Sodium-ion battery electrolyte and sodium-ion battery

By optimizing the solvent composition and additive types of the sodium-ion battery electrolyte, the problems of high-temperature storage and cyclic gas production of sodium-ion batteries are solved, the stability and performance of the battery are improved, the interface impedance is reduced, and better cycle performance is achieved.

CN118782913APending Publication Date: 2024-10-15三一红象电池有限公司

Patent Information

Application Number
CN202411030707.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

The high-temperature storage and cyclic gas production problems of sodium-ion batteries lead to interface instability, which limits their application. Existing technologies have adverse effects on cell performance when improving gas production.

Method used

By optimizing the solvent composition of the sodium-ion battery electrolyte, including propylene carbonate, fluorinated solvents and additives, the mass ratio of the solvent and the type and content of the additives are optimized to improve the stability and antioxidant capacity of the electrolyte and reduce the interface impedance.

Benefits of technology

It effectively improves the high-temperature storage and cycle performance of sodium-ion batteries, reduces the interface impedance, improves the stability and safety performance of the battery, avoids the decomposition of the electrolyte to produce gas, and improves the overall performance of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention relates to the technical field of sodium-ion batteries, in particular to a sodium-ion battery electrolyte and a sodium-ion battery. The sodium-ion battery electrolyte comprises a solvent, a sodium salt and an additive, the solvent comprises a first solvent and a second solvent; the first solvent comprises one or more of propylene carbonate, diethyl carbonate, ethyl methyl carbonate, ethyl propionate, propyl propionate, ethyl acetate, ethyl n-butyrate and gamma-butyrolactone; the second solvent is prepared from one or more of difluoroethyl acetate, ethylene bis (fluorocarbonate), 2, 2, 2-trifluoroethyl acetate, propylene trifluorocarbonate, sulfolane and diethylene glycol dimethyl ether, and the second solvent is prepared from one or more of difluoroethyl acetate, ethylene bis (fluorocarbonate), 2, 2, 2-trifluoroethyl acetate, propylene trifluorocarbonate, sulfolane and diethylene glycol dimethyl ether; wherein the mass ratio of the first solvent to the second solvent is (5-29): 1. By optimizing the solvent composition, the problems of high-temperature storage and cyclic gas production of the sodium-ion battery can be effectively improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of sodium ion batteries, and in particular to a sodium ion battery electrolyte and a sodium ion battery. Background Art

[0002] Sodium-ion batteries have similar theoretical foundations to lithium-ion batteries, relatively low budgets, and abundant sodium resources, and are recognized as the most competitive alternative to lithium-ion batteries. Among the cathode materials of sodium-ion batteries, layered transition metal oxide cathodes have the advantages of large theoretical capacity, non-toxicity, and easy synthesis, and have received widespread attention. However, layered oxide cathode materials are plagued by various interface problems. Among them, interface instability, including surface residual alkali, phase change, loss of active transition metals, and oxygen loss, is the main cause of failure of layered oxide cathodes. The irreversible structural destruction of the cathode material and the generation of cracks in the lattice lead to lattice oxygen release, which accelerates the oxidative decomposition of the electrolyte and the interface film. The gas products of the electrolyte decomposition directly lead to the expansion of the battery thickness during storage and cycling, which limits the application of sodium-ion batteries. Therefore, in order to effectively improve the high-temperature storage and cycle gas production problems of sodium-ion batteries, it is urgent to develop sodium-ion battery electrolytes with good electrode / electrolyte interface compatibility and excellent cycle and storage performance.

[0003] At present, in order to improve the gas production problem of sodium ion batteries in the existing technology, the gas production is often improved at the electrolyte level by adding some high-impedance additives to the electrolyte to inhibit gas production. However, while improving the gas production problem, it will also have an adverse effect on the room temperature performance and cycle of the battery cell. Summary of the invention

[0004] The present invention provides a sodium ion battery electrolyte and a sodium ion battery, which are used to at least partially solve the defects of the prior art. On the basis of ensuring the electrochemical performance of the sodium ion battery, the storage and cycle performance of the sodium ion battery can be effectively improved, and the interface impedance can be reduced.

[0005] In a first aspect, the present invention provides a sodium ion battery electrolyte, comprising a solvent, a sodium salt and an additive; the solvent comprises a first solvent and a second solvent; the first solvent comprises one or more of propylene carbonate, diethyl carbonate, ethyl methyl carbonate, ethyl propionate, propyl propionate, ethyl acetate, ethyl butyrate and γ-butyrolactone; the second solvent comprises one or more of difluoroethyl acetate, difluoroethylene carbonate, ethyl 2,2,2-trifluoroacetate, trifluoropropylene carbonate, cyclopentane sulfone and diethylene glycol dimethyl ether; Wherein, the mass ratio of the first solvent to the second solvent is (5~29):1.

[0006] According to the sodium ion battery electrolyte provided by the present invention, the sodium ion battery electrolyte does not contain ethylene carbonate.

[0007] According to the sodium ion battery electrolyte provided by the present invention, the mass ratio of the first solvent to the second solvent is (5-19):1.

[0008] According to the sodium ion battery electrolyte provided by the present invention, the mass of the first solvent is 70-85wt% of the total mass of the sodium ion battery electrolyte.

[0009] According to the sodium ion battery electrolyte provided by the present invention, the mass of the second solvent is 3-10wt% of the total mass of the sodium ion battery electrolyte.

[0010] According to the sodium ion battery electrolyte provided by the present invention, the additive includes a first additive; the first additive includes: 1,3-propane sultone, fluoroethylene carbonate, trimethyl phosphate, propylene sultone, ethylene glycol bis (propionitrile) ether, biphenyl, vinyl ethylene carbonate, 1,4-butane sultone, triphenyl phosphate, tributyl phosphate, trifluoroethyl phosphate and one or more of fluorine-containing ethers.

[0011] Preferably, the mass of the first additive accounts for 0.5-5wt% of the total mass of the sodium ion battery electrolyte; more preferably, the mass of the first additive accounts for 1.5-4wt% of the total mass of the sodium ion battery electrolyte.

[0012] According to the sodium ion battery electrolyte provided by the present invention, the additive includes a first additive and a second additive; the second additive includes: one or more of vinyl sulfate, tris-(trimethylsilyl) phosphite, methanedisulfonic acid methylene ester and tris-(trimethylsilyl) borate; preferably, the mass of the second additive accounts for 0.5~1.5wt% of the total mass of the sodium ion battery electrolyte.

[0013] According to the sodium ion battery electrolyte provided by the present invention, the mass ratio of the first additive to the second additive is (1.5-4): (0.5-1.5).

[0014] According to the sodium ion battery electrolyte provided by the present invention, the sodium salt includes one or more of sodium hexafluorophosphate, sodium difluorophosphate, sodium perchlorate, sodium trifluoromethanesulfonate, sodium bisoxalatoborate, sodium difluorooxalatoborate, sodium tetrafluoroborate and sodium bistrifluoromethanesulfonimide; preferably, the mass of the sodium salt is 10-16wt% of the total mass of the sodium ion battery electrolyte.

[0015] According to the sodium ion battery electrolyte provided by the present invention, the first solvent includes propylene carbonate, ethyl methyl carbonate and diethyl carbonate; the second solvent includes difluoroethyl acetate; the sodium salt includes sodium hexafluorophosphate and sodium bis(fluorosulfonyl)imide; the first additive includes fluoroethylene carbonate and 1,3-propane sultone; and the second additive includes vinyl sulfate.

[0016] In a second aspect, the present invention provides a sodium ion battery comprising the sodium ion battery electrolyte.

[0017] The sodium ion battery electrolyte and the sodium ion battery provided by the present invention can effectively improve the high-temperature storage and cyclic gas production problems of the sodium ion battery by optimizing the solvent composition. DETAILED DESCRIPTION

[0018] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention is described clearly and completely below. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0019] At present, the prior art has conducted a lot of research to improve the deficiencies of sodium ion batteries in high temperature performance and cycle performance, but there is still room for further improvement. In order to effectively improve the storage and cycle performance of sodium ion batteries while ensuring the electrochemical performance of sodium ion batteries and reduce the interface impedance, the present invention provides the following sodium ion battery electrolyte.

[0020] In a first aspect, the present invention provides a sodium ion battery electrolyte, comprising a solvent, a sodium salt and an additive; the solvent comprises a first solvent and a second solvent; the first solvent comprises one or more of propylene carbonate (PC), diethyl carbonate (DEC), ethyl methyl carbonate (EMC), ethyl propionate (EP), propyl propionate (PP), ethyl acetate (EA), ethyl butyrate (EB) and γ-butyrolactone (GBL); the second solvent comprises one or more of difluoroethyl acetate (DFEA), difluoroethylene carbonate (DFEC), ethyl 2,2,2-trifluoroacetate (TFAE), trifluoropropylene carbonate (TFPC), cyclopentane (THF) and diethylene glycol dimethyl ether (DG); wherein the mass ratio of the first solvent to the second solvent is (5~29):1.

[0021] Preferably, the second solvent includes a fluorinated solvent; specifically, the second solvent includes one or more of difluoroethyl acetate, bisfluoroethylene carbonate, ethyl 2,2,2-trifluoroacetate and trifluoropropylene carbonate.

[0022] The present invention can improve the antioxidant capacity of the solvent while ensuring the basic performance of the electrolyte by optimizing the formula of the solvent in the electrolyte, thereby improving the stability of the electrolyte and reducing the electrolyte from decomposing and producing gas due to oxidation to decompose and deteriorate the battery performance. Wherein, the first solvent is responsible for the dissolution of the sodium salt and promotes the rapid migration of sodium ions between the positive and negative electrodes. The introduction of the second solvent can further improve the stability of the electrolyte, especially the introduction of fluorinated solvents. Since the fluorine element can reduce the highest occupied molecular orbital (HOMO) energy level of the molecule, the fluorinated solvent has higher oxidation resistance, so it is not easy to produce gas by chemical or electrochemical oxidation decomposition. Therefore, the fluorinated solvent helps to improve the stability of the CEI / SEI film formed by the positive and negative electrode film-forming additives by reducing the oxidation reaction, and reduces the safety risk of the battery during use. In addition, the strong electronegativity of the fluorine element can reduce the solvation energy of the solvent system, making it easier for anions to enter the solvation shell of the sodium ion to form NaF, and the decomposition of the fluorinated solvent itself can also form a SEI interface rich in NaF and other fluorinated substances in the battery interface, which can significantly enhance the chemical stability and mechanical stability of SEI.

[0023] According to a preferred embodiment provided by the present invention, the sodium ion battery electrolyte does not contain ethylene carbonate.

[0024] In the present invention, the sodium ion battery electrolyte does not contain the conventional organic solvent, ethylene carbonate (EC). The present invention finds that EC has strong reactivity with the layered oxide positive electrode and poor oxidation resistance under high voltage, and is very easy to decompose and produce gas in the electrolyte. The use of an EC-free system is beneficial to improving the stability of the electrolyte.

[0025] According to a preferred embodiment provided by the present invention, the mass ratio of the first solvent to the second solvent is (5-19):1; for example, 5:1, 6:1, 7:1, 8:1, 9:1, 10:1, 11:1, 12:1, 13:1, 14:1, 15:1, 16:1, 17:1, 18:1 and 19:1.

[0026] Further preferably, the mass ratio of the first solvent to the second solvent is (7-10):1.

[0027] According to a preferred embodiment provided by the present invention, the mass of the first solvent is 70-85wt% of the total mass of the sodium ion battery electrolyte; for example, it can be 70wt%, 71wt%, 72wt%, 73wt%, 74wt%, 75wt%, 76wt%, 77wt%, 78wt%, 79wt%, 80wt%, 81wt%, 82wt%, 83wt%, 84wt% or 85wt%.

[0028] According to a preferred embodiment provided by the present invention, the mass of the second solvent is 3-10wt% of the total mass of the sodium ion battery electrolyte; for example, it can be 3wt%, 4wt%, 5wt%, 6wt%, 7wt%, 8wt%, 9wt% or 10wt%.

[0029] According to a preferred embodiment provided by the present invention, the additive includes a first additive; the first additive includes: 1,3-propane sultone (PS), fluoroethylene carbonate (FEC), trimethyl phosphate (TMP), propylene sultone (PST), ethylene glycol bis (propionitrile) ether (EGBE), biphenyl (BP), vinyl ethylene carbonate (VEC), 1,4-butane sultone (BS), triphenyl phosphate (TPP), tributyl phosphate (TBP), trifluoroethyl phosphate (TFFP) and one or more of fluorine-containing ethers.

[0030] In the present invention, the solvent formula is superimposed with the positive and negative electrode film-forming additives (i.e., the first additive). On the one hand, it can better protect the positive and negative electrode interfaces and reduce the corrosion of the electrolyte to the electrode materials. On the other hand, the oxidation-resistant solvent helps to improve the stability of the CEI / SEI film formed by the positive and negative electrode film-forming additives by reducing the oxidation reaction, thereby reducing the safety risks of the battery during use.

[0031] More preferably, the mass of the first additive accounts for 0.5-5wt% of the total mass of the sodium ion battery electrolyte.

[0032] Further preferably, the mass of the first additive accounts for 1.5-4wt% of the total mass of the sodium ion battery electrolyte; for example, it can be 1.5wt%, 2.0wt%, 2.5wt%, 3.0wt%, 3.5wt% or 4.0wt%.

[0033] According to a preferred embodiment provided by the present invention, the additive includes a first additive and a second additive; the second additive includes: one or more of vinyl sulfate (DTD), tris-(trimethylsilyl) phosphite (TMSP), methylene disulfonate (MMDS) and tris-(trimethylsilyl) borate (TMSB).

[0034] In the present invention, the solvent formula is superimposed with a low-impedance additive (i.e., the second additive) to form a more uniform and denser protective film, further reducing the internal resistance of the battery. At the same time, the low-impedance additive is used in combination with an oxidation-resistant solvent to further improve the charge and discharge efficiency and energy density of the battery without compromising the stability of the battery.

[0035] More preferably, the mass of the second additive accounts for 0.5-1.5wt% of the total mass of the sodium ion battery electrolyte; for example, it can be 0.5wt%, 0.6wt%, 0.7wt%, 0.8wt%, 0.9wt%, 1.0wt%, 1.1wt%, 1.2wt%, 1.3wt%, 1.4wt% or 1.5wt%.

[0036] According to a preferred embodiment provided by the present invention, the mass ratio of the first additive to the second additive is (1.5-4): (0.5-1.5).

[0037] Further preferably, the mass ratio of the first additive to the second additive is (2-4):(1-1.5).

[0038] In the present invention, the additives are selected to cooperate with positive and negative electrode film-forming additives and low impedance additives. On the one hand, the positive and negative electrode film-forming additives can build a stable CEI / SEI film at the interface of the positive and negative electrodes, isolate the release of positive electrode lattice oxygen and the crosstalk reaction at the negative electrode, and effectively reduce the redox decomposition of the solvent at the interface of the positive and negative electrodes; on the other hand, because additives that protect the positive electrode well often bring about a large electrochemical impedance, the electrochemical impedance can be synergistically reduced by introducing compounds containing sulfur, phosphorus, boron and other elements. Among them, sulfide has a lower LUMO orbit and is easier to reduce and form a film at the negative electrode, forming a ROSO 3 Organic matter represented by Li and Li 2 SO 3 A thinner, low-impedance SEI film mainly composed of inorganic substances represented by ; phosphides help to form a phosphate-rich interfacial film, which helps to improve the migration rate of sodium ions and thus reduce the interfacial impedance. In addition, phosphides can also combine with active oxygen dissolved in the electrolyte to form a P=O double bond, which can well protect the positive electrode while inhibiting the oxidative decomposition of the electrolyte; electron-deficient boron-containing compounds can increase the solubility of LiF on the positive electrode surface, forming a thinner SEI film with lower impedance.

[0039] According to a preferred embodiment provided by the present invention, the sodium ion battery electrolyte includes a first solvent, a second solvent, a sodium salt, a first additive and a second additive. The first solvent includes one or more of propylene carbonate (PC), diethyl carbonate (DEC), ethyl methyl carbonate (EMC), ethyl propionate (EP), propyl propionate (PP), ethyl acetate (EA), ethyl butyrate (EB) and γ-butyrolactone (GBL). The second solvent includes one or more of difluoroethyl acetate (DFEA), bisfluoroethylene carbonate (DFEC), ethyl 2,2,2-trifluoroacetate (TFAE), trifluoropropylene carbonate (TFPC), cyclopentane (THF) and diethylene glycol dimethyl ether (DG); wherein the mass ratio of the first solvent to the second solvent is (70~85): (3~10). The first additive includes one or more of 1,3-propane sultone (PS), fluoroethylene carbonate (FEC), trimethyl phosphate (TMP), propene sultone (PST), ethylene glycol bis(propionitrile) ether (EGBE), biphenyl (BP), vinyl ethylene carbonate (VEC), 1,4-butane sultone (BS), triphenyl phosphate (TPP), tributyl phosphate (TBP), trifluoroethyl phosphate (TFFP) and fluorinated ether. The second additive includes one or more of vinyl sulfate (DTD), tri-(trimethylsilyl) phosphite (TMSP), methylene methane disulfonate (MMDS) and tri-(trimethylsilyl) borate (TMSB); wherein the mass ratio of the first additive to the second additive is (2-4): (1-1.5).

[0040] According to a preferred embodiment provided by the present invention, the sodium salt includes one or more of sodium hexafluorophosphate, sodium perchlorate, sodium trifluoromethanesulfonate, sodium bis(oxalatoborate), sodium difluorooxalatoborate, sodium tetrafluoroborate and sodium bis(trifluoromethanesulfonimide).

[0041] In the present invention, when multiple sodium salts are used, the content thereof is not particularly limited as long as the effects of the present application are not significantly impaired.

[0042] More preferably, the mass of the sodium salt is 10-16wt% of the total mass of the sodium ion battery electrolyte; for example, it can be 10wt%, 11wt%, 12wt%, 13wt%, 14wt%, 15wt% or 16wt%.

[0043] According to a preferred embodiment provided by the present invention, the first solvent includes propylene carbonate, ethyl methyl carbonate and diethyl carbonate; the second solvent includes the above-mentioned fluorinated solvent; the sodium salt includes sodium hexafluorophosphate and sodium bis(fluorosulfonyl)imide; the first additive includes fluoroethylene carbonate and 1,3-propane sultone; and the second additive includes vinyl sulfate.

[0044] More preferably, the mass ratio of the total mass of the mixture of propylene carbonate, ethyl methyl carbonate and diethyl carbonate to the mass ratio of the fluorinated solvent is (8-10):1.

[0045] Further preferably, the fluorinated solvent comprises difluoroethyl acetate.

[0046] More preferably, in the first additive, the mass ratio of fluoroethylene carbonate to 1,3-propane sultone is (1-2): (1-2).

[0047] Further preferably, in the first additive, when the mass ratio of fluoroethylene carbonate to 1,3-propane sultone is 1:(1-2), the high temperature storage performance and cycle performance of the sodium ion battery can be further improved.

[0048] More preferably, the mass ratio of the total mass of the fluoroethylene carbonate and 1,3-propane sultone to the mass of the vinyl sulfate is (2-4):(1-1.5).

[0049] More preferably, in the sodium salt, the mass of sodium hexafluorophosphate accounts for 13-14wt% of the total mass of the sodium ion battery electrolyte. The present invention finds that when the mass of sodium hexafluorophosphate in the sodium salt is less than 13wt%, the high temperature storage performance of the battery is significantly affected.

[0050] In a second aspect, the present invention provides a sodium ion battery comprising the sodium ion battery electrolyte.

[0051] In the present invention, the sodium ion battery comprises: a positive electrode, a negative electrode, a separator and the sodium ion battery electrolyte.

[0052] The technical scheme of the present invention is further described below in conjunction with specific embodiments. It should be noted that these embodiments are only used to illustrate the present application and are not used to limit the scope of the present application. In the following examples, the materials, reagents and instruments used can be purchased from commercial sources if there are no special instructions.

[0053] Examples and Comparative Examples

[0054] This embodiment provides a sodium ion battery electrolyte, and the preparation method thereof comprises the following steps: In a glove box filled with argon, the moisture content was less than 0.1 ppm and the oxygen content was less than 0.1 ppm. Propylene carbonate (PC), ethyl methyl carbonate (EMC), diethyl carbonate (DEC), and difluoroethyl acetate (DFEA) were mixed in a mass ratio of 4:3:2:1 to obtain an organic solvent, and then 13 wt% of sodium hexafluorophosphate (NaPF6) based on the total weight of the electrolyte was slowly added to the organic solvent. 6) and sodium bis(fluorosulfonyl)imide (NaFSI) to obtain a mixture of an organic solvent and a sodium salt, and finally add 4wt% of fluoroethylene carbonate (FEC), 1,3-propane sultone (PS), and diethylene sulfate (DTD) based on the total weight of the electrolyte, and stir evenly to obtain the sodium ion battery electrolyte of this embodiment 1. The amounts of various sodium salts and additives are shown in Table 1.

[0055] The remaining examples and comparative examples were prepared by the same preparation method as in Example 1, and the specific formulas and contents are shown in Table 1; it should be noted that in different examples, the total mass of the solvent, the total mass of the sodium salt and the total mass of the additives are the same, but the formulas are different. Among them, ethylene carbonate (EC) is added in Example 16.

[0056] Table 1

[0057]

[0058] Test example

[0059] Preparation of soft-pack batteries: stack the prepared positive electrode sheet, separator, and negative electrode sheet in order, so that the separator is in the middle of the positive and negative electrode sheets, and stack the sheets to obtain a bare battery cell; place the bare battery cell in an aluminum-plastic film outer package, vacuum dry at 85°C, and inject the sodium ion battery electrolyte prepared in the above embodiment and comparative example into the dried battery after the moisture reaches the standard, encapsulate, stand, form, and divide the capacity to complete the preparation of the sodium ion battery.

[0060] Performance test: The batteries made from the sodium ion battery electrolytes obtained in the above embodiments and comparative examples were subjected to relevant performance tests.

[0061] 1) High temperature storage test: Charge the sodium-ion battery to 4.0V at 1C constant current, then charge at constant voltage to a current of 0.05C, and then fully discharge to 1.5V to the fully discharged state. Test the thickness of the lithium-ion battery in the fully discharged state THK1. Store the fully charged battery cell in a 60℃ high temperature furnace for 30D, and test the thickness of the battery cell THK2. Calculate the expansion rate of the sodium-ion battery according to the following formula: Expansion rate = (THK2-THK1) / THK1.

[0062] 2) Cycle performance test: Place the sodium ion battery in a 25℃ constant temperature chamber and a 45℃ constant temperature box respectively, and let it stand for 30 minutes to allow the sodium ion battery to reach a constant temperature. The sodium ion battery that has reached a constant temperature is charged at 1C constant current to 4.0V, then charged at a constant voltage until the current drops to 0.05C, and then discharged at 1C constant current to 1.5V. Repeat this cycle, record the discharge capacity of the first cycle and the discharge capacity of the last cycle, and calculate the capacity retention rate according to the following formula: The Xth cycle capacity retention rate (%) = (Xth cycle discharge capacity / first cycle discharge capacity) × 100%.

[0063] 3) DCR test: Take a fresh cell with 50% SOC and discharge it at a given current of 1C for 360s (100ms sampling point).

[0064] DCR calculation = (discharge initial voltage - battery voltage at 1C discharge for 360s) / 1.0C * 1000; in this system, 1C = 2A.

[0065] The test results are shown in Table 2: Electrical performance test: Table 2

[0066] According to Table 1, compared with Examples 1 to 15, Example 16 contains ethylene carbonate (EC) in the sodium ion battery electrolyte system, and the electrolyte produces more gas, which is not conducive to the stability of the electrolyte and will significantly reduce the battery performance. Compared with Examples 17 to 18 and Comparative Example 1, Examples 1 to 15 contain both the first solvent and the second solvent, which can ensure the basic performance of the electrolyte while improving the stability of the electrolyte and reduce the deterioration of battery performance due to oxidation and decomposition of the electrolyte. At the same time, compared with Example 1 and Example 2 to Example 15, it can be seen that when the amount of sodium salt is less than 13%, it will also affect the battery performance to a certain extent.

[0067] It should be noted that when the solvents and additives described in the examples are replaced with other solvents and additives defined above in the present invention, the effects are equivalent to those of the above examples. Due to space limitations, they will not be described in detail.

[0068] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A sodium ion battery electrolyte, characterized in that: The invention comprises a solvent, a sodium salt and an additive; the solvent comprises a first solvent and a second solvent; the first solvent comprises one or more of propylene carbonate, diethyl carbonate, ethyl methyl carbonate, ethyl propionate, propyl propionate, ethyl acetate, ethyl butyrate and γ-butyrolactone; the second solvent comprises one or more of difluoroethyl acetate, bisfluoroethylene carbonate, ethyl 2,2,2-trifluoroacetate, trifluoropropylene carbonate, cyclopentane sulfone and diethylene glycol dimethyl ether; Wherein, the mass ratio of the first solvent to the second solvent is (5~29):

1.

2. The sodium ion battery electrolyte according to claim 1, characterized in that The sodium ion battery electrolyte does not contain ethylene carbonate.

3. The sodium ion battery electrolyte according to claim 1 or 2, characterized in that: The mass ratio of the first solvent to the second solvent is (5-19):

1.

4. The sodium ion battery electrolyte according to claim 1 or 2, characterized in that: The mass of the first solvent is 70-85wt% of the total mass of the sodium ion battery electrolyte; and / or the mass of the second solvent is 3-10wt% of the total mass of the sodium ion battery electrolyte.

5. The sodium ion battery electrolyte according to any one of claims 1 to 4, characterized in that The additive includes a first additive; the first additive includes: one or more of 1,3-propane sultone, fluoroethylene carbonate, trimethyl phosphate, propylene sultone, ethylene glycol bis(propionitrile) ether, biphenyl, vinyl ethylene carbonate, 1,4-butane sultone, triphenyl phosphate, tributyl phosphate, trifluoroethyl phosphate and fluorine-containing ether; Preferably, the mass of the first additive accounts for 0.5-5wt% of the total mass of the sodium ion battery electrolyte; more preferably, the mass of the first additive accounts for 1.5-4wt% of the total mass of the sodium ion battery electrolyte.

6. The sodium ion battery electrolyte according to any one of claims 1 to 5, characterized in that The additives include a first additive and a second additive; the second additive includes one or more of vinyl sulfate, tris-(trimethylsilyl)phosphite, methylene disulfonate and tris-(trimethylsilyl)borate; preferably, the mass of the second additive accounts for 0.5-1.5wt% of the total mass of the sodium ion battery electrolyte.

7. The sodium ion battery electrolyte according to claim 6, characterized in that: The mass ratio of the first additive to the second additive is (1.5-4):(0.5-1.5).

8. The sodium ion battery electrolyte according to any one of claims 1 to 7, characterized in that The sodium salt includes one or more of sodium hexafluorophosphate, sodium difluorophosphate, sodium perchlorate, sodium trifluoromethanesulfonate, sodium bis(oxalatoborate), sodium difluorooxalatoborate, sodium tetrafluoroborate and sodium bis(trifluoromethanesulfonyl)imide; preferably, the mass of the sodium salt is 10-16wt% of the total mass of the sodium ion battery electrolyte.

9. The sodium ion battery electrolyte according to any one of claims 1 to 8, characterized in that The first solvent includes propylene carbonate, ethyl methyl carbonate and diethyl carbonate; the second solvent includes difluoroethyl acetate; the sodium salt includes sodium hexafluorophosphate and sodium bis(fluorosulfonyl)imide; the first additive includes fluoroethylene carbonate and 1,3-propane sultone; and the second additive includes vinyl sulfate.

10. A sodium ion battery, characterized in that: It contains the sodium ion battery electrolyte according to any one of claims 1 to 8.

Citation Information

Patent Citations

  • Electrolyte and electrochemical battery

    CN107293793A

  • Lithium ion battery electrolyte and lithium ion battery

    CN107508000A

  • An electrolyte and a secondary lithium battery suitable for high-temperature environment

    CN108987810A

  • Electrolyte for high-voltage soft package lithium ion battery suitable for high-rate charging and discharging

    CN110707361A

  • Electrolyte and battery

    CN114927756A

Cited By

  • Electrolyte based on propylene carbonate and secondary battery using same

    CN119674219A

  • Low-temperature electrolyte and preparation method and application thereof

    CN120341363A

  • Sodium-ion battery electrolyte and sodium-ion battery prepared therefrom

    WO2026097814A1