Metal film-medium resonant cavity enhanced negative electron affinity photoelectric cathode and preparation method thereof

By modulating the standing wave resonance effect of the metal film-dielectric resonant cavity structure, the problem of insufficient performance of the negative electron affinity photocathode is solved, realizing efficient photoelectric emission and fast response, which is suitable for high-brightness electron sources and low-light detection.

CN118888409APending Publication Date: 2024-11-01EAST CHINA UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410965745.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

Existing negative electron affinity photocathodes fail to meet the rapidly evolving needs of electron sources and deep-sea exploration in terms of key performance indicators such as quantum efficiency, response speed, and narrowband emission performance, and existing improvement methods are either costly or have limited effectiveness.

Method used

A metal film-dielectric resonant cavity structure is adopted, and the photoelectric performance is modulated through the standing wave resonance effect. It includes a high reflectivity metal film, a dielectric resonant cavity, and a semiconductor photoelectric active layer. It is fabricated using a flip-chip process to achieve high light absorption and narrowband emission.

Benefits of technology

It improves the photoelectric emission quantum efficiency and response speed of the photocathode, reduces electron emission and dark current, and is suitable for high-brightness electron sources and low-light detection. The process is simple and can be mass-produced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118888409A_ABST
    Figure CN118888409A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of vacuum photoelectric emission and application, and discloses a metal film-medium resonant cavity enhanced negative electron affinity photocathode and a preparation method thereof, and the metal film-medium resonant cavity enhanced negative electron affinity photocathode comprises a substrate, a high-reflectivity metal film, a medium resonant cavity, a window layer, a semiconductor photoelectric emission active layer and a negative electron affinity activation layer which are sequentially arranged from bottom to top. Selecting a wafer as a substrate; corroding the barrier layer, the photoelectric emission active layer, the window layer and the dielectric resonant cavity on the substrate; growing a high-reflectivity metal layer; preparing a wafer bonding substrate; bonding the substrate epitaxial wafer with the wafer bonding substrate; placing the sample wafer after wafer bonding in a nitric acid / hydrogen peroxide solution; performing soaking; removing the corrosion barrier layer; immersing a sample into the mixed solution, washing, blow-drying and heating at high temperature; cesium / oxygen activation is carried out; and preparing the cesium / oxygen active layer. Light absorption is enhanced, high light absorption is achieved, the photoelectric emission quantum efficiency and electron beam quality of the photoelectric cathode are improved, and the performance of QE, response speed and the like of the photoelectric cathode is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of vacuum photoelectric emission and application technology, in particular to a metal film-dielectric resonant cavity enhanced negative electron affinity photocathode and a preparation method thereof. Background Art

[0002] Negative electron affinity (NEA) photocathodes represented by gallium arsenide (GaAs) have advantages such as high quantum efficiency (QE), wide response band, and the ability to emit spin-polarized electrons. They have unique application value in the fields of accelerator electron sources, low-light detection, and low-energy electron diffraction characterization, and are a research hotspot in the field of photoemission. With the rapid development of technologies such as electron accelerators, space and deep-sea exploration, higher requirements have been placed on the key performance of negative electron affinity photocathodes used in these applications, such as quantum efficiency (QE), emittance, and response speed. How to improve these performance indicators has become a frontier hotspot and difficulty in the field of photoemission.

[0003] Negative electron affinity photocathodes can achieve the highest spin polarization and low-loss light transmission at wavelengths of 780 nanometers and 532 nanometers, respectively, and have strategic value in the fields of spin polarization electronics and low-light detection. However, the absorption coefficient of negative electron affinity photocathodes is very low at a wavelength of 780 nanometers, which is close to the edge of its intrinsic absorption band. The requirements of light absorption and electrical transport on the thickness of the active layer are opposite. Low QE and tailing effect are still important factors limiting its application. The use of strained superlattices to release the degenerate state of light and heavy holes can achieve 100% theoretical polarization, but due to stress restrictions, its thickness does not exceed 100 nanometers, which is far lower than the light absorption depth of 780 nanometers. Improving cathode performance faces great challenges. In the visible light region with shorter wavelengths, the intrinsic absorption coefficient of direct bandgap GaAs is high, the photoelectric emission bandwidth is large, and background light is easy to participate in photoelectric emission. If high QE narrowband emission can be achieved at the key application wavelength, background emission can be effectively suppressed and emission quality can be improved. Many improvements have been made to address these issues. Thomas Jefferson National Accelerator Laboratory uses distributed Bragg reflectors (DBR) to enhance long-wave light absorption, achieving a GaAs-based strained superlattice photocathode with a QE of 6.4% and a spin polarization of 84% near 780 nanometers, but the DBR structure is complex and the development cost is high. Nanjing University of Science and Technology uses wide-bandgap aluminum gallium arsenide (AlGaAs) semiconductors at a wavelength of 532 nanometers to effectively suppress long-wave emission and reduce the emission bandwidth, but the ability to suppress short-wave emission is limited. Other methods include using anti-reflection films to enhance light absorption, using window layers to reduce the recombination of electrons on the back, and using variable components or variable doping active regions to enhance electrical transport efficiency. These works have effectively improved the light absorption and electrical transport performance of negative electron affinity photocathodes, but their QE, response speed, narrowband emission performance and other qualities still cannot meet the urgent needs of rapidly developing advanced photocathode electron sources, space and deep-sea exploration.

[0004] Therefore, a new technical solution is needed to solve the above technical problems. Summary of the invention

[0005] In order to solve the above problems, the present invention discloses a metal film-dielectric resonant cavity enhanced negative electron affinity photocathode and a preparation method thereof, which utilizes the standing wave resonance effect of the metal film-dielectric cavity to regulate the photoelectric performance of the negative electron affinity photocathode, and fully confines the incident light to the ultra-thin photoelectric emission active layer, which can enhance light absorption, and regulates the light absorption characteristics of the cathode photoelectric emission active layer based on the standing wave resonance effect excited by the dielectric cavity, and realizes high light absorption in the nanometer-level ultra-thin active layer, thereby effectively improving the photoelectric emission quantum efficiency and electron beam quality of the photocathode, and improving important properties of the photocathode such as QE and response speed.

[0006] The technical solution of the present invention is: a metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, comprising a substrate, a high reflectivity metal film, a dielectric resonant cavity, a window layer, a semiconductor photoelectric emission active layer, and a negative electron affinity activation layer. The substrate, the high reflectivity metal film, the dielectric resonant cavity, the window layer, the semiconductor photoelectric emission active layer and the negative electron affinity activation layer are arranged in sequence from bottom to top.

[0007] Preferably, the substrate material is one of silicon (Si), gallium arsenide (GaAs), indium phosphide (InP), gallium phosphide (GaP), gallium nitride (GaN), zinc oxide (ZnO), or one of silicon dioxide (SiO2), silicon nitride (Si3N4), indium tin oxide (ITO), aluminum oxide (Al2O3), and titanium dioxide (TiO2), and the thickness of the substrate is between 100 and 3000 microns.

[0008] By adopting the above technical solution, the substrate can be bonded to the metal film to support the optical and electrical functional film materials of the photocathode thereon.

[0009] Preferably, the high reflectivity metal film material is any one of silver (Ag), aluminum (Al), and gold (Au), and the thickness of the high reflectivity metal film is between 100 and 1000 nanometers.

[0010] By adopting the above technical solution, the main function of the high-reflectivity metal film is to reflect the incident light, stimulate the standing wave resonance effect in the medium optical layer, and regulate the optical performance of the photoelectric active layer.

[0011] Preferably, the dielectric resonant cavity material is silicon dioxide (SiO2), silicon nitride (Si3N4), indium tin oxide (ITO), aluminum oxide (Al2O3), titanium dioxide (TiO2), aluminum gallium arsenide (Al x Ga 1-x As) one of thex Ga 1-x The As component x is between 0.5 and 1, and the thickness of the dielectric resonant cavity is between 100 and 1000 nanometers.

[0012] By adopting the above technical solution, the high reflectivity metal film and the dielectric resonant cavity together form a standing wave resonant cavity. The standing wave resonance absorption peak wavelength can be adjusted by changing the thickness of the dielectric resonant cavity, which functions to enhance the narrowband light absorption in the semiconductor photoelectric emission active layer 5.

[0013] Preferably, the window layer material is selected from aluminum gallium arsenide (Al x Ga 1-x As) compound semiconductors, Al x Ga 1-x The As component x is between 0.7 and 1, the doping type is P-type acceptor doping, and the doping concentration is 10 19 cm -3 , the thickness of the window layer is between 50 and 100 nanometers.

[0014] By adopting the above technical solution and using metal organic chemical vapor deposition for growth preparation, the function of the window layer is to form a built-in electric field on the back side of the photoelectric emission active layer, reduce the recombination rate of photogenerated carriers on the back side, and improve the photoelectric emission efficiency.

[0015] Preferably, the semiconductor photoelectric emission active layer material is selected as Al x Ga 1-x As compound semiconductors, Al x Ga 1-x The As component x is between 0 and 0.5, the doping type is P-type acceptor doping, and the doping concentration is 10 19 cm -3 , the thickness of the semiconductor photoelectric emission active layer is between 20 and 1000 nanometers.

[0016] By adopting the above technical solution and using metal organic chemical vapor deposition method for growth preparation, the function of the semiconductor photoelectric emission active layer is to absorb incident light, excite electrons in the conduction band and diffuse and transport them to the surface and then emit them into the vacuum.

[0017] Preferably, the negative electron affinity activation layer material is selected as a cesium / fluorine or cesium / oxygen film, and the thickness of the negative electron affinity activation layer is between 2 and 3 atomic layers.

[0018] By adopting the above technical solution, the bottom energy level of the conduction band on the upper surface of the semiconductor photoelectric emission active layer is lowered to below the vacuum energy level, reaching a negative electron affinity state, thereby realizing electron emission.

[0019] The method for preparing a metal film-dielectric resonant cavity enhanced negative electron affinity photocathode adopts a flip chip process and comprises the following steps:

[0020] Step 1: Select a 3-inch diameter p-type GaAs Epi-ready wafer as the substrate for epitaxial growth, with a dislocation density of less than 10 3 cm -3 , the crystal direction is (100) plane and (110) plane, with a 5° cut, and the thickness is 300 microns;

[0021] Through the above steps, the growth quality of the photoelectric emission active layer thin film can be improved by selecting a lattice-matched wafer as an epitaxial substrate.

[0022] Step 2: Use low pressure metal organic chemical vapor deposition to sequentially epitaxially grow Al with a thickness of 500 nanometers on the p-type GaAs epi-ready wafer epitaxial substrate in step 1. 0.5 Ga 0.5 As corrosion barrier layer, thickness of 50 nanometers and P-type doping concentration of 10 19 cm -3 The GaAs photoelectric emission active layer has a thickness of 50 nanometers and a P-type doping concentration of 10 19 cm -3 Al 0.7 Ga 0.3 As window layer and Al with a thickness of 376 nm 0.7 Ga 0.3 As dielectric resonant cavity;

[0023] Through the above steps, the metal organic chemical vapor deposition method can be used to achieve large-scale and low-cost growth of high-quality optoelectronic functional thin film materials.

[0024] Step 3: using electron beam evaporation in a high vacuum cavity to grow an aluminum (Al) film as a high reflectivity metal layer of the standing wave resonance cavity, the thickness of the Al film being 1000 nanometers;

[0025] Through the above steps, the electron beam evaporation method can be used to achieve the mass growth and preparation of high-quality metal reflective films.

[0026] Step 4: Prepare a circular SiO2 single crystal substrate with a diameter of 3 inches, a thickness of 500 microns and double-sided polishing as a wafer bonding substrate, requiring its purity to be higher than 99.9% and the roughness of the polished surface to be less than 10 angstroms;

[0027] Through the above steps, the selection of high-quality polished SiO2 wafers with low roughness can improve the success rate and bonding quality of the bonding process.

[0028] Step 5: Bond the GaAs substrate epitaxial wafer to the SiO2 wafer bonding substrate, the bonding method is anodic bonding, and the bonding surface is the upper surface of the high reflectivity metal layer;

[0029] Through the above steps, the bonding process is a necessary means to make a high-reflectivity metal film on the back of the photocathode. The anodic bonding process can effectively bond the metal to the dielectric / semiconductor substrate. The bonding strength is high and can withstand subsequent high-temperature cleaning and other processes.

[0030] Step 6: Place the wafer-bonded sample in a nitric acid / hydrogen peroxide solution with a volume ratio of nitric acid to hydrogen peroxide of 1:20 for 1.5 hours to remove the GaAs epitaxial substrate with a thickness of 300 microns;

[0031] Step 7: Place the sample with the GaAs epitaxial substrate removed in step 6 in a hydrofluoric acid solution and soak for 5 minutes to remove the Al with a thickness of 500 nanometers. 0.5 Ga 0.5 As corrosion barrier;

[0032] Through the above steps, through the above steps 6 and 7, the epitaxial substrate and the barrier layer can be removed by etching, so as to carry out the subsequent activation process of the photoelectric emission active layer.

[0033] Step 8: Immerse the sample with the corrosion barrier layer removed in step 7 in a mixed solution of sulfuric acid: hydrogen peroxide: deionized water = 4:1:100 by volume, etch for 10-20 seconds, rinse with deionized water, blow dry, and quickly send into an ultra-high vacuum system for high-temperature heating treatment at 650°C;

[0034] Through the above steps, the surface of the photoelectric emission active layer is chemically cleaned, thereby improving the growth quality of the subsequent activation layer.

[0035] Step 9: Activate cesium / oxygen in an ultra-high vacuum system, and grow a cesium / oxygen activation layer with a thickness of 2-3 atomic layers on the GaAs photoelectric emission active layer using a vacuum thermal evaporation deposition method.

[0036] Through the above steps, an activation layer is grown on the surface of the GaAs photoelectric emission active layer, and a negative electron affinity state is obtained on the emission surface, so that the electrons transported to the surface can be effectively emitted into the vacuum.

[0037] The benefits of the present invention are as follows: 1. The film-dielectric resonant cavity enhanced negative electron affinity photocathode of the present invention can enhance the light absorption of the active layer by exciting the standing wave resonance effect. The wavelength corresponding to the resonance absorption peak can be adjusted by changing the thickness of the dielectric cavity, covering the ultraviolet to near-infrared light region. When applied to electron sources, it can enhance the photoelectric emission efficiency of the laser light source at a single wavelength. When applied to the field of photoelectric detection, it can enhance the photoelectric response sensitivity.

[0038] 2. The metal film-dielectric resonant cavity enhanced negative electron affinity photocathode of the present invention can obtain high light absorption by using a very thin active layer under the standing wave resonance effect. The thin active layer has a shorter photoelectron transport distance, which can reduce the influence of various scattering mechanisms on transport, thereby improving the photoelectric response speed and reducing the electron emission degree, effectively improving the photoelectric emission performance of the cathode.

[0039] 3. The metal film-dielectric resonant cavity enhanced negative electron affinity photocathode of the present invention can realize a narrow-band light absorption peak through standing wave resonance, has a high resonant absorption peak quality factor, can effectively filter out harmful photoelectric emission caused by background light, and the surface of the photocathode emission layer is flat, which can reduce the emittance of the electron beam and the dark current of the photodetection, thereby realizing high-quality photoelectric emission.

[0040] 4. The metal film-dielectric resonant cavity enhanced negative electron affinity photocathode of the present invention has a high reflectivity metal film and a dielectric layer prepared by physical and chemical vapor deposition methods respectively, a window layer and a photoelectric emission active layer can be grown and prepared by a mature metal organic chemical vapor deposition method, an activation layer on the surface of the photoelectric emission layer can be deposited and prepared in a high vacuum cavity, and a high reflectivity metal film and a dielectric layer can be made on the back of the photoelectric emission active layer by a wafer bonding flip chip process. This photocathode has a simple structure and process, mature technology, and can be mass-produced to meet the application requirements in the fields of actual low-light detection and imaging, electron sources, etc. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] Figure 1 It is a schematic diagram of the structure of the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode of the present invention.

[0042] Figure 2 The invention relates to the change of the standing wave resonance wavelength of the metal film-dielectric resonance cavity enhanced negative electron affinity photocathode with the thickness of the dielectric resonance cavity.

[0043] Figure 3 It is the absorption spectrum of the photoelectric emission active layer of the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode and the negative electron affinity photocathode without metal film-dielectric resonant cavity of the present invention.

[0044] Figure 4 The present invention discloses a photoelectric response quantum efficiency spectrum of the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode and a negative electron affinity photocathode without a metal film-dielectric resonant cavity.

[0045] Figure 5 It is the photoelectric response time characteristic curve of the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode of the present invention.

[0046] Among them: 1. substrate, 2. high reflectivity metal film, 3. dielectric resonant cavity, 4. window layer, 5. semiconductor photoelectric emission active layer, 6. negative electron affinity activation layer. DETAILED DESCRIPTION

[0047] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the accompanying drawings in the embodiments of the present invention.

[0048] like Figure 1 As shown, the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode includes a substrate 1, a high reflectivity metal film 2, a dielectric resonant cavity 3, a window layer 4, a semiconductor photoelectric emission active layer 5, and a negative electron affinity activation layer 6. The substrate 1, the high reflectivity metal film 2, the dielectric resonant cavity 3, the window layer 4, the semiconductor photoelectric emission active layer 5 and the negative electron affinity activation layer 6 are arranged in sequence from bottom to top.

[0049] The material of substrate 1 is one of silicon (Si), gallium arsenide (GaAs), indium phosphide (InP), gallium phosphide (GaP), gallium nitride (GaN), zinc oxide (ZnO), or one of silicon dioxide (SiO2), silicon nitride (Si3N4), indium tin oxide (ITO), aluminum oxide (Al2O3), and titanium dioxide (TiO2). The thickness of the substrate is between 100 and 3000 microns. Substrate 1 can be bonded with a metal film to support the optical and electrical functional film materials of the photocathode thereon.

[0050] The material of the high-reflectivity metal film 2 is any one of silver (Ag), aluminum (Al), and gold (Au). The thickness of the high-reflectivity metal film is between 100 and 1000 nanometers. The main function of the high-reflectivity metal film is to reflect the incident light, excite the standing wave resonance effect in the medium optical layer, and regulate the optical properties of the photoelectric active layer.

[0051] The dielectric resonant cavity 3 material is silicon dioxide (SiO2), silicon nitride (Si3N4), indium tin oxide (ITO), aluminum oxide (Al2O3), titanium dioxide (TiO2), aluminum gallium arsenide (Al x Ga 1-x As) one of the x Ga 1-x The component x of As is between 0.5 and 1, the thickness of the dielectric resonant cavity is between 100 and 1000 nanometers, and the high-reflectivity metal film and the dielectric resonant cavity together form a standing wave resonant cavity. The standing wave resonance absorption peak wavelength can be adjusted by changing the thickness of the dielectric resonant cavity, and its function is to enhance the narrow-band light absorption in the semiconductor photoelectric emission active layer 5.

[0052] The material of the window layer 4 is aluminum gallium arsenide (Al xGa 1-x As) compound semiconductors, Al x Ga 1-x The As component x is between 0.7 and 1, the doping type is P-type acceptor doping, and the doping concentration is 10 19 cm -3 The thickness of the window layer is between 50 and 100 nanometers, and the growth is prepared by metal organic chemical vapor deposition. The function of the window layer is to form a built-in electric field on the back of the photoelectric emission active layer, reduce the recombination rate of photogenerated carriers on the back, and improve the photoelectric emission efficiency.

[0053] The material of the semiconductor photoelectric emission active layer 5 is Al x Ga 1-x As compound semiconductors, Al x Ga 1-x The As component x is between 0 and 0.5, the doping type is P-type acceptor doping, and the doping concentration is 10 19 cm -3 The thickness of the semiconductor photoelectric emission active layer is between 20 and 1000 nanometers, and it is grown and prepared by metal organic chemical vapor deposition. The function of the semiconductor photoelectric emission active layer is to absorb the incident light, excite electrons in the conduction band, diffuse and transport them to the surface, and then emit them into the vacuum.

[0054] The negative electron affinity activation layer material 5 is selected as a cesium / fluorine or cesium / oxygen film. The thickness of the negative electron affinity activation layer is between 2 and 3 atomic layers. It is used to reduce the conduction band bottom energy level on the upper surface of the semiconductor photoelectric emission active layer to below the vacuum energy level, reaching a negative electron affinity state and realizing electron emission.

[0055] The method for preparing a metal film-dielectric resonant cavity enhanced negative electron affinity photocathode adopts a flip chip process and comprises the following steps:

[0056] Step 1: Select a 3-inch diameter p-type GaAs Epi-ready wafer as the substrate 1 for epitaxial growth, and require its dislocation density to be less than 10 3 cm -3 , the crystal orientation is (100) plane and the (110) plane is cut at 5°, the thickness is 300 microns, and a lattice-matched wafer is selected as the epitaxial substrate 1, which can improve the growth quality of the photoelectric emission active layer thin film;

[0057] Step 2: Use low pressure metal organic chemical vapor deposition to sequentially epitaxially grow Al with a thickness of 500 nanometers on the p-type GaAs epi-ready wafer epitaxial substrate in step 1. 0.5 Ga 0.5 As corrosion barrier layer, thickness of 50 nanometers and P-type doping concentration of 10 19 cm-3 The GaAs photoelectric emission active layer is 5, with a thickness of 50 nanometers and a P-type doping concentration of 10 19 cm -3 Al 0.7 Ga 0.3 As window layer and Al with a thickness of 376 nm 0.7 Ga 0.3 As dielectric resonant cavity, using metal organic chemical vapor deposition method, can achieve high-quality optoelectronic functional thin film materials in large quantities and at low cost;

[0058] Step 3: Using electron beam evaporation in a high vacuum cavity to grow an aluminum (Al) film as a high reflectivity metal layer of the standing wave resonance cavity, the thickness of the Al film is 1000 nanometers. The electron beam evaporation method can achieve mass growth and preparation of high-quality metal reflective films;

[0059] Step 4: Prepare a circular SiO2 single crystal substrate with a diameter of 3 inches, a thickness of 500 microns and double-sided polishing as a wafer bonding substrate. Its purity is required to be higher than 99.9% and the roughness of the polished surface is less than 10 angstroms. Selecting a high-quality polished SiO2 wafer with low roughness can improve the success rate and bonding quality of the bonding process.

[0060] Step 5: Bond the GaAs substrate epitaxial wafer to the SiO2 wafer bonding substrate. The bonding method is anodic bonding. The bonding surface is the upper surface of the high-reflectivity metal layer. The bonding process is a necessary means to make a high-reflectivity metal film on the back of the photocathode. The anodic bonding process can effectively bond the metal to the dielectric / semiconductor substrate. The bonding strength is high and can withstand subsequent high-temperature cleaning processes;

[0061] Step 6: Place the wafer-bonded sample in a nitric acid / hydrogen peroxide solution with a volume ratio of nitric acid to hydrogen peroxide of 1:20 for 1.5 hours to remove the GaAs epitaxial substrate with a thickness of 300 microns;

[0062] Step 7: Place the sample with the GaAs epitaxial substrate removed in step 6 in a hydrofluoric acid solution and soak for 5 minutes to remove the Al with a thickness of 500 nanometers. 0.5 Ga 0.5 As etched barrier layer, the epitaxial substrate and barrier layer can be etched away to facilitate the subsequent activation process of the photoelectric emission active layer;

[0063] Step 8: Immerse the sample with the corrosion barrier layer removed in step 7 in a mixed solution of sulfuric acid: hydrogen peroxide: deionized water = 4:1:100 by volume, etch for 10-20 seconds, rinse with deionized water, blow dry, and quickly send it into an ultra-high vacuum system for high-temperature heating treatment at 650°C to achieve chemical cleaning of the surface of the photoelectric emission active layer and improve the growth quality of the subsequent activation layer;

[0064] Step 9: Activate cesium / oxygen in an ultra-high vacuum system, and grow a cesium / oxygen activation layer with a thickness of 2-3 atomic layers on the GaAs photoelectric emission active layer using a vacuum thermal evaporation deposition method. Grow an activation layer on the surface of the GaAs photoelectric emission active layer, and obtain a negative electron affinity state on the emission surface, so that the electrons transported to the surface can be effectively emitted into the vacuum.

[0065] like Figure 2 The figure shows the variation of the standing wave resonance wavelength of the metal film-dielectric resonance cavity of the metal film-dielectric resonance cavity enhanced negative electron affinity photocathode of the present invention with the thickness of the dielectric resonance cavity. F-P Calculated by the following formula:

[0066]

[0067] In the formula, q F-P is the order of standing wave resonance, n i and H i are the refractive index and thickness of the i-th optical film on the high reflectivity metal film, and They are the phase differences caused by light reflection from the top surface and the bottom surface in the standing wave resonant cavity. Figure 2 for Figure 1 The calculation results of the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode shown in the figure, where the substrate 1 is 500 microns thick SiO2, the high reflectivity metal film 2 is 1000 microns thick Al, and the dielectric resonant cavity 3 is Al 0.7 Ga 0.3 As(Thickness Figure 2 As shown), the window layer 4 has a thickness of 50 nanometers and a doping concentration of 10 19 cm -3 Al 0.7 Ga 0.3 As, the semiconductor photoelectric emission active layer 5 has a thickness of 50 nanometers and a doping concentration of 10 19 cm -3 GaAs. Figure 2 It can be seen that the wavelength of the standing wave resonance varies with the thickness of the dielectric resonance cavity 3, and can cover the entire operating band of the GaAs photocathode from 500 to 800 nanometers. When the thickness of the dielectric resonance cavity is set to 376 nanometers, the 6th, 5th, 4th and 3rd order standing wave resonances are excited at wavelengths of 532 nanometers, 600 nanometers, 708 nanometers and 892 nanometers, respectively.

[0068] like Figure 3The figure shows the absorption spectra of the photoelectric emission active layer of the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode and the negative electron affinity photocathode without metal film-dielectric resonant cavity of the present invention. Figure 3 The thickness of the dielectric resonant cavity 3 of the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode is 376 nanometers, and the other structural parameters are the same as Figure 2 The negative electron affinity photocathode without metal film-dielectric resonant cavity is to replace the high reflectivity metal film 2 and the dielectric resonant cavity 3 of the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode with Al2O3 having a thickness of 500 nanometers. 0.7 Ga 0.3 As obtained by Figure 3 It can be seen that for the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, a dielectric resonant cavity with a thickness of 376 nanometers is selected, and the wavelength of the multi-stage standing wave resonance enhanced light absorption peak realized in the ultra-thin GaAs photoelectric emission active layer 5 with a thickness of 50 nanometers is Figure 2 The calculation results are completely consistent. The 6th-order standing wave resonance excited at a wavelength of 532 nanometers makes the light absorption rate of the ultra-thin GaAs photoelectric emission active layer 5 with a thickness of 50 nanometers exceed 80%. However, for the negative electron affinity photocathode without a metal film-dielectric resonant cavity, the light absorption rate of the 50-nanometer ultra-thin GaAs photoelectric emission active layer 5 is less than 25%. This shows that the use of a metal film-dielectric resonant cavity enhances the light absorption rate at the resonance peak wavelength by more than 3 times.

[0069] like Figure 4 As shown in FIG. 1 , the photoelectric response quantum efficiency of the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode and the negative electron affinity photocathode without metal film-dielectric resonant cavity of the present invention is shown in FIG. 1 , wherein the structural parameters adopted by the two cathodes are the same as those of the negative electron affinity photocathode. Figure 3 The same. As can be seen from the figure, for the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, at the designed target wavelength of 532 nanometers, the photoelectric emission quantum efficiency of the ultra-thin GaAs photoelectric emission active layer 5 with a thickness of 50 nanometers exceeds 40%. For the negative electron affinity photocathode without a metal film-dielectric resonant cavity, the photoelectric emission quantum efficiency of the ultra-thin GaAs photoelectric emission active layer 5 with a thickness of 50 nanometers at the working wavelength of 532 nanometers is 12%. This shows that the use of the metal film-dielectric resonant cavity enhances the photoelectric emission quantum efficiency at the standing wave resonance peak wavelength by more than 3 times.

[0070] like Figure 5 As shown in FIG. 1 , the photoelectric response time characteristic curve of the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode of the present invention, the cathode structure parameters used and Figure 3The same. As can be seen from the figure, for the metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, the time required for the ultra-thin GaAs photoemission active layer 5 with a thickness of 50 nanometers to emit 90% of the electrons at a wavelength of 532 nanometers is only 1.2 picoseconds. Related analysis also shows that the lateral average electron energy of the proposed metal film-dielectric resonant cavity enhanced negative electron affinity photocathode at wavelengths of 532 nanometers and 780 nanometers is approximately 140 millielectron volts and 60 millielectron volts, respectively, which meets the application requirements of electron accelerators, ultrafast electron microscopes and other fields for ultrashort pulses and high-brightness electron sources, and the application requirements of ultrafast detection imaging in the field of low-light detection.

[0071] In summary, the use of high-reflectivity metal film 2 and dielectric resonant cavity 3 can effectively stimulate the standing wave optical resonance effect, and the light absorption rate of the 50-nanometer ultra-thin GaAs photoelectric emission active layer 5 can be increased to more than 3 times the original, thereby enhancing the photoelectric emission quantum efficiency of the photocathode by more than 3 times, and obtaining a picosecond ultrafast photoelectric emission response speed. The improvement of these performances has important practical application value for the development of semiconductor photocathode electron sources with high brightness, ultrashort pulses, and high spin polarization, and high-sensitivity, ultrafast response micro-light detection devices. The metal film-dielectric resonant cavity enhanced negative electron affinity photocathode of the present invention has a three-layer film structure composed of a high-reflectivity metal film, a dielectric resonant cavity film, and a photoelectric emission active layer film. The process flow is simple, the manufacturing difficulty and cost are low, and it is convenient for mass production.

[0072] It should be understood by those skilled in the art that the embodiments of the present invention described above and shown in the accompanying drawings are only examples and do not limit the present invention, and the purpose of the present invention has been fully and effectively achieved. The functional and structural principles of the present invention have been demonstrated and explained in the embodiments, and the embodiments of the present invention may be deformed or modified in any way without departing from the principles.

Claims

1. A metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, comprising a substrate, a high reflectivity metal film, a dielectric resonant cavity, a window layer, a semiconductor photoelectric emission active layer, and a negative electron affinity activation layer, characterized in that: The substrate, the high reflectivity metal film, the dielectric resonant cavity, the window layer, the semiconductor photoelectric emission active layer and the negative electron affinity activation layer are arranged in sequence from bottom to top.

2. A metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, characterized in that: The substrate material is one of silicon (Si), gallium arsenide (GaAs), indium phosphide (InP), gallium phosphide (GaP), gallium nitride (GaN), zinc oxide (ZnO), or one of silicon dioxide (SiO2), silicon nitride (Si3N4), indium tin oxide (ITO), aluminum oxide (Al2O3), and titanium dioxide (TiO2), and the thickness of the substrate is between 100 and 3000 microns.

3. A metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, characterized in that: The high reflectivity metal film material is any one of silver (Ag), aluminum (Al) and gold (Au), and the thickness of the high reflectivity metal film is between 100 and 1000 nanometers.

4. A metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, characterized in that: The dielectric resonant cavity material is silicon dioxide (SiO2), silicon nitride (Si3N4), indium tin oxide (ITO), aluminum oxide (Al2O3), titanium dioxide (TiO2), aluminum gallium arsenide (Al x Ga 1-x As) one of the x Ga 1-x The component x of As is between 0.5 and 1, and the thickness of the dielectric resonance cavity is between 100 and 1000 nanometers.

5. A metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, characterized in that: The window layer material is selected from aluminum gallium arsenide (Al x Ga 1-x As) compound semiconductors, Al x Ga 1-x The As component x is between 0.7 and 1, the doping type is P-type acceptor doping, and the doping concentration is 10 19 cm -3 , the thickness of the window layer is between 50 and 100 nanometers.

6. A metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, characterized in that: The semiconductor photoelectric emission active layer material is selected as Al x Ga 1-x As compound semiconductors, Al x Ga 1-x The As component x is between 0 and 0.5, the doping type is P-type acceptor doping, and the doping concentration is 10 19 cm -3 ; The thickness of the semiconductor photoelectric emission active layer is between 20 and 1000 nanometers.

7. A metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, characterized in that: The negative electron affinity activation layer material is selected as a cesium / fluorine or cesium / oxygen film, the thickness of the negative electron affinity activation layer is between 2 and 3 atomic layers, and the vacuum thermal evaporation deposition method is used in a vacuum degree better than 10 -9 The growth was carried out in a vacuum chamber of 1000 Pa.

8. A method for preparing a metal film-dielectric resonant cavity enhanced negative electron affinity photocathode, which is prepared by a flip chip process, characterized in that: The following steps are involved: Step 1: Select a 3-inch diameter p-type GaAs Epi-ready wafer as the substrate for epitaxial growth, with a dislocation density of less than 10 3 cm -3 , the crystal direction is (100) plane and (110) plane, with a 5° cut, and the thickness is 300 microns; Step 2: Use low pressure metal organic chemical vapor deposition to sequentially epitaxially grow Al with a thickness of 500 nanometers on the p-type GaAs epi-ready wafer epitaxial substrate in step 1. 0.5 Ga 0.5 As corrosion barrier layer, thickness of 50 nanometers and P-type doping concentration of 10 19 cm -3 The GaAs photoelectric emission active layer has a thickness of 50 nanometers and a P-type doping concentration of 10 19 cm -3 Al 0.7 Ga 0.3 As window layer and Al with a thickness of 376 nm 0.7 Ga 0.3 As dielectric resonant cavity; Step 3: using electron beam evaporation in a high vacuum cavity to grow an aluminum (Al) film as a high reflectivity metal layer of the standing wave resonance cavity, the thickness of the Al film being 1000 nanometers; Step 4: Prepare a circular SiO2 single crystal substrate with a diameter of 3 inches, a thickness of 500 microns and double-sided polishing as a wafer bonding substrate, requiring its purity to be higher than 99.9% and the roughness of the polished surface to be less than 10 angstroms; Step 5: Bond the GaAs substrate epitaxial wafer to the SiO2 wafer bonding substrate, the bonding method is anodic bonding, and the bonding surface is the upper surface of the high reflectivity metal layer; Step 6: Place the wafer-bonded sample in a nitric acid / hydrogen peroxide solution with a volume ratio of nitric acid to hydrogen peroxide of 1:20 for 1.5 hours to remove the GaAs epitaxial substrate with a thickness of 300 microns; Step 7: Place the sample with the GaAs epitaxial substrate removed in step 6 in a hydrofluoric acid solution and soak for 5 minutes to remove the Al with a thickness of 500 nanometers. 0.5 Ga 0.5 As corrosion barrier; Step 8: Immerse the sample with the corrosion barrier layer removed in step 7 in a mixed solution of sulfuric acid: hydrogen peroxide: deionized water = 4:1:100 by volume, etch for 10-20 seconds, rinse with deionized water, blow dry, and quickly send into an ultra-high vacuum system for high-temperature heating treatment at 650°C; Step 9: Activate cesium / oxygen in an ultra-high vacuum system, and grow a cesium / oxygen activation layer with a thickness of 2-3 atomic layers on the GaAs photoelectric emission active layer using a vacuum thermal evaporation deposition method.