Synthesis method of carbon-coated single crystal cobalt nanoparticles
Through gradient high-temperature pyrolysis reduction technology, the problem of preparing carbon-coated single-crystal cobalt nanoparticles in the existing technology is solved, the close interface contact between the cobalt metal and the carbon layer is achieved, and small and uniformly distributed single-crystal cobalt nanoparticles are obtained. , simplifying the process flow and reducing costs, and significantly improving catalytic performance.
Patent Information
- Application Number
- CN202410747189.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-11
- Publication Date
- 2024-10-18
AI Technical Summary
It is difficult to effectively prepare carbon-coated single-crystal cobalt nanoparticles with existing technology, especially in terms of maintaining the single crystallinity and stability of the nanoparticles while avoiding expensive precursors and complex processes.
Gradient high-temperature pyrolysis reduction technology is used to achieve the preparation of carbon-coated single crystal cobalt nanoparticles by ball milling inorganic cobalt salts and citric acid in proportion and then performing a gradient high-temperature pyrolysis reduction reaction in a vacuum atmosphere, avoiding the use of expensive precursors. and redundant craftsmanship.
Successfully prepared cobalt metal as a single crystal and carbon-coated single-crystal cobalt nanoparticles generated in situ by the carbon layer. It has a tight interface structure, small particles and uniform distribution. The process is simple and low-cost. It is suitable for industrialization and has performed well in the field of catalysis. High active sites and excellent interfacial contact.
Smart Images

Figure CN118788972A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for preparing carbon-coated single-crystal cobalt nanoparticles, and belongs to the field of nano material preparation. Background Art
[0002] Metal nanomaterials are widely used in industry and can be used as catalysts to achieve the synthesis of organic matter, catalytic hydrogen production, oxygen production, reduction, etc. However, due to the small size of these nanomaterials, they are easily corroded in acidic and alkaline environments, so they need to be loaded on a carrier in actual use. Carbon materials have good mechanical strength, high stability, and direct strong interface interaction with metal materials, making them ideal carriers for loading metal nanoparticles. Coating a carbon shell on the surface of metal nanoparticles can not only improve the conductivity of the nanoparticles, but also avoid their corrosion process in alkaline environments, thereby obtaining good durability.
[0003] At present, the methods for carbon-encapsulated metal nanoparticles mainly include two-step and one-step synthesis. In the two-step method, molecules or polymers are coated on the surface of pre-synthesized nanoparticles and formed by carbonization (heat treatment in an inert atmosphere). In the one-step method, a carbon source (usually a carbon-containing molecule) is used simultaneously with a precursor of the nanoparticles, and carbon shell-encapsulated nanoparticles are obtained by one-step pyrolysis. The one-step method has the advantages of simplicity and the ability to control the thickness of the carbon layer. Obviously, both methods have their own advantages and disadvantages. The two-step method for preparing carbon-encapsulated / loaded metal nanoparticles is complicated, while the one-step method usually uses expensive precursors to synthesize metal complexes and heat treats them in an inert or reducing atmosphere, which will cause economic limitations. At present, the metal nanoparticles obtained by this method are mostly polycrystalline, and there are no reports of single-crystalline metal nanoparticles. Summary of the invention
[0004] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a method for preparing carbon-coated single-crystalline cobalt nanoparticles, which can achieve the preparation of carbon-coated single-crystalline cobalt nanoparticles through a simple gradient high-temperature pyrolysis reduction technology, without any additives and redundant processes, and without expensive precursors.
[0005] The cobalt metal element in the carbon-coated single crystal cobalt nanoparticles prepared by the present invention is a single crystal material, and both the cobalt and the carbon layer are generated in situ, and there is a strong interface contact between the two. The single crystal cobalt metal nanoparticles are uniformly dispersed on the surface of the carbon layer and are wrapped by the carbon layer, and the relative content of the two can be controlled by changing the ratio of the cobalt salt to the citric acid.
[0006] A method for preparing carbon-coated single-crystal cobalt nanoparticles adopts a gradient high-temperature pyrolysis reduction technology, comprising the following steps: A certain amount of inorganic cobalt salt and citric acid are ball-milled and mixed evenly in proportion, and then the obtained mixture is subjected to a gradient high-temperature pyrolysis reduction reaction in a vacuum atmosphere to obtain carbon-coated single-crystal cobalt nanoparticles.
[0007] Preferably, the inorganic cobalt salt is mainly any one of cobalt nitrate and cobalt chloride.
[0008] Preferably, the mass ratio of the inorganic cobalt salt to the citric acid is 2:1 to 1:4.
[0009] Preferably, the conditions for ball milling mixing are: ball-to-material mass ratio is 10-300:1; ball milling speed is 200-800 rpm; and ball milling time is 1-2 h.
[0010] Preferably, the pyrolysis reduction reaction conditions are: a heating rate of 1 to 5° / min, a low-temperature thermal decomposition temperature of 300°C to 450°C, a reaction time of 1 to 2 hours, and a high-temperature thermal reduction reaction temperature of 450°C to 700°C, a reaction time of 1 to 4 hours. Compared with the prior art, the carbon-coated single-crystal cobalt nanoparticles prepared by the present invention have the following beneficial effects: The cobalt nanoparticles are single crystals, which are produced by in-situ thermal reduction of carbon produced by pyrolysis of citric acid. The gradient temperature pyrolysis reduction ensures the formation of single crystal cobalt. The obtained carbon-coated single crystal cobalt nanoparticles have a close contact interface structure, small particle size and uniform distribution. The reducibility of carbon produced by thermal decomposition of the material itself is used to avoid the need for subsequent reducing atmosphere. The process flow is simple, the cost is low, the equipment requirements are low, and it is easy to realize industrialization. The nanoparticles obtained by the present invention have many active sites and strong interface contact, which has great advantages in the field of catalysis. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 : XRD pattern of carbon-coated single crystal cobalt nanoparticles prepared in Example 1.
[0012] Figure 2 : Transmission electron microscope image of carbon-coated single-crystalline cobalt nanoparticles prepared in Example 1.
[0013] Figure 3 : A high-resolution transmission electron microscopy image of the carbon-coated single-crystalline cobalt nanoparticles prepared in Example 1.
[0014] Figure 4 : A diagram showing the reduction of p-nitrobenzene by carbon-coated single-crystalline cobalt nanoparticles prepared in Example 1.
[0015] Figure 5 : A diagram showing the reduction of p-nitrobenzene by carbon-coated single-crystalline cobalt nanoparticles prepared in Example 2. DETAILED DESCRIPTION
[0016] The present invention is further explained below in conjunction with specific embodiments. It should be understood that these embodiments are only used to illustrate the present invention and are not used to limit the scope of the present invention. After reading the present invention, various equivalent forms of modifications to the present invention by those skilled in the art all fall within the scope defined by the claims attached to this application.
[0017] Example 1 Weigh 0.5g of cobalt nitrate hexahydrate and 0.5g of citric acid into a ball mill, then add 250g of grinding balls, seal it and mill it at 200 rpm for 2h to get a uniform mixture. Then keep the mixed powder at 350℃ for 2h in a vacuum atmosphere, and then keep it at 550℃ for 2h. Wash the product with deionized water 3 times and dry it to get carbon-coated single crystal cobalt nanoparticles. The XRD diffraction pattern of the obtained nanomaterial is as follows: Figure 1 As shown in Figure 2, the product is pure carbon-coated single-crystalline cobalt nanoparticles. The transmission electron microscope image of the nanomaterial is shown in Figure 2. Figure 2 and Figure 3 As shown, it can be seen that the nanoparticles are nanoparticles uniformly wrapped by carbon layers, and the cobalt nanoparticles are in a single crystal state.
[0018] Prepare a 0.02 g / L p-nitrophenol solution, then add 20 mg NaBH4 to 100 mL p-nitrophenol solution, and weigh 1.5 mg of carbon-coated single crystal cobalt nanoparticle catalyst and add it to the p-nitrophenol solution. Take a sample with a filter syringe at the beginning and every five minutes, and put the obtained solution into an ultraviolet-visible absorption spectrometer (UV-vis) for analysis and comparison. It can be found that the absorption peak at 400 nm corresponding to p-nitrophenol gradually decreases, while the absorption peak at 300 nm corresponding to p-aminophenol gradually increases, proving that p-nitrophenol is successfully degraded to p-aminophenol. The degradation rate of p-nitrophenol reaches more than 95% within 40 minutes. The catalyst loading is 0.2 mg cm -2 During OER electrocatalysis, the current density reached 10 mA·cm -2 The required overpotential η 10 is 1.641 V.
[0019] Example 2 Weigh 0.5g of cobalt nitrate hexahydrate and 1.5g of citric acid into a ball mill, then add 300g of grinding balls, seal and mill at 300 rpm for 1h to obtain a uniform mixture. Then keep the mixed powder at 300℃ for 1.5h, and then keep it at 500℃ for 2h in a vacuum atmosphere to obtain carbon-coated single crystal cobalt nanoparticles.
[0020] Prepare a 0.02 g / L p-nitrophenol solution, then add 20 mg NaBH4 to 100 mL of p-nitrophenol solution, and weigh 1.5 mg of carbon-coated single crystal cobalt nanoparticle catalyst and add it to the p-nitrophenol solution. The degradation rate of p-nitrophenol reaches more than 98% within 40 minutes. The catalyst loading is 0.2 mg cm -2 During ORR electrocatalysis, the current density reached 3 mA·cm -2 The required overpotential η 10 is 0.723 V.
[0021] Example 3 Weigh 1g of cobalt nitrate hexahydrate and 1g of citric acid into a ball mill, then add 200g of grinding balls, seal and mill at 500 rpm for 1h to obtain a uniform mixture. Then keep the mixed powder at 400℃ for 2h, and then keep it at 550℃ for 2h to obtain carbon-coated single crystal cobalt nanoparticles.
[0022] Prepare a 0.05 g / L p-nitrophenol solution, then add 30 mg NaBH4 to 100 mL of p-nitrophenol solution, and weigh 1.5 mg of carbon-coated single crystal cobalt nanoparticle catalyst and add it to the p-nitrophenol solution. The degradation rate of p-nitrophenol reaches more than 90% within 40 minutes. The catalyst loading is 0.2 mg cm -2 During OER electrocatalysis, the current density reached 10 mA cm -2 The required overpotential η 10 is 1.36 V.
Claims
1. A method for synthesizing carbon-coated single-crystal cobalt nanoparticles, characterized in that: The main steps include: A certain amount of inorganic cobalt salt and citric acid are ball-milled and mixed evenly in proportion, and then the obtained mixture is subjected to gradient high-temperature pyrolysis reduction in a vacuum atmosphere to obtain carbon-coated single-crystal cobalt nanoparticles.
2. The method for preparing carbon-coated single-crystal cobalt nanoparticles according to claim 1, characterized in that: The inorganic cobalt salt is mainly any one of cobalt nitrate or cobalt chloride.
3. The method for preparing carbon-coated single-crystal cobalt nanoparticles according to claim 1, characterized in that: The mass ratio of inorganic cobalt salt to citric acid is 2:1~1:
4.
4. The method for preparing carbon-coated single-crystal cobalt nanoparticles according to claim 1, characterized in that: The conditions for ball milling mixing are: ball-to-material mass ratio of 100-300:1; ball milling speed of 200-800 rpm; and ball milling time of 1-2 hours.
5. The method for preparing carbon-coated single-crystal cobalt nanoparticles according to claim 1, characterized in that: In step 3, the heating rate is 1~5° / min, and the obtained mixed powder is first pyrolyzed at a relatively low temperature (300℃~450℃) for 1~2h, and then reduced at a relatively high temperature (450℃~700℃) for 1~4h.
6. The method for preparing carbon-coated single-crystal cobalt nanoparticles according to claim 1, characterized in that: The powder obtained in step 5 was washed three times in deionized water.
7. Use of the carbon-coated single-crystal cobalt nanoparticles prepared according to claims 1-6 in catalytic reduction of p-nitrophenol.
8. Use of the carbon-coated single-crystal cobalt nanoparticles prepared according to claims 1 to 6 in electrocatalytic hydrogen evolution; or in electrocatalytic oxygen evolution.
9. Use of the carbon-coated single-crystal cobalt nanoparticles prepared according to claims 1-6 in fuel cells.
10. Use of the carbon-coated single-crystal cobalt nanoparticles prepared according to claims 1-6 in metal-air batteries.