Experimental method for evaluating damage of tight sandstone immersed in fracturing fluid matrix

By conducting multi-directional damage testing and nuclear magnetic resonance analysis on tight sandstone, we can accurately evaluate the degree of damage caused by fracturing fluid to the core, solve the problem of unclear decomposition of damage types in the existing technology, and provide guidance on fracturing fluid formula and process selection. Technical support.

CN118794859APending Publication Date: 2024-10-18SHAANXI YANCHANG PETROLEUM GRP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411004415.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

Existing technology makes it difficult to accurately evaluate the degree of damage caused by fracturing fluids in tight sandstone, especially in terms of water locking, water sensitivity, adsorption, and solid-phase damage types and proportions, resulting in challenges in fracturing fluid formula optimization and process selection.

Method used

An experimental method for matrix damage evaluation of tight sandstone immersed in fracturing fluid was used to calculate the unidirectional and overall matrix damage rates by conducting gas permeability and porosity tests on the core, combined with water lock, water sensitivity, adsorption and solid phase damage tests. , including the damage rate in the horizontal, horizontal, vertical and vertical directions, using the nuclear magnetic resonance T2 spectrum peak integrated area test and the displacement liquid volume record to calculate the damage rate.

Benefits of technology

It achieves accurate evaluation and prediction of the damage degree of fracturing fluid, decomposes different damage types, provides the basis for fracturing construction design and fluid optimization, and solves the problem of result differences caused by the heterogeneity of multiple cores.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118794859A_ABST
    Figure CN118794859A_ABST
Patent Text Reader

Abstract

The invention relates to the field of tight sandstone gas exploration and development, in particular to an experiment method for evaluating damage of tight sandstone immersed in a fracturing fluid matrix. The invention discloses an experimental method for evaluating damage of tight sandstone immersed in a fracturing fluid matrix. The method comprises the following steps: performing gas logging permeability and porosity test on a rock core; carrying out damage test on the rock core, and obtaining the damage rate of the damage test; the damage tests comprise water blocking, water sensitivity, adsorption and solid phase damage tests in sequence, and a water blocking damage rate, a water sensitivity damage rate, an adsorption damage rate and a solid phase damage rate are obtained respectively; the sum of the water blocking damage rate, the water sensitivity damage rate, the adsorption damage rate and the solid phase damage rate is used as the one-way rock core damage rate; and taking the arithmetic average value of the horizontal transverse, horizontal vertical and vertical one-way rock core damage rate as the overall matrix damage rate. The method provides a basic basis for fracturing construction design and fracturing fluid optimization.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of tight sandstone gas exploration and development, and in particular to an experimental method for evaluating matrix damage of tight sandstone immersed in fracturing fluid. Background Art

[0002] The prospect of tight gas, tight sandstone gas has become an important replacement resource for unconventional oil and gas resources. Fracturing transformation is a necessary way to develop tight sandstone gas, which mainly relies on fracturing fluid carrying proppant to create cracks or filter out sandstone reservoirs, providing seepage channels for tight gas production. There are two types of fracturing fluid transformation of reservoirs. One is to communicate micro-cracks to expand the crack size, and the other is that the fracturing fluid filter through the matrix pores to form a combination of filter holes + support cracks to increase the production of tight sandstone gas.

[0003] Due to the weak brittleness and medium plasticity of tight sandstone, matrix filtration transformation plays an important role in fracturing transformation. However, the fracturing fluid enters the matrix to play a transformation role, and forms different degrees of retention in the backflow process, resulting in reduced backflow rate, clay expansion, organic matter retention, residue blockage and other phenomena. How to quantitatively evaluate the degree of retention is the core issue of fracturing fluid damage evaluation. The industry standard SY / T5358-2010 "Reservoir Sensitivity Flow Experiment Evaluation Method" can evaluate the damage performance of fracturing fluid and evaluate the degree of reservoir damage by the change of liquid permeability. However, this standard is only applicable to clastic reservoirs with high air permeability. The damage rate obtained is a general damage rate, and it is impossible to regionalize water sensitivity, water lock, adsorption and solid phase damage types and proportions, and then accurately screen the fracturing fluid formula. In order to further analyze the adaptability of reservoirs and fracturing fluids, it is necessary to explore and form an evaluation method for different types of fracturing fluid damage to provide technical support for fracturing fluid formula optimization and process selection. Summary of the invention

[0004] The main purpose of the present invention is to provide an experimental method for evaluating matrix damage after dense sandstone is immersed in fracturing fluid, aiming to effectively and accurately evaluate and predict the degree of damage of the fracturing fluid.

[0005] The technical solution of the present invention is: (I) An experimental method for evaluating matrix damage of dense sandstone immersed in fracturing fluid, the method is as follows: Conduct gas permeability and porosity tests on cores; Then, the core is subjected to a damage test, and the damage rate of the damage test is obtained; the damage test is water lock, water sensitivity, adsorption and solid phase damage test, and the water lock damage rate, water sensitivity damage rate, adsorption damage rate and solid phase damage rate are obtained respectively; The sum of water lock damage rate, water sensitive damage rate, adsorption damage rate and solid phase damage rate is taken as the one-way core damage rate; The arithmetic mean of the horizontal, vertical and vertical unidirectional core damage rates is taken as the overall matrix damage rate.

[0006] It also includes: the horizontal and transverse one-way core damage rate uses the full-diameter core drilled along the direction of maximum principal stress as the sample for damage test, the horizontal and vertical one-way core damage rate uses the full-diameter core drilled along the direction of minimum principal stress as the sample for damage test, and the vertical one-way core damage rate uses the full-diameter core drilled vertically as the sample for damage test.

[0007] When the sample is tested for gas permeability and porosity, the weight is recorded. m 1 , pore volume V Gas permeability K 1 ; Perform nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 1 .

[0008] The specific process of the damage test is as follows: the dry core is displaced with the damage fluid, the displacement is stopped after the displacement flow is stable, closed aging is carried out at the formation temperature, and then reverse gas drive is carried out, and the test is stopped after the gas drive flow is stable to complete the damage test; the effective displacement fluid volume at each stage of the damage test is recorded separately m n1 , Gas phase displacement liquid volume m n2 , damage test gas test permeability K n and core retention Δ m n ; Conduct MRI at each stage of injury testing T 2 Spectral peak integral area test, record NMR T 2 Spectral area S n ; Among them, 2≤ n ≤5, n Take the integer.

[0009] Among them, the damaging fluids of the damage test are formation mineralized water, distilled water, fracturing gel-breaking fluid filtrate and fracturing fluid in sequence.

[0010] Also included: the calculation process of the injury rate of the injury test is: P =(λ+ T + R ) / 3; Where λ=( K n-1 - K n ) / K 2 ; T =Δ m n / ( pV )×100%;Δ m n = m n1 - m n2 ; R =( S n-1 - S n ) / S 2 ; In the formula, P is the injury rate, dimensionless; λ is the gas measurement damage rate, dimensionless; T is the liquid retention rate, dimensionless; R For NMR T 2 The damage rate is calculated from the spectrum area and is dimensionless; r is the density of the damaging liquid, g / cm 3 ; V is the pore volume, cm 3 ; The water lock damage rate, water sensitive damage rate, adsorption damage rate and solid phase damage rate are calculated by the above formula respectively.

[0011] (II) An experimental method for evaluating matrix damage of dense sandstone immersed in fracturing fluid, the method is as follows: 1) preparing samples from full-diameter cores of dense sandstone, including horizontal transverse samples, horizontal vertical samples and vertical samples, and performing drying treatment; 2) Use the gas permeability test device to test the gas permeability of the sample K and porosity test, record the weight as m 1 , gas permeability K 1 and pore volume V ; Conduct nuclear magnetic resonance using a nuclear magnetic resonance instrument T 2 Spectral peak integral area test, record NMR T 2 Spectral areaS 1 ; 3) The damaging fluid is mineralized water from the formation. The sample is displaced using a liquid / gas core displacement device. The displacement is stopped after the displacement flow rate is stable. The sample is sealed and aged at the formation temperature. Then, nitrogen reverse gas drive is carried out. The test is stopped after the gas drive flow rate is stable. The water lock damage test is completed. The effective displacement fluid volume in the water lock damage test is recorded. m 21 , Gas phase displacement liquid volume m 22 , test gas permeability K 2 ; Conducting nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 2 ; Calculate the core retention Δ m 2 ; 4) Replace the damaging liquid with distilled water and repeat 3) to complete the water-sensitive damage test; record the effective displacement liquid volume in the water-sensitive damage test m 31 , Gas phase displacement liquid volume m 32 , test gas permeability K 3 ; Conducting nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 3 ; Calculate the core retention Δ m 3 ; 5) Replace the damaging fluid with the filtrate of the fracturing gel breaking fluid, repeat 3) to complete the adsorption damage test; record the effective displacement fluid volume in the adsorption damage test m 41 , Gas phase displacement liquid volume m 42 , test gas permeability K 4 ; Conducting nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 4 ; Calculate the core retention Δ m 4 ; 6) Replace the damaging fluid with fracturing fluid and repeat step 3) to complete the solid phase damage test; record the effective displacement fluid volume in the solid phase damage test m 51 , Gas phase displacement liquid volume m 52 , test gas permeability K 5 ; Conducting nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 5 ; Calculate the core retention Δ m 5 ; The gas test damage rate λ + liquid retention rate of each sample in each damage test was calculated separately T +NMR T 2 Spectral area, and then the water lock damage rate, water sensitive damage rate, adsorption damage rate and solid phase damage rate of each sample were obtained; The sum of the water lock damage rate, water sensitivity damage rate, adsorption damage rate and solid phase damage rate of the same sample is taken as the one-way core damage rate; the one-way core damage rate includes the horizontal transverse core damage rate, the horizontal vertical core damage rate and the vertical core damage rate; The arithmetic average of the horizontal transverse core damage rate, the horizontal vertical core damage rate and the vertical core damage rate is taken as the overall matrix damage rate.

[0012] The coring directions of the full-diameter core of the dense sandstone are the maximum horizontal principal stress direction, the minimum horizontal principal stress direction and the vertical direction, a total of three directions.

[0013] Among them, the displacement volume of the damaging fluid is 0.5-2.0 ml / min; the gas displacement pressure of the reverse gas drive of each damaging test is equal; the closed aging time is not less than 48 hours; and the gas drive flow rate is stable for not less than 60 minutes.

[0014] The viscosity of the fracturing fluid is 50-80 mPa.s at the formation temperature and the heat and shear resistance value.

[0015] The technical effects of the present invention are: (1) This experimental method proposes a new method for evaluating the damage of fracturing fluid after it enters tight sandstone, clarifies the test method of the same damage type of fracturing fluid, solves the problem of a single method for evaluating tight sandstone gas damage, evaluates water lock, water sensitivity, adsorption and solid phase damage rates one by one, and further obtains the unidirectional core damage rate. The unidirectional core damage rates in multiple directions are tested, and the overall matrix damage rate of the core in this layer is comprehensively obtained, providing a basic basis for fracturing construction design and fracturing fluid optimization; (2) Matrix permeability. Dry samples of dense sandstone porous media will cause damage to the matrix during the fracturing process. The damage types are divided into water lock, water sensitivity, adsorption and solid damage. In order to describe the damage type, it is necessary to first evaluate the water lock damage and remove the influence of other damages. Secondly, water sensitivity damage is carried out to determine the influence of clay expansion, and then polymer adsorption damage is carried out. After the evaluation of water lock and water sensitivity damage, adsorption damage can be carried out to determine the damage of polymer electrostatic adsorption, chemical adsorption, etc. Finally, solid damage is evaluated, including impurities, clay migration and other damages. Through the above damage evaluation, a single type of reservoir damage can be determined separately, and the overall matrix damage rate can also be calculated. The test process designed by the present invention realizes the use of the same core to test different damage types and the overall matrix damage rate, solving the problem of large differences in results caused by the heterogeneity of multiple cores. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 Schematic diagram of sampling position of full-diameter core of dense sandstone in the present invention. DETAILED DESCRIPTION

[0017] Example 1 An experimental method for evaluating matrix damage of dense sandstone immersed in fracturing fluid is as follows: Conduct gas permeability and porosity tests on cores; Then, the core is subjected to a damage test, and the damage rate of the damage test is obtained; the damage test is water lock, water sensitivity, adsorption and solid phase damage test, and the water lock damage rate, water sensitivity damage rate, adsorption damage rate and solid phase damage rate are obtained respectively; The sum of water lock damage rate, water sensitive damage rate, adsorption damage rate and solid phase damage rate is taken as the one-way core damage rate; The arithmetic mean of the horizontal transverse, horizontal vertical and vertical unidirectional core damage rates is taken as the overall matrix damage rate; It also includes: the horizontal and transverse one-way core damage rate uses the full-diameter core drilled along the direction of maximum principal stress as the sample for damage test, the horizontal and vertical one-way core damage rate uses the full-diameter core drilled along the direction of minimum principal stress as the sample for damage test, and the vertical one-way core damage rate uses the full-diameter core drilled vertically as the sample for damage test.

[0018] Example 2 On the basis of Example 1, it also includes: When the sample is tested for gas permeability and porosity, the weight is recorded. m 1 , pore volume V Gas permeability K 1 ; Perform nuclear magnetic resonance T 2Spectral peak integral area test, record NMR T 2 Spectral area S 1 .

[0019] Example 3 On the basis of Example 2, the invention further includes: The specific process of the damage test is: displacing the dry core with the damage fluid, stopping the displacement after the displacement flow is stable, sealing and aging at the formation temperature, and then carrying out reverse gas drive, stopping the test after the gas drive flow is stable, and completing the damage test; recording the effective displacement fluid volume at each stage of the damage test m n1 , Gas phase displacement liquid volume m n2 , damage test gas test permeability K n and core retention Δ m n ; Conduct MRI at each stage of injury testing T 2 Spectral peak integral area test, record NMR T 2 Spectral area S n ; Among them, 2≤ n ≤5, n Take the integer; Among them, the damaging fluids of the damage test are formation mineralized water, distilled water, fracturing gel-breaking fluid filtrate and fracturing fluid in sequence.

[0020] Example 4 On the basis of Example 3, the invention further includes: The calculation process of the injury rate of the injury test is: P =(λ+ T + R ) / 3; Where λ=( K n-1 - K n ) / K 2 ; T =Δ m n / ( pV )×100%;Δ m n = m n1 - m n2 ; R =(S n-1 - S n ) / S 2 ; In the formula, P is the injury rate, dimensionless; λ is the gas measurement damage rate, dimensionless; T is the liquid retention rate, dimensionless; R For NMR T 2 The damage rate is calculated from the spectrum area and is dimensionless; r is the density of the damaging liquid, g / cm 3 ; V is the pore volume, cm 3 ; The water lock damage rate, water sensitive damage rate, adsorption damage rate and solid phase damage rate are calculated by the above formula respectively.

[0021] Example 5 An experimental method for evaluating matrix damage of dense sandstone immersed in fracturing fluid is as follows: 1) preparing samples from full-diameter cores of dense sandstone, including horizontal transverse samples, horizontal vertical samples and vertical samples, and performing drying treatment; 2) Use the gas permeability test device to test the gas permeability of the sample K and porosity test, record the weight as m 1 , gas permeability K 1 and pore volume V ; Conduct nuclear magnetic resonance using a nuclear magnetic resonance instrument T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 1 ; 3) The damaging fluid is mineralized water from the formation. The sample is displaced using a liquid / gas core displacement device. The displacement is stopped after the displacement flow rate is stable. The sample is sealed and aged at the formation temperature. Then, nitrogen reverse gas drive is carried out. The test is stopped after the gas drive flow rate is stable. The water lock damage test is completed. The effective displacement fluid volume in the water lock damage test is recorded. m 21 , Gas phase displacement liquid volume m 22 , test gas permeability K 2 ; Conducting nuclear magnetic resonance T2 Spectral peak integral area test, record NMR T 2 Spectral area S 2 ; Calculate the core retention Δ m 2 ; 4) Replace the damaging liquid with distilled water and repeat 3) to complete the water-sensitive damage test; record the effective displacement liquid volume in the water-sensitive damage test m 31 , Gas phase displacement liquid volume m 32 , test gas permeability K 3 ; Conducting nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 3 ; Calculate the core retention Δ m 3 ; 5) Replace the damaging fluid with the filtrate of the fracturing gel breaking fluid, repeat 3) to complete the adsorption damage test; record the effective displacement fluid volume in the adsorption damage test m 41 , Gas phase displacement liquid volume m 42 , test gas permeability K 4 ; Conducting nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 4 ; Calculate the core retention Δ m 4 ; 6) Replace the damaging fluid with fracturing fluid and repeat step 3) to complete the solid phase damage test; record the effective displacement fluid volume in the solid phase damage test m 51 , Gas phase displacement liquid volume m 52 , test gas permeability K 5 ; Conducting nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 5 ; Calculate the core retention Δ m 5 ; The gas test damage rate λ + liquid retention rate of each sample in each damage test was calculated separately T +NMR T 2 Spectral area, and then the water lock damage rate, water sensitive damage rate, adsorption damage rate and solid phase damage rate of each sample were obtained; The sum of the water lock damage rate, water sensitivity damage rate, adsorption damage rate and solid phase damage rate of the same sample is taken as the one-way core damage rate; the one-way core damage rate includes the horizontal transverse core damage rate, the horizontal vertical core damage rate and the vertical core damage rate; The arithmetic average of the horizontal transverse core damage rate, the horizontal vertical core damage rate and the vertical core damage rate is taken as the overall matrix damage rate.

[0022] The coring directions of the full-diameter core of the dense sandstone are the maximum horizontal principal stress direction, the minimum horizontal principal stress direction and the vertical direction, a total of three directions.

[0023] Among them, the displacement volume of the damaging fluid is 0.5-2.0 ml / min; the gas displacement pressure of the reverse gas drive of each damaging test is equal; the closed aging time is not less than 48 hours; and the gas drive flow rate is stable for not less than 60 minutes.

[0024] The viscosity of the fracturing fluid is 50-80 mPa.s at the formation temperature and the heat and shear resistance value.

[0025] Among them, the liquid retention is calculated by recording the effective displacement liquid volume and gas phase displacement liquid volume during the water lock, water sensitivity, adsorption and solid damage tests. The liquid retention in different test processes is calculated. The retained liquid plays two roles in the core: one is the role of imbibition and displacement, which can increase the permeability, and the other is the absorption damage, which causes damage to the core. Combined with gas permeability and nuclear magnetic resonance T 2 Spectral area, the greater the retention during the test, the lower the gas permeability, showing a negative correlation, but there will be a phenomenon that the retention is positive and the damage rate is negative. If only the damage rate is evaluated, the damage rate will be negative, showing a displacement effect, but the retention rate is positive. From the analysis of the damage mechanism, liquid retention will hinder gas production and cause damage. Therefore, the permeability will be negative before and after the damage is tested alone, but the damage size can be judged after the retention rate is introduced, and then combined with nuclear magnetic resonance T 2 The change of spectral peak area was used to further evaluate the injury rate.

[0026] Specific experimental cases An experimental method for evaluating matrix damage of dense sandstone immersed in fracturing fluid is as follows: 1) Sample preparation: According to the reservoir in-situ stress test data, full-diameter cores were selected along the maximum principal stress direction, minimum principal stress direction and vertical direction. Figure 1 Three cores were drilled in the sampling direction as samples, which were horizontal transverse samples, horizontal vertical samples and vertical samples, respectively, with a diameter of 25±0.5 mm, a length of 80 mm, and an end surface flatness of 0.1 mm. The horizontal transverse samples, horizontal vertical samples and vertical samples were dried and set aside; 2) Use the liquid / gas core displacement device to test horizontal transverse samples, horizontal vertical samples and vertical samples; take the horizontal transverse sample as an example to obtain the gas permeability K 1 =0.0952×10 -3 μm 2 , porosity is 4.78%, weight m 1 =96.5g, pore volume V =1.87 cm 3 ; Conduct nuclear magnetic resonance using a nuclear magnetic resonance instrument T 2 Peak integral area test, record S 1 =6998.25; 3) Water lock test: The damaging fluid is mineralized water from the formation. The horizontal transverse sample, horizontal vertical sample and vertical sample are displaced by using a liquid / gas phase core displacement device. The displacement flow rate is 0.5 ml / min. The displacement is stopped after the displacement flow rate is stable. The samples are sealed and aged for 48 hours at the formation temperature. Then, nitrogen reverse gas drive is carried out. The test is stopped after no liquid flows out and the gas drive flow rate is stable. The water lock damage test is completed. Taking the horizontal transverse sample as an example, the effective displacement liquid volume in the water lock damage test is recorded. m 21 =2.4256g, gas phase displacement liquid volume m 22 =2.0599g, gas permeability K 2 =0.0816mD; Conduct NMR T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 2 =5825.75; Calculate the core retention Δ m 2 =0.3657g; 4) Replace the damaging liquid with distilled water and repeat 3) to complete the water-sensitive damage test; taking the horizontal sample as an example, record the effective displacement liquid volume in the water-sensitive damage test m 31=1.7698g, gas phase displacement liquid volume m 32 =1.4623g, gas permeability K 3 =0.0691mD; Conduct NMR T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 3 =4820.26; Calculate the core retention Δ m 3 =0.3075g; 5) Replace the damaging fluid with the filtrate of the fracturing gel breaking fluid, repeat 3) to complete the adsorption damage test; take the horizontal sample as an example, record the effective displacement fluid volume in the adsorption damage test m 41 =1.3525g, gas phase displacement liquid volume m 42 =1.1559g, gas permeability K 4 =0.0615mD; Conduct NMR T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 4 =4281.58; the core retention volume Δ is calculated m 4 =0.1966g; 6) Replace the damaging fluid with a fracturing fluid containing a gel breaker, repeat step 3), and complete the solid phase damage test; take the horizontal sample as an example, and record the effective displacement fluid volume in the solid phase damage test. m 51 =2.0265g, gas phase displacement liquid volume m 52 =1.8737g, gas permeability K 5 =0.0551 mD; conduct NMR T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 5 =3755.82; the core retention volume Δ is calculated m 5 =0.1528g; The water lock damage rate, water sensitive damage rate, adsorption damage rate and solid phase damage rate of horizontal samples were calculated by the above formula respectively; The sum of the water lock damage rate, water sensitive damage rate, adsorption damage rate and solid phase damage rate of the horizontal transverse sample is taken as the horizontal transverse unidirectional core damage rate; the parameter values ​​are shown in Table 1; Table 1. Parameter values ​​of horizontal and unidirectional core damage rate According to the same method as above, the horizontal and vertical unidirectional core damage rates and vertical unidirectional core damage rates were tested and the arithmetic average of the horizontal and vertical core damage rates and the vertical core damage rates was taken as the overall matrix damage rate.

[0027] Table 2. Overall matrix damage rate .

Claims

1. An experimental method for evaluating matrix damage of dense sandstone immersed in fracturing fluid, Features: Here’s how: Conduct gas permeability and porosity tests on cores; Then, the core is subjected to a damage test, and the damage rate of the damage test is obtained; the damage test is water lock, water sensitivity, adsorption and solid phase damage test, and the water lock damage rate, water sensitivity damage rate, adsorption damage rate and solid phase damage rate are obtained respectively; The sum of water lock damage rate, water sensitive damage rate, adsorption damage rate and solid phase damage rate is taken as the one-way core damage rate; The arithmetic mean of the horizontal, vertical and vertical unidirectional core damage rates is taken as the overall matrix damage rate.

2. According to the experimental method for evaluating matrix damage of dense sandstone immersed in fracturing fluid as described in claim 1, Features: Also includes: The horizontal and transverse unidirectional core damage rate is tested by taking the cores drilled from the full-diameter core along the direction of the maximum principal stress as the horizontal and transverse samples. The horizontal and vertical unidirectional core damage rate is tested by taking the cores drilled from the full-diameter core along the direction of the minimum principal stress as the horizontal and vertical samples. The vertical unidirectional core damage rate is tested by taking the cores drilled from the full-diameter core along the vertical direction as the vertical samples.

3. The experimental method for evaluating matrix damage of dense sandstone immersed in fracturing fluid according to claim 2, Features: When the sample is tested for gas permeability and porosity, the weight is recorded. m 1 , pore volume V Gas permeability K 1 ; Perform nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 1 .

4. The method for evaluating matrix damage of dense sandstone immersed in fracturing fluid according to claim 2, Features: The specific process of the damage test is: displacing the dry core with the damage fluid, stopping the displacement after the displacement flow is stable, sealing and aging at the formation temperature, and then carrying out reverse gas drive, stopping the test after the gas drive flow is stable, and completing the damage test; recording the effective displacement fluid volume at each stage of the damage test m n1 , Gas phase displacement liquid volume m n2 , damage test gas permeability test K n and core retention Δ m n ; Conduct MRI at each stage of injury testing T 2 Spectral peak integral area test, record NMR T 2 Spectral area S n ; Among them, 2≤ n ≤5, n Take the integer.

5. The method for evaluating matrix damage of dense sandstone immersed in fracturing fluid according to claim 4, Features: The damaging fluids of the damage test are formation mineralized water, distilled water, fracturing gel-breaking fluid filtrate and fracturing fluid.

6. The method for evaluating matrix damage of dense sandstone immersed in fracturing fluid according to claim 4, Features: The calculation process of the injury rate of the injury test is: P =(λ+ T + R ) / 3; Where λ=( K n-1 - K n ) / K 2 ; T =D m n / ( ρV )×100%;D m n = m n1 - m n2 ; R =( S n-1 - S n ) / S 2 ; In the formula, P is the injury rate, dimensionless; λ is the gas measurement damage rate, dimensionless; T is the liquid retention rate, dimensionless; R For NMR T 2 The damage rate is calculated from the spectrum area and is dimensionless; ρ is the density of the damaging liquid, g / cm 3 ; V is the pore volume, cm 3 ; The water lock damage rate, water sensitive damage rate, adsorption damage rate and solid phase damage rate are calculated by the above formula respectively.

7. The experimental method for evaluating matrix damage of dense sandstone immersed in fracturing fluid according to claim 1, Features: The method is as follows: 1) preparing samples from full-diameter cores of dense sandstone, including horizontal transverse samples, horizontal vertical samples and vertical samples, and performing drying treatment; 2) Use the gas permeability test device to test the gas permeability of the sample K and porosity test, record the weight as m 1 , gas permeability K 1 and pore volume V ; Use nuclear magnetic resonance imaging to carry out nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 1 ; 3) The damaging fluid is mineralized water from the formation. The sample is displaced using a liquid / gas core displacement device. The displacement is stopped after the displacement flow rate is stable. The sample is sealed and aged at the formation temperature. Then, nitrogen reverse gas drive is carried out. The test is stopped after the gas drive flow rate is stable. The water lock damage test is completed. The effective displacement fluid volume in the water lock damage test is recorded. m 21 , Gas phase displacement liquid volume m 22 , test gas permeability K 2 ; Conducting nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 2 ; Calculate the core retention Δ m 2 ; 4) Replace the damaging liquid with distilled water and repeat 3) to complete the water-sensitive damage test; record the effective displacement liquid volume in the water-sensitive damage test m 31 , Gas phase displacement liquid volume m 32 , test gas permeability K 3 ; Conducting nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 3 ; Calculate the core retention Δ m 3 ; 5) Replace the damaging fluid with the filtrate of the fracturing gel breaking fluid, repeat 3) to complete the adsorption damage test; record the effective displacement fluid volume in the adsorption damage test m 41 , Gas phase displacement liquid volume m 42 , test gas permeability K 4 ; Conduct nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 4 ; Calculate the core retention Δ m 4 ; 6) Replace the damaging fluid with fracturing fluid and repeat step 3) to complete the solid phase damage test; record the effective displacement fluid volume in the solid phase damage test m 51 , Gas phase displacement liquid volume m 52 , test gas permeability K 5 ; Conducting nuclear magnetic resonance T 2 Spectral peak integral area test, record NMR T 2 Spectral area S 5 ; Calculate the core retention Δ m 5 ; The gas test damage rate λ + liquid retention rate of each sample in each damage test was calculated separately T +NMR T 2 Spectral area, and then the water lock damage rate, water sensitive damage rate, adsorption damage rate and solid phase damage rate of each sample were obtained; The sum of the water lock damage rate, water sensitivity damage rate, adsorption damage rate and solid phase damage rate of the same sample is taken as the one-way core damage rate; the one-way core damage rate includes the horizontal transverse core damage rate, the horizontal vertical core damage rate and the vertical core damage rate; The arithmetic average of the horizontal transverse core damage rate, the horizontal vertical core damage rate and the vertical core damage rate is taken as the overall matrix damage rate.

8. The method for evaluating matrix damage of dense sandstone immersed in fracturing fluid according to claim 7, Features: The coring directions of the full-diameter core of the dense sandstone are three directions, namely, the direction of maximum horizontal principal stress, the direction of minimum horizontal principal stress and the vertical direction.

9. The method for evaluating matrix damage of dense sandstone immersed in fracturing fluid according to claim 7, Features: The displacement volume of the damaging fluid is 0.5-2.0 ml / min; the gas displacement pressure of the reverse gas drive of each damaging test is equal; the closed aging time is not less than 48 hours; and the gas drive flow rate is stable for not less than 60 minutes.

10. The experimental method for evaluating matrix damage of dense sandstone immersed in fracturing fluid according to claim 7, Features: The viscosity of the fracturing fluid is a heat and shear resistance value of 50-80 mPa.s at the formation temperature.