Perovskite four-terminal laminated assembly and preparation method thereof

By using transparent PET and POE materials to form a composite insulating adhesive film layer in a perovskite four-terminal module, the problem of insufficient temperature resistance of the adhesive film is solved, the laying process is simplified and the product defect rate is reduced, achieving more efficient module production. .

CN118765150APending Publication Date: 2024-10-11TRINA SOLAR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410950943.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-16
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

In the packaging structure of the existing perovskite four-terminal module, the temperature resistance of the adhesive film is insufficient, which leads to the need to add multiple layers of adhesive films and insulation layers, which increases the difficulty of laying and production complexity, and easily forms bubbles, resulting in product defective rates. high.

Method used

A method of preparing a perovskite four-terminal laminated assembly is adopted, by depositing a perovskite power generation layer on an FTO glass substrate, and setting electrode structures on both ends, using transparent PET as an insulating layer, and coating it with fluorocarbon materials As a transparent coating, it forms a composite insulation film layer, reducing the difficulty of laying the insulation film and glue film.

Benefits of technology

It effectively reduces the difficulty of laying insulating films and adhesive films, simplifies the production process, reduces product defect rates, and improves the temperature resistance of components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118765150A_ABST
    Figure CN118765150A_ABST
Patent Text Reader

Abstract

The invention provides a perovskite four-terminal laminated assembly and a preparation method thereof. The preparation method of the perovskite four-end laminated assembly comprises the following steps that a substrate with a perovskite power generation layer is prepared, and electrode structures are arranged at the two ends of the perovskite power generation layer respectively; the first surface of a composite insulating adhesive film layer provided with a plurality of first electrode bus bars in a penetrating mode is laid on the perovskite power generation layer, the first electrode bus bars are connected to the corresponding electrode structures respectively, and an insulating layer and adhesive film layers attached to the two surfaces of the insulating layer are integrated in the composite insulating adhesive film layer; and laying a crystalline silicon cell layer on the second surface of the composite insulating adhesive film layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of new energy technology, and in particular to a method for preparing a perovskite four-terminal stacked component, and a perovskite four-terminal stacked component. Background Art

[0002] Perovskite solar cells use organic-inorganic hybrid metal halides with perovskite crystal structures as light-absorbing layers. The theoretical maximum conversion efficiency of single-junction perovskite cells is 31%, while the theoretical efficiency of multi-junction cells can reach 45%. In addition, compared with the processes of crystalline silicon cells and second-generation GaAs thin-film solar cells, perovskites require less investment to achieve the same production capacity, and the preparation of precursor solutions does not involve any complex processes.

[0003] In the packaging structure of early four-terminal components, a film was used as an insulating material between the perovskite and the crystalline silicon inside the component. Since the temperature resistance of the film is only 80℃~90℃, a layer of film and an insulating layer are usually added to the structure to improve the temperature resistance of the film. However, in the preparation process of this structure, three layers of film and one insulating layer need to be laid as a whole. Not only is the laying difficult and the production process complicated, but it is also very easy to cause dimensional deviations, forming bubbles between the butyl rubber used for packaging and its adjacent structures, resulting in a generally high product defect rate.

[0004] In order to overcome the above-mentioned defects of the prior art, the art is in urgent need of a perovskite four-terminal stacked component technology to reduce the difficulty of laying the insulating film and the adhesive film, thereby reducing the production complexity and product defect rate. Summary of the invention

[0005] A brief summary of one or more aspects is given below to provide a basic understanding of these aspects. This summary is not an exhaustive overview of all conceived aspects, and is neither intended to identify the key or decisive elements of all aspects nor to define the scope of any or all aspects. Its only purpose is to give some concepts of one or more aspects in a simplified form as a prelude to a more detailed description that will be given later.

[0006] In order to overcome the above-mentioned defects of the prior art, the present invention provides a method for preparing a perovskite four-terminal stacked component, and a perovskite four-terminal stacked component, which are used to reduce the difficulty of laying an insulating film and an adhesive film, thereby reducing production complexity and product defective rate.

[0007] Specifically, the preparation method of the perovskite four-terminal stacked component provided according to the first aspect of the present invention includes the following steps: preparing a substrate with a perovskite power generation layer, wherein electrode structures are respectively provided at both ends of the perovskite power generation layer; laying the first surface of a composite insulating film layer having a plurality of first electrode bus bars on the perovskite power generation layer, and connecting each of the first electrode bus bars to the corresponding electrode structure, wherein the composite insulating film layer integrates an insulating layer and film layers respectively attached to the two surfaces of the insulating layer; and laying a crystalline silicon battery layer on the second surface of the composite insulating film layer.

[0008] Furthermore, in some embodiments of the present invention, the substrate is FTO glass, and the step of preparing the substrate with a perovskite power generation layer includes: preparing a FTO glass substrate; depositing the perovskite power generation layer on the first surface of the FTO glass substrate; and respectively arranging electrode structures at both ends of the perovskite power generation layer.

[0009] Furthermore, in some embodiments of the present invention, the insulating layer is selected from at least one of transparent PET, transparent polyolefin materials, transparent polyester materials, transparent olefin copolymer materials, transparent fluororesin materials, and transparent polyamide materials, and the adhesive film layer is selected from POE material.

[0010] Furthermore, in some embodiments of the present invention, the insulating layer is made of transparent PET, and the step of integrating the composite insulating film layer includes: preparing the insulating layer; applying a transparent coating on the first surface and the second surface of the insulating layer, wherein the transparent coating is selected from at least one of fluorocarbon materials, acrylic materials, epoxy materials, and polyester materials; applying the POE material to the transparent coatings on each surface of the insulating layer to form corresponding film layers on each transparent coating; and passing the multiple first electrode bus bars through the target positions corresponding to each electrode structure on the composite insulating film layer.

[0011] Furthermore, in some embodiments of the present invention, the step of applying a transparent coating to the first surface and the second surface of the insulating layer includes: performing a first coating process on the first surface of the unrolled insulating layer to coat the first surface with a transparent coating material; performing a first baking process on the first surface coated with the transparent coating material to generate a first transparent coating on the first surface; performing a second coating process on the second surface of the unrolled insulating layer to coat the transparent coating material on the second surface; performing a second baking process on the second surface coated with the transparent coating material to generate a second transparent coating on the second surface; and winding up the insulating layer with the first transparent coating and the second transparent coating.

[0012] Furthermore, in some embodiments of the present invention, the step of respectively applying the POE material to the transparent coating layers on each of the surfaces of the insulating layer to form corresponding adhesive film layers on each of the transparent coating layers includes: performing a first lamination process on the first transparent coating layer on the first surface of the unwound insulating layer, and performing a second lamination process on the second transparent coating layer on the second surface of the insulating layer, so as to respectively apply the POE material to the surfaces of the first transparent coating layer and the second transparent coating layer and form corresponding adhesive film layers thereon; and rolling up the composite insulating adhesive film having the adhesive film layers on the first surface and the second surface, respectively.

[0013] Furthermore, in some embodiments of the present invention, the baking temperature of the first baking process and / or the second baking process is 50°C to 300°C, and the baking time is 1 min to 60 min. The screw temperature of the film extrusion process of the first coating process and / or the second coating process is 50°C to 80°C, and the die temperature is 90°C to 110°C.

[0014] Furthermore, in some embodiments of the present invention, the thickness of the insulating layer is 30 μm to 200 μm, the thickness of the transparent coating is 1 μm to 20 μm, and the surface density of the adhesive film layer is 100 g / m 2 ~250g / m 2 .

[0015] Furthermore, in some embodiments of the present invention, the step of laying the crystalline silicon cell layer on the second surface of the composite insulating film layer includes: laying the first surface of the crystalline silicon cell layer on the second surface of the composite insulating film layer; laying the first surface of the second film having a plurality of second electrode bus bars on the second surface of the crystalline silicon cell layer, and connecting the plurality of second electrode bus bars to the corresponding first electrode bus bars respectively; and pasting tempered glass to the second surface of the second film.

[0016] Furthermore, in some embodiments of the present invention, after laying the crystalline silicon cell layer on the second surface of the composite insulating film layer, the preparation method also includes the following steps: laminating the perovskite four-terminal stacked components laid layer by layer; trimming and installing a frame on the laminated perovskite four-terminal stacked components; and installing a junction box on the perovskite four-terminal stacked components provided with a frame, and performing assembly line transmission, curing and component cleaning on the components.

[0017] In addition, the perovskite four-terminal stacked component provided according to the second aspect of the present invention is prepared by the preparation method of the perovskite four-terminal stacked component as described in any one of the first aspect of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] The above features and advantages of the present invention can be better understood after reading the detailed description of the embodiments of the present disclosure in conjunction with the following drawings. In the drawings, the components are not necessarily drawn to scale, and components with similar related properties or features may have the same or similar reference numerals.

[0019] Figure 1 A schematic flow chart of a method for preparing a composite insulating adhesive film layer of a four-terminal laminated assembly according to some embodiments of the present invention is shown.

[0020] Figure 2 A schematic diagram of the overall structure of a composite insulating adhesive film layer of a four-terminal stacked assembly provided according to some embodiments of the present invention is shown.

[0021] Figure 3 A schematic diagram of the exploded structure of a composite insulating film layer of a four-terminal stacked assembly provided according to some embodiments of the present invention is shown.

[0022] Figure 4 A schematic diagram of a process for coating a transparent coating on an insulating layer according to some embodiments of the present invention is shown.

[0023] Figure 5 A schematic diagram of a process for coating an adhesive film layer on a transparent coating layer according to some embodiments of the present invention is shown.

[0024] Figure 6 A schematic diagram of the preparation process of a composite insulating adhesive film layer of a four-terminal laminated assembly provided according to some embodiments of the present invention is shown.

[0025] Reference numerals:

[0026] 10 Base

[0027] 20 Perovskite power generation layer

[0028] 21 Electrode

[0029] 30 Composite insulation film layer

[0030] 31 Insulation layer

[0031] 311 Clear Coat

[0032] 32 film layer

[0033] 33, 34 Electrode busbar

[0034] 35 Hot drying tunnel

[0035] 36 Die Head

[0036] 37 Screw

[0037] 40 Crystalline silicon cells

[0038] 50 Second film

[0039] 60 Tempered glass

[0040] 70 Junction Box

[0041] 80 Butyl rubber

[0042] S1 Step 1

[0043] S2 Step 2

[0044] S3 Step 3 DETAILED DESCRIPTION

[0045] The following specific embodiments illustrate the implementation of the present invention, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. Although the description of the present invention will be introduced in conjunction with the preferred embodiment, this does not mean that the features of this invention are limited to this implementation. On the contrary, the purpose of introducing the invention in conjunction with the implementation is to cover other options or modifications that may be extended based on the claims of the present invention. In order to provide a deep understanding of the present invention, the following description will include many specific details. The present invention can also be implemented without using these details. In addition, in order to avoid confusion or blurring the focus of the present invention, some specific details will be omitted in the description.

[0046] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0047] In addition, the terms "upper", "lower", "left", "right", "top", "bottom", "horizontal" and "vertical" used in the following description should be understood as the directions shown in the paragraph and the related drawings. Such relative terms are only used for the convenience of description and do not mean that the device described therein must be manufactured or operated in a specific direction, and therefore should not be understood as limiting the present invention.

[0048] It is understood that although the terms "first", "second", "third", etc. may be used herein to describe various components, regions, layers and / or parts, these components, regions, layers and / or parts should not be limited by these terms, and these terms are only used to distinguish different components, regions, layers and / or parts. Therefore, the first component, region, layer and / or part discussed below may be referred to as a second component, region, layer and / or part without departing from some embodiments of the present invention.

[0049] As mentioned above, in the packaging structure of the early four-terminal components, a film was used as an insulating material between the perovskite and the crystalline silicon inside the component. Since the temperature resistance of the film is only 80-90°C, a layer of film and an insulating layer are usually added to the structure to improve the temperature resistance of the film. However, in the preparation process of this structure, three layers of film and one insulating layer need to be laid as a whole. Not only is the laying difficult and the production process complicated, but it is also very easy to cause dimensional deviations, forming bubbles between the butyl rubber used for packaging and its adjacent structures, resulting in a generally high product defect rate.

[0050] In order to overcome the above-mentioned defects of the prior art, the present invention provides a method for preparing a perovskite four-terminal stacked component, and a perovskite four-terminal stacked component, which are used to reduce the difficulty of laying an insulating film and an adhesive film, thereby reducing production complexity and product defective rate.

[0051] In some non-limiting embodiments, the method for preparing the perovskite four-terminal stacked assembly provided in the first aspect of the present invention can be implemented based on the perovskite four-terminal stacked assembly provided in the second aspect of the present invention. That is, the perovskite four-terminal stacked assembly is prepared by the method for preparing the perovskite four-terminal stacked assembly provided in the first aspect of the present invention.

[0052] The following will describe the preparation principle of the above-mentioned perovskite four-terminal stacked assembly in conjunction with some embodiments of the preparation method of the perovskite four-terminal stacked assembly. Those skilled in the art will understand that these embodiments of the preparation method of the perovskite four-terminal stacked assembly are only some non-restrictive implementation methods provided by the present invention, which are intended to clearly demonstrate the main concept of the present invention and provide some specific schemes that are convenient for the public to implement, rather than to limit all functions or all working modes of the perovskite four-terminal stacked assembly. Similarly, the preparation method of the perovskite four-terminal stacked assembly is also only some non-restrictive implementation methods provided by the present invention, and does not constitute a limitation on the execution subject or execution order of each step of these perovskite four-terminal stacked assemblies.

[0053] Please refer to Figure 1-2 , Figure 1 A schematic flow chart of a method for preparing a composite insulating adhesive film layer of a four-terminal laminated assembly according to some embodiments of the present invention is shown. Figure 2A schematic diagram of the overall structure of a composite insulating adhesive film layer of a four-terminal stacked assembly provided according to some embodiments of the present invention is shown.

[0054] like Figure 1-2 As shown, the method for preparing the perovskite four-terminal stacked component can first perform step one S1: preparing a substrate 10 with a perovskite power generation layer 20, wherein the two ends of the perovskite power generation layer 20 are respectively provided with an electrode 21 structure.

[0055] Specifically, FTO glass can be used as the substrate 10. After the FTO glass substrate 10 is prepared, the perovskite power generation layer 20 is deposited on the first surface of the FTO glass substrate 10, and then the electrode 21 structure is respectively arranged at both ends of the perovskite power generation layer 20. Here, the process of the substrate 10 with the perovskite power generation layer 20 does not involve the technical improvement of the present invention, and will not be repeated here.

[0056] Afterwards, the preparation method of the perovskite four-terminal stacked component can first perform step two S2: laying the first surface of the composite insulating film layer 30 with multiple first electrode bus bars 33 on the perovskite power generation layer 20, and connecting each first electrode bus bar 33 to the corresponding electrode 21 structure respectively.

[0057] Please refer to Figure 3 , Figure 3 A schematic diagram of the exploded structure of a composite insulating film layer of a four-terminal stacked assembly provided according to some embodiments of the present invention is shown.

[0058] like Figure 3 As shown, the composite insulating film layer 30 integrates an insulating layer 31 and film layers 32 respectively attached to the two surfaces of the insulating layer 31. Preferably, the insulating layer 31 can be made of transparent PET, and the film layer 32 can be made of POE material. Optionally, the insulating layer 31 is made of at least one of transparent polyolefin materials, transparent polyester materials, transparent olefin copolymer materials, transparent fluororesin materials, and transparent polyamide materials. Here, the thickness of the insulating layer 31 is 30μm to 200μm.

[0059] Specifically, the preparation method of the perovskite four-terminal stacked component can first apply a transparent coating 311 to the first surface and the second surface of the pre-prepared insulating layer 31. Here, the transparent coating 311 is selected from at least one of fluorocarbon materials, acrylic materials, epoxy materials, and polyester materials. The thickness of the transparent coating 311 is 1 μm to 20 μm, and the surface density of the adhesive film layer 32 is 100 g / m 2 ~250g / m 2 .

[0060] Please refer to Figure 4 , Figure 4A schematic diagram of a process for coating a transparent coating on an insulating layer according to some embodiments of the present invention is shown.

[0061] like Figure 4 As shown, the step of coating the transparent coating 311 on the first surface and the second surface of the insulating layer 31 includes: performing a first coating process on the first surface of the unwound insulating layer 31 to coat the transparent coating 311 material on the first surface; performing a first baking process on the first surface coated with the transparent coating 311 material via a hot drying tunnel 35 to generate the first transparent coating 311 on the first surface; performing a second coating process on the second surface of the unwound insulating layer 31 to coat the transparent coating 311 material on the second surface; performing a second baking process on the second surface coated with the transparent coating 311 material via a hot drying tunnel 35 to generate the second transparent coating 311 on the second surface; and winding up the insulating layer 31 with the first transparent coating 311 and the second transparent coating 311. Here, the baking temperature of the first baking process and / or the second baking process is 50°C to 300°C, and the baking time is 1min to 60min.

[0062] Furthermore, the method for preparing the perovskite four-terminal stacked component can coat the POE material on the transparent coating layer 311 on each surface of the insulating layer 31 to form a corresponding adhesive film layer 32 on each transparent coating layer 311 .

[0063] Please refer to Figure 5 , Figure 5 A schematic diagram of a process for coating an adhesive film layer on a transparent coating layer according to some embodiments of the present invention is shown.

[0064] like Figure 5 As shown, a first coating process is performed on the first transparent coating layer 311 on the first surface of the unwound insulating layer 31, and a second coating process is performed on the second transparent coating layer 311 on the second surface of the insulating layer 31, so that the POE material is coated on the surfaces of the first transparent coating layer 311 and the second transparent coating layer 311, respectively, and corresponding adhesive film layers 32 are formed thereon. Finally, the composite insulating adhesive film with the adhesive film layers 32 on the first surface and the second surface, respectively, is rolled up.

[0065] Here, in the film extrusion process of the first laminating process and / or the second laminating process, the temperature of the screw 37 is 50°C to 80°C, and the temperature of the die head 36 is 90°C to 110°C.

[0066] Furthermore, after the transparent coating 311 is applied to the first surface and the second surface of the pre-prepared insulating layer 31, and the POE material is respectively applied to the transparent coating 311 on each surface of the insulating layer 31, a plurality of first electrode bus bars 33 are respectively passed through the target positions corresponding to each electrode 21 structure on the composite insulating film layer 30.

[0067] Please continue to refer to Figure 1 After the first surface of the composite insulating film layer 30 having a plurality of first electrode bus bars 33 is laid on the perovskite power generation layer 20, and each first electrode bus bar 33 is respectively connected to the corresponding electrode 21 structure, the preparation method of the perovskite four-terminal stacked component can execute step three S3: laying a layer of crystalline silicon cells 40 on the second surface of the composite insulating film layer 30.

[0068] Specifically, the battery string is first welded and EL detection is performed to form a crystalline silicon battery layer 40. The preparation method can lay the first surface of the crystalline silicon battery layer 40 on the second surface of the composite insulating film layer 30; lay the first surface of the second adhesive film 50 with multiple second electrode bus bars 34 on the second surface of the crystalline silicon battery layer 40, and connect the multiple second electrode bus bars 34 to the corresponding first electrode bus bars 33 respectively; and adhere the tempered glass 60 to the second surface of the second adhesive film 50.

[0069] Please refer to Figure 6 , Figure 6 A schematic diagram of the preparation process of a composite insulating adhesive film layer of a four-terminal laminated assembly provided according to some embodiments of the present invention is shown.

[0070] like Figure 6 As shown, after laying 40 layers of crystalline silicon cells on the second surface of the composite insulating film layer 30, the preparation method also includes the following steps: laminating the layered perovskite four-terminal stacked components; using butyl adhesive 80 to trim and install the frame of the laminated perovskite four-terminal stacked components; and installing the junction box 70 on the perovskite four-terminal stacked components with a frame, and performing assembly line transmission, curing and component cleaning.

[0071] Furthermore, the cleaned components are subjected to electroluminescence defect (EL) detection, IV test & safety test, and then the components are sorted and packaged for storage, thus completing the entire preparation process of the perovskite four-terminal stacked components.

[0072] Those skilled in the art can understand that the solution of pre-piercing the first electrode busbar and the second electrode busbar into the adhesive film provided in this specification is only a preferred implementation method provided in this embodiment. Optionally, the busbar can also be perforated during the processing to achieve the same technical effect.

[0073] In summary, the preparation method of the perovskite four-terminal stacked component and the perovskite four-terminal stacked component provided by the present invention utilize a composite insulating layer to connect the perovskite power generation layer and the crystalline silicon battery layer, which effectively reduces the difficulty of laying the insulating film and the adhesive film, thereby reducing the production complexity and product defective rate.

[0074] Although the above methods are illustrated and described as a series of actions for simplicity of explanation, it should be understood and appreciated that these methods are not limited by the order of the actions, because according to one or more embodiments, some actions may occur in a different order and / or concurrently with other actions from those illustrated and described herein or not illustrated and described herein but understandable to those skilled in the art.

[0075] The previous description of the disclosure is provided to enable any person skilled in the art to make or use the disclosure. Various modifications to the disclosure will be apparent to those skilled in the art, and the general principles defined herein may be applied to other variations without departing from the spirit or scope of the disclosure. Thus, the disclosure is not intended to be limited to the examples and designs described herein, but should be granted the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A method for preparing a perovskite four-terminal stacked component, characterized in that: The following steps are involved: Preparing a substrate with a perovskite power generation layer, wherein both ends of the perovskite power generation layer are provided with electrode structures; Laying the first surface of the composite insulating adhesive film layer having a plurality of first electrode bus bars on the perovskite power generation layer, and connecting each of the first electrode bus bars to the corresponding electrode structure, wherein the composite insulating adhesive film layer integrates an insulating layer and adhesive film layers respectively attached to two surfaces of the insulating layer; and Laying the crystalline silicon cell layer on the second surface of the composite insulating adhesive film layer.

2. The preparation method according to claim 1, characterized in that The substrate is selected from FTO glass, and the step of preparing the substrate with the perovskite power generation layer comprises: Prepare FTO glass substrate; Depositing the perovskite power generation layer on the first surface of the FTO glass substrate; and Electrode structures are respectively arranged at both ends of the perovskite power generation layer.

3. The preparation method according to claim 1, characterized in that: The insulating layer is selected from at least one of transparent PET, transparent polyolefin materials, transparent polyester materials, transparent olefin copolymer materials, transparent fluororesin materials, and transparent polyamide materials, and the adhesive film layer is selected from POE material.

4. The preparation method according to claim 3, characterized in that: The insulating layer is made of transparent PET, and the steps of integrating the composite insulating film layer include: preparing the insulating layer; Applying a transparent coating on the first surface and the second surface of the insulating layer, wherein the transparent coating is selected from at least one of fluorocarbon materials, acrylic materials, epoxy materials, and polyester materials; Applying the POE material to the transparent coating layers on the surfaces of the insulating layer to form corresponding adhesive film layers on the transparent coating layers; and The plurality of first electrode bus bars are respectively passed through target positions corresponding to the electrode structures on the composite insulating adhesive film layer.

5. The preparation method according to claim 4, characterized in that: The step of applying a transparent coating to the first surface and the second surface of the insulating layer comprises: Performing a first coating process on a first surface of the unwound insulation layer to coat the first surface with a transparent coating material; Performing a first baking process on the first surface coated with the transparent coating material to generate a first transparent coating on the first surface; Performing a second coating process on the second surface of the unwound insulating layer to coat the second surface with the transparent coating material; performing a second baking process on the second surface coated with the transparent coating material to generate a second transparent coating on the second surface; and The insulating layer with the first transparent coating layer and the second transparent coating layer is rolled up.

6. The preparation method according to claim 5, characterized in that: The step of applying the POE material to the transparent coating layers on the surfaces of the insulating layer to form corresponding adhesive film layers on the transparent coating layers comprises: Performing a first laminating process on the first transparent coating layer on the first surface of the unwound insulating layer, and performing a second laminating process on the second transparent coating layer on the second surface of the insulating layer, so as to apply the POE material to the surfaces of the first transparent coating layer and the second transparent coating layer, respectively, and form corresponding adhesive film layers thereon; and The composite insulating adhesive film having the adhesive film layers on the first surface and the second surface is rolled up.

7. The preparation method according to claim 6, characterized in that: The baking temperature of the first baking process and / or the second baking process is 50℃~300℃, and the baking time is 1min~60min. The screw temperature of the film extrusion process of the first coating process and / or the second coating process is 50℃~80℃, and the die head temperature is 90℃~110℃.

8. The preparation method according to claim 4, characterized in that: The thickness of the insulating layer is 30 μm to 200 μm, the thickness of the transparent coating is 1 μm to 20 μm, and the surface density of the adhesive film layer is 100 g / m 2 ~250g / m 2 .

9. The preparation method according to claim 1, characterized in that: The step of laying the crystalline silicon cell layer on the second surface of the composite insulating film layer comprises: Laying the first surface of the crystalline silicon cell layer on the second surface of the composite insulating film layer; Laying the first surface of the second adhesive film having a plurality of second electrode bus bars on the second surface of the crystalline silicon cell layer, and connecting the plurality of second electrode bus bars to the corresponding first electrode bus bars respectively; and The tempered glass is adhered to the second surface of the second adhesive film.

10. The preparation method according to claim 1, characterized in that: After laying the crystalline silicon cell layer on the second surface of the composite insulating film layer, the preparation method further comprises the following steps: Laminating the perovskite four-terminal stacked components laid layer by layer; Trimming and framing the laminated perovskite four-terminal stacked assembly; and The junction box is installed on the perovskite four-terminal stacked component with a frame, and is subjected to pipeline transmission, curing and component cleaning.

11. A perovskite four-terminal stacked component, characterized in that: The perovskite four-terminal stacked component is prepared by the preparation method of the perovskite four-terminal stacked component according to any one of claims 1 to 10.