Pre-mold of metal wire drawing mold

By using a specific ratio of filler and diamond core assembly in the metal wire drawing mold, combined with high-temperature sintering and slow cooling treatment, the problem of insufficient tensile strength of the existing mold is solved, and high hardness, long life and efficient wire drawing are achieved mold.

CN118744169AActive Publication Date: 2024-10-08ZHEJIANG JINPING WIRE DRAWING DIE CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411017990.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-10-08
Estimated Expiration
2044-07-29

AI Technical Summary

Technical Problem

Due to insufficient tensile strength and hardness, the preformed dies of existing metal wire drawing dies are prone to deformation and cracking under high-intensity extrusion force, resulting in short service life and high scrap rate, and cannot effectively control the straightness and circle diameter of the wire.

Method used

Sintered body made of various fillers, the volume percentage is WC 80-85%, Co 8-12%, Ni 2-5%, Cu 2-3%, Mn 1-2%, Si 0.1-1%, It is assembled through a diamond mold core and mold cover, and the sintering temperature is controlled at 850-860°C. Co penetrates into the WC powder as a binder to form a strong bond, combined with slow cooling to reduce stress.

Benefits of technology

It improves the tensile strength and hardness of the mold, extends the service life, ensures the straightness and circle diameter control of the wire, reduces the scrap rate, and significantly improves the wear resistance and impact resistance of the mold.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118744169A_ABST
    Figure CN118744169A_ABST
Patent Text Reader

Abstract

The invention discloses a pre-mold of a metal wire drawing mold, and relates to the technical field of metal material manufacturing. Comprising a die sleeve, a die core, a sintered body and a die cover, the die core is arranged in the center of the die sleeve and made of diamonds, the periphery of the die core is filled with the sintered body, and the die cover matched with the die sleeve is arranged outside the sintered body; the sintered body is prepared from a plurality of fillers, and the fillers comprise the following components in percentage by volume: 80-85% of WC; 8 to 12 percent of Co; 2-5% of Ni; 2-3% of Cu; 1-2% of Mn; and 0.1-1% of Si. By changing the formula of the traditional filler, the hardness of the sintered pre-mold can reach 120-128, and the prepared pre-mold is high in tensile strength, not prone to deformation, long in service life and high in practicability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of metal material manufacturing, and in particular to a pre-mold of a metal wire drawing die. Background Art

[0002] The pre-mold (also called pre-forming mold) of the metal wire drawing die is a tool used to perform preliminary plastic deformation on the metal wire before the final wire drawing process. Its main purpose is to make the shape and size of the metal wire close to the final desired shape, so that the required accuracy and surface quality can be achieved more effectively in the subsequent wire drawing process. The pre-mold is usually made of carbide or other wear-resistant materials to ensure that it can remain stable for a long time under high pressure and high friction conditions.

[0003] At present, the process of preforming molds for metal wire drawing dies on the market is mostly as follows: a diamond for making a die hole is set at the center of a metal mold sleeve, and powders of various materials are mixed evenly according to a certain ratio to form a mixture, i.e., a filler, which is filled in the metal mold sleeve, sealed with a cover, placed on a sintering machine, heated and pressurized for several minutes, and then cooled randomly to complete. However, the filler currently used, due to the inappropriate materials and their ratios, the pre-mold obtained after sintering, the tensile strength of the sintered filler mixture is insufficient, the hardness HRB is low, and the impact resistance is very poor, so that the metal wire drawing die made of this is easy to deform and expand the sintered body part during the wire drawing process due to the high-intensity extrusion force generated by drawing, which makes it easy for the mold to crack and burst during the hard wire drawing process, and cannot achieve the ideal state of hard wire drawing. Such a mold has a low service life, cannot effectively control the straightness and circle diameter of the drawn wire, and leads to an increase in the scrap rate.

[0004] Therefore, the present invention designs a pre-mold of a metal wire drawing die with higher hardness, better use effect and longer service life. Summary of the invention

[0005] In view of the deficiencies in the prior art, the object of the present invention is to provide a pre-mold for a metal wire drawing die, which has a reasonable design, high tensile strength, is not easy to deform, has a long service life and is highly practical.

[0006] In order to achieve the above-mentioned purpose, the present invention is realized through the following technical scheme: a pre-mold of a metal wire drawing die, comprising a die sleeve, a die core, a sintered body and a die cover, a die core is arranged at the center of the die sleeve, the die core is made of diamond, a sintered body is filled around the die core, and a die cover matching the die sleeve is arranged outside the sintered body; the sintered body is made of a variety of fillers, and the fillers are composed of the following components in volume percentage: WC 80-85%; Co 8-12%; Ni2-5%; Cu 2-3%; Mn 1-2%; Si 0.1-1%.

[0007] Preferably, the filler is composed of the following components in volume percentage: WC 80%; Co 10%; Ni 5%; Cu 3%; Mn 1%; Si 1%.

[0008] Preferably, the filler is composed of the following components in volume percentage: WC 85%, Co 9%, Ni 2%, Cu 2%, Mn 1.5%, and Si 0.5%.

[0009] A process for preparing a pre-mold for a metal wire drawing die comprises the following steps:

[0010] 1. First, the filler with the above volume percentage is made into powder, and mixed evenly by a mixer; a lubricant is added to the above powder to improve the fluidity of the powder;

[0011] 2. Place the diamond mold core at the center of the mold sleeve, fill the powder mixed in step 1 around the mold core, and seal it with a mold cover to obtain a pre-mold for the metal wire drawing die to be formed;

[0012] 3. Place the pre-mold of the metal wire drawing die to be formed in step 2 into a high-temperature furnace for sintering. The time from room temperature to sintering temperature is 1-2 hours. The sintering temperature is 850-860°C and maintained for 2-3 hours. During the sintering process, Co acts as a binder and penetrates into the WC powder to form a strong bond. The HRB is 120-128.

[0013] 4. After sintering, the pre-mold is naturally cooled to 350-360℃ along with the high temperature furnace, then taken out and cooled to room temperature.

[0014] Preferably, the sintering temperature is 850°C.

[0015] Beneficial effects of the present invention: The present invention changes the formula of the traditional filler so that the hardness after sintering can reach 120-128, and the prepared pre-mold has high tensile strength, is not easy to deform, has a long service life, and is highly practical. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] The present invention will be described in detail below with reference to the accompanying drawings and specific embodiments;

[0017] Figure 1 It is a schematic diagram of the pre-mold structure of the present invention. DETAILED DESCRIPTION

[0018] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.

[0019] Reference Figure 1 The present specific embodiment adopts the following technical scheme: a pre-mold of a metal wire drawing die, comprising a die sleeve 1, a die core 2, a sintered body 3 and a die cover 4, wherein the die sleeve 1 is provided with a die core 2 at the center, the die core 2 is made of diamond, the die core 2 is surrounded by a filled sintered body 3, and the sintered body 3 is provided with a die cover 4 matching the die sleeve 1 on the outside; the sintered body 3 is made of a variety of fillers, and the fillers are composed of the following components in volume percentage: WC 80-85%; Co 8-12%; Ni 2-5%; Cu 2-3%; Mn 1-2%; Si 0.1-1%.

[0020] A process for preparing a pre-mold for a metal wire drawing die comprises the following steps:

[0021] 1. First, the filler with the above volume percentage is made into powder, and mixed evenly by a mixer; a lubricant is added to the above powder to improve the fluidity of the powder; this can ensure the uniform distribution of the material components and improve the operating performance in the subsequent processing process.

[0022] 2. Place the diamond mold core at the center of the mold sleeve, and then fill the powder mixed in step 1 around the mold core and seal it with the mold cover to obtain the pre-mold of the metal wire drawing die to be formed; ensure that the powder around the mold core is evenly distributed to ensure the quality of the final pre-mold. By assembling the pre-mold in this way, the shape and dimensional accuracy of the mold can be effectively controlled.

[0023] 3. Place the pre-mold of the metal wire drawing die to be formed in step 2 into a high-temperature furnace for sintering. The time from room temperature to the sintering temperature is 1-2 hours, and the sintering temperature is 850-860°C, which is maintained for 2-3 hours. During the sintering process, Co acts as a binder and penetrates into the WC powder to form a strong bond with an HRB of 120-128. This can significantly improve the strength and wear resistance of the mold.

[0024] 4. After sintering, the pre-mold is naturally cooled to 350-360℃ with the high-temperature furnace. The pre-mold is taken out and cooled to room temperature. The slow cooling process helps to reduce the stress caused by temperature changes in the pre-mold, thereby reducing the risk of pre-mold deformation and ensuring the stability and service life of the mold.

[0025] It is worth noting that the sintering temperature is 850°C.

[0026] It is worth noting that the filler is composed of the following components in volume percentage: WC 80%; Co 10%; Ni 5%; Cu 3%; Mn 1%; Si 1%.

[0027] In addition, the filler is composed of the following components in volume percentage: WC 85%, Co 9%, Ni 2%, Cu 2%, Mn 1.5%, and Si 0.5%.

[0028] The pre-mold of this specific embodiment has high hardness and wear resistance. Diamond is used as the mold core material, which makes it have extremely high hardness and wear resistance, can withstand high-intensity wire drawing operations, and extend the service life of the mold.

[0029] This specific embodiment has excellent heat resistance. The sintered body adopts WC (tungsten carbide) as the main component. WC has high heat resistance and high-temperature stability, and can maintain good performance in high-temperature environment; and has good toughness. Adding alloy elements such as Co (cobalt), Ni (nickel) and Cu (copper) can improve the toughness and impact resistance of the sintered body and reduce the risk of the mold breaking during use; in addition, the corrosion resistance is enhanced. The addition of Mn (manganese) and Si (silicon) can improve the corrosion resistance of the material, so that the mold can maintain a stable working state even in harsh environments.

[0030] The pre-die of the metal wire drawing die of this specific embodiment has a uniform performance distribution: through a reasonable formulation and sintering process, various components in the sintered body can be evenly distributed, thereby ensuring the overall performance and consistency of the die.

[0031] According to different usage requirements, this specific implementation method can optimize the performance of the mold by adjusting the proportion of ingredients in the formula to meet the wire drawing requirements of different metal wires. Compared with molds made of expensive materials as a whole, this design not only ensures the high performance of key parts, but also reduces the overall cost by filling sintered bodies around the mold core, and has a high cost performance. At the same time, the design of the mold cover makes it easy to maintain and replace the mold during use, reducing downtime and maintenance costs.

[0032] The preparation process of the metal wire drawing die preform of this specific embodiment ensures product quality through strict steps. From the preparation and mixing of powders to the assembly of the preform, high-temperature sintering and the final cooling treatment, each step is aimed at improving the performance and durability of the die. In particular, the infiltration of cobalt during the high-temperature sintering process and the slow cooling process significantly enhance the strength and stability of the die, so that the final product can meet the requirements of high performance.

[0033] This specific implementation method changes the formula of the traditional filler so that the hardness after sintering can reach 120-128. The prepared pre-mold has high tensile strength, is not easy to deform, has a long service life, and is highly practical.

[0034] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A pre-mold for a metal wire drawing die, characterized in that: The mold sleeve (1) comprises a mold core (2), a sintered body (3) and a mold cover (4). The mold sleeve (1) is provided with a mold core (2) at its center, the mold core (2) is made of diamond, the mold core (2) is surrounded by a filled sintered body (3), and the sintered body (3) is provided with a mold cover (4) matching the mold sleeve (1) outside. The sintered body (3) is made of a variety of fillers, and the fillers are composed of the following components in volume percentage: WC 80-85%; Co 8-12%; Ni2-5%; Cu2-3%; Mn 1-2%; Si 0.1-1%.

2. A pre-mold for a metal wire drawing die according to claim 1, characterized in that: The filler is composed of the following components in volume percentage: WC 80%, Co 10%, Ni 5%, Cu 3%, Mn 1%, and Si 1%.

3. A pre-mold for a metal wire drawing die according to claim 1, characterized in that: The filler is composed of the following components in volume percentage: WC 85%, Co 9%, Ni 2%, Cu 2%, Mn 1.5%, and Si 0.5%.

4. A process for preparing a pre-mold for a metal wire drawing die, characterized in that: The following steps are involved: (1) First, the filler in the above volume percentage is made into powder, and the powder is stirred and mixed evenly by a mixer; a lubricant is added to the powder to improve the fluidity of the powder; (2) placing the diamond mold core at the center of the mold sleeve, and then filling the powder mixed in step (1) around the mold core, and sealing it with a mold cover to obtain a pre-mold of the metal wire drawing die to be formed; (3) placing the pre-mold of the metal wire drawing die to be formed in step (2) into a high-temperature furnace for sintering, the time from room temperature to the sintering temperature is 1-2 hours, the sintering temperature is 850-860°C, and maintained for 2-3 hours. During the sintering process, Co acts as a binder and penetrates into the WC powder to form a strong bond, and the HRB is 120-128; (4) After sintering, the pre-mold is naturally cooled to 350-360°C in the high-temperature furnace, and then taken out and cooled to room temperature.

5. The process for preparing a pre-mold for a metal wire drawing die according to claim 4, characterized in that: The sintering temperature is 850°C.

Citation Information

Patent Citations

  • Manufacturing process of premould of metal wire drawing mould

    CN101683691A

  • Composite roller

    CN105624512A

  • Stock for wire drawing die, and wire drawing die

    JP2007090371A

  • Composite diamond compact for a wire drawing die and a process for the production of the same

    US4374900A