White board base coating and production process thereof
The addition of defoaming agents controlled by vacuum mixing equipment and electrostatic technology solves the problem of poor film-forming performance of white cardboard paint, improves the film-forming performance and storage stability of the paint, and improves the quality of the finished whiteboard paper.
Patent Information
- Application Number
- CN202411027218.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-10-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
It is difficult to accurately control the amount and rate of defoaming agent addition during the production process of existing white cardboard coatings, resulting in poor coating film-forming performance and affecting construction performance and finished product quality.
Vacuum mixing equipment combined with electrostatic technology is used to reduce the generation of bubbles during the mixing process of the paint through electrostatic blocks and adjusting parts, control the amount and rate of addition of defoaming agent, and ensure the improvement of the film-forming performance of the paint.
It effectively reduces the generation of bubbles during the mixing process of the paint, improves the film-forming performance and storage stability of the paint, and improves the surface forming quality and storage cycle of the whiteboard paper.
Smart Images

Figure CN118745682A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of coating production equipment, and in particular to a white paper primer coating and a production process thereof. Background Art
[0002] At present, white cardboard coating, as the most basic coating for white cardboard, can significantly improve the adhesion of ink or other printing media cardboard during the printing process. This enhanced adhesion can ensure the quality of printed products and reduce losses during the printing process. At the same time, the primer coating can form a uniform coating on the surface of the cardboard, enhancing the fixing performance of the cardboard. In the subsequent processing process, the cardboard is not easy to be damaged or deformed, which improves the quality of the finished product.
[0003] Common white cardboard coatings need to have good water resistance, corrosion resistance and construction performance. The construction performance means that no bubbles should appear when applied on the white cardboard, otherwise bubbles or vacuum will easily appear during the coating process, affecting the flatness and aesthetics of the coating.
[0004] In order to help improve the construction performance of white cardboard coatings, the amount of defoaming agent is often added to the coating composition according to the preparation adaptability. The amount of defoaming agent added will directly affect the compatibility of the coating. When the amount of defoaming agent added is too much, it will affect the film-forming property of the coating. The defoaming agent addition rate will also affect the film-forming property of the coating. Therefore, it is necessary to accurately control the amount of defoaming agent and the defoaming agent addition rate. In addition, in the process of coating production, it is necessary to consider the effect of stirring rate on bubble generation. The faster the stirring rate, the easier it is to generate bubbles. Therefore, the amount of defoaming agent added must also consider the stirring rate, which makes it difficult to control the construction performance of the primer coating, so it needs to be improved. Summary of the invention
[0005] In order to help improve the construction performance of the coating and reduce the difficulty of production, the present application provides a white board paper primer coating and a production process thereof.
[0006] The present application provides a white paper primer coating and a production process thereof using the following technical solutions: A white paper primer coating comprises the following components: 4200-4300 parts of calcium carbonate, 570-600 parts of porcelain clay, 580-610 parts of styrene-butadiene latex, 180-190 parts of starch adhesive, 8-9 parts of dispersant, 15-17 parts of thickener, 17-19 parts of lubricant, 19-20 parts of water repellent, 7-8 parts of blue dye, 17-18 parts of purple fuel, 11-12 parts of caustic soda, 1.3-1.5 parts of defoamer, 11-12 parts of brightener and 50-120 parts of clean water.
[0007] By adopting the above technical solution and adding a defoamer and a dispersant in a certain ratio, the generation of bubbles in the primer coating during its preparation process can be reduced, thereby improving the film-forming performance of the primer coating and further improving the surface quality of the primer coating after film formation.
[0008] The present application also provides a white paper primer coating production process, which comprises the following steps: S1, weighing and concentrating the raw materials of each component, and accurately weighing the required raw materials of each component; S2, adding clean water and calcium carbonate into a sealed stirring device and stirring for 5 minutes to form a base material; S3, adding china clay, styrene-butadiene latex, starch adhesive and dispersant to the base material formed in S2, and stirring at high speed for 10 minutes to form a coating base liquid; S4, adding lubricant, blue fuel, purple fuel, caustic soda and whitening agent to the coating base liquid formed in S3, stirring at a low speed for 5 minutes to form an initial coating; S5, transferring the initial coating to a vacuum mixing device, and adding a defoamer and a thickener through the vacuum mixing device, controlling the amount and rate of addition of the thickener and the defoamer through the vacuum mixing device, and generating static electricity through the vacuum mixing device to reduce the liquid surface tension of the initial coating, thereby further defoaming, reducing bubbles generated during the transfer process and the stirring process, and forming a finished coating; S6, filling and packaging the finished coating formed in S5; The vacuum mixing equipment used in step S5 includes an outer tank body, an inner tank body coaxially arranged in the outer tank body, and a stirring body arranged in the inner tank body. The inner tank body is also provided with a feeding component for adding a defoaming agent and a thickener, and an electrostatic component for adjusting the surface tension of the liquid in the tank body. A accommodating cavity is provided between the outer tank body and the inner tank body; the electrostatic component includes an electrostatic block arranged in the accommodating cavity and in contact with the outer peripheral wall of the inner tank body, the electrostatic block is slidably arranged in the accommodating cavity, and two groups of the electrostatic blocks are provided, and the two groups of the electrostatic blocks are arranged relatively to each other. The accommodating cavity is also provided with an adjusting member for adjusting the two groups of the electrostatic blocks so that the electrostatic blocks are consistent with the coating liquid level in the inner tank body.
[0009] By adopting the above-mentioned vacuum mixing equipment, when producing the primer coating, the initial coating that has been stirred is added into the inner tank body, and the initial coating is stirred by the set stirring body. By setting the feeding component, the defoaming agent is added according to the two sides of the initial coating, thereby reducing the film formation problem caused by the one-time addition of the defoaming agent. In the process of stirring the initial coating in the inner tank body, the electrostatic block set slides relative to the inner tank body, so that the inner tank body generates static electricity. Because the height of the two electrostatic blocks is consistent with the height of the liquid level under the action of the adjustment key, the static electricity generated by the friction between the inner tank body and the electrostatic block directly acts on the liquid surface of the initial coating, thereby reducing the liquid surface tension of the initial coating, thereby reducing the bubbles generated by the initial coating during stirring, and then reducing the addition of defoaming agent, improving the stability of subsequent coating storage, and reducing the problem of reduced film adhesion of the coating due to excessive addition of defoaming agent, thereby improving the quality of the coating after production and the storage period.
[0010] Optionally, the inner tank body and the outer tank body are both arranged at an angle, and the adjusting member includes an adjusting block slidably arranged in the inner tank body, the density of the adjusting block is less than the density of the coating, and a magnetic member is provided on the adjusting block, the buoyancy of the adjusting block is greater than the gravity of the magnetic member, the electrostatic block is provided with an adsorption member that is magnetically attracted to the magnetic member, and the accommodating cavity is also provided with a sliding member for slidingly adjusting the electrostatic block.
[0011] By adopting the above technical solution, when the technician places the initial paint in the inner tank body, since the density of the adjusting block is less than the density of the paint, the adjusting block moves under the action of buoyancy. Due to the magnetic suction part on the adjusting block and the adsorption part of the electrostatic block, when the adjusting block moves under the action of buoyancy, the adsorption part at this time drives the electrostatic block to slide under the action of magnetic force. Since the defoaming effect is best when static electricity acts on the surface of the liquid, the electrostatic block is always kept in contact with the outer surface of the inner tank body at the height of the liquid level under the action of buoyancy to slide, thereby realizing the effect of liquid tension on the surface of the initial paint, thereby improving the efficiency of defoaming bubbles.
[0012] At the same time, the inner tank body and the outer tank body are arranged to be inclined. At this time, when the initial coating is stirred, the surface area of the top of the liquid is increased, thereby improving the stirring efficiency of the initial coating during the stirring process, and the bubbles generated in the previous steps are stirred to the surface and eliminated by static electricity, so that the addition of the defoaming agent is always at an appropriate level, thereby reducing the problem of excessive addition of the defoaming agent.
[0013] Optionally, the sliding member includes a rotating rod rotatably arranged in the accommodating cavity, the electrostatic block is slidably arranged on the rotating rod, the rotating rod is also provided with a limiting structure for limiting the relative rotation of the electrostatic block and the rotating rod, and the rotating rod is also provided with a power member for driving the electrostatic block and the inner tank body to slide relative to each other.
[0014] By adopting the above technical scheme, first, when the initial coating is added, the electrostatic block slides on the rotating rod under the action of the buoyancy of the adjustment block, so that the electrostatic block is always consistent with the liquid level. At the same time, the limiting structure is set to prevent the rotating rod and the electrostatic block from rotating relative to each other. Therefore, when the position of the electrostatic block is adjusted, the electrostatic block is always in contact with the outer surface of the inner tank body, so that the static electricity generated by the relative sliding between the electrostatic block and the outer surface of the inner tank body always acts on the surface of the liquid, thereby improving the defoaming rate.
[0015] Optionally, the stirring body includes a stirring rod coaxially and uniformly rotating inside the inner tank body and a stirring blade provided on the stirring rod, both ends of the stirring rod are rotated and penetrated through the inner tank body, the power part includes a driving gear provided on one end of the stirring rod penetrating the bottom wall of the inner tank body, a driven gear is provided on the rotating rod, the driven gear is in the shape of a half gear ring, the driven gear is movably meshed with the driving gear, and a return part is also provided in the accommodating cavity for driving the rotating rod to rotate so that the driving gear and the driven gear remain meshed.
[0016] By adopting the above technical solution, when the stirring rod rotates to stir and mix the initial paint, the stirring rod drives the active gear to rotate, and the active gear drives the driven gear to rotate. Since the driven gear is in a semi-ring shape at this time, the active gear and the driven gear are movably engaged. When the active gear rotates to a position separated from the driven gear, the driven gear automatically rotates under the action of the return member until the active gear rotates to a position engaged with the driven gear again. At this time, the active gear drives the driven gear to rotate, thereby realizing the sliding drive of the electrostatic block. At this time, the driven gear is driven by the active gear until it is engaged with the active gear next time, which is a cycle. That is, the electrostatic block slides cyclically against the outer wall of the inner tank body, thereby generating static electricity to process the surface tension of the liquid surface of the initial paint.
[0017] Optionally, the feeding assembly includes a feeding box arranged in the accommodating cavity, the feeding box contains a thickener, the stirring rod is arranged in a hollow shape, a feeding hole is opened on the stirring blade, the feeding box is connected with the inner cavity of the stirring rod, the stirring rod is connected with the stirring blade, and a sealing plate is rotatably arranged at the feeding hole, the sealing plate movably blocks the feeding hole, and the end side of the sealing plate protrudes from the stirring blade, the sealing plate protrudes from the end side of the stirring blade and fits with the initial coating, and an elastic member for enabling the sealing plate to always seal the feeding hole is provided at the rotating shaft of the sealing plate.
[0018] By adopting the above technical solution, when the stirring blade and the stirring rod rotate to stir the initial paint, the blocking plate rotates under the damping of the initial paint, thereby opening the feeding hole to achieve the feeding of the thickener.
[0019] Three states are involved at this time. Due to the elastic part, in the initial state, that is, when no initial paint is added, the elastic part blocks the feeding hole. At this time, the thickener in the feeding box and the stirring rod is not easy to flow out from the feeding hole, so that the thickener is not easy to cause waste.
[0020] After adding the initial coating, when the initial coating is stirred, the blocking plate rotates under the damping effect of the initial coating, thereby opening the feeding hole. When the blocking plate rotates to the middle position, the feeding hole is fully opened, thereby realizing the addition of the thickener.
[0021] As the thickener is added, the damping of the initial coating on the sealing plate becomes greater, causing the sealing plate to continue to rotate. At this time, the feeding hole continues to become smaller, thereby controlling the amount of thickener until the sealing plate completely blocks the feeding hole, thereby achieving complete control of the amount of thickener.
[0022] However, there are no clear boundaries between these three states. Therefore, the three states change as the stirring proceeds. This change in quantity is not easy to control through sensors or solenoid valves.
[0023] Optionally, the feeding component also includes a defoaming box arranged on the outer peripheral wall of the inner tank body, a plurality of defoaming holes are opened on the inner peripheral wall of the inner tank body, and the plurality of defoaming holes are evenly spaced along the length direction of the inner tank body, a defoaming tube is provided on the defoaming box, and the defoaming tube is connected with the defoaming holes, and the defoaming holes are rotatably connected to the inner tank body at the defoaming holes. The sealing plate movably blocks the defoaming holes, and the inner tank body is also provided with a defoaming component for adjusting the amount of defoaming agent according to the amount of initial paint added.
[0024] By adopting the above technical scheme, when it is necessary to add defoaming agent to the initial paint, multiple defoaming tubes are set up at this time. When the added amount of the initial paint is different, different liquid levels correspond to different defoaming tubes and defoaming holes. The defoaming holes are blocked or opened by the set sealing plates, so that the added amount of defoaming agent can be adjusted according to the added amount of different initial paints, thereby achieving accurate addition of defoaming agent and reducing excessive addition.
[0025] Optionally, the defoaming component includes a defoaming block slidably disposed on the inner wall of the inner tank body, the density of the defoaming block is less than the density of the initial coating, and the end side of the defoaming block is tightly fitted against the sealing plate.
[0026] By adopting the above technical scheme, since the density of the defoaming block is set less than the density of the initial coating, as the initial coating is added, the defoaming block slides under the action of buoyancy, and the defoaming block rotates against the sealing plate, thereby opening the defoaming holes. The defoaming block above the liquid level does not rotate under the action of gravity at this time, thereby achieving the blocking of the defoaming holes. Through this setting, the addition amount and addition efficiency of the defoaming agent are controlled, the problem of poor film-forming performance caused by the one-time addition of the defoaming agent is reduced, and the quality of subsequent white board paper is improved.
[0027] Optionally, a connecting ring is coaxially provided on the stirring rod, and the connecting ring is connected to the stirring blade, a first connecting hole and a second connecting hole are opened in the connecting ring, the first connecting hole is connected to the inner cavity of the stirring rod, and the second connecting hole is connected to the stirring blade, an adjustment plate is slidably arranged in the connecting ring, a third connecting hole is provided on the adjustment plate, and the third connecting hole is movably corresponding to the first connecting hole and the second connecting hole, an adjustment rod is slidably arranged in the stirring blade, one end of the adjustment rod is movably fitted and pressed against the sealing plate, a pressing block is provided on the adjustment block, the pressing block is wedge-shaped, and one end of the adjustment rod away from the sealing plate is movably pressed against the pressing block.
[0028] By adopting the above technical scheme, during the stirring process, when the amount of thickener added needs to be adjusted, at this time, with the rotation of the stirring rod, under the damping action of the initial paint, the sealing plate begins to rotate. Since the sealing plate is connected to the adjusting rod, the rotation of the sealing plate drives the adjusting rod to slide, and the end side of the adjusting rod presses against the clamping block, thereby realizing the sliding of the adjusting plate. At this time, the third connecting hole is connected to the first connecting hole and the second connecting hole, thereby realizing the addition of the thickener. When stirring without adding the initial paint, the sealing plate is not affected by the damping action and does not rotate. At this time, the third connecting hole of the adjusting plate is staggered with the first connecting hole and the second connecting hole, so that the thickener in the feeding box is not easy to enter the stirring blade, further reducing the waste of the thickener.
[0029] When the blocking plate rotates to the middle position of the feeding hole, the third connecting hole is connected with the first connecting hole and the second connecting hole, so that the thickener can be added, and the added amount of the thickener is the largest.
[0030] When the blocking plate is subjected to greater damping and rotates to completely block the feeding hole, the adjusting plate slides to the third connecting hole to be staggered with the first connecting hole and the second connecting hole, thereby stopping the addition of the thickener and controlling the amount of thickener added.
[0031] In summary, the present application includes at least one of the following beneficial technical effects: 1. By further eliminating bubbles during the stirring process during the process, the amount of defoamer added can be reduced, thereby reducing the problem of poor film-forming performance caused by the defoamer and improving the surface forming quality of white paper; 2. Through the vacuum stirring device and the electrostatic block installed on the stirring device, the static electricity generated during the stirring process can reduce the surface tension of the liquid, thereby eliminating bubbles and reducing the addition of defoaming agent; 3. Through the setting of the adjustment block, magnetic suction piece, electrostatic block and the adsorption piece set on the electrostatic block, as the initial paint is added, the adjustment block slides under the action of buoyancy, and the adsorption piece and the electrostatic block are driven to slide under the action of the magnetic suction piece, so that the electrostatic block is always consistent with the liquid level, thereby achieving stable adjustment of the surface tension of the liquid surface. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 It is a schematic diagram of the overall structure of the vacuum mixing device in the embodiment of the present application; Figure 2 It is a schematic diagram of the connection structure between the inner tank body and the outer tank body; Figure 3 It is a schematic diagram of the connection structure of the electrostatic component; Figure 4 It is a schematic diagram of the connection structure of the feeding component; Figure 5 It is a schematic diagram of the connection structure of the feeding component.
[0033] Figure numerals: 1, outer tank body; 11, inner tank body; 12, stirring body; 121, stirring rod; 122, stirring blade; 2, electrostatic component; 21, electrostatic block; 22, adjusting member; 221, adjusting block; 222, magnetic member; 223, adsorption member; 23, sliding member; 231, rotating rod; 232, limiting rod; 24, power member; 241, driven gear; 242, driving gear; 25, connecting rod; 3, adding Material assembly; 31, feeding box; 32, feeding hole; 33, blocking plate; 34, elastic member; 35, defoaming box; 36, defoaming tube; 37, defoaming hole; 371, sealing plate; 38, defoaming member; 381, defoaming block; 39, feeding member; 391, connecting ring; 392, first connecting hole; 393, second connecting hole; 394, third connecting hole; 395, pressing block; 396, adjusting rod; 397, adjusting plate. DETAILED DESCRIPTION
[0034] The present application firstly discloses a whiteboard paper primer coating, which comprises the following components: 4200-4300 parts of calcium carbonate, 570-600 parts of china clay, 580-610 parts of styrene-butadiene latex, 180-190 parts of starch adhesive, 8-9 parts of dispersant, 15-17 parts of thickener, 17-19 parts of lubricant, 19-20 parts of water repellent, 7-8 parts of blue dye, 17-18 parts of purple fuel, 11-12 parts of caustic soda, 1.3-1.5 parts of defoamer, 11-12 parts of whitening agent and 50-120 parts of clean water.
[0035] According to the above components, a production process of a white paper primer coating is disclosed, comprising the following steps: S1, weigh and concentrate the raw materials of each component, and accurately weigh out the required raw materials of each component; S2, adding clean water and calcium carbonate into a sealed stirring device and stirring for 5 minutes to form a base material; S3, adding china clay, styrene-butadiene latex, starch adhesive and dispersant to the base material formed in S2, and stirring at high speed for 10 minutes to form a coating base liquid; S4, adding lubricant, blue fuel, purple fuel, caustic soda and brightener to the coating base liquid formed in S3, stirring at a low speed for 5 minutes to form an initial coating; S5, transferring the initial coating to a vacuum mixing device, and adding a defoamer and a thickener through the vacuum mixing device, controlling the amount and rate of addition of the thickener and the defoamer through the vacuum mixing device, and generating static electricity through the vacuum mixing device to reduce the liquid surface tension of the initial coating, thereby further defoaming, reducing bubbles generated during the transfer process and the stirring process, and forming a finished coating; S6, filling and packaging the finished coating formed in S5.
[0036] The following is combined with Figure 1-5 The vacuum mixing equipment used in process step S5 of the present application is further described in detail.
[0037] The present application embodiment discloses a white paper primer coating and its production process. Figure 1 and Figure 2 The vacuum mixing equipment includes an outer tank body 1 arranged obliquely in a vertical direction, an inner tank body 11 coaxially fixed in the outer tank body 1, a accommodating cavity is provided between the outer tank body 1 and the inner tank body 11, a stirring body 12 is rotatably provided in the inner tank body 11, the stirring body 12 includes a stirring rod 121 rotatably passing through the inner tank body 11 and the outer tank body 1, and a plurality of groups of stirring blades 122 arranged at intervals along the length direction of the stirring rod 121, each group of stirring blades 122 includes two stirring blades 122 symmetrically arranged on both sides of the stirring rod 121, in the present application, three groups of stirring blades 122 are provided, in other embodiments, the stirring blades 122 can also be set to two groups, four groups, five groups, etc., and are arranged according to the actual volume of the inner tank body 11, a feed inlet is provided at the top end of the inner tank body 11 and the outer tank body 1, and a discharge outlet is provided at the bottom end of the inner tank body 11 and the outer tank body 1.
[0038] It should also be noted that since the outer tank body 1 and the inner tank body 11 are arranged at an angle, during the process of the stirring body 12 stirring the initial paint, the size of the liquid surface in the inner tank body 11 is larger than that when it is arranged vertically, and since the density of the bubbles is smaller than the density of the initial paint, the bubbles rise and float on the liquid surface under the stirring and mixing of the stirring rod 121 and the stirring blades 122. This part of the bubbles is often considered to be that the defoaming agent has not been added in sufficient amount, and this part of the bubbles may be generated during the stirring and transportation process. If the defoaming agent continues to be added, it will affect the subsequent film-forming properties of the paint. Therefore, this part of the bubbles needs to be eliminated.
[0039] In order to solve the above problems, an electrostatic component 2 is provided in the accommodating cavity. Figure 2 and Figure 3 The electrostatic component 2 includes an electrostatic block 21 slidably arranged in the accommodating cavity. The electrostatic block 21 is in an arc shape. The electrostatic block 21 fits the surface of the inner tank body 11. There are two groups of electrostatic blocks 21. The two groups of electrostatic blocks 21 are arranged relatively and at the same height. An adjusting member 22 for slidingly adjusting the two groups of electrostatic blocks 21 is also provided in the accommodating cavity.
[0040] Reference Figure 2, an adjustment groove is provided on the inner circumferential wall of the inner tank body 11, and the width of the opening side of the adjustment groove is smaller than the width of the bottom side of the adjustment groove, and the adjustment groove is provided along the height direction of the inner tank body 11, and the adjustment member 22 includes an adjustment block 221 slidably arranged in the adjustment groove, and a magnetic suction member 222 is provided on the adjustment block 221, and an adsorption member 223 is provided on one side of the electrostatic block 21, and the adsorption member 223 is made of metal. It should be noted that in the present application, the inner tank body 11 is a conductive non-magnetic material, such as a copper-based material, an aluminum-based material, a carbon-based material, etc., and it should be noted that the density of the adjustment block 221 is less than the density of the initial coating, and the buoyancy received by the adjustment block 221 is greater than the gravity of the magnetic suction member 222 and the adjustment block 221 itself, so that when the initial coating is added, as the initial coating is added, the adjustment block 221 drives the magnetic suction member 222 to always be located on the liquid surface under the action of buoyancy, and the magnetic suction member 222 drives the adsorption member 223 to slide, so that the electrostatic block 21 is always located on the liquid surface.
[0041] At the same time, in order to ensure that static electricity always exists on the surface of the liquid and to facilitate the sliding adjustment of the static electricity block 21, a sliding member 23 is provided in the accommodating chamber. The sliding member 23 includes a rotating rod 231 rotatably arranged in the accommodating chamber along the length direction of the inner tank body 11. The static electricity block 21 is slidably arranged on the rotating rod 231, and the static electricity block 21 rotates relative to the outer surface of the inner tank body 11 as the rotating rod 231 rotates, thereby causing static electricity to exist in the inner tank body 11 and defoaming the initial paint.
[0042] In order to facilitate the rotation adjustment of the rotating rod 231, a power member 24 is provided on the rotating rod 231, and the power member 24 includes a driven gear 241 coaxially fixed on the rotating rod 231. A driving gear 242 is coaxially fixed to one end of the stirring rod 121 that passes through the inner tank body 11. The driven gear 241 is meshed with the driving gear 242. In the present application, the driven gear 241 and the driving gear 242 are both semi-ring-shaped, and a return member is provided on the rotating rod 231 for rotating the rotating rod 231 so that the driven gear 241 and the driving gear 242 remain meshed. The return member is a torsion spring fixed to the rotating rod 231.
[0043] Therefore, when the stirring rod 121 rotates, the driving gear 242 drives the driven gear 241 to rotate, thereby driving the electrostatic block 21 to slide against the outer surface of the inner tank body 11 to generate friction, thereby generating static electricity on the outer surface of the inner tank body 11, thereby achieving the elimination of bubbles on the liquid surface.
[0044] At the same time, in order to realize that when the rotating rod 231 rotates, the electrostatic block 21 rotates, a limiting structure is also provided on the rotating rod 231. The limiting structure includes a connecting rod 25 arranged on the electrostatic block 21. A limiting groove is provided on the end side of the connecting rod 25. The limiting groove is polygonal, and the rotating rod 231 is also polygonal. The rotating rod 231 is slidably adapted to the limiting groove.
[0045] At the same time, in the process of stirring the initial coating, it is necessary to adaptively add thickeners and defoamers. In order to control the amount of thickeners and defoamers added, refer to Figure 3 , Figure 4 and Figure 5 The inner tank body 11 is also provided with a feeding assembly 3, which includes a feeding box 31 arranged in the accommodating cavity, and the feeding box 31 is located at the top side of the inner tank body 11, the stirring rod 121 is arranged in a hollow shape, and the stirring blade 122 is also arranged in a hollow shape. The stirring blade 122 is connected to the stirring rod 121, and the stirring rod 121 is connected to the feeding box 31. At the same time, a feeding hole 32 is opened on the stirring blade 122, and a sealing plate 33 is rotatably arranged at the feeding hole 32. The sealing plate 33 is in contact with the inner circumferential wall of the feeding hole 32, and the rotating shaft of the sealing plate 33 is located in the middle of the feeding hole 32, and an elastic member 34 is provided at the rotating shaft of the sealing plate 33. The elastic member 34 in the present application is also a torsion spring. In the initial position, the sealing plate 33 is The blocking plate 33 is fitted with the peripheral wall of the feeding hole 32, and one end of the blocking plate 33 is movably protruded from the surface of the stirring blade 122. The end of the blocking plate 33 protruding from the stirring blade 122 is fitted with the initial paint, so that when the stirring rod 121 and the stirring blade 122 rotate to stir the initial paint, the blocking plate 33 rotates under the damping action of the initial paint to adjust the opening of the feeding hole 32. When the blocking plate 33 rotates to the middle position, the amount of thickener added is the largest. When the viscosity of the initial paint gradually increases, the damping of the blocking plate 33 becomes larger, so that after the rotation exceeds the middle position, the amount of thickener added gradually decreases, thereby achieving control of the amount of thickener added.
[0046] In order to further reduce the leakage problem of the thickener in the initial state, a connecting ring 391 is coaxially provided on the stirring rod 121, and the connecting ring 391 is fixedly connected to the stirring blade 122 and the stirring rod 121. A first connecting hole 392 is provided on the side of the connecting ring 391 close to the stirring blade 122, and a second connecting hole 393 is provided on the side of the connecting ring 391 close to the stirring rod 121. An adjusting plate 397 is slidably arranged in the connecting ring 391, and the sliding direction of the adjusting plate 397 is consistent with the circumference direction of the connecting ring 391. A third connecting hole 394 is provided on the tightening block 395, and the third connecting hole 394 is movably connected to the first connecting hole 392 and the second connecting hole 393.
[0047] An adjusting rod 396 is slidably arranged inside the stirring blade 122, and a tightening block 395 is provided on the side of the adjusting plate 397 close to the stirring blade 122. The tightening block 395 is wedge-shaped, and one end of the adjusting rod 396 is tightly fitted against the inclined side of the tightening block 395, and the other end of the adjusting rod 396 is tightly fitted against the side wall of the sealing plate 33. When the sealing plate 33 rotates, the rotation of the sealing plate 33 drives the adjusting rod 396 to slide, thereby realizing the connection between the third connecting hole 394 and the second connecting hole 393 and the first connecting hole 392.
[0048] An adjusting spring is fixedly connected to the adjusting plate 397 , and the other end of the adjusting spring is fixedly connected to the inner cavity of the connecting ring 391 .
[0049] At the same time, in order to achieve the control of the amount of defoaming agent added, the feeding component 3 also includes a feeding piece 39, which includes a defoaming box 35 fixed on the outer peripheral wall of the inner tank body 11, and a plurality of defoaming holes 37 are opened on the inner peripheral wall of the inner tank body 11. The defoaming agent is stored in the defoaming box 35, and the defoaming box 35 is connected to a defoaming pipe 36, and the defoaming pipe 36 is connected to the plurality of defoaming holes 37. A sealing plate 371 is rotatably connected to the defoaming hole 37, and the sealing plate 371 movably blocks the defoaming hole 37. The inner tank body 11 is also provided with a defoaming piece 38 which is adjusted according to the amount of initial paint added.
[0050] The defoaming member 38 includes a defoaming block 381 slidably disposed on the inner wall of the inner tank body 11 . The density of the defoaming tube 36 is less than the density of the initial paint, and the end side of the defoaming block 381 is tightly fitted against the sealing plate 371 .
[0051] Since the density of the defoaming block 381 is less than the density of the initial paint, as the initial paint is added, the defoaming block 381 slides under the action of buoyancy, and the defoaming block 381 rotates against the sealing plate 33, thereby opening the defoaming hole 37. The defoaming block 381 above the liquid level does not rotate under the action of gravity at this time, thereby achieving the blocking of the defoaming hole 37. Through this setting, the addition amount and addition efficiency of the defoaming agent are controlled, the problem of poor film-forming performance caused by the one-time addition of the defoaming agent is reduced, and the quality of subsequent white board paper is improved.
[0052] The implementation principle of a white paper primer coating and its production process in the embodiment of the present application is as follows: when the primer coating is produced and stirred, the technician places the initial coating in the inner tank body 11, and when the primer coating is produced, the initial coating that has been stirred is added into the inner tank body 11, and the initial coating is stirred by the set stirring body 12, and the feeding component 3 is set to add the defoaming agent according to the two sides of the initial coating, so as to reduce the film formation problem caused by the one-time addition of the defoaming agent, and the electrostatic block 21 is set relative to the stirring process of the initial coating in the inner tank body 11. The inner tank body 11 slides, thereby generating static electricity in the inner tank body 11. Because the height of the two static blocks 21 is consistent with the height of the liquid level under the action of the adjustment key, the static electricity generated by the friction between the inner tank body 11 and the static blocks 21 directly acts on the liquid surface of the initial coating, thereby reducing the liquid surface tension of the initial coating, thereby reducing the bubbles generated by the initial coating during stirring, and further reducing the addition of defoaming agent, thereby improving the stability of subsequent coating storage, and reducing the problem of reduced film adhesion of the coating due to excessive addition of defoaming agent, thereby improving the quality of the coating after production and the storage period.
[0053] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A white paper primer coating, characterized in that: It includes the following components: 4200-4300 parts of calcium carbonate, 570-600 parts of porcelain clay, 580-610 parts of styrene-butadiene latex, 180-190 parts of starch adhesive, 8-9 parts of dispersant, 15-17 parts of thickener, 17-19 parts of lubricant, 19-20 parts of water repellent, 7-8 parts of blue dye, 17-18 parts of purple fuel, 11-12 parts of caustic soda, 1.3-1.5 parts of defoaming agent, 11-12 parts of whitening agent and 50-120 parts of clean water.
2. A process for producing a white paper primer coating, used for producing a white paper primer coating as claimed in claim 1, characterized in that: The steps include: S1, weighing each component raw material and accurately weighing out the required components raw materials; S2, adding clean water and calcium carbonate into a sealed stirring device and stirring for 5 minutes to form a base material; S3, adding china clay, styrene-butadiene latex, starch adhesive and dispersant to the base material formed in S2, and stirring at high speed for 10 minutes to form a coating base liquid; S4, adding lubricant, blue fuel, purple fuel, caustic soda and brightener to the coating base liquid formed in S3, stirring at a low speed for 5 minutes to form an initial coating; S5, transferring the initial coating to a vacuum mixing device, and adding a defoamer and a thickener through the vacuum mixing device, controlling the amount and rate of addition of the thickener and the defoamer through the vacuum mixing device, and generating static electricity through the vacuum mixing device to reduce the liquid surface tension of the initial coating, thereby further defoaming, reducing bubbles generated during the transfer process and the stirring process, and forming a finished coating; S6, filling and packaging the finished coating formed in S5; The vacuum mixing device used in step S5 comprises an outer tank body (1), an inner tank body (11) coaxially arranged in the outer tank body (1), and a stirring body (12) arranged in the inner tank body (11); the inner tank body (11) is further provided with a feeding component (3) for adding a defoaming agent and a thickening agent, and an electrostatic component (2) for adjusting the surface tension of the liquid in the tank body; and a containing cavity is provided between the outer tank body (1) and the inner tank body (11); The electrostatic assembly (2) comprises an electrostatic block (21) disposed in the accommodating cavity and in contact with the outer peripheral wall of the inner tank body (11); the electrostatic block (21) is slidably disposed in the accommodating cavity, and two groups of the electrostatic blocks (21) are provided, the two groups of the electrostatic blocks (21) are arranged relative to each other, and the accommodating cavity is also provided with an adjusting member (22) for adjusting the two groups of the electrostatic blocks so that the electrostatic blocks (21) and the coating liquid level in the inner tank body (11) are consistent.
3. A white paper primer production process according to claim 2, characterized in that: The inner tank body (11) and the outer tank body (1) are both arranged at an inclination, the adjusting member (22) comprises an adjusting block (221) slidably arranged in the inner tank body (11), the density of the adjusting block (221) is less than the density of the paint, and a magnetic member (222) is provided on the adjusting block (221), the buoyancy of the adjusting block (221) is greater than the gravity of the magnetic member (222), the electrostatic block (21) is provided with an adsorption member that is mutually connected with the magnetic member (222), and the accommodating cavity is further provided with a sliding member (23) for slidably adjusting the electrostatic block (21).
4. A white paper primer production process according to claim 3, characterized in that: The sliding member (23) comprises a rotating rod (231) rotatably arranged in the accommodating cavity, the electrostatic block (21) is slidably arranged on the rotating rod (231), the rotating rod (231) is also provided with a limiting structure for limiting relative rotation between the electrostatic block (21) and the rotating rod (231), and the rotating rod (231) is also provided with a power member (24) for driving the electrostatic block (21) and the inner tank body (11) to slide relative to each other.
5. A white paper primer production process according to claim 4, characterized in that: The stirring body (12) comprises a stirring rod (121) coaxially and uniformly rotating inside the inner tank body (11) and a stirring blade (122) arranged on the stirring rod (121); both ends of the stirring rod (121) are arranged to rotate through the inner tank body (11); the power member (24) comprises a driving gear (242) arranged on one end of the stirring rod (121) penetrating the bottom wall of the inner tank body (11); a driven gear (241) is arranged on the rotating rod (231); the driven gear (241) is in the shape of a half gear ring; the driven gear (241) is movably meshed with the driving gear (242); and a return member is also arranged in the accommodating cavity to drive the rotating rod (231) to rotate so that the driving gear (242) and the driven gear (241) remain meshed.
6. A white paper primer production process according to claim 5, characterized in that: The feeding assembly (3) comprises a feeding box (31) arranged in the accommodating cavity, a thickener is stored in the feeding box (31), the stirring rod (121) is arranged in a hollow shape, a feeding hole (32) is opened on the stirring blade (122), the feeding box (31) is connected to the inner cavity of the stirring rod (121), the stirring rod (121) is connected to the stirring blade (122), and the feeding hole (32) is rotatably arranged A blocking plate (33) is provided, the blocking plate (33) movably blocks the feeding hole (32), and the end side of the blocking plate (33) protrudes from the stirring blade (122), the end side of the blocking plate (33) protruding from the stirring blade (122) is in contact with the initial coating material, and an elastic member (34) is provided at the rotating shaft of the blocking plate (33) for enabling the blocking plate (33) to always block the feeding hole (32).
7. A white paper primer production process according to claim 6, characterized in that: The feeding assembly (3) further comprises a defoaming box (35) arranged on the outer peripheral wall of the inner tank body (11); a plurality of defoaming holes (37) are opened on the inner peripheral wall of the inner tank body (11); the plurality of defoaming holes (37) are evenly spaced along the length direction of the inner tank body (11); a defoaming tube (36) is provided on the defoaming box (35); the defoaming tube (36) is connected to the defoaming holes (37); a sealing plate (371) is rotatably connected to the defoaming holes (37) on the inner tank body (11); the sealing plate (371) movably blocks the defoaming holes (37); and a defoaming member (38) is further provided on the inner tank body (11) for adjusting the amount of defoaming agent according to the amount of the initial coating material added.
8. A white paper primer production process according to claim 7, characterized in that: The defoaming member (38) comprises a defoaming block (381) slidably disposed on the inner wall of the inner tank body (11); the density of the defoaming block (381) is less than the density of the initial coating material; and the end side of the defoaming block (381) is tightly fitted against the sealing plate (371).
9. A white paper primer production process according to claim 7, characterized in that: A connecting ring (391) is coaxially provided on the stirring rod (121), and the connecting ring (391) is connected to the stirring blade (122). A first connecting hole (392) and a second connecting hole (393) are provided in the connecting ring (391). The first connecting hole (392) is connected to the inner cavity of the stirring rod (121), and the second connecting hole (393) is connected to the stirring blade (122). An adjusting block (221) is slidably provided in the connecting ring (391), and a third connecting hole (393) is provided on the adjusting block (221). The third connecting hole (394) is movably connected to the first connecting hole (392) and the second connecting hole (393); an adjusting rod (396) is slidably arranged in the stirring blade (122); one end of the adjusting rod (396) is movably fitted and pressed against the sealing plate (33); a pressing block (395) is provided on the adjusting plate (397); the adjusting block (221) is wedge-shaped; and one end of the adjusting rod (396) away from the sealing plate (33) is movably fitted and pressed against the pressing block (395).