A quality inspection system for functional gradient material preparation process

By using a combination of piezoelectric ceramics and AC power supply in the preparation of functional gradient materials, using impedance data to detect the natural frequency and stiffness of the hot-pressed laminate, the problem of strong destructive quality detection in the prior art is solved, and lossless , efficient quality inspection ensures the preparation quality of the material.

CN118777426BActive Publication Date: 2024-11-22CIVIL AVIATION FLIGHT UNIV OF CHINA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411275635.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-12
Publication Date
2024-11-22
Estimated Expiration
2044-09-12

AI Technical Summary

Technical Problem

During the preparation of functional gradient materials, quality problems of multiple plates will lead to poor quality of the final material. The existing detection system may destroy the hot-pressed laminate and cannot achieve non-destructive testing.

Method used

Using a quality detection system including a detection platform, detection device and robotic arms, the natural frequency and stiffness of the hot-pressed laminate is determined by combining piezoelectric ceramics with AC power and impedance collectors, using frequency adjustable AC and impedance data. Realize non-destructive quality inspection.

Benefits of technology

Non-destructive quality detection during the preparation of functional gradient materials is realized, which avoids material failure caused by quality problems and improves the reliability of material preparation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118777426B_ABST
    Figure CN118777426B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of functional gradient materials, and in particular to a quality detection system in the process of preparing functional gradient materials. An embodiment of the present invention provides a quality detection system in the process of preparing functional gradient materials, comprising a detection platform, a detection device and a robotic arm; the detection device comprises an AC power supply, a piezoelectric ceramic and an impedance collector, the piezoelectric ceramic is connected to the hot-pressed layered body to be detected on the detection platform, the piezoelectric ceramic is also respectively connected to the AC power supply and the impedance collector, and the robotic arm is used to move the hot-pressed layered body to be detected to the detection platform; wherein the hot-pressed layered body is a plate body with multiple components and structural gradient changes prepared by a first hot pressing sintering. An embodiment of the present invention provides a quality detection system in the process of preparing functional gradient materials, which can provide a system for detecting quality in the process of preparing functional gradient materials.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of functional gradient materials, and in particular to a quality detection system in the preparation process of functional gradient materials. Background Art

[0002] Functionally gradient materials are an important material used in the aerospace field. They can simultaneously possess two different properties, such as hardness and toughness.

[0003] In the prior art, in the preparation method of functional gradient materials, a plurality of plates with different microstructures and compositions are first prepared, and then the plurality of plates are synthesized to obtain the functional gradient material. However, if any one or more of the plurality of plates have quality problems, the quality of the functional gradient material obtained will be poor.

[0004] Therefore, a system is needed that can detect the quality during the preparation process. Summary of the invention

[0005] An embodiment of the present invention provides a quality detection system during the preparation process of a functional gradient material, which can provide a system for detecting quality during the preparation process of a functional gradient material.

[0006] An embodiment of the present invention provides a quality detection system in a functional gradient material preparation process, including a detection platform, a detection device and a mechanical arm;

[0007] The detection device includes an AC power supply, a piezoelectric ceramic and an impedance collector, wherein the piezoelectric ceramic is connected to the hot-pressed layered body to be detected on the detection platform, and the piezoelectric ceramic is also connected to the AC power supply and the impedance collector respectively, and the mechanical arm is used to move the hot-pressed layered body to be detected to the detection platform; wherein the hot-pressed layered body is a plate body prepared by a first hot-pressing sintering, having multiple components and having a structural gradient change;

[0008] When performing quality inspection, the AC power supply is used to apply frequency-adjustable AC power to the piezoelectric ceramic, the frequency of the AC power is adjusted, and the impedance collector is used to collect impedance data of the piezoelectric ceramic at different frequencies in real time. The frequency of the AC power when the impedance is minimum is the natural frequency of the hot-pressed layered body. The stiffness of the hot-pressed layered body is determined based on the natural frequency to determine whether the quality meets the standard. If the quality of the hot-pressed layered body meets the standard, multiple hot-pressed layered bodies are pressed together through a second hot-pressing sintering to obtain a functional gradient material of qualified quality.

[0009] In a possible design, the piezoelectric ceramic is provided with a reversible glue, and the piezoelectric ceramic is connected and separated from the hot-pressed layered body by the reversible glue. The quality inspection system also includes a heating device, and the heating device is used to heat the reversible glue to make it lose its viscosity.

[0010] In a possible design, the detection platform is provided with a groove, the groove is used to place the piezoelectric ceramic, an electromagnet is provided at the bottom of the groove, a magnet is provided at the bottom of the piezoelectric ceramic that generates a repulsive force when the electromagnet at the bottom of the groove is energized, and the reversible glue is provided on the top of the piezoelectric ceramic;

[0011] When performing quality inspection, the electromagnet at the bottom of the groove is energized to apply magnetic force to the piezoelectric ceramic in the groove, so that the piezoelectric ceramic moves upward to contact and fix the hot-pressed layered body to be inspected on the inspection platform. After the fixed connection, the electromagnet at the bottom of the groove is de-energized. After the inspection is completed, the temperature increasing device is used to heat the reversible glue to make it lose its viscosity, and the piezoelectric ceramic falls to the bottom of the groove.

[0012] In one possible design, magnets are arranged around the groove, and magnets with the same polarity as the magnets around the groove are arranged around the piezoelectric ceramic. Through the cooperation between the magnets around the groove and the magnets around the piezoelectric ceramic, the piezoelectric ceramic does not contact and rub against the inside of the groove during the up and down movement.

[0013] In a possible design, a glue holding portion is fixedly connected to the top of the piezoelectric ceramic, an upper portion of the glue holding portion is a recessed structure, and the reversible glue is placed in the recessed structure.

[0014] In a possible design, magnetic particles are arranged at the bottom of the recessed structure, and the temperature increasing device is an infrared wave emitter, and the temperature increasing device increases the temperature of the magnetic particles by releasing infrared waves to the magnetic particles.

[0015] In a possible design, elastic barriers are arranged around the recessed structure.

[0016] In a possible design, the piezoelectric ceramic is inserted into a glue tray.

[0017] In a possible design, a plurality of protruding structures are provided on the upper portion of the detection platform, and the protruding structures are used to support the hot-pressed layered body to be detected.

[0018] In a possible design, the robot arm is provided with a suction cup, and the suction cup is used to suck or release the hot pressed layered body.

[0019] Compared with the prior art, the present invention has at least the following beneficial effects:

[0020] In the present invention, after the first hot pressing sintering, a plurality of hot pressed layered bodies with gradient changes in composition and structure can be obtained. If a plurality of hot pressed layered bodies are directly pressed together by the second hot pressing sintering, once one or more of the hot pressed layered bodies have quality problems, the obtained functional gradient material will also have quality problems and cannot be used. Therefore, in order to avoid the above problems, after obtaining a plurality of hot pressed layered bodies, it is necessary to detect their quality. However, if a conventional detection system is used, the hot pressed layered body will be destroyed. Therefore, the present application provides a system for non-destructive detection of hot pressed layered bodies. After obtaining the hot pressed layered body, a mechanical arm is used to place it on a detection platform, and it is connected to a piezoelectric ceramic, and an AC power supply provides AC power to the piezoelectric ceramic. Under the action of AC power, the piezoelectric ceramic vibrates with the same frequency as the AC power, and then drives the hot pressed layered body connected to it to vibrate together. During the vibration process, the AC power supply adjusts the frequency of its output electrical signal, and uses an impedance collector to collect impedance data. The amplitude of the vibration of the piezoelectric ceramic is negatively correlated with the impedance generated by it. According to the impedance data, the natural frequency of the hot pressed layered body can be determined. The quality of the hot-pressed laminate can be further obtained based on the natural frequency, and finally the quality inspection of the functional gradient material during the preparation process can be completed. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0022] Figure 1 It is a structural schematic diagram of a quality detection system in a functional gradient material preparation process provided by an embodiment of the present invention;

[0023] Figure 2 It is a structural schematic diagram of a piezoelectric ceramic and its accessories provided by an embodiment of the present invention.

[0024] In the figure:

[0025] 1-Detection platform;

[0026] 2-AC power supply;

[0027] 3- piezoelectric ceramics;

[0028] 4- Impedance collector;

[0029] 5- hot pressing of the laminate;

[0030] 6-Reversible glue;

[0031] 7- Heating device;

[0032] 8-groove;

[0033] 9- Electromagnet;

[0034] 10- Magnet;

[0035] 11- Rubber holding part;

[0036] 12-Elastic enclosure;

[0037] 13-Glue tray. DETAILED DESCRIPTION

[0038] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0039] In the description of the embodiments of the present invention, unless otherwise clearly specified and limited, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance; unless otherwise specified or explained, the term "multiple" refers to two or more; the terms "connected" and "fixed" should be understood in a broad sense, for example, "connected" can be a fixed connection, a detachable connection, an integral connection, or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0040] In the description of this specification, it should be understood that the directional words such as "upper" and "lower" described in the embodiments of the present invention are described at the angles shown in the drawings and should not be understood as limiting the embodiments of the present invention. In addition, in the context, it should also be understood that when it is mentioned that an element is connected to another element "upper" or "lower", it can not only be directly connected to another element "upper" or "lower", but also indirectly connected to another element "upper" or "lower" through an intermediate element.

[0041] Please refer to Figure 1 and Figure 2 , an embodiment of the present invention provides a quality detection system in the process of preparing a functional gradient material, including a detection platform 1, a detection device and a mechanical arm;

[0042] The detection device includes an AC power supply 2, a piezoelectric ceramic 3 and an impedance collector 4, wherein the piezoelectric ceramic 3 is connected to a hot-pressed layered body 5 to be detected on a detection platform 1, and the piezoelectric ceramic 3 is also connected to the AC power supply 2 and the impedance collector 4 respectively, and the mechanical arm is used to move the hot-pressed layered body 5 to be detected to the detection platform 1; wherein the hot-pressed layered body 5 is a plate body prepared by a first hot-pressing sintering, having multiple components and having a structural gradient change;

[0043] When performing quality inspection, an AC power supply 2 is used to apply frequency-adjustable AC power to the piezoelectric ceramic 3, the frequency of the AC power is adjusted, and an impedance collector 4 is used to collect impedance data of the piezoelectric ceramic 3 at different frequencies in real time. The frequency of the AC power when the impedance is minimum is the natural frequency of the hot-pressed layered body 5. The stiffness of the hot-pressed layered body 5 is determined based on the natural frequency to determine whether its quality meets the standard. If the quality of the hot-pressed layered body 5 meets the standard, multiple hot-pressed layered bodies 5 are pressed together through a second hot-pressing sintering to obtain a functional gradient material with qualified quality.

[0044] In the present invention, after the first hot pressing sintering, a plurality of hot pressed layered bodies 5 with gradient changes in composition and structure can be obtained. If the plurality of hot pressed layered bodies 5 are directly pressed together by the second hot pressing sintering, once one or more of the hot pressed layered bodies 5 have quality problems, the obtained functional gradient material will also have quality problems and cannot be used. Therefore, in order to avoid the above problems, after obtaining the plurality of hot pressed layered bodies 5, it is necessary to detect their quality. However, if a conventional detection system is used, the hot pressed layered body 5 will be destroyed. Therefore, the present application provides a system for non-destructive detection of the hot pressed layered body 5. After obtaining the hot pressed layered body 5, a mechanical arm is used to place it on the detection platform 1, and it is connected to the piezoelectric ceramic 3, and the AC power supply 2 provides AC power to the piezoelectric ceramic 3. Under the action of the AC power, the piezoelectric ceramic 3 vibrates with the same frequency as the AC power, thereby driving the hot pressed layered body 5 connected thereto to vibrate together. During the vibration process, the AC power supply 2 adjusts the frequency of its output electrical signal, and uses the impedance collector 4 to collect impedance data. The vibration amplitude of the piezoelectric ceramic 3 is negatively correlated with the impedance it generates, and the natural frequency of the hot-pressed laminate 5 can be determined based on the impedance data. The quality of the hot-pressed laminate 5 can be further obtained based on the natural frequency, and the quality inspection of the functional gradient material during the preparation process can be finally completed.

[0045] Specifically, the frequency of the alternating current is adjusted to adjust the frequency of the piezoelectric ceramic 3 and the hot-pressed layered body 5 connected thereto. When the vibration frequency of the piezoelectric ceramic 3 and the hot-pressed layered body 5 connected thereto is consistent with the natural frequency of the hot-pressed layered body 5, resonance occurs. At this time, the amplitude of the piezoelectric ceramic 3 is the largest and the impedance is the smallest. Therefore, by comparing the impedance data, the minimum impedance that is significantly smaller than other impedances is the natural frequency of the hot-pressed layered body 5. After obtaining the natural frequency, the stiffness of the hot-pressed layered body 5 can be determined according to the natural frequency. The stiffness of the hot-pressed plate bodies made of different metal-ceramic types and different metal-ceramic ratios is different. Stiffness tests are performed on multiple hot-pressed plate bodies that meet the quality standards to obtain the stiffness of the hot-pressed plate bodies that meet the quality standards. The metal-ceramic type and metal-ceramic ratio of the hot-pressed plate body to be tested are compared with the stiffness of the hot-pressed plate body with the same type ratio and quality standards. If the difference in stiffness between the two is large, there may be a density problem, or there may be a hollow structure inside; if the difference in stiffness between the two is small, it can be considered that the quality is up to standard.

[0046] The stiffness of the hot-pressed laminate 5 to be tested is determined according to the natural frequency by the following formula:

[0047] k=h 2 ×m / C 2

[0048] Wherein, k is the stiffness, h is the natural frequency, m is the weight of the hot-pressed layered body 5 to be tested, and C is a constant.

[0049] It should be noted that after the piezoelectric ceramic 3 and the hot-pressed layered body 5 are combined, the natural frequency, stiffness and other properties of the combined body and the hot-pressed layered body 5 are basically the same, that is, the influence of the smaller piezoelectric ceramic 3 crystals on the hot-pressed layered body 5 is negligible.

[0050] In some embodiments of the present invention, the piezoelectric ceramic 3 is provided with a reversible glue 6, and the piezoelectric ceramic 3 is connected and separated from the hot-pressed layered body 5 through the reversible glue 6. The quality inspection system also includes a heating device 7, which is used to heat the reversible glue 6 to make it lose its viscosity.

[0051] In this embodiment, the cooperation of the reversible glue 6 and the temperature increasing device 7 can facilitate the connection and separation of the piezoelectric ceramic 3 and the hot pressed layered body 5 without manual operation.

[0052] In some embodiments of the present invention, the detection platform 1 is provided with a groove 8, the groove 8 is used to place the piezoelectric ceramic 3, an electromagnet 9 is provided at the bottom of the groove 8, a magnet 10 is provided at the bottom of the piezoelectric ceramic 3 that generates a repulsive force with the electromagnet 9 at the bottom of the groove 8 when energized, and a reversible glue 6 is provided on the top of the piezoelectric ceramic 3;

[0053] When performing quality inspection, the electromagnet 9 at the bottom of the groove 8 is energized to apply magnetic force to the piezoelectric ceramic 3 in the groove 8, so that the piezoelectric ceramic 3 moves upward to contact and fix the hot-pressed layered body 5 to be inspected on the inspection platform 1. After the fixed connection, the electromagnet 9 at the bottom of the groove 8 is de-energized. After the inspection is completed, the reversible glue 6 is heated by the heating device 7 to make it lose its viscosity, and the piezoelectric ceramic 3 falls to the bottom of the groove 8.

[0054] In this embodiment, the piezoelectric ceramic 3 can be controlled to move upward by energizing the electromagnet 9, and the piezoelectric ceramic 3 is fixedly connected to the hot-pressed layered body 5 in cooperation with the reversible glue 6; after the quality inspection is completed, the heating device 7 heats the reversible glue 6 to make it lose its viscosity, and the de-energized electromagnet 9 will not provide repulsive force, and the piezoelectric ceramic 3 falls to the bottom of the groove 8 under the action of gravity.

[0055] It should be noted that after the piezoelectric ceramic 3 and the hot-pressed layered body 5 are connected, the electromagnet 9 needs to be powered off to prevent it from affecting the vibration of the piezoelectric ceramic 3 .

[0056] It should also be noted that the piezoelectric ceramic 3 can be connected to the AC power source 2 and the impedance collector 4 through a wire passing through the detection platform 1. The wire can pass through the detection platform 1 and enter the groove 8.

[0057] In some embodiments of the present invention, magnets 10 are arranged around the groove 8, and magnets 10 with the same polarity as the magnets 10 around the groove 8 are arranged around the piezoelectric ceramic 3. Through the cooperation of the magnets 10 around the groove 8 and the magnets 10 around the piezoelectric ceramic 3, the piezoelectric ceramic 3 does not contact or rub against the inside of the groove 8 during the up and down movement.

[0058] In this embodiment, in order to control the piezoelectric ceramic 3 to avoid collision with the inner wall of the groove 8 during the up and down movement, magnets 10 with opposite polarities are arranged on the inner wall of the groove 8 and around the piezoelectric ceramic 3 .

[0059] In some embodiments of the present invention, a glue holding portion 11 is fixedly connected to the top of the piezoelectric ceramic 3 , the upper portion of the glue holding portion 11 is a recessed structure, and the reversible glue 6 is placed in the recessed structure.

[0060] In this embodiment, the fluidity of the reversible glue 6 will increase significantly at high temperature. In order to prevent it from leaking or to reduce its leaking, a glue holding portion 11 is provided on the top of the piezoelectric ceramic 3. The concave structure of the glue holding portion 11 is used to store the reversible glue 6. The concave structure can ensure that the reversible glue 6 does not leak when it is liquefied.

[0061] In some embodiments of the present invention, magnetic particles are arranged at the bottom of the recessed structure, and the heating device 7 is an infrared wave emitter. The heating device 7 heats the magnetic particles by releasing infrared waves to the magnetic particles.

[0062] In this embodiment, the temperature of the reversible glue 6 is precisely increased by utilizing the property that the magnetic particles heat up under the action of infrared light waves.

[0063] In some embodiments of the present invention, elastic barriers 12 are provided around the recessed structure.

[0064] In this embodiment, the elastic enclosure 12 can be deformed after the piezoelectric ceramic 3 moves upward and contacts the hot-pressed layered body 5, so that the reversible adhesive 6 in the concave structure contacts and bonds with the hot-pressed layered body 5. After the reversible adhesive 6 loses its viscosity due to heat and the piezoelectric ceramic 3 is separated from the hot-pressed layered body 5, the elastic enclosure 12 restores its shape to surround the reversible adhesive 6 in the concave structure to prevent leakage.

[0065] In some embodiments of the present invention, the piezoelectric ceramic 3 is disposed in the plastic tray 13 .

[0066] In this embodiment, the glue tray 13 can catch glue that accidentally overflows from the recessed structure.

[0067] In some embodiments of the present invention, a plurality of protruding structures are disposed on the upper portion of the detection platform 1 , and the protruding structures are used to support the hot-pressed layered body 5 to be detected.

[0068] In this embodiment, the protruding structure can lift up the hot-pressed laminate 5 , reduce the contact area, and reduce the obstruction of the detection platform 1 to the vibration of the hot-pressed laminate 5 .

[0069] In some embodiments of the present invention, the robot arm is provided with a suction cup, and the suction cup is used to suck or release the hot pressed layered body 5 .

[0070] In an embodiment of the present invention, the raw materials of the hot-pressed layered body prepared by the first hot-pressing sintering may be metal particles and ceramic powder.

[0071] Specifically, metal particles of different particle sizes are prepared by adjusting the rotation speed of the rotating electrode in the plasma rotating electrode process;

[0072] The metal particles of different particle sizes are mixed with different amounts of ceramic powder to obtain multiple groups of mixed particles; wherein, in the multiple groups of mixed particles, the finer the particle size of the metal particles, the higher the proportion of the ceramic powder;

[0073] Finally, each group of mixed particles is subjected to a first hot pressing and sintering process to obtain a plurality of hot pressed layered bodies;

[0074] In an embodiment of the present invention, when performing the second hot pressing and sintering treatment, a plurality of hot pressed layered bodies are first stacked in the thickness direction in the order of the ceramic content therein, and then the second hot pressing and sintering treatment is performed to obtain a functional gradient material.

[0075] In the present invention, metal particles with different particle sizes are first prepared by controlling the rotation speed of the plasma rotating electrode. The faster the rotation speed, the smaller the particle size of the metal particles, the faster the cooling rate, and the smaller the size of the crystal. Conversely, the slower the rotation speed, the larger the particle size of the metal particles, the slower the cooling rate, and the larger the size of the crystal. The smaller the size of the crystal, the higher the hardness, the larger the size of the crystal, and the better the toughness. In summary, by controlling the electrode rotation speed, small metal particles with small particle size and small crystal size and large metal particles with large particle size and large crystal size can be obtained. Metal particles of different particle sizes are mixed with ceramic powders of different volumes. The smaller the particle size of the metal particles, the higher the proportion of mixed ceramic powder, and multiple groups of mixed particles are obtained. In multiple groups of mixed particles, the smaller the particle size of the metal particles, the higher the proportion of ceramic powder in the mixed particles. The addition of ceramic powder can improve the ablation resistance of the material. At the same time, it can react at the boundary of the metal grains during sintering and forming. The generated ceramic body is filled and distributed at the boundary of the metal grains, increasing the hardness of the material itself. The higher the proportion of ceramic powder, the more obvious the hardness improvement. Conversely, the smaller the proportion of ceramic powder, the higher the toughness. Each group of mixed particles is subjected to a first hot pressing and sintering treatment to obtain a plurality of hot pressing layered bodies, and then the plurality of hot pressing layered bodies are stacked in the thickness direction in the order of the ceramic content therein, and subjected to a second hot pressing and sintering treatment to obtain a functional gradient material. The obtained material has different ceramic contents and different crystal sizes along the thickness direction, with one side having a small crystal size, a high ceramic content, and high hardness, and the other side having a large crystal size, a small ceramic content, or even no ceramic, and good toughness, and the hardness and toughness of the middle part change gradiently.

[0076] It should be noted that the large-size metal particles may be mixed with a small amount of ceramic powder or may not be mixed with the ceramic powder. The above-mentioned different amounts of ceramic powder include 0-content ceramic powder.

[0077] In some embodiments of the present invention, the metal particles include a titanium alloy.

[0078] In this embodiment, the titanium alloy has the characteristics of high temperature resistance, excellent mechanical properties and light weight, and is suitable for the aerospace field.

[0079] In some embodiments of the present invention, the ceramic powder includes ceramic powder containing boron, carbon and / or nitrogen elements.

[0080] In this embodiment, the ceramic powder containing boron, carbon and / or nitrogen elements can react with titanium to obtain a ceramic body with increased hardness.

[0081] In some embodiments of the present invention, the particle size of the ceramic powder is 5-10 μm.

[0082] In this embodiment, the particle size of the ceramic powder is in the range of 5 to 10 μm, which can be well mixed and wrapped with the metal particles, increase the contact surface between the metal particles and the ceramic powder, and increase the efficiency of the combination or reaction.

[0083] In some embodiments of the present invention, metal particles of different particle sizes are prepared by adjusting the rotation speed of the rotating electrode in the plasma rotating electrode process, including:

[0084] Determine the different size ranges of metal particles;

[0085] According to the particle size range, the rotation speed of the rotating electrode in the plasma rotating electrode process is allocated between 8000 and 35000 rpm;

[0086] According to the rotation speed of the rotating electrode, the current value in the plasma rotating electrode process is controlled within the range of 600~1200A; wherein the current and the rotation speed are inversely proportional;

[0087] Micron-sized metal particles with different particle sizes of 5 to 20 μm are obtained.

[0088] In this embodiment, the rotation speed can be controlled to be 8000~10000rpm, 18000~20000rpm, and 30000~35000rpm, respectively, and the three rotation speeds correspond to 1000~1200A, 800~1000A, and 600~800A, respectively. The higher the current, the higher the temperature of the electrode, the higher the melting degree of the metal material, the higher the melting degree, the larger the particles thrown out, and in addition, the slower the rotation speed, the larger the particles thrown out by the centrifugal force. Therefore, low rotation speed combined with high current can obtain metal particles with large particle size, and high rotation speed combined with low current can obtain metal particles with small particle size.

[0089] Of course, you can also set more different speeds between 8000~35000rpm according to your needs to obtain metal particles of more different particle sizes. The current can also be adaptively adjusted according to different speeds.

[0090] In some embodiments of the present invention, each group of mixed particles is subjected to a first hot pressing and sintering process to obtain a plurality of hot pressed layered bodies, including:

[0091] Each group of mixed particles is subjected to a first hot pressing sintering treatment at different temperatures; wherein, the higher the proportion of metal particles in the mixed particles, the higher the temperature of the first hot pressing sintering.

[0092] In the present application, the temperature of the first hot pressing sintering treatment affects the degree of recrystallization of the metal. The higher the temperature, the better the degree of recrystallization and the larger the resulting grains. When the temperature is low, the degree of metal recrystallization is low or no recrystallization occurs. Therefore, by controlling the temperature of the first hot pressing sintering treatment at a higher temperature, the mixed particles of large metal grains can be sintered and the grains can be further enlarged; by controlling the first sintering temperature at a lower temperature, the mixed particles are only combined and compacted with each other, and no or little recrystallization occurs, so that after the mixed particles of small metal grains are sintered, the grains remain at a smaller degree.

[0093] In some embodiments of the present invention, in the plurality of groups of mixed particles, when the total volume of the plurality of groups of mixed particles is 100 parts, the volume fraction of the ceramic powder is 1-8.

[0094] In some embodiments of the present invention, multiple hot-pressed layered bodies are stacked in the thickness direction in order of ceramic content, and subjected to a second hot-pressing sintering process to obtain a functional gradient material, including:

[0095] stacking a plurality of hot-pressed laminates in order of ceramic content along a thickness direction;

[0096] After a heat insulating layer is provided on one side of the hot pressed layered body having the lowest ceramic content, a second hot pressing sintering treatment is performed to obtain a functional gradient material.

[0097] In this embodiment, after a heat-insulating layer is provided on one side of the hot-pressed layered body with the lowest ceramic content, the heating rate is slow during the second hot-pressing sintering, but with the passage of time, it can still reach a temperature (900°C) that can transform the titanium crystals from a close-packed hexagonal structure to a body-centered cubic structure. With the end of the second hot-pressing sintering, the temperature begins to gradually decrease. However, due to the presence of the heat-insulating layer, the cooling rate of the part with a low ceramic content is slow. The cooling rate is related to the content of body-centered cubic structure crystals. The slower the cooling rate, the lower the content of body-centered cubic structure crystals, and the stronger the toughness of the material. The faster the cooling rate, the higher the content of body-centered cubic structure crystals, and the stronger the hardness of the material.

[0098] It should be noted that although the second hot pressing sintering treatment also causes recrystallization, the size relationship between the larger crystals and the smaller crystals remains unchanged after both are recrystallized. In addition, ceramic phases are distributed at the boundaries of the small crystals inside the hot pressing layered body of the smaller crystals, which limits the degree of recrystallization. Therefore, only part of the crystals inside the hot pressing layered body of the smaller crystals are recrystallized, which has little effect on the change of the overall crystal particles.

[0099] In some embodiments of the present invention, the temperature of the first hot pressing sintering includes 800-1200° C., and the pressure of the first hot pressing sintering includes 80-120 MPa.

[0100] In some embodiments of the present invention, the temperature of the second hot pressing sintering process is 950-1100° C., and the pressure is 100-150 MPa.

[0101] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A quality detection system in the process of preparing functional gradient materials, characterized in that: It comprises a detection platform (1), a detection device and a mechanical arm; The detection device comprises an AC power supply (2), a piezoelectric ceramic (3) and an impedance collector (4); the piezoelectric ceramic (3) is connected to a hot-pressed layered body (5) to be detected on the detection platform (1); the piezoelectric ceramic (3) is also connected to the AC power supply (2) and the impedance collector (4), respectively; the mechanical arm is used to move the hot-pressed layered body (5) to be detected onto the detection platform (1); wherein the hot-pressed layered body (5) is a plate body prepared by a first hot-pressing sintering process, has multiple components and has a structural gradient change; When performing quality inspection, the AC power source (2) applies frequency-adjustable AC to the piezoelectric ceramic (3), the frequency of the AC is adjusted, and the impedance collector (4) collects impedance data of the piezoelectric ceramic (3) at different frequencies in real time. The frequency of the AC when the impedance is minimum is the natural frequency of the hot-pressed layered body (5). The stiffness of the hot-pressed layered body (5) is determined based on the natural frequency to determine whether the quality meets the standard. If the quality of the hot-pressed layered body (5) meets the standard, a plurality of the hot-pressed layered bodies (5) are pressed together through a second hot-pressing sintering process to obtain a functional gradient material of qualified quality. The piezoelectric ceramic (3) is provided with a reversible glue (6), and the piezoelectric ceramic (3) is connected and separated from the hot-pressed layered body (5) via the reversible glue (6). The quality detection system further comprises a heating device (7), and the heating device (7) is used to heat the reversible glue (6) so as to make it lose its viscosity; The detection platform (1) is provided with a groove (8), the groove (8) is used to place the piezoelectric ceramic (3), an electromagnet (9) is provided at the bottom of the groove (8), a magnet (10) is provided at the bottom of the piezoelectric ceramic (3) and generates a repulsive force with the electromagnet (9) at the bottom of the groove (8) when electricity is supplied, and the reversible glue (6) is provided at the top of the piezoelectric ceramic (3); When performing quality inspection, the electromagnet (9) at the bottom of the groove (8) is energized to apply magnetic force to the piezoelectric ceramic (3) in the groove (8), so that the piezoelectric ceramic (3) moves upward to contact and fix the hot-pressed layered body (5) to be inspected on the inspection platform (1). After the fixed connection, the electromagnet (9) at the bottom of the groove (8) is de-energized. After the inspection is completed, the reversible glue (6) is heated by the heating device (7) to make it lose its viscosity, and the piezoelectric ceramic (3) falls into the bottom of the groove (8).

2. The quality inspection system according to claim 1, characterized in that: The groove (8) is surrounded by magnets (10), and the piezoelectric ceramic (3) is surrounded by magnets (10) having the same polarity as the magnets (10) around the groove (8). The piezoelectric ceramic (3) does not contact or rub against the inside of the groove (8) during its upward and downward movement by means of the cooperation between the magnets (10) around the groove (8) and the magnets (10) around the piezoelectric ceramic (3).

3. The quality inspection system according to claim 1, characterized in that: The top of the piezoelectric ceramic (3) is fixedly connected to a glue holding portion (11), the upper portion of the glue holding portion (11) is a recessed structure, and the reversible glue (6) is placed in the recessed structure.

4. The quality inspection system according to claim 3, characterized in that: Magnetic particles are arranged at the bottom of the recessed structure, and the temperature increasing device (7) is an infrared wave emitter, and the temperature increasing device (7) increases the temperature of the magnetic particles by releasing infrared waves to the magnetic particles.

5. The quality inspection system according to claim 3, characterized in that: Elastic barriers (12) are arranged around the recessed structure.

6. The quality inspection system according to claim 3, characterized in that: The piezoelectric ceramic (3) is inserted into the glue receiving tray (13).

7. The quality inspection system according to claim 1, characterized in that: A plurality of raised structures are arranged on the upper part of the detection platform (1), and the raised structures are used to support the hot-pressed layered body (5) to be detected.

8. The quality inspection system according to claim 1, characterized in that: The robot arm is provided with a suction cup, and the suction cup is used to suck or release the hot pressed layered body (5).