Preparation method of semiconductor structure and semiconductor structure
By forming the target structure and etching stop layer on the substrate in semiconductor manufacturing, and forming an oxide layer on its side surface, the problem of contact hole over-etching in the traditional process is solved, and the yield and process window of the semiconductor structure are improved. .
Patent Information
- Application Number
- CN202411011219.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-10-11
AI Technical Summary
In semiconductor manufacturing, since the depth of the source and drain is greater than the depth of the gate, the contact hole above the gate may be over-etched in the traditional preparation process, resulting in poor contact hole morphology and affecting the yield and process window of the semiconductor structure. .
By forming the first and second target structures on the substrate, covering the etching stop layer, and forming the first oxide layer on its side surface, ensuring that the top surface of the oxide layer is flush with the top surface of the stop layer, and then forming on the oxide layer In the second oxide layer, part of the oxide layer is removed to form a contact hole to ensure the optimization of the depth and morphology of the contact hole.
It effectively avoids over-etching of the etching stop layer, improves the morphology of the contact hole, increases the yield of the semiconductor structure, increases the process window, and ensures the integrity and accuracy of the contact hole.
Smart Images

Figure CN118763056A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor manufacturing, and in particular to a method for preparing a semiconductor structure and a semiconductor structure. Background Art
[0002] In the field of semiconductor manufacturing technology, in order to form electrical connections, it is usually necessary to form contact holes above transistors, wherein contact holes are usually formed above the gate and source and drain of the transistor to connect the gate and source and drain to an external circuit.
[0003] However, in the traditional preparation process, since the depth of the source and drain is greater than the depth of the gate, the etching depth of the contact hole above the source and drain is greater than the etching depth of the contact hole above the gate. When the contact holes above the gate and the source and drain are formed at the same time, the contact hole above the gate may be over-etched, resulting in poor morphology of the formed contact hole. Summary of the invention
[0004] Based on this, an embodiment of the present application provides a method for preparing a semiconductor structure and a semiconductor structure.
[0005] According to some embodiments, the present application provides a method for preparing a semiconductor structure, the method for preparing a semiconductor structure comprising: providing a substrate, on which a first target structure and a second target structure are formed, the top surface of the first target structure being higher than the top surface of the second target structure; forming an etch stop layer, the etch stop layer at least covering the outer surface of the first target structure and the top surface of the second target structure; forming a first oxide layer on the side surface of the etch stop layer away from the first target structure, the top surface of the first oxide layer being flush with the top surface of the etch stop layer; forming a second oxide layer on the top surface of the first oxide layer; removing portions of the first oxide layer and the second oxide layer to form a first contact hole and a second contact hole, the first contact hole being located directly above the first target structure, the second contact hole being located directly above the second target structure, and both the first contact hole and the second contact hole extending to the top surface of the etch stop layer.
[0006] In the method for preparing the semiconductor structure of the above embodiment, a first oxide layer is formed on the side surface of the etch stop layer away from the first target structure, and a second oxide layer is formed on the top surface of the first oxide layer; a portion of the first oxide layer and the second oxide layer is removed to form a first contact hole and a second contact hole. Since the first contact hole is located directly above the first target structure and the second contact hole is located directly above the second target structure, both the first contact hole and the second contact hole extend to the top surface of the etch stop layer, and it can be concluded that the depth of the second contact hole is greater than the depth of the first contact hole. In this way, since the top surface of the first oxide layer is flush with the top surface of the etch stop layer, when forming the first contact hole and the second contact hole, over-etching of the etch stop layer at the bottom of the first contact hole can be effectively avoided, thereby improving the morphology of the first contact hole and the second contact hole, so as to improve the yield of the semiconductor structure and increase the process window.
[0007] In some embodiments, the oxygen content in the first oxide layer ranges from 55% to 70%.
[0008] In some embodiments, an etching selectivity ratio of the first oxide layer to the etch stop layer is not less than 10:1.
[0009] In the method for preparing the semiconductor structure of the above embodiment, since the etching selectivity ratio between the first oxide layer and the etch stop layer is not less than 10:1, after forming the first contact hole, the first oxide layer can be continuously removed to form the second contact hole, thereby avoiding over-etching of the etch stop layer, thereby ensuring the integrity of the etch stop layer.
[0010] In some embodiments, a first oxide layer is formed on a side surface of the etch stop layer away from the first target structure, including: forming an initial oxide layer on the etch stop layer; removing a portion of the initial oxide layer until the etch stop layer located on the top surface of the first target structure is exposed, and the remaining initial oxide layer constitutes the first oxide layer.
[0011] In some embodiments, the thickness of the initial oxide layer ranges from 1000 Å to 5000 Å.
[0012] In some embodiments, the second oxide layer has a thickness ranging from 1000 Å to 8000 Å.
[0013] In some embodiments, a one-time etching process is used to simultaneously remove a portion of the second oxide layer and the first oxide layer to form the first contact hole and the second contact hole.
[0014] In some embodiments, the first target structure includes a gate structure; and the second target structure includes doped regions located on both sides of the first target structure.
[0015] According to some embodiments, the present application also provides a semiconductor structure, including a substrate, an etch stop layer, a first oxide layer, a second oxide layer, a first contact hole and a second contact hole; a first target structure is formed on the substrate, and a second target structure located on both sides of the first target structure is also formed in the substrate; the etch stop layer at least covers the outer surface of the first target structure and the top surface of the second target structure; the first oxide layer is located on the side surface of the etch stop layer away from the first target structure, and the top surface of the first oxide layer is flush with the top surface of the etch stop layer; the second oxide layer is located on the top surface of the first oxide layer; a first contact hole and a second contact hole, the first contact hole is located directly above the first target structure, and the second contact hole is located directly above the second target structure, and the bottom surface of the first contact hole and the bottom surface of the second contact hole both expose part of the top surface of the etch stop layer.
[0016] In the semiconductor structure of the above embodiment, the first contact hole is located directly above the first target structure, and the second contact hole is located directly above the second target structure. The bottom surface of the first contact hole and the bottom surface of the second contact hole both expose part of the top surface of the etch stop layer, which can improve the morphology of the first contact hole and the second contact hole, thereby improving the yield of the semiconductor structure and increasing the process window.
[0017] In some embodiments, the first target structure includes a gate structure; and the second target structure includes doped regions located on both sides of the gate structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] FIG1 is a schematic cross-sectional view of a structure obtained by a method for preparing a semiconductor structure;
[0019] FIG2 is a schematic diagram of a process for preparing a semiconductor structure according to an embodiment of the present application;
[0020] Figure 3 A schematic cross-sectional view of a structure obtained in step 31 of a method for preparing a semiconductor structure provided in one embodiment of the present application;
[0021] Figure 4 A schematic cross-sectional view of a structure obtained in step 32 of a method for preparing a semiconductor structure provided in one embodiment of the present application;
[0022] Figure 5 A schematic cross-sectional view of a structure obtained in step 40 of a method for preparing a semiconductor structure provided in one embodiment of the present application;
[0023] Figure 6 A schematic cross-sectional view of a structure obtained in step 50 of a method for preparing a semiconductor structure provided in one embodiment of the present application.
[0024] Explanation of the reference numerals: 10, substrate; 11, well region; 12, second target structure; 121, source / drain electrode; 13, isolation structure; 131, first isolation layer; 132, second isolation layer; 20, first target structure; 21, gate conductive layer; 22, gate dielectric layer; 23, gate electrode; 24, gate sidewall; 30, etch stop layer; 40, first oxide layer; 41, initial oxide layer; 50, second oxide layer; 60, first contact hole; 70, second contact hole. DETAILED DESCRIPTION
[0025] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. Preferred embodiments of the present invention are provided in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the understanding of the disclosure of the present invention more thorough and comprehensive.
[0026] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which the present invention belongs. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.
[0027] In the case of using “including”, “having”, and “comprising” described herein, another component may be added unless a clear limiting term such as “only”, “consisting of”, etc. is used. Unless mentioned otherwise, a term in the singular form may include a plural form and should not be understood as being one in number.
[0028] In addition, in order to clearly indicate the multiple layers and regions in the drawings, the thickness of each layer and each region in the drawings are enlarged to clearly illustrate the relative positions between the layers and the distribution of each region. When a layer, film, region, plate, etc. is expressed as being located on the "side" of another part, the expression includes not only the case where it is "directly" above the other part, but also the case where there are other layers in between. And, it is understood that when a layer, film, region, plate, etc. is expressed as being located on the "side" of another part, it generally refers to the side located directly above the other part.
[0029] It should be understood that when an element or layer is referred to as "on ...", "adjacent to ...", "connected to" or "coupled to" other elements or layers, it can be directly on, adjacent to, connected to or coupled to other elements or layers, or there can be intervening elements or layers. On the contrary, when an element is referred to as "directly on ...", "directly adjacent to ...", "directly connected to" or "directly coupled to" other elements or layers, there is no intervening element or layer. It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, regions, layers, doping types and / or parts, these elements, components, regions, layers, doping types and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer, doping type or part from another element, component, region, layer, doping type or part. Therefore, without departing from the teachings of the present disclosure, the first element, component, region, layer, doping type or part discussed below can be represented as a second element, component, region, layer or part.
[0030] Spatially relative terms such as "under," "beneath," "below," "under," "above," "above," and the like may be used herein to describe the relationship of an element or feature shown in the figures to other elements or features. It should be understood that, in addition to the orientations shown in the figures, spatially relative terms also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is flipped, an element or feature described as "under other elements" or "under it" or "under it" will be oriented as being "above" the other elements or features. Thus, the exemplary terms "under" and "under" may include both upper and lower orientations. In addition, the device may also include additional orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptors used herein are interpreted accordingly.
[0031] Embodiments of the invention are described herein with reference to cross-sectional views that are schematic representations of idealized embodiments (and intermediate structures) of the present disclosure, such that variations in the shapes shown due to, for example, manufacturing techniques and / or tolerances are anticipated. Thus, embodiments of the present disclosure should not be limited to the specific shapes of the regions shown herein, but rather include deviations in shapes due to, for example, manufacturing techniques. Thus, the regions shown in the figures are schematic in nature, their shapes do not represent the actual shapes of the regions of the device, and do not limit the scope of the present disclosure.
[0032] As shown in FIG. 1 , in a conventional preparation process, after the first contact hole 60 and the second contact hole 70 are simultaneously formed, the etch stop layer 30 at the bottom of the first contact hole 60 is usually over-etched, causing the first contact hole 60 to extend to the top surface of the gate structure 20 , resulting in poor morphology of the first contact hole 60 .
[0033] Based on this, in order to solve the above problems, an embodiment of the present application provides a method for preparing a semiconductor structure and a semiconductor structure.
[0034] Please refer to FIG. 2 . The present application provides a method for preparing a semiconductor structure. The method for preparing a semiconductor structure includes the following steps.
[0035] Step S10, providing a substrate, on which a first target structure and a second target structure are formed, wherein a top surface of the first target structure is higher than a top surface of the second target structure;
[0036] Step S20, forming an etch stop layer, wherein the etch stop layer at least covers the outer surface of the first target structure and the top surface of the second target structure;
[0037] Step S30, forming a first oxide layer on a side surface of the etch stop layer away from the first target structure, wherein a top surface of the first oxide layer is flush with a top surface of the etch stop layer;
[0038] Step S40, forming a second oxide layer on the top surface of the first oxide layer;
[0039] Step S50, removing a portion of the first oxide layer and the second oxide layer to form a first contact hole and a second contact hole, wherein the first contact hole is located directly above the first target structure, and the second contact hole is located directly above the second target structure, and both the first contact hole and the second contact hole extend to the top surface of the etch stop layer.
[0040] In the method for preparing the semiconductor structure of the above embodiment, a first oxide layer is formed on the side surface of the etch stop layer away from the first target structure, and a second oxide layer is formed on the top surface of the first oxide layer; a portion of the first oxide layer and the second oxide layer is removed to form a first contact hole and a second contact hole. Since the first contact hole is located directly above the first target structure and the second contact hole is located directly above the second target structure, both the first contact hole and the second contact hole extend to the top surface of the etch stop layer, and it can be concluded that the depth of the second contact hole is greater than the depth of the first contact hole. In this way, since the top surface of the first oxide layer is flush with the top surface of the etch stop layer, when forming the first contact hole and the second contact hole, over-etching of the etch stop layer at the bottom of the first contact hole can be effectively avoided, thereby improving the morphology of the first contact hole and the second contact hole, so as to improve the yield of the semiconductor structure and increase the process window.
[0041] In some embodiments, the oxygen content in the first oxide layer ranges from 55% to 70%.
[0042] In some embodiments, an etching selectivity ratio of the first oxide layer to the etch stop layer is not less than 10:1.
[0043] In the method for preparing the semiconductor structure of the above embodiment, since the etching selectivity ratio between the first oxide layer and the etch stop layer is not less than 10:1, after forming the first contact hole, the first oxide layer can be continuously removed to form the second contact hole, thereby avoiding over-etching of the etch stop layer, thereby ensuring the integrity of the etch stop layer.
[0044] In some embodiments, step S30, forming a first oxide layer on a side surface of the etch stop layer away from the first target structure, comprises:
[0045] Step S31, forming an initial oxide layer on the etch stop layer;
[0046] Step S32, removing part of the initial oxide layer until the etching stop layer located on the top surface of the first target structure is exposed, and the remaining initial oxide layer constitutes a first oxide layer.
[0047] In some embodiments, the thickness of the initial oxide layer ranges from 1000 Å to 5000 Å.
[0048] In some embodiments, the second oxide layer has a thickness ranging from 1000 Å to 8000 Å.
[0049] In some embodiments, a one-time etching process is used to simultaneously remove a portion of the second oxide layer and the first oxide layer to form the first contact hole and the second contact hole.
[0050] In some embodiments, the first target structure includes a gate structure; and the second target structure includes doped regions located on both sides of the first target structure.
[0051] In the above embodiments of the present disclosure, unless otherwise specified herein, the execution of each step in the method is not strictly limited in order, and these steps may not necessarily be executed in the order described, and may be executed in other ways. Moreover, at least a part of any step may include multiple sub-steps or multiple stages, and these sub-steps or stages are not necessarily executed at the same time, but may be executed at different times, and the execution order of these sub-steps or stages is not necessarily sequential, but may be executed in turn or alternately with other steps or at least a part of the sub-steps or stages of other steps.
[0052] In order to more clearly illustrate the method for preparing the semiconductor structure provided in the above embodiment, the following is a method for preparing the semiconductor structure provided in the above embodiment in combination with FIG. Figure 6 The method is described in detail.
[0053] like Figure 3 As shown, in step S10, a substrate 10 is provided, on which a first target structure and a second target structure are formed, and a top surface of the first target structure is higher than a top surface of the second target structure.
[0054] As an example, in the embodiment of the present disclosure, the substrate 10 may be made of a semiconductor material, an insulating material, a conductor material, or any combination of their material types. The substrate 10 may be a single-layer structure or a multi-layer structure. For example, the substrate 10 may be a silicon (Si) substrate 10, a silicon germanium (SiGe) substrate 10, a silicon germanium carbon (SiGeC) substrate 10, a silicon carbide (SiC) substrate 10, a gallium arsenide (GaAs) substrate 10, an indium arsenide (InAs) substrate 10, an indium phosphide (InP) substrate 10, or other III / V semiconductor substrates 10 or II / VI semiconductor substrates 10. Alternatively, for example, the substrate 10 may be a layered substrate 10 including a stack of Si and SiGe, a stack of Si and SiC, a silicon on insulator (SOI), or a silicon germanium on an insulator. A person skilled in the art may select the type of substrate 10 according to the type of transistor formed on the substrate 10, so the type of substrate 10 should not limit the scope of protection of the present disclosure.
[0055] In some embodiments, the first target structure includes a gate structure 20 ; and the second target structure includes doping regions 12 located on both sides of the first target structure.
[0056] In some embodiments, the gate structure 20 includes a gate dielectric layer 22 , a gate conductive layer 21 , a gate electrode 23 , and gate spacers 24 located on sidewalls of the gate conductive layer 21 and the gate electrode 23 , which are sequentially stacked in a direction perpendicular to the substrate 10 .
[0057] In some embodiments, the doped region 12 is located in the substrate 10 , and a source / drain electrode 121 is formed on the top surface of the doped region 12 . The source / drain electrode 121 is located on both sides of the gate dielectric layer 22 .
[0058] In some embodiments, the substrate 10 further includes a well region 11, and the doping region 12 is located on the well region 11. By way of example, the well region 11 has a first doping type, and the doping region 12 has a second doping type, and the first doping type is opposite to the second doping type. By way of example, the doping type of the well region 11 is N-type, and the doping type of the doping region 12 is P-type. Alternatively, the doping type of the well region 11 is P-type, and the doping type of the doping region 12 is N-type.
[0059] In some embodiments, the substrate 10 includes at least two well regions 11, and the two well regions 11 have different doping types. The doping types of the doping regions 12 located on different well regions 11 are also different.
[0060] In an embodiment in which two well regions are included in the substrate, an isolation structure 13 is further formed between the two well regions 11 to achieve insulation between the two well regions 11. By way of example, the isolation structure 13 may be a single-layer structure or a multi-layer structure. In an embodiment in which the isolation structure 13 is a multi-layer structure, the isolation structure 13 includes a first isolation layer 131 and a second isolation layer 132. By way of example, the materials of the first isolation layer 131 and the second isolation layer 132 are different. For example, the first isolation layer 131 may be made of at least one material selected from silicon oxide, silicon nitride, and silicon oxynitride, and the second isolation layer 132 may be made of at least one material selected from silicon oxide, silicon nitride, and silicon oxynitride.
[0061] like Figure 3 As shown, in step S20, an etch stop layer 30 is formed, and the etch stop layer 30 at least covers the outer surface of the first target structure and the top surface of the second target structure.
[0062] In some embodiments, the etch stop layer 30 covers at least the outer surface of the gate structure 20 and the top surface of the source / drain electrode 121 .
[0063] Illustratively, the etch stop layer 30 includes a silicon nitride layer.
[0064] like Figure 3 to Figure 4 As shown, in step S30, a first oxide layer 40 is formed on the side surface of the etch stop layer 30 away from the first target structure, and the top surface of the first oxide layer 40 is flush with the top surface of the etch stop layer 30. For example, the first oxide layer 40 is formed on the side surface of the etch stop layer 30 away from the gate structure 20.
[0065] In some embodiments, the oxygen content of the first oxide layer 40 ranges from 55% to 70%. For example, the oxygen content of the first oxide layer 40 is 55%, 60%, 65% or 70%.
[0066] In the method for preparing the semiconductor structure of the above embodiment, since the oxygen content in the first oxide layer 40 ranges from 55% to 70%, the oxygen content in the first oxide layer 40 is relatively high, which is beneficial to improving the etching selectivity ratio between the first oxide layer 40 and the etching stop layer 30.
[0067] In some embodiments, the etching selectivity ratio of the first oxide layer 40 to the etch stop layer 30 is not less than 10: 1. For example, the etching selectivity ratio of the first oxide layer 40 to the etch stop layer 30 is 10: 1, 11: 1, or 12: 1.
[0068] In the method for preparing the semiconductor structure of the above-mentioned embodiment, since the etching selectivity ratio between the first oxide layer 40 and the etch stop layer 30 is not less than 10:1, after forming the first contact hole 60, the first oxide layer 40 can be continuously removed to form the second contact hole 70, thereby avoiding over-etching of the etch stop layer 30, thereby ensuring the integrity of the etch stop layer 30.
[0069] Illustratively, the first oxide layer 40 includes a silicon oxide layer.
[0070] In some embodiments, step S30 of forming a first oxide layer 40 on a side surface of the etch stop layer 30 away from the first target structure includes the following steps S31 and S32 .
[0071] Step S31: Figure 3 As shown, an initial oxide layer 41 is formed on the etch stop layer 30 .
[0072] For example, a sub-atmospheric chemical vapor deposition (SACVD) process may be used to form the initial oxide layer 41 on the etch stop layer 30. The SACVD process refers to a deposition process performed under conditions below atmospheric pressure, and the SACVD process can achieve higher film density and uniformity.
[0073] In some embodiments, the thickness of the initial oxide layer 41 ranges from 1000 Å to 5000 Å. For example, the thickness of the initial oxide layer 41 is 1000 Å, 2000 Å, 3000 Å, 4000 Å, or 5000 Å.
[0074] Step S32: Figure 4 As shown, a portion of the initial oxide layer 41 is removed until the etching stop layer 30 located on the top surface of the first target structure is exposed, and the remaining initial oxide layer 41 constitutes the first oxide layer 40 .
[0075] For example, in step S32 , a portion of the initial oxide layer 41 is removed until the etching stop layer 30 located on the top surface of the gate structure 20 is exposed.
[0076] For example, a planarization process (chemical mechanical polishing, CMP) may be used to remove a portion of the initial oxide layer 41 .
[0077] like Figure 5 As shown, in step S40 , a second oxide layer 50 is formed on the top surface of the first oxide layer 40 .
[0078] In some embodiments, the thickness of the second oxide layer 50 ranges from 1000A to 8000A. For example, the thickness of the second oxide layer 50 is 1000A, 2000A, 3000A, 4000A, 5000A, 6000A, 7000A or 8000A.
[0079] For example, the second oxide layer 50 may be formed on the top surface of the first oxide layer 40 by using processes such as chemical vapor deposition or physical vapor deposition (PVD). The chemical vapor deposition process may include one or more of atmospheric pressure chemical vapor deposition (APCVD), low pressure chemical vapor deposition (LPCVD) or plasma enhanced chemical vapor deposition (PECVD). For example, the second oxide layer 50 may be formed by using plasma enhanced chemical vapor deposition, which is performed by ionizing the film layer by glow discharge in a deposition chamber and then chemically reacting on the film layer to deposit and form the second oxide layer 50. The plasma enhanced chemical vapor deposition method can enhance the activity of chemical vapor reaction substances through plasma activation, increase the surface reaction rate, and significantly reduce the deposition temperature through high-energy ions.
[0080] For example, the second oxide layer 50 includes a silicon oxide layer. In an embodiment in which the first oxide layer 40 includes a silicon oxide layer, the content of oxygen in the first oxide layer 40 is greater than the content of oxygen in the second oxide layer 50; the etching selectivity ratio of the second oxide layer 50 to the etch stop layer 30 is less than the etching selectivity ratio of the first oxide layer 40 to the etch stop layer 30. For example, the etching selectivity ratio of the second oxide layer 50 to the etch stop layer 30 is 5:1.
[0081] like Figure 6 As shown, in step S50, a portion of the first oxide layer 40 and the second oxide layer 50 are removed to form a first contact hole 60 and a second contact hole 70. The first contact hole 60 is located directly above the first target structure, and the second contact hole 70 is located directly above the second target structure. The first contact hole 60 and the second contact hole 70 both extend to the top surface of the etch stop layer 30.
[0082] By way of example, the first contact hole 60 is located directly above the gate structure 20 , and the second contact hole 70 is located directly above the doped region 12 .
[0083] In some embodiments, the process may further include coating a photoresist material layer on the surface of the second oxide layer 50, and the photoresist material layer undergoes a series of steps such as exposure and development to form a patterned photoresist layer, wherein the patterned photoresist layer has an opening pattern that defines the position and shape of the first contact hole 60 and the second contact hole 70, and the photoresist may be a positive photoresist or a negative photoresist, and the development method may be a positive development or a negative development. In step S50, an etching process may be used to etch the first oxide layer 40 and the second oxide layer 50 using the patterned photoresist layer as a mask to form the first contact hole 60 and the second contact hole 70.
[0084] In some embodiments, a one-time etching process is used to simultaneously remove a portion of the second oxide layer 50 and the first oxide layer 40 to form the first contact hole 60 and the second contact hole 70 .
[0085] It should be added that the "one-time etching process" mentioned in some embodiments of the present disclosure can be understood as: etching based on the pattern of the same mask plate at the same time to form multiple patterns in one etching process; it is not limited to a specific etching method, for example, it can be implemented by dry etching, it can be implemented by wet etching, or it can be implemented by both dry etching and wet etching, etc.
[0086] In the method for preparing the semiconductor structure of the above embodiment, a first oxide layer 40 is formed on the side surface of the etch stop layer 30 away from the gate structure 20, and a second oxide layer 50 is formed on the top surface of the first oxide layer 40; a portion of the first oxide layer 40 and the second oxide layer 50 are removed to form a first contact hole 60 and a second contact hole 70. Since the first contact hole 60 is located directly above the gate structure 20, and the second contact hole 70 is located directly above the doping region 12, the first contact hole 60 and the second contact hole 70 both extend to the top surface of the etch stop layer 30, and it can be concluded that the depth of the second contact hole 70 is greater than the depth of the first contact hole 60. In this way, since the top surface of the first oxide layer 40 is flush with the top surface of the etch stop layer 30, when forming the first contact hole 60 and the second contact hole 70, over-etching of the etch stop layer 30 at the bottom of the first contact hole 60 can be effectively avoided, thereby improving the morphology of the first contact hole 60 and the second contact hole 70, so as to improve the yield of the semiconductor structure and increase the process window.
[0087] According to some embodiments, the present application also provides a semiconductor structure, including a substrate 10, an etch stop layer 30, a first oxide layer 40, a second oxide layer 50, a first contact hole 60 and a second contact hole 70; a first target structure is formed on the substrate 10, and a second target structure located on both sides of the first target structure is also formed in the substrate 10; the etch stop layer 30 at least covers the outer surface of the first target structure and the top surface of the second target structure; the first oxide layer 40 is located on the side surface of the etch stop layer 30 away from the first target structure, and the top surface of the first oxide layer 40 is flush with the top surface of the etch stop layer 30; the second oxide layer 50 is located on the top surface of the first oxide layer 40; the first contact hole 60 and the second contact hole 70, the first contact hole 60 is located directly above the first target structure, the second contact hole 70 is located directly above the second target structure, and the bottom surface of the first contact hole 60 and the bottom surface of the second contact hole 70 both expose a portion of the top surface of the etch stop layer 30.
[0088] In the semiconductor structure of the above embodiment, the first contact hole 60 is located directly above the first target structure, and the second contact hole 70 is located directly above the second target structure. The bottom surface of the first contact hole 60 and the bottom surface of the second contact hole 70 both expose part of the top surface of the etching stop layer 30, which can improve the morphology of the first contact hole 60 and the second contact hole 70, thereby improving the yield of the semiconductor structure and increasing the process window.
[0089] In some embodiments, the first target structure includes a gate structure 20 ; and the second target structure includes doped regions 12 located on both sides of the gate structure 20 .
[0090] In some embodiments, the oxygen content of the first oxide layer 40 ranges from 55% to 70%. For example, the oxygen content of the first oxide layer 40 is 55%, 60%, 65% or 70%.
[0091] In some embodiments, the etching selectivity ratio of the first oxide layer 40 to the etch stop layer 30 is not less than 10: 1. For example, the etching selectivity ratio of the first oxide layer 40 to the etch stop layer 30 is 10: 1, 11: 1, or 12: 1.
[0092] In some embodiments, the thickness of the second oxide layer 50 ranges from 1000A to 8000A. For example, the thickness of the second oxide layer 50 is 1000A, 2000A, 3000A, 4000A, 5000A, 6000A, 7000A or 8000A.
[0093] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0094] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A method for preparing a semiconductor structure, characterized in that: include: Providing a substrate, on which a first target structure and a second target structure are formed, wherein a top surface of the first target structure is higher than a top surface of the second target structure; forming an etch stop layer, wherein the etch stop layer at least covers an outer surface of the first target structure and a top surface of the second target structure; forming a first oxide layer on a side surface of the etch stop layer away from the first target structure, wherein a top surface of the first oxide layer is flush with a top surface of the etch stop layer; forming a second oxide layer on a top surface of the first oxide layer; Portions of the first oxide layer and the second oxide layer are removed to form a first contact hole and a second contact hole, wherein the first contact hole is located directly above the first target structure, and the second contact hole is located directly above the second target structure, and both the first contact hole and the second contact hole extend to the top surface of the etch stop layer.
2. The method for preparing a semiconductor structure according to claim 1, characterized in that: The content of oxygen in the first oxide layer ranges from 55% to 70%.
3. The method for preparing a semiconductor structure according to claim 1 or 2, characterized in that: An etching selectivity ratio of the first oxide layer to the etch stop layer is not less than 10:
1.
4. The method for preparing a semiconductor structure according to claim 1, characterized in that: The step of forming a first oxide layer on a side surface of the etch stop layer away from the first target structure comprises: forming an initial oxide layer on the etch stop layer; A portion of the initial oxide layer is removed until the etch stop layer located on the top surface of the first target structure is exposed, and the remaining initial oxide layer constitutes the first oxide layer.
5. The method for preparing a semiconductor structure according to claim 4, characterized in that: The thickness of the initial oxide layer ranges from 1000 Å to 5000 Å.
6. The method for preparing a semiconductor structure according to claim 1, characterized in that: The thickness of the second oxide layer ranges from 1000 Å to 8000 Å.
7. The method for preparing a semiconductor structure according to claim 1, characterized in that: A one-time etching process is adopted to simultaneously remove a portion of the second oxide layer and the first oxide layer to form the first contact hole and the second contact hole.
8. The method for preparing a semiconductor structure according to claim 1, characterized in that: The first target structure comprises a gate structure; The second target structure includes doped regions located on both sides of the first target structure.
9. A semiconductor structure, characterized in that: include: A substrate, wherein a first target structure is formed on the substrate, and second target structures are also formed in the substrate and are located on both sides of the first target structure; an etch stop layer, covering at least an outer surface of the first target structure and a top surface of the second target structure; A first oxide layer is located on a side surface of the etch stop layer away from the first target structure, and a top surface of the first oxide layer is flush with a top surface of the etch stop layer; a second oxide layer, located on a top surface of the first oxide layer; A first contact hole and a second contact hole, the first contact hole is located directly above the first target structure, the second contact hole is located directly above the second target structure, and the bottom surfaces of the first contact hole and the second contact hole both expose a portion of the top surface of the etching stop layer.
10. The semiconductor structure according to claim 9, characterized in that: The first target structure comprises a gate structure; The second target structure includes doped regions located on both sides of the gate structure.
Citation Information
Cited By
Preparation method of semiconductor structure and semiconductor structure
CN120730762A
Method for manufacturing a semiconductor structure and semiconductor structure
CN120730762B