High-nitrogen-content Se-COF structural material as well as preparation method and application thereof
The preparation of high nitrogen-containing Se-COF materials through the Mann's reaction of selenocycinamine and aryl formaldehyde has solved the problem of insufficient crystallinity and stability of COFs materials, achieved efficient and rapid synthesis and high application performance, and expanded its in-electricity Application prospects in the fields of catalysis, photocatalysis and pollutant adsorption.
Patent Information
- Application Number
- CN202410915269.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-09
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2044-07-09
AI Technical Summary
Covalent organic frame materials (COFs) have shortcomings in terms of crystallinity and stability, especially selenium-rich COFs materials are scarce, resulting in application limitations in actual applications.
Se-COF structural materials with high nitrogen content are prepared by using selenocysamine and aryl formaldehyde as raw materials, and the dropwise addition reaction is carried out through Mann's reaction under the protection of inert gas. The temperature and dropwise acceleration are controlled to achieve efficient and rapid synthesis. Improve the crystallinity and stability of the material.
It has achieved high yield and short reaction time preparation of COFs materials. The products have good crystallinity and stability. They are suitable for electrocatalysis, photocatalysis and pollutant adsorption, and have high application potential.
Smart Images

Figure CN118878765A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of porous crystal materials, and in particular to a high-nitrogen-containing Se-COF structural material and a preparation method and application thereof. Background Art
[0002] Covalent organic frameworks (COFs) are an emerging class of crystalline porous materials connected by covalent organic ligands, which have attracted great attention. COFs have a well-defined two-dimensional (2D) or three-dimensional (3D) crystal structure. In the 2D structure, the building blocks are covalently connected into atomic layers and further stacked into overlapping layers through π-π interactions, while in the 3D structure, COFs are covalently connected and arranged three-dimensionally into an extended network. COFs achieve structural designability by precisely incorporating organic subunits into a predetermined framework at the atomic level. In addition, as a type of porous material, they also have the characteristics of low density, high surface area, high thermal stability, adjustable pore size and structure.
[0003] As COFs material synthesis technology matures, its synthesis methods are becoming more and more diverse. Conventional solvothermal synthesis of COFs usually requires high temperatures and long reaction times (3 days or longer), which poses a great obstacle to the accelerated discovery and exploration of new COFs materials in practical applications. Therefore, from the perspective of cost, time and energy consumption, it is very attractive to quickly synthesize COFs without compromising their inherent properties.
[0004] Furthermore, while in principle COFs have been shown to be competitive with metal-organic frameworks (MOFs) and zeolites in terms of functional group tolerance, structural tunability, and stability, achieving these functionalities in a covalently linked crystalline backbone remains a daunting challenge. The combination of covalent connectivity and crystallinity in COFs requires special functional groups and reaction conditions, which are usually applicable to reversible reactions. Therefore, when designing COFs materials based on reversible bonding reactions via dynamic covalent chemistry (DCC), it is usually difficult to achieve a balance between recrystallization and stability, which has always been a difficulty in designing new COFs and has also limited the exploration of COFs materials in practical applications.
[0005] The connecting bonds in most COFs materials reported so far are boron-oxygen bonds and imine bonds. Since they are reversible covalent bonds, they will decompose in harsh environments and cause the collapse of the COFs skeleton, which limits the application of COFs materials. How to build more stable COFs materials is a problem that restricts the development of COFs materials. Since 2016, COFs (sp 2 COFs) were first synthesized, and since then, COFs materials with carbon-carbon double bonds have begun to develop. 2Types of COFs and development of new applications, construction of new sp 2 COFs materials are very important.
[0006] However, there are few reports on selenium-rich COFs materials. For example, CN 113831510A discloses a covalent organic framework based on benzoselenadiazole and its preparation method and application. The covalent organic framework material connected by carbon-carbon double bonds has a high specific surface area and strong chemical stability, and has high application value in photoelectrocatalysis and separation.
[0007] Therefore, in order to prepare COFs materials with high crystallinity, good stability and practical application potential, it is necessary to introduce functional structures and functional groups into the materials. It is worth further exploring the preparation of COFs materials with high crystallinity and good application performance by functionalizing the COFs materials by changing the functional groups of the ligands. Summary of the invention
[0008] The present invention aims to solve the problems of low crystallinity and insufficient stability of covalent organic framework materials and provides a method for preparing a selenium-rich Se-COF structural material. The method uses selenocystamine and aromatic formaldehyde ligands as raw materials and obtains selenium COFs rich in nitrogen through the Mann-Brown reaction. The method has high yield, short reaction time and good product crystallinity.
[0009] To achieve the above object, the technical solution adopted by the present invention is:
[0010] A method for preparing a high-nitrogen Se-COF structural material comprises the steps of: dissolving selenocystamine and an aromatic formaldehyde ligand in ultra-dry DMF respectively for standby use; under the protection of an inert gas, dripping the selenocystamine solution into an aromatic formaldehyde ligand solution for reflux reaction, and washing and drying the product to obtain the high-nitrogen Se-COF structural material.
[0011] In the present invention, selenocystamine is used as a linking ligand of the COFs material, and a Se-Se structure is introduced into the COFs material. An efficient and rapid synthesis effect can be achieved through the Mann reaction. By controlling the temperature and the rate of ligand addition, the selenium-rich COF structure material prepared under heating reflux has good crystallinity, high nitrogen content, and good charge transfer effect, and has good application prospects in the fields of pollutant adsorption and photoelectrocatalysis. In addition, the material is prepared into a self-supporting film, which is expected to achieve the adsorption, separation, and selective permeation of organic pollutants, and has great potential in the treatment of environmental pollutants.
[0012] The aromatic formaldehyde ligand includes one or more of 2-hydroxy-1,3,5-benzenetricarboxaldehyde, 1,3,5-benzenetricarboxaldehyde, 2,4,6-trihydroxy-1,3,5-benzenetricarboxaldehyde, and [1,1'-biphenyl]-3,3',5,5'-tetracarboxaldehyde.
[0013] Preferably, the aromatic formaldehyde ligand is 2,4,6-trihydroxy-1,3,5-benzenetricarbaldehyde. Since the ligand has a high degree of symmetry and the hydroxyl functional group on the ligand easily promotes the nucleophilic addition reaction of the surrounding aldehyde groups, the COFs material prepared by the ligand has better crystallization properties.
[0014] The total molar ratio of the amino group of the selenocystamine to the hydroxyl group and the aldehyde group of the arylformaldehyde ligand is 3:1-1:3.
[0015] Preferably, the total molar ratio of the amino group of selenocystamine to the hydroxyl and aldehyde groups of the aromatic formaldehyde ligand is 1:1, and the COF structure does not have defects of exposed amino groups or hydroxyl / aldehyde end structures, so that the COF material has more excellent crystallization properties.
[0016] The molar concentration of selenocystamine in the selenocystamine solution is 1.5-4mmol / L. The molar concentration of the arylformaldehyde ligand in the arylformaldehyde ligand solution is 1-3mmol / L. The higher the concentration of the two raw materials, the higher the contact probability and the faster the reaction, but the crystallinity of the product may decrease slightly. In this range, the synthesis efficiency is high and the obtained product has good crystallinity.
[0017] The dripping speed of the selenocystamine solution is 2-10 mL / h. Preferably, the dripping speed is 3-7 mL / h. The dripping speed during the reaction process affects the yield and structure of the COFs material. The dripping of the sample at this speed can control the local reaction rate, so that the ligand functional groups can be fully contacted, so that the reaction is always maintained in a dynamic equilibrium process, and the formation of carbon-nitrogen bonds is maximized.
[0018] The reflux reaction temperature is 130-150° C. and the reaction time is 12-36 hours. Continuing the reaction at this temperature can ensure that the reaction proceeds smoothly, and the reaction within this time period can ensure that the reaction proceeds fully.
[0019] The preparation method of the invention has high yield, short time, relatively mild reaction conditions and low requirements on equipment, and can achieve a yield of more than 70%, or even more than 80%.
[0020] On the other hand, the present invention also provides a high nitrogen-containing Se-COF structural material prepared by the preparation method.
[0021] In another aspect, the present invention also provides the use of the high nitrogen content Se-COF structural material in electrocatalysis or photocatalysis.
[0022] The present invention also provides the use of the high nitrogen-containing Se-COF structural material as an adsorption material in the adsorption of heavy metal pollutants or transition metals, with high adsorption efficiency. The heavy metal pollutants include metals or metal salts containing Pb, Pd, Pt or Cr; the transition metals include metals or metal salts containing Ni, As, Cd or Hg.
[0023] Compared with the prior art, the present invention has the following beneficial effects:
[0024] In the present invention, selenocystamine is used to connect aromatic formaldehyde ligands, and Se-Se structures are introduced into COFs materials through the Mann reaction, thereby successfully preparing a series of nitrogen-rich selenium-rich COFs structural materials. The preparation method is simple and has a high yield. The product can greatly promote charge transfer in chemical reactions, and has great application prospects in the fields of electrocatalysis and photocatalysis. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 is the carbon NMR spectrum of Se-COF-1 obtained in Example 1 ( 13 C NMR).
[0026] Figure 2 is the X-ray powder diffraction (XRD) pattern of Se-COF-2 obtained in Example 2.
[0027] Figure 3 This is the X-ray powder diffraction (XRD) pattern of Se-COF-3 obtained in Example 3.
[0028] Figure 4 It is the adsorption of transition metal Ni in Application Example 1 2+ Ultraviolet-visible (UV-vis) spectrum.
[0029] Figure 5 This is a graph showing the removal rate of adsorbed Pb, Pd and Pt metal salts in Application Example 2.
[0030] Figure 6 It is the adsorption of heavy metal pollutants CrO in Application Example 3 4 2- UV-vis diagram. DETAILED DESCRIPTION
[0031] In order to make the purpose, technical scheme and advantages of the present invention clearer, the present invention is further described in detail below in conjunction with embodiment. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. Those skilled in the art can make modifications or equivalent substitutions based on the understanding of the technical scheme of the present invention without departing from the spirit and scope of the technical scheme of the present invention, and all should be included in the protection scope of the present invention.
[0032] The raw materials used in the following specific embodiments are all purchased from the market.
[0033] Example 1
[0034] A method for preparing a Se-COF structural material comprises the following steps:
[0035] Dissolve 0.2 g of 2,4,6-trihydroxy-1,3,5-benzenetricarboxaldehyde in 20 mL of ultra-dry DMF solution, place in a round-bottom flask, and pass N 2 Remove water and oxygen for later use; dissolve 0.6 g of selenocystamine in 10 mL of ultra-dry DMF and heat it under N 2 The mixture was stored in a vacuum oven at 75°C for 6 hours and then the selenocystamine solution was dropped into the aromatic formaldehyde ligand solution at a rate of 5 mL / h using a syringe. The mixture was heated to 150°C and refluxed for 12 hours. The unreacted substrate was removed by filtration using 60 mL of DMF and 60 mL of ethanol to prepare a Se-COF structural material with a high nitrogen content. The material was placed in a vacuum drying oven at 75°C and dried for 6 hours. The product obtained was recorded as Se-COF-1 with a yield of up to 90%.
[0036] The selenium-rich COFs prepared in the present invention have high stability. The material successfully generates CN single bonds and CN double bonds through solid nuclear magnetic carbon spectrum testing. The carbon spectrum is as follows: Figure 1 As shown in the figure, the positions of the fronts at a, b, c, d and e in the figure respectively represent the chemical environment of the carbon bonds at a, b, c, d and e in the structural formula, which shows that the target structure COFs were successfully prepared.
[0037] Example 2
[0038] A method for preparing a Se-COF structural material comprises the following steps: dissolving 0.3 g of 1,3,5-benzenetricarboxaldehyde in 20 mL of ultra-dry DMF solution, placing the solution in a round-bottom flask, and introducing N 2 Next, 0.3 g of selenocystamine was dissolved in 10 mL of ultra-dry DMF and heated under N 2 The mixture was stored in a vacuum oven at 75°C for 6 hours. The product was recorded as Se-COF-2 with a yield of 87%. Its X-ray powder diffraction (XRD) pattern is shown in Figure 2. Figure 2 As shown, the sharp peak at 2.74° proves that the material has good crystallinity.
[0039] Example 3
[0040] A method for preparing a Se-COF structural material comprises the following steps:
[0041] First, 0.5 g of [1,1'-biphenyl]-3,3',5,5'-tetracarboxaldehyde was dissolved in 20 mL of ultra-dry DMF solution and placed in a round-bottom flask. N 2 Next, 0.3 g of selenocystamine was dissolved in 10 mL of ultra-dry DMF and heated under N 2 The mixture was stored in a vacuum oven at 75°C for 6 hours. The product was recorded as Se-COF-3 with a yield of up to 90%. Its X-ray powder diffraction (XRD) pattern is shown in Figure 1. Figure 3 As shown, the sharp peak at 2.75° also shows that Se-COF-3 has good crystallinity.
[0042] Comparative Example 1
[0043] According to the process of Example 1, the dropping speed of the selenocystamine solution was modified to 50 mL / h. It can be observed that the speed of solid generation from the solution increased, and after the same reaction time, the yield was less than 50%.
[0044] Comparative Example 2
[0045] According to the process of Example 1, the reflux reaction temperature was modified to 200° C., and an increase in the rate of solid formation was also observed. However, after the same reaction time, the yield was less than 70%.
[0046] Application Example 1
[0047] Weigh 10 mg of the material from Example 1 and place it in 20 mL of 100 ppm NiCl 2 The solution was stirred for adsorption, and samples were taken for testing at intervals of 30 min, 5 h and 10 h. Under the monitoring of UV-Vis spectroscopy, it was found that the transition metal Ni was adsorbed within 10 h. 2+ Up to 80% or more. Adsorption of transition metal Ni 2+ The UV-visible spectrum of Figure 4 As shown, it can be seen that the material has a strong affinity to the transition metal Ni 2+ There is absorption in half an hour, and a wide range of absorption appears in about 5 hours. The absorbance is the lowest at 10 hours, and its absorbance is reduced by more than 80%, achieving Ni 2+ More than 80% adsorption effect.
[0048] Application Example 2
[0049] Weigh 10 mg of each material from Example 3 and place them in 20 mL of 100 ppm PbCl 2 , PdCl 2 and K 2 PtCl 6 The adsorption was stirred in the solution for 10 h. Under the monitoring of ICP spectrum, it was found that Pb 2+ , Pd 2+ , Pt 2+ The adsorption of salt is as high as 90%, 85%, and 80% or more. The removal rate of adsorbed Pb, Pd, and Pt metal salts is shown in the figure below. Figure 5 As shown, it can be seen that its effect on Pb 2 + , Pd 2+ , Pt 2+ The salts all have an adsorption effect close to 90%.
[0050] Application Example 3
[0051] Weigh 10 mg of the material from Example 3 and place it in 20 mL of 100 ppm Na 2 CrO 4 The solution was stirred and adsorbed, and samples were taken for testing at intervals of 1h, 5h and 10h. Under the monitoring of UV-vis spectrum, the results showed that the low concentration of heavy metal pollutants CrO 4 2- The removal rate is as high as 98%. Adsorption of heavy metal pollutants CrO 4 2- The UV-vis diagram is as follows Figure 6 shown.
Claims
1. A method for preparing a high nitrogen-containing Se-COF structural material, It is characterized in that The method comprises the following steps: dissolving selenocystamine and aromatic formaldehyde ligand in ultra-dry DMF respectively for standby use; under the protection of inert gas, dropping selenocystamine solution into aromatic formaldehyde ligand solution for reflux reaction, washing and drying the product to obtain the high nitrogen-containing Se-COF structural material.
2. The method for preparing the high nitrogen-containing Se-COF structural material according to claim 1, It is characterized in that The aromatic formaldehyde ligand includes one or more of 2-hydroxy-1,3,5-benzenetricarboxaldehyde, 1,3,5-benzenetricarboxaldehyde, 2,4,6-trihydroxy-1,3,5-benzenetricarboxaldehyde, and [1,1'-biphenyl]-3,3',5,5'-tetracarboxaldehyde.
3. The method for preparing the high nitrogen-containing Se-COF structural material according to claim 1, It is characterized in that The total molar ratio of the amino group of the selenocystamine to the hydroxyl group and the aldehyde group of the arylformaldehyde ligand is 3:1-1:
3.
4. The method for preparing the high nitrogen-containing Se-COF structural material according to claim 1, It is characterized in that The molar concentration of selenocystamine in the selenocystamine solution is 1.5-4 mmol / L.
5. The method for preparing the high nitrogen-containing Se-COF structural material according to claim 1, It is characterized in that The molar concentration of the aromatic formaldehyde ligand in the aromatic formaldehyde ligand solution is 1-3 mmol / L.
6. The method for preparing the high nitrogen-containing Se-COF structural material according to claim 1, It is characterized in that The dropping speed of the selenocystamine solution is 2-10 mL / h.
7. The method for preparing the high nitrogen-containing Se-COF structural material according to claim 1, It is characterized in that The reflux reaction temperature is 130-150° C. and the reaction time is 12-36 hours.
8. A high nitrogen-containing Se-COF structural material prepared according to the preparation method according to any one of claims 1 to 7.
9. Use of the high nitrogen-containing Se-COF structural material according to claim 8 in electrocatalysis or photocatalysis.
10. Use of the high nitrogen-containing Se-COF structural material according to claim 8 as an adsorption material in adsorbing heavy metal pollutants or transition metals, It is characterized in that The heavy metal pollutants include metals or metal salts containing Pb, Pd, Pt or Cr; the transition metals include metals or metal salts containing Ni, As, Cd or Hg.
Citation Information
Patent Citations
Combined hybrid cross-linked dynamic polymer and application thereof
CN111378165A
Covalent organic framework based on benzoselenadiazole as well as preparation method and application of covalent organic framework
CN113831510A
Covalent organic framework synthesized based on Mannich reaction as well as preparation method and application of covalent organic framework