Fluent-based method for solving erosive wear of desulfurizing tower of circulating fluidized bed

Through CFD simulation and numerical simulation of Fluent software, a desulfurization tower inner wall erosion and wear model is constructed, which solves the problem of judging the wear location and degree of the circulating fluidized bed desulfurization tower, achieves accurate wear analysis and full life cycle management, and reduces safety Risks and design costs.

CN118839628APending Publication Date: 2024-10-25HUATIAN NANJING ENG & TECH CORP MCC +1

Patent Information

Application Number
CN202410842638.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-27
Publication Date
2024-10-25

AI Technical Summary

Technical Problem

It is difficult to accurately judge the erosion and wear parts and degree of wear of the circulating fluidized bed desulfurization tower with existing technology, leading to an increased risk of cylinder leakage and safety accidents. Moreover, traditional detection methods are limited and cannot effectively manage the entire life cycle of the desulfurization tower.

Method used

Fluent software is used to build an erosion and wear model for the inner wall of the desulfurization tower based on CFD simulation. Through 3D modeling, meshing and numerical simulation, combined with the turbulence and discrete phase models, the erosion cloud map and overall erosion rate are generated to accurately judge the desulfurization tower. The location and extent of wear.

Benefits of technology

It achieves an accurate solution to the erosion and wear of the desulfurization tower, shortens the design time and cost, overcomes the roughness of engineering experience and limitations of testing equipment, and provides a theoretical basis for full life cycle management.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118839628A_ABST
    Figure CN118839628A_ABST
Patent Text Reader

Abstract

The invention discloses a circulating fluidized bed desulfurization tower erosive wear solving method based on Fluent. Comprising the following steps: constructing an erosive wear model of the inner wall of the desulfurization tower; establishing a three-dimensional geometric model for the desulfurization tower; performing unstructured grid division on the 3D model; importing the grid file into a solver; opening a DPM discrete phase in the solver; if yes, an erosion cloud picture of the wall face of the desulfurizing tower is generated, the erosive wear portion of the desulfurizing tower is judged, the erosion rate of the unit area of the wall face of the desulfurizing tower is collected, and the wall face erosion rate is integrated with the area to obtain the overall erosion rate of the desulfurizing tower. Motion characteristics of flue gas and a desulfurizing agent in the desulfurizing tower can be simulated, abrasion and erosion conditions caused by continuous scouring of desulfurizing agent particles carried by the flue gas to the inner wall of the desulfurizing tower are analyzed, and model calculation results accord with actual working conditions; the method plays a key role in accurately judging the erosive wear part of the desulfurizing tower and determining the wear degree of the tower body.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a circulating fluidized bed desulfurization system, and in particular to a Fluent-based solution method for erosion and wear of a circulating fluidized bed desulfurization tower. Background Art

[0002] As the country continues to promote ultra-low emission transformation of flue gas in industries such as steel and building materials. The semi-dry circulating fluidized bed desulfurization process has been widely used for its simple operation, high desulfurization efficiency, no wastewater, and small footprint. As the core equipment of the circulating fluidized bed desulfurization process, the desulfurization tower has a large dust concentration (dust concentration 800-1000g / Nm3), a fast flow rate (Venturi throat flow rate 50-80m / s), and turbulent air flow in the tower. The flue gas entrained desulfurizer particles directly scour the inner wall of the tower, causing erosion and wear, and eventually leading to cylinder leakage. In severe cases, quality and safety accidents such as collapse and tilting of the desulfurization tower occur. Due to the closed operation of the desulfurization tower, it is impossible to judge the wear position and degree of the tower body by experience, and the desulfurization tower is covered with insulation cotton, and the detection equipment is restricted by many conditions and cannot accurately detect the thickness of the cylinder. Therefore, how to quickly and accurately judge the erosion and wear parts of the desulfurization tower and determine the degree of wear of the tower body is an urgent problem that technicians in this field need to solve. Summary of the invention

[0003] In view of the above problems, the purpose of the present invention is to provide a Fluent-based solution method for erosion and wear of a circulating fluidized bed desulfurization tower, which replaces traditional on-site inspections and engineering experience, achieves accurate solution to the erosion and wear of the desulfurization tower, and provides a theoretical basis for the full life cycle management of the desulfurization tower.

[0004] To achieve the above-mentioned purpose, the Fluent-based circulating fluidized bed desulfurization tower erosion and wear solution method of the present invention includes the following steps.

[0005] Step 1: construct an erosion and wear model of the inner wall of a circulating fluidized bed desulfurization tower according to the gas-solid flow field characteristics of the desulfurization tower;

[0006] Step 2, using 3D modeling software to establish a three-dimensional geometric model of the desulfurization tower;

[0007] Step 3, performing unstructured meshing on the 3D model of step 2;

[0008] Step 4, import the grid file into the solver, set the turbulence model, calculation domain, boundary conditions, perform continuous phase numerical simulation on the flue gas, and obtain the velocity cloud map and pressure cloud map of the desulfurization tower cross section;

[0009] Step 5: Open the DPM discrete phase in the solver, turn on the coupling between the DPM discrete phase and the continuous phase, activate the discrete phase model, set the particle parameters, activate the random walk model; set the material properties, computational domain, and boundary conditions; set the calculation method and residual, and start iterative solution;

[0010] Step 6, judging whether it has converged: if the calculated residual value tends to be stable or is lower than the set residual value, it is judged to be converged and proceeds to step 8; otherwise, it is judged to be non-convergent and proceeds to step 7;

[0011] Step 7, open the mesh model, improve the mesh quality, adjust the relaxation factor, and return to step 5;

[0012] Step 8, generate an erosion cloud map of the desulfurization tower wall, determine the location of the desulfurization tower where erosion and wear occur, collect the erosion rate per unit area of ​​the desulfurization tower wall, and integrate the wall erosion rate over the area to obtain the overall erosion rate of the desulfurization tower.

[0013] Furthermore, in step 1, according to the gas-solid flow field characteristics of the circulating fluidized bed desulfurization tower, the erosion and wear model of the inner wall of the desulfurization tower is constructed as follows:

[0014] During the desulfurization tower reaction, the desulfurizer particles are entrained by the flue gas and directly impact the inner wall of the desulfurization tower, and leave the wall at a certain reflection angle, causing a certain degree of erosion and wear on the inner wall surface during the collision, and finally resulting in a reduction in the surface material mass. When the particles collide with the inner wall, their momentum also changes. The wall restitution coefficient is used to characterize the movement behavior of the particles after colliding with the wall, and is a model parameter that reflects the momentum and energy loss of the particles. The wall restitution coefficient model adopts the Grant and Tabakoff model, and the wall restitution coefficient equation is shown in the following formulas (1)(2);

[0015] e n =0.993-0.030717795α+0.000475203α 2 -2.60512×10 -6 α 3 (1)

[0016] e t =0.988-0.028972466α+0.000642743α 2 -3.56211×10 -6 α 3 (2)

[0017] Where e n is the wall normal restitution coefficient, e t is the tangential restitution coefficient of the wall; α is the impact angle, unit angle;

[0018] When analyzing the trajectory of desulfurizer particles in the desulfurization tower, the interaction between the gas and solid phases is considered. The exchange of momentum, mass and heat on the particle trajectory is affected by the flue gas flow field. Assuming that the mass of the particles remains unchanged during the movement and the temperature change is not considered, the momentum exchange mainly occurs between the flue gas and the particles. The equation for the change of particle momentum is shown in the following formula (3):

[0019]

[0020] Where ΔF is the momentum change value, μ is the flue gas dynamic viscosity, unit is Pa.s; C D is the resistance coefficient; R er is the relative Reynolds number; V p is the particle velocity in m / s; V F is the fluid velocity in m / s; F other is other interphase forces; r p is the particle density in kg / m 3 ;dp particle diameter, unit: m;

[0021] Considering the influence of parameters such as particle incident angle, velocity, shape and mass flow rate, the erosion and wear model of the inner wall of the desulfurization tower is shown in the following formula (4);

[0022]

[0023] F(α)=9.42478×10 -2 α-3.07968×10 -3 α 2 +5.81102×10 -5 α 3

[0024] -5.87372×10 -7 α 4 +2.29972×10 -9 α 5 (5)

[0025] In the formula, R erosion is the erosion rate, kg / (m 2 .s);m p is the mass flow rate of the particles, in kg / s; C(dp) is the particle size function, which is 1.8×10 -9 ; F(α) is the impact angle function, calculated as shown in equation (5); v is the velocity of the particle relative to the wall, in m / s; b(v) is the velocity exponential function, which is 2.6; A face is the area of ​​erosion, unit: m 2 ; F(α) is the impact angle function, α is the impact angle, unit angle.

[0026] Furthermore, in step 2, the 3D modeling software used is one of Inventor, Solidworks or ICEM.

[0027] Furthermore, the turbulence model in step 4 uses the Realizable K-ε model and enhanced wall conditions; the velocity inlet and pressure outlet are used, and the turbulence intensity and hydraulic diameter are calculated by the following formula;

[0028] I=0.16×Re -1 / 8 (6)

[0029]

[0030]

[0031] Where Ι is the turbulence intensity; Re is the Reynolds number; r is the smoke density, unit kg / m 3 ; u is the inlet velocity in m / s; μ is the flue gas dynamic viscosity coefficient in Pa.s; D H is the hydraulic diameter, in m; b and h are the width and height of the desulfurization tower inlet pipe, in m.

[0032] Furthermore, the discrete phase model in step 5 is the Saffman lift model, pressure gradient model, virtual mass force model, and erosion / wear model; the particle injector parameters select surface injection, and set the particle injection velocity, diameter, and mass flow rate; the fluid density selects ideal gas, and the particle density is set to 600-1200kg / m 3 ; Select smoke as the fluid calculation domain.

[0033] Furthermore, for the boundary conditions in step 5, the DPM mode for the inlet and outlet boundaries is selected as "escape", the DPM mode for the wall boundary is selected as "reflect", the wall restitution coefficient model is shown in equations (1) and (2), the wear and erosion model is selected as the "GenericModel" model, the impact angle function is expressed in equation (5), and the particle size function and velocity index function values ​​are shown in the desulfurization tower inner wall erosion and wear model equations (4) and (5) for the formula description.

[0034] Furthermore, the calculation method in step 5 adopts a pressure-based coupled solver, with a continuity residual value of 1e-5 and other residual values ​​of 1e-3.

[0035] Furthermore, the relaxation factor of the momentum equation in step 7 is 0.4-0.8.

[0036] Furthermore, the step 3 also includes: locally encrypting the positions of the elbows, return chute, and guide plates to improve accuracy, the number of grid divisions is 300,000 to 800,000, and the size distortion rate and angle distortion rate of the grid are less than 0.8.

[0037] The present invention has the following advantages:

[0038] 1) The present invention uses Fluent software to simulate the motion characteristics of flue gas and desulfurizer in the desulfurization tower, and analyzes the wear and erosion caused by the flue gas carrying desulfurizer particles continuously scouring the inner wall of the desulfurization tower. The model calculation results are consistent with the actual working conditions. This plays a key role in accurately judging the erosion and wear parts of the desulfurization tower and determining the degree of tower wear.

[0039] 2) The present invention can effectively shorten the design time and cost. Numerical simulation calculations are not limited by experimental conditions, and simulation conditions can be adjusted at any time as needed, completely or partially replacing small-scale working condition experiments to obtain more comprehensive and more realistic data.

[0040] 3) The present invention can overcome the roughness and insufficiency of engineering experience and provide a basis for the design optimization of the desulfurization tower through numerical simulation.

[0041] 4) The present invention can overcome the limitations and shortcomings of engineering detection instruments, and through numerical simulation, visualize and fully display the wear and erosion process of the desulfurization tower to provide a basis for the full life cycle management of the desulfurization tower. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] Figure 1 It is the overall flow chart of the present invention;

[0043] Figure 2 It is a physical model of the desulfurization tower of the present invention;

[0044] Figure 3 It is a velocity cloud diagram of the cross section of the desulfurization tower of the present invention;

[0045] Figure 4 It is a motion trajectory diagram of the desulfurizer particles of the present invention;

[0046] Figure 5 It is a cloud diagram of erosion and wear of the inner wall of the desulfurization tower of the present invention. DETAILED DESCRIPTION

[0047] The embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0048] In the description of the present invention, it should be understood that the terms "center", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0049] The terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "plurality" means two or more.

[0050] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0051] The Fluent software used in the present invention is one of the most comprehensive software packages in the field of CFD (computational fluid dynamics) simulation in the world today. It has a wide range of physical models and can quickly and accurately obtain CFD analysis results.

[0052] like Figure 1 As shown, the Fluent-based circulating fluidized bed desulfurization tower erosion and wear solution method of the present invention includes the following steps.

[0053] Step 1: construct an erosion and wear model of the inner wall of a circulating fluidized bed desulfurization tower according to the gas-solid flow field characteristics of the desulfurization tower;

[0054] Step 2, using 3D modeling software to establish a three-dimensional geometric model of the desulfurization tower;

[0055] Step 3, performing unstructured meshing on the 3D model of step 2;

[0056] Step 4, import the grid file into the solver, set the turbulence model, calculation domain, boundary conditions, perform continuous phase numerical simulation on the flue gas, and obtain the velocity cloud map and pressure cloud map of the desulfurization tower cross section;

[0057] Step 5: Open the DPM discrete phase in the solver, turn on the coupling between the DPM discrete phase and the continuous phase, activate the discrete phase model, set the particle parameters, activate the random walk model; set the material properties, computational domain, and boundary conditions; set the calculation method and residual, and start iterative solution;

[0058] Step 6, judging whether it has converged: if the calculated residual value tends to be stable or is lower than the set residual value, it is judged to be converged and proceeds to step 8; otherwise, it is judged to be non-convergent and proceeds to step 7;

[0059] Step 7, open the mesh model, improve the mesh quality, adjust the relaxation factor, and return to step 5;

[0060] Step 8, generate an erosion cloud map of the desulfurization tower wall, determine the location of the desulfurization tower where erosion and wear occur, collect the erosion rate per unit area of ​​the desulfurization tower wall, and integrate the wall erosion rate over the area to obtain the overall erosion rate of the desulfurization tower.

[0061] Example 1

[0062] The present invention provides a Fluent-based solution method for erosion and wear of a circulating fluidized bed desulfurization tower, which is applied to a circulating fluidized bed flue gas desulfurization system of a certain incinerator. Basic parameters of the desulfurization tower: The flue gas volume of the desulfurization tower inlet is 7800m 3 / h, flue gas temperature 150℃, flue gas standard density 1.26kg / Nm 3 The desulfurization tower has a diameter of 0.66 meters and a height of 6.1 meters. The desulfurization tower has an inlet width / height of 0.4 meters / 0.4 meters. A guide plate is set at the elbow. The diameter of the venturi throat at the lower part of the desulfurization tower is 0.21 meters. The tower material is ordinary carbon steel Q235-B. The size of the return chute (width × height) is 0.15 × 0.03 meters. The inlet flue gas velocity of the desulfurization tower is 13m / s, the outlet velocity is 10m / s, the desulfurizer dosage is 1.7kg / s, and the density is 1000kg / m 3 , particle size is 50um.

[0063] The implementation steps are as follows:

[0064] Step 1: According to the gas-solid flow field characteristics of the circulating fluidized bed desulfurization tower, an erosion and wear model of the inner wall of the desulfurization tower is constructed.

[0065] The wall restitution coefficient model adopts the Grant and Tabakoff model, and the wall restitution coefficient equation is shown in the following equations (1) and (2);

[0066] e n =0.993-0.030717795α+0.000475203α 2 -2.60512×10 -6 α 3 (1)

[0067] e t =0.988-0.028972466α+0.000642743α 2 -3.56211×10 -6 α 3 (2)

[0068] Where e n is the wall normal restitution coefficient, e t is the tangential restitution coefficient of the wall; α is the impact angle, unit angle.

[0069] When analyzing the trajectory of desulfurizer particles in the desulfurization tower, the interaction between the gas and solid phases is considered. The momentum exchange mainly occurs between the flue gas and the particles. The equation for the change of particle momentum is shown in the following formula (3):

[0070]

[0071] Where ΔF is the momentum change value, μ is the flue gas dynamic viscosity, unit is Pa.s; C D is the resistance coefficient; R er is the relative Reynolds number; V p is the particle velocity in m / s; V F is the fluid velocity in m / s; F other is other interphase forces; r p is the particle density in kg / m 3 ;dp particle diameter, unit: m.

[0072] Considering the influence of parameters such as particle incident angle, velocity, shape and mass flow rate, the erosion and wear model of the inner wall of the desulfurization tower is shown in the following formula (4).

[0073]

[0074] F(α)=9.42478×10 -2 α-3.07968×10 -3 α 2 +5.81102×10 -5 α 3

[0075] -5.87372×10 -7 α 4 +2.29972×10 -9 α 5 (5)

[0076] In the formula, R erosion is the erosion rate, kg / (m 2 .s);m p is the mass flow rate of the particles, in kg / s; C(dp) is the particle size function, which is 1.8×10 -9 ; F(α) is the impact angle function, calculated as shown in equation (5); v is the velocity of the particle relative to the wall, in m / s; b(v) is the velocity exponential function, which is 2.6; A face is the area of ​​the computational domain, in m 2 ; F(α) is the impact angle function, α is the impact angle, unit angle.

[0077] Step 2: Based on the basic parameters of the desulfurization tower, Inventor software is used to build a 1:1 three-dimensional geometric model of the desulfurization tower and return chute.

[0078] Step 3, perform unstructured meshing on the 3D model of step 2, and perform local encryption on the elbows, guide plates, and return chute to improve installation accuracy. The number of mesh divisions is 312,000, and the size distortion rate and angle distortion rate of the mesh are 0.79.

[0079] Step 4: Import the mesh file into the solver, select the Realizable K-ε model as the turbulence model, and enhance the wall condition; set the boundary conditions, and set the smoke density to a constant (1.26 kg / Nm 3 ), the wall boundary uses a non-slip adiabatic wall, the model inlet is set as the velocity inlet (the inlet velocity is 13m / s), the hydraulic pressure is calculated to be 0.4 meters, the turbulence intensity is calculated to be 3%, the temperature is 150℃, and the model outlet is set as the pressure outlet. The continuous phase numerical simulation of the flue gas is carried out to obtain the velocity cloud map and pressure cloud map of the desulfurization tower cross section.

[0080] The hydraulic diameter and turbulence intensity are calculated as follows:

[0081] I=0.16×Re -1 / 8

[0082]

[0083]

[0084] Where Ι is the turbulence intensity, Re is the Reynolds number, r is the fluid density, u is the fluid velocity, μ is the fluid dynamic viscosity coefficient, D H is the hydraulic diameter, b is the pipe width, and h is the pipe height.

[0085] The flow equation of the Realizable K-ε model is as follows:

[0086]

[0087]

[0088] Where: C m =0.09,C 1ε =1.44,C 2ε =1.92,δ k =1.0,δ ε =1.3

[0089] G k --Turbulent kinetic energy k caused by mean velocity gradient

[0090] G b --The generation term of turbulent kinetic energy k caused by buoyancy

[0091] YM --Contribution of pulsation expansion in compressible flow

[0092] S k S g --User-defined source items

[0093] Step 5. Open the DPM discrete phase in the Fluent solver, turn on the coupling of the DPM discrete phase and the continuous phase, and activate the Saffman lift model, pressure gradient model, virtual mass force model, and erosion / wear model; select surface injection as the particle injector parameter, set the particle injection speed to 8m / s, the particle size to 50nm, and the particle mass flow rate to 1.7kg / s; select flue gas as the material property fluid medium, with a density of 1.26kg / Nm3; the density of the desulfurizer in the material properties is 1000kg / m 3 ; Select smoke as the fluid calculation domain.

[0094] For the inlet / outlet boundary condition, the DPM interface particle mode selects the "escape" mode, for the wall boundary condition, the DPM interface option particle mode selects the "reflect" mode, the wall restitution coefficient model is shown in equations (1) and (2), the wear and erosion model selects the "Generic Model" model, the impact angle function expression is shown in equation (5), the particle size function and velocity index function values ​​are shown in equations (4) and (5) of the desulfurization tower inner wall erosion and wear model.

[0095] Step 6, judging whether it has converged: if the calculated residual value tends to be stable or is lower than the set residual value, it is judged to be converged and proceeds to step 8; otherwise, it is judged to be non-convergent and proceeds to step 7;

[0096] Step 7, open the mesh model, improve the mesh quality, adjust the relaxation factor, and return to step 5;

[0097] Step 8, generate an erosion cloud map of the desulfurization tower wall, determine the location of the desulfurization tower where erosion and wear occur, collect the erosion rate per unit area of ​​the desulfurization tower wall, and integrate the wall erosion rate with respect to the area to obtain the overall erosion rate of the desulfurization tower.

[0098] The present invention is described in detail above in conjunction with the accompanying drawings, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge of ordinary technicians in the field without departing from the purpose of the present invention. Many other changes and modifications that do not depart from the concept and scope of the present invention should be regarded as the protection scope of the present invention.

[0099] In the description of this specification, specific features, structures, materials or characteristics may be combined in an appropriate manner in any one or more embodiments or examples.

[0100] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any person skilled in the art can easily think of changes or substitutions within the technical scope disclosed by the present invention, which should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.

Claims

1. A Fluent-based solution method for erosion and wear of circulating fluidized bed desulfurization towers. It is characterized in that The following steps are involved: Step 1, constructing an erosion and wear model of the inner wall of a circulating fluidized bed desulfurization tower according to the gas-solid flow field characteristics of the desulfurization tower; Step 2, using 3D modeling software to establish a three-dimensional geometric model of the desulfurization tower; Step 3, performing unstructured meshing on the 3D model of step 2; Step 4, import the grid file into the solver, set the turbulence model, calculation domain, boundary conditions, perform continuous phase numerical simulation on the flue gas, and obtain the velocity cloud map and pressure cloud map of the desulfurization tower cross section; Step 5: Open the DPM discrete phase in the solver, turn on the coupling between the DPM discrete phase and the continuous phase, activate the discrete phase model, set the particle parameters, activate the random walk model; set the material properties, computational domain, and boundary conditions; set the calculation method and residual, and start iterative solution; Step 6, judging whether it has converged: if the calculated residual value tends to be stable or is lower than the set residual value, it is judged to be converged and proceeds to step 8; Otherwise, it is judged as non-convergence and goes to step 7; Step 7, open the mesh model, improve the mesh quality, adjust the relaxation factor, and return to step 5; Step 8, generate an erosion cloud map of the desulfurization tower wall, determine the location of the desulfurization tower where erosion and wear occur, collect the erosion rate per unit area of ​​the desulfurization tower wall, and integrate the wall erosion rate over the area to obtain the overall erosion rate of the desulfurization tower.

2. A method for solving erosion and wear of a circulating fluidized bed desulfurization tower based on Fluent as claimed in claim 1, It is characterized in that The step 1, based on the gas-solid flow field characteristics of the circulating fluidized bed desulfurization tower, constructs the desulfurization tower inner wall erosion and wear model specifically as follows: During the desulfurization tower reaction, the desulfurizer particles are entrained by the flue gas and directly impact the inner wall of the desulfurization tower, and leave the wall at a certain reflection angle, causing a certain degree of erosion and wear on the inner wall surface during the collision, and finally resulting in a reduction in the surface material mass. When the particles collide with the inner wall, their momentum also changes. The wall restitution coefficient is used to characterize the movement behavior of the particles after colliding with the wall, and is a model parameter that reflects the momentum and energy loss of the particles. The wall restitution coefficient model adopts the Grantand Tabakoff model, and the wall restitution coefficient equation is shown in the following formulas (1)(2); e n =0.993-0.030717795α+0.000475203α 2 -2.60512×10 -6 α 3 (1) e t =0.988-0.028972466α+0.000642743α 2 -3.56211×10 -6 α 3 (2) Where e n is the wall normal restitution coefficient, e t is the tangential restitution coefficient of the wall; α is the impact angle, unit angle; When analyzing the trajectory of desulfurizer particles in the desulfurization tower, the interaction between the gas and solid phases is considered. The exchange of momentum, mass and heat on the particle trajectory is affected by the flue gas flow field. Assuming that the mass of the particles remains unchanged during the movement and the temperature change is not considered, the momentum exchange mainly occurs between the flue gas and the particles. The equation for the change of particle momentum is shown in the following formula (3): Where ΔF is the momentum change value, μ is the flue gas dynamic viscosity, unit is Pa.s; C D is the resistance coefficient; R er is the relative Reynolds number; V p is the particle velocity in m / s; V F is the fluid velocity in m / s; F other is other interphase forces; r p is the particle density in kg / m 3 ; dp particle diameter, unit: m; Considering the influence of parameters such as particle incident angle, velocity, shape and mass flow rate, the erosion and wear model of the inner wall of the desulfurization tower is shown in the following formula (4); F(α)=9.42478×10 -2 α-3.07968×10 -3 α 2 +5.81102×10 -5 α 3 -5.87372×10 -7 α 4 +2.29972×10 -9 α 5 (5) In the formula, R erosion is the erosion rate, kg / (m 2 .s);m p is the mass flow rate of particles, in kg / s; C(dp) is the particle size function, which is 1.8×10 -9 ; F(α) is the impact angle function, calculated as shown in equation (5); v is the velocity of the particle relative to the wall, in m / s; b(v) is the velocity exponential function, which is 2.6; A face is the area of ​​erosion, in m 2 ; F(α) is the impact angle function, α is the impact angle, unit angle.

3. According to the Fluent-based solution method for erosion and wear of a circulating fluidized bed desulfurization tower as claimed in claim 1, It is characterized in that In step 2, the 3D modeling software used is one of Inventor, Solidworks or ICEM.

4. A method for solving erosion and wear of a circulating fluidized bed desulfurization tower based on Fluent according to claim 1, It is characterized in that The turbulence model in step 4 uses the Realizable K-ε model and enhanced wall conditions; the velocity inlet and pressure outlet are used, and the turbulence intensity and hydraulic diameter are calculated using the following formula; I=0.16×Re -1 / 8 (6) Where Ι is the turbulence intensity; Re is the Reynolds number; r is the smoke density, unit kg / m 3 ; u is the inlet velocity in m / s; μ is the flue gas dynamic viscosity coefficient in Pa.s; D H is the hydraulic diameter, in m; b and h are the width and height of the desulfurization tower inlet pipe, in m.

5. A Fluent-based solution method for erosion and wear of a circulating fluidized bed desulfurization tower as claimed in claim 1, Features The discrete phase models in step 5 are Saffman lift model, pressure gradient model, virtual mass force model, and erosion / wear model; select surface injection for particle injector parameters, set the particle injection velocity, diameter, and mass flow rate; select ideal gas for fluid density, and set the particle density to 600-1200 kg / m 3 ; Select smoke as the fluid calculation domain.

6. A Fluent-based solution method for erosion and wear of a circulating fluidized bed desulfurization tower as claimed in claim 1, Features For the boundary conditions in step 5, select "escape" for the DPM mode of the inlet and outlet boundaries, select "reflect" for the DPM mode of the wall boundary, see equations (1) and (2) for the wall restitution coefficient model, select the "Generic Model" model for the wear and erosion model, and see equation (5) for the expression of the impact angle function. See equation (4) and equation (5) for the desulfurization tower inner wall erosion and wear model for the values ​​of the particle size function and velocity index function.

7. A Fluent-based solution method for erosion and wear of a circulating fluidized bed desulfurization tower as claimed in claim 1, It is characterized in that The calculation method in step 5 uses a pressure-based coupled solver with a continuity residual value of 1e-5 and other residual values ​​of 1e-3.

8. A Fluent-based solution method for erosion and wear of a circulating fluidized bed desulfurization tower according to claim 1, It is characterized in that The relaxation factor for the momentum equation in step 7 is 0.4-0.

8.

9. A Fluent-based solution method for erosion and wear of a circulating fluidized bed desulfurization tower as claimed in claim 1, It is characterized in that The step 3 also includes: locally encrypting the elbow, the return chute, and the guide plate position to improve the accuracy, the number of grid divisions is 300,000 to 800,000, and the size distortion rate and angle distortion rate of the grid are less than 0.8.

Citation Information

Patent Citations

  • Method for predicting erosion rate of dilute-phase gas-solid two-phase flow

    CN114813424A

  • High-pressure black water angle valve multiphase flow erosion corrosion characteristic numerical value prediction method

    CN117172151A

  • Methods and systems for simulating hydrodynamics in gas-solid fluidized beds

    US20170061048A1

Cited By

  • Desulfurization wastewater zero discharge system and method for intelligent coal-fired power generation unit

    CN119370935A