Method for producing a dry electrode on a current collector by means of a rolling device
By using multiple rollers and a control unit in the rolling equipment to adjust the lamination gap, the problems of incomplete layers and roller clogging in dry electrode manufacturing are solved, achieving high-quality and efficient electrode production and reducing costs and maintenance. need.
Patent Information
- Application Number
- CN202410358361.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-03-30
- Filing Date
- 2024-03-27
- Publication Date
- 2024-10-01
AI Technical Summary
When using roller pressing equipment to manufacture dry electrodes, incomplete layers are prone to occur, resulting in poor electrode quality, and the roller gap is blocked, affecting equipment operation and cost.
Using a rolling equipment with three rollers, the lamination gap is adjusted through the control unit so that the powder forms a consistent thin layer between the second and third rollers, and the defective powder is processed through the removal device to ensure that the powder Apply evenly to the current collector to avoid roller clogging.
It improves the quality and manufacturing efficiency of dry electrodes, reduces costs, reduces the maintenance requirements of roller pressing equipment, and ensures high-quality electrode production.
Smart Images

Figure CN118738255A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates generally to the field of electrode manufacturing and in particular dry electrode manufacturing. In particular, the present invention relates to a method for manufacturing a dry electrode on a current collector by means of a roller pressing device, a roller pressing device, a dry electrode, a computer program product and a computer readable medium. Background Art
[0002] When dry electrodes are produced using a multi-roll calender or a roller press, a state occurs when the process is started in which incomplete layers are present on the rollers. If these incomplete layers are laminated onto the current collector, poor-quality electrodes or even unusable electrodes are produced.
[0003] If this continues, an incomplete layer may not be completely transferred to the current collector and the coating may remain partially on the roller. If material is fed back to the film-forming gap, this may clog the rolling gap (Walzenspalt, sometimes called roller gap), so that the process must be stopped and, in the worst case, the roller may be damaged. Summary of the invention
[0004] The object of the present invention is to at least partially overcome the disadvantages described above. In particular, the object of the present invention is to improve the efficiency and reliability of the method for manufacturing a dry electrode and to reduce the costs when manufacturing a dry electrode by such a method. In addition, the object of the present invention is to improve the quality of the dry electrode manufactured by such a method.
[0005] The above-mentioned task is solved by a method for manufacturing a dry electrode on a current collector by means of a rolling device with the features described below, by a rolling device with the features described below, by a dry electrode with the features described below, by a computer program product with the features described below, and by a computer-readable medium with the features described below. Other features and details of the present invention are derived from the description and the drawings. Here, the features and details described in terms of the method according to the present invention are obviously also applicable in terms of the rolling device, dry electrode, computer program product and / or computer-readable medium according to the present invention and vice versa, respectively, so that the disclosure of the various inventive aspects is always mutually referenced or can be mutually referenced.
[0006] With the embodiments of the invention, an improved method for producing dry electrodes on current collectors by means of a roller press can be provided in an advantageous manner. With such a method, high-quality dry electrodes can be produced cost-effectively and reliably.
[0007] One aspect of the present disclosure relates to a method for manufacturing a dry electrode on a current collector by means of a roller pressing device. The roller pressing device has at least three rollers and a current collector arranged between a second roller of the at least three rollers and a third roller of the at least three rollers. The method has the following steps:
[0008] rotating a first roller and a second roller of the at least three rollers in opposite rotational directions,
[0009] pouring the powder into a calendering gap formed by a rotating first roller and a rotating second roller, where the powder is guided at the second roller,
[0010] triggering a signal for adjusting the lamination gap between the second roller and the third roller by means of a control unit, wherein the third roller and / or the first roller and the second roller are moved towards each other towards the current collector,
[0011] rotating at least a third roller of the at least three rollers in a direction opposite to the second roller, and
[0012] • Move the current collector through the lamination gap.
[0013] The lamination gap is adjusted in this case such that the powder is applied as a thin layer on the current collector for the formation of a dry electrode.
[0014] In other words, a method for producing a dry electrode on a current collector by means of a roller pressing device is proposed, which method provides that the roller pressing device is first started before the powder is applied as a thin layer on the current collector as a whole. It is thus possible to distinguish between two states or operating states. Before the signal for adjusting the lamination gap is triggered, the roller pressing device can be operated in the operation or state being started. After the signal for adjusting the lamination gap is triggered, the roller pressing device can be operated in the operation or state that has been started.
[0015] The lamination gap may be a gap that is arranged between at least two rollers and through which the current collector may be arranged and preferably may pass. In contrast to the lamination gap, the calendering gap is the spacing between at least two rollers through which the powder may be poured. There is usually only one roller between the lamination gap and the calendering gap. In the recompression process, two rollers may be arranged between the lamination gap and the calendering gap.
[0016] The powder can be a powdered material. The powder preferably contains no solvent and is converted into a layer by means of a rolling device. The powder has in particular an active material, a conductive additive and a binder. The components of the powder can be mixed in the preparatory stage of the method for producing a dry electrode. The electrode can be referred to as a double layer or a single layer layer applied to a substrate. The electrode can be, for example, a double layer cathode material and / or a double layer anode material.
[0017] The current collector may be referred to as a current collector or a substrate. The current collector may have as a main function to serve as a substrate for the thin layer.
[0018] The quality of the manufactured electrode can depend on the distribution of the powder or powdered material as a thin layer. High-quality electrodes are preferably produced by a consistent thin layer. Therefore, it can prove to be advantageous to apply the powder to the current collector only when the powder directed onto the second roller forms a consistent thin layer.
[0019] For this purpose, the method provides that rollers which together form a calendering gap are rotated. In the calendering gap, preferably powder is already poured, which is guided at or on the second roller. The powder can thus be at least partially formed into a thin layer in the calendering gap by the calendering process. However, usually the powder first only forms an incomplete thin layer or a layer which may have defects. The powder which is partially turned into a thin layer may have cracks, orifices, etc. Such an incomplete or defective layer is therefore not usable for an electrode or only results in an electrode of poor quality.
[0020] The method is therefore provided that the laminating gap is only adjusted when a signal is triggered by means of the control unit. The triggering of the signal can be synonymous with the transition to the started state. The signal is preferably triggered when the powder now forms a uniform thin layer on the second roller. The signal is preferably triggered when the layer(s) carried by the roller are completely present on the roller.
[0021] Specifically, the control unit can trigger a signal according to a user's command. The user of the roller pressing device can observe the powder or the thin layer and decide accordingly that the lamination gap should be adjusted at this time, that is, so that the powder can be applied as a thin layer to the current collector for the construction of the dry electrode.
[0022] Alternatively or additionally, the control unit can trigger a signal after a preset number of rotations of the roller based on an empirical value. Alternatively or additionally, a removal device, for example, arranged at the second roller can obtain how much powder has been removed from the corresponding roller, so that the control unit can trigger a signal based on the obtained amount of removed powder.
[0023] When the signal has been triggered for adjusting the lamination gap, the rollers of the rolling device can be controlled by the control unit in such a way that the lamination gap is reduced around the current collector. All rollers arranged on one side of the current collector can move synchronously in a radial direction toward the current collector. Alternatively, not only the rollers on one side of the current collector but also the rollers on the other side of the current collector can move radially toward the current collector. If the powder is applied to the current collector as a thin layer on both sides, it can be proved to be advantageous to move the rollers toward the current collector from both sides of the current collector. In the case of adjusting the lamination gap, the spacing between two adjacent rollers arranged around the current collector is adjusted and especially reduced. It should be noted that the lamination gap does not have to be constant when the rolling device is running.
[0024] The width of the laminating gap can be adjusted by the control unit further in the activated state. The laminating gap can be adjusted force-controlled or stroke-controlled.
[0025] The lamination gap can be varied when the powder is applied as a thin layer. The lamination gap can be varied in this respect, i.e. the powder can continue to be applied as a thin layer even when it is varied. The force-controlled regulation of the lamination gap takes into account the force or pressure applied to the current collector when the powder is applied as a thin layer. If the force and / or pressure acting on the current collector increases, the lamination gap is adjusted to be wider. However, this means that the thin layer also becomes thicker. In the force-controlled regulation of the lamination gap, it can be provided that the electrode thus produced is reprocessed in order to adjust the thickness of the electrode.
[0026] In the stroke-controlled regulation of the lamination gap, the actual spacing between the current collector and the adjacent roller or between two adjacent rollers around the current collector is regulated. In the stroke-controlled regulation of the lamination gap, the lamination gap can be constant throughout the started operation or state.
[0027] As soon as the remaining rollers of the rolling device rotate, the lamination gap can be adjusted, more precisely, so that the powder can now be applied to the current collector as a thin layer. Alternatively, the remaining rollers of the rolling device can be put into motion simultaneously with the current collector. However, it can be important that the remaining rollers first rotate or at least rotate freely before the lamination gap is retracted (zusammengefahren), because otherwise web cracks can occur. In an embodiment in which the thin layer is only applied on one side of the current collector, the third roller is now brought into rotation. In an embodiment of the rolling device that is symmetrical around the current collector, it can be conceivable that all rollers of the rolling device have rotated before the lamination gap is adjusted. It can be important that all rollers adjacent to the pouring device have rotated before the lamination gap is adjusted.
[0028] Directly after the adjustment or triggering signal for adjusting the lamination gap, the current collector can move or pass through the second and third rollers. During the entire time in which the lamination gap is too wide to apply powder to the current collector at all, the current collector and the current collector film can be stationary. Energy can thus be saved.
[0029] It should be noted that when the rolling device is constructed symmetrically around the current collector, a two-sided dry electrode can be produced. The powder can thus be poured into two calendering gaps and the two layers are accordingly guided at the rollers adjacent to the current collector.
[0030] This method can provide high-quality electrodes in an efficient and precise manner. This method can also avoid or at least reduce the clogging of the roller press. This method can reduce the maintenance expenditure of the roller press for producing dry electrodes.
[0031] According to one embodiment of the method, the method further comprises at least one of the following steps:
[0032] · Obtain the thickness of the powder that has become a thin layer at the second roller, and
[0033] Triggering a signal based on the detected thickness by means of a control unit.
[0034] In order to avoid the powder being applied to the current collector as an incomplete thin layer, it can be configured to obtain the thickness of the powder that has become a thin layer at the second roller, or alternatively, additionally at the third roller. This can be performed with the aid of a layer thickness sensor. Alternatively or additionally, the camera can film the second roller, or alternatively also the third roller, and play back the filmed content on the user interface. The user can obtain whether the thickness of the powder that has become a thin layer meets a preset standard, such as, for example, a preset thickness, based on the filmed content of the second roller and / or the third roller. Alternatively or additionally, an artificial intelligence-based program can run on the filmed content filmed by the camera.
[0035] It should be noted that the layer should not only have a preset thickness, but also have at least substantially constant thickness over a preset section. In other words, a signal can be triggered by means of a control unit when the acquired thickness meets a preset criterion. The preset criterion can be surface load, minimum defect-free area, etc.
[0036] As a result, the triggering time of the signal can be adjusted more accurately, thereby further improving the quality of the produced electrode.
[0037] According to one embodiment of the invention, the method further comprises the step of removing the powder guided at the second roller, in particular the powder that has become a defective thin layer, by means of a removal device, which is arranged after the laminating gap in the direction of rotation. The removed powder guided at the second roller can be a defective layer located on the second roller, i.e., for example, a layer with an incorrect thickness or an irregular thickness. The removal of the powder guided at the second roller, which preferably has at least partially become a defective layer, can be performed during the start-up operation.
[0038] Thus, material or powder that is not applied to the current collector is removed at the corresponding rollers, both during startup and during operation of the roller press, which minimizes the risk of blockage at the corresponding rollers of the roller press.
[0039] The powder or material that has been removed by the removal device can be supplied to the pouring device again. The powder can thus be reused and the powder consumption in the case of producing electrodes can be reduced. Before the removed powder can be directed again, it can prove to be advantageous to process the removed powder in a preceding process step.
[0040] According to one embodiment of the method, the rotational speeds of the first roller, the second roller, the third roller and / or the passing speed of the current collector are controlled by means of a control unit, preferably based on the detected thickness of the powder formed into a thin layer.
[0041] In other words, the rolling device and in particular the rollers of the rolling device can be controlled in such a way that predefined criteria are met, such as, for example, the surface load of the powder formed into a thin layer, the thickness of the thin layer, etc. The thickness of the powder formed into a thin layer can depend on the rotational speed of the rollers of the rolling device and vice versa.
[0042] This allows high-quality electrodes to be produced.
[0043] According to one embodiment of the method, during the removal of powder guided past the second roller, in particular powder that has become a defective layer, the powder is captured and / or sucked away by the removal device.
[0044] According to one embodiment of the method, a signal is triggered after a predefined time for adjusting the laminating gap between the second roller and the third roller.
[0045] The roller pressing device may, for example, have a virtual twin. Based on simulations or experiments using the virtual twin of the roller pressing device, it can be known that after a predefined time, the thickness, surface load and / or other parameters of the powder formed into a thin layer meet preset criteria. Such a predefined time can, for example, be stored in a storage medium of the control unit. The signal for adjusting the lamination gap can therefore be automatically triggered after a predefined time.
[0046] The predefined time may likewise be based on experimental and / or empirical data.The predefined time may thus be stored by a user in a storage medium of the control unit, for example by means of a user interface.
[0047] Furthermore, it can be provided that the predefined time defines a maximum time. In other words, the signal is triggered after the maximum time, for example independently of the thickness detected. This can prove advantageous, for example, if the control unit is set up, for example, to trigger the signal only upon a command from a user. If the user forgets to output a command, it can be avoided that the rolling device is kept running for an unnecessarily long time in the starting operation or state.
[0048] It may also prove to be advantageous to trigger the signal after a predefined time if, for example, a layer thickness sensor is malfunctioning and therefore cannot reliably trigger a signal based on the detected thickness.
[0049] According to one embodiment of the method, the method further comprises at least one of the following steps:
[0050] Obtain the amount of powder that has been poured into the calendering gap, and / or
[0051] Obtaining the rotation of the second roller,
[0052] Based on the detected amount of powder and / or the detected ongoing rotation of the second roller, a signal is triggered by means of the control unit.
[0053] In order to be able to determine which amount of powder has been poured into the calendering gap, provision can be made to determine the amount of powder removed from the metering unit.
[0054] It should be noted that when the roller pressing device is stopped, the exact opposite can be done in order not to transfer an unusable coating to the current collector. In other words, it can be provided that when the roller pressing device is stopped, the lamination gap is first adjusted in such a way that the powder cannot be applied as a thin layer to the current collector. The corresponding roller can only be stopped after the lamination gap has been adjusted accordingly, i.e. after the lamination gap has been increased.
[0055] A second aspect of the present disclosure relates to a rolling device for manufacturing dry electrodes on a current collector. The rolling device has a control unit, at least three rollers, and a current collector arranged in a lamination gap, which is configured to capture powder that has become a thin layer. The lamination gap is defined here as the spacing between the first roller among the at least three rollers and the second roller among the at least three rollers. The rolling device also has a pouring device, which is configured to pour powder into the calendering gap. The calendering gap is defined here as the spacing between the first roller and the second roller. The rolling device also has a removal device, which is set up to remove the powder guided at the second roller. The removal device is arranged after the lamination gap in the direction of rotation. The control unit is set up here to trigger a signal for adjusting the lamination gap, especially the thickness of the lamination gap.
[0056] The advantages explained above and below with reference to this method also apply to the roller pressing device.
[0057] According to one embodiment of the roller pressing device, the roller pressing device further comprises a layer thickness sensor which is designed to detect the thickness of the powder formed into a thin layer on the second roller, in particular in the direction of rotation before the laminating nip.
[0058] A third aspect of the present disclosure relates to a dry electrode manufactured by means of the method as described above and below.
[0059] A fourth aspect of the present disclosure relates to a computer program product comprising instructions which, when implemented, allow a control unit of a rolling device as described above and below to implement at least some of the steps of the method as described above and below.
[0060] A fourth aspect of the present disclosure relates to a computer-readable medium on which a computer program product as described above is stored.
[0061] All disclosures and advantages described above and below with respect to one aspect of the disclosure are equally applicable to all other aspects of the disclosure. BRIEF DESCRIPTION OF THE DRAWINGS
[0062] In the following, embodiments of the present invention are described with reference to the accompanying drawings.
[0063] Figure 1 Schematically shows a side view of a rolling device according to an embodiment,
[0064] Figure 2 Schematically shows a top view of a rolling device according to an embodiment,
[0065] Figure 3 Schematically shows a side view of a rolling device according to another embodiment,
[0066] Figure 4 Schematically shows a side view of a rolling device according to another embodiment, Figure 5 and 6 The roller of the rolling device according to one embodiment is schematically shown, and
[0067] Figures 7 to 9 A side view of a rolling device according to a further exemplary embodiment is schematically shown.
[0068] Similar, similarly acting, identical or identically acting elements are provided with similar or identical reference symbols in the figures. The figures are merely schematic and are not drawn to scale. DETAILED DESCRIPTION
[0069] Figure 1 A side view of a rolling device 100 according to an embodiment is schematically shown. Such a rolling device 100 can be used to perform a method for manufacturing a dry electrode 10 on a current collector 12. Figure 1The rolling device 100 has four rollers. A gap is provided between the first roller 13 and the second roller 14, which is called the calendering gap 20. The first roller 13 can be called the coating roller. The gap between the third roller 15 and the fourth roller 16 is also called the calendering gap 20. Such a pressing roller unit can have one or more rollers. A gap is also provided between the second roller 14 and the third roller 15, which is however called the lamination gap 18. The current collector 12 is arranged in the lamination gap 18. The second roller 14 and the third roller 15 can be part of the pressing roller unit. The second roller 14 and the third roller 15 can therefore be called pressing rollers. The lamination gap 18, which can also be called the pressing gap, can be implemented to be used for transferring the powder 11 that becomes a thin layer from the rollers of the pressing roller unit, that is, from the second roller 14 and / or from the third roller 15 to one side of the current collector 12 and, if necessary, to both sides by means of a pressing force. For the sake of completeness it should be noted that the rollers are cylindrical in design and are preferably arranged parallel to one another with respect to their axial axes.
[0070] Figure 1 The rolling device 100 is constructed substantially symmetrically around the current collector 12. That is, the powder 11 may be applied in a thin layer on both sides of the current collector 12. Figure 1 The elements and / or components described on one side of the current collector 12 of the rolling device 100 may also be located mirror-symmetrically. Figure 1 The other side of the current collector 12 of the roller pressing device 100 is provided. By applying the thin layer to both sides of the current collector 12, the efficiency of the dry electrode 10 can be improved. The produced dry electrode 10 is composed of a thin layer and a current collector 12. Depending on whether the current collector 12 is coated with a thin layer on both sides, it can be referred to as a single-sided dry electrode 10 or a double-sided dry electrode 10. Asymmetric embodiments are also conceivable (see Figure 7 ).
[0071] exist Figure 1 In the case of a roller pressing device 100, two rollers, a first roller 13 and a second roller 14, are arranged on a first side of the current collector 12 or on the left side of the current collector 12. A pouring device 26 set up for pouring the powder 11 can be at least partially arranged in the two calendering gaps 20 of the roller pressing device 100. The pouring device 26 can be called a dosing unit. In addition, a removal device 22 can be provided on one of the two sides of the current collector 12. The two rollers arranged closest to the current collector 12 can be provided with such a removal device 22. The removal device 22 can have a scraper 23 and a capture device 24.
[0072] The first roller 13 and the second roller 14 are set up for rotation in opposite directions. The powder 11 can be poured into the calendering gap 20 between the first roller 13 and the second roller 14 by means of a pouring device 26. The powder 11 is then guided at the second roller 14.
[0073] Figure 1 The roller pressing device 100 is in operation, in particular in started operation. This can be seen from Figure 1 It is known that the lamination gap 18 is adjusted so that the powder 11 poured into the corresponding calendering gap 20 becomes a thin layer and is applied to the current collector 12 as a thin layer to form the dry electrode 10. That is, the lamination gap 18 is small enough to allow the powder 11 to be applied to the current collector 12 as a thin layer.
[0074] Figure 2 A top view of a rolling device 100 according to an embodiment is schematically shown. Figure 2 The rolling device 100 may be, for example, Figure 1 Unless otherwise described, Figure 2 The rolling device 100 has Figure 1 The two thin layers, which are respectively directed onto the second roller 14 and the third roller 15, are then applied onto the current collector 12. In order to be able to adjust the predetermined width of the dry electrode 10, each roller may be provided with at least one edge trimming piece 30, preferably two edge trimming pieces 30. The edge trimming piece 30 can accurately define or trim the edge or edge of the dry electrode 10. With the aid of the edge trimming piece 30, the width of the (multiple) electrodes 10 can be adjusted. In order to remove the excess material or powder 11 that remains beyond the edge or the powder 11 that has become a layer, a removal unit 28 is preferably arranged directly next to the edge trimming piece 30. The removal unit 28 can remove or capture the material. The removal unit 28 can have a capture container. The removal unit 28 can also have a scraper 23, with which the corresponding roller can be cleaned.
[0075] The powder 11 guided onto the second roller 14 and the third roller 15 forms a thin layer. Once the thin layer is applied to the current collector 12, the thin layer can be called a dry electrode 10. In order to be able to manufacture a functional dry electrode 10, the thin layer must be formed as uniformly as possible. The thin layer must be formed without defects or flaws. Cracks, pores and / or fractures in the layer can be regarded as defects, for example. Preferably, the thin layer also has a preset minimum layer thickness. Figure 2 The thin layer or dry electrode 10 has no defects. It can be seen that Figure 2 The roller pressing device 100 is also in operation, in particular in the started operation. Because the roller pressing device 100 according to the invention is designed to capture the powder 11 in a thin layer by means of the current collector 12 only in the started operation.
[0076] Figure 3 A side view of a rolling device 100 according to an embodiment is schematically shown. Unless otherwise described, Figure 3The rolling device 100 has Figure 1 and 2 The same elements and features as the rolling equipment.
[0077] and Figure 1 and 2 Compared with the rolling equipment 100, Figure 3 The roller pressing device 100 is in the operation being started, that is, not yet in the operation that has been started. The gap between the second roller 14 and the third roller 15, that is, the laminating gap 18, is larger in the operation being started than in the operation that has been started. Figure 3 The lamination gap 18 of the roller pressing device 100 is adjusted in such a way that the powder 11 and / or the partially thinned powder 11 cannot be placed on the current collector 12. Therefore, during the start-up operation, it can prove to be advantageous, for example, to save energy in order not to move the current collector 12 through the lamination gap 18.
[0078] exist Figure 3 The second roller 14 and the third roller 15 of the rolling device 100 present fragments 19 or debris of the powder 11. The fragments 19 can form a defective layer. The powder 11 poured into the calendering gap 20 has not yet become a thin layer during the startup operation. On the contrary, the thin layer has just begun to form, which leads to the appearance of fragments 19 or debris of the powder 11. The powder 11 is only partially turned into a thin layer in the startup state. In other words, the quality of the thin layer is not enough to make a dry electrode 10 from it. It is therefore advantageous to remove the fragments 19 or debris of the powder 11. This is achieved with the help of a removal device 22. The removal device 22 can be oriented to remove the powder 11 at the second and / or third roller 15, preferably after the lamination gap 18 in the direction of rotation. In addition, it can be arranged that the removal device 22 cleans or cleans the corresponding roller when removing the powder 11 or the fragments 19. For this purpose, the removal device 22 can have a scraper 23. In order to remove the material, ie the powder 11 and / or the fragments 19, from the respective rollers, the removal device 22 preferably has a catch device 24. The catch device 24 can mechanically catch the material and / or suck it away.
[0079] Figure 3 The roller pressing device 100 further comprises a layer thickness sensor 17. The layer thickness sensor 17 is preferably arranged in front of the laminating gap 18 in the direction of rotation. It is also conceivable that another layer thickness sensor 17 is arranged in front of the laminating gap 18. Figure 3 The third roller 15 of the roller pressing device 100 is provided. Because the powder 11 which is formed into a thin layer is also guided at the third roller 15.
[0080] The thickness of the powder 11 at least partially turned into a thin layer can be acquired or measured by means of the layer thickness sensor 17. When the thickness of the powder 11 and / or the powder 11 at least partially turned into a thin layer is acquired, it can be determined or the control unit can determine whether the acquired thickness meets a preset criterion. If the acquired thickness meets the preset criterion, the control unit can trigger a signal for adjusting the lamination gap 18. When adjusting the lamination gap 18, the third roller 15 can move towards each other towards the current collector 12, especially together with the fourth roller 16 and / or the first roller 13 and the second roller 14.
[0081] Figure 4 A side view of a rolling device 100 according to an embodiment is schematically shown. Unless otherwise described, Figure 4 The rolling device 100 has Figures 1 to 3 The same elements and features as the rolling device 100.
[0082] exist Figure 4 It can be seen that no dry electrode 10 or thin layer is applied on the current collector 12. From this point, it can be recognized that Figure 4 The rolling device 100 is still in the process of starting up. Figure 3 In contrast, the powder 11 guided at the second roller 14 and the third roller 15 forms a uniform thin layer. In other words, the roller pressing device 100 has been running long enough in the starting operation and has thus transitioned to the started operation. The control unit (not shown here) of the roller pressing device 100 can therefore trigger a signal to adjust the lamination gap 18 in such a way that the powder 11 that has become a thin layer can now be applied to the current collector 12. In order to adjust the lamination gap 18, the rollers can be moved in pairs, that is, the first and second rollers 14 together and / or the third and fourth rollers 16 together in the radial direction toward the current collector 12. The paired movement of the rollers makes it possible to keep the corresponding calendering gap 20 constant. In an asymmetric embodiment of the roller pressing device 100, it is conceivable that, for example, only two rollers move toward the current collector 12 on one side of the current collector 12. The corresponding rollers move radially toward the current collector 12 until the powder 11 that has become a thin layer can be applied to the current collector 12. The radial movement or multiple radial movements are by means of Figure 4 The arrow in the figure is shown.
[0083] Figure 5 and 6 The rollers of a rolling device 100 according to an embodiment are schematically shown. Figure 5 and 6 The roller shown in the figure may be the third roller 15. If Figure 5 and 6 If the roller of 100 is viewed in mirror-inverse form, this may also be the second roller 14 of the rolling device 100 .
[0084] As reference Figures 1 to 4 As described, a removal device 22 may be arranged at the second roller 14 and optionally also at the third roller 15. The removal device 22 may be used on the one hand to remove material at the corresponding roller and on the other hand to clean the corresponding roller. In order to clean the corresponding roller, the removal device 22 may have a brush 25. The brush 25 may be a rotating brush. A cleaning device 34 may be further provided after the removal device 22 in the direction of rotation of the roller. In addition to the removal device 22, the cleaning device 34 may also additionally clean the surface of the roller. The cleaning device 34 may have one or more cleaning rollers 38, which are designed to apply fiber material or nonwoven material to the surface of the corresponding roller or to press it onto the roller. A higher cleaning effect can thereby be achieved. The fiber material can be unwound from one reel 33 via the cleaning roller 38 and then rolled up again onto another reel 33. Figure 6 In the embodiment of can additionally be provided that the cleaning agent is applied to the surface of the fiber material and / or the corresponding roller. Figure 5 In the embodiment of the present invention, the cleaning of the roller can be carried out dry.
[0085] Figures 7 to 9 FIG. 1 shows a schematic side view of a rolling device 100 according to a further embodiment. Unless otherwise described, Figures 7 to 9 The rolling device 100 has Figures 1 to 4 The same elements and features as the rolling device 100.
[0086] In principle, any configuration of rollers is conceivable which enables the thin layer to be applied to one or both sides of the current collector 12. It is also conceivable to produce a dry electrode 10 that is only one-sided. In this case, the rolling device 100 can have only three rollers. In this way, for example, only one roller can be provided. Figure 7 The lower three rollers of the rolling device 100. Fig. 9 In addition, four rollers can be provided for transferring the thin layer onto the current collector 12. In other words, it is conceivable to provide a pressing roller unit with four pressing rollers. The powder 11 pressed flat on Fig. 9 In the exemplary case of , it is therefore guided on two second rollers 14 , 14 ′ and likewise on two third rollers 15 , 15 ′.
[0087] In addition, it should be pointed out that the terms "comprising" and "having" do not exclude other elements, and the indefinite article "a" or "an" does not exclude a plurality. Furthermore, it should be pointed out that features and steps that have been described with reference to one of the above embodiments can also be used in combination with other features and steps of other embodiments described above. Reference numerals in the claims should not be considered as limiting.
[0088] Reference Numbers List
[0089] 10 electrodes
[0090] 11 Powder
[0091] 12 current collectors
[0092] 13. First roller
[0093] 14 Second roller
[0094] 15Third roller
[0095] 16 Fourth roller
[0096] 17-layer thick sensor
[0097] 18Lamination gap
[0098] 19 pieces
[0099] 20 calendering gap
[0100] 22Remove device
[0101] 23 Scraper
[0102] 24 Capture Device
[0103] 25 brushes
[0104] 26Pouring device
[0105] 28 Take-away unit
[0106] 30 Edge cutting parts
[0107] 33 scrolls
[0108] 34 Cleaning device
[0109] 38 Cleaning roller
[0110] 100 Roller Pressing Equipment
Claims
1. A method for producing a dry electrode (10) on a current collector (12) by means of a roller pressing device, wherein the roller pressing device (100) has at least three rollers (13, 14, 15) and the current collector (12) is arranged between a second roller (14) of the at least three rollers and a third roller (15) of the at least three rollers, and wherein the method comprises the following steps: Rotating the first roller (13) and the second roller (14) of the at least three rollers in opposite directions of rotation, pouring the powder (11) into a calendering gap (20) formed by the rotating first roller (13) and the rotating second roller (14), wherein the powder (11) is guided at the second roller (14), triggering a signal for adjusting the lamination gap (18) between the second roller (14) and the third roller (15) by means of a control unit, wherein the third roller (15) and / or the first roller (13) and the second roller (14) are moved towards each other towards the current collector (12), rotating at least the third roller (15) of the at least three rollers in a direction opposite to the second roller (14), and · moving the current collector (12) through the lamination gap (18), The lamination gap (18) is adjusted in such a way that the powder (11) is applied as a thin layer to the current collector (12) for forming the dry electrode (10).
2. The method according to claim 1, characterized in that The method further comprises at least one of the following steps: Obtaining the thickness of the powder (11) formed into a thin layer at the second roller (14), and The signal is triggered by means of the control unit based on the detected thickness.
3. The method according to claim 1 or 2, characterized in that: The method further comprises the following steps: Powder (11) guided over the second roller (14), in particular powder (11) that has become a defective thin layer, is removed by a removal device (22) which is arranged downstream of the laminating gap (18) in the direction of rotation.
4. The method according to any one of the preceding claims, characterized in that The rotation speeds of the first roller (13), the second roller (14), the third roller (15) and / or the passing speed of the current collector (12) are controlled by means of the control unit, preferably based on the thickness of the powder (11) obtained to be turned into a thin layer.
5. The method according to any one of the preceding claims, characterized in that In the case of removing powder (11) guided at the second roller (14), in particular powder (11) that has become a defective thin layer, the powder (11) is captured and / or sucked away by the removal device (22).
6. The method according to any one of the preceding claims, characterized in that After a predefined time, the signal is triggered for adjusting the laminating gap (18) between the second roller (14) and the third roller (15).
7. The method according to any one of the preceding claims, characterized in that The method further comprises at least one of the following steps: Obtaining the amount of powder that has been poured into the calendering gap (20), · obtaining the rotation of the second roller (14), The signal is triggered by means of the control unit based on the detected amount of powder and / or the detected ongoing rotation of the second roller (14).
8. A roller pressing device (100) for manufacturing a dry electrode (10) on a current collector (12), comprising: Control unit, At least three rollers, a current collector (12) arranged in a lamination gap (18) configured to capture the powder (11) in a thin layer, wherein the lamination gap (18) defines the spacing between a first roller (13) of the at least three rollers and a second roller (14) of the at least three rollers, a pouring device (26) configured to pour the powder (11) into the calendering gap (20), wherein the calendering gap (20) is defined as a spacing between the first roller (13) and the second roller (14), and a removal device (22) which is designed to remove the powder (11) guided at the second roller (14), wherein the removal device (22) is arranged behind the laminating gap (18) in the direction of rotation, The control unit is designed to trigger a signal for adjusting a lamination gap (18), in particular a thickness of the lamination gap (18).
9. The rolling device (100) according to claim 8 further has a layer thickness sensor (17), which is designed to obtain the thickness of the powder (11) that has been transformed into a thin layer at the second roller (14) before the laminating gap (18), especially in the rotational direction.
10. A dry electrode (10) produced by means of a method according to any one of claims 1 to 7.
11. A computer program product comprising instructions which, when implemented, allow a control unit of a rolling device (100) according to any one of claims 8 and 9 to implement at least some of the steps of the method according to any one of claims 1 to 7.
12. A computer readable medium having stored thereon a computer program product according to claim 11.