High-puncture-resistance composite film as well as preparation method and application thereof

By using a combined structure of coating layer, adhesive layer and high-strength composite substrate layer in the TPU film, the problem of poor puncture resistance performance of TPU film is solved, and a composite film with high puncture resistance and high tensile strength is achieved, improving The product's protective performance and lightweight properties are provided.

CN118876554APending Publication Date: 2024-11-01DONGGUAN XIONGLIN NEW MATERIAL TECH
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411114411.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-14
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The existing thermoplastic polyurethane (TPU) films have poor puncture resistance, resulting in poor protection, high weight and easy to break, making it difficult to achieve high protection functions.

Method used

Using a highly puncture-resistant composite film composed of a coating layer, an adhesive layer and a high-strength composite substrate layer, the coating layer and an adhesive layer are formed by gradient drying, combined with a temperature-resistant foam layer to improve flexibility and lightness. Quantification, the adhesive is oil glue, hot melt glue or silicone adhesive, and the high-strength composite substrate layer includes puncture-proof fabric and hot melt adhesive film.

Benefits of technology

It achieves high puncture resistance and tensile strength, which is 3 times that of ordinary polyurethane composite films, and has 2-3 times that of ordinary polyurethane composite films. It also has good bond fastness and high and low temperature stability. sex.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118876554A_ABST
    Figure CN118876554A_ABST
Patent Text Reader

Abstract

The invention discloses a high-puncture-resistance composite film and a preparation method and application thereof, and belongs to the field of materials.The high-puncture-resistance composite film comprises a coating layer, an adhesive layer and a high-strength composite substrate layer which are sequentially compounded from top to bottom, hot melt adhesive master batches are subjected to tape casting extrusion to form a hot melt adhesive film, the hot melt adhesive film is attached to an anti-puncture fabric, and the high-strength composite substrate layer is obtained; the preparation method comprises the following steps: coating a release surface of a polyester release film with a coating, drying to obtain a coating layer, coating the surface of the coating layer with an adhesive, drying, laminating with a high-strength composite substrate layer, and drying to obtain the high-puncture-resistance composite film. Meanwhile, the adhesive has good bonding fastness and high and low temperature stability, the mechanical strength of the adhesive is equivalent to that of a common polyurethane film, in addition, the film has high puncture resistance and tensile strength, the puncture resistance is 3 times that of a common polyurethane composite adhesive film, and the tensile strength is 2-3 times that of the common polyurethane composite adhesive film.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a composite film and a preparation method and application thereof, and in particular to a highly puncture-resistant composite film and a preparation method and application thereof, belonging to the field of materials. Background Art

[0002] Polyurethane (PU), whose full name is polyurethane, is a polymer material with excellent mechanical properties formed by the condensation reaction of polyols and polyisocyanates. It has strong plasticity. The main classifications of polyurethane include polyether type, polyester type, polyimide type, polyurea type, etc. They can be made into polyurethane plastics, polyurethane fibers, polyurethane rubbers and elastomers, polyurethane films and other materials.

[0003] Thermoplastic polyurethane film is becoming increasingly popular due to its superior performance and environmental protection concept. Thermoplastic polyurethane (TPU) not only has the characteristics of high tension, high tensile strength, strong and aging resistance, but is also a mature environmentally friendly material. TPU has been widely used in: shoes, clothing, inflatable toys, water and underwater sports equipment, medical equipment, fitness equipment, car seat materials, umbrellas, suitcases, bags, etc.

[0004] However, most existing TPUs have poor puncture resistance and high density, which also makes the products made from them have poor protection, high weight, easy to break when bumped, and not light enough. Mesh, synthetic leather, and TPU are all reduced in weight by reducing thickness, changing processes, and replacing raw materials, but TPU is a plastic with poor protection performance. It is very challenging to give it high protection against punctures. Summary of the invention

[0005] In view of this, the present invention provides a highly puncture-resistant composite film and a preparation method and application thereof, so as to solve the problems of poor puncture resistance of polyurethane composite films in the prior art, poor product protection performance, fastness and bending resistance of puncture-resistant composite films.

[0006] In order to achieve the above object, the present invention adopts the following technical solution: A highly puncture-resistant composite film comprises a coating layer, an adhesive layer and a high-strength composite base material layer which are composited in sequence from top to bottom.

[0007] The coating layer is obtained by coating one or more layers of coating, and the coating layer thickness is 0.02-0.2 mm; The thickness of the adhesive layer is 0.02mm-1mm; The high-strength composite substrate layer comprises a puncture-proof fabric and a film with a thickness of 0.012 mm to 1 mm coated on the fabric.

[0008] Furthermore, according to the requirements of light weight, softness and comfort, a heat-resistant foaming layer is also included. The heat-resistant foaming layer is arranged between the coating layer and the adhesive layer, or between multiple coating layers. The thickness of the heat-resistant foaming layer is 0.005-0.5mm.

[0009] The present invention also provides a method for preparing the above-mentioned highly puncture-resistant composite film, the steps of which are as follows: S1. Apply two-liquid adhesive on both sides of the puncture-proof fabric, dry it in a gradient manner after coating, form a hot-melt adhesive film by cast extrusion through hot melt adhesive masterbatch, and adhere it to one side of the dried puncture-proof fabric, and adhere the TPU film formed by cast extrusion on the other side to obtain a high-strength composite substrate layer; S2, coating the coating on the release surface of the polyester release film, and drying it in a gradient manner until it is dry to obtain a coating layer; S3, coating the adhesive on the surface of the coating layer, and drying the coating layer in a gradient manner until the coating layer is semi-dry or dry, to obtain an adhesive composite layer; S4. After laminating the adhesive composite layer and the high-strength composite base material layer, gradient drying is performed until they are semi-dry or dry to obtain a highly puncture-resistant composite film.

[0010] Wherein, the coating is any one of PU coating, PVC coating, and silicone coating; The adhesive is any one of oil adhesive, hot melt adhesive, silicone adhesive, two-component adhesive, and thermosetting adhesive.

[0011] Furthermore, the raw materials of the PU coating include, by weight, 50-100 parts of polyurethane resin, 0.03-1.5 parts of anti-hydrolysis agent, and 0.1-1.5 parts of anti-yellowing agent; Furthermore, the raw materials of PU coatings also include color powder.

[0012] Furthermore, the residual bonding strength of the polyester release film is 30-70%.

[0013] Furthermore, the gradient drying is drying in a bridge drying chamber at a temperature of 40°C-160°C.

[0014] The present invention also provides the application of the high puncture-resistant composite film in the fields of textiles, footwear materials and electronics.

[0015] The beneficial effects of the present invention are: The highly puncture-resistant composite film produced by the present invention has a functionalized surface, controllable thickness, and designable texture. It also has good bonding strength and high and low temperature stability, and is comparable to the mechanical strength of ordinary polyurethane films. In addition, the film has high puncture resistance and tensile strength, and its puncture resistance is 3 times that of ordinary polyurethane composite films, and its tensile strength is 2-3 times that of ordinary polyurethane composite films. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 Schematic diagram of the layer structure of the present invention.

[0017] In the accompanying drawings, the components represented by the reference numerals are listed as follows: 1. Coating layer, 2. Adhesive layer, 3. High-strength composite substrate layer. DETAILED DESCRIPTION

[0018] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0019] In the following examples, the preparation method of the highly puncture-resistant composite film is carried out according to the following steps: S1. Apply two-liquid glue (a combined adhesive consisting of two kinds of glues, urea-formaldehyde resin glue and polyvinyl acetate emulsion adjusted with hydrochloric acid) on both sides of the puncture-proof fabric, dry the coated product at a temperature of 40°C-160°C in a bridge oven in a manner of increasing and decreasing temperature until dry, form a hot-melt adhesive film by cast extrusion of the hot-melt adhesive masterbatch, adhere it to one side of the dried puncture-proof fabric, and adhere the TPU film formed by cast extrusion to the other side to obtain a high-strength composite base material layer; S2. Use the slit coating head of a bridge coating machine to evenly coat the coating (any one of PU coating, PVC coating, and silicone coating) on ​​the release surface of the polyester release film with a residual bonding strength of 30-70%, and dry it in a bridge oven at 40°C-160°C in a gradually increasing and decreasing manner to obtain a coating layer; S3, using the slit coating head of a bridge coating machine to evenly coat the adhesive (any one of oil adhesive, hot melt adhesive, silicone adhesive, two-component adhesive, and thermosetting adhesive) on the surface of the coating layer, and baking it in a bridge oven at 40°C-160°C in a gradually increasing and decreasing manner until it is semi-dry, to obtain an adhesive composite layer; S4. Compound the adhesive composite layer and the high-strength composite substrate layer through a bonding wheel, with a bonding pressure of 40-80 kgf and a temperature of 100-150°C, and dry the bonded product at a temperature of 40°C-160°C in a bridge oven in a temperature increasing and decreasing manner; S5. The dried product in S4 is ripened (>24h), peeled, and cut into appropriate specifications.

[0020] Example 1 The highly puncture-resistant composite film is prepared by the above method, and comprises, from top to bottom, a coating layer, an adhesive layer and a high-strength composite substrate layer.

[0021] Among them, the coating layer is 0.2mm thick, the adhesive layer is 0.1mm thick, and the high-strength composite substrate layer includes 210D puncture-proof fabric and hot-melt adhesive film and 0.05mm TPU film with thicknesses of 0.1mm and 0.05mm respectively; The raw materials of the coating are calculated by weight, including: 95 parts of polyurethane resin, 1 part of hydrolysis resistance agent, 0.3 parts of yellowing resistance agent, and 0.2 parts of color powder; The raw materials of the adhesive are calculated by weight and include: 100 parts of polyurethane adhesive resin and 2 parts of hydrolysis resistance agent.

[0022] The prepared high puncture resistance composite film was tested for performance and compared with conventional TPU film. The test items, methods and results are shown in the following table:

[0023] Example 2 The highly puncture-resistant composite film is prepared by the above method, and comprises, from top to bottom, a coating layer, an adhesive layer and a high-strength composite substrate layer.

[0024] The coating layer has a thickness of 0.02 mm, the adhesive layer has a thickness of 0.02 mm, and the high-strength composite substrate layer includes 210D puncture-proof fabric and a hot-melt adhesive film with a thickness of 0.012 mm and a TPU film with a thickness of 0.05 mm; The raw materials of the coating are calculated by weight, including: 50 parts of polyurethane resin, 0.03 parts of hydrolysis resistance agent, 0.1 parts of yellowing resistance agent, and 0.1 parts of color powder; The adhesive is a thermosetting adhesive.

[0025] Example 3 The highly puncture-resistant composite film is prepared by the above method, and comprises, from top to bottom, a coating layer, a temperature-resistant foaming layer, an adhesive layer and a high-strength composite substrate layer.

[0026] Among them, the coating layer is 0.2mm thick, the heat-resistant foaming layer is 0.005mm thick, the adhesive layer is 1mm thick, and the high-strength composite base material layer includes 210D puncture-proof fabric and a hot-melt adhesive film with a thickness of 1mm; The coating is PVC coating, the adhesive is hot melt adhesive, and the raw material of the heat-resistant foaming layer is PP foaming coating.

[0027] Example 4 The highly puncture-resistant composite film is prepared by the above method, and comprises, from top to bottom, a first coating layer, a temperature-resistant foaming layer, a second coating layer, an adhesive layer and a high-strength composite substrate layer.

[0028] Among them, the thickness of the two coating layers is 0.1mm in total, the thickness of the heat-resistant foaming layer is 0.5mm, the thickness of the adhesive layer is 0.02mm, and the high-strength composite base material layer includes 210D puncture-proof fabric and a hot-melt adhesive film with a thickness of 0.012mm; The coating is an organic silicon coating, the adhesive is an organic silicon adhesive, and the raw material of the heat-resistant foaming layer is TPEE foaming coating.

Claims

1. A highly puncture-resistant composite film, characterized in that: It includes a coating layer, an adhesive layer and a high-strength composite base material layer which are composited in sequence from top to bottom.

2. The highly puncture-resistant composite film according to claim 1, characterized in that: The coating layer is obtained by coating one or more layers of coating, and the coating layer has a thickness of 0.02-0.2 mm.

3. The highly puncture-resistant composite film according to claim 2, characterized in that: It also includes a heat-resistant foaming layer, which is arranged between the coating layer and the adhesive layer, or between multiple coating layers, and the thickness of the heat-resistant foaming layer is 0.005-0.5 mm.

4. The highly puncture-resistant composite film according to claim 1, characterized in that: The thickness of the adhesive layer is 0.02 mm-1 mm.

5. The highly puncture-resistant composite film according to claim 1, characterized in that: The high-strength composite base material layer comprises a puncture-proof fabric and a hot-melt adhesive film with a thickness of 0.012 mm to 1 mm coated on the fabric.

6. A method for preparing a highly puncture-resistant composite film, characterized in that: Here are the steps: S1. Apply two-liquid adhesive on both sides of the puncture-proof fabric, dry it in a gradient manner after coating, form a hot-melt adhesive film by cast extrusion through the hot-melt adhesive masterbatch, and laminate it on one side of the dried puncture-proof fabric, and laminate the TPU film formed by cast extrusion on the other side to obtain a high-strength composite substrate layer; S2, coating the coating on the release surface of the polyester release film, and drying it in a gradient manner until it is dry to obtain a coating layer; S3, coating the adhesive on the surface of the coating layer, and drying the coating layer in a gradient manner until the coating layer is semi-dry or dry, to obtain an adhesive composite layer; S4. After laminating the adhesive composite layer and the high-strength composite base material layer, gradient drying is performed until they are semi-dry or dry to obtain a highly puncture-resistant composite film.

7. The method for preparing the highly puncture-resistant composite film according to claim 6, characterized in that: The coating is any one of PU coating, PVC coating and silicone coating; The adhesive is any one of oil adhesive, hot melt adhesive, silicone adhesive, two-component adhesive, and thermosetting adhesive; The residual bonding strength of polyester release film is 30-70%; Gradient drying is bridge drying room drying with a temperature of 40℃-160℃.

8. The method for preparing the highly puncture-resistant composite film according to claim 7, characterized in that: The raw materials of the PU coating are calculated by weight and include: 50-100 parts of polyurethane resin, 0.03-1.5 parts of anti-hydrolysis agent, and 0.1-1.5 parts of anti-yellowing agent.

9. The method for preparing the highly puncture-resistant composite film according to claim 8, characterized in that: The raw materials of PU coatings also include color powder.

10. Application of the highly puncture-resistant composite film according to any one of claims 1 to 5 or the highly puncture-resistant composite film prepared by the preparation method according to any one of claims 6 to 9 in the fields of textiles, footwear materials, and electronics.

Citation Information

Patent Citations

  • TPU composite material for oil storage bag

    CN104527190A

  • Manufacturing method of hot melt adhesive-added cloth-based patch

    CN107652914A

  • Production process of lace needle-punched composite fabric

    CN109910382A