Method for manufacturing vibration element, vibration element, and vibration device

By forming a protective film in the piezoelectric vibration element and etching the metal layer, the problem of easy disconnection of the lead electrode is solved, a reasonable distribution of the thin-walled part and the thick-walled part of the electrode is achieved, and the excellent vibration characteristics and electrical conductivity of the vibrating element are ensured. reliability.

CN118740097APending Publication Date: 2024-10-01SEIKO EPSON CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410357893.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-29
Filing Date
2024-03-27
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In existing piezoelectric vibration elements, the lead electrode is prone to disconnection, especially in applications with high-frequency and thin-film electrodes, resulting in an increase in sheet resistance.

Method used

A vibration element manufacturing method is used to form a metal layer on the substrate, form a protective film in the connection area between the excitation electrode and the pad electrode, and etch the metal layer through the protective film to form the thin-walled portion and the thick-walled portion of the electrode. Make sure that the thickness of the extraction electrode is greater than that of the excitation electrode, and that the thin-walled part and the thick-walled part of the electrode are integrated to avoid overlap and disconnection.

Benefits of technology

It effectively suppresses the disconnection phenomenon of the extraction electrode, controls the increase in sheet resistance, and achieves excellent vibration characteristics and electrical reliability of the vibrating element.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118740097A_ABST
    Figure CN118740097A_ABST
Patent Text Reader

Abstract

The invention provides a method for manufacturing a resonator element, a resonator element, and a resonator device with excellent electrical connection. The resonator element includes: a substrate having a thin portion and a thick portion; and an electrode portion including an excitation electrode disposed in the excitation electrode placement region of the thin portion, a pad electrode disposed in the pad electrode placement region of the thick portion, and a lead-out electrode disposed in the lead-out electrode placement region of the substrate and connecting the excitation electrode and the pad electrode. The method of manufacturing a resonator element includes: a metal layer forming step of forming a metal layer on a substrate; a protective film forming step of forming a protective film in a region overlapping at least a part of the extraction electrode arrangement region in plan view on the metal layer; and a metal layer etching step in which the thickness of the metal layer disposed in the excitation electrode arrangement region is reduced by etching via the protective film.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for manufacturing a vibration element, a vibration element and a vibration device. Background Art

[0002] Patent document 1 discloses a piezoelectric vibration element of a so-called inverted mesa structure that achieves high frequency by forming a recessed portion in a part of the main surface. In order to suppress the expansion of stress caused by bonding and fixing, the piezoelectric vibration element has a gap between the thick wall portion and the vibration portion that fix the piezoelectric vibration element. In addition, since the thin film of the electrode is reduced along with the high frequency, especially in the narrow lead electrode that electrically connects the excitation electrode and the pad electrode, the thickness of the lead electrode is made thicker than the thickness of the excitation electrode to prevent the increase of the sheet resistance.

[0003] Patent Document 1: Japanese Patent Application Publication No. 2014-7693

[0004] However, in the piezoelectric vibration element of Patent Document 1, in order to make the thickness of the extraction electrode greater than the thickness of the excitation electrode, after the extraction electrode is formed, the extraction electrode having the same thickness as the excitation electrode is stacked in a manner overlapping a portion of the extraction electrode. In addition, the thin extraction electrode is stacked in a manner spanning the end portion, i.e., the step, of the previously formed thick extraction electrode. Therefore, there is a problem that the extraction electrode formed later at the step portion is easily disconnected. Summary of the invention

[0005] A method for manufacturing a vibration element, the vibration element comprising: a substrate having a thin-walled portion and a thick-walled portion having a thickness greater than that of the thin-walled portion; and an electrode portion having: an excitation electrode arranged in an excitation electrode arrangement area of ​​the thin-walled portion; a pad electrode arranged in a pad electrode arrangement area of ​​the thick-walled portion; and an extraction electrode connecting the excitation electrode to the pad electrode and arranged in an extraction electrode arrangement area of ​​the substrate, the method for manufacturing the vibration element comprising the following steps: a metal layer forming step of forming a metal layer on the substrate; a protective film forming step of forming a protective film in an area on the metal layer that overlaps with at least a portion of the extraction electrode arrangement area when viewed from above; and a metal layer etching step of thinning the metal layer arranged in the excitation electrode arrangement area by etching through the protective film.

[0006] A vibration element comprises: a substrate having a thin-walled portion and a thick-walled portion having a thickness greater than that of the thin-walled portion; and an electrode portion having: an excitation electrode arranged in an excitation electrode arrangement area of ​​the thin-walled portion; a pad electrode arranged in a pad electrode arrangement area of ​​the thick-walled portion; and an extraction electrode connecting the excitation electrode to the pad electrode and arranged in an extraction electrode arrangement area of ​​the substrate, the electrode portion comprising: a first electrode layer arranged in the pad electrode arrangement area, the extraction electrode arrangement area and the excitation electrode arrangement area on the substrate; and a second electrode layer arranged on the first electrode layer in an area overlapping with the pad electrode arrangement area, the extraction electrode arrangement area and the excitation electrode arrangement area when viewed from above, and having a thickness greater than that of the first electrode layer, the second electrode layer having: an electrode thin-walled portion overlapping with the excitation electrode arrangement area when viewed from above; and an electrode thick-walled portion overlapping with the extraction electrode arrangement area when viewed from above, and having a thickness greater than that of the electrode thin-walled portion.

[0007] The vibration device includes: the vibration element described above; and a package that accommodates the vibration element and fixes the vibration element via a bonding material. BRIEF DESCRIPTION OF THE DRAWINGS

[0008] Figure 1 It is a perspective view showing the structure of the vibration element according to the first embodiment.

[0009] Figure 2 This is a diagram for explaining the relationship between an AT-cut quartz substrate and the crystal axis of quartz.

[0010] Figure 3 yes Figure 1 A top view of the vibrating element is shown.

[0011] Figure 4 yes Figure 3 A1-A1 line section view.

[0012] Figure 5 yes Figure 3 A2-A2 line section view.

[0013] Figure 6 yes Figure 3 A3-A3 line section view.

[0014] Figure 7 is a flowchart showing a method for manufacturing a vibration element.

[0015] Figure 8 It is a cross-sectional view for explaining the manufacturing method of the vibration element.

[0016] Fig. 9 It is a cross-sectional view for explaining the manufacturing method of the vibration element.

[0017] Fig.10 It is a cross-sectional view for explaining the manufacturing method of the vibration element.

[0018] Fig.11 It is a cross-sectional view for explaining the manufacturing method of the vibration element.

[0019] Fig.12 It is a cross-sectional view for explaining the manufacturing method of the vibration element.

[0020] Fig.13 It is a cross-sectional view for explaining the manufacturing method of the vibration element.

[0021] Fig.14 It is a cross-sectional view for explaining the manufacturing method of the vibration element.

[0022] Fig.15 It is a plan view showing the structure of the vibration element according to the second embodiment.

[0023] Fig.16 yes Fig.15 B1-B1 line section view.

[0024] Fig.17 It is a perspective view showing the structure of a vibration element according to a third embodiment.

[0025] Fig.18 It is a cross-sectional view showing the structure of a vibration device according to a fourth embodiment.

[0026] Description of symbols

[0027] 1, 1a, 1b: vibration element; 2: vibration device; 10: substrate; 11: thin-walled portion; 12: thick-walled portion; 13: excitation electrode configuration area; 14: pad electrode configuration area; 15: extraction electrode configuration area; 16: first area; 17: second area; 21: first outer edge; 22: second outer edge; 23: third outer edge; 24: fourth outer edge; 25, 26: connection portion; 30: electrode portion; 31, 32: excitation electrode; 33, 34: pad electrode; 35, 36: extraction electrode; 37: electrode thickness Wall portion; 38: electrode thin-wall portion; 40: metal layer; 41: first electrode layer; 42: second electrode layer; 50: package; 51: recessed portion; 52: storage space; 53: inner bottom surface; 54: second surface; 55: first surface; 56, 57: connecting electrodes; 58, 59: external mounting terminals; 60: cover; 61: bonding material; 62: bonding wire; 71: base film; 72: metal film; 73: protective film; 74: recessed portion; 75: protective film; T1, T2: thickness; L: maximum length; W: maximum width. DETAILED DESCRIPTION

[0028] 1. First Implementation

[0029] 1.1. Vibration element

[0030] Reference Figure 1 to Figure 6 The vibration element 1 according to the first embodiment will be described.

[0031] In addition, for the sake of convenience, Figure 2 and Figure 7 In the subsequent figures other than the above, the X-axis, Y'-axis, and Z'-axis are illustrated as three mutually perpendicular axes. In addition, the length direction of the vibration element 1 is referred to as the "X direction" as the direction along the X-axis, the thickness direction of the vibration element 1 is referred to as the "Y' direction" as the direction along the Y' axis, and the direction perpendicular to the X-axis and the Y' axis is referred to as the direction along the Z' axis as the "Z' direction". In addition, the arrow side of each axis is also referred to as the "positive side", and the side opposite to the arrow is referred to as the "negative side". In addition, the positive side of the Y' direction is also referred to as the "front side", and the negative side of the Y' direction is referred to as the "back side".

[0032] like Figure 1 As shown, the vibration element 1 of the present embodiment includes a substrate 10 and an electrode portion 30 formed on the substrate 10 .

[0033] The substrate 10 is a plate-shaped quartz substrate. Here, the quartz used as the material of the substrate 10 belongs to the trigonal system, such as Figure 2 As shown, it has mutually perpendicular crystal axes X, Y, and Z. The X-axis, Y-axis, and Z-axis are respectively referred to as the electrical axis, the mechanical axis, and the optical axis. The substrate 10 of this embodiment is a "rotated Y-cut quartz substrate" cut along a plane after rotating the XZ plane around the X-axis by a predetermined angle θ. For example, a substrate cut along a plane after rotating θ=35°15' is referred to as an "AT-cut quartz substrate." By using such a quartz substrate, a vibration element 1 having excellent temperature characteristics is obtained.

[0034] However, as long as the thickness shear vibration can be excited, the substrate 10 is not limited to an AT-cut quartz substrate, and a BT-cut quartz substrate may be used. In addition, as the substrate 10, various piezoelectric substrates such as lithium niobate and lithium tantalate may be used in addition to a quartz substrate.

[0035] In addition, hereinafter, the Y axis and the Z axis which are rotated around the X axis according to the angle θ are referred to as the Y′ axis and the Z′ axis. That is, the substrate 10 has a thickness in the Y′ direction and extends in the XZ′ plane direction.

[0036] The substrate 10 is in a strip shape with the X direction as the long side and the Z' direction as the short side when viewed from above. In addition, the negative X direction is the terminal side of the substrate 10, and the positive X direction is the base side. When the maximum length of the substrate 10 in the X direction is L and the maximum width in the Z' direction is W, L / W is not particularly limited, and is preferably set to about 1.1 to 1.4, for example.

[0037] like Figure 1 and Figure 3 As shown, the substrate 10 has a thin-walled portion 11 as a vibration region that seals vibration energy, and a thick-walled portion 12 that is integrated with the thin-walled portion 11 and has a greater thickness than the thin-walled portion 11. The thin-walled portion 11 is formed by etching the substrate 10 in the negative Y' direction and providing a recessed portion 74.

[0038] The thin-walled portion 11 is offset to the negative side in the X direction and the negative side in the Z' direction relative to the center of the substrate 10, and a portion of its outer edge is exposed from the thick-walled portion 12. When the vibration element 1 is viewed from above, the area of ​​the thin-walled portion 11 is preferably less than 1 / 2 of the area of ​​the substrate 10. Thus, the thick-walled portion 12 having high mechanical strength can be formed to be sufficiently wide, so that the rigidity of the thin-walled portion 11 can be sufficiently ensured.

[0039] When the vibration element 1 is viewed from above, the thin-walled portion 11 has: a first outer edge 21 and a second outer edge 22, which are separated in the vibration direction of thickness shear vibration, i.e., the X direction, and extend in the Z' direction; and a third outer edge 23 and a fourth outer edge 24, which are separated in the Z' direction and extend in the X direction. Of the first outer edge 21 and the second outer edge 22, the first outer edge 21 is located on the positive side of the X direction, and the second outer edge 22 is located on the negative side of the X direction. In addition, of the third outer edge 23 and the fourth outer edge 24, the third outer edge 23 is located on the positive side of the Z' direction, and the fourth outer edge 24 is located on the negative side of the Z' direction. In addition, the third outer edge 23 connects the ends of the first outer edge 21 and the second outer edge 22 on the positive side of the Z' direction to each other, and the fourth outer edge 24 connects the ends of the first outer edge 21 and the second outer edge 22 on the negative side of the Z' direction to each other.

[0040] In addition, if Figure 1 As shown, the main surface or surface on the positive side in the Y' direction of the thick-walled portion 12 is arranged to protrude further toward the positive side in the Y' direction than the main surface or surface on the positive side in the Y' direction of the thin-walled portion 11. On the other hand, the main surface or back surface on the negative side in the Y' direction of the thick-walled portion 12 and the main surface or back surface on the negative side in the Y' direction of the thin-walled portion 11 are arranged on the same plane.

[0041] The thick-walled portion 12 includes a thick-walled portion 12 disposed along the first outer edge 21 and a thick-walled portion 12 disposed along the third outer edge 23. Therefore, the thick-walled portion 12 has a structure that is bent along the thin-walled portion 11 when viewed from above, and is substantially L-shaped. On the other hand, the thick-walled portion 12 is not formed at the second outer edge 22 and the fourth outer edge 24 of the thin-walled portion 11, and these second outer edges 22 and fourth outer edges 24 are exposed from the thick-walled portion 12. In this way, the thick-walled portion 12 is partially disposed at the outer edge of the thin-walled portion 11 to form a substantially L-shape, and is not disposed along the second outer edge 22 and the fourth outer edge 24, thereby maintaining the rigidity of the thin-walled portion 11 of the vibration element 1 and reducing the mass of the end side of the vibration element 1. In addition, the vibration element 1 can be miniaturized.

[0042] The thick-walled portion 12 has: a connecting portion 26, which connects the thick-walled portion 12 and the thin-walled portion 11, is continuously provided with the first outer edge 21, and has an inclined portion whose thickness gradually increases toward the positive X direction; and a connecting portion 25, which is continuously provided with the third outer edge 23, and has an inclined portion whose thickness gradually increases toward the positive Z' direction. In addition, the thick-walled portion 12 on the side of the connecting portion 26 becomes a mounting portion, and is fixed to a package or the like using a conductive adhesive or the like.

[0043] The electrode unit 30 includes a pair of excitation electrodes 31 and 32 , a pair of pad electrodes 33 and 34 , and a pair of extraction electrodes 35 and 36 .

[0044] The excitation electrodes 31 and 32 are arranged in the excitation electrode arrangement region 13 of the thin portion 11. The excitation electrode 31 is formed on the surface of the thin portion 11. On the other hand, the excitation electrode 32 is arranged on the back surface of the thin portion 11 to face the excitation electrode 31. The excitation electrodes 31 and 32 are each substantially rectangular with the long side in the X direction and the short side in the Z' direction.

[0045] Pad electrodes 33 and 34 are arranged in pad electrode arrangement region 14 of thick portion 12. Pad electrode 33 is formed on the surface of thick portion 12 on the connection portion 26 side. Pad electrode 34 is formed on the back surface of thick portion 12 on the connection portion 26 side to face pad electrode 33.

[0046] The extraction electrodes 35 and 36 are arranged in the extraction electrode arrangement region 15 of the substrate 10. In addition, the extraction electrode arrangement region 15 is composed of a first region 16 including a portion located in the thick wall portion 12 including the connection portions 25 and 26, and a second region 17 including a portion located in the thin wall portion 11. The extraction electrode 35 electrically connects the excitation electrode 31 to the pad electrode 33. On the other hand, the extraction electrode 36 electrically connects the excitation electrode 32 to the pad electrode 34. The extraction electrodes 35 and 36 are arranged so as not to overlap with each other across the substrate 10. Thus, the electrostatic capacitance between the extraction electrodes 35 and 36 can be suppressed.

[0047] In addition, if Figure 3 , Figure 4 , Figure 5 as well as Figure 6 As shown, the electrode portion 30 is composed of a first electrode layer 41 and a second electrode layer 42, the first electrode layer 41 is configured in the pad electrode configuration area 14, the lead electrode configuration area 15 and the excitation electrode configuration area 13 on the substrate 10, and the second electrode layer 42 is configured in an area overlapping with the pad electrode configuration area 14, the lead electrode configuration area 15 and the excitation electrode configuration area 13 when viewed from above on the first electrode layer 41, and the thickness is greater than the first electrode layer 41.

[0048] When viewed from above, the second electrode layer 42 has: an electrode thin-walled portion 38, which overlaps with the excitation electrode configuration area 13; and an electrode thick-walled portion 37, which overlaps with the lead-out electrode configuration area 15 and is thicker than the electrode thin-walled portion 38. The electrode thin-walled portion 38 is configured in the excitation electrode configuration area 13 on the thin-walled portion 11 and the second area 17 of the lead-out electrode configuration area 15, and the electrode thick-walled portion 37 is configured in the pad electrode configuration area 14 on the thick-walled portion 12 including the connecting portions 25 and 26 and the first area 16 of the lead-out electrode configuration area 15.

[0049] Specifically, the electrode thin portion 38 is the excitation electrodes 31 , 32 and the extraction electrodes 35 , 36 on the thin portion 11 , and the electrode thick portion 37 is the pad electrodes 33 , 34 and the extraction electrodes 35 , 36 on the thick portion 12 including the connection portions 25 , 26 .

[0050] The electrode thin-walled portion 38 is formed by etching the metal layer 40 having the same thickness as the thickness T1 of the electrode thick-walled portion 37 to a thickness T2. Therefore, the surface of the electrode thin-walled portion 38 opposite to the substrate 10 is an etched surface. In addition, when etching is performed by dry etching, the surface of the electrode thin-walled portion 38 opposite to the substrate 10 is a dry-etched surface.

[0051] Furthermore, since the electrode thin portion 38 and the electrode thick portion 37 of the extraction electrodes 35 and 36 are integrally formed, disconnection is prevented, and since most of the narrow extraction electrodes 35 and 36 are formed by the electrode thick portion 37 , increase in sheet resistance can be suppressed.

[0052] In addition, the thickness T1 of the electrode thick wall portion 37 and the thickness T2 of the electrode thin wall portion 38 preferably satisfy 0.05≤T2 / T1≤0.7. When T2 / T1 is less than 0.05, the thickness of the lead-out electrodes 35 and 36 is thin, and the increase in sheet resistance cannot be fully suppressed. In addition, when T2 / T1 is greater than 0.7, the etching time for forming the electrode thin wall portion 38 becomes longer, and the manufacturing cost increases.

[0053] Regarding the constituent material of the electrode portion 30 , the second electrode layer 42 is gold (Au), and the first electrode layer 41 is at least one of nickel (Ni), chromium (Cr), and chromium nitride (CrN).

[0054] As described above, in the vibration element 1 of the present embodiment, the pad electrodes 33, 34 and the extraction electrodes 35, 36 on the thick wall portion 12 including the connection portions 25, 26 of the substrate 10 are formed by the electrode thick wall portion 37, and the excitation electrodes 31, 32 and the extraction electrodes 35, 36 on the thin wall portion 11 are formed by the electrode thin wall portion 38. Therefore, the thickness of the excitation electrodes 31, 32 can be made thin enough to prevent unnecessary parasitics from occurring, and the thickness of the extraction electrodes 35, 36 can be made thick enough to prevent sheet resistance from increasing. Therefore, the vibration element 1 having excellent vibration characteristics and excellent electrical reliability can be obtained.

[0055] 1.2. Manufacturing method of vibration element

[0056] Next, refer to Figure 7 to Figure 14 A method for manufacturing the vibration element 1 will be described.

[0057] in addition, Figure 8 to Figure 14 is equivalent to Figure 3 The sectional view is located along the A2-A2 line sectional view.

[0058] like Figure 7 As shown, the method for manufacturing the vibration element 1 of the present embodiment includes a recessed portion forming step, a metal layer forming step, an electrode pattern forming step, a protective film forming step, and a metal layer etching step.

[0059] 1.2.1. Depression forming process

[0060] In step S1, a base film 71 of chromium (Cr) or the like and a metal film 72 of gold (Au) or the like are formed in the order of base film 71 and metal film 72 on the entire surface of substrate 10 by using a sputtering device or an evaporation device. Next, a protective film 73 of a resist or the like is applied on the metal film 72, and a photolithography technique such as Figure 8 As shown, a pattern of recessed portions is formed.

[0061] The substrate 10 having the recessed portion pattern formed thereon is wet-etched using an etching solution, such as a mixture of hydrofluoric acid and ammonium fluoride. Fig. 9 As shown, the recessed portion 74 is formed in the substrate 10. Through this process, the thin-walled portion 11 and the thick-walled portion 12 are formed in the substrate 10.

[0062] 1.2.2. Metal layer formation process

[0063] In step S2, after removing the base film 71, the metal film 72, and the protective film 73, a first electrode layer 41 of chromium (Cr) or the like and a second electrode layer 42 of gold (Au) or the like are sequentially formed on the entire surface of the substrate 10 having the recessed portion 74 by a sputtering device or an evaporation device, in the order of the first electrode layer 41 and the second electrode layer 42, and Fig.10 As shown, a metal layer 40 is formed on the substrate 10. In addition, the thickness of the metal layer 40 is T1.

[0064] 1.2.3. Electrode pattern forming process

[0065] In step S3, the metal layer 40 on the substrate 10 is etched using photolithography and etching techniques. Fig.11 More specifically, excitation electrodes 31 and 32 are formed in the excitation electrode arrangement region 13 , pad electrodes 33 and 34 are formed in the pad electrode arrangement region 14 , and extraction electrodes 35 and 36 are formed in the extraction electrode arrangement region 15 .

[0066] 1.2.4. Protective film formation process

[0067] In step S4, a protective film 75 such as a resist is applied on the substrate 10 on which the electrode pattern of the metal layer 40 is formed. Fig.12 As shown, a protective film 75 is formed by photolithography on the metal layer 40 in an area overlapping at least a portion of the extraction electrode configuration area 15. More specifically, the protective film 75 is formed in an area overlapping the first area 16 of the extraction electrode configuration area 15 in the pad electrode configuration area 14 and the thick wall portion 12 including the connection portions 25 and 26.

[0068] 1.2.5. Metal layer etching process

[0069] In step S5, Fig.13 As shown, etching is performed through the protective film 75 to thin the metal layer 40 arranged in the second region 17 of the extraction electrode arrangement region 15 and the excitation electrode arrangement region 13. The etching is terminated when the thickness T2 of the metal layer 40 reaches a thickness satisfying 0.05≤T2 / T1≤0.7. Fig.14 As shown, the completed vibration element 1 is obtained. In addition, the method of etching the metal layer 40 to thin the wall may be dry etching using a dry etching device or wet etching using an etching solution. Dry etching has the advantage of being easy to control the thickness T2 of the metal layer 40 compared to wet etching.

[0070] By the above manufacturing method, the following vibration element 1 can be manufactured: the pad electrodes 33, 34 and the extraction electrodes 35, 36 composed of the electrode thick wall portion 37 are provided in the thick wall portion 12 including the connection portions 25, 26 of the substrate 10, and the excitation electrodes 31, 32 and the extraction electrodes 35, 36 composed of the electrode thin wall portion 38 are provided in the thin wall portion 11. Therefore, the thickness of the excitation electrodes 31, 32 can be made thin enough to prevent unnecessary parasitics from occurring, and the thickness of the extraction electrodes 35, 36 can be made thick enough to prevent sheet resistance from increasing. Therefore, the vibration element 1 having excellent vibration characteristics and excellent electrical reliability can be obtained.

[0071] 2. Second Implementation

[0072] 2.1. Vibration element

[0073] Next, refer to Fig.15 and Fig.16 A vibration element 1 a according to the second embodiment will be described.

[0074] The vibration element 1a of this embodiment is the same as the vibration element 1 of the first embodiment except that the configuration position structure of the electrode portion 30a is different from that of the vibration element 1 of the first embodiment. In addition, the description will focus on the differences from the first embodiment described above, and the same items are denoted by the same reference numerals and their descriptions are omitted.

[0075] like Fig.15 As shown, the vibration element 1 a includes a substrate 10 and an electrode portion 30 a formed on the substrate 10 .

[0076] The electrode portion 30a of the vibration element 1a includes: pad electrodes 33 and 34 formed by the electrode thick wall portion 37; extraction electrodes 35a and 36a formed by the electrode thick wall portion 37 and the electrode thin wall portion 38; and excitation electrodes 31 and 32 formed by the electrode thin wall portion 38. The first region 16a of the extraction electrode configuration region 15a, where the extraction electrodes 35a and 36a formed by the electrode thick wall portion 37 are formed, also includes a portion located in the thin wall portion 11. That is, as Fig.16 As shown, the extraction electrode 35 a constituted by the electrode thick portion 37 is formed on the thick portion 12 including the connection portion 25 and a part of the thin portion 11 .

[0077] The manufacturing method of the vibration element 1a of this embodiment is the same as the manufacturing method of the vibration element 1 of the first embodiment, and in the protective film forming process of step S4, the protective film 75 is formed on the pad electrode arrangement region 14 when viewed from above and the region overlapping the first region 16a located at the thin-walled portion 11 and the connecting portions 25 and 26 on the metal layer 40. Through this process, the extraction electrode 35a composed of the electrode thick-walled portion 37 can be formed in the thick-walled portion 12 including the connecting portions 25 and 26 and the first region 16a of the thin-walled portion 11.

[0078] With such a structure, the vibration element 1a can shorten the extraction electrodes 35a and 36a formed by the electrode thin portion 38, and can further suppress the increase in sheet resistance. Therefore, there is no possibility of disconnection, the electrical connection reliability is excellent, and the vibration element 1a with a low CI value can be obtained.

[0079] 3. Third Implementation

[0080] 3.1. Vibration element

[0081] Next, refer to Fig.17 A vibration element 1 b according to the third embodiment will be described.

[0082] The vibration element 1b of this embodiment is the same as the vibration element 1 of the first embodiment except that the shape of the substrate 10b is different. The description will focus on the differences from the first embodiment, and the same items are denoted by the same reference numerals and their description will be omitted.

[0083] like Fig.17 As shown, the vibration element 1 b includes a substrate 10 b and an electrode portion 30 formed on the substrate 10 b.

[0084] The main surface, i.e., the surface, on the positive side in the Y' direction of the thick-walled portion 12 of the substrate 10b of the vibration element 1b is arranged to protrude toward the positive side in the Y' direction more than the main surface, i.e., the surface, on the positive side in the Y' direction of the thin-walled portion 11b. On the other hand, the main surface, i.e., the back surface, on the negative side in the Y' direction of the thick-walled portion 12 is arranged to protrude toward the negative side in the Y' direction more than the main surface, i.e., the back surface, on the negative side in the Y' direction of the thin-walled portion 11b. That is, the thin-walled portion 11b is formed by forming a recessed portion 74b on the surface and the back surface of the substrate 10b. Therefore, in the manufacturing method, compared with the first embodiment described above, the etching depth of the recessed portion 74b can be made shallower, thereby achieving low cost.

[0085] By adopting such a structure, the vibration element 1b will not be disconnected, the reliability of electrical connection is excellent, and the vibration element 1b can be obtained at a low cost.

[0086] 4. Fourth Implementation

[0087] 4.1. Vibration devices

[0088] Next, refer to Fig.18 A resonator device 2 according to a fourth embodiment will be described. In this description, a resonator device 2 including the resonator element 1 described above will be described as an example.

[0089] like Fig.18 As shown, the vibration device 2 includes a vibration element 1 , a package 50 that accommodates the vibration element 1 , and a cover 60 that forms a storage space 52 together with the package 50 .

[0090] The package 50 has a recessed portion 51 opened on a first surface 55, and a cover 60 for closing the opening of the recessed portion 51 is bonded to the first surface 55. By closing the recessed portion 51 of the package 50 with the cover 60, a storage space 52 for storing the vibration element 1 is formed. The storage space 52 may be in a reduced pressure or vacuum state, or may be filled with an inert gas such as nitrogen (N), helium (He), or argon (Ar).

[0091] There is no particular limitation on the constituent material of the package 50, and various ceramics such as alumina can be used. There is no particular limitation on the constituent material of the cover 60, and it can be a member having a linear expansion coefficient similar to that of the constituent material of the package 50. There is no particular limitation on the bonding between the package 50 and the cover 60, and they can be bonded via an adhesive, or by seam welding, etc.

[0092] Connection electrodes 56 and 57 are formed on the inner bottom surface 53 of the package 50. In addition, external mounting terminals 58 and 59 are formed on the second surface 54 of the package 50. The connection electrode 56 is electrically connected to the external mounting terminal 58 via a through electrode (not shown) formed on the package 50, and the connection electrode 57 is electrically connected to the external mounting terminal 59 via a through electrode (not shown) formed on the package 50.

[0093] The vibration element 1 accommodated in the accommodation space 52 has the main surface of the thick wall portion 12 on the positive side in the Y' direction facing the package 50 side, and the mounting portion of the thick wall portion 12 is fixed to the package 50 by the bonding material 61 as a conductive adhesive. The bonding material 61 is provided to contact the connection electrode 56 and the pad electrode 33. Thus, the connection electrode 56 and the pad electrode 33 are electrically connected via the bonding material 61. By supporting the vibration element 1 at one place or one point using the bonding material 61, for example, stress generated in the vibration element 1 due to the difference in thermal expansion coefficient between the package 50 and the substrate 10 can be suppressed.

[0094] The pad electrode 34 of the vibration element 1 is electrically connected to the connection electrode 57 via the bonding wire 62. As described above, the pad electrode 34 is arranged opposite to the pad electrode 33, so that when the vibration element 1 is fixed to the package 50, the pad electrode 34 is located directly above the bonding material 61. Therefore, it is possible to suppress leakage of ultrasonic vibration applied to the pad electrode 34 during wire bonding, and the bonding wire 62 can be connected to the pad electrode 34 more reliably.

[0095] By adopting such a structure, the vibration device 2 has a vibration element 1, which makes the thickness of the excitation electrodes 31 and 32 thin enough to avoid unnecessary parasitics, and makes the thickness of the lead electrodes 35 and 36 thick enough to avoid increasing the sheet resistance. Therefore, a vibration device 2 with good vibration characteristics and excellent electrical reliability can be obtained.

Claims

1. A method for manufacturing a vibration element, The vibration element comprises: a substrate having a thin-walled portion and a thick-walled portion having a thickness greater than that of the thin-walled portion; and an electrode portion, comprising: an excitation electrode arranged in an excitation electrode arrangement region of the thin-walled portion; a pad electrode arranged in a pad electrode arrangement region of the thick-walled portion; and an extraction electrode connecting the excitation electrode and the pad electrode and arranged in an extraction electrode arrangement region of the substrate, The manufacturing method of the vibration element comprises the following steps: A metal layer forming step of forming a metal layer on the substrate; a protective film forming step of forming a protective film on a region of the metal layer that overlaps at least a portion of the extraction electrode arrangement region when viewed from above; The metal layer etching step thins the metal layer arranged in the excitation electrode arrangement region by etching through the protection film.

2. The method for manufacturing a vibration element according to claim 1, wherein: The metal layer forming step comprises: forming the metal layer with a thickness T1, The metal layer etching step includes: thinning the metal layer arranged in the excitation electrode arrangement region to form the metal layer with a thickness T2; Satisfies 0.05≤T2 / T1≤0.

7.

3. The method for manufacturing a vibration element according to claim 1 or 2, wherein: The extraction electrode configuration area includes: A first region including a portion located in the thick wall portion; and a second region including a portion located in the thin-walled portion, The protective film forming step includes: forming the protective film in a region on the metal layer that overlaps with the first region when viewed from above; The metal layer etching step includes thinning the metal layer arranged in the second region and the excitation electrode arrangement region by etching through the protective film.

4. The method for manufacturing a vibration element according to claim 3, wherein: The protective film forming step includes forming the protective film on the metal layer in the pad electrode arrangement region and in a region overlapping with the first region located in the thin-walled portion when viewed from above.

5. The method for manufacturing a vibration element according to claim 3, wherein: The substrate includes a connecting portion, the connecting portion connecting the thick wall portion and the thin wall portion and having an inclined portion. The protective film forming step includes forming the protective film on the metal layer in the pad electrode arrangement region and in a region overlapping with the first region located in the thin-walled portion and the connecting portion when viewed from above.

6. The method for manufacturing a vibration element according to claim 3, wherein: The metal layer etching step includes thinning the metal layer arranged in the second region and the excitation electrode arrangement region by performing dry etching via the protective film.

7. A vibration element, comprising: a substrate having a thin-walled portion and a thick-walled portion having a thickness greater than that of the thin-walled portion; and an electrode portion, comprising: an excitation electrode arranged in an excitation electrode arrangement region of the thin-walled portion; a pad electrode arranged in a pad electrode arrangement region of the thick-walled portion; and an extraction electrode connecting the excitation electrode and the pad electrode and arranged in an extraction electrode arrangement region of the substrate, The electrode portion comprises: A first electrode layer is arranged in the pad electrode arrangement region, the extraction electrode arrangement region and the excitation electrode arrangement region on the substrate; and The second electrode layer is arranged on the first electrode layer in an area overlapping the pad electrode arrangement area, the lead electrode arrangement area and the excitation electrode arrangement area when viewed from above, and has a thickness greater than that of the first electrode layer. The second electrode layer includes an electrode thin portion overlapping the excitation electrode arrangement region in a plan view, and an electrode thick portion overlapping the extraction electrode arrangement region in a plan view and having a thickness greater than that of the electrode thin portion.

8. The vibration element according to claim 7, wherein: When the thickness of the thick-walled portion of the electrode is T1 and the thickness of the thin-walled portion of the electrode is T2, Satisfies 0.05≤T2 / T1≤0.

7.

9. The vibration element according to claim 7 or 8, wherein: The extraction electrode configuration area includes: A first region including a portion located in the thick wall portion; and a second region including a portion located in the thin-walled portion, The electrode thin portion overlaps the second region and the excitation electrode arrangement region in a plan view, and the electrode thick portion overlaps the first region and the pad electrode arrangement region in a plan view.

10. The vibration element according to claim 7 or 8, wherein: The second electrode layer is gold, The first electrode layer contains at least one of nickel, chromium and chromium nitride.

11. The vibration element according to claim 7 or 8, wherein: A surface of the electrode thin portion opposite to the substrate is an etched surface.

12. The vibration element according to claim 7 or 8, wherein: A surface of the electrode thin-walled portion opposite to the substrate is a dry-etched surface.

13. A vibration device, comprising: The vibration element according to claim 7 or 8; and The package accommodates the vibration element and fixes the vibration element via a bonding material.