Method and system for evaluating corrosion state of tower drum of offshore wind turbine

By acquiring and analyzing tower images, corrosion rate, coating thickness and tensile strength data, combined with a scoring system, the uncertainty and inefficiency of traditional methods are solved, and efficient and accurate assessment of the corrosion status of offshore wind turbine towers is achieved. Reliable evaluation extends the service life of the fan.

CN118757335APending Publication Date: 2024-10-11中电华创(苏州)电力技术研究有限公司
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202410922759.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-10
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Traditional methods for assessing the corrosion status of offshore wind turbine towers rely on manual inspections and visual inspections, which are uncertain, inefficient and costly. They are difficult to meet the needs of large-scale wind farms and cannot provide an in-depth understanding of the internal conditions and development trends of corrosion.

Method used

By acquiring tower image data, corrosion rate data, coating thickness data and hanging sample tensile strength data, combined with image recognition, corrosion rate score, coating thickness score and mechanical property score, a weight calculation formula is used to calculate the rust status and provide offshore A wind turbine tower corrosion status assessment method and system includes an image acquisition module, a corrosion monitoring module, a coating thickness module, a mechanical performance module and a condition assessment module.

Benefits of technology

It achieves efficient, reliable and accurate assessment of the corrosion status of offshore wind turbine towers, and improves the power generation efficiency and service life of wind turbines.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118757335A_ABST
    Figure CN118757335A_ABST
Patent Text Reader

Abstract

The invention provides an offshore wind turbine tower corrosion state assessment method and assessment system. The evaluation method comprises the following steps: obtaining tower drum image data, corrosion rate data, coating thickness data and hanging sample tensile strength data; and the corrosion state of the offshore wind turbine tower drum is calculated according to the tower drum image data, the corrosion rate data, the coating thickness data and the hanging sample tensile strength data. According to the method, the corrosion state of the offshore wind turbine tower can be efficiently, reliably and accurately evaluated, the power generation efficiency of the wind turbine can be improved, and the service life of the wind turbine can be prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the technical field of new energy equipment maintenance, and specifically, relates to a method for evaluating the corrosion status of an offshore wind turbine tower. Background Art

[0002] As the global demand for renewable energy continues to grow, offshore wind power generation, as a clean, renewable energy form, is receiving more and more attention. However, the offshore environment is complex and changeable, and factors such as high humidity, high salinity, and strong winds and waves have a particularly significant impact on the corrosion of offshore wind turbine towers. Offshore wind turbine towers that have been in operation for a long time often face serious corrosion problems, which not only affects the structural strength and service life of the tower, but may also pose a threat to the safe operation of the wind farm.

[0003] Traditional methods for evaluating the corrosion status of offshore wind turbine towers mainly rely on manual inspections and visual inspections, which have many limitations. First, manual inspections are limited by the experience and subjective judgment of inspectors, and the evaluation results often have large uncertainties. Second, visual inspections can only make simple observations of the tower surface, and cannot provide an in-depth understanding of the internal conditions and development trends of the corrosion. In addition, traditional methods also face problems such as low efficiency and high costs, making it difficult to meet the needs of large-scale wind farms.

[0004] Therefore, developing an accurate, efficient and reliable method and system for evaluating the corrosion status of offshore wind turbine towers is of great significance for ensuring the safe operation of wind farms and extending the service life of wind turbine towers. Summary of the invention

[0005] The technical problem solved by the present application is: how to provide a method and system for evaluating the corrosion status of an offshore wind turbine tower, which can accurately evaluate the corrosion status of an offshore wind turbine tower, improve the power generation efficiency of the wind turbine, and extend the service life of the wind turbine.

[0006] The present application provides a method for evaluating the corrosion status of an offshore wind turbine tower, the method comprising:

[0007] Obtain tower image data, corrosion rate data, coating thickness data, and hanging sample tensile strength data;

[0008] The corrosion state of the offshore wind turbine tower is calculated based on the tower image data, the corrosion rate data, the coating thickness data, and the hanging sample tensile strength data.

[0009] Optionally, the method for calculating the corrosion state of the offshore wind turbine tower according to the tower image data, the corrosion rate data, the coating thickness data, and the hanging sample tensile strength data includes:

[0010] Calculate the image recognition rust score, corrosion rate score, coating thickness score, and mechanical property score according to the tower image data, the corrosion rate data, the coating thickness data, and the hanging sample tensile strength data;

[0011] The corrosion status of the offshore wind turbine tower is calculated based on the image recognition corrosion score, corrosion rate score, coating thickness score and mechanical property score.

[0012] Optionally, the method for calculating the corrosion state of the offshore wind turbine tower according to the image recognition corrosion score, corrosion rate score, coating thickness score, and mechanical property score is:

[0013] The corrosion status is calculated according to the following formula:

[0014] RAI=a*IRR+b*CCR+c*CT+d*ML

[0015] Among them, RAI represents the corrosion state, IRR represents the image recognition corrosion score, CCR represents the corrosion rate score, CT represents the coating thickness score, ML represents the mechanical property score, a, b, c, d represent the weight coefficients, a+b+c+d=1.

[0016] Optionally, the method for obtaining an image recognition corrosion score based on the tower image data includes:

[0017] Identify the corrosion area of ​​the tower image data to obtain the corrosion area and corrosion depth;

[0018] The image recognition rust score is calculated based on the ratio of the rust area to the total area and the rust depth.

[0019] Optionally, the method for calculating the corrosion rate score according to the corrosion rate data includes:

[0020] A corrosion rate score is obtained based on the measured corrosion rate data and a preset corrosion rate score standard, wherein the faster the corrosion rate, the higher the score.

[0021] Optionally, a method for calculating a coating thickness score based on the coating thickness data includes:

[0022] A coating thickness score is obtained according to the measured coating thickness data and a preset coating thickness score standard, wherein the thinner the coating is, the higher the score is.

[0023] Optionally, the method for calculating the mechanical property score according to the tensile strength data of the hanging sample includes:

[0024] A mechanical property score is obtained according to the tensile strength data of the hanging sample obtained from the test and a preset mechanical property score standard. In the mechanical property score standard, the smaller the tensile strength data of the hanging sample is, the higher the mechanical property score is.

[0025] The present application provides an offshore wind turbine tower corrosion status assessment system, the assessment system comprising:

[0026] An image acquisition module is used to acquire tower image data;

[0027] Corrosion monitoring module, used to monitor and obtain corrosion rate data;

[0028] Coating thickness module, used to obtain coating thickness data;

[0029] Mechanical properties module, used to obtain the tensile strength data of hanging samples;

[0030] The status assessment module is used to calculate the corrosion status of the offshore wind turbine tower based on the tower image data, the corrosion rate data, the coating thickness data, and the hanging sample tensile strength data.

[0031] The present application provides an offshore wind turbine tower corrosion status assessment method and assessment system, which have the following technical effects:

[0032] This method can realize efficient, reliable and accurate evaluation of the corrosion status of offshore wind turbine towers, and can also improve the power generation efficiency of wind turbines and extend the service life of wind turbines. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 is a flow chart of a method for evaluating the corrosion status of an offshore wind turbine tower according to one or more embodiments;

[0034] Figure 2 A schematic diagram of an offshore wind turbine tower according to one or more embodiments;

[0035] Figure 3 The schematic diagram is a functional block diagram of a system for evaluating the corrosion status of an offshore wind turbine tower according to one or more embodiments.

[0036] The corresponding relationship between the reference numerals and the component names is as follows:

[0037] 1-tower wall, 2-corrosion sensor, 3-tower wall-mounted sample, 4-corrosion area, 10-image acquisition module, 20-corrosion monitoring module, 30-coating thickness module, 40-mechanical properties module, 50-state assessment module, 60-image processing module, 70-feature extraction module. DETAILED DESCRIPTION

[0038] In order to make the purpose, technical solution and advantages of the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.

[0039] Before describing the various embodiments of the present application in detail, the technical concept of the present application is first briefly described: the current offshore wind turbine tower corrosion status assessment method mainly relies on manual inspection and visual inspection, which has many limitations. To this end, the offshore wind turbine tower corrosion status assessment method provided by the present application obtains the offshore wind turbine tower corrosion status through comprehensive assessment based on tower image data, corrosion rate data, coating thickness data, and hanging sample tensile strength data, which can achieve efficient, reliable, and accurate assessment of the offshore wind turbine tower corrosion status, and can also improve the wind turbine power generation efficiency and extend the service life of the wind turbine. The specific principles of the offshore wind turbine tower corrosion status assessment method of the present application are described below in combination with more embodiments.

[0040] Specifically, Figure 1 As shown, the method for evaluating the corrosion status of an offshore wind turbine tower provided in the first embodiment includes the following steps:

[0041] Step S10: obtaining tower image data, corrosion rate data, coating thickness data, and hanging sample tensile strength data;

[0042] Step S20: Calculate the corrosion status of the offshore wind turbine tower according to the tower image data, corrosion rate data, coating thickness data, and hanging sample tensile strength data.

[0043] In one or more embodiments, a drone equipped with a high-definition camera is used to regularly collect image and video data of offshore wind turbine towers, and the collected image information is preprocessed, including steps such as denoising and contrast enhancement, to improve image quality and obtain the required tower image data. Figure 2 As shown, the image recognition technology is then used to identify the rusted area of ​​the processed image, and the characteristic parameters of the tower rusted area 4, such as the rusted area, rusted depth, rusted shape, etc., are extracted through image segmentation and feature extraction algorithms. Further, a quantitative score is given according to the proportion of the area of ​​the rusted area to the total area and the rusted depth. The larger the proportion of the rusted area and the deeper the rusted depth, the higher the score.

[0044] In one or more embodiments, Figure 2As shown, 4 corrosion sensors 2 are installed at the upper, middle and lower heights of the outer wall 1 of the tower, for a total of 12 sensors. The corrosion sensors monitor the corrosion rate of the tower in real time and transmit the data to the data center. The data center stores and analyzes the received corrosion rate data to form a historical record of the tower corrosion rate and obtain the required corrosion rate data. Then, the corrosion rate score is obtained based on the measured corrosion rate data and the preset corrosion rate scoring standard. In the corrosion rate scoring standard, the faster the corrosion rate, the higher the score.

[0045] In one or more embodiments, a coating thickness gauge is used to measure the thickness of the coating on the upper, middle and lower walls of the wind turbine tower every quarter. Multiple measuring points are selected in each area for measurement to ensure the accuracy and representativeness of the measurement results. The measured coating thickness data is synchronized with the data center to form a historical record of the coating thickness and obtain the required coating thickness data. The coating thickness score is obtained based on the measured coating thickness data and the preset coating thickness scoring standard. In the coating thickness scoring standard, the thinner the coating, the higher the score, because the thinner the coating means the weakened protective effect of the coating.

[0046] In one or more embodiments, samples are hung in the upper, middle and lower areas of the tower wall, and multiple hanging points 3 are set in each area. Samples are taken every quarter, and tensile strength mechanical property tests are performed to obtain the required tensile strength data of the hanging samples. By comparing the mechanical property test results at different time points, the degree of influence of corrosion on material properties is evaluated. A mechanical property score is obtained based on the tensile strength data of the hanging samples obtained from the test and a preset mechanical property scoring standard. In the mechanical property scoring standard, the smaller the tensile strength data of the hanging samples, the higher the mechanical property score, because the decline in material performance will affect the safety performance of the tower.

[0047] Furthermore, the corrosion status of the offshore wind turbine tower is calculated based on the calculated image recognition corrosion score, corrosion rate score, coating thickness score, and mechanical property score. The status assessment formula is as follows:

[0048] RAI=a*IRR+b*CCR+c*CT+d*ML

[0049] Among them, RAI represents the corrosion state, IRR represents the image recognition corrosion score, CCR represents the corrosion rate score, CT represents the coating thickness score, ML represents the mechanical property score, a, b, c, d represent the weight coefficients, a+b+c+d=1. For example, a=40%, b=20%, c=20%, d=20%.

[0050] This second embodiment also discloses a system for evaluating the corrosion status of an offshore wind turbine tower. Figure 3As shown, the evaluation system includes an image acquisition module 10, a corrosion monitoring module 20, a coating thickness module 30, a mechanical property module 40, and a state evaluation module 50. The image acquisition module 10 is used to acquire tower image data, the corrosion monitoring module 20 is used to monitor and obtain corrosion rate data, the coating thickness module 30 is used to acquire coating thickness data, the mechanical property module 40 is used to acquire hanging sample tensile strength data, and the state evaluation module 50 is used to calculate the corrosion state of the offshore wind turbine tower according to the tower image data, corrosion rate data, coating thickness data, and hanging sample tensile strength data.

[0051] The evaluation system further includes an image processing module 60 and a feature extraction module 70. The image processing module 60 is used to receive the image information transmitted by the image acquisition module and perform pre-processing steps such as denoising and contrast enhancement to improve the image quality. Through advanced image processing algorithms, the characteristic parameters of the tower corrosion area, such as the corrosion area and corrosion depth, are accurately identified and extracted. Based on the results output by the image processing module, the feature extraction module 70 further extracts key features closely related to the corrosion state and transmits the key data to the state evaluation module 50.

[0052] Exemplarily, the corrosion monitoring module 20 monitors the corrosion rate of the tower in real time through the corrosion sensor installed on the tower wall, and transmits the data to the state assessment module 50 for analysis. The coating thickness module 30 regularly detects the coating thickness of the tower wall to evaluate the protective effect of the coating, and transmits the data to the state assessment module 50 for analysis. The mechanical properties module 40 is used to characterize the mechanical properties of the tower wall and feedback the stability of the material. The state assessment module 50 is the core of the system. This module integrates the acquired image recognition corrosion score, corrosion rate score, coating thickness score, and mechanical property score, and uses the state assessment formula to obtain the corrosion state of the offshore wind turbine tower.

[0053] The offshore wind turbine tower corrosion status assessment method provided in this embodiment can achieve efficient, reliable and accurate assessment of the offshore wind turbine tower corrosion status, and can also improve the power generation efficiency of the wind turbine and extend the service life of the wind turbine.

[0054] The specific implementation methods of the present application are described in detail above. Although some embodiments have been shown and described, those skilled in the art should understand that these embodiments can be modified and improved without departing from the principles and spirit of the present application whose scope is defined by the claims and their equivalents. These modifications and improvements should also be within the scope of protection of the present application.

Claims

1. A method for evaluating the corrosion status of an offshore wind turbine tower, characterized in that: The evaluation methods include: Obtain tower image data, corrosion rate data, coating thickness data, and hanging sample tensile strength data; The corrosion state of the offshore wind turbine tower is calculated based on the tower image data, the corrosion rate data, the coating thickness data, and the hanging sample tensile strength data.

2. The offshore wind turbine tower corrosion status assessment method according to claim 1, characterized in that: The method for calculating the corrosion state of an offshore wind turbine tower according to the tower image data, the corrosion rate data, the coating thickness data, and the hanging sample tensile strength data comprises: Calculate the image recognition rust score, corrosion rate score, coating thickness score, and mechanical property score according to the tower image data, the corrosion rate data, the coating thickness data, and the hanging sample tensile strength data; The corrosion status of the offshore wind turbine tower is calculated based on the image recognition corrosion score, corrosion rate score, coating thickness score and mechanical property score.

3. The offshore wind turbine tower corrosion status assessment method according to claim 2, characterized in that: The method for calculating the corrosion state of the offshore wind turbine tower according to the image recognition corrosion score, corrosion rate score, coating thickness score, and mechanical property score is: The corrosion status is calculated according to the following formula: RAI=a*IRR+b*CCR+c*CT+d*ML Among them, RAI represents the corrosion state, IRR represents the image recognition corrosion score, CCR represents the corrosion rate score, CT represents the coating thickness score, ML represents the mechanical property score, a, b, c, d represent the weight coefficients, a+b+c+d=1.

4. The offshore wind turbine tower corrosion status assessment method according to claim 2, characterized in that: Methods for obtaining image recognition corrosion scores based on tower image data include: Identify the corrosion area of ​​the tower image data to obtain the corrosion area and corrosion depth; The image recognition rust score is calculated based on the ratio of the rust area to the total area and the rust depth.

5. The offshore wind turbine tower corrosion status assessment method according to claim 2, characterized in that: The method for calculating the corrosion rate score according to the corrosion rate data includes: A corrosion rate score is obtained based on the measured corrosion rate data and a preset corrosion rate score standard, wherein the faster the corrosion rate, the higher the score.

6. The offshore wind turbine tower corrosion status assessment method according to claim 2, characterized in that: The method for calculating the coating thickness score according to the coating thickness data includes: A coating thickness score is obtained according to the measured coating thickness data and a preset coating thickness score standard, wherein the thinner the coating is, the higher the score is.

7. The offshore wind turbine tower corrosion status assessment method according to claim 2, characterized in that: The method for calculating the mechanical property score according to the tensile strength data of the hanging sample includes: A mechanical property score is obtained according to the tensile strength data of the hanging sample obtained from the test and a preset mechanical property score standard. In the mechanical property score standard, the smaller the tensile strength data of the hanging sample is, the higher the mechanical property score is.

8. An offshore wind turbine tower corrosion status assessment system, characterized in that: The evaluation system comprises: An image acquisition module is used to acquire tower image data; Corrosion monitoring module, used to monitor and obtain corrosion rate data; Coating thickness module, used to obtain coating thickness data; Mechanical properties module, used to obtain the tensile strength data of hanging samples; The status assessment module is used to calculate the corrosion status of the offshore wind turbine tower based on the tower image data, the corrosion rate data, the coating thickness data, and the hanging sample tensile strength data.

Citation Information

Cited By

  • Marine navigation mark coating life cycle evaluation method and system

    CN119204832A

  • A method and system for life cycle assessment of marine navigation mark coatings