Preparation method of anti-corrosion and anti-insect composite board

By adding anti-corrosion and insect-proof intermediate layer and polymer protective layer to the wood base, the problem of perishable pests in traditional wood is solved, and excellent anti-corrosion and insect-proof performance and environmental protection are achieved, extending service life and improving physics performance.

CN118876167AInactive Publication Date: 2024-11-01ZHANGPU COUNTY YANGSEN WOOD IND CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410902274.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-06
Publication Date
2024-11-01
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Traditional wood is susceptible to moisture, decay and pests, and its service life is shortened. The existing anti-corrosion and insect prevention technology has problems such as poor environmental protection, uneven handling or insufficient durability.

Method used

The composite panel preparation method is adopted, consisting of a wood base layer, an anti-corrosion and insect-proof intermediate layer and a protective layer. The anti-corrosion and insect-proof intermediate layer contains nano silver oxide, acetic acid, polyacrylonitrile-based carbon fiber, lignin, copper sulfate solution and other components, and is treated by drying. , uniform mixing, hot pressing bonding and curing steps, and the protective layer is covered with polymer material.

Benefits of technology

It achieves excellent anti-corrosion and insect resistance, extends service life, reduces the use of harmful chemicals, improves the ecological friendliness and physical properties of the products, and makes it suitable for diversified environmental conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118876167A_ABST
    Figure CN118876167A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of composite boards, and particularly relates to a preparation method of an anti-corrosion and anti-insect composite board, through the processes of wood pretreatment, middle layer preparation, coating and hot pressing, curing and forming and cutting and detection, the composite board has excellent anti-corrosion and anti-insect performance, the service life is prolonged, the adopted material combination pays attention to environmental protection, and the production cost is reduced. The use of harmful chemical substances is reduced, the ecological friendliness of the product is improved, in addition, the overall physical performance of the board is enhanced through the special middle layer design and the surface protection layer, and the board is more durable and suitable for diversified environmental conditions.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of composite boards, and in particular relates to a method for preparing an anticorrosive and insect-proof composite board. Background Art

[0002] Traditional wood is susceptible to moisture, decay and insect pests, which shortens its service life. Although there are many anti-corrosion and anti-insect treatment technologies, they often have problems such as poor environmental protection, uneven treatment or insufficient durability. Therefore, it is particularly important to develop a method for preparing composite panels that can effectively prevent corrosion and insect pests, and is environmentally friendly and durable. Summary of the invention

[0003] In order to solve the problems raised in the above background technology, the present invention provides a method for preparing an anticorrosive and insect-proof composite board, which comprises, from top to bottom, a wood base layer, an anticorrosive and insect-proof middle layer, and a protective layer.

[0004] As the anticorrosive and insect-proof composite board of the present invention, preferably, the wood base layer is made of natural hardwood or softwood as the base material, and the thickness is about 8-15 mm.

[0005] As the anti-corrosion and insect-proof composite board of the present invention, preferably, the anti-corrosion and insect-proof middle layer is composed of the following components: nano silver oxide: 5-10 parts, acetic acid: 15-25 parts, diphenylmethane diisocyanate: 15-25 parts, polyacrylonitrile-based carbon fiber: 8-12 parts, lignin and bark extract: 8-12 parts each, copper sulfate solution and chitosan solution: 5-10 parts each, polyethyleneimine aqueous solution: 5-7 parts, plant essential oil, sodium pyrosulfite, tebuconazole, silicon dioxide, platycodon saponin, calcium chloride, borax: the total amount is controlled at 2-10 parts.

[0006] As the anti-corrosion and insect-proof composite board of the present invention, preferably, the protective layer is made of polymer materials such as polyurethane or epoxy resin and covers the outside of the anti-corrosion and insect-proof middle layer to enhance the surface protection ability.

[0007] As the method for preparing the anticorrosion and insect-proof composite board of the present invention, preferably, it comprises the following steps:

[0008] Step 1: Wood pretreatment: Dry the wood substrate to ensure the moisture content is 8-10%;

[0009] Step 2: Preparation of the intermediate layer: Mix the above components in proportion and disperse them evenly using a specific solvent or heating method;

[0010] Step 3: Coating and hot pressing: Evenly apply the prepared antiseptic and anti-insect liquid to both sides of the wood base, then cover with the protective layer material, and use a hot press machine to heat press at 140-160℃ for 1.0-1.2min / mm to make each layer tightly bonded;

[0011] Step 4: Curing and forming: After hot pressing, the board enters the constant temperature room for curing to ensure that all components react fully;

[0012] Step 5: Cutting and testing: After curing, cut the board into required size and conduct corrosion resistance, insect resistance and mechanical strength testing.

[0013] Compared with the prior art, the present invention has the following beneficial effects:

[0014] The composite board of the present invention not only has excellent anti-corrosion and anti-insect properties and extends its service life, but also uses a material combination that pays attention to environmental protection, reduces the use of harmful chemicals, and improves the eco-friendliness of the product. In addition, the special middle layer design and surface protection layer enhance the overall physical properties of the board, making it more durable and suitable for a variety of environmental conditions. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:

[0016] Figure 1 It is a schematic diagram of the structure of the composite plate of the present invention;

[0017] Figure 2 is a flow chart of the steps of the method for preparing the composite board of the present invention;

[0018] In the figure:

[0019] 1. Wood substrate;

[0020] 2. Anti-corrosion and insect-proof middle layer;

[0021] 3. Protective layer. DETAILED DESCRIPTION

[0022] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0023] Example 1

[0024] like Figure 1 As shown;

[0025] The invention discloses a method for preparing an anti-corrosion and insect-proof composite board, which comprises an anti-corrosion and insect-proof composite board body.

[0026] In this embodiment: In order to solve the technical problems existing in this prior art, such as the above background technology disclosed that "traditional wood is susceptible to moisture, decay and insect pests, which shortens its service life. Although there are various anti-corrosion and anti-insect treatment technologies, they often have problems such as poor environmental protection, uneven treatment or insufficient durability". Combined with actual use, this problem is obviously a real problem that is difficult to solve. In view of this, in order to solve this technical problem, a method for preparing an anti-corrosion and anti-insect composite board is provided.

[0027] like Figure 1-Figure 2 As shown;

[0028] In combination with the above contents, it includes, from top to bottom: a wood base layer 1, an anticorrosive and insect-proof middle layer 2, and a protective layer 3.

[0029] In an optional embodiment, the wood base layer 1 is made of natural hardwood or softwood as a base material, and has a thickness of about 8-15 mm.

[0030] In an optional embodiment, the anti-corrosion and insect-proof intermediate layer 2 is composed of the following components: nano silver oxide: 5-10 parts, providing long-lasting antibacterial properties, acetic acid: 15-25 parts, as a preservative, diphenylmethane diisocyanate: 15-25 parts, enhancing adhesion, polyacrylonitrile-based carbon fiber: 8-12 parts, increasing the strength of the board, lignin and bark extract: 8-12 parts each, natural preservatives, copper sulfate solution and chitosan solution: 5-10 parts each, enhancing the anti-corrosion effect, polyethyleneimine aqueous solution: 5-7 parts, improving water resistance, plant essential oils, sodium metabisulfite, tebuconazole, silica, platycodon saponin, calcium chloride, borax: the total amount is controlled at 2-10 parts, for comprehensive insect and mildew prevention.

[0031] In an optional embodiment, the protective layer 3 is made of a polymer material such as polyurethane or epoxy resin and covers the outer side of the anti-corrosion and anti-insect intermediate layer to enhance the surface protection capability.

[0032] In an optional embodiment, the following steps are included:

[0033] Step 1: Wood pretreatment: Dry the wood substrate to ensure the moisture content is 8-10%;

[0034] Step 2: Preparation of the intermediate layer: Mix the above components in proportion and disperse them evenly using a specific solvent or heating method;

[0035] Step 3: Coating and hot pressing: Evenly apply the prepared antiseptic and anti-insect liquid to both sides of the wood base, then cover with the protective layer material, and use a hot press machine to heat press at 140-160℃ for 1.0-1.2min / mm to make each layer tightly bonded;

[0036] Step 4: Curing and forming: After hot pressing, the board enters the constant temperature room for curing to ensure that all components react fully;

[0037] Step 5: Cutting and testing: After curing, cut the board into the required size and test its corrosion resistance, insect resistance and mechanical strength.

[0038] Finally, it should be noted that the above are only preferred embodiments of the present invention and are not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or replace some of the technical features therein by equivalents. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. Anti-corrosion and anti-insect composite board, characterized by: It comprises, from top to bottom, a wood base layer (1), an anticorrosive and insect-proof middle layer (2), and a protective layer (3).

2. The anticorrosion and insect-proof composite board according to claim 1, characterized in that: The wood base layer (1) is made of natural hardwood or softwood as the base material, and has a thickness of about 8-15 mm.

3. The anticorrosion and insect-proof composite board according to claim 1, characterized in that: The anticorrosion and insect-proof middle layer (2) is composed of the following components: 5-10 parts of nano silver oxide, 15-25 parts of acetic acid, 15-25 parts of diphenylmethane diisocyanate, 8-12 parts of polyacrylonitrile-based carbon fiber, 8-12 parts of lignin and bark extract, 5-10 parts of copper sulfate solution and chitosan solution, 5-7 parts of polyethyleneimine aqueous solution, plant essential oil, sodium pyrosulfite, tebuconazole, silicon dioxide, platycodon saponin, calcium chloride, borax: the total amount is controlled to be 2-10 parts.

4. The anticorrosion and insect-proof composite board according to claim 3, characterized in that: The protective layer (3) is made of a polymer material such as polyurethane or epoxy resin and covers the outer side of the anti-corrosion and anti-insect intermediate layer to enhance the surface protection capability.

5. A method for preparing an anticorrosive and insect-proof composite board, characterized in that: The following steps are involved: Step 1: Wood pretreatment: Dry the wood substrate to ensure the moisture content is 8-10%; Step 2: Preparation of the intermediate layer: Mix the above components in proportion and disperse them evenly using a specific solvent or heating method; Step 3: Coating and hot pressing: Evenly apply the prepared antiseptic and anti-insect liquid to both sides of the wood base, then cover with the protective layer material, and use a hot press machine to heat press at 140-160℃ for 1.0-1.2min / mm to make each layer tightly bonded; Step 4: Curing and forming: After hot pressing, the board enters the constant temperature room for curing to ensure that all components react fully; Step 5: Cutting and testing: After curing, cut the board into required size and conduct corrosion resistance, insect resistance and mechanical strength testing.

Citation Information

Patent Citations

  • Wood preservative

    CN107813388A

  • Anticorrosive composite board and preparation method thereof

    CN109021309A

  • Waterproof mould proof plank

    CN206495404U

  • Longacting mothproof composite wood floor

    CN213626454U