Oil-based drilling fluid flocculant and preparation method thereof
The flocculant is prepared through the polymerization reaction of stearyl acrylate, divinylbenzene and cetyldimethylallylammonium chloride, which solves the problem of removing micro-nano cuttings from oil-based drilling fluids and significantly improves the solid-phase particle size and drilling fluid performance, reducing waste volume and costs.
Patent Information
- Application Number
- CN202411053726.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-02
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-08-02
AI Technical Summary
Existing technologies have limited effectiveness in reducing the content of micro-nano cuttings in oil-based drilling fluids, leading to problems such as increased drilling fluid viscosity, deterioration of lubricity, and wellbore instability, and traditional solids control equipment is ineffective at removing small-sized cuttings. Not good.
The flocculant is prepared through polymerization reaction using monomers such as stearyl acrylate, divinylbenzene and cetyldimethylallylammonium chloride. It is initiated and condensed by the initiator to obtain strong adsorption and good dispersion. Flocculant for oil-based drilling fluids.
This flocculant can effectively adsorb and aggregate micro-nano cuttings in oil-based drilling fluids, significantly increase the solid particle size, improve the rheological properties of the drilling fluid, reduce the amount of waste, reduce the cost of the drilling fluid, and improve the stability of the well wall.
Smart Images

Figure CN118755014A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of flocculants, and in particular to an oil-based drilling fluid flocculant and a preparation method thereof. Background Art
[0002] In recent years, my country's oil and gas resource exploration technology has been continuously developing towards deep formations, and the formation conditions encountered during drilling have become increasingly complex, and water-based drilling fluids cannot meet the corresponding mining needs. Oil-based drilling fluids have better wellbore stability, inhibition, lubricity, temperature resistance and pollution resistance than water-based drilling fluids, and are the first choice for difficult wells such as unconventional oil and gas wells, complex structure wells, deep and ultra-deep water wells, high-temperature and high-pressure deep wells, and ultra-deep wells.
[0003] Due to the high cost of oil-based drilling fluids and other factors, oil-based drilling fluids are usually recycled. However, long-term drilling operations will increase the content of cuttings in the drilling fluid, thereby increasing the viscosity of the drilling fluid, which will lead to problems such as slow drilling time, excessive drilling pressure, deterioration of lubricity, and increased filtration loss. In severe cases, it will cause wellbore instability accidents. At present, the main method to reduce the content of cuttings in oil-based drilling fluids is through solid control equipment. However, this method can only remove cuttings with larger particle sizes and has little effect on micro-nano cuttings. Flocculants can aggregate and enlarge micro-nano cuttings to meet the particle size requirements of solid control equipment and thus remove them.
[0004] For example, the publication number CN109652026A discloses a "method for preparing a flocculant flow type regulator for oil-based drilling fluid", which includes the following steps: (1) adding nano activated carbon to a beaker equipped with a stirrer and a thermometer; (2) adding a low-viscosity synthetic base oil to the reactor of step (1) and stirring at 50°C to 90°C for 3 to 6 hours; (3) adding an emulsifier to the reactor of step (1) and stirring for 3 to 6 hours; (4) adding a wetting agent to the reactor of step (1) and stirring for 3 to 5 hours, and the obtained suspension is a flocculant flow type regulator for oil-based drilling fluid. This method can reduce the content of finely dispersed particles in oil-based drilling fluid, but the flocculation effect is general.
[0005] For example, the publication number CN113292731A discloses a "method for preparing a flocculant for removing rock cuttings from oil-based drilling fluids", which includes the following steps: (1) a hydrophilic monomer, a cationic monomer and glycidyl methacrylate are subjected to a first polymerization reaction in the presence of a first solvent and a first initiator to obtain a prepolymer A; (2) an oil-soluble monomer, acrylamide and 2-mercaptoethylamine hydrochloride are subjected to a second polymerization reaction in the presence of a dispersant, a second solvent and a second initiator to obtain a prepolymer B; (3) prepolymers A and B are subjected to a graft polymerization reaction to obtain a flocculant. This method has a cumbersome synthesis process and a relatively limited flocculation effect. Summary of the invention
[0006] Aiming at the problems existing in the prior art, the present invention provides an oil-based drilling fluid flocculant and a preparation method thereof.
[0007] The technical solution adopted by the present invention is:
[0008] A method for preparing an oil-based drilling fluid flocculant comprises the following steps:
[0009] Step 1: Add divinylbenzene and hexadecyl dimethyl allyl ammonium chloride to the octadecyl acrylate solution and mix thoroughly;
[0010] Step 2: Add initiator, condense and reflux under protective atmosphere, stir and react; after the reaction is completed, filter and dry to obtain flocculant;
[0011] The molar ratio of octadecyl acrylate, divinylbenzene and hexadecyl dimethyl allyl ammonium chloride is 15-60:5-20:5-20.
[0012] Furthermore, the cationic monomer is one of hexadecyldimethylallyl ammonium chloride, dimethylallyldipropyl ammonium chloride and methacryloyloxyethyltrimethylammonium chloride.
[0013] Furthermore, the initiator is any one of potassium persulfate, ammonium persulfate, azobisisobutyl cyanide, potassium persulfate and sodium sulfite, ammonium persulfate and sodium bisulfite; wherein potassium persulfate and sodium sulfite are mixed in any proportion, and ammonium persulfate and sodium bisulfite are mixed in any proportion.
[0014] Furthermore, the mass ratio of the initiator to the monomer is 0.5 to 3:100, and the mass of the monomer is the total amount of octadecyl acrylate, divinylbenzene, and hexadecyl dimethyl allyl ammonium chloride.
[0015] Furthermore, in the step 1, the solvent of the octadecyl acrylate solution is anhydrous ethanol, and the octadecyl acrylate and the anhydrous ethanol are ultrasonicated for 20 minutes to fully dissolve them.
[0016] Furthermore, after the initiator is added in step 2, argon is passed for 30 minutes, the temperature is raised to 50-65° C., and condensed and refluxed.
[0017] Furthermore, in step 2, the stirring speed is 300 to 800 rpm, and the stirring reaction is performed for 4 to 12 hours.
[0018] Furthermore, in step 2, anhydrous ethanol is used for washing three times, and then dried at 60° C. for 12 hours.
[0019] The invention discloses an oil-based drilling fluid flocculant, which is obtained by polymerization reaction of octadecyl acrylate, divinylbenzene and hexadecyl dimethyl allyl ammonium chloride under the initiation of an initiator.
[0020] Furthermore, the structure of the flocculant is as follows:
[0021]
[0022] Wherein, n, p and q are natural numbers.
[0023] The beneficial effects of the present invention are:
[0024] (1) The preparation method of the present invention is simple to operate, has little pollution, is relatively environmentally friendly, and has low requirements on production equipment;
[0025] (2) The main chain atoms of the flocculant obtained by the present invention are soluble in oil and have good dispersibility, so that it has a good flocculation effect in the drilling fluid;
[0026] (3) The quaternary ammonium group in the flocculant obtained by the present invention has a strong adsorption capacity and can adsorb the rock cuttings dispersed in the oil-based drilling fluid, and at the same time provide conditions for the flocculant to selectively flocculate. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 It is a schematic diagram of the reaction flow of the present invention.
[0028] Figure 2 This is the infrared spectrum of the flocculant obtained in Example 1 of the present invention. DETAILED DESCRIPTION
[0029] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments.
[0030] Process such as Figure 1 As shown, a method for preparing an oil-based drilling fluid flocculant comprises the following steps:
[0031] Step 1: Add divinylbenzene and a cationic monomer to the octadecyl acrylate solution and mix thoroughly; the cationic monomer is one of hexadecyl dimethyl allyl ammonium chloride, dimethyl allyl dipropyl ammonium chloride and methacryloyloxyethyl trimethyl ammonium chloride.
[0032] First, octadecyl acrylate was placed in a beaker and anhydrous ethanol was added, and the solution was fully dissolved by ultrasonication for 20 minutes to obtain an octadecyl acrylate solution; the optimal mass ratio of octadecyl acrylate to anhydrous ethanol was 16:120. Divinylbenzene and cationic monomer were added to the octadecyl acrylate solution, and the solution was fully stirred and then transferred to a three-necked flask.
[0033] The molar ratio of octadecyl acrylate, divinylbenzene and cationic monomer is 15-60:5-20:5-20.
[0034] Step 2: Add initiator, pass argon for 30 minutes, heat to 50-65°C, condense and reflux with high-speed stirring for 4-12 hours, and the stirring speed is 300-800 rpm.
[0035] The initiator is one of potassium persulfate, ammonium persulfate, azobisisobutyl cyanide, potassium persulfate and sodium sulfite, ammonium persulfate and sodium bisulfite, wherein the total mass ratio of the monomer to the mass of the initiator is 100:0.5-3.
[0036] After the reaction is completed, the product in the three-necked flask is vacuum filtered for excess liquid, the filtered white solid is repeatedly washed 3 times with ethanol, and placed in a vacuum oven for drying at 60°C for 12 hours. The drying requires that the ethanol content in the flocculant is less than 5% to obtain a flocculant.
[0037] Example 1
[0038] A method for preparing an oil-based drilling fluid flocculant comprises the following steps:
[0039] Step 1: put 16.7g of octadecyl acrylate into a beaker, add 120g of anhydrous ethanol, and sonicate for 20 minutes to fully dissolve it to obtain an octadecyl acrylate solution;
[0040] 2.8 g of divinylbenzene and 10.3 g of hexadecyldimethylallylammonium chloride were added to the octadecyl acrylate solution, and the mixture was fully stirred and then transferred to a three-necked flask.
[0041] Step 2: Add 0.45g of azobisisobutyronitrile as an oil-soluble initiator at 25°C, pass argon for 30 minutes to remove oxygen in the system, and heat to 65°C in a water bath. React for 12 hours under stirring at 300rpm, and vacuum filter to obtain a white oil-based drilling fluid flocculant; the flocculant is repeatedly washed with ethanol three times, and placed in a vacuum oven at 60°C for 12 hours. The drying requires that the ethanol content in the flocculant is less than 5%, and the flocculant is obtained.
[0042] Figure 2 The infrared spectrum of the flocculant obtained in this example shows that the copolymer has a SDCD structure. -1 and 2851cm -1 The stretching vibration peaks of -CH3 and -CH2 are 1731cm -1 The characteristic peak of carbonyl C=O is 1467cm -1 The characteristic peak of disubstituted benzene ring is 1377cm -1 The characteristic absorption peak of -CH2 connected to nitrogen cation is 1269cm -1 The peak of COC contraction vibration is 700-1000cm -1There is no strong absorption peak between the two, indicating that the double bonds are basically polymerized. Therefore, the flocculant obtained in this embodiment is Figure 1 The structure shown.
[0043] Example 2
[0044] A method for preparing an oil-based drilling fluid flocculant comprises the following steps:
[0045] Step 1: put 16.7g of octadecyl acrylate into a beaker, add 120g of anhydrous ethanol, and sonicate for 20 minutes to fully dissolve it to obtain an octadecyl acrylate solution;
[0046] 2.8 g of divinylbenzene and 10.3 g of dimethylallyldipropylammonium chloride were added to the octadecyl acrylate solution, and the mixture was fully stirred and then transferred to a three-necked flask.
[0047] Step 2: Add 0.45g of azobisisobutyronitrile as an oil-soluble initiator at 25°C, pass argon for 30 minutes to remove oxygen in the system, and heat to 65°C in a water bath. React for 6 hours under stirring at 600rpm, and vacuum filter to obtain a white oil-based drilling fluid flocculant; the flocculant is repeatedly washed three times with ethanol, and placed in a vacuum oven at 60°C for 12 hours. The drying requires that the ethanol content in the flocculant is less than 5%, and the flocculant is obtained.
[0048] Example 3
[0049] A method for preparing an oil-based drilling fluid flocculant comprises the following steps:
[0050] Step 1: put 16.7g of octadecyl acrylate into a beaker, add 120g of anhydrous ethanol, and sonicate for 20 minutes to fully dissolve it to obtain an octadecyl acrylate solution;
[0051] 2.8 g of divinylbenzene and 10.3 g of methacryloyloxyethyltrimethylammonium chloride were added to the octadecyl acrylate solution, and the mixture was fully stirred and then transferred to a three-necked flask.
[0052] Step 2: Add 0.45g of azobisisobutyronitrile as an oil-soluble initiator at 25°C, pass argon for 30 minutes to remove oxygen in the system, and heat to 65°C in a water bath. React for 4 hours under stirring at 800rpm, and vacuum filter to obtain a white oil-based drilling fluid flocculant; the flocculant is repeatedly washed with ethanol three times, and placed in a vacuum oven at 60°C for 12 hours. The drying requires that the ethanol content in the flocculant is less than 5%, and the flocculant is obtained.
[0053] Example 4
[0054] The preparation method of this embodiment is the same as that of embodiment 1, except that the mass of hexadecyl dimethyl allyl ammonium chloride is 20 g.
[0055] Example 5
[0056] The preparation method of this embodiment is the same as that of embodiment 1, except that the temperature in step 2 is 50°C.
[0057] Example 6
[0058] The preparation method of this embodiment is the same as that of embodiment 1, except that the mass of divinylbenzene is 8.93 g.
[0059] Example 7
[0060] The preparation method of this embodiment is the same as that of embodiment 1, except that the mass of divinylbenzene is 0.56 g.
[0061] Comparative Example 1
[0062] The preparation method of this embodiment is the same as that of embodiment 1, except that octadecyl acrylate is replaced by methyl methacrylate.
[0063] Comparative Example 2
[0064] The preparation method of this embodiment is the same as that of embodiment 1, except that hexadecyl dimethyl allyl ammonium chloride is not added.
[0065] The flocculants prepared in Examples 1 to 5 and Comparative Examples 1 to 2 were used to treat oil-based drilling fluids to evaluate the performance of the flocculants.
[0066] The plastic viscosity (mPa·s), shear force (Pa), and initial and final shear force (Pa) of the drilling fluid were measured using a six-speed viscometer according to the method specified in GB / T16783.2-2012.
[0067] The median solid particle size of the drilling fluid was tested using Zeta PALS190Plus (Brookhaven, USA).
[0068] The density of the drilling fluid, the low-density solid content and the barite solid content in the drilling fluid are measured according to the method specified in GB / T16783.2-2012. Unless otherwise specified, the low-density solid content and the barite solid content refer to the volume content.
[0069] The manufacturer of the six-speed viscometer is Qingdao Tongchun Petroleum Instrument Co., Ltd., and the model is ZNN-D6B;
[0070] The manufacturer of the low-speed mixer is Qingdao Tongchun Petroleum Instrument Co., Ltd., model D90;
[0071] Preparation of spent drilling fluid samples:
[0072] Add 315mL 5# white oil to the slurry cup, add 2% organic soil, 3% primary emulsifier, 0.5% auxiliary emulsifier, 35mL brine (25% CaCl2) in sequence under continuous stirring, and stir at 12000r / min for 20min. Then add 3% CaO, 1% wetting agent, appropriate amount of barite in sequence, stir at 12000r / min for 40min, add cuttings (kaolin) to the base slurry and continue to stir at high speed for 20min, and heat at 150℃ for 16h. The density of the oil-based drilling fluid is 1.5g / cm 3 , the rock fragments content is 10% and the barite content is 28%.
[0073] The flocculated solid phase components and density test methods after adding flocculants to the drilling fluid are as follows:
[0074] The waste oil-based drilling fluid was poured into an enamel cup and stirred at a low speed while adding the obtained organic drilling fluid flocculant. The mixture was stirred at a low speed for 20 minutes to fully disperse the mixture, and then allowed to stand for 15 minutes. The mixture was then poured into a 200-mesh screen and the vibrating screen was turned on to remove the solid phase in the waste drilling fluid. The solid phase on the screen surface was washed at 120°C for 24 hours using a Soxhlet extractor with cyclohexane as the solvent, and then dried at 80°C to obtain a flocculated solid phase. The test results are shown in Table 1.
[0075] Table 1. Density and solid content of waste oil-based drilling fluid after flocculation and screening
[0076]
[0077]
[0078] It can be seen from Table 1 that after adding flocculants to the waste oil-based drilling fluid samples for treatment, the content of inferior solid phase in the obtained flocculated solid phase is higher than 50wt.%. It can be seen that the flocculant provided by the present invention has a good effect of selectively flocculating inferior solid phases in oil-based drilling fluids, and the flocculation effect on barite is relatively weak, so that the oil-based drilling fluid after flocculation treatment can maintain good performance.
[0079] In Examples 1 to 5 of the present invention, it is still possible to detect that the flocculated solid phase contains more than 10 wt.% of barite. This is because during the screening process of the flocculated drilling fluid, the drilling fluid is inevitably adsorbed on the surface of the flocculated solid phase. After washing with cyclohexane, the solid phase (including barite) in the adsorbed drilling fluid remains in the flocculated solid phase.
[0080] The flocculant obtained in Comparative Example 1 has poor solubility in waste oil-based drilling fluid due to the short hydrocarbon carbon chain of methyl methacrylate. After being added into the system, it interacts with the water phase in the system, and the viscosity increases significantly, so that the waste oil-based drilling fluid cannot be sieved. Therefore, the oil-based drilling fluid flocculant cannot achieve the recycling of waste oil-based drilling fluid.
[0081] The flocculant obtained in Comparative Example 2 does not use hexadecyl dimethyl allyl ammonium chloride, and the synthesized product has no cations, which greatly weakens the adsorption effect on rock debris, so the content of rock debris in the solid phase after screening is relatively small. In addition, the flocculation effect on barite is also weak. The flocculant obtained in Comparative Example 2 has basically no flocculation effect, and the recovered treatment liquid cannot meet the use standards in terms of density and solid content.
[0082] The flocculants obtained in Examples 1 to 5 of the present invention were used to evaluate the slurry matching performance of the recovered liquid phase after flocculation and screening of waste oil-based drilling fluid.
[0083] 2.5 wt % of the flocculants prepared in Examples 1 to 5 of the present invention and Comparative Examples 1 to 2 were added to 300 mL of an oil-based drilling fluid sample (as a base slurry), and stirred at 100 r / min for 20 min using a low-speed stirrer to flocculate the oil-based drilling fluid sample. The sample was allowed to stand for 15 min and was sieved with a 200-mesh screen to obtain a flocculated drilling fluid. The rheological parameters (apparent viscosity, plastic viscosity, dynamic shear force) of the treated drilling fluid, as well as the median solid phase particle size after adding the flocculant, are shown in Table 2.
[0084] Table 2. Evaluation of drilling fluid performance after flocculation and screening of waste oil-based drilling fluid
[0085]
[0086]
[0087] It can be seen from the table that after the flocculant obtained by the present invention is added to the waste oil-based drilling fluid sample for treatment, the median solid phase particle size of the drilling fluid is greatly increased from 10μm to more than 60μm. Among them, the median solid phase particle size of the drilling fluid after flocculation treatment in Examples 1, 4, and 5 is increased to more than 80μm. As can be seen from Table 2, the flocculant provided by the present invention has a significant flocculation effect on micro-nano-level fine rock cuttings in the waste oil-based drilling fluid sample, and can significantly increase the median solid phase particle size of the drilling fluid. The hydrocarbon carbon chain of methyl methacrylate used in the comparative example is relatively short, and its solubility in the waste oil-based drilling fluid is relatively poor. It cannot produce flocculation with rock cuttings in the system, but because it will combine with water to make the system viscous and make some rock cuttings aggregate together, the median particle size is slightly larger than the sample slurry. In Comparative Example 2, since hexadecyl dimethyl allyl ammonium chloride was not added, there was no flocculation effect on the rock cuttings, so the median particle size was very close to the sample.
[0088] In terms of drilling fluid rheology, after adding the flocculant provided by the present invention to the waste oil-based drilling fluid sample for flocculation treatment, the flocculated solid phase is removed, and the apparent viscosity, plastic viscosity, and dynamic shear force in Examples 1 to 5 are all reduced, and the performance of the waste oil-based drilling fluid after treatment is significantly improved. After the oil-based drilling fluid flocculant prepared by the present invention is recycled and treated, the amount of oil-based waste can be significantly reduced, and the preparation cost of the oil-based drilling fluid can be reduced by recycling the waste oil-based drilling fluid, which is conducive to the large-scale and efficient application of oil-based drilling fluid technology.
Claims
1. A method for preparing an oil-based drilling fluid flocculant, characterized in that: The following steps are involved: Step 1: Add divinylbenzene and cationic monomer to the octadecyl acrylate solution and mix thoroughly; Step 2: Add initiator, condense and reflux under protective atmosphere, stir and react; after the reaction is completed, filter and dry to obtain flocculant; The molar ratio of octadecyl acrylate, divinylbenzene and cationic monomer is 15-60:5-20:5-20.
2. The method for preparing an oil-based drilling fluid flocculant according to claim 1, characterized in that: The cationic monomer is one of hexadecyldimethylallyl ammonium chloride, dimethylallyldipropyl ammonium chloride and methacryloyloxyethyltrimethylammonium chloride.
3. The method for preparing an oil-based drilling fluid flocculant according to claim 1, characterized in that: The initiator is any one of potassium persulfate, ammonium persulfate, azobis(isobutyl cyanide), potassium persulfate and sodium sulfite, ammonium persulfate and sodium bisulfite; wherein potassium persulfate and sodium sulfite are mixed in any proportion, and ammonium persulfate and sodium bisulfite are mixed in any proportion.
4. The method for preparing an oil-based drilling fluid flocculant according to claim 1, characterized in that: The mass ratio of the initiator to the monomer is 0.5-3:100, and the mass of the monomer is the total amount of octadecyl acrylate, divinylbenzene and hexadecyl dimethyl allyl ammonium chloride.
5. The method for preparing an oil-based drilling fluid flocculant according to claim 1, characterized in that: In the step 1, the solvent of the octadecyl acrylate solution is anhydrous ethanol, and the octadecyl acrylate and the anhydrous ethanol are ultrasonicated for 20 minutes to fully dissolve them.
6. The method for preparing an oil-based drilling fluid flocculant according to claim 1, characterized in that: After the initiator is added in step 2, argon is passed for 30 minutes, the temperature is raised to 50-65° C., and condensed and refluxed.
7. The method for preparing an oil-based drilling fluid flocculant according to claim 1, characterized in that: In step 2, the stirring speed is 300-800 rpm, and the stirring reaction is carried out for 4-12 hours.
8. The method for preparing an oil-based drilling fluid flocculant according to claim 1, characterized in that: In the step 2, the mixture is washed with anhydrous ethanol for 3 times and then dried at 60° C. for 12 hours.
9. The oil-based drilling fluid flocculant obtained by the preparation method according to any one of claims 1 to 8, characterized in that: The oil-based drilling fluid flocculant is obtained by polymerization reaction of octadecyl acrylate, divinylbenzene and hexadecyl dimethyl allyl ammonium chloride under the initiation of an initiator.
10. The oil-based drilling fluid flocculant according to claim 9, characterized in that: The structure of the flocculant is as follows: Wherein, n, p and q are natural numbers.
Citation Information
Patent Citations
Hydrophobic group-containing cationic terpolymer and preparation method and application thereof
CN101613435A
High-temperature-resistant cationic polyacrylamide inhibitor, and preparation method and application thereof
CN106967196A
High-wax thickened oil cross-linked polymer nanometer material pour point depressant and preparation method thereof
CN106986966A
Water dispersible polymer and application thereof
CN107964071A
High-temperature-resistant high-density reversible water-in-oil / oil-in-water drilling fluid and preparation method thereof
CN109097010A