Optical fiber micropore refractive index sensor and manufacturing method thereof
By using femtosecond laser processing and wet etching manufacturing technology in optical fiber micropore refractive index sensors, the problems of insufficient working ability and complex cross-sensitivity in harsh environments are solved, and high sensitivity and fast response refraction are achieved Rate detection, suitable for chemical, biological and medical monitoring.
Patent Information
- Application Number
- CN202410904531.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-08
- Publication Date
- 2024-11-01
AI Technical Summary
Traditional conductivity and MEMS micro-nano sensors lack the ability to operate in high-temperature, low-temperature, strong electromagnetic interference, and flammable and explosive environments, and the refractive index sensors have complex cross-sensitivity problems, making it difficult to achieve efficient monitoring.
A fiber micropore refractive index sensor was designed, manufactured by femtosecond laser processing and wet etching, including an open cavity and a closed solid cavity. It forms a reflective surface at the solid-liquid interface through Fresnel reflection to achieve high Sensitivity and fast response refractive index detection.
The sensor has good mechanical stability, fast response, high temperature resistance, excellent optical performance, low cost, suitable for chemical, biological and medical monitoring, with negligible temperature cross-sensitivity and high sensitivity, and is suitable for a wide range of applications.
Smart Images

Figure CN118883501A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of sensors, and in particular relates to an optical fiber microhole refractive index sensor and a manufacturing method thereof. Background Art
[0002] Traditional conductivity sensors and MEMS-based micro-nano sensors are based on the principle of electrical parameter measurement, and there are still many problems in their ability to withstand harsh environments. In particular, it is difficult for them to work under harsh conditions such as high temperature (above 600°C), low temperature (below -60°C), strong electromagnetic interference, and flammable and explosive environments, which limits their special applications in many important fields.
[0003] Refractive index is an important parameter that reflects the optical properties of an object. By measuring the refractive index of a transparent liquid or gas, its concentration can be determined and monitored. Therefore, refractive index sensing has become an important means of liquid and gas sensing. The refractive index sensor based on optical fiber not only has the characteristics of high sensitivity, fast response speed, large dynamic range, anti-electromagnetic interference, flame retardant and explosion-proof, and not easy to be poisoned, but also can realize long-distance data collection and monitoring. It has gradually become one of the mainstream development directions of the new generation of sensor technology. At the same time, due to the rapid development of biology, medicine, energy, environment, aerospace, military and other fields, very urgent requirements have been put forward for the miniaturization, lightweight, low energy consumption, and resistance to harsh environments of sensors. Micro-nano sensors have become one of the major international scientific and technological frontiers.
[0004] The rapid development of laser micromachining technology has provided a new technical means for the research of a new generation of micro-nano optical fiber sensors. Therefore, how to use modern micro-nano processing technologies such as laser to realize various micro-nano functional sensors on optical fibers is an important trend in the future development of optical fiber sensors and a very cutting-edge and important scientific topic in the field of sensors. On this basis, the optical fiber Fabry-Perot refractive index sensor came into being.
[0005] In the field of refractive index sensing, fiber Bragg grating refractive index sensing is currently commonly used, but due to its large cross-sensitivity, the processing of measurement results becomes complicated. Summary of the invention
[0006] In order to overcome the above problems existing in the prior art, the purpose of the present invention is to provide an optical fiber micropore refractive index sensor and a method for manufacturing the same. The sensor has the characteristics of good mechanical stability, fast response, high temperature resistance and good optical performance. The preparation method can be manufactured in batches with high yield and high repetition rate.
[0007] In order to achieve the above object, the technical solution adopted by the present invention is:
[0008] An optical fiber micro-hole refractive index sensor comprises an optical fiber, a micro-groove is provided on the side of the optical fiber, and a micro-hole is provided at the center of the bottom of the micro-groove;
[0009] The optical fiber includes an open cavity and a closed solid cavity; a solid-liquid interface is formed at the contact point between the liquid and the open cavity and the closed solid cavity;
[0010] Fresnel reflection occurs at the solid-liquid interface, forming three reflection surfaces on the sensor head, which are denoted as M1, M2, and M3 respectively; M1 and M2 form an air FP sensing cavity, denoted as Cavity1, and M2 and M3 form a fiber FP reference cavity, denoted as Cavity2; Cavity3 is composed of M1 and M3.
[0011] The lengths of Cavity1, Cavity2 and Cavity3 are L1, L2 and L1+L2 respectively, and the refractive indexes of the optical fiber and the liquid are n2 and n1 respectively;
[0012] The reflection coefficients R1, R2, R3 of M1, M2, M3 depend on the refractive index of the liquid, which is equal to (n2-n1) 2 / (n2+n1) 2 ;
[0013] The total reflected electric field of the sensor is approximately represented by the sum of the first-order reflected electric fields of the three reflection surfaces; the total reflected electric field Er can be expressed as:
[0014]
[0015] Where E i is the input electric field, A1, A2, A3 are the optical attenuation factors at M1, M2, M3 respectively, β is the propagation constant of the fiber guided mode, α is the loss factor of Cavity1, there is a π phase shift at M2, and when n1>n2, there is also a π phase shift at M3.
[0016] The refractive index range of the liquid measured in this application is between 1.3 and 1.4, that is, n1≤n2. Therefore, the normalized reflected light intensity is obtained by formula (1):
[0017]
[0018] A=(1-α)(1-A1)(1-R1), B=(1-α)(1-A1)(1-A2)(1-R1)(1-R2);
[0019] Respectively represent the phase difference of light waves in Cavity1 and Cavity2, where λ is the wavelength of incident light;
[0020] Furthermore, the microgrooves are in the shape of a cuboid or a cube.
[0021] Furthermore, the microgroove depth is less than the optical fiber cladding thickness.
[0022] Furthermore, the transverse projection distance of the microgroove along the optical fiber is smaller than the diameter of the optical fiber.
[0023] Furthermore, the projection distance of the microgroove along the axial direction of the optical fiber is smaller than the length of the optical fiber.
[0024] Furthermore, the micropores are cylindrical, cuboid or cubic.
[0025] Furthermore, the microhole vertically penetrates the axial direction of the optical fiber and passes through the fiber core.
[0026] Furthermore, the transverse projection distance of the microhole along the optical fiber is smaller than the transverse distance of the microgroove along the optical fiber.
[0027] Furthermore, the projection distance of the microhole along the axial direction of the optical fiber is smaller than the axial distance of the microgroove along the axial direction of the optical fiber.
[0028] Furthermore, the Cavity 1 is an open cavity inside the optical fiber.
[0029] Furthermore, the Cavity2 is a closed solid cavity inside the optical fiber.
[0030] A method for manufacturing a sensor, the method comprising the following steps:
[0031] 1) Process a microgroove on the side of the optical fiber;
[0032] 2) machining a micro hole at the center of the bottom of the micro groove;
[0033] 3) Cut off a portion of the optical fiber so that the cut end surface forms a reflecting surface M3, which can be a plane or an inclined surface.
[0034] 4) Immerse the processed part of the optical fiber in HF solution and polish the reflective surface.
[0035] Furthermore, in step 3), the distance L2 between the reflection surface M3 and Cavity1 is between tens and hundreds of micrometers.
[0036] Furthermore, in step 4), the concentration of the HF solution is between 5% and 10%, and the immersion time is between 5 and 10 minutes; and the reflective surface includes M1, M2, and M3.
[0037] Beneficial effects of the present invention:
[0038] Refractive index sensing with hollow cavities fabricated by femtosecond laser machining and wet etching has been demonstrated, with good sensitivity and response speed compared to other fiber-based sensors. In addition, this configuration is less affected by temperature, with a temperature sensitivity of 0.015nm / °C and negligible temperature cross-sensitivity, which are extremely important features for in situ sensing. The innovative fabrication process of the cavity is quite simple and low-cost, and it is based on two simple steps, namely femtosecond laser machining and wet etching. The characterization of the sensor was carried out in the refractive index range between 1.3352 and 1.3792, with a sensitivity of 149.19nm / RIU.
[0039] The sensor has the advantages of good robustness, fast response speed, high sensitivity, low cost, and easy production and packaging. It can be widely used in chemical, biological, and medical monitoring fields. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Figure 1 It is a structural diagram of embodiment 1 of the present invention.
[0041] Figure 2 It is a schematic diagram of embodiment 1 of the present invention.
[0042] Figure 3 1 is a top view of the microgroove of Example 1 of the present invention.
[0043] Figure 4 3 is a top view of the micropores of Example 1 of the present invention.
[0044] Figure 5 It is a back view of the micropore of Example 1 of the present invention.
[0045] Figure 6 It is an overall side view of embodiment 1 of the present invention.
[0046] Figure 7 It is a structural block diagram of a refractive index sensing device according to Example 1 of the present invention.
[0047] Figure 8 This is an experimental diagram of the interference spectrum change of the optical fiber refractive index sensor under different refractive index conditions in Example 1 of the present invention.
[0048] Fig. 9 It is a linear fitting diagram of the refractive index sensitivity of Example 1 of the present invention.
[0049] Fig.10 4 is a structural block diagram of a temperature sensing device according to the first embodiment of the present invention.
[0050] Fig.11 This is an experimental diagram of the interference spectrum change of the optical fiber refractive index sensor under different temperature conditions in Example 1 of the present invention.
[0051] Fig.12 It is a temperature sensitivity linear fitting diagram of Example 1 of the present invention.
[0052] Figure numerals: 1. optical fiber, 2. microgroove, 3. microhole, 4. Cavity 1, 5. Cavity 2, 6. light source, 7. spectrometer, 8. circulator, 9. solution, 10. constant temperature box. DETAILED DESCRIPTION
[0053] The present invention will be further described in detail below in conjunction with the accompanying drawings.
[0054] like Figure 1 , Figure 2 As shown:
[0055] An optical fiber micro-hole refractive index sensor comprises an optical fiber 1, a micro-groove 2 is provided on the side of the optical fiber 1, and a micro-hole 3 is provided at the center of the bottom of the micro-groove 2;
[0056] The optical fiber 1 includes an open cavity and a closed solid cavity; a solid-liquid interface is formed where the liquid contacts the open cavity and the closed solid cavity;
[0057] Due to the different refractive indices of solids and liquids, Fresnel reflection occurs at the solid-liquid interface, forming three reflection surfaces on the sensor head, which are denoted as M1, M2, and M3 respectively; M1 and M2 form an air FP sensing cavity 4, denoted as Cavity1, and M2 and M3 form a fiber FP reference cavity 5, denoted as Cavity2; Cavity3 is composed of M1 and M3.
[0058] The lengths of Cavity1, Cavity2 and Cavity3 are L1, L2 and L1+L2 respectively, and the refractive indexes of the optical fiber and the liquid are n2 and n1 respectively. -6 / ℃) and thermal expansion coefficient (0.55×10 -6 / ℃) is very small, so the fiber refractive index n2 and the two FP cavity lengths L1 and L2 can be regarded as constants within the normal operating temperature range of the sensor;
[0059] The reflection coefficients R1, R2, R3 of M1, M2, M3 depend on the refractive index of the liquid, which is equal to (n2-n1) 2 / (n2+n1) 2 , which is much smaller than 1 in practice.
[0060] The total reflected electric field of the sensor is approximately represented by the sum of the first-order reflected electric fields of the three reflecting surfaces; due to the low reflection coefficient, the total proportion of high-order reflections is less than 0.1%, so it can be ignored. The total reflected electric field Er can be expressed as:
[0061]
[0062]
[0063] Where E i is the input electric field, A1, A2, A3 are the light attenuation factors at M1, M2, M3 respectively, which are caused by surface defects (such as roughness), β is the propagation constant of the fiber guided mode, α is the loss factor of Cavity1, which is mainly caused by diffraction in Cavity1. Ignore the loss in Cavity2, which is only the fiber loss in a short distance. For the sake of simplicity, the effect of surface defects on the reflection coefficient is also ignored. The effects of these three reflection surfaces are almost the same, mainly causing changes in the background light intensity. There is a π phase shift at M2, because the light is reflected from a denser medium. When n1>n2, there is also a π phase shift at M3.
[0064] The refractive index range of the liquid measured in this application is between 1.3 and 1.4, that is, n1≤n2. Therefore, the normalized reflected light intensity is obtained by formula (1):
[0065]
[0066] A=(1-α)(1-A1)(1-R1), B=(1-α)(1-A1)(1-A2)(1-R1)(1-R2);
[0067] They represent the phase difference of light waves in Cavity 1 and Cavity 2 respectively, where λ is the wavelength of incident light; further, the microgroove 2 is in the shape of a cuboid or a cube.
[0068] Furthermore, the depth of the microgroove 2 is less than the cladding thickness of the optical fiber 1 .
[0069] Furthermore, the lateral projection distance of the microgroove 2 along the optical fiber 1 is smaller than the diameter of the optical fiber 1 .
[0070] Furthermore, the projection distance of the microgroove 2 along the axial direction of the optical fiber 1 is smaller than the length of the optical fiber 1 .
[0071] Furthermore, the micropores 3 are cylindrical, cuboid or cubic.
[0072] Furthermore, the microhole 3 vertically penetrates the axial direction of the optical fiber 1 and passes through the fiber core.
[0073] Furthermore, the lateral projection distance of the microhole 3 along the optical fiber 1 is smaller than the lateral distance of the microgroove 2 along the optical fiber 1. Considering that when processing high aspect ratio microholes, the nonlinear absorption and refraction of the optical fiber to the laser will further hinder the feeding of the laser in the depth direction. Therefore, before the microhole processing, a microgroove 2 is first milled on the surface of the optical fiber with a laser to minimize the loss of the laser when propagating in the optical fiber, so as to ensure that the FP cavity 4 has a smaller taper. At the same time, this FP cavity in the form of a countersunk hole has an inconsistent contact area between the upper and lower surfaces with the liquid, resulting in a faster flow rate of the liquid at the large mouth than at the small mouth, thereby forming a one-way flow channel, which is convenient for the liquid to flow in and out, improves the response speed of the sensor, and effectively avoids the capillary force on the optical fiber surface from hindering the free flow of liquid in or out.
[0074] Furthermore, the projection distance of the microhole 3 along the axial direction of the optical fiber 1 is smaller than the axial distance of the microgroove 2 along the axial direction of the optical fiber 1 .
[0075] Furthermore, the Cavity 1 is an open cavity inside the optical fiber 1. It ensures the free entry and exit of liquid, so that the liquid directly participates in light transmission. The change of the refractive index of the liquid will cause the change of the effective refractive index of the light path, thereby affecting the output spectrum.
[0076] Furthermore, the Cavity 2 is a closed solid cavity inside the optical fiber 1, which ensures the normal transmission of the optical path.
[0077] The optical fiber 1 of the present invention is a single-mode or multi-mode optical fiber 1 made of quartz, polymer, gemstone or photonic crystal material;
[0078] The processing described in the present invention adopts ultraviolet laser processing, femtosecond laser processing, infrared laser processing or electron beam etching; the cutting described in the present invention adopts laser, ultrasonic wave, cutting knife or grinding method to cut; the optical fiber 1 of the present invention is composed of cladding and core.
[0079] Example 1: Figure 3-Figure 6 As shown:
[0080] 1) A cuboid microgroove 2 is processed on the side of the optical fiber 1 using a femtosecond laser;
[0081] 2) processing a cylindrical microhole 3 at the bottom center of the microgroove 2 using a femtosecond laser;
[0082] 3) Cut off a part of the optical fiber 1 so that the cut end surface forms a reflection surface M3 of the optical fiber Fabry-Perot refractive index sensor, and M3 is a plane;
[0083] 4) The processed part of the optical fiber 1 is immersed in a 5% HF solution 9 for 10 minutes to manufacture the Fabry-Perot refractive index sensor of the optical fiber 1 of the present invention.
[0084] See also Figure 7The optical fiber Fabry-Perot refractive index sensing device comprises a light source 6, wherein the light source 6 is connected to an optical fiber circulator 8, wherein one interface of the optical fiber circulator 8 is connected to an optical fiber Fabry-Perot refractive index sensor prepared by a femtosecond laser as described in Example 1, wherein the sensing head is completely immersed in a solution to be tested 9, and the other interface is connected to a spectrum analyzer; the light emitted by the light source 6 is introduced into the optical fiber Fabry-Perot refractive index sensor of the optical fiber 1 prepared by the femtosecond laser through the optical fiber circulator 8; the optical fiber Fabry-Perot refractive index sensor prepared by the femtosecond laser collects the external refractive index signal and finally displays it on the spectrum analyzer through the optical fiber circulator 8.
[0085] Figure 8 The figure below shows the interference spectrum change at different refractive indices under room temperature. It can be seen that when the refractive index of the liquid applied to the sensor head changes in the range of 1.3352 to 1.3792, the sensor's reflection spectrum shifts toward the long-wave direction as the refractive index increases. The trough near the wavelength of 1597nm is selected as the observation point dip. A linear fit is performed on the change of dip, and the results are as follows: Fig. 9 As shown, the linearity is 0.98014, with a good linear relationship, and the sensitivity is 149.19nm / RIU. Fig.10 The light is transmitted from the broadband light source to the circulator and then to the structure. After reflection, it enters the spectrometer. The experiment uses a programmable constant temperature and humidity test box with a temperature control accuracy of 0.01°C. The temperature range in the experiment is -5 to 45°C, and the spectrum change is recorded every 10°C. When the temperature reaches the set temperature, it is kept for 15 minutes before recording the spectrum. Put the sensor head into the test box and plug the furnace plug tightly.
[0086] The spectrum corresponding to the sensor changes at different temperatures is as follows Fig.11 As shown in the figure, as the temperature increases, the interference spectrum gradually redshifts, and the trough near the wavelength of 1603nm is selected as the observation point dip. A linear fit is performed on the change of dip, and the results are as follows: Fig.12 As shown, the linearity is 0.98329, which has a good linear relationship, and the sensitivity is 0.015nm / ℃. The temperature sensitivity of the sensor is low, which means that temperature crosstalk can be ignored in sensing of different refractive indices.
Claims
1. An optical fiber micropore refractive index sensor, characterized in that: The optical fiber (1) comprises a microgroove (2) on the side of the optical fiber (1) and a microhole (3) at the center of the bottom of the microgroove (2); The optical fiber (1) comprises an open cavity and a closed solid cavity inside; a solid-liquid interface is formed at the contact point between the liquid and the open cavity and the closed solid cavity; Fresnel reflection occurs at the solid-liquid interface, forming three reflection surfaces on the sensor head, which are denoted as M1, M2, and M3 respectively; M1 and M2 form an air FP sensing cavity (4), denoted as Cavity1, and M2 and M3 form a fiber FP reference cavity (5), denoted as Cavity2; Cavity3 is composed of M1 and M3.
2. The optical fiber microhole refractive index sensor according to claim 1, characterized in that: The lengths of Cavity1, Cavity2 and Cavity3 are L1, L2 and L1+L2 respectively, and the refractive indexes of the optical fiber and the liquid are n2 and n1 respectively; The reflection coefficients R1, R2, R3 of M1, M2, M3 depend on the refractive index of the liquid, which is equal to (n2-n1) 2 / (n2+n1) 2 .
3. The optical fiber micropore refractive index sensor according to claim 2, characterized in that: The total reflected electric field of the sensor is approximately represented by the sum of the first-order reflected electric fields of the three reflection surfaces; the total reflected electric field Er can be expressed as: Where E i is the input electric field, A1, A2, A3 are the optical attenuation factors at M1, M2, M3 respectively, β is the propagation constant of the fiber guided mode, α is the loss factor of Cavity1, there is a π phase shift at M2, and when n1>n2, there is also a π phase shift at M3.
4. The optical fiber microhole refractive index sensor according to claim 3, characterized in that: The refractive index of the liquid ranges from 1.3 to 1.4, that is, n1≤n2. Therefore, the normalized reflected light intensity is obtained by formula (1): A=(1-α)(1-A1)(1-R1), B=(1-α)(1-A1)(1-A2)(1-R1)(1-R2); They represent the phase difference of light waves in Cavity1 and Cavity2 respectively, where λ is the wavelength of incident light.
5. The optical fiber microhole refractive index sensor according to claim 1, characterized in that: The microgrooves (2) are in the shape of a cuboid or a cube; The depth of the microgroove (2) is less than the cladding thickness of the optical fiber 1; The lateral projection distance of the microgroove (2) along the optical fiber (1) is smaller than the diameter of the optical fiber (1). The projection distance of the microgroove (2) along the axial direction of the optical fiber (1) is smaller than the length of the optical fiber (1). The micropore (3) is cylindrical, cuboid or cubic; The microhole (3) vertically penetrates the axial direction of the optical fiber (1) and passes through the fiber core; The transverse projection distance of the microhole (3) along the optical fiber (1) is smaller than the transverse distance of the microgroove (2) along the optical fiber (1); The projection distance of the microhole (3) along the axial direction of the optical fiber (1) is smaller than the axial distance of the microgroove (2) along the axial direction of the optical fiber (1).
6. The method for manufacturing a sensor according to any one of claims 1 to 5, characterized in that: The method comprises the following steps: 1) machining a micro groove (2) on the side of the optical fiber (1); 2) machining a micro hole (3) at the center of the bottom of the micro groove (2); 3) cutting off a portion of the optical fiber (1) so that the cut end surface forms a reflection surface M3, and the reflection surface M3 is a plane or an inclined surface; 4) Immerse the processed part of the optical fiber (1) in an HF solution (9) to polish the reflective surface.
7. The method for manufacturing a sensor according to claim 6, characterized in that: Step 3) The distance L2 between the reflection surface M3 and Cavity1 is between tens and hundreds of microns.
8. The method for manufacturing a sensor according to claim 6, characterized in that: Step 4) The concentration of the HF solution 9 is between 5% and 10%, and the soaking time is between 5 and 10 minutes; the reflective surface includes M1, M2, and M3.