Cookware coating and preparation method thereof
Through the pot coating and graded grinding technology divided into two components, the problems of shrinkage, fish eyes, brush marks and other problems during the drying and film formation of the pot coating are solved, which improves the gloss and adhesion of the coating, and solves the problem of the coating. The problems of surface defects and low grinding efficiency in the prior art are achieved, and a more uniform and wear-resistant coating effect is achieved.
Patent Information
- Application Number
- CN202411106777.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-13
- Publication Date
- 2024-11-01
AI Technical Summary
During the drying and film formation process, existing pot coatings are prone to surface defects such as shrinkage, fish eyes, brush marks, etc., which affects the gloss and aesthetics of the coating. The grinding treatment efficiency is low and requires multiple rework.
Use pot and trench coatings divided into two components, including the first component (titanium dioxide, barium sulfate, talc, phosphorus and zinc white, dispersant, vapor phase silica, polyester resin, diethylene glycol monobutyl ether, PMA and ethylene glycol monobutyl ether) and the second component (carbon black, phthalocyanine blue, permanent purple, WB204 polyester resin, alkyd resin, amino resin, BYK-358 leveling agent, isobutanol, tetrahydrofuran Toluene and BYK-300 leveling agent), improves the smoothness and adhesion of the coating through graded grinding and color-to-tuning treatment, prevents surface defects, and enhances the gloss of the coating with BYK-358 and BYK-300 leveling agents and transparency.
Significantly improve the appearance quality of the coating, prevent surface defects during drying and film formation, enhance the adhesion and wear resistance of the coating, reduce uneven problems caused by poor wetting, and improve the overall aesthetics and performance of the coating. .
Smart Images

Figure CN118879164A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of cookware coatings, and in particular to a cookware coating and a preparation method thereof. Background Art
[0002] At present, pot coatings are generally sprayed on the surface of pots, the main purpose of which is to enhance the non-stick, wear resistance, corrosion resistance and other properties of the pots, while improving the cooking experience and cleaning convenience. However, before spraying the existing pot coatings on the surface of the pots, the surface of the pots must be thoroughly cleaned to remove oil, rust and other impurities to ensure that the surface is clean and free of dirt. Then grind the pot surface: grinding can improve the roughness and adhesion of the pot surface, which is conducive to the adhesion and uniform distribution of the coating. If needed, a layer of primer or base coating can be sprayed on the surface of the pot to improve the adhesion and durability of the coating; then dry and form a film. The existing coatings are prone to surface defects such as shrinkage holes, fish eyes, and brush marks during the drying and film-forming process. Summary of the invention
[0003] In view of the above problems, the present invention proposes a cookware coating, which solves the problem that the existing cookware coating is prone to surface defects such as shrinkage holes, fish eyes, brush marks, etc. during the drying and film-forming process when the coating is sprayed on the cookware surface.
[0004] The technical solution adopted by the present invention is as follows:
[0005] A cookware coating comprises a first component and a second component, wherein the first component comprises titanium dioxide, barium sulfate, talcum powder, phosphorus zinc white, a dispersant, fumed silica, a polyester resin, diethylene glycol monobutyl ether, PMA and ethylene glycol monobutyl ether; the second component comprises carbon black, phthalocyanine blue, permanent violet, WB204 polyester resin, alkyd resin, amino resin, amino resin, BYK-358 leveling agent, isobutyl alcohol, tetramethylbenzene and BYK-300 leveling agent, wherein by mass percentage, the BYK-358N leveling agent is 0.3-0.4%, and the BYK-300 leveling agent is 0.3-0.4%. The present invention is divided into two components for mixing and coloring, so the dispersion effect is better and the color is richer. BYK-358 leveling agent, BYK-300 leveling agent, BYK-358N leveling agent are set at 0.3-0.4%, and BYK-300 leveling agent is 0.3-0.4%, which can further significantly improve the appearance quality of the coating, make the coating surface smoother and more uniform, thereby improving the gloss and transparency of the coating. It is helpful to prevent the occurrence of surface defects such as shrinkage holes, fish eyes, brush marks, etc. in the drying and film-forming process of the coating, and improve the overall aesthetics of the coating. The liquid is prompted to better wet the substrate during the coating process, thereby improving the adhesion between the coating and the substrate. The improvement of adhesion helps to enhance the wear resistance, weather resistance and other properties of the coating. The wettability of the coating is improved, so that the coating can be more evenly covered on the surface of the substrate, and the problem of uneven coating caused by poor wetting is reduced.
[0006] Optionally, the mass percentage of the titanium dioxide is 20-22%.
[0007] Optionally, the barium sulfate is 3.5-4.0% by mass.
[0008] Optionally, the mass percentage of the WB204 polyester resin is 16-20%.
[0009] Optionally, the mass percentage of the alkyd resin is 11-13%.
[0010] Optionally, the mass percentage of the amino resin is 11-13%.
[0011] Optionally, the mass percentage of the polyester resin is 9-11%.
[0012] The present invention also discloses a method for preparing a pot coating, comprising the following steps:
[0013] 1) putting the first component into a disperser according to a proportion, stirring and dispersing it, then putting the dispersed first component into a grinding device for coarse grinding, detecting the fineness of the coarsely ground first component, and performing fine grinding again according to the detected fineness of the first component to obtain a finely ground first component;
[0014] 2) adding the second component into a disperser according to a certain proportion, stirring and dispersing, and obtaining a semi-finished varnish;
[0015] 3) Mix the finely ground first component and semi-finished varnish to disperse the color.
[0016] Optionally, a method for preparing a cookware coating further comprises step 4), wherein step 4) is to color-match the dispersed and toned materials, and then add a solvent to adjust the viscosity to obtain a finished product for packaging.
[0017] Optionally, in step 1), the material to be ground is placed in the primary grinding chamber of the tank body of the multi-stage grinding equipment for coarse grinding, at which time the group partition seals the sampling tube, and sampling is performed through the upper sampling port. When the coarse grinding is completed, the sampling tube is pulled so that the group partition contacts the limit ring, and the coarsely ground material flows through the sampling tube into the secondary grinding chamber for fine grinding.
[0018] Beneficial Effects
[0019] 1. The present invention is divided into two components for mixing and coloring, so the dispersion effect is better and the color is richer. BYK-358 leveling agent, BYK-300 leveling agent, BYK-358N leveling agent are set at 0.3-0.4%, and BYK-300 leveling agent is 0.3-0.4%, which can further significantly improve the appearance quality of the coating, make the coating surface smoother and more uniform, thereby improving the gloss and transparency of the coating. It helps to prevent the occurrence of surface defects such as shrinkage holes, fish eyes, and brush marks in the coating during the drying and film forming process, and improve the overall aesthetics of the coating. It promotes the liquid to better wet the substrate during the coating process, thereby improving the adhesion between the coating and the substrate. The improvement of adhesion helps to enhance the wear resistance, weather resistance and other properties of the coating. The wettability of the coating is improved, so that the coating can be more evenly covered on the surface of the substrate, reducing the problem of uneven coating caused by poor wetting.
[0020] 2. In the present invention, the first component is subjected to graded grinding, which solves the drawback of the prior art that multiple reworks are often required. The graded grinding ensures the grinding quality and eliminates the need for multiple reworks.
[0021] 3. The first grinding teeth and the second grinding teeth in the present invention cooperate with the auxiliary grinding cylinder to grind the material, and the grinding efficiency is higher than that of the existing single grinding teeth. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 is a diagram showing the internal structure of a multi-stage grinding device for cookware coatings according to Embodiment 3 of the present invention;
[0023] Figure 2 is a partial three-dimensional view of the first grinding head of the cookware coating according to the third embodiment of the present invention;
[0024] Figure 3 It is a cross-sectional structural diagram of an auxiliary grinding cylinder of a cookware coating according to Embodiment 3 of the present invention.
[0025] The reference numerals in the figures are:
[0026] 1. Tank body, 2. Partition plate, 3. Primary grinding chamber, 4. Secondary grinding chamber, 5. Rotating shaft, 6. Driving device, 7. First grinding head, 8. Second grinding head, 9. Partition ring, 10. First grinding teeth, 11. Auxiliary grinding cylinder, 12. Second grinding teeth, 13. Loading port, 14. Discharging pipe, 15. Protruding ring, 16. Sampling tube, 17. Sampling port, 18. Elastic sheet, 19. Limiting ring, 20. Blocking plate, 21. Feed port, 22. Sampling cover. DETAILED DESCRIPTION
[0027] The specific implementation of the present invention is further described in detail below in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.
[0028] In the description of the present invention, unless otherwise specified, "multiple" means two or more than two; the orientation or position relationship indicated by the terms "upper", "lower", "left", "right", "inner", "outer", "front end", "rear end", "head", "tail", etc. is based on the orientation or position relationship shown in the drawings, which is only for the convenience of describing the present invention and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. In addition, the terms "first", "second", "third", etc. are only used for descriptive purposes and cannot be understood as indicating or implying relative importance. In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "connected" and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, a direct connection, or an indirect connection through an intermediate medium. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0029] Example 1
[0030] The technical solution adopted by the present invention is as follows:
[0031] The invention discloses a cookware coating, comprising a first component and a second component, wherein the first component comprises titanium dioxide, barium sulfate, talcum powder, phosphorus zinc white, a dispersant, fumed silica, a polyester resin, diethylene glycol monobutyl ether, PMA and ethylene glycol monobutyl ether; and the second component comprises carbon black, phthalocyanine blue, permanent violet, WB204 polyester resin, alkyd resin, amino resin, amino resin, BYK-358 leveling agent, isobutyl alcohol, tetramethylbenzene and BYK-300 leveling agent.
[0032] The mass percentage of the titanium dioxide is 20%. The mass percentage of the barium sulfate is 3.5%. The mass percentage of the WB204 polyester resin is 16%. The mass percentage of the alkyd resin is 11%. The mass percentage of the amino resin is 11%. The mass percentage of the polyester resin is 9%. By mass percentage, the BYK-358N leveling agent is 0.3%, and the BYK-300 leveling agent is 0.3%.
[0033] Example 2
[0034] The invention discloses a cookware coating, comprising a first component and a second component, wherein the first component comprises titanium dioxide, barium sulfate, talcum powder, phosphorus zinc white, a dispersant, fumed silica, a polyester resin, diethylene glycol monobutyl ether, PMA and ethylene glycol monobutyl ether; and the second component comprises carbon black, phthalocyanine blue, permanent violet, WB204 polyester resin, alkyd resin, amino resin, amino resin, BYK-358 leveling agent, isobutyl alcohol, tetramethylbenzene and BYK-300 leveling agent.
[0035] The mass percentage of the titanium dioxide is 22%. The mass percentage of the barium sulfate is 4.0%. The mass percentage of the WB204 polyester resin is 20%. The mass percentage of the alkyd resin is 13%. The mass percentage of the amino resin is 13%. The mass percentage of the polyester resin is 11%. By mass percentage, the BYK-358N leveling agent is 0.4%, and the BYK-300 leveling agent is 0.4%.
[0036] Example 3
[0037] The invention discloses a method for preparing a pot coating, comprising the following steps:
[0038] 1) The first component is put into the disperser in proportion to stir and disperse, and then the dispersed first component is put into the multi-stage grinding equipment for coarse grinding. The fineness of the coarsely ground first component is detected, and fine grinding is performed again according to the detected fineness of the first component to obtain the finely ground first component; the material to be ground is put into the first-level grinding chamber in the tank of the multi-stage grinding equipment for coarse grinding. At this time, the group partition seals the sampling tube, and sampling is performed through the upper sampling port. When the coarse grinding is completed, the group partition contacts the limit ring by pulling the sampling tube, and the coarsely ground material flows into the secondary grinding chamber through the sampling tube for fine grinding.
[0039] 2) adding the second component into a disperser according to a certain proportion, stirring and dispersing, and obtaining a semi-finished varnish;
[0040] 3) Mix the finely ground first component and semi-finished varnish to disperse the color.
[0041] 4) To color the dispersed and toned materials, and then add solvent to adjust the viscosity to obtain the finished product for packaging.
[0042] Among them, Figure 1 , Figure 2 and Figure 3 As shown, the multi-stage grinding equipment includes a tank body 1, in which a transversely arranged partition plate 2 is provided to divide the tank body into an upper primary grinding chamber 3 and a lower secondary grinding chamber 4, a rotating shaft 5 is rotated in the tank body, and the rotating shaft is externally connected to a driving device 6; the rotating shaft extends downward into the primary grinding chamber and the secondary grinding chamber, and a first grinding head 7 is provided in the part of the rotating shaft located in the primary grinding chamber, and a second grinding head 8 is provided in the part of the rotating shaft located in the secondary grinding chamber; the first grinding head and the second grinding head each include a plurality of separation rings 9, and a vertically arranged first grinding tooth 10 is provided between adjacent separation rings; the tank body is provided with a plurality of hollow auxiliary grinding cylinders 11 that simultaneously penetrate the first grinding chamber and the second grinding chamber, and the outer surface of the auxiliary grinding cylinder is provided with a second grinding tooth 12. A loading port 13 is provided at the top of the tank body, and a discharge pipe 14 is provided at the bottom of the tank body. An opening is provided at the bottom of the auxiliary grinding cylinder.
[0043] A protruding ring 15 is provided on the inner wall of the auxiliary grinding cylinder at the position facing the partition plate, a hollow sampling tube 16 for easy sampling is provided inside the auxiliary grinding cylinder, and a lower sampling port 17 is provided at the bottom of the sampling tube; a feed port 21 is provided near the protruding ring on the upper part of the auxiliary grinding cylinder, an elastic sheet 18 is provided on the inner wall of the auxiliary grinding cylinder at the lower end of the feed port, and a limiting ring 19 is provided on the inner wall of the auxiliary grinding cylinder at the lower end of the feed port. A blocking plate 20 for sealing the sampling tube is provided on the outer wall of the sampling tube. A sampling cover 22 is provided at the connection part between the auxiliary grinding cylinder and the top of the tank body.
[0044] When this embodiment is implemented, the material to be ground is placed in the primary grinding chamber in the tank body for rough grinding. At this time, the group partition seals the sampling tube, and sampling is performed through the upper sampling port. When the rough grinding is completed, the sampling tube is pulled so that the group partition contacts the limit ring. At this time, the rough ground material flows into the secondary grinding chamber through the sampling tube for fine grinding. The operator uses a sampler to reach into the sampling tube, extracts the sample in the secondary grinding chamber through the lower sampling port, and directly extends the sampler into the auxiliary grinding cylinder by opening it to extract the sample of the primary grinding chamber.
[0045] The above description is only a preferred embodiment of the present invention, and does not limit the patent protection scope of the present invention. Any equivalent structural transformation made by using the contents of the present invention and the drawings, directly or indirectly used in other related technical fields, is also included in the protection scope of the present invention.
Claims
1. A pot coating, It is characterized in that include: The invention comprises a first component and a second component, wherein the first component comprises titanium dioxide, barium sulfate, talc, phosphorus zinc white, a dispersant, fumed silica, a polyester resin, diethylene glycol monobutyl ether, PMA and ethylene glycol monobutyl ether; and the second component comprises carbon black, phthalocyanine blue, permanent violet, WB204 polyester resin, alkyd resin, amino resin, amino resin, BYK-358N leveling agent, isobutyl alcohol, tetramethylbenzene and BYK-300 leveling agent, wherein the BYK-358N leveling agent is 0.3-0.4% by mass and the BYK-300 leveling agent is 0.3-0.4% by mass.
2. A cookware coating as claimed in claim 1, It is characterized in that The mass percentage of the titanium dioxide is 20-22%.
3. A cookware coating as claimed in claim 1 or 2, It is characterized in that The mass percentage of the barium sulfate is 3.5-4.0%.
4. A cookware coating as claimed in claim 3, It is characterized in that The mass percentage of the WB204 polyester resin is 16-20%.
5. A cookware coating as claimed in claim 4, It is characterized in that The mass percentage of the alkyd resin is 11-13%.
6. A cookware coating as claimed in claim 5, It is characterized in that The mass percentage of the amino resin is 11-13%.
7. A cookware coating as claimed in claim 6, It is characterized in that The mass percentage of the polyester resin is 9-11%.
8. A method for preparing a cookware coating, wherein the cookware coating is the cookware coating according to claims 1 to 7, It is characterized in that The following steps are involved: 1) putting the first component into a disperser according to a proportion, stirring and dispersing it, then putting the dispersed first component into a multi-stage grinding device for coarse grinding, detecting the fineness of the coarsely ground first component, and performing fine grinding again according to the detected fineness of the first component to obtain a finely ground first component; 2) adding the second component into a disperser according to a certain proportion, stirring and dispersing, and obtaining a semi-finished varnish; 3) Mix the finely ground first component and semi-finished varnish to disperse the color.
9. A method for preparing a cookware coating as claimed in claim 8, It is characterized in that The method further comprises step 4), wherein the step 4) is to color-match the dispersed and toned materials, and then add a solvent to adjust the viscosity to obtain a finished product for packaging.
10. A method for preparing a cookware coating as claimed in claim 9, It is characterized in that In step 1), the material to be ground is placed in the primary grinding chamber of the tank body of the multi-stage grinding equipment for coarse grinding. At this time, the group partition seals the sampling tube, and sampling is performed through the upper sampling port. When the coarse grinding is completed, the sampling tube is pulled so that the group partition contacts the limit ring. At this time, the coarsely ground material flows into the secondary grinding chamber through the sampling tube for fine grinding.
Citation Information
Patent Citations
Automotive OEM (original equipment manufacturer) intermediate coat with high solid content and low viscosity and preparation method of intermediate coat
CN106118388A
Graded smashing and grinding equipment of solid chemical raw materials
CN108906252A
High-hardness paper tape wear-resistant household appliance color plate coating and preparation method thereof
CN111777927A
High-solid coiled material finish paint and preparation method thereof
CN112608661A