Damp-proof combined system of brick-concrete structure ancient building wall and construction method of damp-proof combined system
By setting up ground and underground moisture-proof structures on the walls of ancient buildings, and using self-compacting glue and splicing boards to achieve waterproofing, the problem of damage caused by moisture return in the existing technology has been solved, long-term waterproofing effects and construction convenience have been achieved, and the needs of ancient buildings have been met. Building restoration requirements.
Patent Information
- Application Number
- CN202411153925.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-10-11
AI Technical Summary
Existing technologies often lead to physical or chemical damage when preventing moisture in the walls of ancient brick-concrete buildings. It is difficult to effectively prevent biological erosion, salt crystallization, chemical erosion and freezing damage in the long term. Moreover, the construction process is complex and the environment is polluted, which cannot satisfy the needs of ancient buildings. Requirements to keep things as they were before.
The ground and underground moisture-proof structures are set up around the wall, including the water distribution part and drainage ditch on the top slope, as well as the concrete layer surrounding the underground part of the wall. The self-compacting glue and splicing plates are used to achieve sealing to ensure that groundwater does not penetrate and prevent Return of tide.
It can effectively prevent underground water erosion, slow down material deterioration and structural damage, maintain building stability and cultural attributes, is convenient to construct, low-cost, environmentally friendly, and meets the requirements for the restoration of ancient buildings.
Smart Images

Figure CN118756756A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of ancient building protection construction, and in particular relates to a moisture-proof combined system for an ancient building wall with a brick-concrete structure and a construction method thereof. Background Art
[0002] Brick wall architectural relics account for a large proportion of the historical architectural relics left in my country. They are non-renewable cultural resources with immeasurable cultural and social values. The existing measures to prevent moisture from returning to the walls of brick-concrete structures mainly adopt physical repair or the setting of physical or chemical barriers, such as the plastering repair method, which has a good initial effect, but the plastering material may crack due to the dry-wet cycle of groundwater and salt crystallization, so the durability of the plastering repair layer is poor; another example is to set up a physical barrier on the wall: such as replacing bricks and adding a waterproof layer, so that the brick wall can restore its moisture-proof function, but it cannot avoid damaging the walls of the original building, making it lose its ancient building attributes, and at the same time, the construction disturbance of the wall will destroy the integrity of the brick wall and cause the wall stability to deteriorate; another example is drilling holes in the wall and injecting waterproofing agents, the overall process is relatively complicated and cannot be applied to thicker brick wall structures, because the waterproofing agent cannot completely penetrate into the interior, resulting in poor chemical waterproofing effect, and improper handling of chemical waterproofing agents will cause environmental pollution. The corresponding anti-moisture measures of the existing technology have relatively positive feedback effects within a certain period of time, but various problems will still arise in the long run. At the same time, the immediate condition of the wall will be changed, making it difficult to achieve the technological requirements of restoring the ancient buildings to their original state. Summary of the invention
[0003] In view of the deficiencies in the prior art, the purpose of the present invention is to provide a moisture-proof combined system for the wall of an ancient building with a brick-concrete structure and a construction method thereof. The present invention adopts a moisture-proof structure to surround the wall without causing physical and chemical damage to the wall, effectively preventing the intrusion of groundwater on the wall, preventing biological erosion, salt crystallization, chemical erosion, clay stone expansion, frost damage, etc. caused by moisture return, and slowing down the problem of material degradation and even structural damage.
[0004] To achieve the above object, the present invention provides the following technical solutions: A moisture-proof composite system for the wall of an ancient building with a brick-concrete structure, the system comprising a ground moisture-proof structure arranged around the ground part of the outer wall of the wall and an underground moisture-proof structure arranged around the underground part of the outer wall of the wall; The ground moisture-proof structure includes a water-spreading part with a slope on the top surface, wherein the higher end of the water-spreading part is arranged close to the corresponding side of the wall ground, and the lower end transitions to a drainage ditch arranged away from the wall; The underground moisture-proof structure includes an enclosure mechanism located directly below the ground moisture-proof structure and a concrete layer poured on the inner and outer side walls of the enclosure mechanism and connected to the ground moisture-proof structure. The enclosure mechanism surrounds the underground part of the wall.
[0005] Preferably, the water dispersion part and the drainage ditch are both concrete structures, and the bottom surface of the drainage ditch has a slope for guiding water to flow toward the municipal underground pipe network.
[0006] Preferably, a water guide hole with its bottom facing the inside of the drainage ditch and its top below the ground is opened on the side of the drainage ditch away from the wall, and an anti-blocking component is provided at the top of the water guide hole. The anti-blocking component can be made of geotextile to prevent soil from blocking the water guide hole.
[0007] Preferably, the top surface of the drainage ditch on the side away from the wall is at least not higher than the ground height. This design is intended to allow surface water caused by heavy rainfall that fills the soil and produces flow to quickly enter the drainage ditch, preventing excessive surface water head from causing groundwater away from the wall to seep into the wall foundation, thereby causing the wall to dampen.
[0008] Preferably, the enclosure mechanism includes a plurality of splicing plates that are plugged into each other, and the plate bodies at both ends in the length direction of the splicing plates include an insertion portion and a plug-in edge that is in a free state in a non-plug-in state, and the insertion portion is an arc-shaped cylindrical structure with an axis extending along the width direction of the splicing plate, and the two ends of the insertion portion are integrally transitionally connected with the plate body and the plug-in edge.
[0009] Preferably, the inlet of the insertion portion is gap-matched with the plug-in edge of the adjacent splicing plate.
[0010] Preferably, the insertion portions and the insertion edges of adjacent splicing plates in the mating state are mated with each other.
[0011] Preferably, the inserting portion is filled with a self-compacting adhesive or a bagged container for containing the self-compacting adhesive.
[0012] Preferably, when the insertion portions and the insertion edges of adjacent splicing plates are in a mating state, the two splicing plates are in a vertical or parallel state.
[0013] The construction method of the above-mentioned brick-concrete structure ancient building wall moisture-proof combination system comprises the following steps: 1) An initial foundation pit is excavated at 0.5m~1m along the periphery of the wall for the later preparation of the water dispersion part and the drainage ditch, and then a secondary foundation pit with a width of 0.1~0.15m is excavated directly below the designed position of the side wall foundation on the side of the drainage ditch close to the wall for burying the enclosure mechanism; 2) The sealing bag containing liquid self-compacting glue is completely filled with the insertion part of the splicing plate to be plugged in, and then the splicing plates are vertically inserted into the secondary foundation pit in sequence to complete the mutual plugging of the insertion parts and the plugging edges of the adjacent splicing plates. At the same time, the plugging edge punctures the sealing bag of the corresponding insertion part to complete the filling of the gap between the insertion part and the plugging edge with the self-compacting glue, and then the sealing bag is pulled out; 3) After the self-compacting adhesive is completely cured, pour concrete into the remaining space of the secondary foundation pit to complete the secondary foundation pit landfill; 4) Pour concrete in the initial foundation pit and reserve a water guide hole forming mold to wait for the drainage ditch to be formed. After the drainage ditch is formed, level the ground between the drainage ditch and the wall and compact it, then lay the reinforced concrete layer to form the water dispersion part.
[0014] Compared with the prior art, the present invention has the following advantages: 1) The present invention simultaneously establishes moisture-proof and waterproof barriers in both the surface and underground directions around the outer periphery of the wall. The surface water dispersion part can quickly divert rainwater, surface water, etc. to the drainage ditch by using the slope guidance. At the same time, the drainage ditch guides the moisture in the external soil into itself through the water guide hole and discharges it, blocking the path of surface soil moisture entering the wall; the underground enclosure barrier cooperates with the ground moisture-proof structure to establish a physical blockade surrounding the underground part of the wall, effectively preventing the intrusion of underground moisture on the wall. At the same time, the system described in the present invention will not destroy the material properties and structural stability of the building itself, has little impact on the surrounding environment of the building surface, is environmentally friendly, and meets the repair standard of repairing the old as it is; 2) The construction operation is convenient. The splicing plates in the enclosure mechanism can be plugged in with specially shaped insertion parts and plug-in edges to achieve straight-line splicing and corner splicing. Not only is the installation difficult, but the self-compacting glue can be released during the plug-in process to seal the plug-in parts of the splicing plates, effectively ensuring that the enclosure mechanism blocks underground moisture.
[0015] 3) Low cost. The splicing plates of the enclosure mechanism in the present invention are made of stainless steel corrugated plates with excellent corrosion resistance, structural strength and durability. The price is relatively cheap and the single plate is light and small in size, which reduces transportation costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a structural schematic diagram of a moisture-proof composite system for a brick-concrete structure building wall according to a specific implementation method; Figure 2 It is a structural schematic diagram of one of the splicing plates described in the specific implementation method; Figure 3 It is a structural schematic diagram of the second splicing plate described in the specific implementation method; Figure 4 It is a schematic diagram of the structure of the splicing plate in a vertical plug-in state according to the specific implementation method; Figure 5 It is a schematic diagram of the structure of the spliced plates in a parallel state as described in the specific implementation method. DETAILED DESCRIPTION
[0017] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0018] like Figure 1-5 As shown, a moisture-proof composite system for the wall of an ancient building with a brick-concrete structure, the system includes a ground moisture-proof structure arranged around the ground part of the outer wall of the wall 1 and an underground moisture-proof structure arranged around the underground part of the outer wall of the wall 1: The ground moisture-proof structure includes a water-spreading part 21 with a slope on the top surface. The higher end of the water-spreading part 21 is arranged close to the corresponding side of the wall 1 on the ground, and the lower end transitions to the drainage ditch 22 arranged away from the wall 1. The water-spreading part 21 and the drainage ditch 22 are both concrete structures, and the bottom surface of the drainage ditch 22 has a slope to guide water to the municipal underground pipe network. The side of the drainage ditch 22 away from the wall is provided with a water guide hole 23 with the bottom facing the inside of the drainage ditch 22 and the top below the ground, and an anti-blocking component 24 is provided at the top of the water guide hole 23. The anti-blocking component 24 can be a conventional anti-blocking component such as geotextile to prevent soil from blocking the water guide hole 23. The top surface of the drainage ditch 22 away from the wall 1 is at least not higher than the ground height. This design is intended to prevent the surface water head from being too high and causing groundwater away from the wall to seep into the wall foundation, thereby causing the wall to return moisture.
[0019] The underground moisture-proof structure includes an enclosure mechanism 3 located directly below the ground moisture-proof structure and a concrete layer 31 cast on the inner and outer walls of the enclosure mechanism 3 and connected to the ground moisture-proof structure. The enclosure mechanism 3 surrounds the underground part of the wall 1. The enclosure mechanism 3 includes a plurality of splicing plates 32 that are plugged into each other. The plate bodies at both ends of the length direction of the splicing plate 32 include an insertion portion 33 and a plug-in edge 34 that is in a free state in a non-plug-in state. The insertion portion 33 is an arc-shaped cylindrical structure extending along the width direction of the splicing plate with an axis, and the two ends of the insertion portion 33 are integrally transitionally connected with the plate body and the plug-in edge 34. The entrance of the insertion portion is gap-matched with the plug-in edge 34 of the adjacent splicing plate 32, and the insertion portion and the plug-in edge of the adjacent splicing plate in the plug-in state are plugged into each other. The insertion portions 33 and the plug-in edges 34 of the adjacent splicing plates are in the plug-in state, and the two splicing plates 32 are in a vertical or parallel state. The inserting portion is filled with a self-compacting glue 35 or a bagged container for containing the self-compacting glue 35 .
[0020] The construction method of the above-mentioned brick-concrete structure ancient building wall moisture-proof combination system comprises the following steps: 1) An initial foundation pit is excavated at 0.5m~1m along the periphery of the wall for the later preparation of the water dispersion part and the drainage ditch, and then a secondary foundation pit with a width of 0.1~0.15m is excavated directly below the designed position of the side wall foundation on the side of the drainage ditch close to the wall for burying the enclosure mechanism; 2) The sealing bag containing liquid self-compacting glue is completely filled with the insertion part of the splicing plate to be plugged in, and then the splicing plates are vertically inserted into the secondary foundation pit in sequence to complete the mutual plugging of the insertion parts and the plugging edges of the adjacent splicing plates. At the same time, the plugging edge punctures the sealing bag of the corresponding insertion part to complete the filling of the gap between the insertion part and the plugging edge with the self-compacting glue, and then the sealing bag is pulled out; 3) After the self-compacting adhesive is completely cured, pour concrete into the remaining space of the secondary foundation pit to complete the secondary foundation pit landfill; 4) Pour concrete in the initial foundation pit and reserve a water guide hole forming mold to wait for the drainage ditch to be formed. After the drainage ditch is formed, level the ground between the drainage ditch and the wall and compact it, then lay the reinforced concrete layer to form the water dispersion part.
[0021] The present invention has been applied in secret to the damp-recovery construction of an ancient building wall in a certain place, specifically: The plan dimensions of the ancient building are 36.6m long and 21.6m wide. The first floor wall suffers from severe moisture, which causes the plaster layer to peel off, the bricks to deteriorate and chip, and the wall to crack, seriously affecting the appearance and safety of use.
[0022] Before the construction of the system described in the present invention, the structural design parameters are as follows: The water dispersion part is made of mixed reinforced concrete, with a width of 1m and a thickness of 0.2m, and is arranged along the length of the wall; The depth of the drainage ditch is set to 600mm and the width is 500mm. The wall thickness of the seepage ditch is 30cm. A water diversion hole is set on the side wall away from the wall. The inclination angle of the water diversion hole is 10°, the diameter is 4cm, and the distance from the top surface of the side wall is 20cm. The interval is 0.5m. Geotextile is placed at the higher end of the water diversion hole as a blocking component.
[0023] The splicing plate adopts two types, Type I and Type II. The length of the two types of plates is 1m, the height is 1m, and the thickness is 5mm, ensuring sufficient strength and durability. The inner diameter of the insertion part is 20mm, and the length of the plug-in edge is 50mm. The angle between the plug-in edge of the Type I plate and the plate body is 20°. Figure 2 As shown; the angle between one plug-in edge of the type II plate and the plate is 110°, as shown Figure 3 As shown in Figure 1, this design is conducive to the close connection and stable layout between the panels. The mutual insertion of type I panels forms a linear structure as shown in Figure 1. Figure 5 As shown, the mutual mating of type I plate and type II plate forms a vertical angle structure as shown in Figure 4As shown; the self-compacting glue used for the gap of the mating part in the later stage is epoxy resin glue and is packaged in a flat bag with a diameter of 2cm and a height of 1m.
[0024] During construction: 1) Use a pit excavator to accurately dig an initial foundation pit with a depth of 0.9m, a width of 1.1m, and a length of 36.6m and 24.6m respectively along the periphery of the building. The initial foundation pit maintains a safety distance of 0.5m from the outer wall of the building; then, in the initial foundation pit, 0.1m away from the outer wall of the building, further dig a secondary foundation pit with a depth of 1m, a width of 0.15m, and a length adjusted to 38m and 23m according to the outline of the building; 2) Inject the pre-mixed epoxy resin glue into the flat bag strip plastic bag and seal the plastic bag, and then fill the plastic bag into the insertion part of each splicing board. Then insert the splicing boards vertically into the secondary foundation pit one by one and complete the mutual mating. During the mating process, the splicing edge punctures the plastic bag in the corresponding insertion part, so that the epoxy resin glue is evenly released and self-compacted in the gap between the plug-in board and the insertion part, and then the plastic bag body is pulled out. A total of 122 splicing boards are installed in the entire building; 3) After the epoxy resin glue is completely cured, pour concrete in the remaining space of the secondary foundation pit to reinforce and seal the structure, thereby completing the construction of the moisture-proof structure under the ground; 4) Continue construction of the bottom and both sides of the initial foundation pit: pour a concrete layer with a thickness of 30cm to enhance the stability and waterproof performance of the overall structure. At the same time, on the side away from the wall, reserve the installation position of the seepage hole pipe according to the design to ensure that the drainage ditch can effectively drain water. Then, level the ground between the seepage ditch and the wall, compact it effectively, lay a 6@300 reinforced concrete layer as the water dispersion part, and set a 2% slope on the surface pointing to the drainage ditch to drain rainwater and further prevent water infiltration. The corresponding construction is completed.
Claims
1. A moisture-proof composite system for the wall of an ancient brick-concrete structure, comprising a ground moisture-proof structure arranged around the ground portion of the outer wall of the wall and an underground moisture-proof structure arranged around the underground portion of the outer wall of the wall, characterized in that ; The ground moisture-proof structure includes a water dispersion portion with a sloped top surface, wherein the higher end of the water dispersion portion is arranged close to the corresponding side of the wall and the lower end transitions to a drainage ditch arranged away from the wall; The underground moisture-proof structure includes an enclosure mechanism located directly below the ground moisture-proof structure and a concrete layer poured on the inner and outer side walls of the enclosure mechanism and connected to the ground moisture-proof structure. The enclosure mechanism surrounds the underground part of the wall.
2. The moisture-proof composite system for the wall of an ancient brick-concrete structure building according to claim 1, characterized in that: The water dispersion part and the drainage ditch are both concrete structures, and the bottom surface of the drainage ditch has a slope for guiding water to flow toward the municipal underground pipe network.
3. The moisture-proof composite system for the wall of an ancient brick-concrete structure building according to claim 2, characterized in that: A water guide hole with a bottom end facing the inside of the drainage ditch and a top end located below the ground is opened on the side of the drainage ditch away from the wall, and an anti-blocking component is provided at the top end of the water guide hole.
4. The moisture-proof composite system for the wall of an ancient brick-concrete structure building according to claim 2, characterized in that: The top surface of the drainage ditch on the side away from the wall is at least not higher than the ground level.
5. The moisture-proof composite system for the wall of an ancient brick-concrete structure building according to claim 1, characterized in that: The enclosure mechanism includes several splicing plates that are plugged into each other. The plate bodies at both ends in the longitudinal direction of the splicing plates include an insertion portion and a plug-in edge that is in a free state when not plugged into the splicing plate. The insertion portion is an arc-shaped cylindrical structure with an axis extending along the width direction of the splicing plate, and the two ends of the insertion portion are transitionally connected to the plate body and the plug-in edge as a whole.
6. The moisture-proof composite system for the wall of an ancient brick-concrete structure building according to claim 5, characterized in that: The inlet of the inserting portion is clearance-matched with the plugging edge of the adjacent splicing plate.
7. The moisture-proof composite system for the wall of an ancient brick-concrete structure building according to claim 5, characterized in that: The inserting portions and the inserting edges of adjacent splicing plates in the mating state are mated with each other.
8. The moisture-proof composite system for the wall of an ancient brick-concrete structure building according to claim 5, characterized in that: The inserting portion is filled with self-compacting glue or a bagged container for containing the self-compacting glue.
9. The moisture-proof composite system for the wall of an ancient brick-concrete structure building according to claim 5, characterized in that: When the inserting parts and the plugging edges of the adjacent splicing plates are in a mating state, the two splicing plates are in a vertical or parallel state.
10. The construction method of the moisture-proof composite system for the wall of an ancient brick-concrete structure building according to any one of claims 1 to 9, characterized in that Here are the steps: 1) Dig an initial foundation pit 0.5m to 1m away from the periphery of the wall for the later preparation of the water dispersion part and drainage ditch. Then, dig a secondary foundation pit with a width of 0.1 to 0.15m for burying the enclosure mechanism just below the designed position of the side wall foundation on the side of the drainage ditch close to the wall. 2) The sealed bag containing the liquid self-compacting glue is completely filled with the insertion part of the splicing plate to be plugged in, and then the splicing plates are vertically inserted into the secondary foundation pit in sequence and the insertion parts and plug-in edges of the adjacent splicing plates are plugged in. At the same time, the plug-in edge punctures the sealed bag of the corresponding insertion part to complete the filling of the gap between the insertion part and the plug-in edge with the self-compacting glue, and then the sealed bag is pulled out; 3) After the self-compacting adhesive is completely solidified, concrete is poured into the remaining space of the secondary foundation pit to complete the secondary foundation pit landfill; 4) Pour concrete in the initial foundation pit and reserve a water guide hole forming mold for the drainage ditch to be formed. After the drainage ditch is formed, level the ground between the drainage ditch and the wall and tamp it, then lay a reinforced concrete layer to form the water dispersion part.