Molten iron spheroidizing device

By setting expansion gaps and anchoring steel structures in the molten iron spheroidizing device to form a heat-insulating space, and using central air ducts and open slots to improve the uniformity of the spheroidizing agent distribution, the existing device is easily cracked and burned out at high temperatures. It improves the absorption rate and spheroidization effect of magnesium and prolongs the service life of the spray gun.

CN118808567APending Publication Date: 2024-10-22HUANGSHI XINXING PIPES CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410763170.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-13
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

The existing molten iron spheroidizing device is prone to cracking and burning under high temperature conditions, has a short service life, is inconvenient to operate, and has low magnesium absorption rate, resulting in poor spheroidizing effect.

Method used

A device including an external pouring pipe and a steel casing was designed. Expansion gaps and anchoring steel structures were set up to prevent cracks, a heat-insulating space was formed to reduce the impact of high temperatures, and the central air duct and open slots were used to improve the uniform distribution of the spheroidizing agent. The performance and gas mixing effect increase the service life of the spray gun.

Benefits of technology

It effectively prevents the expansion and cracking of the spray gun, improves the working stability and service life, enhances the absorption rate and spheroidization effect of magnesium, and reduces the difficulty and cost of operation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808567A_ABST
    Figure CN118808567A_ABST
Patent Text Reader

Abstract

The molten iron spheroidizing device comprises an outer pouring pipe, a steel sleeve is arranged in the middle of the outer pouring pipe, an expansion gap is formed between the steel sleeve and the outer pouring pipe, a plurality of anchoring steel structures used for being connected with the outer pouring pipe are arranged on the outer side of the steel sleeve, and mounting holes are formed in the middles of the two ends of the steel sleeve. A feeding pipe is arranged between the two mounting holes, a heat insulation space located on the outer side of the feeding pipe is formed in an inner cavity of the steel sleeve, a feeding connecting pipe is arranged at the top end of the feeding pipe, a flaring reaction chamber is arranged at the bottom end of the outer pouring pipe, and the steel sleeve and the bottom end of the feeding pipe are connected with the flaring reaction chamber. The top of the steel sleeve is provided with a connecting structure used for being detachably connected with a steel ladle cover. The invention has the advantages of stable work, expansion cracking prevention and convenient use.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of molten iron treatment equipment, and in particular relates to a molten iron spheroidizing device. Background Art

[0002] The spheroidization treatment of molten iron is to add a certain amount of spheroidizing agent to the molten iron that meets specific conditions, so as to promote the precipitation of graphite in the form of small, uniform spheres during the solidification process, thereby obtaining cast iron with excellent mechanical properties. This kind of cast iron is called ductile iron because the graphite is spherical, and this treatment method is called spheroidization. The additive that makes the graphite in cast iron crystallize into spheres is called "spheroidizing agent". The main components of "spheroidizing agent" are spheroidizing elements, such as Mg, Ce, and Ca. The spheroidal graphite in ductile iron is formed by spheroidizing the molten iron, which makes its strength much higher than that of gray cast iron and its toughness better than that of malleable cast iron, while maintaining a series of advantages of gray cast iron.

[0003] There are many spheroidizing processes, such as flushing method, subcontracting method, wire feeding method, and pressure plus magnesium method.

[0004] Since magnesium has a low boiling point and is difficult to dissolve in molten iron, and the temperature of molten iron can reach 1500°C during spheroidization, magnesium is prone to violent reactions in molten iron, resulting in a low absorption rate. When the pressure of the medium surrounding magnesium increases, the boiling temperature of magnesium increases accordingly, the burning loss of magnesium decreases, and the absorption rate of magnesium increases. Based on this characteristic, the pressure-added magnesium method uses pure magnesium for spheroidization. The absorption rate of magnesium is high, reaching 70% to 80%, and there is no smoke and dust during the treatment process, the working environment is good, the cost is low, and it is suitable for mass production.

[0005] The problems with the existing technology are that the spray gun works in poor conditions during the molten iron spheroidization reaction, which is prone to cracking and burning; the spray gun has a short service life and needs to be replaced frequently, which is inconvenient to operate. Summary of the invention

[0006] The purpose of the present invention is to provide a molten iron spheroidizing device in view of the problems existing in the prior art. The device has the advantages of stable operation, prevention of expansion and cracking, and easy use.

[0007] To achieve the above-mentioned purpose, the technical solution adopted by the present invention is: a molten iron spheroidizing device, including an external pouring tube, a steel casing is arranged in the middle of the external pouring tube, an expansion gap is arranged between the steel casing and the external pouring tube, a plurality of anchoring steel structures for connecting the external pouring tube are arranged on the outside of the steel casing, mounting holes are opened in the middle of both ends of the steel casing, a feed pipe is arranged between the two mounting holes, the inner cavity of the steel casing forms an insulating space located outside the feed pipe, a feed connecting pipe is arranged at the top of the feed pipe, a flaring reaction chamber is arranged at the bottom end of the external pouring tube, the bottom ends of the steel casing and the feed pipe are connected to the flaring reaction chamber, and a connecting structure for detachably connecting a ladle cover is arranged at the top of the steel casing.

[0008] In the above scheme, the external pouring pipe is used to isolate the high-temperature molten iron and protect the internal pipe body. An expansion gap is set to allow the internal steel pipe structure and the external pouring pipe to expand and contract, so as to prevent the interaction force caused by the difference in expansion coefficient between the internal steel pipe structure and the external pouring pipe at high temperature, which may lead to cracks. The connection between the steel casing and the external pouring pipe is ensured by anchoring the steel structure. The feed pipe is connected to the mounting holes at both ends of the steel casing, which is convenient for feeding and unloading the feed pipe. There is no direct contact between the steel casing and the axial middle section of the feed pipe, forming an insulating space to reduce the influence of the external molten iron heat on the feed pipe. The feed connecting pipe is used for the entry of spheroidizing agent and inert gas. The expanded reaction chamber is used for the diffusion of spheroidizing agent and contact with high-temperature molten iron for spheroidizing reaction. The top of the steel casing is detachably connected to the ladle cover through a connecting structure, which is convenient for maintenance and replacement.

[0009] Furthermore, a steel mesh cage is provided on the anchoring steel structure, and the steel mesh cage is located inside the outer casting pipe.

[0010] The external pouring pipe structure is strengthened by arranging a steel mesh cage on the anchoring steel structure to improve the stability of the external pouring pipe structure.

[0011] Furthermore, the steel mesh cage includes an expansion cage, and the expansion cage is located inside the expansion reaction chamber.

[0012] The expanded reaction chamber is strengthened by providing an expanded cage structure, thereby improving structural stability and preventing the expanded reaction chamber from being deformed due to impact.

[0013] Furthermore, a central air duct is provided in the middle of the feeding pipe, a central inlet pipe is connected to the top of the central air duct, and the central inlet pipe penetrates the feeding pipe.

[0014] The central air duct in the middle of the feeding pipe is used to pressurize the middle of the spheroidizer in the bottom reaction chamber to disperse the spheroidizer outward, avoid uneven distribution of the spheroidizer, improve the spheroidizing effect, and avoid backflow of molten iron and blockage of the pipe mouth. The central inlet pipe is used to connect the air source.

[0015] Furthermore, a plurality of opening grooves are provided on the bottom end surface of the expanded reaction chamber.

[0016] The opening groove is opened in the horizontal direction. By opening the opening groove at the bottom of the expanding reaction chamber, it is convenient to discharge the high-pressure gas in the expanding reaction chamber to the surroundings, thereby improving the stirring effect of the gas on the molten iron and allowing the spheroidizing agent to fully react with the molten iron.

[0017] Furthermore, the cross section of the expanded reaction chamber is circular, and the open grooves are equidistantly distributed along the circumference of the expanded reaction chamber.

[0018] The circular structure is easy to set up, and the open grooves are arranged at equal intervals around the circumference to improve the uniformity of the distribution of the spheroidizer and enhance the stirring effect of the gas on the molten iron.

[0019] Furthermore, the connection structure includes a fixed flange and a movable flange, and a threaded fastener is detachably provided between the fixed flange and the movable flange.

[0020] When in use, the fixed flange and the movable flange are respectively arranged on both sides of the ladle cover, and a threaded connection hole is opened on the fixed flange, and the fixed flange and the movable flange are fixedly connected with the ladle cover through the threaded fasteners. The fixed flange is fixedly connected with the steel casing.

[0021] Furthermore, the thermal insulation space is filled with a thermal insulation material layer.

[0022] The heat-insulating material layer is wrapped around the outside of the feeding pipe to isolate the high temperature in the molten iron, avoid excessive temperature at the feeding pipe, and prevent the spheroidizer from being heated and causing blockage in the pipe.

[0023] Furthermore, the anchoring steel structure includes a plurality of steel columns or steel discs arranged outside the steel casing.

[0024] The stability of the connection between the external pouring pipe and the steel casing is enhanced by a number of steel columns or steel discs, and the strength of the external pouring pipe is enhanced to prevent deformation and cracking due to impact.

[0025] Furthermore, the central inlet pipe and the feed connecting pipe are respectively provided with connecting valves.

[0026] The connecting valves facilitate the corresponding connection of the central air source and the spheroidizing agent airflow, and are also convenient for controlling the switch.

[0027] Compared with the prior art, the present invention has the following beneficial effects:

[0028] 1. By setting a steel casing and strengthening the steel structure inside the outer tube body, the structural stability of the outer tube body is improved to prevent the tube body from being deformed, cracked or burned due to the impact of molten iron, and to improve the working stability of the spray gun;

[0029] 2. By setting an expansion gap between the steel casing and the external pouring pipe to leave expansion space, the cracking problem caused by the different expansion degrees of the two after heating can be solved, and the connection between the steel casing and the external pouring pipe can be ensured to be stable by anchoring the steel structure;

[0030] 2. A feed pipe and a central air duct are arranged in the middle of the inner cavity of the steel casing to form an insulation space. An insulation material layer is arranged in the insulation space to improve the insulation effect, reduce the temperature influence of the external high-temperature molten iron on the internal feed pipe and spheroidizing agent, and avoid the spheroidizing agent in the feed pipe being blocked by the high temperature; the air pressure at the bottom expansion reaction chamber is strengthened by the central air duct, and under the action of magnesium steam and air pressure of the air duct, the backflow of molten iron is avoided to cause blockage of the pipe mouth. It has the characteristics of not easy to be blocked and easy to clean, which can effectively increase the number of times a single spray gun is used and prolong the life of the spray gun;

[0031] 3. The spray gun and the ladle cover are detachably connected by setting a connection structure on the steel casing, which is convenient for maintenance and replacement of the spray gun and easy to use;

[0032] 4. By setting the opening slot, the scouring of the airflow and molten iron on the expanded reaction chamber is reduced, so that the small flow of gas impacts the surrounding of the expanded reaction chamber, which improves the mixing efficiency, helps to increase the solubility of magnesium gas in the molten iron, and thus improves the utilization rate of magnesium;

[0033] 5. The outer casting pipe is structurally strengthened by setting a steel mesh cage on the anchoring steel structure, and the expansion cage is used to structurally strengthen the expansion reaction chamber to improve the overall working stability and service life of the barrel. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Figure 1 This is a schematic structural diagram of a molten iron spheroidizing device according to Example 1 of the present invention;

[0035] Figure 2 It is a structural stereogram of a steel mesh cage in Example 1 of the present invention;

[0036] Figure 3 This is a schematic diagram of the installation of a steel mesh cage in Example 1 of the present invention;

[0037] In the figure: 1. External pouring pipe; 2. Steel casing; 3. Anchoring steel structure; 4. Mounting hole; 5. Feed pipe; 6. Insulation space; 7. Central air duct; 8. Central inlet pipe; 9. Feed connecting pipe; 10. Expanding reaction chamber; 11. Fixed flange; 12. Movable flange; 13. Threaded fastener; 14. Open groove; 15. Insulation material layer; 16. Connecting valve; 17. Steel mesh cage; 18. Expanding cage; 19. Ladle; 20. Ladle cover; 21. Expansion gap. DETAILED DESCRIPTION

[0038] The technical solution of the present invention will be clearly and completely described below in conjunction with the drawings in the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. In the description of the present invention, it should be noted that the terms front, back, left, right, etc. indicating directions or positional relationships are based on the directions or positional relationships shown in the drawings, or are the directions or positional relationships in which the invented product is usually placed when used. They are only for the convenience of describing the present invention or simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed or operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0039] Example 1

[0040] like Figure 1-3 As shown, a molten iron spheroidizing device comprises an external pouring tube 1, a steel casing 2 is arranged in the middle of the external pouring tube 1, an expansion gap 21 is arranged between the steel casing 2 and the external pouring tube 1, a plurality of anchoring steel structures 3 for connecting the external pouring tube 1 are arranged on the outside of the steel casing 2, mounting holes 4 are opened in the middle of both ends of the steel casing 2, a feed pipe 5 is arranged between the two mounting holes 4, the inner cavity of the steel casing 2 forms an insulating space 6 located outside the feed pipe 5, a feed connecting pipe 9 is arranged at the top of the feed pipe 5, a flaring reaction chamber 10 is arranged at the bottom end of the external pouring tube 1, the bottom ends of the steel casing 2 and the feed pipe 5 are connected to the flaring reaction chamber 10, and a connecting structure for detachably connecting a ladle cover 20 is arranged at the top of the steel casing 2.

[0041] In the above scheme, the outer pouring tube 1 is used to isolate the high-temperature molten iron and protect the internal pipe body. An expansion gap 21 is set to allow the internal steel pipe structure and the outer pouring tube 1 to expand and contract, so as to prevent the interaction force caused by the difference in expansion coefficient between the internal steel pipe structure and the outer pouring tube 1 at high temperature, resulting in cracks. The connection between the steel casing 2 and the outer pouring tube 1 is ensured by anchoring the steel structure 3. The feed pipe 5 is connected to the mounting holes 4 at both ends of the steel casing 2, which is convenient for feeding and unloading the feed pipe 5. There is no direct contact between the steel casing 2 and the axial middle section of the feed pipe 5, forming an insulating space 6 to reduce the influence of the external molten iron heat on the feed pipe 5. The feed connecting pipe 9 is used for the entry of spheroidizing agent and inert gas, and the expanded reaction chamber 10 is used for the diffusion of spheroidizing agent, which contacts with the high-temperature molten iron for spheroidizing reaction. The top of the steel casing 2 is detachably connected to the ladle cover 20 through a connecting structure, which is convenient for maintenance and replacement.

[0042] The steel casing 2, the material delivery pipe 5, the central air duct 7, and the external pouring pipe 1 are arranged coaxially. The material of the external pouring pipe 1 is a high-aluminum mullite refractory material. The width of the expansion gap 21 is 2-5 mm. The ladle cover 20 is provided with a positioning hole for matching with the steel casing 2, and the feed connection pipe 9 and the central inlet pipe 8 are located within the projection range of the steel casing 2, so as to facilitate the installation in coordination with the positioning hole.

[0043] Furthermore, a steel mesh cage 17 is provided on the anchoring steel structure 3 , and the steel mesh cage 17 is located inside the outer pouring pipe 1 .

[0044] The structure of the external pouring pipe 1 is strengthened by arranging a steel mesh cage 17 on the anchoring steel structure 3 , thereby improving the structural stability of the external pouring pipe 1 .

[0045] The steel mesh cage 17 uses castable heat-resistant steel bar material.

[0046] Furthermore, the steel mesh cage 17 includes an expansion cage 18 , and the expansion cage 18 is located inside the expansion reaction chamber 10 .

[0047] The expanded reaction chamber 10 is reinforced by providing the expanded cage 18 structure, thereby improving the structural stability and preventing the expanded reaction chamber 10 from being deformed due to impact.

[0048] Furthermore, a central air duct 7 is provided in the middle of the feeding pipe 5 , and a central inlet pipe 8 is connected to the top of the central air duct 7 , and the central inlet pipe 8 penetrates the feeding pipe 5 .

[0049] The central air duct 7 in the middle of the feeding pipe 5 is used to pressurize the middle of the spheroidizing agent at the bottom reaction chamber to disperse the spheroidizing agent outward, avoid uneven distribution of the spheroidizing agent, improve the spheroidizing effect, and avoid backflow of molten iron to block the pipe mouth. The central inlet pipe 8 is used to connect the air source.

[0050] The wind source is an inert gas, such as nitrogen.

[0051] Furthermore, a plurality of opening grooves 14 are formed on the bottom surface of the expanded reaction chamber 10 .

[0052] The opening groove 14 is opened in the horizontal direction. By opening the opening groove 14 at the bottom of the expanding reaction chamber 10, it is convenient to discharge the high-pressure gas in the expanding reaction chamber 10 to the surroundings, thereby improving the stirring effect of the gas on the molten iron and allowing the spheroidizing agent to fully react with the molten iron.

[0053] When molten iron is spheroidized by the pressure-added magnesium method, the boiling point of magnesium increases under high pressure, and the overall pressure in the ladle 19 needs to be increased to increase the absorption rate of magnesium. The provision of the open groove 14 is conducive to the discharge of high-pressure gas from the reaction chamber, reducing the pressure on the expanded reaction chamber 10, and accumulating the gas between the ladle cover 20 and the top surface of the molten iron, thereby pressurizing the molten iron.

[0054] Furthermore, the cross section of the expanded reaction chamber 10 is circular, and the open grooves 14 are distributed equidistantly along the circumference of the expanded reaction chamber 10 .

[0055] The circular structure is convenient to set up, and the open grooves 14 are arranged at equal intervals in the circumferential direction, so as to improve the uniformity of the distribution of the spheroidizing agent and the stirring effect of the gas on the molten iron.

[0056] The opening groove 14 is a strip groove consisting of a bottom rectangular groove and an upper arc groove.

[0057] Furthermore, the connection structure includes a fixed flange 11 and a movable flange 12 , and a threaded fastener 13 is detachably provided between the fixed flange 11 and the movable flange 12 .

[0058] When in use, the fixed flange 11 and the movable flange 12 are respectively arranged on both sides of the ladle cover 20, and a threaded connection hole is opened on the fixed flange 11, and the fixed flange 11 and the movable flange 12 are fixedly connected to the ladle cover 20 through the threaded fasteners 13. The fixed flange 11 is fixedly connected to the steel casing 2.

[0059] The threaded fastener 13 includes bolts, and bolt holes are provided on the movable flange 12 and the ladle cover 20. The movable flange 12 can also be removed, and the fastening between the fixed flange 11 and the ladle cover 20 can be directly performed with bolts.

[0060] Furthermore, the heat insulating space 6 is filled with a heat insulating material layer 15 .

[0061] The heat insulating material layer 15 is coated on the outside of the feeding pipe 5 to isolate the high temperature in the molten iron, avoid the feeding pipe 5 from being too high in temperature, and prevent the spheroidizing agent from being heated and causing the pipe body to be blocked.

[0062] The heat insulating material layer 15 comprises quartz sand and has a thickness of not less than 5 mm.

[0063] Furthermore, the anchoring steel structure 3 includes a plurality of steel columns or steel discs arranged outside the steel casing 2 .

[0064] The stability of the connection between the outer pouring pipe 1 and the steel casing 2 is enhanced by a plurality of steel columns or steel discs, and the strength of the outer pouring pipe 1 is enhanced to prevent deformation and cracking due to impact.

[0065] Furthermore, the central inlet pipe 8 and the feed connecting pipe 9 are respectively provided with connecting valves 16 .

[0066] The connecting valve 16 facilitates the corresponding connection of the central air source and the spheroidizing agent airflow, and is also convenient for controlling the switch.

[0067] During operation: open the connecting valve 16, first deliver nitrogen through the central inlet pipe 8 and the feed connecting pipe 9, deliver it to the reaction chamber along the seamless steel pipe feed pipe 5 and enter the molten iron, then deliver the passivated magnesium particles through the feed connecting pipe 9, deliver it to the reaction chamber along the seamless steel pipe feed pipe 5 and enter the molten iron, and under the action of nitrogen, the passivated magnesium particles are fully contacted and reacted with the molten iron to achieve the purpose of spheroidizing the molten iron. When the spray gun needs to be maintained and replaced, only the connection structure on the ladle cover 20 needs to be disassembled.

[0068] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A molten iron spheroidizing device, It is characterized in that It includes an external pouring tube, a steel casing is arranged in the middle of the external pouring tube, an expansion gap is arranged between the steel casing and the external pouring tube, a plurality of anchoring steel structures for connecting the external pouring tube are arranged on the outside of the steel casing, mounting holes are opened in the middle of both ends of the steel casing, a feed pipe is arranged between the two mounting holes, an inner cavity of the steel casing forms an insulating space located outside the feed pipe, a feed connecting pipe is arranged at the top of the feed pipe, a flaring reaction chamber is arranged at the bottom end of the external pouring tube, the bottom ends of the steel casing and the feed pipe are connected to the flaring reaction chamber, and a connecting structure for detachably connecting a ladle cover is arranged at the top of the steel casing.

2. The molten iron spheroidizing device according to claim 1, It is characterized in that A steel mesh cage is arranged on the anchoring steel structure, and the steel mesh cage is located inside the outer pouring pipe.

3. The molten iron spheroidizing device according to claim 2, It is characterized in that The steel mesh cage comprises an expansion cage, and the expansion cage is located inside the expansion reaction chamber.

4. The molten iron spheroidizing device according to claim 1, It is characterized in that A central air duct is arranged in the middle of the feeding pipe, and a central inlet pipe is connected to the top of the central air duct, and the central inlet pipe penetrates the feeding pipe.

5. The molten iron spheroidizing device according to claim 1, It is characterized in that A plurality of opening grooves are formed on the bottom end surface of the expanded reaction chamber.

6. The molten iron spheroidizing device according to claim 5, It is characterized in that The cross section of the expanded reaction chamber is circular, and the open grooves are evenly distributed along the circumference of the expanded reaction chamber.

7. The molten iron spheroidizing device according to claim 1, It is characterized in that The connection structure includes a fixed flange and a movable flange, and a threaded fastener is detachably arranged between the fixed flange and the movable flange.

8. The molten iron spheroidizing device according to claim 1, It is characterized in that The heat-insulating space is filled with a heat-insulating material layer.

9. The molten iron spheroidizing device according to claim 1, It is characterized in that The anchoring steel structure comprises a plurality of steel columns or steel discs arranged outside the steel casing.

10. The molten iron spheroidizing device according to claim 4, It is characterized in that The central inlet pipe and the feed connecting pipe are respectively provided with connecting valves.