Buried gate double-junction barrier Schottky diode and manufacturing method thereof
By using multiple grid segments and different Schottky material layer structures in a buried-gate double-junction barrier Schottky diode, the problem of insufficient performance of diodes in the existing technology under forward and reverse direction voltages is solved, achieving Better current conduction and blocking performance.
Patent Information
- Application Number
- CN202311425748.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-04-20
- Filing Date
- 2023-10-30
- Publication Date
- 2024-10-22
AI Technical Summary
Existing buried-gate double-junction barrier Schottky diodes do not block current perfectly when voltage is applied in the opposite direction, and do not conduct current perfectly when voltage is applied in the forward direction, resulting in leakage current and unsatisfactory thresholds. voltage, forward voltage drop, and on-resistance.
Adopting a structure including a drift layer, a grid layer, a regrowth layer, a first Schottky material layer and a second Schottky material layer, wherein a plurality of grid segments define a grid spacing area between adjacent grid segments , the first Schottky material layer is at least partially located on the regrowth layer and overlaps the grid layer, the second Schottky material layer is at least partially located on the regrowth layer and overlaps the grid spacing area, and has different Schottky Base barrier height.
Through this structure, it is possible to reduce the threshold voltage, forward voltage drop and on-resistance in the forward direction and improve the current conduction performance; to reduce the leakage current and increase the breakdown voltage in the opposite direction to maintain the blocking performance.
Smart Images

Figure CN118825084A_ABST
Abstract
Description
Technical Field
[0001] The presently disclosed subject matter relates generally to junction barrier Schottky diodes and, in some non-limiting embodiments or aspects, to buried gate double junction barrier Schottky diodes and methods of making the same. Background Art
[0002] Certain diodes are particularly useful in power electronics for a variety of applications such as automotive equipment, photovoltaic inverters (e.g., for solar energy), wind power generation equipment, power distribution, etc. For example, certain diodes conduct current when voltage is applied in one direction (e.g., forward direction, from anode to cathode, etc.) and block current when voltage is applied in another direction (e.g., reverse direction, from cathode to anode, etc.).
[0003] However, such diodes may not perfectly block current when voltage is applied in the reverse direction. For example, such diodes may have leakage current, which may be current that leaks when voltage is applied in the reverse direction (e.g., conducted in the reverse direction, from cathode to anode, etc.). Even a small amount of leakage current may be undesirable and / or problematic, especially in high power (e.g., relatively high voltage, current, etc.) applications. In addition, such diodes may not perfectly conduct current when voltage is applied in the forward direction. For example, such diodes may have unsatisfactory (e.g., higher than desired) threshold voltage, forward voltage drop, on-resistance, and / or conduction loss. Moreover, adopting such diodes (e.g., changing the structure, topology, and / or materials of such diodes) to improve one of the performance of blocking (e.g., when voltage is applied in the reverse direction) and / or current conduction (e.g., when voltage is applied in the forward direction) may result in a reduction in the performance of the other (e.g., improving blocking performance may result in a reduction in current conduction performance, and vice versa). Summary of the invention
[0004] It is therefore an object of the presently disclosed subject matter to provide a buried-gate double-junction barrier Schottky diode and method of making the same that overcomes some or all of the above-mentioned deficiencies.
[0005] According to a non-limiting embodiment or aspect, a buried gate double junction barrier Schottky diode is provided. For example, the buried gate double junction barrier Schottky diode may include a drift layer, a grid layer including a plurality of grid segments at least partially in the drift layer, a regrown layer on the grid layer and the drift layer, a first Schottky material layer, and a second Schottky material layer. The plurality of grid segments may define at least one grid spacing region between adjacent grid segments in the plurality of grid segments. The first Schottky material layer may be at least partially located on the regrown layer and / or may at least partially overlap the plurality of grid segments of the grid layer. The second Schottky material layer may be at least partially located on the regrown layer and / or may at least partially overlap at least one grid spacing region. The second Schottky material layer may have a Schottky barrier height different from that of the first Schottky material layer.
[0006] In some non-limiting embodiments or aspects, the buried gate double junction barrier Schottky diode may further include a substrate layer. For example, the substrate layer may be below the drift layer.
[0007] In some non-limiting embodiments or aspects, the buried gate double junction barrier Schottky diode may further include a metallization layer. For example, the substrate layer may be on the metallization layer.
[0008] In some non-limiting embodiments or aspects, the buried gate double junction barrier Schottky diode may further include a buffer layer on the substrate layer. For example, the drift layer may be on the buffer layer.
[0009] In some non-limiting embodiments or aspects, the top surface of the grid layer may be in a plane and the top surface of the drift layer may be in the plane (eg, the same plane). The regrown layer may be on the top surface of the grid layer and the top surface of the drift layer.
[0010] In some non-limiting embodiments or aspects, the second Schottky material layer may have a higher Schottky barrier height than the first Schottky material layer.
[0011] In some non-limiting embodiments or aspects, the first Schottky material layer can be on the second Schottky material layer, and the second Schottky material layer can be at least partially in the first Schottky material layer.
[0012] In some non-limiting embodiments or aspects, the second Schottky material layer can be on the first Schottky material layer, and the first Schottky material layer can be at least partially in the second Schottky material layer.
[0013] In some non-limiting embodiments or aspects, at least one of the first Schottky material layer or the second Schottky material layer may include an anode. Additionally or alternatively, the buried gate double junction barrier Schottky diode may further include a cathode on a side of the drift layer opposite to the anode.
[0014] In some non-limiting embodiments or aspects, when a positive voltage greater than a threshold voltage is applied from the anode to the cathode, the buried gate double junction barrier Schottky diode can be operated in a current conduction mode. Additionally or alternatively, when a negative voltage is applied from the anode to the cathode, the buried gate double junction barrier Schottky diode can be operated in a voltage blocking mode.
[0015] In some non-limiting embodiments or aspects, the buried gate double junction barrier Schottky diode may further include an anode at least partially on at least one of the first Schottky material layer or the second Schottky material layer. Additionally or alternatively, the buried gate double junction barrier Schottky diode may further include a cathode on the side of the drift layer opposite to the anode.
[0016] In some non-limiting embodiments or aspects, the first Schottky material layer may include a plurality of segments, each respective segment of the first Schottky material layer at least partially overlapping a respective grid segment of the plurality of grid segments of the grid layer.
[0017] In some non-limiting embodiments or aspects, a width of each respective segment of the first Schottky material layer may be smaller than a width of a respective grid segment of the plurality of grid segments of the grid layer.
[0018] In some non-limiting embodiments or aspects, a width of each respective segment of the first Schottky material layer may be greater than or equal to a width of a respective grid segment of the plurality of grid segments of the grid layer.
[0019] In some non-limiting embodiments or aspects, at least one grid spacing region may include multiple grid spacing regions, and the second Schottky material layer may include multiple fragments, and each corresponding fragment of the second Schottky material layer at least partially overlaps a corresponding grid spacing region in the multiple grid spacing regions.
[0020] In some non-limiting embodiments or aspects, a width of each respective segment of the second Schottky material layer may be smaller than a width of a respective grid pitch region of the plurality of grid pitch regions.
[0021] In some non-limiting embodiments or aspects, a width of each respective segment of the second Schottky material layer may be greater than or equal to a width of a respective grid pitch region of the plurality of grid pitch regions.
[0022] According to a non-limiting embodiment or aspect, a method for manufacturing a buried gate double junction barrier Schottky diode is provided. The method may include forming a drift layer. The method may include forming a grid layer including a plurality of grid segments at least partially in the drift layer, and the plurality of grid segments may define at least one grid spacing region between adjacent grid segments in the plurality of grid segments. The method may include forming a regrown layer on the grid layer and the drift layer. The method may include forming a first Schottky material layer of a plurality of grid segments at least partially on the regrown layer and at least partially overlapping the grid layer. The method may include forming a second Schottky material layer at least partially on the regrown layer and at least partially overlapping at least one grid spacing region, the second Schottky material layer having a different Schottky barrier height than the first Schottky material layer.
[0023] In some non-limiting embodiments or aspects, the method may further include providing a substrate layer. In some non-limiting embodiments or aspects, the method may further include forming a buffer layer on the substrate layer. In some non-limiting embodiments or aspects, forming a drift layer may include forming a drift layer on the buffer layer.
[0024] In some non-limiting embodiments or aspects, forming the first Schottky material layer may include forming an intermediate first Schottky material layer on the regrown layer, and patterning the intermediate first Schottky material layer to form a first Schottky material layer that at least partially overlaps a plurality of grid segments of the grid layer. Additionally or alternatively, forming the second Schottky material layer may include forming the second Schottky material layer on the first Schottky material layer.
[0025] In some non-limiting embodiments or aspects, forming the second Schottky material layer may include forming an intermediate second Schottky material layer on the regrown layer, and patterning the intermediate second Schottky material layer to form a second Schottky material layer that at least partially overlaps at least one grid spacing region. Additionally or alternatively, forming the first Schottky material layer may include forming the first Schottky material layer on the second Schottky material layer.
[0026] In some non-limiting embodiments or aspects, the method may further include forming a metallization layer on a side of the substrate layer opposite to the buffer layer.
[0027] Further embodiments or aspects are set forth in the following numbered clauses:
[0028] Item 1: A buried-gate double-junction barrier Schottky diode comprising: a drift layer; a grid layer comprising a plurality of grid segments at least partially in the drift layer, the plurality of grid segments defining at least one grid spacing region between adjacent grid segments in the plurality of grid segments; a regrown layer on the grid layer and the drift layer; a first Schottky material layer at least partially on the regrown layer and at least partially overlapping the plurality of grid segments of the grid layer; and a second Schottky material layer at least partially on the regrown layer and at least partially overlapping at least one grid spacing region, the second Schottky material layer having a different Schottky barrier height than the first Schottky material layer.
[0029] Item 2: The buried gate double junction barrier Schottky diode of Item 1, further comprising: a substrate layer, wherein the substrate layer is below the drift layer.
[0030] Item 3: The buried gate double junction barrier Schottky diode of Item 1 or Item 2, further comprising: a metallization layer, wherein the substrate layer is on the metallization layer.
[0031] Item 4: The buried gate double junction barrier Schottky diode of any one of items 1-3, further comprising: a buffer layer on the substrate layer, wherein the drift layer is on the buffer layer.
[0032] Item 5: The buried gate double junction barrier Schottky diode of any one of items 1-4, wherein a top surface of the grid layer is in a plane, a top surface of the drift layer is in the plane, and the regrown layer is on a top surface of the grid layer and a top surface of the drift layer.
[0033] Item 6: The buried gate double junction barrier Schottky diode of any of items 1-5, wherein the second Schottky material layer has a higher Schottky barrier height than the first Schottky material layer.
[0034] Clause 7: The buried gate double junction barrier Schottky diode of any of clauses 1-6, wherein the first Schottky material layer is on the second Schottky material layer, and the second Schottky material layer is at least partially in the first Schottky material layer.
[0035] Clause 8: The buried gate double junction barrier Schottky diode of any of clauses 1-7, wherein the second Schottky material layer is on the first Schottky material layer, and the first Schottky material layer is at least partially in the second Schottky material layer.
[0036] Clause 9: The buried gate double junction barrier Schottky diode of any one of clauses 1-8, wherein at least one of the first Schottky material layer or the second Schottky material layer comprises an anode, the buried gate double junction barrier Schottky diode further comprising: a cathode on a side of the drift layer opposite the anode.
[0037] Item 10: The buried gate double junction barrier Schottky diode of any one of items 1-9, wherein when a positive voltage greater than a threshold voltage is applied from the anode to the cathode, the buried gate double junction barrier Schottky diode operates in a current conduction mode, and wherein when a negative voltage is applied from the anode to the cathode, the buried gate double junction barrier Schottky diode operates in a voltage blocking mode.
[0038] Clause 11: The buried gate double junction barrier Schottky diode of any of clauses 1-10, further comprising: an anode at least partially on at least one of the first Schottky material layer or the second Schottky material layer; and a cathode on a side of the drift layer opposite the anode.
[0039] Clause 12: The buried-gate double junction barrier Schottky diode of any of clauses 1-11, wherein the first Schottky material layer comprises a plurality of segments, each respective segment of the first Schottky material layer at least partially overlapping a respective grid segment of the plurality of grid segments of the grid layer.
[0040] Clause 13: The buried-gate double junction barrier Schottky diode of any of clauses 1-12, wherein a width of each respective segment of the first Schottky material layer is less than a width of a respective grid segment of the plurality of grid segments of the grid layer.
[0041] Clause 14: The buried-gate double junction barrier Schottky diode of any of clauses 1-13, wherein a width of each respective segment of the first Schottky material layer is greater than or equal to a width of a respective grid segment of the plurality of grid segments of the grid layer.
[0042] Item 15: The buried gate double junction barrier Schottky diode of any of items 1-14, wherein at least one grid spacing region includes a plurality of grid spacing regions, and wherein the second Schottky material layer includes a plurality of fragments, each respective fragment of the second Schottky material layer at least partially overlapping a respective grid spacing region of the plurality of grid spacing regions.
[0043] Item 16: A buried gate double junction barrier Schottky diode of any one of items 1-15, wherein one of the following: the width of each corresponding segment of the second Schottky material layer is less than the width of the corresponding grid spacing region in the plurality of grid spacing regions, or the width of each corresponding segment of the second Schottky material layer is greater than or equal to the width of the corresponding grid spacing region in the plurality of grid spacing regions.
[0044] Item 17: A method for manufacturing a buried gate double junction barrier Schottky diode, comprising: forming a drift layer; forming a grid layer including a plurality of grid segments at least partially in the drift layer, the plurality of grid segments defining at least one grid spacing region between adjacent grid segments in the plurality of grid segments; forming a regrown layer on the grid layer and the drift layer; forming a first Schottky material layer at least partially on the regrown layer and at least partially overlapping the plurality of grid segments of the grid layer; and forming a second Schottky material layer at least partially on the regrown layer and at least partially overlapping at least one grid spacing region, the second Schottky material layer having a different Schottky barrier height than the first Schottky material layer.
[0045] Item 18: The method of Item 17, further comprising: providing a substrate layer; and forming a buffer layer on the substrate layer, wherein forming the drift layer comprises forming the drift layer on the buffer layer.
[0046] Item 19: The method of Item 17 or Item 18, wherein forming a first Schottky material layer comprises: forming an intermediate first Schottky material layer on the regrown layer; and patterning the intermediate first Schottky material layer to form a first Schottky material layer of multiple grid segments that at least partially overlap the grid layer, wherein forming a second Schottky material layer comprises forming a second Schottky material layer on the first Schottky material layer.
[0047] Item 20: The method of any of items 17-19, wherein forming the second Schottky material layer includes: forming an intermediate second Schottky material layer on the regrown layer; and patterning the intermediate second Schottky material layer to form a second Schottky material layer that at least partially overlaps at least one grid spacing region, wherein forming the first Schottky material layer includes forming the first Schottky material layer on the second Schottky material layer.
[0048] Clause 21: The method of any of clauses 17-20, further comprising: forming a metallization layer on a side of the substrate layer opposite the buffer layer.
[0049] These and other features and characteristics of the presently disclosed subject matter, as well as the methods of operation and function of the related elements of the structure and the incorporation of parts and the economy of manufacture will become more apparent by considering the following description and appended claims with reference to the accompanying drawings, all of which form a part of this specification, wherein like reference numerals indicate corresponding parts in the various figures. It should be expressly understood, however, that the drawings are for purposes of illustration and description only and are not intended as a definition of the limitations of the disclosed subject matter. As used in the specification and claims, the singular forms of "a", "an", and "the" include plural referents unless the context clearly dictates otherwise. BRIEF DESCRIPTION OF THE DRAWINGS
[0050] Additional advantages and details of the disclosed subject matter are explained in more detail below with reference to exemplary embodiments or aspects illustrated in the accompanying drawings, in which:
[0051] Figure 1A and Figure 1B is a diagram of an exemplary buried-gate double-junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter;
[0052] Figure 2 is a flow chart of an exemplary method of fabricating a buried-gate double-junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter;
[0053] Figure 3A and Figure 3B is a diagram of an exemplary implementation of a buried-gate double-junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter;
[0054] Figure 4 is a graph of normalized electric field for an exemplary implementation of a buried gate double junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter;
[0055] Figure 5A is a graph of reverse current density and voltage for an exemplary implementation of a buried gate double junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter;
[0056] Figure 5B is a graph of forward current density and voltage for an exemplary implementation of a buried gate double junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter; and
[0057] Figure 6 is a graph of a ratio of a width of a first Schottky material layer to a width of a grid segment, forward voltage drop, and leakage current for an exemplary implementation of a buried-gate double-junction barrier Schottky diode according to some non-limiting examples or aspects of the presently disclosed subject matter. DETAILED DESCRIPTION
[0058] For purposes of the description below, the terms "end," "upper," "lower," "right," "left," "vertical," "horizontal," "top," "bottom," "lateral," "longitudinal," and their derivatives shall relate to the disclosed subject matter as it is oriented in the accompanying drawings. However, it should be understood that the disclosed subject matter may assume various alternative variations and step sequences unless expressly indicated to the contrary. It should also be understood that the specific devices and processes illustrated in the accompanying drawings and described in the following specification are merely exemplary embodiments or aspects of the disclosed subject matter. Therefore, unless otherwise indicated, specific dimensions and other physical characteristics associated with the embodiments or aspects disclosed herein should not be considered limiting.
[0059] Unless explicitly described as such, any aspect, component, element, structure, action, step, function, instruction, etc. used in this article should not be interpreted as critical or necessary. Moreover, as used herein, the articles "one" and "an" are intended to include one or more items, and can be used interchangeably with "one or more" and "at least one". In addition, as used herein, the term "set" is intended to include one or more items (e.g., related items, unrelated items, combinations of related and unrelated items, etc.), and can be used interchangeably with "one or more" or "at least one". In the case of only one item intended, the term "one" or similar language is used. Moreover, as used herein, the terms "having", "having", etc. are intended to be open terms. In addition, the phrase "based on" is intended to mean "based at least in part on", unless otherwise explicitly stated.
[0060] Some non-limiting embodiments or aspects are described herein in conjunction with a threshold value. As used herein, satisfying a threshold value may refer to being greater than a threshold value, more than a threshold value, above a threshold value, greater than or equal to a threshold value, less than a threshold value, less than a threshold value, below a threshold value, less than or equal to a threshold value, a value equal to a threshold value, etc.
[0061] Non-limiting embodiments or aspects of the disclosed subject matter are directed to a buried gate double junction barrier Schottky diode and a method for manufacturing the same. For example, non-limiting embodiments or aspects of the disclosed subject matter provide a buried gate double junction barrier Schottky diode, which may include a drift layer, a grid layer, a regrown layer, a first Schottky material layer, and a second Schottky material layer. The grid layer may include a plurality of grid segments at least partially in the drift layer, and the grid segments may define at least one grid spacing region between adjacent grid segments. The regrown layer may be on the grid layer and the drift layer. The first Schottky material layer may be at least partially on the regrown layer and / or may at least partially overlap the grid segments of the grid layer. The second Schottky material layer may be at least partially on the regrown layer and / or may at least partially overlap (one or more) grid spacing regions. The second Schottky material layer may have a different Schottky barrier height than the first Schottky material layer. Such embodiments or aspects provide a diode having two different Schottky contact materials (e.g., double junction), the two different Schottky contact materials being arranged to improve at least one of blocking performance and / or current conduction performance (e.g., while also maintaining and / or improving the other). For example, a first Schottky material layer (e.g., having a lower Schottky barrier height) that at least partially overlaps a grid segment of a grid layer improves current conduction (e.g., when voltage is applied in a forward direction) by reducing threshold voltage, forward voltage drop, on-resistance, and / or conduction losses, and a second Schottky material layer (e.g., having a higher Schottky barrier height) that at least partially overlaps (one or more) grid spacing regions maintains and / or improves blocking performance (e.g., when voltage is applied in a reverse direction) by having similar or reduced leakage current and / or similar or increased breakdown voltage (e.g., compared to a diode having a single Schottky material layer).
[0062] For purposes of illustration, in the following description, although the presently disclosed subject matter is described with respect to a junction barrier Schottky diode, such as a buried gate double junction barrier Schottky diode and methods of manufacturing the same, those skilled in the art will recognize that the disclosed subject matter is not limited to the illustrative embodiments or aspects. For example, the systems and methods described herein can be used with a variety of settings, such as semiconductor devices such as diodes, rectifiers, transistors, integrated circuits, etc., in any setting where it may be useful to conduct current in one direction and block voltage in another direction.
[0063] Reference now Figure 1A and Figure 1B , Figure 1A and Figure 1B is a diagram of an exemplary buried gate double junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter. Figure 1A and Figure 1BAs shown in the figure, the buried gate double junction barrier Schottky diode 100 may include at least one of a metallization layer 102, a substrate layer 104, a buffer layer 106, a drift layer 108, a grid layer 110, a grid spacing region 111, a regrown layer 112, a first Schottky material layer 114, and a second Schottky material layer 116 and / or any combination thereof.
[0064] The metallization layer 102 may include a layer of a metal material and / or other conductive material. For example, the metal and / or conductive material of the metallization layer 102 may include a layer of aluminum (Al), silver (Ag), gold (Au), copper (Cu), titanium (Ti), nickel (Ni), an alloy of at least two metals, a compound including at least one metal, polysilicon, silicide, an ohmic contact (e.g., silicide), any combination thereof, and the like. For example, an ohmic contact (e.g., silicide) may be formed by depositing a thin layer of nickel (Ni), followed by annealing (e.g., thermal annealing, laser annealing, etc.) to form a nickel silicide layer. Additionally or alternatively, a metal and / or conductive material (e.g., as described above) may be deposited on the nickel silicide layer.
[0065] The substrate layer 104 may include a layer of material on (e.g., above, in contact with, etc.) the metallization layer 102. For example, the substrate layer 104 may include a layer of n-type (e.g., lightly n-doped) semiconductor material, such as silicon carbide (SiC), silicon (Si), a compound including at least one semiconductor material, any combination thereof, etc. Additionally or alternatively, the substrate layer 104 may include a layer of a highly conductive material (e.g., a semiconductor material, a metallic material, any combination thereof, etc.).
[0066] The buffer layer 106 may include a material layer on (e.g., above, in contact with, etc.) the substrate layer 104. Additionally or alternatively, the buffer layer 106 may be above (and / or on and / or in contact with) the metallization layer 102. In some non-limiting embodiments or aspects, the buffer layer 106 may include n + The buffer layer 106 may include a layer of a type (e.g., highly n-doped) semiconductor material, such as silicon carbide (SiC), silicon (Si), a compound including at least one semiconductor material, any combination thereof, etc. Additionally or alternatively, the buffer layer 106 may include a layer of a material having the same type of doping as the substrate layer 104. In some non-limiting embodiments or aspects, the buffer layer 106 may include an epitaxial buffer layer.
[0067] The drift layer 108 may include a layer of material on (e.g., above, in contact with, etc.) the buffer layer 106. Additionally or alternatively, the drift layer 108 may be above (and / or on and / or in contact with) the buffer layer 106, the substrate layer 104, and / or the metallization layer 102. In some non-limiting embodiments or aspects, the buffer layer 106 may include a layer of n-type (e.g., lightly n-doped) semiconductor material, such as a layer of silicon carbide (SiC), silicon (Si), a compound including at least one semiconductor material, any combination thereof, and the like. Additionally or alternatively, the drift layer 108 may include a layer of material having the same type of doping as the substrate layer 104 and / or the buffer layer 106. In some non-limiting embodiments or aspects, the drift layer 108 may include an epitaxial drift layer.
[0068] The grid layer 110 may include a plurality of grid segments at least partially within (eg, embedded within, in contact with, etc.) the drift layer 108. Figure 1A and Figure 1B As shown in , the grid layer 110 includes three grid segments, but may include any suitable number of grid segments. In some non-limiting embodiments or aspects, the grid segments of the grid layer 110 may have a repeating structure in at least one direction. For example, the grid segments may have a repeating structure in a first direction, and the repeating structure may be repeated at regular distances at least in the first direction (e.g., grid segments shaped like bars of the same and / or substantially similar size are spaced apart by grid spacing regions 111 of the same and / or substantially similar size in the first direction). Additionally or alternatively, the grid segments may have a repeating structure in both the first direction and the second direction (e.g., the grid segments may be squares, circles, hemispherical shapes, and / or any other suitable shapes spaced apart by first grid spacing regions 111 of the same and / or substantially similar size in the first direction and spaced apart by second grid spacing regions 111 of the same and / or substantially similar size, rather than linearly spaced bars in one direction, wherein the first and second grid spacing regions 111 may be the same or different sizes). In some non-limiting embodiments or aspects, a plurality of grid segments may define at least one grid spacing region 111 between adjacent grid segments. Figure 1A and Figure 1B As shown in FIG, two grid spacing regions 111 are shown between three grid segments, but any suitable number of grid spacing regions (e.g., based on the number of grid segments) may be included. In some non-limiting embodiments or aspects, the grid layer 110 may include p-type (e.g., lightly p-doped) and / or p-type. +The grid layer 110 may include a material layer having a doping type (e.g., highly p-doped) semiconductor material such as silicon carbide (SiC), silicon (Si), a compound including at least one semiconductor material, any combination thereof, etc. Additionally or alternatively, the grid layer 110 may include a material layer having a doping type opposite to that of the substrate layer 104, the buffer layer 106, and / or the drift layer 108. In some non-limiting embodiments or aspects, the grid layer 110 may include a material layer having a higher doping level than the drift layer 108.
[0069] The regrown layer 112 may include a material layer on (e.g., above, in contact with, etc.) the drift layer 108 and / or the grid layer 110. For example, the top surface of the grid layer 110 may be in a plane, the top surface of the drift layer 108 may be in the plane (e.g., the top surfaces of the grid layer 110 and the drift layer 108 may be in the same plane), and the regrown layer 112 may be on (e.g., above, in contact with, etc.) the top surfaces of the grid layer and the drift layer (e.g., on the plane). In some non-limiting embodiments or aspects, the regrown layer 112 may include a layer of n-type (e.g., lightly n-doped) semiconductor material, such as silicon carbide (SiC), silicon (Si), a compound including at least one semiconductor material, any combination thereof, and the like. Additionally or alternatively, the regrown layer 112 may include a material layer having the same type of doping as the substrate layer 104, the buffer layer 106, and / or the drift layer 108. In some non-limiting embodiments or aspects, the regrown layer 112 may include an epitaxial regrown layer.
[0070] The first Schottky material layer 114 may include a material layer that at least partially overlaps (e.g., is above, etc.) a grid segment of the grid layer 110. For example, the first Schottky material layer 114 may be at least partially on (e.g., above, in contact with, etc.) the regrown layer 112. In some non-limiting embodiments or aspects, the first Schottky material layer 114 may include a metal material and / or other conductive material. For example, the first Schottky material layer 114 may include a layer of titanium (Ti), titanium disulfide (TiS2), titanium nitride (TiN), tungsten silicide (WSi2), polysilicon, silicide, an alloy of at least two metals, a compound including at least one metal (e.g., a compound of at least one semiconductor material and at least one metal material), any combination thereof, etc. In some non-limiting embodiments or aspects, the first Schottky material layer 114 may be surface treated to adjust (e.g., reduce, etc.) its Schottky barrier height. For example, the surface treatment of the first Schottky material layer 114 may include at least one of annealing, temperature treatment, ion sputtering, any combination thereof, etc.
[0071] The second Schottky material layer 116 may include a material layer that at least partially overlaps (one or more) grid spacing regions 111 (e.g., above them, etc.). For example, the second Schottky material layer 116 may be at least partially on the regrown layer 112 (e.g., above them, in contact with them, etc.). In some non-limiting embodiments or aspects, the second Schottky material layer 116 may include a metal material and / or other conductive material. For example, the second Schottky material layer 116 may include titanium (Ti), titanium disulfide (TiS2), titanium nitride (TiN), tungsten silicide (WSi2), polysilicon, silicide, an alloy of at least two metals, a compound including at least one metal (e.g., a compound of at least one semiconductor material and at least one metal material), any combination thereof, and the like. In some non-limiting embodiments or aspects, the second Schottky material layer 116 may be surface treated to adjust (e.g., increase, etc.) its Schottky barrier height. For example, the surface treatment of the second Schottky material layer 116 may include at least one of annealing, temperature treatment, ion sputtering, any combination thereof, and the like.
[0072] In some non-limiting embodiments or aspects, the second Schottky material layer 116 may have a different (e.g., higher, larger, etc.) Schottky barrier height than the first Schottky material layer 114. For example, the second Schottky material layer 116 may include a different material than the first Schottky material layer 114 (e.g., different materials may have different Schottky barrier heights). Additionally or alternatively, the second Schottky material layer 116 may be surface treated differently from the first Schottky material layer 114 (e.g., even if the first Schottky material layer 114 and the second Schottky material layer 116 include the same material, if the first Schottky material layer 114 and the second Schottky material layer 116 receive different surface treatments, then the first Schottky material layer 114 and the second Schottky material layer 116 may also have different Schottky barrier heights). For example, the first Schottky material layer 114 may be surface treated to reduce its Schottky barrier height, and the second Schottky material layer 116 may be surface treated to increase its Schottky barrier height. In some non-limiting embodiments or aspects, the first Schottky material layer 114 and the second Schottky material layer 116 may include different materials and may receive different surface treatments.
[0073] In some non-limiting embodiments or aspects, the second Schottky material layer 116 can have a higher Schottky barrier height than the first Schottky material layer 114. For example, the first Schottky material layer 114 can include a lower Schottky barrier height material (LSBM), and the second Schottky material layer 116 can include a higher Schottky barrier height material (HSBM), as described herein. For example, the LSBM can have a Schottky barrier height of 1 electron volt (eV) or less, and the HSBM can have a Schottky barrier height of 1.2 eV or greater (e.g., 1.22 eV or greater).
[0074] In some non-limiting embodiments or aspects, the first Schottky material layer 114 may be on (eg, formed on top of, etc.) the second Schottky material layer 116, and the second Schottky material layer 116 may be at least partially in the first Schottky material layer 114 (eg, as Figure 1B ). For example, the second Schottky material layer 116 may include a plurality of segments, and each respective segment of the second Schottky material layer 116 may at least partially overlap a respective grid spacing region 111 of (one or more) grid spacing regions 111 defined between grid segments of the grid layer 110 (e.g., as shown in FIG. Figure 1B In some non-limiting embodiments or aspects, the width of each corresponding segment of the second Schottky material layer 116 may be greater than or equal to the width of the corresponding grid spacing region 111. Alternatively, the width of each corresponding segment of the second Schottky material layer 116 may be less than the width of the corresponding grid spacing region 111.
[0075] In some non-limiting embodiments or aspects, the second Schottky material layer 116 can be on (e.g., formed on top of) the first Schottky material layer 114, and the first Schottky material layer 114 can be at least partially in the second Schottky material layer 116 (e.g., as shown in FIG. Figure 1A For example, the first Schottky material layer 114 may include a plurality of segments, and each corresponding segment of the first Schottky material layer 114 may at least partially overlap a corresponding grid segment of the grid layer 110 (eg, as shown in FIG. Figure 1A ). In some non-limiting embodiments or aspects, the width of each corresponding segment of the first Schottky material layer 114 may be less than the width of the corresponding grid segment of the grid layer 110. Alternatively, the width of each corresponding segment of the first Schottky material layer 114 may be greater than or equal to the width of the corresponding grid segment of the grid layer 110.
[0076] In some non-limiting embodiments or aspects, at least one of the first Schottky material layer 114 or the second Schottky material layer 116 (e.g., whichever of the two layers is on the top) may include (e.g., may serve as) an anode. Additionally or alternatively, an additional layer of a metal material (not shown) may be deposited on the first Schottky material layer 114 or the second Schottky material layer 116 (e.g., whichever of the two layers is on the top) to serve as an anode. In some non-limiting embodiments or aspects, the buried gate double junction barrier Schottky diode 100 may include a cathode on the side of the drift layer 108 opposite to the anode. For example, the metallization layer 102 may include (e.g., may serve as) a cathode.
[0077] In some non-limiting embodiments or aspects, when a voltage greater than a threshold voltage (V TH ) (e.g., a positive voltage) (e.g., a voltage is applied in the forward direction), the buried gate double junction barrier Schottky diode 100 can be operated in a current conduction mode. Additionally or alternatively, when a voltage (e.g., a positive voltage) is applied from the cathode to the anode (e.g., a voltage is applied in the forward direction, a negative voltage is applied from the anode to the cathode, etc.), the buried gate double junction barrier Schottky diode 100 can be operated in a blocking mode (e.g., a voltage blocking mode).
[0078] Figure 1A and Figure 1B The number and arrangement of layers and / or elements are provided as examples. Figure 1A and Figure 1B There may be additional layers and / or elements, fewer layers and / or elements, different layers and / or elements, and / or differently arranged layers and / or elements than those shown in FIG. Figure 1A and Figure 1B Two or more layers and / or elements shown in the figure may be implemented in a single layer and / or element, or Figure 1A and Figure 1B The single layers and / or elements shown in the figure may be implemented as multiple layers and / or elements. Additionally or alternatively, the set of layers and / or the set of elements of the buried gate double junction barrier Schottky diode 100 may perform one or more functions described as being performed by another set of layers and / or another set of elements of the buried gate double junction barrier Schottky diode 100. Figure 1A and Figure 1B The doping of the materials and / or layers described is by way of example. There may be additional doping, less doping and / or different doping than those described above. For example, all n-type and / or n- + Type materials can be interchanged as p-type and / or p +For example, substrate layer 104 may be p-type and buffer layer 106 may be p-type. + type, the drift layer 108 may be of p-type, and the grid layer 110 may be of n-type and / or n + type, and / or the regrown layer 112 may be of p-type.
[0079] Reference now Figure 2 , Figure 2 is a flow chart of an exemplary process 200 for fabricating a buried-gate double-junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter. Figure 2 The number and arrangement of steps shown in are provided as examples. In some non-limiting embodiments or aspects, Figure 2 Process 200 may include additional steps, fewer steps, different steps, or a different arrangement of steps than those shown in FIG.
[0080] like Figure 2 As shown in , at step 204, process 200 may include forming and / or providing a substrate layer. For example, substrate layer 104 may be provided (e.g., may be previously fabricated) as a layer of semiconductor material (e.g., n-type semiconductor material) on which other layers of buried gate double junction barrier Schottky diode 100 may be formed. Additionally or alternatively, substrate layer 104 may be formed. For example, substrate layer 104 may be formed by forming a crystal of semiconductor material, cutting the crystal to form a wafer, and / or doping the crystal and / or wafer to form substrate layer 104.
[0081] In some non-limiting embodiments or aspects, the substrate layer 104 can be doped (e.g., lightly n-doped) after forming the substrate layer 104. Additionally or alternatively, the substrate layer 104 (and / or its materials) can be doped before and / or during providing and / or forming the substrate layer 104.
[0082] like Figure 2 As shown in FIG. 2 , at step 206, process 200 may include forming a buffer layer. For example, buffer layer 106 may be formed on one side (e.g., the top side, the side opposite to metallization layer 102, etc.) of substrate layer 104. In some non-limiting embodiments or aspects, forming buffer layer 106 may include depositing a semiconductor material (e.g., n + For example, the deposition may include adhering the buffer layer 106 to the substrate layer 104, fixing the buffer layer 106 to the substrate layer 104, forming the buffer layer 106 by epitaxy (e.g., epitaxial growth) on the substrate layer 104, any combination thereof, and the like.
[0083] In some non-limiting embodiments or aspects, the buffer layer 106 can be doped (e.g., highly n-doped) after forming the buffer layer 106. Additionally or alternatively, the buffer layer 106 (and / or its materials) can be doped before and / or during forming (e.g., depositing) the buffer layer 106.
[0084] like Figure 2 As shown in , at step 208, process 200 may include forming a drift layer. For example, drift layer 108 may be formed on one side (e.g., the top side, the side opposite to metallization layer 102, etc.) of buffer layer 106. In some non-limiting embodiments or aspects, forming drift layer 108 may include depositing a layer of semiconductor material (e.g., n-type semiconductor material) on one side of buffer layer 106. For example, depositing may include adhering drift layer 108 to buffer layer 106, fixing drift layer 108 to buffer layer 106, forming drift layer 108 by epitaxy (e.g., epitaxial growth) on buffer layer 106, any combination thereof, etc.
[0085] In some non-limiting embodiments or aspects, the drift layer 108 can be doped (e.g., lightly n-doped) after forming the drift layer 108. Additionally or alternatively, the drift layer 108 (and / or its materials) can be doped before and / or during forming (e.g., depositing) the drift layer 108.
[0086] like Figure 2 As shown in FIG. 2 , at step 210, process 200 may include forming a grid layer. For example, the grid layer 110 may be formed by patterning (e.g., by etching, stripping, etc.) the drift layer 108 to form a plurality of trenches and / or forming grid segments of the grid layer 110 in the trenches. In some non-limiting embodiments or aspects, forming the grid segments of the grid layer 110 may include depositing a semiconductor material (e.g., p-type and / or p-type) in the trenches of the drift layer 108. + type semiconductor material). For example, the deposition may include adhering the grid segments into the trenches, fixing the grid segments into the trenches, forming the grid segments by epitaxy (e.g., epitaxial growth) in the trenches, any combination thereof, etc. In some non-limiting embodiments or aspects, forming the grid layer 110 may include forming the grid segments of the grid layer 110 by implantation.
[0087] In some non-limiting embodiments or aspects, the grid segments of the grid layer 110 may be doped (e.g., lightly p-doped, highly p-doped, etc.) after forming the grid segments of the grid layer 110. Additionally or alternatively, the grid segments of the grid layer 110 (and / or its material) may be doped before and / or during forming (e.g., depositing) the grid segments of the grid layer 110.
[0088] like Figure 2As shown in , at step 212, the process 200 may include forming a regrown layer. For example, the regrown layer 112 may be formed on the drift layer 108 and / or the grid layer 110. In some non-limiting embodiments or aspects, forming the regrown layer 112 may include depositing a semiconductor material (e.g., an n-type semiconductor material) layer on top of the drift layer 108 and / or the grid layer 110. For example, the deposition may include adhering the regrown layer 112 to the drift layer 108 and / or the grid layer 110, fixing the regrown layer 112 to the drift layer 108 and / or the grid layer 110, forming the regrown layer 112 on the drift layer 108 and / or the grid layer 110 by epitaxy (e.g., epitaxial growth), any combination thereof, and the like.
[0089] In some non-limiting embodiments or aspects, the regrown layer 112 can be doped (e.g., lightly n-doped) after forming the regrown layer 112. Additionally or alternatively, the regrown layer 112 (and / or its materials) can be doped before and / or during forming (e.g., depositing) the regrown layer 112.
[0090] like Figure 2 As shown in , at step 214, process 200 may include forming a first Schottky material layer. For example, the first Schottky material layer 114 may be formed at least partially on (e.g., above, in contact with, etc.) the regrown layer 112 and / or at least partially overlapping (e.g., above, etc.) the grid segments of the grid layer 110. In some non-limiting embodiments or aspects, forming the first Schottky material layer 114 may include depositing a metal material and / or other conductive material layer on the regrown layer 112 (and / or the second Schottky material layer 116). For example, the deposition may include sputtering the first Schottky material layer 114 onto the regrown layer 112 (and / or the second Schottky material layer 116), depositing the first Schottky material layer 114 onto the regrown layer 112 (and / or the second Schottky material layer 116) by evaporation, adhering the first Schottky material layer 114 to the regrown layer 112 (and / or the second Schottky material layer 116), fixing the first Schottky material layer 114 to the regrown layer 112 (and / or the second Schottky material layer 116), forming the first Schottky material layer 114 on the regrown layer 112 (and / or the second Schottky material layer 116) by chemical vapor deposition (CVD), any combination thereof, and the like.
[0091] In some non-limiting embodiments or aspects, the first Schottky material layer 114 may be surface treated after forming the first Schottky material layer 114. Additionally or alternatively, the first Schottky material layer 114 (and / or its material) may be surface treated before and / or during forming (e.g., depositing) the first Schottky material layer 114.
[0092] In some non-limiting embodiments or aspects, forming the first Schottky material layer 114 may include forming an intermediate first Schottky material layer on the regrown layer 112 (e.g., depositing a metal material and / or other conductive material layer on the regrown layer 112). The intermediate first Schottky material layer may be patterned (e.g., by etching, stripping, etc.) to form a first Schottky material layer 114 that at least partially overlaps a grid segment of the grid layer 110 (e.g., to form a plurality of segments of the first Schottky material layer 114, each respective segment at least partially overlapping a respective grid segment of the grid layer 110). (For example, after forming the first Schottky material layer 114 by patterning the intermediate first Schottky material layer, a second Schottky material layer 116 may be formed on the first Schottky material layer 114 and / or the regrown layer 112.)
[0093] like Figure 2 As shown in , at step 216, process 200 may include forming a second Schottky material layer. For example, the second Schottky material layer 116 may be formed at least partially on (e.g., above, in contact with, etc.) the regrown layer 112 and / or at least partially overlapping (e.g., above, etc.) the grid spacing region 111. In some non-limiting embodiments or aspects, forming the second Schottky material layer 116 may include depositing a metal material and / or other conductive material layer on the regrown layer 112 (and / or the first Schottky material layer 114). For example, the deposition may include sputtering the second Schottky material layer 116 onto the regrown layer 112 (and / or the first Schottky material layer 114), depositing the second Schottky material layer 116 onto the regrown layer 112 (and / or the first Schottky material layer 114) by evaporation, adhering the second Schottky material layer 116 to the regrown layer 112 (and / or the first Schottky material layer 114), fixing the second Schottky material layer 116 to the regrown layer 112 (and / or the first Schottky material layer 114), forming the second Schottky material layer 116 on the regrown layer 112 (and / or the first Schottky material layer 114) by CVD, any combination thereof, and the like.
[0094] In some non-limiting embodiments or aspects, the second Schottky material layer 116 may be surface treated after forming the second Schottky material layer 116. Additionally or alternatively, the second Schottky material layer 116 (and / or its material) may be surface treated before and / or during forming (e.g., depositing) the second Schottky material layer 116.
[0095] In some non-limiting embodiments or aspects, forming the second Schottky material layer 116 may include forming an intermediate second Schottky material layer on the regrown layer 112 (e.g., depositing a metal material and / or other conductive material layer on the regrown layer 112). The intermediate second Schottky material layer may be patterned (e.g., by etching, stripping, etc.) to form a second Schottky material layer 116 that at least partially overlaps (one or more) grid spacing regions 111 (e.g., to form a plurality of segments of the second Schottky material layer 116, each respective segment at least partially overlapping a respective grid spacing region 111). (For example, after forming the second Schottky material layer 116 by patterning the intermediate second Schottky material layer, the first Schottky material layer 114 may be formed on the second Schottky material layer 116 and / or the regrown layer 112.)
[0096] In some non-limiting embodiments or aspects, step 216 may be performed before step 214 (e.g., the second Schottky material layer 116 may be formed first, and the first Schottky material layer 114 may be formed thereon). In some non-limiting embodiments or aspects, step 216 may be performed after step 214 (e.g., the first Schottky material layer 114 may be formed first, and the second Schottky material layer 116 may be formed thereon).
[0097] like Figure 2 As shown in , at step 218, process 200 may include forming a metallization layer. For example, metallization layer 102 may be formed on one side of substrate layer 104 (e.g., bottom side; opposite side from buffer layer 106, drift layer 108, grid layer 110, regrown layer 112, first Schottky material layer 114, and / or second Schottky material layer 116, etc.). For example, substrate layer 104 may be formed and / or provided (e.g., may have been previously fabricated) as described herein, and forming metallization layer 102 may include depositing a metal material and / or other conductive material layer on one side of substrate layer 104. For example, depositing may include sputtering metallization layer 102 onto substrate layer 104, depositing metallization layer 102 onto substrate layer 104 by evaporation, adhering metallization layer 102 to substrate layer 104, fixing metallization layer 102 to substrate layer 104, forming metallization layer 102 by CVD on substrate layer 104, any combination thereof, etc.
[0098] In some non-limiting embodiments or aspects, an ohmic contact (e.g., silicide) may be formed by depositing a thin layer of nickel (Ni) followed by annealing (e.g., thermal annealing, laser annealing, etc.) to form nickel silicide. Additionally or alternatively, a metal and / or conductive material (e.g., as described above) may be deposited on the nickel silicide layer to form the metallization layer 102.
[0099] In some non-limiting embodiments or aspects, step 218 can be performed after step 204 (e.g., substrate layer 104 can be formed and / or provided, and metallization layer 102 can be formed thereon). In some non-limiting embodiments or aspects, step 218 can be performed after step 212, step 214, and / or step 216, as described herein.
[0100] Reference now Figure 3A , Figure 3A is a diagram of an exemplary implementation 300a of a buried gate double junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter. Figure 3A As shown in , the embodiment 300a may include at least one of a drift layer 308, a grid layer 310, a grid spacing region 311, a regrown layer 312, a LSBM layer 314, and a HSBM layer 316, and / or any combination thereof. In some non-limiting embodiments or aspects, the embodiment 300a may be the same or similar to the buried gate double junction barrier Schottky diode 100. In some non-limiting embodiments or aspects, the drift layer 308 may be the same or similar to the drift layer 108. In some non-limiting embodiments or aspects, the grid layer 310 may be the same or similar to the grid layer 110. In some non-limiting embodiments or aspects, the grid spacing region 311 may be the same or similar to the grid spacing region 111. In some non-limiting embodiments or aspects, the regrown layer 312 may be the same or similar to the regrown layer 112. In some non-limiting embodiments or aspects, the LSBM layer 314 may be the same or similar to the first Schottky material layer 114. In some non-limiting embodiments or aspects, the HSBM layer 316 can be the same as or similar to the second Schottky material layer 116 . Figure 3A The number and arrangement of layers and / or elements in are provided as examples. Figure 3A There may be additional layers and / or elements, fewer layers and / or elements, different layers and / or elements, and / or differently arranged layers and / or elements than those shown in FIG. Figure 3A Two or more layers and / or elements shown in the figure may be implemented in a single layer and / or element, or Figure 3A The single layer and / or element shown in can be implemented as multiple layers and / or elements. Additionally or alternatively, the set of layers and / or the set of elements of embodiment 300a can perform one or more functions described as being performed by another set of layers and / or another set of elements of embodiment 300a. In some non-limiting embodiments or aspects, embodiment 300a can include at least one additional layer below drift layer 308, such as a metallization layer, a substrate layer, a buffer layer, any combination thereof, etc.
[0101] In some non-limiting embodiments or aspects, the LSBM layer 314 can be on (e.g., formed on top of, etc.) the HSBM layer 316, and the HSBM layer 316 can be at least partially in the LSBM layer 314, as described herein. For example, the HSBM layer 316 can include a plurality of segments, and each respective segment of the HSBM layer 316 can at least partially overlap a respective grid spacing region 311 of (one or more) grid spacing regions 311 defined between grid segments of the grid layer 310, as described herein. In some non-limiting embodiments or aspects, the width of each respective segment of the HSBM layer 316 can be greater than or equal to the width of the respective grid spacing region 311. Alternatively, the width of each respective segment of the HSBM layer 316 can be less than the width of the respective grid spacing region 311.
[0102] Reference now Figure 3B , Figure 3B is a diagram of an exemplary implementation 300b of a buried gate double junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter. Figure 3B As shown in , the embodiment 300b may include at least one of a drift layer 308, a grid layer 310, a grid spacing region 311, a regrown layer 312, a LSBM layer 314, and a HSBM layer 316, and / or any combination thereof. In some non-limiting embodiments or aspects, the embodiment 300b may be the same or similar to the buried gate double junction barrier Schottky diode 100. In some non-limiting embodiments or aspects, the drift layer 308 may be the same or similar to the drift layer 108. In some non-limiting embodiments or aspects, the grid layer 310 may be the same or similar to the grid layer 110. In some non-limiting embodiments or aspects, the grid spacing region 311 may be the same or similar to the grid spacing region 111. In some non-limiting embodiments or aspects, the regrown layer 312 may be the same or similar to the regrown layer 112. In some non-limiting embodiments or aspects, the LSBM layer 314 may be the same or similar to the first Schottky material layer 114. In some non-limiting embodiments or aspects, the HSBM layer 316 can be the same as or similar to the second Schottky material layer 116 . Figure 3B The number and arrangement of layers and / or elements in are provided as examples. Figure 3B There may be additional layers and / or elements, fewer layers and / or elements, different layers and / or elements, and / or differently arranged layers and / or elements than those shown in FIG. Figure 3B Two or more layers and / or elements shown in the figure may be implemented in a single layer and / or element, or Figure 3BThe single layer and / or element shown in can be implemented as multiple layers and / or elements. Additionally or alternatively, the set of layers and / or the set of elements of embodiment 300b can perform one or more functions described as being performed by another set of layers and / or another set of elements of embodiment 300b. In some non-limiting embodiments or aspects, embodiment 300b can include at least one additional layer below drift layer 308, such as a metallization layer, a substrate layer, a buffer layer, any combination thereof, etc.
[0103] In some non-limiting embodiments or aspects, the HSBM layer 316 can have a higher Schottky barrier height than the LSBM layer 314 , as described herein.
[0104] In some non-limiting embodiments or aspects, the HSBM layer 316 can be on (e.g., formed on top of, etc.) the LSBM layer 314, and the LSBM layer 314 can be at least partially in the HSBM layer 316, as described herein. For example, the LSBM layer 314 can include a plurality of segments, and each respective segment of the LSBM layer 314 can at least partially overlap a respective grid segment of the grid layer 310, as described herein. In some non-limiting embodiments or aspects, the width of each respective segment of the LSBM layer 314 can be less than the width of the respective grid segment of the grid layer 310. Alternatively, the width of each respective segment of the LSBM layer 314 can be greater than or equal to the width of the respective grid segment of the grid layer 310.
[0105] Continue to refer Figure 3A and Figure 3B , the embodiment 300a and / or the embodiment 300b can be realized by lowering the threshold voltage (V TH ), improving (e.g., reducing) the on-resistance, and maintaining and / or improving the voltage blocking capability to improve the performance of the diode (e.g., compared to a diode having a single Schottky material layer). For example, embodiment 300a and / or embodiment 300b may include a semiconductor material layer of silicon carbide (SiC) and a buried gate (BG) junction barrier Schottky (JBS) structure having a double Schottky contact material. In some non-limiting embodiments or aspects, the LSBM may be implemented (at least partially) above the grid segments of the grid layer 310 to reduce the threshold voltage (V TH ) and / or HSBM can be (at least partially) implemented above (one or more) grid spacing regions 311 to maintain and / or improve blocking voltage (e.g., maintain and / or increase blocking voltage) and leakage current (e.g., maintain and / or reduce leakage current).
[0106] In some non-limiting embodiments or aspects, one or more suitable Schottky materials (e.g., titanium or a compound including titanium) may be used to form a potential barrier at the surface of the SiC layer (e.g., the regrown layer 312, the grid layer 310, and / or the drift layer 308), and this may result in a low forward voltage drop (V F ) and low leakage current. In addition, the thin regrown layer 312 between the grid layer 310 and the Schottky material(s) can shield the Schottky contact area from high electric fields in blocking mode, which can result in reduced leakage current.
[0107] In some non-limiting embodiments or aspects, having two different Schottky material layers (e.g., LSBM layer 314 and HSBM layer 316) on the regrown layer 312 can reduce on-resistance and / or conduction losses. For example, the LSBM layer 314 can be implemented (at least partially) at a region above the grid segments of the grid layer 310, and the HSBM layer 316 can be implemented (at least partially) at a region above the grid spacing region 311. In the blocking mode, the HSBM layer 316 can maintain and / or improve the leakage current (e.g., reduce the leakage current) and the breakdown voltage (e.g., increase the breakdown voltage). In the current conduction mode, the LSBM layer 314 can start conducting earlier (e.g., at a lower voltage), resulting in a lower threshold voltage (V TH ), lower forward voltage drop (V F ) and lower conduction losses (e.g., especially under light load conditions).
[0108] Reference now Figure 4 , Figure 4 is a graph of normalized electric field (eg, in blocking mode) of an exemplary implementation 400 of a buried gate double junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter. Figure 4As shown in , embodiment 400 may include a drift layer 408, a grid layer 410, a grid spacing region 411, a regrown layer 412, a LSBM layer 414, and a HSBM layer 416. In some non-limiting embodiments or aspects, embodiment 400 may be the same or similar to buried gate double junction barrier Schottky diode 100, embodiment 300a, and / or embodiment 300b. In some non-limiting embodiments or aspects, drift layer 408 may be the same or similar to drift layer 108 and / or drift layer 308. In some non-limiting embodiments or aspects, grid layer 410 may be the same or similar to grid layer 110 and / or grid layer 310. In some non-limiting embodiments or aspects, grid spacing region 411 may be the same or similar to grid spacing region 111 and / or grid spacing region 311. In some non-limiting embodiments or aspects, the regrown layer 412 may be the same as or similar to the regrown layer 112 and / or the regrown layer 312. In some non-limiting embodiments or aspects, the LSBM layer 414 may be the same as or similar to the first Schottky material layer 114 and / or the LSBM layer 314. In some non-limiting embodiments or aspects, the HSBM layer 416 may be the same as or similar to the second Schottky material layer 116 and / or the HSBM layer 316. Figure 4 The number and arrangement of layers and / or elements in are provided as examples. Figure 4 There may be additional layers and / or elements, fewer layers and / or elements, different layers and / or elements, and / or differently arranged layers and / or elements than those shown in FIG. Figure 4 Two or more layers and / or elements shown in the figure may be implemented in a single layer and / or element, or Figure 4 The single layer and / or element shown in can be implemented as multiple layers and / or elements. Additionally or alternatively, the set of layers and / or the set of elements of embodiment 400 can perform one or more functions described as being performed by another set of layers and / or another set of elements of embodiment 400. In some non-limiting embodiments or aspects, embodiment 400 can include at least one additional layer below drift layer 408, such as a metallization layer, a substrate layer, a buffer layer, any combination thereof, etc.
[0109] like Figure 4 As shown in FIG. 4 , in the blocking mode, a higher electric field exists below the grid segments of the grid layer 410 than above. This may demonstrate that the LSBM layer 414 above the grid layer 410 may not affect the blocking capability of the diode (e.g., despite the inclusion of the LSBM layer 314, the HSBM layer 316 still allows the diode to maintain blocking capability, even though a material with a lower Schottky barrier height might otherwise be expected to have reduced blocking capability).
[0110] For purposes of illustration and not limitation, Figure 4As shown in , the electric field can be lowest in the grid layer 410 and relatively low in the portion of the regrown layer 412 located above the grid layer 410 and below the LSBM layer 314. The electric field can be relatively high in the portion of the regrown layer 412 located above the grid spacing region 411 and below the HSBM layer 416. The electric field can be even higher in the grid spacing region 411 and the portion of the drift layer 408 located below the grid spacing region 411. The electric field can be highest in the portion of the drift layer 408 located below the grid layer 410. In some non-limiting embodiments or aspects, the electric field can be absent in the LSBM layer 414 and / or the HSBM layer 416.
[0111] Reference now Figure 5A , Figure 5A Graph 500a shows reverse current density and voltage for an exemplary implementation of a buried gate double junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter. Figure 5A As shown in FIG. 5 , the graph 500 a may include a vertical axis of current density (J) (e.g., in amperes per square centimeter (A / cm 2 ) in units) and a horizontal axis of voltage (e.g., in volts (V)). In addition, the vertical axis may include a logarithmic scale.
[0112] like Figure 5A As shown in , the first curve 501a can represent a buried gate junction barrier Schottky diode with a single Schottky material layer, and the second curve 502a can represent a buried gate double junction barrier Schottky diode as described herein (e.g., with two Schottky material layers, the two Schottky material layers having different Schottky barrier heights). At or above the rated voltage, the second curve 502a can exhibit the same or lower reverse current density (e.g., the same or reduced leakage current) compared to the first curve 501a. Even at a lower voltage, the second curve 502a can also exhibit a comparable reverse current density (e.g., maintaining leakage current) compared to the first curve 501a.
[0113] Reference now Figure 5B , Figure 5B Graph 500b shows forward current density and voltage for an exemplary implementation of a buried gate double junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter. Figure 5B As shown in FIG. 5 , graph 500 b may include a vertical axis of current density (J) (e.g., in amperes per square centimeter (A / cm 2 ) in units of ) and a horizontal axis of voltage (for example, in volts (V)).
[0114] like Figure 5BAs shown in FIG. 5 , the first curve 501b may represent a buried gate junction barrier Schottky diode having a single Schottky material layer, and the second curve 502b may represent a buried gate double junction barrier Schottky diode as described herein (e.g., having two Schottky material layers, the two Schottky material layers having different Schottky barrier heights). The second curve 502b may exhibit a lower threshold voltage (V TH ). In addition, at the rated current density, the second curve 502b may exhibit a lower forward voltage drop (V F ).
[0115] In some non-limiting embodiments or aspects, the buried gate double junction barrier Schottky diodes described herein can reduce the area (and / or production cost) compared to diodes with a single Schottky material layer and still have the same forward voltage drop (V F ).
[0116] Reference now Figure 6 , Figure 6 1 and 2 show a ratio (W) of a width of a first Schottky material layer to a width of a grid segment of an exemplary implementation of a buried-gate double-junction barrier Schottky diode according to some non-limiting embodiments or aspects of the presently disclosed subject matter. LSBM / W Grid ), forward voltage drop (V F ) and leakage current (I R ) is a graph 600. Figure 6 As shown in FIG. 6 , the graph 600 may include a forward voltage drop (V F ) (e.g., in volts (V)), the leakage current at rated voltage (I R ) (eg, in amperes (A)) and a ratio (W) of the width of the first Schottky material layer (eg, LSBM layer) to the width of the grid segment. LSBM / W Grid ). Figure 6 As shown in , the left vertical axis may include a linear scale and the right vertical axis may include a logarithmic scale.
[0117] like Figure 6 As shown in FIG. 6 , a first curve 601 may represent a forward voltage drop (V ) of a buried gate double junction barrier Schottky diode (e.g., having two Schottky material layers with different Schottky barrier heights (e.g., LSBM is 1 eV and HSBM is 1.22 eV)). F ) and the second curve 602 may represent the leakage current (I R ), as described in this article. Figure 6 As shown in the figure, the forward voltage drop (VF ) and leakage current (I R ), depending on the width of the LSBM layer fragments compared to the width of the grid layer fragments (e.g., the ratio W LSBM / W Grid For example, increasing the width of the LSBM layer can reduce the forward voltage drop (V F ), but may increase the leakage current (I R Reducing the width of the LSBM layer may increase the forward voltage drop (V F ), but can reduce the leakage current (I R ).
[0118] In some non-limiting embodiments or aspects, the width of the LSBM layer (eg, relative to the width of the grid segment) can be based on a target forward voltage drop (V F ), target leakage current (I R ), any combination thereof, etc. Additionally or alternatively, the target forward voltage drop (V F ), target leakage current (I R ), any combination thereof, etc. to adjust the Schottky barrier height of at least one of the LSBM layer and / or the HSBM layer (e.g., by selecting different materials and / or by applying different surface treatments) (e.g., and the width of the LSBM can remain the same).
[0119] In some non-limiting embodiments or aspects, the second Schottky material layer (eg, HSBM layer) may cover all areas (eg, of the regrown layer) not covered by the segments of the first Schottky material layer (eg, LSBM layer).
[0120] Although the disclosed subject matter has been described in detail for purposes of illustration based on what are presently considered to be the most practical and preferred embodiments or aspects, it should be understood that such details are provided for that purpose only and that the disclosed subject matter is not limited to the disclosed embodiments or aspects, but rather is intended to cover modifications and equivalent arrangements within the spirit and scope of the appended claims. For example, it should be understood that the presently disclosed subject matter contemplates that, to the extent possible, one or more features of any embodiment or aspect may be combined with one or more features of any other embodiment or aspect.
Claims
1. A buried-gate double-junction barrier Schottky diode, comprising: drift layer; a grid layer comprising a plurality of grid segments at least partially in the drift layer, the plurality of grid segments defining at least one grid spacing region between adjacent grid segments of the plurality of grid segments; a regrown layer on the grid layer and the drift layer; a first Schottky material layer at least partially on the regrown layer and at least partially overlapping the plurality of grid segments of the grid layer; as well as A second Schottky material layer is at least partially on the regrown layer and at least partially overlaps the at least one grid spacing region, the second Schottky material layer having a different Schottky barrier height from the first Schottky material layer.
2. The buried-gate double-junction barrier Schottky diode according to claim 1, further comprising: Substrate layer, Wherein, the substrate layer is below the drift layer.
3. The buried-gate double-junction barrier Schottky diode according to claim 2, further comprising: Metallization layer, Wherein, the substrate layer is on the metallization layer.
4. The buried-gate double-junction barrier Schottky diode according to claim 2, further comprising: a buffer layer on the substrate layer, Wherein, the drift layer is on the buffer layer.
5. The buried-gate double-junction barrier Schottky diode according to claim 1, wherein: A top surface of the grid layer is within a plane, a top surface of the drift layer is within the plane, and the regrown layer is on the top surface of the grid layer and the top surface of the drift layer.
6. The buried-gate double-junction barrier Schottky diode according to claim 1, wherein: The second Schottky material layer has a higher Schottky barrier height than the first Schottky material layer.
7. The buried-gate double-junction barrier Schottky diode according to claim 1, wherein: The first Schottky material layer is on the second Schottky material layer, and the second Schottky material layer is at least partially in the first Schottky material layer.
8. The buried-gate double-junction barrier Schottky diode according to claim 1, wherein: The second Schottky material layer is on the first Schottky material layer, and the first Schottky material layer is at least partially in the second Schottky material layer.
9. The buried-gate double-junction barrier Schottky diode according to claim 1, wherein: At least one of the first Schottky material layer or the second Schottky material layer includes an anode, and the buried-gate double-junction barrier Schottky diode further includes: A cathode is on a side of the drift layer opposite the anode.
10. The buried-gate double-junction barrier Schottky diode according to claim 9, wherein: When a positive voltage greater than a threshold voltage is applied from the anode to the cathode, the buried gate double junction barrier Schottky diode operates in a current conduction mode, and Wherein, when a negative voltage is applied from the anode to the cathode, the buried-gate double-junction barrier Schottky diode operates in a voltage blocking mode.
11. The buried-gate double-junction barrier Schottky diode according to claim 1 , further comprising: an anode, at least partially on at least one of the first Schottky material layer or the second Schottky material layer; as well as A cathode is located on a side of the drift layer opposite to the anode.
12. The buried gate double junction barrier Schottky diode according to claim 1, wherein: The first Schottky material layer includes a plurality of segments, and each respective segment of the first Schottky material layer at least partially overlaps a respective grid segment of the plurality of grid segments of the grid layer.
13. The buried gate double junction barrier Schottky diode according to claim 12, wherein: A width of each corresponding segment of the first Schottky material layer is smaller than a width of a corresponding grid segment of the plurality of grid segments of the grid layer.
14. The buried-gate double-junction barrier Schottky diode according to claim 12, wherein: A width of each corresponding segment of the first Schottky material layer is greater than or equal to a width of a corresponding grid segment of the plurality of grid segments of the grid layer.
15. The buried gate double junction barrier Schottky diode according to claim 1, wherein: The at least one grid pitch region includes a plurality of grid pitch regions, and wherein the second Schottky material layer includes a plurality of segments, each respective segment of the second Schottky material layer at least partially overlaps a respective grid pitch region of the plurality of grid pitch regions.
16. The buried gate double junction barrier Schottky diode according to claim 15, wherein: One of the following: The width of each corresponding segment of the second Schottky material layer is smaller than the width of a corresponding grid spacing region of the plurality of grid spacing regions, or A width of each corresponding segment of the second Schottky material layer is greater than or equal to a width of a corresponding grid spacing region of the plurality of grid spacing regions.
17. A method for manufacturing a buried-gate double-junction barrier Schottky diode, comprising: Formation of drift layer; forming a grid layer comprising a plurality of grid segments at least partially in the drift layer, the plurality of grid segments defining at least one grid spacing region between adjacent grid segments of the plurality of grid segments; forming a regrown layer on the grid layer and the drift layer; forming a first Schottky material layer at least partially on the regrown layer and at least partially overlapping the plurality of grid segments of the grid layer; as well as A second Schottky material layer is formed at least partially on the regrown layer and at least partially overlapping the at least one grid pitch region, the second Schottky material layer having a different Schottky barrier height than the first Schottky material layer.
18. The method according to claim 17, further comprising: providing a substrate layer; as well as A buffer layer is formed on the substrate layer, wherein forming the drift layer includes forming the drift layer on the buffer layer.
19. The method according to claim 18, wherein: Forming the first Schottky material layer includes: forming an intermediate first Schottky material layer on the regrown layer; and patterning the intermediate first Schottky material layer to form the first Schottky material layer at least partially overlapping the plurality of grid segments of the grid layer, Wherein, forming the second Schottky material layer includes forming the second Schottky material layer on the first Schottky material layer.
20. The method according to claim 18, wherein: Forming the second Schottky material layer includes: forming an intermediate second Schottky material layer on the regrown layer; and patterning the intermediate second Schottky material layer to form the second Schottky material layer at least partially overlapping the at least one grid spacing region, Wherein, forming the first Schottky material layer includes forming the first Schottky material layer on the second Schottky material layer.