Round tube blade one-time forming die and forming method
By designing a one-time molding mold for circular tube blades that includes a driving rod and a wedge forming block, the problems of cumbersome molding steps and inconsistent angles in the existing technology are solved, and efficient and high-quality blade molding is achieved.
Patent Information
- Application Number
- CN202411003132.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-10-25
Smart Images

Figure CN118832050A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of blade molding, and in particular to a one-step molding die and a molding method for a circular tube blade. Background Art
[0002] like Figure 1 The shorter round tube-shaped part shown in the figure has a plurality of blades 200 evenly distributed on the circumferential surface of the round tube part 100. Here, 12 blades 200 are taken as an example. In view of the molding requirements of the round tube part 100, the conventional blade molding mold, such as Figure 2 , including an upper forming block 1' and a lower forming block 2', the upper forming block 1' is provided with a convex block 3', and the lower forming block 2' is provided with a concave cavity 4' corresponding to the convex block 3'. During processing, the round tube part 100 is sandwiched between the upper forming block 1' and the lower forming block 2', and the convex block 3' cooperates with the concave cavity 4' to realize the forming of the blade 200.
[0003] It can be seen that the above-mentioned blade forming mold can only form about three blades 200 at a time. After forming once, the blades 200 need to be rotated and formed again. A round tube part 100 needs to be formed four times, resulting in too many processing steps, too long production cycle time, and extremely inconvenient operation. In addition, the angle consistency of the blades 200 formed in batches is poor, which affects the performance of the entire product. Summary of the invention
[0004] Based on the above problems, one object of the present invention is to provide a one-time forming mold for round tube blades to solve the problems of complicated processing, low efficiency and poor forming quality of existing forming molds.
[0005] Another object of the present invention is to provide a one-time forming method for circular tube blades, which completes the forming of all blades through a single stamping and ensures that the angles of each blade after forming are consistent.
[0006] To achieve the above object, on the one hand, the present invention adopts the following technical solutions:
[0007] A one-time forming mold for round tube blades comprises an upper mold plate and a lower mold plate, wherein a driving rod is arranged on the upper mold plate, and a forming die and a forming punch are arranged on the lower mold plate, wherein the forming punch is inserted into the mold cavity of the forming die, and the round tube part to be processed is placed between the forming die and the forming punch, and the forming punch is composed of a plurality of fan-shaped wedge forming blocks, wherein the driving rod is inserted into the forming punch, and the driving rod cooperates with the inner surface of each wedge forming block, so that the axial movement of the driving rod is converted into the radial movement of each wedge forming block, and the outer surface of each wedge forming block is provided with a forming protrusion, and the forming protrusion is used to apply pressure to the tube wall of the round tube part when the wedge forming block moves radially outward.
[0008] Optionally, a guide seat is fixed on the lower template, a pressure plate is fixed on the upper surface of the guide seat, a cavity is formed between the guide seat and the pressure plate, the forming die is fixed on the upper surface of the pressure plate, the lower end of the forming punch extends into the cavity, and a flange edge is provided at the bottom of each inclined wedge forming block, the flange edge is limited by the cavity, so that each inclined wedge forming block can only move horizontally between the guide seat and the pressure plate.
[0009] Optionally, a return spring is provided between the flange edge of each oblique wedge forming block and the side wall of the cavity, and the return spring applies a radially inward force to the oblique wedge forming block.
[0010] Optionally, the upper end hoop of the forming punch is provided with a tightening ring, and the top of each inclined wedge forming block is provided with a groove for limiting the tightening ring, and the tightening ring applies a radially inward force to each inclined wedge forming block.
[0011] Optionally, a diverter block is provided on the bottom surface of each inclined wedge forming block, and a guide groove for radially limiting each diverter block is provided on the guide seat.
[0012] Optionally, a positioning step is provided on the outer surface of each inclined wedge forming block and below the forming protrusion, and the positioning step is used to support the lower end of the round tube part.
[0013] Optionally, a raising block is provided on the lower template, a first limiting column is provided on the raising block, and a second limiting column vertically aligned with the first limiting column is provided on the lower surface of the upper template. When the first limiting column abuts against the second limiting column, the downward stroke of the driving rod is limited.
[0014] Optionally, a guide column is arranged on one of the raising block and the upper template, and a guide sleeve cooperating with the guide column is arranged on the other of the raising block and the upper template.
[0015] In summary, compared with the prior art, the one-time forming mold for round tube blades is suitable for the one-time forming of all blades on round tube parts, and ensures the consistency of the angles of each blade. The mold has a simple structure, low cost, easy operation, high processing efficiency and good forming quality.
[0016] On the other hand, the present invention adopts the following technical solutions:
[0017] A one-step forming method for a circular tube blade, based on the above-mentioned one-step forming mold for a circular tube blade, comprises the following steps:
[0018] Step 1: The driving rod is completely separated from the forming punch, each wedge forming block is retracted inward, and the round tube part to be processed is placed between the forming die and the forming punch;
[0019] Step 2: The driving rod moves downward along with the upper template. The driving rod inserts into the forming punch, and through the cooperation of the inclined wedge, each inclined wedge forming block moves radially outward, and the forming convex block presses on the pipe wall of the circular pipe part, starting to form the blade by turning it outwards.
[0020] Step 3: When the downward movement of the driving rod ends, the forming of the blade ends.
[0021] Step 4: The driving rod moves upward along with the upper template. The driving rod completely disengages from the forming punch, and each inclined wedge forming block retracts inwards, and the formed circular pipe part is taken out.
[0022] Optionally, before Step 1, a cut groove in the shape of "匚" is pre-punched on the pipe wall of the circular pipe part, and the area cut out by the cut groove is correspondingly pressed by the forming convex block.
[0023] In summary, compared with the prior art, this one-step forming method for circular pipe blades can improve the production rhythm of forming blades on circular pipe parts, ensure the consistency of the forming angle of the blades, and reduce the processing difficulty and production cost. Description of the Drawings
[0024] In order to more clearly illustrate and understand the technical solutions in the embodiments of the present invention, the following will briefly introduce the drawings required for the background art and the description of the embodiments of the present invention. Obviously, the drawings described below are only some embodiments of the present invention. For those of ordinary skill in the art, without creative efforts, other drawings can also be obtained based on the content of the embodiments of the present invention and these drawings.
[0025] Figure 1 It is a schematic diagram of the formed circular pipe part provided by the embodiment of the present invention;
[0026] Figure 2 It is a schematic structural diagram of the existing blade forming die;
[0027] Figure 3 It is a schematic structural diagram of the one-step forming die for circular pipe blades provided by the embodiment of the present invention;
[0028] Figure 4 It is a top view of the forming punch in the one-step forming die for circular pipe blades provided by the embodiment of the present invention;
[0029] Figure 5 It is a schematic diagram of the circular pipe part before forming provided by the embodiment of the present invention.
[0030] In the figure:
[0031] 1', upper forming block; 2', lower forming block; 3', convex block; 4', concave cavity;
[0032] 100, circular pipe part; 200, blade; 300, cut groove;
[0033] 1. Upper template; 2. Lower template; 3. Driving rod; 4. Forming die; 5. Wedge forming block; 6. Forming convex block; 7. Guide seat; 8. Press plate; 9. Cavity; 10. Flange edge; 11. Return spring; 12. Tightening ring; 13. Groove; 14. Diverter block; 15. Positioning step; 16. Heightening block; 17. First limiting column; 18. Second limiting column; 19. Guide column; 20. Guide sleeve. DETAILED DESCRIPTION
[0034] In order to make the technical problems solved by the present invention, the technical solutions adopted and the technical effects achieved clearer, the technical solutions of the embodiments of the present invention will be further described in detail below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.
[0035] See also Figure 3 to Figure 4 As shown, the preferred embodiment provides a one-time forming mold for circular tube blades, including an upper template 1 and a lower template 2, a driving rod 3 is provided on the upper template 1, a forming die 4 and a forming punch are provided on the lower template 2, the forming punch is inserted into the mold cavity of the forming die 4, the circular tube part 100 to be processed is placed between the forming die 4 and the forming punch, the forming punch is composed of a plurality of fan-shaped wedge forming blocks 5, the driving rod 3 is inserted into the forming punch, and the driving rod 3 is wedge-matched with the inner surface of each wedge forming block 5, so that the axial movement of the driving rod 3 is converted into the radial movement of each wedge forming block 5, and the outer surface of each wedge forming block 5 is provided with a forming protrusion 6, and the forming protrusion 6 is used to apply pressure to the tube wall of the circular tube part 100 when the wedge forming block 5 moves radially outward. Figure 4 The direction of the dashed arrow is the direction in which the wedge forming block 5 moves radially outward.
[0036] Therefore, the one-time forming mold for round tube blades is suitable for one-time forming of all blades 200 on the round tube part 100, and ensures the consistency of the angles of each blade 200. The mold has a simple structure, low cost, convenient operation, high processing efficiency, and good forming quality. In addition, considering that the round tube part 100 should be easily loaded into the mold, it is more suitable for processing and using shorter round tube parts.
[0037] As an optional solution, a guide seat 7 is fixed on the lower template 2, a pressure plate 8 is fixed on the upper surface of the guide seat 7, a cavity 9 is formed between the guide seat 7 and the pressure plate 8, the forming die 4 is fixed on the upper surface of the pressure plate 8, the lower end of the forming punch extends into the cavity 9, and a flange edge 10 is provided at the bottom of each inclined wedge forming block 5, and the flange edge 10 is limited by the cavity 9, so that each inclined wedge forming block 5 can only move horizontally between the guide seat 7 and the pressure plate 8.
[0038] In particular, a return spring 11 is arranged between the flange edge 10 of each inclined wedge forming block 5 and the side wall of the cavity 9. The return spring 11 applies a radial inward force to the inclined wedge forming block 5 so that when the driving rod 3 moves upward and exits the forming punch, each inclined wedge forming block 5 automatically retracts inward to facilitate the loading and unloading of the round tube part 100.
[0039] In particular, a tightening ring 12 is provided at the upper end hoop of the forming punch, and a groove 13 for limiting the tightening ring 12 is provided at the top of each inclined wedge forming block 5. The tightening ring 12 applies a radial inward force to each inclined wedge forming block 5, so that when the driving rod 3 moves upward and exits the forming punch, each inclined wedge forming block 5 automatically retracts inward to facilitate the loading and unloading of the round tube part 100.
[0040] Furthermore, a diverter block 14 is disposed on the bottom surface of each inclined wedge forming block 5 , and a guide groove for radially limiting each diverter block 14 is disposed on the guide seat 7 , thereby ensuring accurate radial reciprocating movement of each inclined wedge forming block 5 .
[0041] As an optional solution, a positioning step 15 is provided on the outer surface of each wedge forming block 5 and below the forming protrusion 6 , and the positioning step 15 is used to support the lower end of the circular tube part 100 so as to determine the axial position of the blade 200 on the circular tube part 100 .
[0042] Furthermore, the positioning step 15 is connected to the flange edge 10 by an arc surface. Even if the lower end of the round tube part 100 slides onto the flange edge 10 when the inclined wedge forming block 5 is retracted, as the inclined wedge forming block 5 moves radially outward, the lower end of the round tube part 100 will return to the positioning step 15 along the arc surface.
[0043] As an optional solution, a padding block 16 is provided on the lower template 2, and a first limiting column 17 is provided on the padding block 16. A second limiting column 18 vertically aligned with the first limiting column 17 is provided on the lower surface of the upper template 1. When the first limiting column 17 abuts against the second limiting column 18, the downward stroke of the driving rod 3 is limited. Specifically, the four corners of the circular tube blade one-time molding mold are respectively provided with the first limiting column 17 and the second limiting column 18. When the first limiting column 17 contacts the second limiting column 18, the downward movement of the driving rod 3 ends, thereby preventing the molding protrusion 6 from applying excessive pressure to the tube wall of the circular tube part 100, and ensuring the molding quality of the blade 200.
[0044] Further, a guide post 19 is provided on one of the spacer block 16 and the upper template 1, and a guide sleeve 20 that cooperates with the guide post 19 is provided on the other of the spacer block 16 and the upper template 1. Specifically, the guide post 19 and the guide sleeve 20 are respectively provided on both sides of the one-time forming die for the circular tube blade, so as to ensure the accurate mold closing and mold opening actions of the upper template 1 relative to the lower template 2, and further ensure the accurate axial movement of the driving rod 3.
[0045] It should be noted that among the above various optional embodiments, they can be combined in any combination manner, and the combined embodiments all fall within the protection scope of the present invention.
[0046] Based on the above one-time forming die for the circular tube blade, this embodiment further provides a one-time forming method for the circular tube blade, which includes the following steps:
[0047] Step 1: Completely separate the driving rod 3 from the forming punch, and each wedge-shaped forming block 5 retracts inwardly. The circular tube part 100 to be processed is placed between the forming die 4 and the forming punch.
[0048] Step 2: The driving rod 3 moves downward along with the upper template 1. The driving rod 3 is inserted into the forming punch. Through the wedge cooperation, each wedge-shaped forming block 5 moves radially outward, and the forming convex block 6 presses on the tube wall of the circular tube part 100, and the blade 200 starts to be formed by outward turning.
[0049] Step 3: When the downward movement of the driving rod 3 ends, the forming of the blade 200 ends. Specifically, this is because the first limit post 17 contacts the second limit post 18.
[0050] Step 4: The driving rod 3 moves upward along with the upper template 1. The driving rod 3 completely separates from the forming punch, and each wedge-shaped forming block 5 retracts inwardly, and the formed circular tube part 100 is taken out.
[0051] Particularly, before Step 1, a cut groove 300 in a "C" shape is pre-punched on the tube wall of the circular tube part 100, and the area cut out by the cut groove 300 is correspondingly pressed by the forming convex block 6 so as to facilitate the forming of the blade 200. For details, see Figure 5 .
[0052] Thus, this one-time forming method for the circular tube blade can improve the production rhythm of forming the blade 200 on the circular tube part 100, ensure the consistency of the forming angle of the blade 200, and reduce the processing difficulty and production cost.
[0053] It can be seen that the one-time forming die and the forming method for the circular tube blade have the following advantages:
[0054] 1) All blades are formed in one mold closing, which improves the production rhythm and significantly improves the processing efficiency;
[0055] 2) The molding angles of each blade are consistent, and product quality is guaranteed;
[0056] 3) Simple structure, easy operation, suitable for blade forming similar to most short round tubes;
[0057] 4) The mold manufacturing and maintenance are convenient and the cost is low.
[0058] The above embodiments are only to illustrate the basic principles and characteristics of the present invention. The present invention is not limited by the above embodiments. Without departing from the spirit and scope of the present invention, the present invention may be subjected to various changes and modifications, which are within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. A one-step forming die for round tube blades, characterized in that: The invention comprises an upper mold plate (1) and a lower mold plate (2), wherein a driving rod (3) is arranged on the upper mold plate (1), and a forming die (4) and a forming punch are arranged on the lower mold plate (2), wherein the forming punch is inserted into the mold cavity of the forming die (4), and a round tube part (100) to be processed is placed between the forming die (4) and the forming punch, wherein the forming punch is composed of a plurality of fan-shaped wedge forming blocks (5), wherein the driving rod (3) is inserted into the forming punch, and the driving rod (3) is wedge-matched with the inner surface of each of the wedge forming blocks (5), so that the axial movement of the driving rod (3) is converted into the radial movement of each of the wedge forming blocks (5), and the outer surface of each of the wedge forming blocks (5) is provided with a forming protrusion (6), wherein the forming protrusion (6) is used to apply pressure to the tube wall of the round tube part (100) when the wedge forming block (5) moves radially outward.
2. The one-step forming die for round tube blades according to claim 1, characterized in that: A guide seat (7) is fixed on the lower template (2), a pressure plate (8) is fixed on the upper surface of the guide seat (7), a cavity (9) is formed between the guide seat (7) and the pressure plate (8), the forming die (4) is fixed on the upper surface of the pressure plate (8), the lower end of the forming punch extends into the cavity (9), and a flange edge (10) is provided at the bottom of each of the inclined wedge forming blocks (5), and the flange edge (10) is limited by the cavity (9), so that each of the inclined wedge forming blocks (5) can only move horizontally between the guide seat (7) and the pressure plate (8).
3. The one-step forming die for round tube blades according to claim 2, characterized in that: A return spring (11) is provided between the flange edge (10) of each of the inclined wedge forming blocks (5) and the side wall of the cavity (9), and the return spring (11) applies a radially inward force to the inclined wedge forming block (5).
4. The one-step forming die for round tube blades according to claim 2, characterized in that: The upper end hoop of the forming punch is provided with a tightening ring (12), and the top of each of the inclined wedge forming blocks (5) is provided with a groove (13) for limiting the tightening ring (12), and the tightening ring (12) applies a radial inward force to each of the inclined wedge forming blocks (5).
5. The one-step forming die for round tube blades according to claim 2, characterized in that: The bottom surface of each of the inclined wedge forming blocks (5) is provided with a diverter block (14), and the guide seat (7) is provided with a guide groove for radially limiting each of the diverter blocks (14).
6. The one-step forming die for round tube blades according to claim 1, characterized in that: A positioning step (15) is provided on the outer surface of each of the inclined wedge forming blocks (5) and below the forming protrusion (6), and the positioning step (15) is used to support the lower end of the circular tube part (100).
7. The one-step forming die for round tube blades according to claim 1, characterized in that: The lower template (2) is provided with a raising block (16), and the raising block (16) is provided with a first limiting column (17). The lower surface of the upper template (1) is provided with a second limiting column (18) vertically aligned with the first limiting column (17). When the first limiting column (17) abuts against the second limiting column (18), the downward stroke of the driving rod (3) is limited.
8. The one-step forming die for round tube blades according to claim 7, characterized in that: A guide post (19) is provided on one of the shim block (16) and the upper template (1), and a guide sleeve (20) cooperating with the guide post (19) is provided on the other of the shim block (16) and the upper template (1).
9. A one-step forming method for a circular tube blade, based on the one-step forming mold for a circular tube blade according to any one of claims 1 to 8, characterized in that: It includes the steps of: Step 1: Completely separate the driving rod (3) from the forming punch, and each of the wedge forming blocks (5) retracts inwardly. The pipe part (100) to be processed is placed between the forming die (4) and the forming punch. Step 2: The driving rod (3) moves downward along with the upper template (1), the driving rod (3) is inserted into the forming punch, and each of the wedge forming blocks (5) moves radially outward through wedge cooperation. The forming convex block (6) presses on the pipe wall of the pipe part (100), and the blade (200) starts to be formed by outward turning. Step 3: The driving rod (3) finishes descending, and the forming of the blade (200) is completed. Step 4: The driving rod (3) moves upward along with the upper template (1), the driving rod (3) completely separates from the forming punch, and each of the wedge forming blocks (5) retracts inwardly. The formed pipe part (100) is taken out.
10. The one-step forming method of a circular tube blade according to claim 9, characterized in that: Before Step 1, a cut groove (300) in a "匚" shape is pre-punched on the pipe wall of the pipe part (100), and the area cut out by the cut groove (300) is correspondingly pressed by the forming convex block (6).