Aerosol generating device as well as preparation method and application thereof

By adding hollow devices and flow guide layers in the hollow section of the aerosol generating device, the problem of matrix displacement caused by the interaction between the heating appliance and the aerosol matrix is ​​solved, the heating efficiency and the release efficiency of aroma substances are improved, and the sensory quality and Consumer satisfaction.

CN118749706APending Publication Date: 2024-10-11CHINA TOBACCO HUNAN IND CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411124076.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

When the heating appliance in the aerosol generating device interacts with the aerosol matrix, it often causes matrix displacement, reducing heating efficiency and fragrance substance release efficiency, and affecting sensory quality.

Method used

A hollow device is added to the hollow section of the aerosol generating device. The hollow device has a flow guide layer and a flow guide channel to block substrate displacement, and increases the air passage through the flow guide layer to improve the release efficiency of fragrance substances.

Benefits of technology

It improves the heating efficiency, reduces the difficulty and cost of processing technology, and improves the sensory quality and consumer satisfaction of the aerosol generating device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118749706A_ABST
    Figure CN118749706A_ABST
Patent Text Reader

Abstract

The invention provides an aerosol generating device which comprises a filtering section, a hollow section and an aerosol matrix section which are sequentially connected, the hollow section comprises a hollow device, the hollow device is provided with a flow guide layer, and the flow guide layer is provided with a flow guide channel. According to the aerosol generating device, the hollow device is additionally arranged in the hollow section, the effect of preventing the aerosol matrix from displacing can be achieved by additionally arranging the hollow device in the hollow section, the aerosol matrix can be prevented from displacing, and then the heating efficiency and the sensory quality of the aerosol generating device are improved. In addition, the flow guide layer of the hollow device is provided with the flow guide channels, air passing channels are increased, more air paths are formed, the release efficiency of the fragrant substances is improved, and the sensory quality of the aerosol generating device is further improved. The flow guide layer of the hollow device reduces the suction resistance, so that the aerosol generating device is low in suction resistance and good in suction easiness.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of aerosol heating, and in particular to an aerosol generating device and a preparation method and application thereof. Background Art

[0002] With the enhancement of health awareness, people have realized that traditional cigarettes are harmful to health, so aerosol generating devices came into being.

[0003] The aerosol generating device heats the aerosol matrix through a heating device to release the aerosol. Because the heating temperature is usually between 200℃ and 400℃, no complex chemical reaction occurs, and the harmful components produced are greatly reduced compared to the high-temperature combustion of the aerosol matrix at 600~900℃.

[0004] The aerosol generating device is used in conjunction with a heating device for heating. When the heating device is used for heating, there are usually two methods: peripheral heating and central heating. For centrally heated heated cigarettes, the heating device usually has a needle-type or sheet-type central heating device. When in use, the heating component is inserted into the aerosol matrix of the aerosol generating device, and electricity is turned on to generate high temperature to heat the aerosol matrix of the aerosol generating device, thereby releasing aerosol.

[0005] The aerosol matrix of an aerosol generating device is generally made of reconstituted tobacco leaves, shredded tobacco, shredded tobacco stems, etc. When the aerosol matrix is ​​heated by a heating device, the heating device of the heating device interacts with the aerosol matrix, such as: the central heating device pushes on the aerosol matrix when inserted into it, and the surrounding heating devices squeeze the aerosol matrix, which often causes the aerosol matrix to deform or displace, reducing the heating efficiency, low the efficiency of releasing flavor substances, and affecting the sensory quality. Summary of the invention

[0006] Based on this, it is necessary to provide an aerosol generating device and a preparation method and application thereof, aiming to avoid displacement of the aerosol matrix and improve the sensory quality of the aerosol generating device.

[0007] In a first aspect of the present application, an aerosol generating device is provided, comprising a filter section, a hollow section and an aerosol matrix section connected in sequence, wherein the hollow section comprises a hollow device, the hollow device has a guide layer, and the guide layer has a guide channel.

[0008] The aerosol generating device of the present application adds a hollow device in the hollow section. Adding a hollow device in the hollow section can play a role in preventing the displacement of the aerosol matrix. When the heating device heats the aerosol matrix and the heating device interacts with the aerosol matrix, the aerosol matrix can be prevented from being displaced, thereby improving the heating efficiency, reducing the difficulty and cost of the processing technology, and improving the sensory quality of the aerosol generating device. The hollow channel of the hollow device forms a first air path. At the same time, a guide layer is arranged on the hollow device. The guide layer has a guide channel, thereby increasing the air passage and forming more air paths, thereby improving the release efficiency of the aroma substance and further improving the sensory quality of the aerosol generating device. The guide layer of the hollow device reduces the suction resistance, so that the aerosol generating device has low suction resistance, good suction ease, less adsorption and retention of the aroma substance generated by the aerosol matrix section, and finally obtains unexpected results in improving the sensory quality and consumer satisfaction of the aerosol generating device.

[0009] In some of the embodiments, the wall thickness of the hollow device is 0.6-2.7 mm.

[0010] In some embodiments, the guide layer is a hollow guide layer provided with the guide channel.

[0011] In some embodiments, the guide layer is rolled to form a hollow tubular structure.

[0012] In some embodiments, the hollow device further comprises wrapping paper, and the wrapping paper is arranged on at least one of the inner wall and the outer wall of the hollow tubular structure formed by rolling the guide layer.

[0013] In some embodiments, at least one surface of the guide layer has a concave-convex structure.

[0014] In some embodiments, the guide layer material is paper, rubber or plastic.

[0015] In some embodiments, the concave-convex structure includes at least one of a corrugated structure or a matrix concave-convex structure.

[0016] In some embodiments, the guide layer is corrugated paper, the corrugation height of the corrugated paper is 0.5 mm to 2.5 mm, and the number of corrugations in the corrugated paper in the extension direction of the corrugations per 300 mm length is 100 to 200.

[0017] In some embodiments, the guide layer is a convex dot paper, and the convex dot paper is provided with a plurality of protrusions, the average height of the protrusions is 0.5mm~2.5mm, and the area occupied by a single protrusion is 1mm 2 ~4mm 2, all of the protrusions account for 5% to 60% of the area of ​​the convex point paper.

[0018] In some embodiments, the guide layer is a convexo-convex paper, and the convexo-convex paper is provided with a plurality of protrusions and pits, the average height of the protrusions is 0.5 mm to 2.5 mm, the average depth of the pits is 0.5 mm to 2.5 mm, and the area occupied by a single protrusion or a single pit is 1 mm 2 ~4mm 2 , all the protrusions and the pits account for 5% to 60% of the area of ​​the convex-concave paper.

[0019] In some embodiments, the guide layer carries aroma substances.

[0020] In some embodiments, the guide layer further includes particulate matter, the aroma substance is loaded on the particulate matter to form a complex, and the complex is disposed on the guide layer.

[0021] In some embodiments, the composite is bonded to the surface of the guide layer.

[0022] In some embodiments, the average particle size of the particles is 60-120 mesh.

[0023] In some embodiments, the amount of particles added is 10 g / m 2 ~300g / m 2 .

[0024] In some embodiments, the particulate matter is one or more of diatomaceous earth, montmorillonite, sepiolite, kaolin, calcium oxide, calcium carbonate, calcium hydroxide, calcium sulfate, activated carbon, molecular sieve, tea stem particles, tangerine peel particles, orange peel particles, grapefruit peel particles, peanut shell particles and tangerine peel particles.

[0025] In some embodiments, the loading mass of the aroma substance in the guide layer is 1% to 50%.

[0026] In some embodiments, the aroma substance is one or more of cocoa aroma, coffee aroma, nut aroma, milk aroma, tea aroma, cantaloupe aroma, cucumber aroma, orange aroma, grapefruit aroma, watermelon aroma, date aroma, clove, mint aroma and hay aroma.

[0027] In some embodiments, the hollow device comprises a fragrance segment and a fragrance-free segment connected to each other, the fragrance segment is located between the aerosol matrix and the fragrance-free segment, and the fragrance segment is loaded with fragrance substances.

[0028] In some embodiments, the axial length ratio of the fragrance segment to the fragrance-free segment is 1:5 to 5:1.

[0029] In some embodiments, the ratio of the wall thickness of the fragrance segment to the wall thickness of the non-scented segment is 1:0.5~1.

[0030] In some embodiments, the total length of the hollow device is 5 to 50 mm.

[0031] In some embodiments, the hollow device is cylindrical and coaxially attached to the inner wall of the hollow section.

[0032] The second aspect of the present application provides a method for preparing the aerosol generating device as described in the first aspect, the method comprising the steps of preparing the hollow device:

[0033] 1) Wrapping the guide layer with wrapping paper on the outside or both sides of the guide layer to form a hollow tubular device;

[0034] 2) Cutting the hollow tubular device into pieces to obtain the hollow device.

[0035] In some embodiments, the preparation of the hollow device further comprises at least one of the following preparation steps:

[0036] 1) Loading the aroma substance on the guide layer;

[0037] 2) Loading the aroma substance on the particles, and then loading the particles on the guide layer.

[0038] In some embodiments, the aroma substance is loaded onto the guide layer and / or the particulate matter by spraying, coating or soaking.

[0039] A third aspect of the present application provides an aerosol generating system, comprising the aerosol generating device and a heating device as described in the first aspect.

[0040] In some embodiments, the heating device includes a heating component, a battery component for powering the heating device, a control component for controlling the battery component, and a housing for accommodating the heating component, the battery component, and the control component.

[0041] In some embodiments, the heating length of the heating component in the hollow segment is 0-100% of the length of the hollow segment, and the heating position extends from the adjacent portion of the hollow segment and the aerosol matrix to the adjacent portion of the hollow segment and the filter segment. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] Figure 1 This is a schematic diagram of the axial cross-sectional structure of an aerosol generating device according to one embodiment of the present application.

[0043] Figure 2Schematic diagram of corrugated paper structure.

[0044] Figure 3 for Figure 2 Schematic diagram of the cross-sectional structure of medium corrugated paper.

[0045] Figure 4 for Figure 2 Schematic diagram of the structure of the medium corrugated paper roll when it is made into a guide layer.

[0046] Figure 5 Schematic diagram of the convex paper structure.

[0047] Figure 6 for Figure 5 Schematic diagram of the cross-sectional structure of the convex dot paper.

[0048] Figure 7 Schematic diagram of the cross-sectional structure of convexo-concave paper.

[0049] Figure 8 Schematic diagram of the position relationship between the outer wrapping paper and the corrugated paper during rolling.

[0050] Fig. 9 For Press Figure 8 Schematic diagram of the cross-sectional structure of the hollow device obtained by rolling.

[0051] Fig.10 Schematic diagram of the position relationship between the outer wrapping paper and the corrugated paper during rolling.

[0052] Fig.11 For Press Fig.10 Schematic diagram of the cross-sectional structure of the hollow device obtained by rolling.

[0053] Fig.12 This is a schematic diagram of the positional relationship between the outer wrapping paper, corrugated paper and inner wrapping paper during rolling.

[0054] Fig.13 For Press Fig.12 Schematic diagram of the cross-sectional structure of the hollow device obtained by rolling.

[0055] Fig.14 This is a schematic diagram of the positional relationship between the outer wrapping paper, corrugated paper and inner wrapping paper during rolling.

[0056] Fig.15 For Press Fig.14 Schematic diagram of the cross-sectional structure of the hollow device obtained by rolling.

[0057] Fig.16 This is a schematic diagram of the cross-sectional structure of the first hollow device made of convex paper for the guide layer.

[0058] Fig.17 This is a schematic diagram of the cross-sectional structure of the second hollow device whose guide layer is made of convex paper.

[0059] Fig.18 This is a schematic diagram of the cross-sectional structure of the third hollow device made of convex paper as the guide layer.

[0060] Fig.19 Schematic diagram of the loading state of particles on corrugated paper.

[0061] Fig. 20 Schematic diagram of the loading state of particles on corrugated paper after being rolled into a hollow device.

[0062] Description of reference numerals:

[0063] 1. Wrapping material; 11. Filter section; 12. Hollow section; 13. Aerosol matrix section; 2. Filter body; 3. Aerosol matrix; 4. Hollow device; 41. Guide layer; 411. Guide channel; 5. Hollow gap; 6. Particles; 7. Outer paper; 8. Inner paper. DETAILED DESCRIPTION

[0064] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present invention, so the present invention is not limited by the specific embodiments disclosed below.

[0065] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0066] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which the present invention belongs. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.

[0067] In a first aspect of the present application, an aerosol generating device is provided, which will be described in detail below with reference to the accompanying drawings.

[0068] An aerosol generating device according to one embodiment of the present application comprises a filter section, a hollow section and an aerosol matrix section connected in sequence, wherein the hollow section comprises a hollow device, the hollow device has a guide layer, and the guide layer has a guide channel.

[0069] It is understandable that the filter section here includes wrapping material and filter body, the hollow section includes wrapping material and hollow device, and the aerosol matrix section includes wrapping material and aerosol matrix. The wrapping material includes but is not limited to wrapping paper and tipping paper.

[0070] The aerosol generating device of the present application adds a hollow device in the hollow section. Adding a hollow device in the hollow section can play a role in preventing the displacement of the aerosol matrix. When the heating device heats the aerosol matrix and the heating device interacts with the aerosol matrix, the aerosol matrix can be prevented from being displaced, thereby improving the heating efficiency, reducing the difficulty and cost of the processing technology, and improving the sensory quality of the aerosol generating device. The hollow channel of the hollow device forms a first air path. At the same time, a guide layer is arranged on the hollow device. The guide layer has a guide channel, thereby increasing the air passage and forming more air paths, thereby improving the release efficiency of the aroma substance and further improving the sensory quality of the aerosol generating device. The guide layer of the hollow device reduces the suction resistance, so that the aerosol generating device has low suction resistance, good suction ease, less adsorption and retention of the aroma substance generated by the aerosol matrix section, and finally obtains unexpected results in improving the sensory quality and consumer satisfaction of the aerosol generating device.

[0071] As an example, the aerosol generating device may be a heat-not-burn cigarette, but is not limited thereto.

[0072] In some of these implementations, see Figure 1 An aerosol generating device according to one embodiment of the present application comprises a wrapping material 1, a filter body 2, a hollow device 4 and an aerosol matrix 3, wherein the filter body 2 is arranged in the filter segment 11, the hollow device 4 is arranged on the inner wall of the hollow segment 12 and fills part of the hollow segment 12, the aerosol matrix 3 is arranged in the aerosol matrix segment 13, one end of the hollow device 4 abuts against the filter body 2, and the other end abuts against the aerosol matrix 3; a guide layer 41 is arranged on the hollow device 4, and the guide layer 41 carries fragrance substances.

[0073] In some of these implementations, see Figure 1 The hollow device 4 is cylindrical and coaxially attached to the inner wall of the hollow section 12 .

[0074] It can be understood that the cylindrical hollow device has a hollow portion, which serves as a flue gas passage and cooling channel.

[0075] It can be understood that the aerosol generating device includes a cylindrical structure formed by a wrapping material, one end of the cylindrical structure is a filter section, a filter body is arranged inside the filter section, the other end of the cylindrical structure is an aerosol matrix section, an aerosol matrix is ​​arranged inside, and a hollow section is between the filter section and the aerosol matrix section. The hollow section is not filled with a filter body and an aerosol matrix material to form a channel, and the hollow device is arranged on the inner wall of the hollow section and fills part of the channel.

[0076] In some embodiments, the wall thickness of the hollow device is 0.6-2.7 mm, preferably 1.0-2.7 mm, more preferably 1.2-2.7 mm, and most preferably 1.5-2.5 mm.

[0077] As an example, the wall thickness of the hollow device can be 0.6mm, 0.7mm, 0.8mm, 0.9mm, 1.0mm, 1.1mm, 1.2mm, 1.3mm, 1.4mm, 1.5mm, 1.6mm, 1.7mm, 1.8mm, 1.9mm, 2.0mm, 2.1mm, 2.2mm, 2.3mm, 2.4mm, 2.5mm, 2.6mm, 2.7mm, 2.8mm, 2.9mm, 3.0mm, 3.1mm, 3.2mm, or within a range consisting of any two of the aforementioned values ​​as end values.

[0078] In some embodiments, the guide layer is a hollow guide layer provided with the guide channel. The guide channel is not only conducive to the passage of smoke and reduces the inhalation resistance, but also can improve the release efficiency of the flavor substance.

[0079] In some embodiments, the guide layer is rolled to form a hollow tubular structure.

[0080] In some embodiments, the hollow device further comprises wrapping paper, and the wrapping paper is arranged on at least one of the inner wall and the outer wall of the hollow tubular structure formed by rolling the guide layer.

[0081] Understandably, see Fig.13 The outer paper 7 is arranged on the outer wall of the hollow tubular structure formed by rolling the guide layer, and the inner paper 8 is arranged on the inner wall of the hollow tubular structure formed by rolling the guide layer.

[0082] In some embodiments, at least one surface of the guide layer has a concave-convex structure. The concave-convex structure on the surface is to form a gap space between the concave and convex surfaces of the guide layer and the wrapping paper, thereby forming a guide channel, thereby reducing the suction resistance and improving the release efficiency of the aroma substance.

[0083] In some embodiments, the guide layer material is paper, rubber or plastic.

[0084] In some embodiments, the concave-convex structure includes at least one of a corrugated structure or a matrix concave-convex structure.

[0085] In some of these implementations, see Figure 2 and Figure 3 , the guide layer is corrugated paper, the corrugation height of the corrugated paper is 0.5mm~2.5mm, and in the extension direction of the corrugations in the corrugated paper, the number of corrugations per 300mm length is 100~200. The corrugation height of the corrugated paper is preferably 1.0mm~2.0mm, more preferably 1.2mm~1.8mm. The number of corrugations of the corrugated paper is preferably 140~160 / 300mm. Corrugated paper is used as the guide layer on the hollow device, the hollow channel of the hollow device forms the first air path, the internal gap of the corrugated paper constitutes the second air path, and the corrugated surface of the corrugated paper constitutes the third air path, thereby improving the release efficiency of the flavor substance, reducing the inhalation resistance, and ultimately improving the sensory quality of the aerosol generating device.

[0086] Corrugated paper is also called corrugated paper, which is a single-layer corrugated paper, that is, one side of the corrugated paper is bonded to the flat paper. Figure 4 After being wound and rolled into a hollow device, the corrugated paper forms a guide layer, and the corrugations of the corrugated paper form a spiral guide channel 411.

[0087] In some of these implementations, see Figure 5 and Figure 6 The guide layer is a convex dot paper, and the convex dot paper is provided with a plurality of protrusions, the average height of the protrusions is 0.5mm~2.5mm, and the area occupied by a single protrusion is 1mm 2 ~4mm 2 , all the protrusions account for 5% to 60% of the area of ​​the convex paper. The protrusions of the convex paper play a supporting role, and the gaps between the protrusions form a guide channel, which is conducive to gas circulation.

[0088] Furthermore, the average height of the protrusions is preferably 1.0 mm to 2.0 mm, more preferably 1.2 mm to 1.8 mm. The total protrusions preferably account for 10% to 40% of the area of ​​the convex point paper, more preferably 15% to 20%.

[0089] Further, the protrusions on the convex point paper are evenly distributed, but are not limited to horizontal and vertical distribution. The cross-sectional shape of the protrusions can be any shape, can be a triangle, square, circle, polygon, etc., or can be a combination of multiple shapes.

[0090] In some embodiments, the guide layer is a concave dot paper, and a plurality of pits are provided on the concave dot paper. The average depth of the pits is 0.5 mm to 2.5 mm, and the area occupied by a single pit is 1 mm.2 ~4mm 2 , all of the pits account for 5% to 60% of the area of ​​the pit paper.

[0091] In some of these implementations, see Figure 7 The guide layer is a convexo-convex paper, and the convexo-convex paper is provided with a plurality of protrusions and pits, the average height of the protrusions is 0.5mm~2.5mm, the average depth of the pits is 0.5mm~2.5mm, and the area occupied by a single protrusion or pit is 1mm 2 ~4mm 2 , all the protrusions and the pits account for 5% to 60% of the area of ​​the convex-concave paper.

[0092] In some embodiments, the guide layer is a rubber sheet with a plurality of protrusions on the surface, the average height of the protrusions is 0.5 mm to 2.5 mm, and the area occupied by a single protrusion is 1 to 5 mm. 2 The number of protrusions is 1 to 20 per cm 2 The guide layer is made of rubber, which has good flexibility, high strength and is easy to process; the protrusions not only play a supporting role but also facilitate gas circulation.

[0093] Furthermore, the average height of the protrusions is preferably 1.2 mm to 1.8 mm.

[0094] Furthermore, the total area of ​​all the protrusions accounts for 5% to 60% of the total area of ​​the rubber sheet, preferably 10% to 20%.

[0095] Furthermore, the protrusions on the surface of the undulating rubber sheet are solid.

[0096] Furthermore, the material of the rubber sheet with undulating surface is not limited to silicone, latex and natural rubber.

[0097] In some embodiments, the guide layer is a rubber sheet with a plurality of pits on the surface, the average depth of the pits is 0.5 mm to 2.5 mm, and the area occupied by a single pit is 1 to 4 mm. 2 , all of the pits account for 5 to 60% of the area of ​​the pit paper.

[0098] In some embodiments, the guide layer is a plastic sheet or a rubber sheet having the same structure as the aforementioned corrugated paper.

[0099] In some of the embodiments, the guide layer is a plastic sheet or a rubber sheet having the same structure as the aforementioned bump paper.

[0100] In some embodiments, the guide layer is a plastic sheet or a rubber sheet having the same structure as the aforementioned concave dot paper.

[0101] In some embodiments, the guide layer is a plastic sheet or a rubber sheet having the same structure as the aforementioned convexo-concave paper.

[0102] Furthermore, when the guide layer is made of plastic material, the guide layer is made of plastic molding, without winding molding, and is directly molded into a hollow device with a guide layer, and some round holes can be opened on the side wall of the hollow device. The wall thickness of the hollow device is 1.3mm~3mm, preferably 1.5mm~2.5mm, more preferably 1.5~2.0mm, and the diameter of the hollow cavity of the hollow device is 1.0mm~2.0mm.

[0103] In some embodiments, the guide layer carries a fragrance substance. The hollow channel of the hollow device forms a first air path, the guide layer of the hollow device has a guide channel, which increases the air passage and forms more air paths, and the fragrance substance is carried in the guide layer to improve the release efficiency of the fragrance substance; adding fragrance substances to the guide layer, the fragrance is rich, natural, coordinated, and released for a long time, and the front and back suctions are uniform and consistent, and a large amount of smoke aerosol is released, thereby achieving unexpected results in improving the sensory quality of the aerosol generating device.

[0104] In some embodiments, the guide layer further includes particulate matter, the aroma substance is loaded on the particulate matter to form a complex, and the complex is disposed on the guide layer.

[0105] In some embodiments, the composite is bonded to the surface of the guide layer.

[0106] For understanding, please refer to Fig.19 and Fig. 20 The particles 6 can be loaded on the surface of the guide layer 41 by bonding, and after being rolled into a hollow device, the particles 6 are filled in the gaps of the guide layer structure.

[0107] In some embodiments, the average particle size of the particles is 60-120 mesh (average particle diameter is 0.125-0.250 mm), preferably 80-100 mesh (average particle diameter is 0.150-0.180 mm).

[0108] As an example, the average particle size of the particulate matter can be 60 mesh, 65 mesh, 70 mesh, 75 mesh, 80 mesh, 85 mesh, 90 mesh, 95 mesh, 100 mesh, 105 mesh, 110 mesh, 115 mesh, 120 mesh, or within a range consisting of any two of the aforementioned values ​​as end values.

[0109] In some embodiments, the amount of particles added is 10 g / m 2 ~300g / m 2 .

[0110] As an example, the amount of particles added may be 10 g / m 2 , 20 g / m 2 , 30 g / m 2 , 40g / m 2 , 50 g / m 2 , 80g / m 2 , 100g / m 2 , 120 g / m 2 , 150g / m 2 , 180 g / m 2 , 200g / m 2 , 220 g / m 2 , 250g / m 2 , 280 g / m 2 and 300g / m 2 , or within the range of any two of the above values ​​as end values. Preferably 40 to 300 g / m 2 , more preferably 80~300g / m 2 , the most preferred range is 100~300g / m 2 .

[0111] In some embodiments, the particulate matter is one or more of diatomaceous earth, montmorillonite, sepiolite, kaolin, calcium oxide, calcium carbonate, calcium hydroxide, calcium sulfate, activated carbon, molecular sieve, tea stem particles, tangerine peel particles, orange peel particles, grapefruit peel particles, peanut shell particles and tangerine peel particles.

[0112] In some embodiments, the aroma substance is loaded on the guide layer at a mass ratio of 1% to 50%.

[0113] As an example, the load mass of the aroma substance in the guide layer can be 1%, 2%, 3%, 4%, 5%, 6%, 7%, 8%, 9%, 10%, 15%, 20%, 25%, 30%, 35%, 40%, 45%, 50%, or a range consisting of any two of the above values ​​as end values, preferably 2-40%, more preferably 3-30%, and most preferably 5-10%.

[0114] In some embodiments, the aroma substance is one or more of cocoa aroma, coffee aroma, nut aroma, milk aroma, tea aroma, cantaloupe aroma, cucumber aroma, orange aroma, grapefruit aroma, watermelon aroma, date aroma, clove, mint aroma and hay aroma.

[0115] In some embodiments, the hollow device includes a connected flavoring section and a non-flavoring section, the flavoring section is located between the aerosol matrix and the non-flavoring section, and the flavoring substance is loaded in the flavoring section. According to actual needs, the flavoring substance can be directly added to the guide layer material by methods such as spraying, coating or soaking during the preparation of the flavoring section, or the flavoring substance can be first loaded on the particulate matter, and then these flavoring particulate matter is filled or glued to the guide layer. Adding the particulate matter after flavoring in the flavoring section not only enhances the supporting effect of the hollow device, but also because the heating temperature of the hollow section is higher than the temperature of the filter section, it is more conducive to the release of the flavoring substance. In addition, compared with the addition of the flavoring substance in the heated cigarette aerosol matrix section, the release of the flavoring substance is difficult to coordinate due to the influence of various factors during heating, and the addition of the flavoring substance in the hollow section, the process of heat release is relatively simple, easy to control the release, and the cigarette aroma and taste are better.

[0116] In some embodiments, the axial length ratio of the fragrance section to the fragrance-free section is 1:5 to 5:1, preferably 2:3 to 3:2.

[0117] In some embodiments, the ratio of the wall thickness of the fragrance segment to the wall thickness of the non-scented segment is 1:0.5~1.

[0118] In some embodiments, the total length of the hollow device is 5 to 50 mm.

[0119] As an example, the total length of the hollow device can be 5 mm, 10 mm, 15 mm, 20 mm, 25 mm, 30 mm, 35 mm, 40 mm, 45 mm, 50 mm, or a range consisting of any two of the above values ​​as end values, preferably 5.0 to 40.0 mm, more preferably 10.0 to 30.0 mm.

[0120] In some embodiments, the hollow device is cylindrical and coaxially attached to the inner wall of the hollow section.

[0121] In a second aspect of the present application, there is provided a method for preparing the aerosol generating device as described in the first aspect, the method comprising the following steps:

[0122] 1) Wrapping the filter body and the hollow device connected in sequence with a wrapping material to form a whole, and wrapping the aerosol matrix with the wrapping material;

[0123] 2) Wrapping the filter body and the hollow device as a whole and the wrapped aerosol matrix part with a wrapping material to obtain the aerosol generating device. After wrapping to form a whole, the filter body constitutes the filter segment of the aerosol generating device, the hollow device constitutes the hollow segment, and the aerosol matrix constitutes the aerosol matrix segment.

[0124] The second aspect of the present application provides a method for preparing the aerosol generating device as described in the first aspect, the method comprising the steps of preparing the hollow device:

[0125] 1) Wrapping the guide layer with wrapping paper on the outside or both sides of the guide layer to form a hollow tubular device;

[0126] 2) Cutting the hollow tubular device into pieces to obtain the hollow device.

[0127] In some of these implementations, see Figure 8 The guide layer is made of corrugated paper, with the corrugations facing outward (the side away from the central axis of the hollow section is the outer side, and the side close to the central axis of the hollow section is the inner side). Then, a piece of wrapping paper, i.e., outer paper 7, is used on the outside of the corrugated paper. The corrugated paper is wound and rolled into a hollow device. Please refer to Figure 4 After the hollow device is wound, the corrugations of the corrugated paper form a spiral flow guide channel 411. After winding, the cross-sectional structure of the hollow device formed can be seen in FIG. Fig. 9 That is, the hollow device is formed by compounding thicker ordinary paper and corrugated paper.

[0128] In some of these implementations, see Fig.10 The guide layer is made of corrugated paper with the corrugations facing inwards. Then a piece of wrapping paper is used on the outside of the corrugated paper to wrap the corrugated paper to form a hollow device. After wrapping, the cross-sectional structure of the hollow device formed is shown in the figure. Fig.11 .

[0129] In some of these implementations, see Fig.12 The guide layer is made of corrugated paper with the corrugations facing outwards. Then, a piece of wrapping paper is used on both sides of the corrugated paper to wrap the corrugated paper to form a hollow device. After wrapping, the cross-sectional structure of the hollow device formed is shown in FIG. Fig.13 , the outer side is outer paper 7, and the inner side is inner paper 8.

[0130] In some of these implementations, see Fig.14 The guide layer is made of corrugated paper with the corrugations facing inwards. Then, a piece of wrapping paper is used on both sides of the corrugated paper to wrap the corrugated paper to form a hollow device. After wrapping, the cross-sectional structure of the hollow device formed is shown in FIG. Fig.15 .

[0131] In some embodiments, the guide layer is made of concave paper, convex paper, or concave-convex paper, and then a wrapping paper is used on the outside of the guide layer to wrap the guide layer to form a hollow device. The cross-sectional structure of the hollow device formed after the outer paper and the convex paper are wrapped is shown in FIG. Fig.16When the guide layer is made of rubber material, the preparation method of the hollow device is the same.

[0132] In some embodiments, the guide layer is made of concave paper, convex paper, or concave-convex paper, and then the guide layer is wound with a piece of wrapping paper on both sides of the guide layer to form a hollow device, wherein the cross-sectional structure of the hollow device formed after the outer paper, convex paper and inner paper are wound is shown in Figure 17, that is, the hollow device is a composite of thicker ordinary paper and convex paper. When the guide layer is made of rubber material, the preparation method of the hollow device is the same.

[0133] For further information, see Fig.18 The inner paper can be a hollow wrapping paper with a number of hollow notches 5 evenly distributed. These hollow notches 5 can be of any shape, such as triangle, square, circle, polygon, etc., or a combination of multiple shapes. The area of ​​a single hollow notch is 1~3mm 2 , the total area of ​​the hollow gap is 1~3 mm 2 .

[0134] In some embodiments, when the guide layer is made of plastic material, the guide layer is made of plastic molding. The guide layer is made of plastic material and can be directly molded into a hollow device with the guide layer without winding molding.

[0135] In some embodiments, the preparation of the hollow device further comprises at least one of the following preparation steps:

[0136] 1) Loading the aroma substance on the guide layer;

[0137] 2) The aroma substance is loaded on the particles, and then the particles are loaded on the guide layer.

[0138] In some embodiments, the aroma substance is loaded onto the guide layer and / or the particulate matter by spraying, coating or soaking.

[0139] In some embodiments, the particles are loaded on the surface of the guide layer having the concavo-convex structure by bonding.

[0140] In some of the embodiments, the hollow device adopts an integral breathable paper tube, the wall thickness of the hollow device is greater than the side wall thickness of the hollow section, the hollow device has good supporting strength, and is not easily squeezed by the heating device and significantly thinned.

[0141] In some of the embodiments, the hollow device is disposed in the hollow section by bonding.

[0142] In some of the embodiments, under the condition of satisfying the supporting strength, the hollow device can be based on a cylindrical shape with some hollowing out designs on the cylindrical surface; or holes can be opened inside the hollow device to form an air flow channel.

[0143] A third aspect of the present application provides an aerosol generating system, comprising the aerosol generating device and a heating device as described in the first aspect.

[0144] In some embodiments, the heating device includes a heating component, a battery component for powering the heating device, a control component for controlling the battery component, and a housing for accommodating the heating component, the battery component, and the control component.

[0145] In some embodiments, the heating length of the heating component in the hollow section is 0-100% of the length of the hollow section, and the heating position extends from the hollow section adjacent to the aerosol substrate to the hollow section adjacent to the filter section, preferably 10-90%, more preferably 20-80%, and most preferably 30-70%.

[0146] It can be understood that the aerosol generating device cooperates with the heated smoking device for heating, and the length of the hollow device and the heated smoking device cooperates with each other for heating is 0 to 100% of the length of the hollow section.

[0147] Specifically, when the central heating method is adopted, the heating section of the heating device only heats the aerosol matrix of the aerosol generating device, so the length of the hollow section that is heated in cooperation with the heating device is 0; when the peripheral heating method is adopted, the smoking device can be designed to heat or not heat the hollow section, so the length of the hollow section that is heated in cooperation with the heating device is 0%~100% of the length of the hollow section.

[0148] In some embodiments, the aerosol generating device includes a guide layer, and the guide layer also includes wrapping paper.

[0149] The present application adds a hollow device to the hollow part of the hollow section of the aerosol generating device, and adds fragrance to the hollow device, which greatly improves the sensory quality of the aerosol generating device, which is explained below in conjunction with specific embodiments and comparative examples.

[0150] Example 1

[0151] Spray the mint flavor substance on the corrugated paper at 0.03 mg / aerosol generating device, then compound the corrugated paper as a guide layer with ordinary paper to prepare a composite guide layer in which one side of the corrugated paper is compounded with ordinary paper; then cut the composite guide layer into appropriate widths, wrap and bond with ordinary paper to form a hollow tubular device, the composite guide layer is on the inner side of the hollow tubular device, and the hollow tubular device containing the composite guide layer is cut into appropriate lengths to obtain a hollow device, the corrugated paper layer constitutes the guide layer of the hollow device, and the concave part of the corrugated paper constitutes the guide channel of the smoke. Among them, the corrugation height of the corrugated paper is 2.0 mm, and the number of corrugations is 100 / 300 mm. The length of the prepared hollow device is 30 mm, the wall thickness of the hollow device is 2.1 mm, and the diameter of the hollow device is 6.7 mm.

[0152] The filter body and the hollow device connected in sequence are wrapped with wrapping paper to form a whole, and the aerosol matrix is ​​wrapped with the wrapping paper; then the whole formed by the filter body and the hollow device and the wrapped aerosol matrix are partially wrapped with the wrapping paper to obtain the aerosol generating device.

[0153] Example 2

[0154] The aerosol generating device prepared in Example 2 is basically the same as that in Example 1, except that the mint flavoring substance is sprayed on the corrugated paper at 0.05 mg / aerosol generating device, the corrugation height of the corrugated paper is 0.5 mm, and the number of corrugations is 200 / 300 mm.

[0155] Example 3

[0156] The aerosol generating device prepared in Example 3 is substantially the same as that in Example 1, except that 0.05 mg of blueberry flavoring material is sprayed onto the corrugated paper per aerosol generating device.

[0157] Example 4

[0158] The aerosol generating device prepared in Example 4 is basically the same as that in Example 1, the difference is that particulate matter is used for aroma, diatomaceous earth particles carrying coffee aroma and tea aroma substances are added into the gaps between the corrugated paper, the particle size of the diatomaceous earth particles is 60 mesh, and the amount of aroma substance added is 0.02 mg / aerosol generating device.

[0159] Example 5

[0160] The aerosol generating device prepared in Example 5 is basically the same as that in Example 1, except that particulate matter is used for fragrance, and activated carbon particles loaded with blueberry aroma substances are filled in the gaps between the corrugated paper, and the particle size of the activated carbon particles is 120 meshes.

[0161] Example 6

[0162] The aerosol generating device prepared in Example 6 is basically the same as that in Example 1, except that: the material of the guide layer is convex dot paper, and the blueberry flavor material is coated on the convex dot paper; the average height of the convex dot paper is 0.5 mm, and the area occupied by a single convex is 1 mm 2 , all protrusions account for 5% of the convex paper area.

[0163] Example 7

[0164] The aerosol generating device prepared in Example 7 is substantially the same as that in Example 1, except that the coffee aroma and tea aroma flavor substances are coated on the corrugated paper.

[0165] Example 8

[0166] The aerosol generating device prepared in Example 8 is basically the same as that in Example 1, except that the coffee and tea aroma substances are coated on the convex dot paper; the average height of the convex dot paper is 2.5 mm, and the area occupied by a single convex is 4 mm 2 , all the bumps account for 60% of the bump paper area.

[0167] Comparative Example 1

[0168] The aerosol generating device prepared in Comparative Example 1 is substantially the same as that in Example 1, except that the hollow device is omitted and the flavoring material is added to the filter segment.

[0169] Comparative Example 2

[0170] The aerosol generating device prepared in Comparative Example 2 is substantially the same as that in Example 1, except that the hollow device is omitted and the flavoring substance is added into the aerosol matrix.

[0171] Comparative Example 3

[0172] The aerosol generating device prepared in Comparative Example 3 is substantially the same as that in Example 2, except that the hollow device is omitted and the flavoring material is added to the filter segment.

[0173] Comparative Example 4

[0174] The aerosol generating device prepared in Comparative Example 4 is substantially the same as that in Example 2, except that the hollow device is omitted and the flavoring substance is added into the aerosol matrix.

[0175] Comparative Example 5

[0176] The aerosol generating device prepared in Comparative Example 5 is substantially the same as that in Example 3, except that the hollow device is omitted and the flavoring material is added to the filter segment.

[0177] Comparative Example 6

[0178] The aerosol generating device prepared in Comparative Example 6 is substantially the same as that in Example 3, except that the hollow device is omitted and the flavoring substance is added to the aerosol matrix segment.

[0179] Comparative Example 7

[0180] The aerosol generating device prepared in Comparative Example 7 is substantially the same as that in Example 4, except that the hollow device is omitted and the flavoring material is added to the filter segment.

[0181] Comparative Example 8

[0182] The aerosol generating device prepared in Comparative Example 8 is substantially the same as that in Example 4, except that the hollow device is omitted and the flavoring substance is added into the aerosol matrix.

[0183] Comparative Example 9

[0184] The aerosol generating device prepared in Comparative Example 9 is basically the same as that in Example 5, except that the hollow device is omitted, and particulate matter is used for fragrance, and the fragrance particles are added into the cavity of the hollow part of the hollow section.

[0185] Comparative Example 10

[0186] The aerosol generating device prepared in Comparative Example 10 is substantially the same as that in Example 5, except that the hollow device is omitted and the aroma substance is coated on the inner wall of the hollow section.

[0187] Comparative Example 11

[0188] The aerosol generating device prepared in Comparative Example 11 is basically the same as that in Example 7, except that the hollow device is omitted, and particulate matter is used for fragrance, and the fragrance particles are added into the cavity of the hollow part of the hollow section.

[0189] Comparative Example 12

[0190] The aerosol generating device prepared in Comparative Example 12 is substantially the same as that in Example 7, except that the hollow device is omitted and the aroma substance is coated on the inner wall of the hollow section.

[0191] An evaluation panel consisting of 7 experts in cigarette sensory quality evaluation conducted a sensory quality evaluation on the prepared aerosol generating device.

[0192] The aroma substances, the amount of aroma substances added, the positions where the aroma substances are added and the sensory quality evaluation results in the aerosol generating device preparation methods of Examples 1 to 4 and Comparative Examples 1 to 8 are shown in Table 1.

[0193] Table 1

[0194]

[0195] Among them, the first group uses central heating; the second to fourth groups use peripheral heating; the first to third groups add the aroma substances in the hollow device by directly adsorbing them on the corrugated paper through spraying. The fourth group adds the aroma particles in the gaps of the guide layer structure.

[0196] The aroma substances, aroma substance adding positions, sensory quality evaluation results and glycerol release amounts in the aerosol generating device preparation methods of Examples 5 to 8 and Comparative Examples 9 to 12 are shown in Table 2.

[0197] Table 2

[0198]

[0199] Among them, the detection conditions of glycerol release are: ambient heating method, the heating temperature setting value is 220℃; using a linear smoking machine for smoking, the smoking parameters are: smoking volume 55mL; smoking time 2s; smoking interval 30s; number of puffs 8; preheating time 18s; the smoking curve is bell-shaped.

[0200] From the results in Table 1, it can be seen that when flavoring substances are added to the filter, the aroma is lighter, the naturalness is better, and the aroma concentration in the first few puffs is smaller; when flavoring substances are added to the aerosol matrix, the aroma is strong, but the naturalness is not enough, and the front and back puffs are inconsistent; when flavoring substances are added to the hollow device, the aroma is strong, the naturalness is better, the aroma is coordinated, the release is long-lasting, and the front and back puffs are uniform and consistent.

[0201] From the results in Table 2, it can be seen that when flavoring material particles are added into the hollow cavity of the hollow section, the aroma release is uneven, the front and back inhalation is inconsistent, and the smoke aerosol release is significantly reduced; when flavoring material is coated on the inner wall of the hollow section, the aroma release is uneven, and the front and back inhalation is inconsistent; when flavoring material is added into the guide layer, the aroma is rich, the naturalness is good, the aroma is coordinated, the release is long-lasting, the front and back inhalation is uniform and consistent, and the smoke aerosol release is large.

[0202] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0203] The above embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for those of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be based on the attached claims, and the description and drawings may be used to interpret the contents of the claims.

Claims

1. An aerosol generating device, characterized in that: It comprises a filter section, a hollow section and an aerosol matrix section which are connected in sequence. The hollow section comprises a hollow device. The hollow device has a flow-guiding layer. The flow-guiding layer has a flow-guiding channel.

2. The aerosol generating device according to claim 1, characterized in that: The wall thickness of the hollow device is 0.6-2.7 mm.

3. The aerosol generating device according to claim 1, characterized in that: The guide layer is a hollow guide layer provided with the guide channel.

4. The aerosol generating device according to claim 1, characterized in that: The guide layer is rolled to form a hollow tubular structure.

5. The aerosol generating device according to claim 1, characterized in that: The hollow device further comprises a wrapping paper, and the wrapping paper is arranged on at least one of the inner wall and the outer wall of the hollow tubular structure formed by rolling the guide layer.

6. The aerosol generating device according to any one of claims 1 to 5, characterized in that: At least one surface of the guide layer has a concave-convex structure.

7. The aerosol generating device according to any one of claims 1 to 5, characterized in that: The guide layer is made of paper, rubber or plastic.

8. The aerosol generating device as claimed in claim 6, characterized in that The concave-convex structure includes at least one of a corrugated structure and a matrix concave-convex structure.

9. The aerosol generating device according to any one of claims 1 to 5, characterized in that: The guide layer is corrugated paper, the corrugation height of the corrugated paper is 0.5 mm to 2.5 mm, and in the extension direction of the corrugations in the corrugated paper, the number of corrugations per 300 mm length is 100 to 200.

10. The aerosol generating device according to any one of claims 1 to 5, characterized in that: The guide layer is a convex dot paper, and a plurality of convexities are arranged on the convex dot paper. The average height of the convexities is 0.5 mm to 2.5 mm, and the area occupied by a single convexity is 1 mm. 2 ~4mm 2 , all of the protrusions account for 5% to 60% of the area of ​​the convex point paper.

11. The aerosol generating device according to any one of claims 1 to 5, characterized in that: The guide layer is a convexo-concave paper, on which a plurality of protrusions and concave pits are arranged, the average height of the protrusions is 0.5 mm to 2.5 mm, the average depth of the concave pits is 0.5 mm to 2.5 mm, and the area occupied by a single protrusion or a single concave pit is 1 mm 2 ~4mm 2 , all the protrusions and the pits account for 5% to 60% of the area of ​​the convex-concave paper.

12. The aerosol generating device according to any one of claims 1 to 5, characterized in that: The guide layer carries aroma substances.

13. The aerosol generating device according to claim 12, characterized in that: The guide layer further comprises particles, the aroma substance is loaded on the particles to form a composite, and the composite is arranged on the guide layer.

14. The aerosol generating device according to claim 13, characterized in that: The composite is bonded to the surface of the guide layer.

15. The aerosol generating device according to claim 13, characterized in that: The average particle size of the particles is 60-120 meshes.

16. The aerosol generating device according to any one of claims 13 to 15, characterized in that: The amount of particles added is 10 g / m 2 ~300g / m 2 .

17. The aerosol generating device according to any one of claims 13 to 15, characterized in that: The particulate matter is one or more of diatomaceous earth, montmorillonite, sepiolite, kaolin, calcium oxide, calcium carbonate, calcium hydroxide, calcium sulfate, activated carbon, molecular sieve, tea stem particles, tangerine peel particles, orange peel particles, grapefruit peel particles, peanut shell particles and tangerine peel particles.

18. The aerosol generating device according to claim 12, characterized in that: The load mass of the aroma substance in the guide layer is 1% to 50%.

19. The aerosol generating device according to claim 12, characterized in that: The aroma substances are one or more of cocoa aroma, coffee aroma, nut aroma, milk aroma, tea aroma, cantaloupe aroma, cucumber aroma, orange aroma, grapefruit aroma, watermelon aroma, date aroma, clove aroma, mint aroma and hay aroma.

20. The aerosol generating device according to any one of claims 1 to 5, characterized in that: The hollow device comprises a fragrance section and a fragrance-free section connected to each other, wherein the fragrance section is located between the aerosol matrix and the fragrance-free section, and the fragrance section is loaded with fragrance substances.

21. The aerosol generating device according to claim 20, characterized in that The axial length ratio of the fragrance section to the fragrance-free section is 1:5 to 5:

1.

22. The aerosol generating device according to claim 20, characterized in that: The ratio of the wall thickness of the fragrance section to the wall thickness of the fragrance-free section is 1:0.5~1.

23. The aerosol generating device according to any one of claims 1 to 5, characterized in that: The total length of the hollow device is 5-50 mm.

24. The aerosol generating device according to any one of claims 1 to 5, characterized in that: The hollow device is cylindrical and coaxially attached to the inner wall of the hollow section.

25. A method for preparing an aerosol generating device as claimed in any one of claims 1 to 24, characterized in that: The preparation method comprises the steps of preparing the hollow device: 1) Wrapping the guide layer with wrapping paper on the outside or both sides of the guide layer to form a hollow tubular device; 2) Cutting the hollow tubular device into pieces to obtain the hollow device.

26. The method for preparing an aerosol generating device according to claim 25, characterized in that: The preparation of the hollow device further comprises at least one of the following preparation steps: 1) Loading the aroma substance on the guide layer; 2) Loading the aroma substance on the particles, and then loading the particles on the guide layer.

27. The method for preparing an aerosol generating device according to claim 26, characterized in that: The aroma substance is loaded onto the guide layer and / or the particles by spraying, coating or soaking.

28. An aerosol generating system, characterized in that: The invention comprises an aerosol generating device and a heating device as described in any one of claims 1 to 24.

29. The aerosol generating system of claim 28, wherein: The heating device comprises a heating component, a battery component for supplying power to the heating device, a control component for controlling the battery component, and a housing for accommodating the heating component, the battery component and the control component.

30. The aerosol generating system of claim 29, wherein: The heating length of the heating component in the hollow section is 0-100% of the length of the hollow section, and the heating position extends from the adjacent portion of the hollow section and the aerosol matrix to the adjacent portion of the hollow section and the filter section.

Citation Information

Patent Citations

  • Heating non-combustion cigarette

    CN109998160A

  • Fragrance slow-release cooling unit and heating type aerosol generating product comprising fragrance slow-release cooling unit

    CN111150111A

  • Limiting element for heating cigarette and preparation method of limiting element

    CN113925199A

  • Aerosol generating product with perfumed supporting section

    CN115363235A