench are shown.
[0037] The drawings are for illustrative purposes only and are not intended to limit the scope of protection defined by the claims. DETAILED DESCRIPTION
[0038] It is readily understood that the components of the embodiments as generally described herein and illustrated in the accompanying drawings may be arranged and designed in a variety of different configurations. Therefore, the following more detailed description of various embodiments, as shown in the drawings, is not intended to limit the scope of the disclosure of the present invention, but is merely representative of various embodiments. Although various aspects of the embodiments are presented in the drawings, the drawings are not necessarily drawn to scale unless otherwise indicated.
[0039] The described embodiments should be considered in all respects to be illustrative only and not restrictive. Therefore, the scope of the disclosure of the present invention is indicated by the appended claims rather than by the specific embodiments. All changes within the equivalent meaning and scope of the claims will be included within their scope.
[0040] References to features, advantages, or similar language throughout the specification do not imply that all features and advantages that can be achieved using the disclosure of the present invention are or should be in any single example of the disclosure of the present invention. Rather, language referring to features and advantages is understood to mean that a particular feature, advantage, or characteristic described in conjunction with an embodiment is included in at least one embodiment of the disclosure of the present invention. Therefore, throughout the specification, discussions of features and advantages and similar language may, but do not necessarily, refer to the same example.
[0041] In addition, the described features, advantages and characteristics of the disclosure of the present invention can be combined in one or more embodiments in any suitable manner. According to the description herein, those skilled in the relevant art will recognize that the disclosure of the present invention can be implemented without one or more specific features or advantages of a particular embodiment. In other cases, additional features and advantages that may not exist in all embodiments of the disclosure of the present invention can be recognized in certain embodiments. Throughout the specification, reference to "one embodiment", "embodiment" or similar language means that the specific features, structures or characteristics described in conjunction with the indicated embodiment are included in at least one embodiment of the disclosure of the present invention. Therefore, throughout the specification, the phrases "in one embodiment", "in an embodiment" and similar language may but do not necessarily all refer to the same embodiment.
[0042] In the following examples, the layers of a semiconductor device may be identified as being composed of a particular material, such as SiN x The passivation layer, Cu metal layer or AlCu metal layer. It should be understood that the disclosure of the present invention is not limited to these materials, and any other suitable material can be used for each layer. The proposed solution can be applied to various passivation layer materials, including polymer layers. However, for simplicity, in the following embodiments, SiN is used as the passivation layer. x passivation layer to illustrate the technology.
[0043] The stress levels in the passivation layer that can lead to cracks are usually caused by a ratcheting mechanism, which will combine Figure 3 The examples are explained.
[0044] Figure 3 A schematic cross-sectional view of a portion of an exemplary power MOSFET 300 is shown, oriented with the die edge toward the left and the middle of the die toward the right. For purposes of explanation, the middle is shown here as being on the right, so that movement toward and away from the middle proceeds in a straight line from left to right. In reality, the middle would be at the center of the die, resulting in concentric forces and movement. Silicon layer 302, metal layer 304, SiN x Passivation layer 306 and EMC 308. Metal layer 304 may form a source metal, a gate metal, or any other metal layer.
[0045] Initially, all layers in the device are bonded to each other and there are no cracks in the passivation film. When the temperature is cycled, for example between -55°C and +150°C, the material begins to contract and expand at a rate determined by the CTE of the material. As a result, shear (or friction) stresses are generated at the material interfaces, and initially the materials simply "carry" each other toward the middle of the device, causing the stress to ratchet with each thermal cycle. This carrying of each other would continue indefinitely if it were not for the fact that in actual devices the metal typically has an edge 310, which serves as an anchor for the upper passivation layer. The presence of the metal layer edge 310 is a stress raiser and is a key factor in causing passivation layer fatigue, which ultimately leads to crack initiation and subsequent release of tensile energy in the form of uncontrolled crack growth.
[0046] The anchor point 312 can be defined as the point where the passivation layer wraps around the edge 310 of the metal layer. The anchor point is not necessarily a single point, but can follow the edge 310 of the metal layer. The anchor point 312 is relatively fixed and according to the parameters described in Equation 1, the tensile stress σ SiNx Accumulation in the passivation layer near the edge 310 of the metal layer:
[0047]
[0048] In Equation 1, σ D is the built-in stress of the deposit (a characteristic of the passivation deposition process), and τ0 is the relative strength of EMC and SiN x The interfacial shear stress between the passivation layers, L is the distance from the zero stress point near the middle of the device to the anchor point 312, and t is the passivation film thickness. L, t, and τ0 are also Figure 3 Shown in.
[0049] From Equation 1, it can be seen that stress can exist at all points in the passivation film and reaches its peak at the point farthest from the zero stress point, i.e., at a large distance L. For the vast majority of power devices constructed according to known good practices, the highest stresses will be present at the device corners and along the device edges, as Figure 2 shown.
[0050] Mechanical failure may occur once the accumulated (ratcheting) stress exceeds the yield strength at the interface, at which point the materials are no longer bonded to each other and so one of the materials is left alone to withstand the shear stresses still acting on it from the other surrounding materials.
[0051] In SiN x In the context of cracks in the passivation layer, the initial AlCu and SiN x The initial carry (ratchet effect) is done by AlCu (due to its higher CTE) until the interface bond fatigue between these two layers causes the SiN x Separation. At this time, SiN x are left alone to support the thermo-mechanical stresses incurred by the EMC.
[0052] Once left alone, SiN x is considered to be in its stable state, and subsequent thermal cycling begins to wear away the SiN x The mechanical integrity of the Si Cu is compromised, resulting in local differences in the first passivation layer cracks, Si globules, and residual bonding to the AlCu that initiate at the manufacturing defects.
[0053] For most power MOSFETs, the ratio L / t in Equation 1 is large, typically 1000 to 3000, which greatly amplifies the passivation layer stress at the metal layer edge 310, even for a modest value of τ0. It has been found that by utilizing the ratcheting mechanism and making SiN xThe passivation layer can be decoupled from its anchorage at the edge 310 of the metal layer, enabling an edge with almost zero stress to be achieved in the passivation layer, regardless of its structure and material selection.
[0054] In Figure 4 an exemplary embodiment of Figure 4 FIG. 1 shows a schematic cross-sectional view of a portion of an exemplary power MOSFET 400, oriented with the die edge towards the left and the die center towards the right. Similarly, for purposes of explanation, the center is shown here on the right, such that movement towards and away from the center proceeds linearly from left to right. In reality, the center will be at the center of the die, resulting in concentric forces and movement. The silicon layer 402, metal layer 404, passivation layer 406, and EMC 408 are shown. Additionally, the trench 410, oxide layer 412, and gate busbar 414 are shown.
[0055] The passivation layer 406 is shown as having a plurality of regions, in this instance a first region A 452 and a second region B 454. The passivation layer trench 450 separates the first region A 452 from the second region B 454.
[0056] The first region A 452 can be bonded to the EMC 408 and the metal layer 404, but is otherwise not anchored to the edge 416 of any metal layer. The passivation layer trench 450 decouples the first region A 452 from its metal anchorage at the edge 416. The first region A 452 can thus be characterized by an edge 418 in the passivation layer 406 that naturally has zero stress, since for this region the dimension "L" in Equation 1 is zero due to the absence of an anchorage. The first region A 452 can be referred to as a floating passivation.
[0057] The second region B 454 can be the portion of the passivation layer 406 that is anchored to the edge 416 of the metal layer 404 in a conventional manner, but with a significantly (e.g., ~100 times) reduced dimension "L". The second region B 454 can be referred to as an anchored passivation. In Figure 4 FIG. 2, L0 represents the distance L that would be applicable in the absence of the passivation layer trench 450, and L B represents the distance L of the second region B 454. Thus, introducing the passivation layer trench 450 results in L B << L0, and according to Equation 1, a much lower tensile stress σ SiNx is generated in the passivation layer in the second region B 454. Therefore, by applying the passivation layer trench, cracks can be avoided near the corners and edges of the die.
[0058] Preferably, LB 10 to 10,000 times smaller than the original L0, which in practice means that for most power MOSFETs L B It can be smaller than 20μm.
[0059] One or more stress reducing passivation layer grooves 450 may be formed at strategic locations on the chip. The passivation layer grooves 450 may play a dual role: (i) providing a zero stress edge with robust resistance to thermomechanical loads from the EMC; and (ii) allowing passivation layer cracks to be guided and contained within their fracture range.
[0060] A new reticle design may be used to form one or more passivation layer grooves 450. The redesigned reticle may be used in, for example, contact bond, CB or via, VI lithography for passivation layer patterning.
[0061] The redesigned passivation layer openings forming the passivation layer grooves 450 can be divided into two categories: continuous grooves and discontinuous grooves.
[0062] The continuous groove can be used to provide (i) a continuous zero stress edge, and (ii) reduced tensile stress in the passivation layer at the edge of the metal layer on the other side of the groove. Figure 4 The passivation layer trench 450 shown is an example of a continuous trench.
[0063] As an alternative, discontinuous grooves (e.g., perforations) can be used to guide the passivation layer fracture direction during thermomechanical loading. This can be achieved, for example, by having alternating regions, such as Figure 5 As shown, the passivation layer is removed 502 and retained 504 in an alternating pattern in the alternating regions. This may typically form a high stress region at or near the retained region 504 where the passivation layer may fracture, adjacent to a low stress or zero stress region, i.e., adjacent to the region 502 where the passivation layer has been removed, where the fracture terminates. The high stress difference between these regions 502, 504 can result in effective guidance of the fracture path.
[0064] Note that in addition to the shape of the passivation layer groove, Figure 4 and Figure 5 The exemplary power MOSFETs 400 and 500 also include similar layers and features, in Figure 5 No further identification is given in .
[0065] exist Figure 4 and Figure 5 In the embodiment, the passivation layer grooves are drawn as having sharp or right-angled edges and corners. It is understood that the edges and corners may be more rounded and / or irregular due to the manufacturing process.
[0066] Fig. 6A and Figure 6B is an exemplary embodiment of a passivation layer groove in the form of a continuous passivation layer groove. Here, continuous should be understood as having a considerable length. A plurality of continuous passivation layer grooves can be formed, such as Fig. 6A and Figure 6B , where in these examples, in the corners of the bottom, the passivation layer grooves 606, 616 are interrupted by small portions without grooves. Such portions without grooves enable the definition of controlled portions of the die where stress may be concentrated and cracks may occur.
[0067] Fig. 6A and Figure 6B A quarter of a die 600, 610 is shown. The middle of the die is depicted as 604, 614, and the die edges are depicted as 602, 612.
[0068] exist Fig. 6A In the example of FIG. 6 , near the edge 602 of the die 600, typically, for example, Figure 4 As shown, a continuous passivation layer groove 606 is formed near the edge 416 of the metal layer. Fig. 6A In the example of FIG. 6 , one of the edges 602 is located near the gate bus bar 414 and is Figure 4 The example is similar. Fig. 6A In FIG. 6 , arrow 602 points to one location, but it should be understood that edge 602 generally exists along passivation layer groove 606. In this example, two passivation layer regions can be formed: a first passivation layer region with almost no stress between passivation layer groove 606 and the middle of the die, and a second passivation layer region with a limited amount of stress between passivation layer groove 606 and die edge 602. Passivation layer groove 606 can be cut near the edge of the metal layer to minimize dimension L, and the scope of any passivation layer crack can be suppressed to a few μm outside near the edge of the metal layer. In this scheme, any crack that occurs can terminate at the outer edge of the groove.
[0069] exist Figure 6B In, similar to Fig. 6A The passivation layer groove 606 and the edge 602 are formed to form a continuous passivation layer groove 616 near the edge 612. Figure 6BIn the example of , an additional continuous passivation layer groove 618 is formed at the middle 614 closer to the tube core 610, thereby forming an additional passivation layer area. This design may be advantageous when, for example, there are multiple edges in the underlying layer such as a metal layer, which may result in multiple physical anchors on the passivation layer. It should be understood that the number of passivation layer grooves 606, 616, 618 and their locations may vary depending on the design of the chip. Therefore, multiple ring passivation layer grooves 616, 618 can be formed at multiple locations where the passivation layer stress may be interrupted / reset, allowing the passivation film to be carried more freely by the EMC and AlCu during thermal mechanical loading.
[0070] 7A to 7D is an exemplary embodiment of a passivation layer groove in the form of a passivation layer perforation. The passivation layer perforation may have perforation openings of various shapes and sizes, and the stress relief openings are provided as a regular repeating pattern or a pattern overlapping another pattern to guide the direction of cracks and provide a termination point.
[0071] 7A to 7D A quarter of a die is shown 700, 710, 720, and 730. The middle of the die is depicted as 704, 714, 724, 734, and the edges of the die are depicted as 702, 712, 722, 732.
[0072] exist Fig. 7A In the example of FIG. 7 , a regularly repeating pattern of passivation layer grooves 706 is applied near the edge 702 of the die 700. Figure 7B In the example, similar to Fig. 7A A passivation layer groove 706 is formed in the form of a passivation layer, and a passivation layer groove 716 having a regular repeating pattern is applied near the edge 712 of the tube core 710. Figure 7B In the example of , an additional regularly repeating pattern of passivation layer grooves 718 is applied closer to the middle 714 of the die 710. Figure 7C In the example, similar to Fig. 7A A passivation layer groove 706 is formed in the form of a passivation layer. A passivation layer groove 726 having a regular repeating pattern is applied near the edge 722 of the die 720. Figure 7C In the example of , an additional regularly repeating pattern of passivation layer grooves 728 is applied even closer to the middle 724 of the die 720. Fig.7D In the example of FIG. 7 , an overlapping pattern of passivation layer grooves 736 with different sized perforations are applied on the die 730. It is understood that other patterns of perforations may be applied depending on the chip design and desired stress relief.
[0073] For example 7A to 7D As shown in the example of FIG. 1 , alternating perforations and passivation layer regions can allow cracks to propagate between the perforations and be suppressed in the general vicinity of the perforations.
[0074] Figure 8 is an exemplary embodiment of a polygonal passivation layer groove in the form of a serpentine passivation layer groove. The serpentine passivation layer groove can reduce the inherent material hardness of the passivation layer near the groove compared to a straight or perforated groove. This clever patterning technique allows for improved stress distribution, thereby enabling the layer to withstand higher stresses generated during thermal loads.
[0075] Figure 8 A quarter of a die 800 is shown. The middle of the die is depicted as 804, and the edge of the die is depicted as 802. Figure 8 In the example of FIG. 8 , a serpentine passivation layer groove 806 is applied in a region 808 (region 808 is depicted as a dashed area) that enhances mechanical deformation. The alternating long / short pattern of passivation layer width at the edge of the metal layer due to the serpentine shape can reduce the chance of pattern shift behind the passivation layer groove 806.
[0076] 9A to 9C is an exemplary embodiment of an alternative polygonal form of the passivation layer groove having a similar effect to the serpentine passivation layer groove 806 .
[0077] 9A to 9C A quarter of a die 900, 910, 920 is shown. The middle of the die is depicted as 904, 914, 924, and the edges of the die are depicted as 902, 912, 922.
[0078] exist Fig. 9A In the example of , a honeycomb passivation layer groove 906 is applied. Fig. 9B In the example of , a criss-cross passivation layer groove 916 is applied. Fig. 9C In the example of FIG. 9 , a zigzag passivation layer groove 926 is applied.
[0079] The polygonal shape of the passivation layer groove can be changed, for example, by changing the pitch, length and / or angle. For example, a sawtooth passivation layer groove such as a sawtooth passivation layer groove 926 can have a sawtooth shape with an angle between 10 degrees and 80 degrees. Preferably, all sawtooth shapes are formed using substantially the same angle, but different angles can also be applied to a sawtooth passivation layer groove. In an exemplary embodiment, the sawtooth shape can have an angle of 30 degrees. In another exemplary embodiment, the sawtooth shape can have an angle of 45 degrees. Similarly, corners in polygonal passivation layer grooves such as honeycomb passivation layer grooves 906, and corners in cross-shaped passivation layer grooves such as cross-shaped passivation layer grooves 916, can have an angle between 5 degrees and 175 degrees. Preferably, the honeycomb shape in the honeycomb passivation layer groove is similarly shaped, but honeycombs of different shapes are possible. Preferably, the cross-shaped shape in the cross-shaped passivation layer groove is similarly shaped, but cross-shaped shapes of different shapes are possible. Different serpentine passivation layer grooves may have serpentine structures of different shapes. For example, the size of the serpentine structures constituting the serpentine passivation layer grooves may vary. The serpentine structures of a passivation layer groove preferably have substantially similar shapes, but may also have different shapes.
[0080] exist Figure 4 In the example of , the passivation layer groove 450 is positioned so that an anchor point is retained near the edge 416 of the metal layer 404. Advantageously, as Figure 4 As shown, L B is much smaller than L0, resulting in only a limited amount of stress in the second passivation layer region B 454. Further improvement can be achieved by coinciding the passivation layer groove with the edge of the metal layer. Fig.10 An example of this is shown in .
[0081] Fig.10 1 shows a 2-dimensional schematic cross-sectional view of a portion of an exemplary power MOSFET 1000. An epitaxial layer 1002, an AlCu metal layer 1004, oxide layers 1006, 1014, a Ti / TiN barrier layer 1008, and a SiN x Passivation layers 1052, 1054 of the film. Furthermore, edges 1010 of the metal layer 1004 and trenches 1012 are shown.
[0082] The passivation layer is shown as having multiple regions, in this example having a first region 1052 and a second region 1054. A passivation layer trench 1050 separates the first region 1052 from the second region 1054. In addition, the passivation layer trench 1050 is positioned on top of the edge 1010 of the metal layer 1004. Fig.10In the example of FIG. 1 , one edge 1056 of the passivation layer trench 1050 is disposed above the metal layer 1004, while the other edge 1058 is disposed outside the metal layer but still on top of the Ti / TiN barrier foot 1008 to provide a convenient endpoint for, for example, a stage VI dry etch.
[0083] In addition to separating the passivation layer, other layers may also be separated through the passivation layer grooves (such as the passivation layer grooves 1050). Fig.10 As shown, the passivation layer groove 1050 can separate the first region 1052 and the oxide layers 1006, 1014 from the second region 1054 and the additional layer 1014. Non-limiting examples of the additional layer 1014 are additional regions of the oxide layer and additional regions of the metal layer. Other layers can be separated by the passivation layer groove 1050, and the number of layers separated by the passivation layer groove 1050 can be different on each side of the passivation layer groove.
[0084] The passivation layer trench is typically formed in a single manufacturing step.
[0085] By decoupling the passivation layers 1052, 1054 from their anchor points (i.e., Fig.10 In the example of FIG. 1 , there is no anchor point at the edge 1010 of the metal layer 1004), the stress in the passivation layer can be reduced to its baseline value determined by the stress of the deposit because the dimension L at all points in the passivation layer is zero ( Where L = 0).
[0086] exist Fig.11 Process steps for manufacturing semiconductor devices such as power MOSFETs are shown in an exemplary embodiment of the present invention. Steps related to the disclosure of the present invention are shown, and other steps can be applied as needed to form other layers and features of the semiconductor device. In step 1102, a metal layer, such as metal layer 304, 404, or 1004, can be formed. The metal layer includes an edge, such as edge 310 or edge 1010, at which the metal layer ends. In step 1104, a passivation layer, such as passivation layer 406, can be formed so that the passivation layer at least partially covers the metal layer. In step 1106, a passivation layer groove, such as shown in the above examples, can be formed in the passivation layer. The passivation layer groove is at least partially positioned above the metal layer and divides the passivation layer into multiple regions, such as Figure 4 Areas 452 and 454 or Fig.10 Each region is subjected to a reduced tensile stress σ due to the passivation layer groove. SiNx .
[0087] In order to reduce stress and thereby reduce cracks in the passivation layer, other shapes of passivation layer grooves may be applied, and different shapes of passivation layer grooves may be mixed. The width and length of the passivation layer grooves may vary depending on the design of the chip and the location of the passivation layer grooves on the chip. In an exemplary embodiment, the passivation layer grooves may have a width of about 5 μm to 20 μm.
[0088] The manufacturing processes used to form the various layers of the semiconductor device are not described in detail. Any known processes may be used to form the various layers, and in particular to form the metal layers and the passivation layers.
[0089] As mentioned above, in order to form one or more passivation layer grooves, passivation patterning can be performed using, for example, CB or VI photolithography. Using CB / VI photolithography, a photoresist layer can be deposited on a wafer, and a photomask can be used to expose the photoresist with a pattern of one or more passivation layer grooves. The exposed photoresist can be developed, and the passivation layer groove can be etched out in the wafer. Then, a second layer of photoresist can be deposited on the top of the first layer, and a second photomask can be used to expose the area where the passivation layer will be removed. The exposed photoresist can be developed, and the passivation layer in the exposure area can be etched away.
[0090] The passivation layer trenches may be fabricated during the same etching process used to fabricate the main contact bond pads.
[0091] The disclosure of the present invention is not limited to the power MOSFET example shown in the accompanying drawings. In addition, the disclosure of the present invention is not limited to the specific layered structure of the semiconductor device as shown in the accompanying drawings. It is understood that the proposed passivation layer groove can be applied to other semiconductor devices and other layered structures of semiconductor devices to achieve tensile stress σ SiNx of reduction.
[0092] Other features and advantages of the present disclosure will be apparent from the description and from the claims.
Claims
1. A method (1100) of manufacturing a semiconductor device (400, 500, 600, 610, 700, 710, 720, 730, 800, 900, 910, 920, 1000), the method comprising: forming (1102) a metal layer (404, 1004) over a silicon epitaxial layer (104, 304, 402, 1002) of the semiconductor device, the metal layer comprising an edge (1010) at which the metal layer terminates; forming (1104) a passivation layer (406) at least partially covering the metal layer; as well as forming (1106) a passivation layer groove (450, 502, 606, 616, 618, 706, 716, 718, 726, 728, 736, 806, 906, 916, 926, 1050) in the passivation layer, wherein the passivation layer groove is at least partially positioned above the metal layer, and wherein the passivation layer groove divides the passivation layer into a plurality of regions (452, 454, 1052, 1054), wherein each region is subjected to a reduced tensile stress σ due to the passivation layer groove SiNx , The passivation layer groove is formed as a continuous passivation layer groove (606, 616, 618, 806, 906, 916, 926). Wherein, the passivation layer groove is a polygonal shape, The passivation layer groove is formed into one of the following: a serpentine passivation layer groove (806); a honeycomb passivation layer groove (906); a cross-shaped passivation layer groove (916); or a sawtooth-shaped passivation layer groove (926).
2. The method according to claim 1, wherein: The passivation layer groove is positioned above the metal layer to form a first region (452) in the passivation layer and a second region (454) in the passivation layer, wherein the first region does not have an anchor point with the edge of the metal layer, and wherein the second region has an anchor point (416) with the edge of the metal layer.
3. The method according to claim 2, wherein: The second region has an average width L measured from the passivation layer groove to the anchor point. B , wherein the anchor point is located at a distance L0 from the middle of the tube core, and wherein L B In the range of L0 / 10 to L0 / 10000.
4. The method according to claim 1, wherein: The passivation layer groove is positioned above the edge of the metal layer to form a first region (1052) in the passivation layer and a second region (1054) in the passivation layer, wherein the first region and the second region do not have an anchor point with the edge of the metal layer.
5. The method according to claim 4, wherein: One edge of the passivation layer groove is placed above the metal layer, while the other edge of the passivation layer groove is placed outside the metal layer but still on top of the barrier base (1008).
6. The method according to any one of claims 1 to 5, wherein: The passivation layer grooves are formed as discontinuous passivation layer grooves (706, 716, 718, 726, 728, 736).
7. The method according to claim 6, wherein: The passivation layer grooves are formed as a series of through holes.
8. A method according to any one of the preceding claims, wherein: The passivation layer groove follows the edge of the metal layer.
9. The method according to any one of the preceding claims, further comprising: A portion defined as a controlled fracture zone is formed at a position in the passivation layer where the passivation layer groove is not formed, and the controlled fracture zone is configured to concentrate tensile stress in the passivation layer to the controlled fracture zone.
10. The method according to claim 9, wherein: The controlled fracture zone is formed between the passivation layer grooves.
11. A semiconductor device (400, 500, 600, 610, 700, 710, 720, 730, 800, 900, 910, 920, 1000), comprising: a metal layer (404, 1004) formed over the silicon epitaxial layer (104, 304, 402, 1002) of the semiconductor device, the metal layer comprising an edge (1010) at which the metal layer terminates; a passivation layer (406) at least partially covering the metal layer; as well as A passivation layer groove (450, 502, 606, 616, 618, 706, 716, 718, 726, 728, 736, 806, 906, 916, 926, 1050) in the passivation layer, wherein the passivation layer groove is at least partially positioned above the metal layer, and wherein the passivation layer grooves are configured to divide the passivation layer into a plurality of regions (452, 454, 1052, 1054), wherein each region is subjected to a reduced tensile stress σ due to the passivation layer grooves SiNx , Wherein, the passivation layer groove is a continuous passivation layer groove (606, 616, 618, 806, 906, 916, 926), Wherein, the passivation layer groove is a polygonal shape, The passivation layer groove is one of the following: a serpentine passivation layer groove (806); a honeycomb passivation layer groove (906); a cross-shaped passivation layer groove (916); or a sawtooth-shaped passivation layer groove (926).
12. The semiconductor device according to claim 11, wherein The semiconductor device is a power MOSFET.