Preparation method of semiconductor structure

By using etching stop layers and chemical mechanical polishing technology in the preparation of semiconductor components to form trenches and deposit conductive materials, the problems of component flatness and uniformity are solved, and the electrical performance and reliability of the semiconductor structure are improved.

CN118804591APending Publication Date: 2024-10-18NAN YA TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410476152.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-04-11
Filing Date
2023-09-27
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

During semiconductor device fabrication, as device dimensions shrink and distances decrease, maintaining flatness and uniformity becomes a challenge, resulting in limitations in device reliability and performance.

Method used

An etch stop layer is used to protect the landing pad during the planarization process, and trenches are formed in the conductive pad and dielectric layer through chemical mechanical polishing operations to ensure a high degree of uniformity and electrical reliability of the conductive pad, followed by deposition of conductive material to form Conductive vias and bit lines further improve memory cell performance.

Benefits of technology

It achieves a high degree of planarization of the semiconductor structural material layer, improves the uniformity of component quality and electrical performance, reduces the cost of process changes, and enhances the reliability of memory cells and equipment reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118804591A_ABST
    Figure CN118804591A_ABST
Patent Text Reader

Abstract

The invention provides a preparation method of a semiconductor structure. The method comprises the following steps: forming a word line in a first dielectric layer, wherein the first dielectric layer is positioned above a substrate; forming a channel layer to pass through the word line; forming a conductive material over the channel layer; forming an etch stop layer over the conductive material; patterning the etch stop layer to form a pattern of a conductive pad; etching the conductive material by using the pattern of the etch stop layer as an etch mask to form a conductive pad; depositing a second dielectric layer over the etch stop layer and the first dielectric layer; planarizing the second dielectric layer, wherein at least a portion of the etch stop layer is left on the conductive pad after planarizing; and forming a second trench in the second dielectric layer by etching a portion of the conductive pad and a portion of the second dielectric layer. Forming the second trench causes a bit line formed in the second trench to electrically couple with the conductive pad.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of Chinese invention patent application No. 2023112641072, filed on September 27, 2023, with the invention name of “Semiconductor structure and preparation method thereof”. Application No. 2023112641072 claims priority and benefits of U.S. formal application No. 18 / 133,056 filed on April 11, 2023. The contents of the U.S. formal application are incorporated herein by reference in their entirety. Technical Field

[0002] The present disclosure relates to a semiconductor structure and a method for manufacturing the same. In particular, the present disclosure includes a semiconductor memory structure and a method for manufacturing the same. Background Art

[0003] As the semiconductor industry moves into advanced technology nodes, it has achieved advanced precision in lithography in pursuit of higher device performance and higher device density. To further reduce device size, component size and the distance between different components must be reduced proportionally. However, as component size decreases and the distance between different components decreases, challenges arise in precisely controlling size and distance.

[0004] One of the issues with shrinking semiconductor components is the flatness of the components across the semiconductor wafer. In order to maintain quality consistency between different semiconductor component levels, high flatness uniformity needs to be achieved between a single semiconductor wafer and between different semiconductor wafers to ensure that the component layer achieves high flatness uniformity. However, when preparing semiconductor components, the flatness of the prepared semiconductor components is usually limited by the limitations of shrinking the equipment footprint and the various material layers involved in the planarization process. Therefore, it is necessary to study improved methods and structures to provide reliable planarization solutions to ensure the reliability and performance of semiconductor components.

[0005] The above “prior art” description is only to provide background technology, and does not admit that the above “prior art” description reveals the subject matter of the present disclosure, does not constitute the prior art of the present disclosure, and any description of the above “prior art” should not be regarded as any part of this case. Summary of the invention

[0006] One aspect of the present disclosure provides a method for preparing a semiconductor structure. The preparation method includes: forming a word line in a first dielectric layer, the first dielectric layer is located above a substrate; forming a channel layer passing through the word line; forming a conductive material above the channel layer; forming an etch stop layer above the conductive material; patterning the etch stop layer to form a pattern of a conductive pad; etching the conductive material using the pattern of the etch stop layer as an etch mask to form a conductive pad; depositing a second dielectric layer above the etch stop layer and the first dielectric layer; planarizing the second dielectric layer, wherein at least a portion of the etch stop layer is left on the conductive pad after planarization; and forming a second trench in the second dielectric layer by etching a portion of the conductive pad and a portion of the second dielectric layer. Forming the second trench causes a bit line formed in the second trench to be electrically coupled to the conductive pad.

[0007] According to some embodiments of the present disclosure, planarizing includes using a chemical mechanical polishing operation.

[0008] According to some embodiments of the present disclosure, during a chemical mechanical polishing operation, the etch stop layer is flush with the second dielectric layer.

[0009] According to some embodiments of the present disclosure, the preparation method further includes removing the entire etch stop layer from the conductive pad.

[0010] According to some embodiments of the present disclosure, removing the entire etch stop layer will leave a first trench in the second dielectric layer, and further includes depositing the conductive material over the second dielectric layer and in the first trench.

[0011] According to some embodiments of the present disclosure, the preparation method further includes thinning the conductive material to expose the second dielectric layer.

[0012] According to some embodiments of the present disclosure, the substrate includes a first region and a second region, the conductive pad is disposed in the first region of the substrate, and further includes etching a through hole in the second region before the conductive material is deposited in the first trench.

[0013] According to some embodiments of the present disclosure, the step of depositing the conductive material in the first trench includes filling the via with the conductive material to form a conductive via.

[0014] According to some embodiments of the present disclosure, the step of depositing the conductive material in the first trench includes filling the via with the conductive material to form a conductive via.

[0015] According to some embodiments of the present disclosure, the preparation method further includes forming a second trench in the second dielectric layer by etching a portion of the conductive pad and a portion of the second dielectric layer.

[0016] According to some embodiments of the present disclosure, forming the second trench may result in a bit line formed in the second trench being electrically coupled to the conductive pad.

[0017] According to some embodiments of the present disclosure, the preparation method further includes depositing a third dielectric layer to fill the second trench.

[0018] According to some embodiments of the present disclosure, the preparation method further includes forming a capacitor in a fourth dielectric layer, where the fourth dielectric layer is located below the first dielectric layer.

[0019] According to some embodiments of the present disclosure, the preparation method further includes depositing an insulating film on a side wall of the word line before forming the channel layer.

[0020] According to some embodiments of the present disclosure, the second dielectric layer laterally surrounds the conducting pad.

[0021] One aspect of the present disclosure provides a method for fabricating a semiconductor structure. The method includes: forming a data storage unit in a first dielectric layer; depositing a word line above the data storage unit; forming a conductive material above the word line; forming a patterned hard mask layer above the conductive material; etching the conductive material through the patterned hard mask layer to form a conductive pad; depositing a second dielectric layer above the patterned hard mask layer; and removing the second dielectric layer, wherein at least a portion of the patterned hard mask layer is left during the removal.

[0022] According to some embodiments of the present disclosure, the preparation method further includes removing the etching stop layer.

[0023] According to some embodiments of the present disclosure, the preparation method further includes forming a first conductive oxide layer through the word line.

[0024] According to some embodiments of the present disclosure, the first conductive oxide layer includes indium gallium zinc oxide.

[0025] According to some embodiments of the present disclosure, the preparation method further includes depositing a second conductive oxide layer on the first conductive oxide layer and the word line before depositing the conductive material.

[0026] According to some embodiments of the present disclosure, the second oxide layer includes titanium indium oxide.

[0027] According to some embodiments of the present disclosure, the patterned hard mask is formed of a different material than the first dielectric layer.

[0028] According to some embodiments of the present disclosure, the preparation method further includes depositing a third dielectric layer to cover the second dielectric layer.

[0029] According to some embodiments of the present disclosure, the second dielectric layer is removed so that the upper surface of the second dielectric layer is flush with the upper surface of the third dielectric layer.

[0030] According to some embodiments of the present disclosure, the preparation method further includes depositing another portion of the conductive material on the conductive pad after removing the patterned hard mask.

[0031] Through the planarization scheme proposed in the present disclosure, the material layer of the semiconductor structure can be highly planarized, and the electrical performance and reliability can be further improved. Therefore, the uniformity of component quality can be improved while minimizing the additional cost of process changes.

[0032] The above has outlined the technical features and advantages of the present disclosure in a fairly broad manner, so that the detailed description of the present disclosure below can be better understood. Other technical features and advantages that constitute the subject matter of the claims of the present disclosure will be described below. It should be understood by those with ordinary knowledge in the technical field to which the present disclosure belongs that the concepts and specific embodiments disclosed below can be used to modify or design other structures or processes to achieve the same purpose as the present disclosure. It should also be understood by those with ordinary knowledge in the technical field to which the present disclosure belongs that such equivalent constructions cannot depart from the spirit and scope of the present disclosure as defined by the appended claims. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] A more complete understanding of the disclosure of the present application may be obtained by referring to the embodiments and claims in conjunction with the drawings, in which the same reference numerals refer to the same elements.

[0034] Figure 1A , Figure 1B , Figure 1C , Figure 1D , Figure 1E , Figure 1F , Figure 1G , Figure 1H , Fig. 1I , Figure 1J , Figure 1K , Figure 1L , Figure 1M , Figure 1N , Fig.1O , Figure 1P , Figure 1Q , Figure 1R , Figure 1S , Figure 1T , Figure 1U , Figure 1V , Figure 1W , Figure 1X , Figure 1Y , Figure 1Z , Figure 1AA and Fig. 1AB2 is a cross-sectional view illustrating an intermediate stage of a method for fabricating a semiconductor structure according to some embodiments of the present disclosure.

[0035] Figure 2 1 is a top view illustrating a semiconductor structure according to some embodiments of the present disclosure.

[0036] Figures 3A to 3G 2 is a cross-sectional view illustrating an intermediate stage of a method for preparing a semiconductor structure in some comparative embodiments of the present disclosure.

[0037] Figure 4A , Figure 4B and Figure 4C The flowchart illustrates a method for preparing a semiconductor structure according to some embodiments of the present disclosure.

[0038] The reference numerals are described as follows:

[0039] 100: Semiconductor structure

[0040] 100A: First Area

[0041] 100B: Second area

[0042] 104: Active area

[0043] 106: Semiconductor components

[0044] 110: Base

[0045] 112: Dielectric layer

[0046] 114: Conductive vias

[0047] 120: First floor

[0048] 124: Data storage unit

[0049] 126: Conductive layer

[0050] 128: Pad

[0051] 132: Dielectric layer

[0052] 134: Dielectric layer

[0053] 140: Second floor

[0054] 142: Dielectric layer

[0055] 142T: Groove

[0056] 144: Conductive pad

[0057] 146: Conductive thread

[0058] 148: Character line

[0059] 151: Conductive oxide layer

[0060] 152: Channel layer

[0061] 153: Insulation film

[0062] 154: Insulation film

[0063] 161: Conductive materials

[0064] 162: Conductive layer

[0065] 163: Conductive materials

[0066] 164: Conductive pad

[0067] 165: Etch stop layer

[0068] 166: Patterned etch stop layer

[0069] 166P: Space

[0070] 167: Hard Mask Layer

[0071] 168: Patterned hard mask layer

[0072] 169: Mask layer

[0073] 169: Photoresist

[0074] 170: Patterned mask layer

[0075] 170: Patterned photoresist

[0076] 170P: Pattern

[0077] 172: Photoresist

[0078] 174: Dielectric layer

[0079] 174R: Partial

[0080] 174S: Upper surface

[0081] 174T: Groove

[0082] 176: Dielectric layer

[0083] 176S: Upper surface

[0084] 176T: Through hole

[0085] 178: Conductive materials

[0086] 180: Tools

[0087] 182: Conductive pad

[0088] 182T: Partial

[0089] 184: Conductive vias

[0090] 185: Conductive layer

[0091] 186: Dielectric layer

[0092] 186T: Groove

[0093] 187: Conductive pad

[0094] 188: Bit Line

[0095] 190: Dielectric layer

[0096] 192: Conductive vias

[0097] 206: Isolation Area

[0098] 274: Dielectric layer

[0099] 276: Dielectric layer

[0100] 300: Semiconductor structure

[0101] 301: Semiconductor structure

[0102] 364: Conductive pad

[0103] 374: Dielectric layer

[0104] 376: Dielectric layer DETAILED DESCRIPTION

[0105] The following description of the present disclosure is accompanied by the drawings which are incorporated into and constitute a part of the specification, and illustrate embodiments of the present disclosure, but the present disclosure is not limited to the embodiments. In addition, the following embodiments can be appropriately integrated to complete another embodiment.

[0106] "One embodiment", "an embodiment", "an exemplary embodiment", "another embodiment", "another embodiment", etc. mean that the embodiment described in the present disclosure may include specific features, structures or characteristics, but not every embodiment must include the specific features, structures or characteristics. Furthermore, repeated use of the phrase "in an embodiment" does not necessarily refer to the same embodiment, but it can be the same embodiment.

[0107] In order to make the present disclosure fully understood, the following description provides detailed steps and structures. Obviously, the implementation of the present disclosure will not be limited to the specific details known to those skilled in the art. In addition, the known structures and steps are no longer described in detail to avoid unnecessarily limiting the present disclosure. The preferred embodiments of the present disclosure are described in detail below. However, in addition to the detailed description, the present disclosure can also be widely implemented in other embodiments. The scope of the present disclosure is not limited to the content of the detailed description, but is defined by the claims.

[0108] Embodiments of the present disclosure discuss a semiconductor structure composed of a plurality of memory cells and a method for preparing the semiconductor structure. According to some embodiments of the present disclosure, each memory cell is composed of a transistor, the transistor including a word line, a bit line, a source line and a channel layer, and a data storage unit electrically coupled to the transistor. The transistor can be used to control access operations of the data storage unit, such as read and write operations. According to some embodiments of the present disclosure, the channel layer is electrically coupled to the bit line through a landing pad. According to some comparative embodiments, the process of forming a landing pad array on a channel layer array is usually by forming a dielectric layer on the channel layer array, then etching the dielectric layer to form a plurality of through holes, and a conductive material is deposited in the through holes to form a landing pad array. In order to improve the performance of the memory cell, in some embodiments of the present disclosure, the arrangement order of the landing pad array and the dielectric layer is exchanged. However, in some cases, during the subsequent planarization operation, the uniformity of the height of the landing pad may not be maintained according to the predetermined specification, and the electrical properties of the landing pad may not be guaranteed. Therefore, the device reliability of the storage unit will be compromised.

[0109] To solve the above problems, an etch stop layer is introduced to protect the landing pad during the planarization process. The planarization process is compatible with conventional processing recipes and the height uniformity of the landing pad can be maintained. Therefore, the reliability of forming the landing pad is improved and defects when preparing a new memory cell structure will be minimized.

[0110] Figure 1A , Figure 1B , Figure 1C , Figure 1D , Figure 1E , Figure 1F , Figure 1G , Figure 1H , Fig. 1I , Figure 1J , Figure 1K , Figure 1L , Figure 1M , Figure 1N , Fig.1O , Figure 1P , Figure 1Q , Figure 1R , Figure 1S , Figure 1T , Figure 1U , Figure 1V , Figure 1W , Figure 1X , Figure 1Y , Figure 1Z , Figure 1AA and Fig. 1AB is a cross-sectional view illustrating an intermediate stage of a method for preparing a semiconductor structure 100 according to some embodiments of the present disclosure. Figures 1A to 1AB Before, during and after the steps shown, other steps may also be provided, and in other embodiments of the preparation method, some of the following steps may be replaced or eliminated. These steps may be performed independently, and the order of the steps may be interchangeable.

[0111] Reference Figure 1A According to some embodiments of the present disclosure, the semiconductor structure 100 is formed by a memory array, wherein the memory array includes a dynamic random-access memory (DRAM) cell. A DRAM cell (e.g., represented by a memory cell of the semiconductor structure 100) is typically formed by a data storage unit 124 (memory cell) configured to store data information and a control unit configured to perform access operations on the data storage unit, such as read operations and write operations. The control unit is typically implemented by a transistor, such as a field-effect transistor (FET), such as a metal-oxide semiconductor (MOS) FET (MOSFET). Depending on the different architectures of the transistor, the control unit of the DRAM can be composed of a planar FET. However, other types of FETs, such as fin FETs (FinFETs), gate-all-around (GAA) FETs, nanosheet FETs, nanowire FETs, or similar elements, are also within the scope of the present disclosure.

[0112] Reference Figure 1A, a substrate 110 is formed, received or provided. According to some embodiments of the present disclosure, the substrate 110 includes a semiconductor material, such as bulk silicon. According to some embodiments of the present disclosure, the substrate 110 includes other semiconductor materials, such as silicon germanium, silicon carbide, gallium arsenide, etc. According to some embodiments of the present disclosure, the substrate 110 is a p-type semiconductor substrate (acceptor type) or an n-type semiconductor substrate (donor type). Alternatively, the substrate 110 may include another semiconductor element, such as germanium; a compound semiconductor including gallium arsenide, gallium phosphide, indium phosphide, indium arsenide or indium antimonide; an alloy semiconductor including SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP or GaInAsP; or a combination thereof. According to another embodiment of the present disclosure, the substrate 110 includes a portion forming a semiconductor-on-insulator (SOI) substrate. In other alternatives, the substrate 110 may include a doped epitaxial layer, a gradient semiconductor layer, and / or a semiconductor layer overlying another semiconductor layer of a different type, such as a silicon layer over a silicon germanium layer. According to some embodiments of the present disclosure, the substrate 110 is a hybrid substrate including a first portion formed of a bulk silicon substrate and a second portion formed of an SOI substrate.

[0113] According to some embodiments of the present disclosure, the semiconductor structure 100 includes a first region 100A and a second region 100B adjacent to the first region 100A. The first region 100A may be regarded as a memory array region in the present disclosure; and the second region 100B may be regarded as a peripheral region in the present disclosure. According to some embodiments of the present disclosure, the second region 100B is located at the periphery of the substrate 110 or laterally surrounds the first region 100A.

[0114] According to some embodiments of the present disclosure, an array of active regions 104 is formed in a substrate 110. The active regions 104 may be formed by doped regions to which N-type or P-type dopants are applied. According to some embodiments of the present disclosure, the N-type dopant includes phosphorus (P), arsenic (As), antimony (Sb), or other suitable materials. According to some embodiments of the present disclosure, the P-type dopant includes boron (B) or indium (In), or other suitable materials. The top view of the active regions 104 is shown in FIG. Figure 2 Reference Figure 2, the active region 104 may be separated by an isolation region 206, wherein the isolation region 206 is formed of a dielectric material, such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, a high-k dielectric material, or other suitable dielectric material. According to some embodiments of the present disclosure, the active region 104 is oval-shaped or ellipse-shaped in a top-down view. The active region 104 may be formed to include a source / drain region for each control unit. According to some embodiments of the present disclosure, the isolation region 206 defines and electrically separates the active region 104.

[0115] Reference Figure 1A , one or more semiconductor elements 106 are formed in the substrate 110 of the second region 100B. The semiconductor elements 106 can be used to perform auxiliary control functions of the storage cells of the semiconductor structure 100, for example, they can perform data multiplexing, data demultiplexing, data encoding, data decoding, signal filtering, etc. The semiconductor element 106 may include one or more active elements, such as transistors or other similar elements, or one or more passive elements, such as resistors, capacitors, inductors, diodes, fuses or other similar elements. Transistors generally use field effect transistors (FETs), such as metal oxide semiconductor field effect transistors (MOSFETs). According to different architectures, the transistors 106 in the second region 100B can be formed as planar field effect transistors. However, other types of field effect transistors, such as fin field effect transistors (FinFETs), gate-all-around (GAA) field effect transistors, nanosheet field effect transistors, nanowire field effect transistors, etc., are also within the scope of consideration of the present disclosure.

[0116] A first layer 120 is formed on the substrate 110. According to some embodiments of the present disclosure, a dielectric layer 112 is formed in the first layer 120. The dielectric layer 112 may include an insulating material, such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, a high dielectric constant insulating material, or other suitable insulating materials. The first layer 120 may be a single layer structure or a multilayer structure formed by different sublayers of the dielectric layer 112. The dielectric layer 112 may be formed by deposition, such as chemical vapor deposition (CVD), physical vapor deposition (PVD), atomic layer deposition (ALD), spin coating, or other suitable deposition methods.

[0117] According to some embodiments of the present disclosure, a conductive via 114 is formed in the first layer 120 of the second region 100B and passes through the dielectric layer 112. The conductive via 114 can be electrically coupled to the semiconductor element 106 located thereunder. The conductive via 114 is formed of a conductive material, such as copper, aluminum, tungsten, silver, gold, titanium, titanium nitride, tantalum, tantalum nitride, alloys thereof, and the like. As an example of a formation process of the conductive via 114, a patterning operation is performed to form a trench (not shown separately) that extends through the first layer 120 located above the semiconductor element 106. The patterning operation may include lithography and etching operations. The etching operation may include dry etching, wet etching, a combination thereof (e.g., reactive ion etching, reactive ion etch, RIE), or the like. Then, a conductive material may be deposited on the upper surface of the trench and the dielectric layer 112 using CVD, PVD, ALD, or the like. According to some embodiments, a planarization operation, such as chemical mechanical polishing (CMP) or mechanical grinding, is performed to remove excess conductive material to form the conductive via 114 and to make the upper surface of the conductive via 114 flush with the upper surface of the dielectric layer 112 .

[0118] According to some embodiments of the present disclosure, one or more dielectric layers 132, 134 are formed in the first layer 120 of the first region 100A. Each dielectric layer 132, 134 may include a dielectric material, such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, a high dielectric constant dielectric material, or other suitable dielectric materials. The formation method of the dielectric layers 132, 134 may be similar to that of the dielectric layer 112. According to some embodiments, the first layer 120 is not a single-layer structure formed by the dielectric layer 112, but includes a multi-layer structure formed by the dielectric layers 132, 134, and spans the first region 100A and the second region 100B.

[0119] An array of data storage cells 124 is formed in the first layer 120, for example, in the dielectric layers 132, 134 of the first region 100A. The array of data storage cells 124 can be electrically coupled to the active region 104 located thereunder. Each data storage cell 124 is composed of a capacitor, which can be a deep-trench type capacitor or a metal-insulator-metal (MIM) capacitor. According to some embodiments of the present disclosure, each data storage cell 124 is composed of two electrode plates and an insulating film located between the two electrode plates, wherein only the dielectric layer 132, 134 is electrically coupled to the active region 104 located thereunder. Figure 1A1 and 2 , one electrode plate (also labeled 124) for each data storage unit 124 is depicted. The electrode plates of the data storage unit 124 are made of a conductive material, such as copper, aluminum, tungsten, silver, gold, titanium, titanium nitride, tantalum, tantalum nitride, alloys thereof, etc., formed using CVD, PVD, ALD or other suitable deposition methods. The insulating film between the electrode plates can be made of a dielectric material, such as silicon oxide, silicon nitride, a high dielectric constant material or the like.

[0120] According to some embodiments of the present disclosure, the semiconductor structure 100 further includes a conductive layer 126 disposed on the upper side of each data storage unit 124. The conductive layer 126 may include a conductive oxide layer formed of a conductive oxide material, for example, indium tin oxide (ITO), indium tungsten oxide (IWO) or other conductive oxide layers. According to some embodiments, the conductive layer 126 includes a transparent conductive oxide. The conductive layer 126 can be used to electrically couple the electrode plate of the data storage unit 124 with the structure located thereon. The conductive layer 126 can be formed by CVD, PVD, ALD or other suitable deposition methods.

[0121] According to some embodiments of the present disclosure, each data storage unit 124 includes a liner 128 formed on the sidewall of the electrode plate. The liner 128 may include a dielectric material, such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, a high dielectric constant dielectric material, or other suitable dielectric material. According to some embodiments of the present disclosure, the liner 128 is conformally deposited along the sidewall of the electrode plate with a substantially uniform thickness. According to some embodiments of the present disclosure, the upper surfaces of the dielectric layer 112, the conductive via 114, the dielectric layer 134, the liner 128, and the conductive layer 126 are coplanar with each other.

[0122] According to some embodiments of the present disclosure, the electrode plate marked with number 124 includes two sections from a cross-section view. The upper section of the electrode plate 124 is connected to the lower section, wherein the width of the upper section may be greater than the width of the lower section.

[0123] Reference Figure 1B , forming a second layer 140 above the first layer 120. The second layer 140 includes a dielectric layer 142 formed through the first region 100A and the second region 100B. The dielectric layer 142 may include a dielectric material, such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, a high dielectric constant dielectric material, or other suitable dielectric materials. The dielectric layer 142 may be a single-layer structure or a multi-layer structure, formed by sub-layers of different dielectric materials, for example, by CVD, PVD, ALD or other suitable deposition methods.

[0124] A word line 148 is formed in the second layer 140 located in the first region 100A. The word line 148 may be surrounded and electrically insulated by the dielectric layer 142. The word line 148 may include a conductive material, such as tungsten; however, other suitable conductive materials, such as copper, aluminum, silver, gold, titanium, titanium nitride, tantalum, tantalum nitride, and alloys thereof, are also within the contemplation of the present disclosure.

[0125] A conductive pad 144 and a conductive line 146 are formed in the second layer 140 located in the second region 100B. The conductive pad 144 can electrically couple the conductive via 114 with the conductive line 146. According to some embodiments of the present disclosure, the conductive line 146 and the word line 148 are formed at the same height of the second layer 140 during a single deposition operation. The conductive pad 144 and the conductive line 146 may include a conductive material, such as tungsten; however, other suitable conductive materials, such as copper, aluminum, silver, gold, titanium, titanium nitride, tantalum, tantalum nitride and alloys thereof, are also within the contemplation of the present disclosure.

[0126] As an example of a formation process, a first dielectric sublayer (not shown separately) of dielectric layer 142 is deposited on the surface of first layer 120. A patterning operation is performed to form a plurality of recesses on the upper surface of the first dielectric sublayer. The conductive material of conductive pad 144 is deposited in the recesses of the first dielectric sublayer. According to some embodiments of the present disclosure, a planarization operation may be used to remove excess portions of the conductive material on the upper surface of the first dielectric sublayer to form conductive pad 144. Subsequently, a second dielectric sublayer (not shown separately) is deposited on the first dielectric sublayer and conductive pad 144 using an appropriate deposition method. A patterning operation is performed to form a plurality of recesses on the upper surface of the second dielectric sublayer. Conductive material for word line 148 and conductive line 146 is deposited in the recesses of the second dielectric sublayer. According to some embodiments of the present disclosure, a planarization operation may be used to remove excess portions of the conductive material on the upper surface of the second dielectric sublayer to form word line 148 and conductive line 146. Then, a third dielectric sublayer (not shown separately) is deposited over the second dielectric sublayer, the word line 148 and the conductive line 146 by a suitable deposition method.

[0127] Reference Figure 1C , the second layer 140 is patterned to form a plurality of trenches 142T in the first region 100A, wherein the trenches 142T pass through the word lines 148 and are aligned with the corresponding data storage cells 124. The upper surface of the corresponding conductive layer 126 is exposed accordingly. The trenches 142T may have a diameter or width that is smaller than the width of the word lines 148, whereby the portion of the trenches 142T that is at the same level as the word lines 148 is located within the circumference of the word lines 148. According to some embodiments of the present disclosure, the trenches 142T are formed by lithography and etching operations. The etching operation may be performed by dry etching, wet etching, RIE, or the like.

[0128] Reference Figure 1D , an insulating film 153 is deposited on the sidewalls and bottom of the trench 142T. The insulating film 153 may be further deposited on the surface of the dielectric layer 142. The insulating film 153 may include a dielectric material, such as silicon dioxide; however, other dielectric materials, such as silicon nitride, silicon carbide, silicon nitride oxide, high dielectric constant dielectric materials or other suitable dielectric materials, are also within the scope of the present disclosure. The insulating film 153 can be deposited with an almost uniform thickness using CVD, ALD or other suitable deposition methods, i.e., conformally deposited.

[0129] Figure 1E The etching operation of the insulating film 153 is shown. Accordingly, a plurality of insulating films 154 are formed on the sidewalls of the single trench 142T. The etching operation may use an anisotropic etching operation to etch the horizontal portion of the insulating film 153 at the bottom of the trench 142T and the upper surface of the dielectric layer 142. The etching operation may include dry etching, wet etching, RIE, etc.

[0130] Reference Figure 1F , a conductive oxide layer 151 is deposited in the trench 142T between the insulating films 154. The conductive oxide layer 151 may also be deposited on the surface of the dielectric layer 142. According to some embodiments, the conductive oxide layer 151 includes a transparent conductive oxide. According to some embodiments of the present disclosure, the conductive oxide layer 151 includes indium gallium zinc oxide (IGZO) or other suitable conductive oxide materials.

[0131] Reference Figure 1G , a planarization operation is performed to remove excess material of the conductive oxide layer 151 to form an independent channel layer 152. The planarization operation may also cause the upper surface of the channel layer 152 to be horizontally aligned with the surface of the dielectric layer 142. The planarization operation may be performed using CMP, mechanical grinding, or other suitable grinding operations. According to some embodiments of the present disclosure, the channel layer 152 acts as a channel for each control unit to allow access current to flow. The word line 148 is electrically isolated from the channel layer 152 by an intervening insulating film 154, and is configured to control the movement of carriers in the channel layer 152 with an appropriate voltage bias during read and write operations. According to some embodiments of the present disclosure, each channel layer 152 passes through the word line 148 and is therefore surrounded by the word line 148 on the side.

[0132] Reference Figure 1H , the conductive material 161 is deposited on the upper surface of the second layer 140. According to some embodiments of the prior art, the conductive material 161 extends over the first region 100A and the second region 100B. The conductive material 161 may cover each channel layer 152. The conductive material 161 (or the patterned conductive layer 162 formed therefrom, see Figure 1M ) can be used to electrically couple the channel layer 152 with the upper structure through a patterning operation, the details of which will be discussed later. According to some embodiments of the present disclosure, the conductive material 161 includes a conductive oxide material (for example, indium tin oxide (ITO), indium tungsten oxide (IWO) or other conductive oxide materials). According to some embodiments, the conductive material 161 includes a transparent conductive oxide. The conductive material 161 may include a material similar to the conductive layer 126. The conductive material 161 can be formed by CVD, PVD, ALD or other appropriate deposition methods. According to some embodiments of the present disclosure, the channel layer 152, the conductive layer 126 and the conductive material 161 (or the patterned conductive layer 162) are all formed of a conductive oxide material. According to some embodiments of the present disclosure, the channel layer 152 includes a conductive oxide material different from the conductive layer 126 or the conductive material 161 (or the patterned conductive layer 162).

[0133] See also Fig. 1I , another conductive material 163 is deposited on the upper surface of the conductive material 161. According to some embodiments of the present disclosure, the conductive material 163 extends to the first region 100A and the second region 100B. According to some embodiments of the present disclosure, the conductive material 163 includes a metal material, such as tungsten; however, other suitable conductive materials, such as copper, aluminum, silver, gold, titanium, titanium nitride, tantalum, tantalum nitride and alloys thereof, are also within the scope of consideration of the present disclosure. The conductive material 163 can be formed by CVD, PVD, ALD or other suitable deposition methods. According to some embodiments of the present disclosure, the conductive material 163 includes a metal material similar to the word line 148.

[0134] Reference Figure 1J , depositing an etch stop layer 165 on the upper surface of the conductive material 163. According to some embodiments of the present disclosure, the etch stop layer 165 spans the first region 100A and the second region 100B. According to some embodiments of the present disclosure, the etch stop layer 165 includes silicon nitride, silicon carbide, carbon, silicon nitride oxide, a high dielectric constant dielectric material or other suitable dielectric materials. The etch stop layer 165 can serve as a hard mask, which will be patterned during the patterning operation so that the conductive material 161 and the conductive material 163 form an array of patterned conductive pads. The etch stop layer 165 can be prepared by chemical vapor deposition (CVD), physical vapor deposition (PVD), atomic layer deposition (ALD) or other suitable deposition methods.

[0135] Reference Figure 1K, a hard mask layer 167 is deposited on the etch stop layer 165. According to some embodiments of the present disclosure, the hard mask layer 167 extends across the first region 100A and the second region 100B. According to some embodiments of the present disclosure, the hard mask layer 167 includes a material different from that of the etch stop layer 165, for example, the hard mask layer is formed of carbon or other suitable materials such as silicon oxynitride and high dielectric constant dielectric materials. The hard mask layer 167 can serve as a mask layer, be patterned during a patterning operation to form a pattern, and transfer the pattern to the etch stop layer 165. The hard mask layer 167 can be formed by CVD, PVD, ALD or other suitable deposition methods.

[0136] refer to Figure 1L , a photoresist 169 (or a mask layer 169) is deposited on the upper surface of the hard mask layer 167. According to some embodiments of the present disclosure, the photoresist 169 extends across the first region 100A and the second region 100B. According to some embodiments of the present disclosure, the photoresist 169 can be etched into a specific pattern during a lithography operation to facilitate the etching operation of the underlying layer. According to some embodiments of the present disclosure, the photoresist 169 is formed using a multilayer structure and includes a bottom layer used as an anti-reflective coating. The bottom layer may contain a polymer-based material. According to some embodiments of the present disclosure, the photoresist 169 further includes a dielectric antireflection coating (DARC) deposited on the bottom layer. According to some embodiments described in the present disclosure, the DARC includes a dielectric material such as silicon oxide, silicon nitride, silicon oxynitride or other suitable dielectric materials. According to some embodiments of the present disclosure, the bottom layer and the DARC may be formed by CVD, PVD, ALD, spin coating or other appropriate deposition methods.

[0137] Reference Figure 1M, one or more patterning operations are performed to continuously pattern the stack of hard mask layer 167, etch stop layer 165, conductive material 163, and conductive material 161. As an example of a formation process, photoresist 169 is etched into patterned photoresist 170 or patterned mask layer 170, wherein patterned photoresist 170 includes a pattern corresponding to pattern 170P of the conductive pad. Hard mask layer 167 is converted into patterned hard mask layer 168 through a first etching operation using patterned photoresist 170 as an etching mask. Therefore, pattern 170P is transferred from patterned photoresist 170 to patterned hard mask layer 168. Subsequently, etch stop layer 165 is converted into patterned etch stop layer 166 through a second etching operation using patterned hard mask layer 168 as an etching mask. Therefore, pattern 170P is transferred to patterned etch stop layer 166. The third etching operation uses the patterned etch stop layer 166 to pattern the conductive material 163 and the conductive material 161 to form an array of conductive pads 164 and conductive layer 162. Therefore, the pattern 170P is transferred to the conductive pads 164 and the conductive layer 162. According to some embodiments, the conductive pads 164 serve as landing pads to be electrically coupled to the bit lines 188 (described later) of the semiconductor structure 100.

[0138] According to some embodiments of the present disclosure, each of the first etching operation, the second etching operation, and the third etching operation can be implemented by dry etching, wet etching, RIE, etc. The first etching operation, the second etching operation, and the third etching operation can be performed in one operation or separately. Similarly, the etching of the conductive material 161 and the conductive material 163 can be performed by subsequent etching operations or a single etching operation. According to some embodiments of the present disclosure, through one or more etching operations, a portion of the upper surface of the dielectric layer 142 located between the conductive layers 162 is exposed. According to some embodiments of the present disclosure, the etchant used to etch the conductive material 163 or 161 is selective for the conductive material 163 or 161 compared to the material of the etching stop layer 165 or the dielectric layer 142, so that the etching stops at the dielectric layer 142.

[0139] Reference Figure 1N , when the patterning of the conductive materials 161 and 163 is completed, the patterned photoresist 170 will be removed or stripped. According to some embodiments of the present disclosure, the patterned hard mask layer 168 is also removed or stripped. Removing the patterned photoresist 170 and the patterned hard mask layer 168 may include dry etching, wet etching, RIE, ashing operations, etc. Therefore, the upper surface of the patterned etch stop layer 166 is exposed.

[0140] Reference Fig.1O, a photoresist 172 is provided to cover the first region 100A. The second region 100B is exposed accordingly. The photoresist 172 can be deposited on the first region 100A by a suitable deposition method such as CVD, PVD, spin coating, etc. According to some embodiments of the present disclosure, the photoresist 172 includes a single-layer structure or a multi-layer structure.

[0141] See also Figure 1P , the portions of the patterned etch stop layer 166, the conductive material 163, and the conductive material 161 remaining in the second region 100B will be removed. The removal operation can be performed by performing an etching operation using the photoresist 172 as an etching mask. The etching operation may include dry etching, wet etching, RIE, or a similar method. Therefore, the upper surface of the dielectric layer 142 of the second region 100B is exposed. According to some embodiments of the present disclosure, after the etching operation is completed, the photoresist 172 is removed. In the first region 100A, the patterned etch stop layer 166 and the dielectric layer 142 are exposed again.

[0142] Figure 1Q The process of forming a dielectric layer 174 on the dielectric layer 142 and the conductive pad 164 is shown. The dielectric layer 174 may span the first region 100A and the second region 100B. According to some embodiments of the present disclosure, the dielectric layer 174 covers the patterned etch stop layer 166 and fills the space 166P between adjacent conductive layers 162, between adjacent conductive pads 164, and between adjacent portions of the patterned etch stop layer 166. The deposited dielectric layer 174 covers the entire surface of the patterned etch stop layer 166 in the first region 100A and the upper surface of the dielectric layer 142 in the second region 100B. The dielectric layer 174 is also in contact with the upper surface of the dielectric layer 174 in the first region 100A. The dielectric layer 174 may include a dielectric material, such as silicon dioxide, which is different from the patterned etch stop layer 166. Dielectric layer 174 may be formed by ALD to improve filling performance in space 166P; however, other deposition methods such as PVD or CVD may also be used.

[0143] Reference Figure 1R , another dielectric layer 176 is deposited over the dielectric layer 174. The dielectric layer 176 may span the first region 100A and the second region 100B. According to some embodiments of the present disclosure, the dielectric layer 176 covers the dielectric layer 174. The dielectric layer 176 may include a different dielectric material than the patterned etch stop layer 166, such as silicon dioxide. The dielectric layer 176 may include a similar material to the dielectric layer 174, such as silicon dioxide. The dielectric layer 176 may be formed by CVD, PVD, ALD, spin coating, or other suitable deposition methods.

[0144] Reference Figure 1S, a planarization operation is performed using a tool 180. According to some embodiments of the present disclosure, the planarization operation includes chemical mechanical polishing. Therefore, a portion of the dielectric layer 176 and a portion of the dielectric layer 174 are thinned or removed. According to some embodiments of the present disclosure, the tool 180 includes a polishing pad configured to remove the thickness of the dielectric layer 174 or the dielectric layer 176. Since the material of the patterned etch stop layer 166 is different from the material of the dielectric layers 174 and 176, for example, the patterned etch stop layer 166 is harder than the dielectric layers 174 and 176, the planarization operation may stop at the patterned etch stop layer 166 during the thinning of the dielectric layers 174 and 176. Therefore, during the planarization operation, each upper surface of the patterned etch stop layer 166 is exposed. The upper surface of the patterned etch stop layer 166 may be almost flush with the upper surface 174S of the dielectric layer 174 and the upper surface 176S of the dielectric layer 176, and the surface roughness is caused by the polishing pad. According to some embodiments of the present disclosure, the thickness of the patterned etch stop layer 166 may be slightly consumed during the planarization operation, but the patterned etch stop layer 166 will not be completely removed during the planarization operation, so the conductive pad 164 located thereunder can be well protected, that is, the upper surface of the conductive pad 164 is covered during the planarization operation.

[0145] Reference Figure 1T , the patterned etch stop layer 166 is removed from the upper surface of the conductive pad 164. Removing the patterned etch stop layer 166 may include dry etching, wet etching, RIE and the like. The upper surface of the conductive pad 164 is accordingly exposed. The etchant of the etching operation is selective to the dielectric layers 174, 176 and the conductive pad 164 relative to the patterned etch stop layer 166, so that during the etching of the patterned etch stop layer 166, the dielectric layers 174, 176 and the conductive pad 164 can remain substantially intact. Therefore, a plurality of trenches 174T are formed in the dielectric layer 174 on the conductive pad 164.

[0146] See also Figure 1U , a through hole 176T is formed in the second region 100B and is located above the conductive line 146. The through hole 176T passes through the dielectric layer 176, the dielectric layer 174 and the dielectric layer 142, and exposes the conductive line 146 thereunder. The through hole 176T may be formed by photolithography and etching operations. The etching operation may include dry etching, wet etching, RIE, etc. The etching operation may include anisotropic etching.

[0147] Reference Figure 1V, conductive material 178 is deposited on dielectric layer 174 and dielectric layer 176, and fills deposition trench 174T and through hole 176T. According to some embodiments of the present disclosure, conductive material 178 extends to the surface of dielectric layers 174 and 176. Conductive material 178 can be the same material as conductive pad 164, such as tungsten; or other conductive materials, such as copper, aluminum, silver, gold, titanium, titanium nitride, tantalum, tantalum nitride, or alloys thereof. The deposition of conductive material 178 can be achieved by chemical vapor deposition to facilitate the filling performance of conductive material 178 in trench 174T and through hole 176T.

[0148] Reference Figure 1W , the excess portion of the conductive material 178 is removed by a planarization operation, such as CMP or mechanical grinding. During the planarization operation, the upper surfaces of the dielectric layers 174 and 176 are exposed again. The height of the original conductive pad 164 is increased to form a conductive pad 182, wherein the conductive pad 182 includes an upper surface that is flush with the upper surface of the dielectric layer 174 or the dielectric layer 176. In addition, according to some embodiments of the present disclosure, the planarization operation forms a conductive via 184 in the second region 100B, and the upper surface of the conductive via 184 is flush with the upper surface of the dielectric layer 174 or the dielectric layer 176. The conductive via 184 can be electrically coupled to the bottom conductive line 146.

[0149] Reference Figure 1X , a conductive layer 185 is formed on the dielectric layers 174, 176, the conductive pad 182 and the conductive via 184. The conductive layer 185 can be the same material as the conductive pad 164 or the conductive material 178, such as tungsten or other conductive materials, such as copper, aluminum, silver, gold, titanium, titanium nitride, tantalum, tantalum nitride or alloys thereof. The deposition of the conductive material can be performed by PVD to improve the electrical or mechanical properties of the conductive layer 185. According to some embodiments of the present disclosure, a planarization operation, such as CMP, is performed to make the surface of the conductive layer 185 flat.

[0150] Reference Figure 1Y , a dielectric layer 186 is deposited on the conductive layer 185. The dielectric layer 186 may include a dielectric material, such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, a high dielectric constant dielectric material, or other suitable dielectric material. The dielectric layer 186 may be a single layer structure or a multilayer structure formed by sublayers of various dielectric materials. The dielectric layer 186 may be formed by deposition, such as CVD, PVD, ALD, spin coating, or other suitable deposition methods.

[0151] Reference Figure 1Z, a patterning operation is performed on the dielectric layer 186 to form a trench 186T passing through the dielectric layer 186. The trench 186T further extends to the dielectric layer 174, the conductive layer 185 and the conductive pad 182. Therefore, a conductive pad 187 is formed on the conductive via 184. According to some embodiments of the present disclosure, the width or surface area of ​​the conductive pad 187 is larger than the conductive via 184. According to some embodiments of the present disclosure, the patterning operation removes a portion of the conductive pad 182 to form a plurality of bit lines 188 located above the conductive pad 182. During the patterning operation, a portion 182T of the conductive pad 182 and a portion 174R of the dielectric layer 174 are etched to form the bit line 188 and the conductive pad 182. According to some embodiments of the present disclosure, the remaining portion of the dielectric layer 174 laterally surrounds the conductive pad 182.

[0152] Although not shown, it is understood that the conductive pad 182 is formed on the channel layer 152 of the corresponding data storage unit 124, and each bit line 188 is formed as a conductive line, extending in the direction from the 1Z figure to the outside of the paper, and electrically coupled to each channel layer 152. In addition, from the perspective of the cross-sectional view, each portion of the dielectric layer 174 located between adjacent conductive pads 182 may be lower than the surface of the dielectric layer 176. An interface between the dielectric layer 174 and the conductive pad 182 may be exposed. The groove 186T can be formed by lithography and etching operations. The etching operation may include dry etching, wet etching, RIE or the like. The etching operation may include anisotropic etching.

[0153] Reference Figure 1AA , dielectric layer 190 is deposited on dielectric layers 174, 176, 186, bit line 188 and conductive pad 182. Dielectric layer 190 may fill trench 186T. Dielectric layer 190 may include a dielectric material, such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, a high dielectric constant dielectric material, or other suitable dielectric material. Dielectric layer 190 may be a single layer structure or a multilayer structure formed by sublayers of various dielectric materials. Dielectric layer 190 may be formed by CVD, PVD, ALD, spin coating, or other suitable deposition methods.

[0154] Reference Fig. 1AB, a trench (not shown separately) is formed through the dielectric layer 190 and the dielectric layer 186 located on the conductive pad 187 to expose the conductive pad 187. A conductive material is deposited in the trench to form a conductive via 192, which is electrically coupled to the conductive pad 187. The material of the conductive via 192 may be the same as that of the conductive pad 164, the bit line 188 or the conductive pad 187, such as tungsten; or other conductive materials, such as copper, aluminum, silver, gold, titanium, titanium nitride, tantalum, tantalum nitride or alloys thereof. A chemical vapor deposition method can be used to deposit a conductive material on the conductive via 192 to improve its gap filling capability. According to some embodiments of the present disclosure, a planarization operation (e.g., CMP) is performed to remove excess material of the conductive via 192 and make its surface planar.

[0155] Figure 2 FIG. 1 is a top view illustrating a semiconductor structure 100 according to some embodiments of the present disclosure. Figures 1A to 1AA The cross-section shown is from Figure 2 To better illustrate the components to be shown, some features of the semiconductor structure 100 are shown in FIG. Figure 2 Omitted in . Figure 2 , the active region 104, word line 148 and bit line 188 in the substrate 110 are shown. According to some embodiments of the present disclosure, in a top view, the word line 148 crosses the bit line 188, and the data storage unit 124 (not shown) Figure 2 148) is arranged just above the active region 104 where the word line 148 crosses the bit line 188. According to some embodiments of the present disclosure, the control unit of each memory cell is composed of the bit line 188, the word line 148 and the source line (not shown separately), wherein the bit line 188 and the source line are coupled to the two electrode plates 114, respectively.

[0156] Figures 3A to 3G 3 is a cross-sectional view illustrating an intermediate stage of a method for preparing a semiconductor structure 300 or a semiconductor structure 301 in some comparative embodiments of the present disclosure. Figures 3A to 3G Other steps may be provided before, during, and after the steps shown, and steps 3A to 3B may be provided. Figure 3G In other embodiments of the preparation method shown, some of the following steps can be replaced or eliminated. These steps can be performed independently, and the order of the steps can be interchanged. Figures 3A to 3G The method shown in the figure is similar to the method for preparing the semiconductor structure 100. Figures 1A to 1I , Figure 1O to Figure 1S as well as Figure 1X to Figure 1AB The preparation steps described are the same and these shared steps will not be repeated here.

[0157] FIG. 3A to FIG. 3E It shows that according to some comparative embodiments of the present disclosure, the conventional semiconductor structure 300 is insufficiently polished under CMP. Figure 3A is a cross-sectional diagram, shown in Figures 3A to 3G An intermediate stage of a method for preparing a semiconductor structure 300 is shown. Figure 3A The steps shown are followed by Figure 1H The stage shown and immediately proceed with Fig. 1I The steps corresponding to the stages shown. Figure 3A , the conductive material 163 is deposited on the conductive material 161. Figure 3B , the conductive material 163 and the conductive material 161 are patterned to form a conductive pad 164 and a conductive layer 162 respectively. The patterning operation can be performed using a lithography process and an etching operation, wherein the etching operation includes dry etching, wet etching, RIE and other methods. Figure 1L The photoresist 169 described in the above may be used for a patterning operation, wherein the photoresist 169 is first patterned into a patterned photoresist 170 with a pattern 170P, and then an etching operation is performed on the conductive materials 163 and 161 to form an array of conductive pads 164 and conductive layers 162. According to some comparative embodiments of the present disclosure, a hard mask layer similar to the hard mask layer 167 may be used. If the hard mask layer 167 formed of carbon is used, an adhesion layer (not shown separately) may be introduced between the conductive material 163 and the hard mask layer 167 due to insufficient adhesion between the carbon of the hard mask layer 167 and the conductive material 163 (e.g., tungsten). According to some comparative embodiments of the present disclosure, the carbon-based hard mask layer 167 is omitted during the patterning operation.

[0158] According to some comparative embodiments of the present disclosure, in order to simplify the manufacturing process, the etching stop layer 165 is omitted in the patterning operation. Figure 3B During the coating operation in the first region 100A, the upper surface of the conductive pad 164 is exposed. According to some comparative embodiments of the present disclosure, when the patterning operation is performed, a portion of the upper surface of the dielectric layer 142 located between adjacent conductive layers 162 or between adjacent conductive pads 164 in the first region 100A is also exposed.

[0159] According to some comparative embodiments of the present disclosure, using Fig.1O Then, the photoresist 172 is used as an etching mask to cover the first region 100A. Fig.1O According to the method described above, the conductive materials 163 and 161 remaining on the dielectric layer 142 located in the second region 100B will be removed. Figure 3B As shown, the entire upper surface of the dielectric layer 142 located in the second region 100B will also be exposed.

[0160] Reference Figure 3C, dielectric layers 174 and 176 are subsequently deposited over dielectric layer 142 and conductive pad 164. The materials and methods for forming dielectric layers 174 and 176 are similar to those of reference Figure 1Q and 1R The semiconductor structure 300 is different from the semiconductor structure 100 mainly in that the dielectric layer 174 is in direct contact with the conductive pad 164 without the etch stop layer 165 or any other etch stop structure.

[0161] Reference Figure 3D , similar to reference Figure 1S In the manner described, a planarization operation is performed on the semiconductor structure 300. Tool 180 is used to planarize dielectric layers 174 and 176, such as chemical mechanical polishing (CMP), to form corresponding dielectric layers 274 and 276. According to some comparative embodiments of the present disclosure, since there is no etch stop layer between dielectric layer 274 and conductive pad 164, the performance of CMP performed using tool 180 is highly dependent on the polishing time and the surface uniformity that can be achieved by tool 180. Since the height of each conductive pad 164 is not designed to be very large in order to reduce the size of the component and improve the electrical performance of the semiconductor structure, the non-ideal surface uniformity of tool 180 is more obvious for conductive pad 164.

[0162] Reference Figure 3D After the tool 180 performs a planarization operation (e.g., CMP), an under-polishing problem may occur, resulting in an uneven surface of the ground dielectric layer 274. The surface roughness of the ground surface of the dielectric layer 274 results in only some (e.g., Figure 3D In the planarization operation, the conductive pad 164 (the second conductive pad 164 from the left in FIG. 1 ) is exposed through the dielectric layer 274, while some other conductive pads 164 remain covered by at least a portion of the remnants of the dielectric layer 274. Under-polishing by the CMP operation may occur not only on the dielectric layer 274 on different semiconductor wafers, but also on different portions of the dielectric layer 274 on a single semiconductor wafer. Therefore, after the planarization operation is performed, the upper surfaces of at least some of the conductive pads 164 are not exposed.

[0163] Reference Figure 3E , dielectric layer 186 and bit line 188 are similar to reference Figures 1X to 1AB The above-described method is formed on the dielectric layer 174 and the conductive pad 164. Figure 3E As shown, due to the dielectric layer 274 remaining on the conductive pad 164, disconnection defects may be found between some bit lines 188 and corresponding conductive pads 164. Therefore, the problematic bit lines 188 may not be properly electrically connected to the corresponding channel layer 152, and the reliability of the semiconductor structure 300 may be impaired.

[0164] Figure 3A , Figure 3B , Figure 3C and Figure 3F to Figure 3G The semiconductor structure 301 is shown in some comparative embodiments of the present disclosure as being over-polished by CMP. The formation method of the semiconductor structure 301 is similar to the process of forming the semiconductor structure 300, please refer to Figure 3A , Figure 3B and Figure 3C Then, refer to Figure 3F After a planarization operation (e.g., CMP) is performed by tool 180 to form planarized dielectric layers 374 and 376, an over-grinding problem may occur on the ground dielectric layer 374 and the conductive pad 164 surface. The surface roughness of the dielectric layer 374 after grinding causes almost all the conductive pads 164 to be thinned to conductive pads 364 with a lower height. According to some comparative embodiments of the present disclosure, the conductive pad 364 has a rounded upper surface, so the effective contact area of ​​the conductive pad 364 may be reduced relative to the conductive pad 164. During this period, the portion of the dielectric layer 374 located between the conductive pads 364 is also over-etched. The thinned dielectric layer 374 between adjacent conductive pads 364 formed by over-grinding in the chemical mechanical polishing (CMP) operation may further increase the probability of short circuit defects between adjacent conductive pads 364. Over-grinding in the CMP operation may occur not only on the dielectric layer 374 and the conductive pad 364 of different semiconductor wafers, but also on the dielectric layer 374 and the conductive pad 364 of different parts of a single semiconductor wafer. According to some comparative embodiments of the present disclosure, although Figure 3F Although not shown, some of the conductive pads 364 may be thinned below the upper surface of the dielectric layer 374. As a result, after the planarization operation is performed, at least some of the conductive pads 364 may not maintain a sufficient height for subsequent electrical coupling.

[0165] Reference Figure 3G , dielectric layer 186 and bit line 188 are similar to Figure 1X to Figure 1AB The described manner is formed on the dielectric layer 174 and the conductive pad 364. Figure 3G As can be seen in FIG. 1 , at the interface between the bit line 188 and the conductive pad 364, a high resistance or disconnection defect may be found due to a reduction in the height or contact area of ​​the upper portion of the conductive pad 364. Therefore, the problematic bit line 188 or conductive pad 364 may not be properly electrically coupled to the channel layer 152, and the reliability of the semiconductor structure 301 may be impaired.

[0166] Figure 4A , Figure 4B and Figure 4C is a flow chart illustrating a method S400 for preparing a semiconductor structure in some embodiments of the present disclosure. FIG. 4A to FIG. 4C Additional steps may be provided before, during, and after the steps shown, and in additional embodiments of the preparation method S400, some of the steps described below may be replaced or eliminated. These steps may be performed independently, and the order of the steps may be interchanged. FIG. 4A to FIG. 4C The semiconductor structure depicted may be similar to semiconductor structure 100 .

[0167] Reference Figure 4A In step S402, a substrate including a first region and a second region is provided. According to some embodiments of the present disclosure, the first region is a storage array region. According to some embodiments of the present disclosure, the second region is a peripheral region. The second region may be arranged on the side, surrounding the first region.

[0168] In step S404 , an active region and a semiconductor element are formed in the first region and the second region, respectively. The active region may be similar to the active region 104 , and the semiconductor element may be similar to the semiconductor element 106 .

[0169] In step S406, an array of data storage units, such as data storage unit 124, is formed in a first layer above the substrate. According to some embodiments of the present disclosure, each data storage unit is formed by a capacitor for storing data information.

[0170] In step S408, a first conductive layer, such as a conductive oxide layer 126, is first deposited on the first layer to cover each data storage unit. The first conductive layer may include ITO, IWO or other suitable conductive oxide materials.

[0171] In step S410 , word lines, such as word line 148 , are deposited in a first dielectric layer (such as dielectric layer 142 ) on a first layer.

[0172] In step S412, a plurality of channel layers, such as channel layer 152, are formed through word lines. According to some embodiments of the present disclosure, an insulating film (such as insulating film 154) is formed on the sidewalls of each channel layer. The channel layer is electrically coupled to the conductive layer located thereunder.

[0173] In step S414, a second conductive layer, such as a conductive oxide layer 162, is deposited on each channel layer. The second conductive layer may include ITO, IWO or other suitable conductive oxide materials.

[0174] In step S416, a conductive material is deposited on the second conductive layer, such as conductive material 163. According to some embodiments of the present disclosure, the conductive material includes tungsten. According to some other embodiments of the present disclosure, the conductive material includes aluminum, silver, gold, titanium, titanium nitride, tantalum, tantalum nitride, alloys thereof, or similar materials.

[0175] Reference Figure 4B In step S418, an etch stop layer, such as etch stop layer 165, is deposited on the conductive material. The etch stop layer may include silicon nitride, silicon carbide, high-k dielectric material or other suitable materials.

[0176] In step S420, a hard mask layer is deposited on the etching stop layer. According to some embodiments of the present disclosure, the hard mask layer is substantially formed of carbon.

[0177] In step S422, a patterned mask layer, such as patterned mask layer 170, is deposited on the hard mask layer. The patterned mask layer may include an under layer and a DARC. According to some embodiments of the present disclosure, the patterned mask layer 170 includes a pattern consisting of a plurality of conductive pads or landing pads.

[0178] In step S424, the hard mask layer, the etch stop layer, and the conductive material are etched into a pattern of a conductive pad, for example, using the patterned mask layer as an etching mask to form the conductive pad 164. According to some embodiments of the present disclosure, the etching operations for forming the hard mask layer, the etch stop layer, and the conductive material are performed sequentially or completed during a single etching operation.

[0179] In step S426, the patterned mask layer and the hard mask layer are removed. Removing the patterned mask layer and the hard mask layer may include an etching operation, such as dry etching, wet etching, RIE, etc.

[0180] In step S428, a second dielectric layer (e.g., dielectric layer 174) and a third dielectric layer (e.g., dielectric layer 176) are deposited on the first region and the second region. According to some embodiments of the present disclosure, the second dielectric layer and the third dielectric layer are formed using different deposition methods, for example, the second dielectric layer is formed using ALD, and the third dielectric layer is formed using CVD. The third dielectric layer covers the entire second dielectric layer.

[0181] In step S430, the second dielectric layer and the third dielectric layer are thinned. The thinning operation may include a CMP operation. According to some embodiments of the present disclosure, during the thinning operation, the second dielectric layer is horizontally aligned with the third dielectric layer. According to some embodiments of the present disclosure, during the thinning operation, the upper surface of the etch stop layer is flush with the second dielectric layer.

[0182] In step S432, the etching stop layer is thinned to form a groove on the conductive pad. According to some embodiments of the present disclosure, during the thinning operation, the etching stop layer is removed from the upper surface of the conductive pad to expose the upper surface of the conductive pad. The thinning operation can be performed by dry etching, wet etching, RIE, etc.

[0183] Reference Figure 4C In step S434, a through hole, such as through hole 176T, is etched in the second region near the conductive pad. The through hole 176T may extend through the second dielectric layer and the third dielectric layer and etch the thickness of the first dielectric layer.

[0184] In step S436 , a conductive material is deposited in the trench and the via. According to some embodiments of the present disclosure, the conductive material fills the trench and the via and extends onto the second dielectric layer and the third dielectric layer.

[0185] In step S438, the conductive material is thinned to form conductive pads with increased height and conductive vias in the through-holes. According to some embodiments of the present disclosure, the thinning operation includes CMP or mechanical grinding.

[0186] In step S440, a third conductive layer, such as conductive layer 185, is formed on the second dielectric layer, the third dielectric layer and the conductive pad. According to some embodiments of the present disclosure, the third conductive layer covers the second dielectric layer, the third dielectric layer and the conductive pad.

[0187] In step S442, a fourth dielectric layer is formed on the third conductive layer, such as dielectric layer 186. According to some embodiments of the present disclosure, the fourth dielectric layer covers the third conductive layer.

[0188] In step S444, the fourth dielectric layer, the second dielectric layer and the conductive pad are etched to form a bit line, such as bit line 188, above the conductive pad. According to some embodiments of the present disclosure, the bit line and the data storage unit are electrically coupled through the conductive pad, the first conductive layer, the channel layer and the second conductive layer.

[0189] The memory cell planarization method proposed in this case has advantages. Since the performance of chemical mechanical polishing (CMP), such as surface roughness, is proportional to the CMP etching thickness, when the material layer to be planarized, such as the conductive pad 164, has a relatively low thickness or height, the final surface flatness may not meet the design requirements compared to the etching height of the material layer thinned by CMP. Surface roughness may cause over-polishing defects in some conductive pads, and may also cause under-polishing defects in some other conductive pads. Moreover, over-polishing and under-polishing may occur in a single semiconductor wafer.

[0190] By placing the proposed etch stop layer, such as etch stop layer 165, on the conductive pad, the tolerance of the surface roughness of the CMP operation can be greatly increased. If the CMP polishing can stop on the etch stop layer without consuming the bottom conductive pad or leaving more dielectric residue on the conductive pad, the CMP polishing can be easily performed. In addition, due to the presence of the etch stop layer, the performance of the endpoint detection scheme used during CMP can be more effectively performed. Therefore, the process window of the planarization operation is expanded, and the conductive pad can be deposited and planarized with high reliability and uniformity. The robustness and yield of the semiconductor memory structure can be further improved.

[0191] Although the present disclosure and its advantages have been described in detail, it should be understood that various changes, substitutions and replacements may be made without departing from the spirit and scope of the present disclosure as defined in the claims. For example, many of the above processes may be implemented in different ways, and other processes or combinations thereof may be used to replace many of the above processes.

[0192] Furthermore, the scope of the present application is not limited to the specific embodiments of the processes, machines, manufactures, compositions of matter, means, methods, and steps described in the specification. A person skilled in the art can understand from the disclosure of the present disclosure that existing or future developed processes, machines, manufactures, compositions of matter, means, methods, or steps that have the same functions or achieve substantially the same results as the corresponding embodiments described herein can be used according to the present disclosure. Accordingly, such processes, machines, manufactures, compositions of matter, means, methods, or steps are included in the claims of the present application.

Claims

1. A method for preparing a semiconductor structure, comprising: forming a word line in a first dielectric layer located above a substrate; forming a channel layer passing through the word line; forming a conductive material above the channel layer; forming an etch stop layer over the conductive material; patterning the etch stop layer to form a pattern of a conducting pad; Using the pattern of the etching stop layer as an etching mask to etch the conductive material to form a conductive pad; depositing a second dielectric layer over the etch stop layer and the first dielectric layer; planarizing the second dielectric layer, wherein at least a portion of the etch stop layer remains on the conductive pad after planarization; as well as forming a second trench in the second dielectric layer by etching a portion of the conductive pad and a portion of the second dielectric layer, The formation of the second trench may result in a bit line formed in the second trench being electrically coupled to the conductive pad.

2. The preparation method according to claim 1, further comprising: A third dielectric layer is deposited to fill the second trench.

3. The preparation method according to claim 1, further comprising: A capacitor is formed in a fourth dielectric layer, wherein the fourth dielectric layer is located below the first dielectric layer.

4. The preparation method according to claim 1, further comprising: Before forming the channel layer, an insulating film is deposited on a side wall of the word line. The manufacturing method as claimed in claim 1 , wherein the second dielectric layer laterally surrounds the conducting pad.

6. A method for preparing a semiconductor structure, comprising: forming a data storage unit in a first dielectric layer; depositing a word line above the data storage unit; forming a conductive material above the word line; forming a patterned hard mask layer over the conductive material; etching the conductive material through the patterned hard mask layer to form a conductive pad; depositing a second dielectric layer over the patterned hard mask layer; and removing the second dielectric layer, Wherein at least a portion of the patterned hard mask layer is left behind during the removal.

7. The preparation method according to claim 6, further comprising: A first conductive oxide layer is formed through the word line. 8 . The method as claimed in claim 7 , wherein the first conductive oxide layer comprises indium gallium zinc oxide.

9. The preparation method according to claim 7, further comprising: Prior to depositing the conductive material, a second conductive oxide layer is deposited on the first conductive oxide layer and the word line. 10 . The method as claimed in claim 9 , wherein the second conductive oxide layer comprises titanium indium oxide. 11 . The method of claim 6 , wherein the patterned hard mask is formed of a material different from that of the first dielectric layer.

12. The preparation method according to claim 6, further comprising: A third dielectric layer is deposited to cover the second dielectric layer. 13 . The method of claim 12 , wherein removing the entire etch stop layer leaves a first trench in the second dielectric layer, and further comprising depositing the conductive material over the second dielectric layer and in the first trench. 14 . The preparation method according to claim 12 , wherein the second dielectric layer is removed so that an upper surface of the second dielectric layer is flush with an upper surface of the third dielectric layer.