Efficient mist collector and preparation method thereof
By designing an optimized heat sink structure in the fog collector, combined with a graphene PDMS layer and a copper sheet layer, the problem of insufficient thermodynamic influence in the existing technology is solved, achieving efficient fog capture, rapid water delivery and accelerated condensation, significantly improving It improves water collection efficiency and transportation speed and avoids droplet clogging.
Patent Information
- Application Number
- CN202410660538.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-27
- Publication Date
- 2024-10-08
AI Technical Summary
The thermodynamic heat absorption and release of existing fog collectors during the fog collection process have little impact on the fog collection efficiency, resulting in limited fog collection capabilities, slow transportation speed, easy clogging of droplets, and the need to improve the heat dissipation and condensation effects.
A high-efficiency mist collector including a heat sink is designed. A transport groove is set on the surface of the heat sink, using a graphene PDMS layer and a copper layer. The angle between the spines and the transport groove is 30 to 90°, and the tips of the spines are hydrophobic. , the tail end is hydrophilic, the trapezoidal connection and the arc-arc transition connection optimize the droplet transport channel structure and improve thermal management and droplet transport efficiency.
Significantly improve the mist catching performance and water transport performance of the mist collector, the transport speed is increased by about 2.8 times, the condensation efficiency is greatly improved, the water collection efficiency is increased by 300%, avoids droplet clogging, and achieves efficient mist capture and rapid transportation. water and accelerated condensation.
Smart Images

Figure CN118745756A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a mist collector and a manufacturing method thereof, in particular to a high-efficiency mist collector and a manufacturing method thereof. Background Art
[0002] Fresh water is necessary for the survival of all living things on Earth, but due to the rapid growth of population and the pollution of water bodies, people's demand for clean water resources is increasing. Therefore, developing direct and efficient water collection methods is the most direct way to solve this crisis.
[0003] Fog is a widely existing resource on the earth. Fog in the air can be directly converted into fresh water resources for people to use after condensation. By studying the efficient fog collection ability of the structural surfaces in animals and plants, scientists are inspired to develop artificial bionic fog collectors. The existing methods for preparing fog collectors include kirigami cutting, electrospinning, 3D printing, etc., but the fog collectors prepared by these technologies only focus on the improvement of a single performance, and rarely study the influence of thermodynamic heat absorption and heat release on the fog collection efficiency during the fog collection process. Therefore, the fog collection capacity is extremely limited. The ideal fog collector should have the functions of quickly capturing droplets and realizing ultra-fast water transportation, and at the same time have a good thermal management interface to help accelerate the condensation of droplets. The existing two-dimensional fog collectors have low water collection efficiency and slow transportation speed. The transportation speed is slow during the water collection process and even the droplets are prone to clogging. The heat dissipation effect and condensation effect need to be further improved. Summary of the invention
[0004] Purpose of the invention: In order to overcome the deficiencies in the prior art, the purpose of the present invention is to provide an efficient mist collector with efficient fog capture, rapid water delivery and accelerated condensation. Another purpose of the present invention is to provide a method for preparing an efficient mist collector with high processing precision, low processing cost and good wetting performance.
[0005] Technical solution: An efficient mist collector of the present invention comprises a heat sink, and a transport groove is arranged on one of the surfaces of the heat sink; the heat sink comprises a plurality of mist collecting structural units, and the mist collecting structural units are connected by connecting arc transitions, the mist collecting structural units comprise spines and trapezoidal connecting parts, and a plurality of evenly spaced spines are symmetrically arranged on both sides of the trapezoidal connecting part; the tip of the spine is hydrophobic and the tail end is hydrophilic; the angle between the spine and the transport groove is 30 to 90 degrees.
[0006] Furthermore, the heat sink includes a graphene PDMS layer and a copper sheet layer, and a transport groove is arranged in the center of the copper sheet layer.
[0007] Furthermore, the length of the spines is 0.5-1.1 mm, and the angle is 10-23°. The wetting properties of the spines are super hydrophobic, super hydrophobic-super hydrophilic, and super hydrophilic. Preferably, the length of the spines is 0.7 mm, the angle is 12°, and the angle between the spines and the transport groove is 60°.
[0008] Furthermore, the trapezoidal connecting portion and the connecting arc are both hydrophilic.
[0009] Furthermore, the radius of the connecting arc is 1.0-1.4 mm, and the arc length is 0.6-1.0 mm. Preferably, the radius of the connecting arc is 1.2 mm, and the arc length is 0.8 mm.
[0010] Further, the upper base of the trapezoidal connecting portion is 0.3-0.4 mm, the lower base is 0.7-0.9 mm, and the height is 2-2.5 mm. Preferably, the upper base of the trapezoidal connecting portion is 0.35 mm, the lower base is 0.8 mm, and the height is 2.2 mm.
[0011] The method for preparing a high-efficiency mist collector according to the present invention comprises the following steps:
[0012] Step 1, spin coating the PDMS graphene suspension onto the surface of the copper sheet and curing to obtain a copper-graphene PDMS composite layer;
[0013] Step 2: laser cutting the copper-graphene PDMS composite layer according to a preset shape, cleaning it, and obtaining a heat sink with a transport groove on the surface;
[0014] Step three, perform hydrophobic treatment on the tip of the spine, and perform hydrophilic treatment on the tail end, trapezoidal connecting part, and connecting arc of the spine.
[0015] Further, in step 1, the PDMS graphene suspension is prepared by mixing PDMS, a crosslinking agent, and graphene powder in a mass ratio of 10:1:0.2-0.5, with a curing temperature of 60-80°C and a curing time of 4-6 hours. Preferably, the mass ratio of PDMS, a crosslinking agent, and graphene powder is 10:1:0.5. The crosslinking agent is any one of dibutyl phthalate and dibutyltin dilaurate.
[0016] Furthermore, in step 2, the central wavelength of the laser pulse for laser cutting is 350-360 nm, the peak power is 3.8-3.9 W, the beam diameter is 8.5-9.0 μm, the marking speed is 190-200 mm / s, the frequency is 100-120 kHz, the pulse width is 5-7 ns, and the pulse energy density is 25-26 J / cm 2 , the laser scanning path spacing is 4 to 6 μm and the cutting speed is 90 to 100 mm / s.
[0017] Furthermore, in step three, the hydrophobic treatment is to apply the dodecanethiol solution with a cotton swab and then dry it; the hydrophilic treatment is to apply the silicon hydrophilic agent with a cotton swab and then dry it.
[0018] Working principle:
[0019] 1. Mist capture and transportation by thorns: By analyzing the force on a single droplet on the surface of the thorn, it can be known that when the angle between the thorn and the channel is 90°, the droplet receives the Laplace pressure (FL) from the tip of the thorn to the root, the downward gravity (G), and the adhesion force in the opposite direction (FVx, FVy). When the thorn is tilted, the gravity G can be decomposed into Fy and Fx, Fx is coaxial with FL (providing additional driving force for the droplet), according to the trigonometric cosine formula: Fx = G*cosα, when the angle between the thorn and the channel is smaller, the gravity component Fx is greater, the force on the droplet is greater, and the transportation rate is faster. However, when the angle between the cone thorn and the channel is too small, the liquid nucleated on the sides of the adjacent cone thorns will easily form a liquid film after condensation, thereby hindering the transport of droplets on the cone thorns.
[0020] 2. Trapezoidal transport channel: When a droplet passes through the junction of the ladder blocks without transition arcs, the forces acting on the droplet include gravity G, capillary force Fc, Laplace force FL, viscous force Fv composed of pinning force and friction force, and boundary resistance force Fp generated by the boundary of the large end of the wedge block. Among them, Fc and FL are driving forces, and Fv and Fp are reaction forces. The resultant force F1 = G + Fc + FL-Fp-Fv. Among them, FL originates from the special wedge structure; Fc originates from the multi-scale rough microstructure of the grooves on the channel; Fp originates from the pinning force generated on the longitudinal boundary line of the large end of the wedge, which is perpendicular to the direction of droplet transport. Previous literature has shown that once a water droplet moves to the junction of the wedge channel, it will be resisted by the pinning force Fp, resulting in a decrease in the transport rate or even stagnation of droplet transport. In order to reduce the impact of this resistance on the water transport process, we use an arc-shaped joint transition at the wedge connection. Since the water droplets are in a passing state at the connection, the boundary resistance of the droplets at the connection is negligible, and the optimized channel can achieve continuous transportation of droplets. After using the arc connection, the resultant force on the droplets is F2 = G + Fc + FL-Fv. Therefore, the droplet resultant force F2 on the designed arc-optimized wedge channel is greater than the droplet resultant force F1 on the non-optimized channel, so the use of arc-optimized grouped wedge transportation can improve the transportation effect.
[0021] 3. Transport channel grooves: The resultant force during the wetting process from the narrow end to the bottom of the directional trapezoidal channel is: F3 = G + Fc + FL-Fv. The capillary force (Fc) induced by the small groove channel is the dominant driving force, the Laplace pressure (FL) induced by the conical geometry and the liquid gravity G are auxiliary forces, and the main resistance is the viscous force (Fv) composed of pinning force and friction force, which is generated by the interaction of pollutants or molecules on the contact line, resulting in liquid-solid adhesion and hindering the movement of objects on the surface. For channels without grooves: F4 = G + FL-Fv. Due to the loss of capillary force Fc, the liquid resultant force F4 on the channel is reduced, which will rapidly reduce its transport rate. This is why the transport rate of channels with grooves is higher than that of channels without grooves when the channel shape is the same.
[0022] Beneficial effects: Compared with the prior art, the present invention has the following significant features:
[0023] 1. The fog collecting performance and water transport performance of the mist collector have been significantly improved, and the transport speed has been increased by about 2.8 times. There will be no droplet blockage, achieving efficient fog collecting, rapid water transport, and accelerated condensation;
[0024] 2. Integrate thermal management into the mist collector to help significantly improve the condensation efficiency of the mist collector. The mist collection efficiency of the prepared mist collector with heat dissipation film is increased by 126% compared with the mist collector without heat dissipation film.
[0025] 3. The obtained mist collector has excellent water collection efficiency, and the overall mist collection efficiency of the mist collector is increased by 300% compared with the original mist collector. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a schematic diagram of the structure of the present invention; Figure 2 : are optical microscopic images of the present invention, (a) optical image of the copper sheet layer; (a1) optical image of the graphene PDMS layer; (b) microscopic image of the copper sheet layer; (c) microscopic image of the graphene PDMS layer; (d) a local magnified image of the transport groove 2 on the surface of the copper sheet layer; (e) a local magnified image of the graphene PDMS layer;
[0027] Figure 3 It is a schematic diagram of the preparation process of the present invention;
[0028] Figure 4 The morphological characterization diagrams of the present invention include: (a) wetting images of the transport channel at the tip and tail of the spine 111; (b) energy spectrum analysis diagram of the spine 111; (c) energy spectrum analysis diagram of the transport groove 2; (d) scanning electron microscope image of the graphene PDMS layer;
[0029] Figure 5 It is a diagram of the mist collection efficiency of the spines 111 of different sizes of the present invention;
[0030] Figure 6 It is a diagram of the mist collection efficiency at different angles between the spines 111 and the transport channel of the present invention;
[0031] Figure 7 It is a diagram of the mist collection efficiency of different modification treatment methods of the thorn 111 of the present invention;
[0032] Figure 8 is a diagram of droplet transport rates on different channel structures of the present invention;
[0033] Fig. 9 This is a diagram showing the temperature rise of graphene-PDMS heat dissipation films with different ratios of the present invention when irradiated by a xenon lamp;
[0034] Fig.10This is a diagram of mist collection efficiency of mist collectors loaded with graphene-PDMS heat dissipation films of different proportions according to the present invention;
[0035] Fig.11 It is a comparison diagram of the mist collecting effects of the mist collector of the present invention and the comparative example. DETAILED DESCRIPTION
[0036] A method for preparing a high-efficiency mist collector comprises the following steps:
[0037] (1) Preparation of copper-graphene PDMS composite heat sink 1: First, clean a copper sheet with a thickness of 80 μm with ethanol in an ultrasonic cleaner for 10 minutes, and then rinse with deionized water for further use. Then, the PDMS solution (PDMS: cross-linking agent mass ratio 10:1) and graphene powder are fully mixed in a mass ratio (20:1). The cross-linking agent is any one of dibutyl phthalate and dibutyltin dilaurate. The PDMS-graphene suspension is spin-coated on the surface of the copper sheet at a speed of 2000 rpm for 1 minute, and then the Cu-PDMS sheet is cured in a drying oven at 80°C for 4 hours to obtain a copper-graphene PDMS composite layer.
[0038] (2) Laser cutting: The copper-graphene PDMS composite layer was irradiated by a laser processing system. The laser pulse was a near-Gaussian pulse with a central wavelength of 355 nm, a peak power of 3.83 W, a beam diameter of 8.6 μm, a marking speed of 200 mm / s, a frequency of 100 kHz, a pulse width of 5 ns, and a pulse energy density of 25.89 J / cm 2 , the laser scanning path spacing is 5μm. All sketches are first designed using EzcadZeu soft, and the transport groove 2 (gradient micro groove) is etched on the copper sheet at a speed of 800mm / s, and then a two-dimensional high-efficiency fog collector structure is cut from the copper-graphene PDMS composite layer at a speed of 100mm / s. The laser-processed sheet is cleaned with ethanol in an ultrasonic cleaner for 3min to remove surface residues. Rinse with deionized water for 3 minutes to remove the alcohol on the surface, and obtain a heat sink 1 with a transport groove 2 on the surface.
[0039] (3) Treatment of mist collector wetting properties: Use a cotton swab to apply n-dodecyl mercaptan solution to the tip of the cut spines 111 for hydrophobic treatment and dry it in a drying oven at 60°C for 30 minutes, so that the tip of the mist collector spines 111 has super hydrophobic properties. Use a cotton swab to evenly apply a silicone hydrophilic agent to the transport groove 2, the tail end of the spines 111, the trapezoidal connecting part 112, and the connecting arc 12 of the copper sheet layer for hydrophilic treatment and dry it in a drying oven at 60°C for 30 minutes, so that the transport channel and the tail end of the spines 111 have super hydrophilic properties.
[0040] like Figures 1-2The high-efficiency mist collector obtained in this embodiment includes a heat sink 1, which is composed of a graphene PDMS layer and a copper sheet layer bonded up and down. A transport groove 2 is arranged in the center of the copper sheet layer. The heat sink 1 includes a plurality of mist collecting structural units 11, and the mist collecting structural units 11 are connected by a connecting arc 12. The mist collecting structural unit 11 includes a spine 111 and a trapezoidal connecting portion 112, and a plurality of evenly spaced spines 111 are symmetrically arranged on both sides of the trapezoidal connecting portion 112. The tip of the spine 111 is hydrophobic, and the tail end is hydrophilic. The angle between the spine 111 and the transport groove 2 is 30 to 90°. The length of the spine is 0.5 to 1.1 mm, and the angle is 10 to 15°. The radius of the connecting arc 12 is 1.0 to 1.4 mm, and the arc length is 0.6 to 1.0 mm. The upper base of the trapezoidal connecting portion 112 is 0.3-0.4 mm, the lower base is 0.7-0.9 mm, and the height is 2-2.5 mm. Preferably, the length of the spine is 0.7 mm, the angle is 12°, and the angle between the spine 111 and the transport groove is 60°.
[0041] The preparation process of the mist collector is as follows: Figure 3 After the preparation, the contact angles of the hydrophobic treated thorn tip and the hydrophilic treated transport channel were measured to be 142° and 2°, respectively. Figure 4 As shown in a. Figure 4 As shown in b, the results of energy dispersive spectroscopy (EDS) analysis of the spike tip show that carbon (C), oxygen (O), and sulfur (S) elements are evenly distributed on the surface of the SH-S2 sample, and their contents can reach up to 31.2%, 0.9%, and 0.1%, respectively, indicating that the sulfur element has been successfully deposited and the channel surface has been successfully super-hydrophobic modified; Figure 4 The microstructure of the groove channel shown in c is a typical laser processing morphology, with micro / nano-scale particles produced by the melting and resolidification of Cu. The path composed of the laser spot forms the groove channel, so the SEM image of the groove channel appears as interconnected circular pits. The results of energy spectrum analysis (EDS) on the channel surface show that carbon (C), oxygen (O), and silicon (Si) elements are evenly distributed on the surface of the SH-S2 sample, and their contents can reach up to 32.8%, 18.5%, and 2.6%, respectively, indicating that the silicon hydrophilic agent has been successfully deposited and the channel surface has been successfully super-hydrophilic modified; Figure 4 As shown in Figure e, the cross-sectional SEM image of the heat dissipation film with a PDMS: graphene mass ratio of 20:1 shows that the PMDS is colloidal with smooth edges, and the graphene nanosheets are thin, with uneven edges and irregular shapes. The image shows that the graphene nanosheets are evenly distributed on the composite material.
[0042] In order to explore the effect of different sizes of thorns 111 on the fog collection efficiency, Figure 5The included angles between the spines 111 and the transport groove 2 are set to 30°, 45°, 60°, 75°, and 90°, respectively. The length of the spines is 0.7 mm, and the included angle is 12°. It can be seen that when the included angle between the spines 111 and the transport groove is 60°, the WCR is 19.89 g·cm -2 ·h -1 , the fog collection efficiency is the highest. Figure 6 The lengths of the spines 111 are set to 0.5 mm, 0.7 mm, 0.9 mm, and 1.1 mm, respectively, with an angle of 12°. The angle between the spines 111 and the transport groove is 60°, with an angle of 12°. It can be seen that when the length of the spines 111 is 0.7 mm, the WCR is 20.07 g·cm -2 ·h -1 , the fog collection efficiency is the highest. Figure 7 , the wettability of the spine 111 was set to be completely hydrophobic (SHB), completely hydrophilic (SHL), and hydrophobic tip and hydrophilic tail (SHB-SHL), the angle with the transport groove was 60°, the angle was 12°, the length was 0.7 mm, and the WCR was 21.25 g·cm -2 ·h -1 , the fog collection efficiency is the highest.
[0043] Channel transport rate test: The prepared super-hydrophilic channels SC, SCG, CC, and CCG are clamped vertically and horizontally, and a droplet of about 2 μm is dropped 1 cm away from the end of the channel. The droplet drips rapidly along different channels. Figure 4 As shown in a, at 0.03s, the droplet transport on CCG is the fastest, followed by SCG; at 0.05s, the droplet transport speed on CC surpasses SCG, and the droplets on CCG channel reach the tail; the droplets on CC also reach the bottom at 0.07s, and finally at 0.14s, all the droplets on the four channels reach the tail. Figure 8 As shown in Figure 2, we calculated the transport rates of the four channels and found that CCG>CC>SCG>SC, with the transport rate of CCG reaching 200 mm·s -1 , which is about 2.8 times the transport rate of CC.
[0044] PDMS-graphene heat sink heat dissipation performance test:
[0045] The composite sheets with PDMS-Graphene heat dissipation film attached to the surface were irradiated with a xenon lamp. The irradiation power of the xenon lamp was 1 sun intensity and the distance between the xenon lamp and the sheet was 20 cm. The surface temperature of the composite sheet was measured after irradiation for 5, 10, 20 and 30 minutes. It can be seen that the surface temperature of the PDMS-Graphene heat dissipation film is continuously lower than the Cu surface and the surface temperature of the heat dissipation film is uniform. Fig. 9The surface temperature rise of the PDMS-Graphene heat dissipation film when the mass ratios are 20:1, 30:140:1, and 50:1 respectively, after irradiation with a xenon lamp for 30 minutes. It can be seen that the surface temperature of the heat dissipation film of 20:1 is the lowest, and it has the best heat dissipation effect. As the ultra-high thermal conductivity of graphene shows, the higher the amount of graphene added, the higher the heat dissipation rate of the composite film. However, experiments have found that too high an addition amount will cause the PDMS to fail to solidify into a film, and the weight ratio of 20:1 is the best ratio for film formation under the condition of a high graphene mass ratio.
[0046] Fog collection performance test:
[0047] A self-made indoor fog collection experimental system was built, and a universal sample holder was used to clamp the prepared fog collector with spines of different shapes and wettability. In order to simulate the fog in the natural environment, a humidifier (fog flow rate of 370ml / h) was used to generate fog flow. The distance between the sample and the humidifier nozzle was 3cm, and the droplet diameter was 1-5μm. The relative humidity in the laboratory was ≥90%, and the temperature was ≤25±1℃. The water collection rate (WCR) was calculated by the formula: Calculate, where M is the water mass, A (cm 2 ) is the surface area of the fog collector, and t(h) is the fog collection experiment time. Fog collection experiments were carried out on fog collectors containing four auxiliary heat dissipation films with different mass ratios. Fig.10 It can be seen that with the increase of graphene content, the mist collection efficiency increases, but it is still higher than that of the mist collector without PDMS-Graphene heat dissipation film. In addition, it can be seen that the WCR with a mass ratio of 20:1 is the highest, which is ≈48.94 g·cm -2 ·h -1 , which is 1.3 times that of the fog collector without PDMS-Graphene heat dissipation film. These results strongly verify that loading PDMS-Graphene heat dissipation film does play a key role in improving the fog collection performance.
[0048] Comparative Example
[0049] In this comparative example, step (3) in the above embodiment is omitted, and the wettability treatment is not performed to obtain an original mist collector.
[0050] like Fig.11, a comparative analysis was conducted in the initial fog collection wetting stage and the continuous fog collection stage. The fog collection performance of the optimized fog collector in the two stages was significantly better than that of the original fog collector in the comparative example. In the initial wetting stage, when the fog flow reaches the fog collector 1s after, the droplets captured on the thorns of the fog collector of this embodiment are significantly more than those of the original fog collector, and the nucleated droplets are larger. When the fog collector is wetting, it is observed that the volume of droplets on the thorns of the fog collector of this embodiment is much larger than that of the original fog collector. When the fog collector continues to capture fog, due to the surface viscosity of the original fog collector, the collected droplets continue to merge and increase in the transport channel until the channel is blocked, and smooth transportation cannot be carried out. In addition, the fog capture efficiency of the thorns is low, and the fog capture cannot be continuous. The water collected on the mist collector channel of this embodiment can be continuously transported without channel blockage, and it can also be observed that the droplets on the optimized mist collector spines are continuously condensing and transporting them to the channel. These experimental phenomena can prove that the mist collector of this embodiment after multi-path optimization has excellent water collection performance.
Claims
1. A high-efficiency mist collector, Features: The invention comprises a heat sink (1), wherein a transport groove (2) is arranged on one of the surfaces of the heat sink (1); the heat sink (1) comprises a plurality of mist collecting structural units (11), wherein the mist collecting structural units (11) are connected to each other by a connecting arc (12) in a circular arc transition manner, wherein the mist collecting structural units (11) comprise spines (111) and a trapezoidal connecting portion (112), wherein a plurality of evenly spaced spines (111) are symmetrically arranged on both sides of the trapezoidal connecting portion (112); the tip of the spine (111) is hydrophobic, and the tail end is hydrophilic; and the angle between the spine (111) and the transport groove (2) is 30 to 90 degrees.
2. A high-efficiency mist collector according to claim 1, Features: The heat sink (1) comprises a graphene PDMS layer and a copper sheet layer, and a transport groove (2) is arranged at the center of the copper sheet layer.
3. A high-efficiency mist collector according to claim 1, Features: The length of the thorn is 0.5-1.1 mm, and the angle is 10-23°.
4. A high-efficiency mist collector according to claim 1, Features: The trapezoidal connecting portion (112) and the connecting arc (12) are both hydrophilic.
5. A high-efficiency mist collector according to claim 1, Features: The radius of the connecting arc (12) is 1.0-1.4 mm, and the arc length is 0.6-1.0 mm.
6. A high-efficiency mist collector according to claim 1, Features: The upper base of the trapezoidal connecting portion (112) is 0.3-0.4 mm, the lower base is 0.7-0.9 mm, and the height is 2-2.5 mm.
7. The method for preparing a high-efficiency mist collector according to claim 1, It is characterized in that The following steps are involved: Step 1, spin coating the PDMS graphene suspension onto the surface of the copper sheet and curing to obtain a copper-graphene PDMS composite layer; Step 2: laser cutting the copper-graphene PDMS composite layer according to a preset shape, cleaning it, and obtaining a heat sink (1) having transport grooves (2) and spines (111) on the surface; Step three, performing a hydrophobic treatment on the tip of the thorn (111), and performing a hydrophilic treatment on the tail end of the thorn (111), the trapezoidal connecting portion (112), and the connecting arc (12).
8. The method for preparing a high-efficiency mist collector according to claim 7, Features: In the step 1, the PDMS graphene suspension is prepared by mixing PDMS, a cross-linking agent, and graphene powder in a mass ratio of 10:1:0.2-0.5, with a curing temperature of 60-80° C. and a curing time of 4-6 hours.
9. The method for preparing a high-efficiency mist collector according to claim 7, Features: In the step 2, the central wavelength of the laser pulse for laser cutting is 350-360nm, the peak power is 3.8-3.9W, the beam diameter is 8.5-9.0μm, the marking speed is 190-200mm / s, the frequency is 100-120kHz, the pulse width is 5-7ns, and the pulse energy density is 25-26J / cm 2 , the laser scanning path spacing is 4 to 6 μm and the cutting speed is 90 to 100 mm / s.
10. The method for preparing a high-efficiency mist collector according to claim 7, Features: In the step three, the hydrophobic treatment is to apply the n-dodecanethiol solution with a cotton swab and then dry it; the hydrophilic treatment is to apply the silicon hydrophilic agent with a cotton swab and then dry it.
Citation Information
Cited By
Bionic aloe evaporation and capture integrated all-weather water collecting device and manufacturing method
CN120441011A
Manufacturing method of mist collector with spiral structure and mist collector
CN121374033A