Full-flexible solar cell array suitable for low-temperature and low-light-intensity environment

By introducing the matching design of the micro-concentrating structure layer and the solar array module into the solar cell array, the problem of the decrease in the output power of the solar cell array in the low temperature and low light intensity environment is solved, and efficient optical convergence and radiation protection are achieved, reducing the The weight and cost of the battery array extend the reliability and life of the spacecraft battery array.

CN118888620APending Publication Date: 2024-11-01HARBIN INST OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410958460.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-17
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The existing solar cell array technology cannot achieve radiation-resistant reinforcement and light concentration design at the same time under low temperature and low light intensity conditions, resulting in a decrease in the output power of the spacecraft cell array, increasing weight and high cost.

Method used

Design a fully flexible solar cell array, consisting of a micro-concentrating structure layer and a solar cell array module, and arrange the micro-structural unit array on the surface or inside the shielding layer through the micro-structural unit array to gather parallel light sources, improve the light intensity, and pass through matching solar cells. Array modules are deployed in the concentrating center to reduce the size and area of ​​the solar cell.

Benefits of technology

It improves the output power of solar cells, reduces the deployment area and weight of solar cells, extends the reliability and service life of solar array systems, and is suitable for low-temperature and low-light intensity environments such as Jupiter orbit and Mars orbit.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118888620A_ABST
    Figure CN118888620A_ABST
Patent Text Reader

Abstract

The invention discloses a full-flexible solar cell array suitable for a low-temperature and low-light-intensity environment, and belongs to the technical field of space energy systems. The invention aims to solve the problem that the existing solar cell array technology cannot realize radiation hardening and condensation design of the cell array at the same time under the conditions of low temperature and low light intensity. The solar cell array is composed of a micro-condensation structure layer and a solar cell array module. The micro-condensation structure layer is composed of a shielding layer and a micro-structure unit. The solar cell array module is formed by connecting solar cells in series or in parallel and adhering the solar cells to the substrate; and the shielding layer of the micro-condensation structure layer is adhered to the surface of one side of a solar cell of the solar cell array module, so that the solar cell corresponds to the condensation center point of the parallel light source converged by the micro-structure unit in position. The full-flexible solar cell array is suitable for a low-temperature and low-light-intensity environment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of space energy systems. Background Art

[0002] With the development of aerospace technology, the mission of exploring the universe has gradually shifted from near-Earth space to deep space. Deep space exploration spacecraft serve in orbits farther away from the Earth, and the light intensity and temperature they receive are lower. For example, the intensity of sunlight in outer space is about 1353W / m 2 In the orbit of Mars, the light intensity drops to about 590W / m 2 , while the light intensity in Jupiter’s orbit is only 46W / m 2 ~54W / m 2 . Spacecraft solar arrays rely on photoelectric conversion to generate electricity, and a decrease in light intensity will lead to a significant drop in the output power of the solar array. Under the condition of meeting the same load power requirements, the spacecraft needs to carry a larger solar array, which greatly increases the weight of the array and is more expensive. At present, solar array technology cannot simultaneously provide radiation-resistant reinforcement and focusing design for the array under low temperature and low light intensity conditions. Therefore, it is of great significance to develop a flexible solar cell power generation system suitable for low temperature, low light intensity and irradiation service environments for deep space exploration missions. Summary of the invention

[0003] The present invention aims to solve the problem that the existing solar cell array technology cannot realize the radiation resistance reinforcement and light focusing design of the cell array under low temperature and low light intensity conditions, and provide a fully flexible solar cell array suitable for low temperature and low light intensity environment.

[0004] A fully flexible solar cell array suitable for low temperature and low light intensity environments, which consists of a micro-concentrating structure layer and a solar cell array module;

[0005] The micro-light-gathering structure layer is composed of a shielding layer and micro-structure units; the micro-structure unit array is arranged on the surface of the shielding layer or the array is arranged inside the shielding layer; when the micro-structure unit array is arranged on the surface of the shielding layer, the distance between adjacent micro-structure units is 5mm to 50mm; when the micro-structure unit array is arranged inside the shielding layer, the micro-structure units are located in the same horizontal plane and in the middle of the shielding layer, and the distance between adjacent micro-structure units is 10mm to 15mm; the micro-structure units are hemispherical, spherical, convex lens-shaped or cylindrical; the diameter of the hemispherical shape is 5mm to 50mm; the diameter of the spherical shape is 5mm to 50mm; the focal length of the convex lens shape is 1mm to 15mm; the height of the cylindrical shape is 1mm to 20mm, and the diameter is 10mm to 100mm;

[0006] The solar cell array module is a solar cell array module that is connected in series or in parallel and bonded to a substrate;

[0007] The shielding layer of the micro-light-concentrating structure layer is bonded to the surface of one side of the solar cell of the solar cell array module, so that the solar cell corresponds to the focusing center point where the parallel light source converges through the micro-structure unit.

[0008] The beneficial effects of the present invention are:

[0009] 1. The present invention converts weak sunlight into high-intensity light beams through the focusing effect of the micro-light-concentrating structure layer, and can adjust the concentration ratio and the size of the optical convergence center by adjusting the size of the micro-structure unit and the doping ratio, thereby increasing the intensity of light entering the solar cell and thus increasing the output power of the solar cell per unit area. In addition, the micro-light-concentrating structure layer encapsulated on the surface of the flexible solar cell array also has the function of radiation protection.

[0010] 2. The present invention designs a solar cell array module that matches the micro-concentrating structure layer and deploys solar cells of the same size as the focusing center at the focusing center. Since the focusing spot is smaller, the size of the solar cells in this system is smaller than that of traditional spacecraft solar cells, thereby significantly reducing the weight and cost while reducing the solar cell deployment area.

[0011] 3. The present invention can significantly reduce the use area of ​​solar cells compared with traditional design solutions by matching the micro-concentrating structure layer and the solar cell array module under the same power output conditions. Space solar cell arrays are subject to harsh space radiation environments during service. Reducing the use area of ​​solar cells can reduce the radiation dose received by the array, delay the damage and degradation of solar cells, and thus significantly improve the operational reliability and service life of the solar cell array system.

[0012] 4. The fully flexible solar cell array of the present invention can be used in low-temperature service environments of -250°C to 50°C and low-light intensity environments (low-light intensity environments refer to light intensity less than the standard spectrum AM0 outside the Earth's atmosphere), such as Jupiter orbit and Mars orbit.

[0013] The present invention is used for a fully flexible solar cell array suitable for low temperature and low light intensity environment. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 This is a schematic structural diagram of the micro-light-concentrating structure layer described in Example 1;

[0015] Figure 2 The incident light intensity is 50W / m 2When, the embodiment 1 is applicable to the light intensity distribution of the parallel light source of the fully flexible solar cell array in the low temperature and low light intensity environment after passing through the micro-light-concentrating structure layer, 1 is a hemispherical shape, 2 is a shielding layer, 3 is a solar cell, and 4 is a substrate;

[0016] Figure 3 The incident light intensity is 100W / m 2 When, the second embodiment is applicable to the light intensity distribution of the parallel light source of the fully flexible solar cell array in a low temperature and low light intensity environment after passing through the micro-concentrating structure layer;

[0017] Figure 4 The incident light intensity is 100W / m 2 When the IV curves of the fully flexible solar cell array suitable for low temperature and low light intensity environment in Example 1 and the solar cell array encapsulated by the pseudo-shaped glass cover sheet in the comparative experiment are shown in Figure 1, and Figure 2 is the comparative experiment. DETAILED DESCRIPTION

[0018] The technical solution of the present invention is not limited to the specific implementation modes listed below, but also includes any combination of the specific implementation modes.

[0019] Specific implementation method 1: This implementation method is a fully flexible solar cell array suitable for low temperature and low light intensity environment, which is composed of a micro-concentrating structure layer and a solar cell array module;

[0020] The micro-light-gathering structure layer is composed of a shielding layer and micro-structure units; the micro-structure unit array is arranged on the surface of the shielding layer or the array is arranged inside the shielding layer; when the micro-structure unit array is arranged on the surface of the shielding layer, the distance between adjacent micro-structure units is 5mm to 50mm; when the micro-structure unit array is arranged inside the shielding layer, the micro-structure units are located in the same horizontal plane and in the middle of the shielding layer, and the distance between adjacent micro-structure units is 10mm to 15mm; the micro-structure units are hemispherical, spherical, convex lens-shaped or cylindrical; the diameter of the hemispherical shape is 5mm to 50mm; the diameter of the spherical shape is 5mm to 50mm; the focal length of the convex lens shape is 1mm to 15mm; the height of the cylindrical shape is 1mm to 20mm, and the diameter is 10mm to 100mm;

[0021] The solar cell array module is a solar cell array module that is connected in series or in parallel and bonded to a substrate;

[0022] The shielding layer of the micro-light-concentrating structure layer is bonded to the surface of one side of the solar cell of the solar cell array module, so that the solar cell corresponds to the focusing center point where the parallel light source converges through the micro-structure unit.

[0023] In this specific implementation method, the micro-light-concentrating structure layer needs to be set with alignment mark points during the design process; the micro-light-concentrating structure layer is designed, and the spectral distribution of the incident light source after passing through the micro-light-concentrating structure layer is calculated, and then the solar cell array module is designed according to the spectral distribution characteristics; the spectral distribution includes the focusing position, focusing shape and focusing size; the solar cell array module is set with alignment mark points corresponding to the micro-light-concentrating structure layer during the design process. The micro-light-concentrating structure layer and the solar cell array module are bonded and bonded by an adhesive, wherein the alignment between the two is ensured by relying on the alignment mark points pre-set in the micro-light-concentrating structure layer and the solar cell array module.

[0024] The beneficial effects of this embodiment are:

[0025] 1. This embodiment converts weak sunlight into high-intensity light beams through the focusing effect of the micro-light-concentrating structure layer, and can adjust the concentration ratio and the size of the optical convergence center by adjusting the size of the micro-structure unit and the doping ratio, thereby increasing the intensity of light entering the solar cell and thus increasing the output power of the solar cell per unit area. In addition, the micro-light-concentrating structure layer encapsulated on the surface of the flexible solar cell array also has the function of radiation protection.

[0026] 2. This embodiment designs a solar cell array module that matches the micro-concentrating structure layer and deploys solar cells of the same size as the focusing center at the focusing center. Since the focusing spot is smaller, the size of the solar cells in this system is smaller than that of traditional spacecraft solar cells, thereby significantly reducing the weight and cost while reducing the solar cell deployment area.

[0027] 3. This embodiment can significantly reduce the use area of ​​solar cells compared with traditional design solutions by matching the micro-concentrating structure layer and the solar cell array module under the same power output conditions. Space solar cell arrays are subject to harsh space radiation environments during service. Reducing the use area of ​​solar cells can reduce the radiation dose received by the array, delay the damage and degradation of solar cells, and thus significantly improve the operational reliability and service life of the solar cell array system.

[0028] 4. The fully flexible solar cell array of this embodiment can be used in low-temperature service environments of -250°C to 50°C and low-light intensity environments (low-light intensity environments refer to light intensity less than the standard spectrum AM0 outside the Earth's atmosphere), such as Jupiter orbit and Mars orbit.

[0029] Specific implementation example 2: This implementation example is different from specific implementation example 1 in that the solar cell is a silicon solar cell, a gallium arsenide solar cell, a perovskite solar cell or a copper indium gallium selenide solar cell. The rest is the same as specific implementation example 1.

[0030] Specific embodiment 3: This embodiment is different from specific embodiment 1 or 2 in that the material of the shielding layer and the microstructure unit is quartz, cerium-doped quartz, borosilicate, cerium-doped borosilicate, silicone rubber, transparent polyimide, polytetrafluoroethylene, ethylene-tetrafluoroethylene copolymer, polyester film, epoxy resin and polysilsesquioxane, or a combination of several of them. The rest is the same as specific embodiment 1 or 2.

[0031] Specific implementation method 4: This implementation method is different from specific implementation methods 1 to 3 in that the microstructure unit is a solid structure or a hollow structure. The rest is the same as specific implementation methods 1 to 3.

[0032] Specific embodiment 5: This embodiment differs from specific embodiments 1 to 4 in that: when the microstructure unit array is arranged on the surface of the shielding layer, the thickness of the shielding layer is 0.06 mm to 0.2 mm; when the microstructure unit array is arranged inside the shielding layer, the thickness of the shielding layer is ≥ the maximum size of the microstructure unit. Other aspects are the same as specific embodiments 1 to 4.

[0033] Specific implementation example 6: This implementation example is different from specific implementation examples 1 to 5 in that the solar cell and the light-concentrating center point have the same shape and size. The rest is the same as specific implementation examples 1 to 5.

[0034] Specific embodiment 7: This embodiment differs from any one of specific embodiments 1 to 6 in that: when the microstructure unit array is arranged on the surface of the shielding layer, the microstructure unit is bonded to the surface of the shielding layer by an adhesive and then combined by a lamination process; the lamination process is specifically carried out in the following steps: applying pressure on both the upper and lower sides, and at a vacuum degree of 1×10 -3 Pa~1×10 -4 Pa, room temperature, upper pressure of 50kPa ~ 150kPa and lower pressure of 50kPa ~ 150kPa, lamination for 30min ~ 60min, after lamination, at room temperature and vacuum degree of 1×10 -3 Pa~1×10 -4 Pa, and the curing time is 36 to 72 hours. The other steps are the same as those in the first to sixth embodiments.

[0035] Specific embodiment 8: This embodiment differs from specific embodiments 1 to 7 in that the solar cell is bonded to the substrate by an adhesive and then combined by a lamination process; the lamination process is specifically carried out in the following steps: ① Apply pressure on both the upper and lower sides, and at a vacuum degree of 1×10 -3 Pa~1×10 -4Pa, the first lamination temperature is 50℃~150℃, the upper pressure is 30kPa~150kPa and the lower pressure is 30kPa~150kPa, and the lamination is performed for 45min~60min;

[0036] ② Wait until the temperature drops to room temperature for the second lamination, apply pressure on the upper side, and keep the vacuum at 1×10 -3 Pa~1×10 -4 Pa, room temperature and upper pressure of 50kPa to 100kPa, lamination for 15min to 30min;

[0037] ③ Apply pressure on the lower side and keep the vacuum at 1×10 -3 Pa~1×10 -4 Pa, room temperature and lower side pressure of 50kPa ~ 100kPa, lamination for 15min ~ 30min;

[0038] ④ After lamination, at room temperature and vacuum degree of 1×10 -3 Pa~1×10 -4 Pa, and the curing time is 48 to 96 hours. The other steps are the same as those in the first to seventh embodiments.

[0039] Specific embodiment 9: This embodiment differs from any one of specific embodiments 1 to 8 in that the shielding layer of the micro-concentrating structure layer is bonded to the surface of one side of the solar cell of the solar cell array module by an adhesive and then combined by a lamination process; the lamination process is specifically carried out in the following steps: applying pressure on both the upper and lower sides, and in a vacuum degree of 1×10 -3 Pa~1×10 -4 Pa, lamination temperature of 50 ℃ ~ 150 ℃, upper pressure of 30 kPa ~ 150 kPa and lower pressure of 30 kPa ~ 150 kPa, lamination for 30 min ~ 120 min, after lamination at room temperature and vacuum degree of 1 × 10 -3 Pa~1×10 -4 Pa, and the curing time is 36 to 72 hours. The other steps are the same as those in the first to eighth embodiments.

[0040] Specific embodiment 10: This embodiment differs from specific embodiments 1 to 9 in that the adhesive is silicone rubber, resin glue, polytetrafluoroethylene glue, transparent polyimide glue or EVA glue. Other aspects are the same as specific embodiments 1 to 9.

[0041] The following examples are used to verify the beneficial effects of the present invention:

[0042] Embodiment 1, combined with Figure 1 Specific instructions:

[0043] A fully flexible solar cell array suitable for low temperature and low light intensity environments, which consists of a micro-concentrating structure layer and a solar cell array module;

[0044] The micro-light-concentrating structure layer is composed of a shielding layer and micro-structure units; the micro-structure unit array is arranged on the surface of the shielding layer, and the distance between adjacent micro-structure units is 7.5 mm; the micro-structure unit is hemispherical; the hemispherical diameter is 40 mm; the micro-structure array is a solid structure; the thickness of the shielding layer is 0.12 mm;

[0045] The solar cell array module is a module that uses an interconnection sheet to connect 20 solar cells in series and bond them to a substrate; the substrate is 0.2 mm thick and made of polyimide;

[0046] The shielding layer of the micro-light-concentrating structure layer is bonded to the surface of one side of the solar cell of the solar cell array module, so that the solar cell corresponds to the focusing center point where the parallel light source passes through the micro-structure unit, and the solar cell and the focusing center point have the same shape and size;

[0047] The solar cell is a GaInP / GaAs / Ge TJ-30 triple-junction solar cell produced by the 18th Institute of China Electronics Technology Group Corporation. Using the GB / T 6494-2017 aerospace solar cell electrical performance test method, the open circuit voltage of the single solar cell is measured to be 2.75V, the short circuit current is 0.22A, the maximum power point is 0.4887W, the photoelectric conversion efficiency is 31.57%, and the thickness is about 120μm.

[0048] The shielding layer and the microstructure unit are both made of silicone rubber (company: Dow Corning, model: DC-900).

[0049] When the microstructure unit array is arranged on the surface of the shielding layer, the microstructure unit is bonded to the surface of the shielding layer through silicone rubber (company: Dow Corning, model: DC-900), and then combined through a lamination process; the lamination process is specifically carried out in the following steps: applying pressure on both the upper and lower sides, and at a vacuum degree of 1×10 -4 Pa, room temperature, upper pressure of 50 kPa and lower pressure of 50 kPa, lamination for 40 min, after lamination, at room temperature and vacuum degree of 1 × 10 -4 Pa, and cured for 72h.

[0050] The solar cell is bonded to the substrate by silicone rubber (company: Dow Corning, model: DC-900) and then combined by lamination process; the lamination process is specifically carried out in the following steps: ① Apply pressure on both the upper and lower sides, and at a vacuum degree of 1×10 -4Pa, the first lamination temperature is 80 ° C, the upper pressure is 100 kPa and the lower pressure is 100 kPa, and the lamination is performed for 50 minutes;

[0051] ② Wait until the temperature drops to room temperature for the second lamination, apply pressure on the upper side, and keep the vacuum at 1×10 -4 Pa, room temperature and upper pressure of 50 kPa, lamination for 20 min;

[0052] ③ Apply pressure on the lower side and keep the vacuum at 1×10 -4 Pa, room temperature and lower side pressure of 50kPa, lamination for 30min;

[0053] ④ After lamination, at room temperature and vacuum degree of 1×10 -4 Pa, and cured for 72h.

[0054] The shielding layer of the micro-concentrating structure layer is bonded to the surface of one side of the solar cell of the solar cell array module by an adhesive (company: Dow Corning, model: 93-076-2RF), and then combined by a lamination process; the lamination process is specifically carried out in the following steps: applying pressure on both the upper and lower sides, and in a vacuum degree of 1×10 -4 Pa, lamination temperature of 100 ° C, upper pressure of 40 kPa and lower pressure of 50 kPa, lamination for 45 min, after lamination at room temperature and vacuum degree of 1 × 10 - 4 Pa, and cured for 72h.

[0055] When a microstructure unit is involved in the lamination process, the surface of the microstructure unit is protected by lamination through a mold having the same shape as the microstructure unit.

[0056] According to calculations, in this embodiment, the focal point where the parallel light source converges through the microstructure unit is a circle with a diameter of 10 mm.

[0057] Embodiment 2: This embodiment is different from Embodiment 1 in that: the diameter of the hemispherical shape is 40 mm; the thickness of the shielding layer is 0.1 mm; the solar cell is a Si-HE solar cell produced by TCL, and the open circuit voltage of the single solar cell is 0.65 V, the short circuit current is 1.072 A, the maximum power point is 0.6221 W, the photoelectric conversion efficiency is 21.33%, and the thickness is about 200 μm. Others are the same as Embodiment 1.

[0058] According to calculations, in this embodiment, the focal point where the parallel light sources converge through the microstructure unit is a circle with a diameter of 15 mm.

[0059] Embodiment 3: This embodiment is different from Embodiment 1 in that: the microstructure unit array is arranged inside the shielding layer, the microstructure units are located in the same horizontal plane and in the middle of the shielding layer, and the distance between adjacent microstructure units is 10 mm; the thickness of the shielding layer is 7.5 mm; the shielding layer is DC-300 silicone rubber produced by Dow Corning; the microstructure unit is spherical; the diameter of the sphere is 5 mm. Others are the same as Embodiment 1.

[0060] According to calculations, in this embodiment, the focal point where the parallel light source converges through the microstructure unit is a circle with a diameter of 1.5 mm.

[0061] Comparative experiment: The difference between this comparative experiment and Example 1 is that a pseudo-glass cover is used to replace the micro-condensing structure layer to obtain a solar cell array encapsulated by a pseudo-glass cover; the material of the pseudo-glass cover is a mixture of cerium-containing glass microspheres and silicone rubber; the cerium element percentage content of the cerium-containing glass microspheres is 2.5%; the particle size of the cerium-containing glass microspheres is 38.5 μm; the mass ratio of the cerium-containing glass microspheres to the silicone rubber is 1.5:1; the silicone rubber is purchased from DC-900 silicone rubber produced by Dow Corning. The rest is the same as Example 1.

[0062] According to calculations, in this embodiment, the focal point where the parallel light source converges through the microstructure unit is a circle with a diameter of 16 μm.

[0063] Figure 2 The incident light intensity is 50W / m 2 Embodiment 1 is suitable for the light intensity distribution of the fully flexible solar cell array parallel light source in low temperature and low light intensity environment after passing through the micro-light-concentrating structure layer. 1 is a hemispherical shape, 2 is a shielding layer, 3 is a solar cell, and 4 is a substrate. As can be seen from the figure, when the incident light intensity is 50W / m 2 When the light intensity at the center of the convergence is Gaussian, the light intensity at the center is 2500W / m 2 , the focusing ratio is about 50 times.

[0064] When the incident light intensity is 100W / m 2 When the parallel light source of the fully flexible solar cell array suitable for low temperature and low light intensity environment passes through the micro-concentrating structure layer, the illumination intensity at the center point is 5000W / m 2 .

[0065] When the incident light intensity is 50W / m 2 When the parallel light source of the fully flexible solar array in the second embodiment is applied to low temperature and low light intensity environment, the illumination intensity at the center point is 2500W / m 2 .

[0066] Figure 3The incident light intensity is 100W / m 2 Embodiment 2 is applicable to the light intensity distribution of the fully flexible solar array parallel light source after passing through the micro-concentrating structure layer in a low temperature and low light intensity environment; as can be seen from the figure, when the incident light intensity is 100W / m 2 When the light intensity at the center of the convergence is Gaussian, the light intensity at the center is 5000W / m 2 , the focusing ratio is about 50 times.

[0067] When the incident light intensity is 588.6W / m 2 When the parallel light source of the fully flexible solar cell array suitable for low temperature and low light intensity environment passes through the micro-concentrating structure layer, the illumination intensity at the center point is 10000W / m 2 .

[0068] When the incident light intensity is 50W / m 2 When the short circuit current of the fully flexible solar cell array in the first embodiment suitable for low temperature and low light intensity environment is 1.9A, the output power is 147.53W.

[0069] Figure 4 The incident light intensity is 100W / m 2 1 is the IV curve of the fully flexible solar cell array for low temperature and low light intensity environment in Example 1 and the solar cell array encapsulated by pseudo-glass cover in the comparative experiment. 1 is Example 1 and 2 is the comparative experiment. The solar cell arrays in the two experiments have the same cell area and number of cells. When the incident light intensity is 100W / m 2 When the comparison test is carried out, the short-circuit current of the solar cell array encapsulated with the pseudo-glass cover is 0.48A, and the output power is 3.24W; the short-circuit current of the fully flexible solar cell array suitable for low temperature and low light intensity environment in Example 1 is 47.2A, and the output power is 305.86W. If the power generation of the comparison test is the same as that of Example 1, the number and area of ​​the cells in the comparison test are 98 times that of Example 1.

[0070] The incident light intensity is 50W / m 2 In the comparative experiment, the short-circuit current of the solar cell array encapsulated with the pseudo-glass cover is 1.28A, and the output power is 23.57W; the short-circuit current of the fully flexible solar cell array suitable for low temperature and low light intensity environment in Example 2 is 58.32A, and the output power is 158.86W.

[0071] The incident light intensity is 100W / m 2 When the short circuit current of the fully flexible solar cell array in the second embodiment suitable for low temperature and low light intensity environment is 2.51A, the output power is 302.12W.

[0072] In the simulated Mars orbit on the ground (irradiance is about 588.6W / m 2, the temperature is about -120℃), in the comparative experiment, the short-circuit current of the solar cell array encapsulated with the pseudo-glass cover is 0.38A, the output power is 48.77W, and the operating temperature of the cell array is -32℃. The short-circuit current of the fully flexible solar cell array suitable for low temperature and low light intensity environment in embodiment 3 is 6.46A, the output power is 731.55W, and the operating temperature of the cell array is 37℃.

[0073] Table 1 shows the fully flexible solar cell array for low temperature and low light intensity environment in Example 1 and the solar cell array encapsulated by pseudo-glass cover in the comparative experiment with an injection of 1×10 15 e / cm 2 And the normalized data of electrical properties before and after 1MeV electron irradiation; when the incident light intensity is 100W / m 2 When, before irradiation, the short-circuit current of the solar cell array encapsulated with the pseudo-glass cover in the comparative experiment was 0.048A, the open-circuit voltage was 2.75V, and the maximum power was 3.24W; after electron irradiation, the short-circuit current was 0.038A, the open-circuit voltage was 2.28V, and the maximum power was 2.39W. Before irradiation, the short-circuit current of the fully flexible solar cell array suitable for low-temperature and low-light-intensity environments in Example 1 was 4.2A, the open-circuit voltage was 2.73V, and the maximum power was 305.86W; after irradiation, the short-circuit current was 3.55A, the open-circuit voltage was 2.31V, and the maximum power was 248.73W. It can be seen from the table that the radiation resistance of the solar cell array of Example 1 is significantly better than that of the solar cell array prepared by the comparative test method.

[0074] Table 1 Electrical performance degradation results of two solar cell arrays after 1MeV electron irradiation

[0075] Open circuit voltage degradation Short circuit current degradation Maximum power point degradation Embodiment 1 82.90% 79.17% 73.77% Comparative test 84.62% 84.52% 81.32%

Claims

1. A fully flexible solar cell array suitable for low temperature and low light intensity environments, Features It consists of a micro-concentrating structure layer and a solar cell array module; The micro-light-gathering structure layer is composed of a shielding layer and micro-structure units; the micro-structure unit array is arranged on the surface of the shielding layer or the array is arranged inside the shielding layer; when the micro-structure unit array is arranged on the surface of the shielding layer, the distance between adjacent micro-structure units is 5mm to 50mm; when the micro-structure unit array is arranged inside the shielding layer, the micro-structure units are located in the same horizontal plane and in the middle of the shielding layer, and the distance between adjacent micro-structure units is 10mm to 15mm; the micro-structure units are hemispherical, spherical, convex lens-shaped or cylindrical; the diameter of the hemispherical shape is 5mm to 50mm; the diameter of the spherical shape is 5mm to 50mm; the focal length of the convex lens shape is 1mm to 15mm; the height of the cylindrical shape is 1mm to 20mm, and the diameter is 10mm to 100mm; The solar cell array module is a solar cell array module that is connected in series or in parallel and bonded to a substrate; The shielding layer of the micro-light-concentrating structure layer is bonded to the surface of one side of the solar cell of the solar cell array module, so that the solar cell corresponds to the focusing center point where the parallel light source converges through the micro-structure unit.

2. According to claim 1, a fully flexible solar cell array suitable for low temperature and low light intensity environment, Features The solar cell is a silicon solar cell, a gallium arsenide solar cell, a perovskite solar cell or a copper indium gallium selenide solar cell.

3. According to claim 1, a fully flexible solar cell array suitable for low temperature and low light intensity environment, Features The materials of the shielding layer and the microstructure unit are quartz, cerium-doped quartz, borosilicate, cerium-doped borosilicate, silicone rubber, transparent polyimide, polytetrafluoroethylene, ethylene-tetrafluoroethylene copolymer, polyester film, epoxy resin and polysilsesquioxane, or a combination of several of them.

4. According to claim 1, a fully flexible solar cell array suitable for low temperature and low light intensity environment, Features The microstructure unit is a solid structure or a hollow structure.

5. According to claim 1, a fully flexible solar cell array suitable for low temperature and low light intensity environment, Features When the microstructure unit array is arranged on the surface of the shielding layer, the thickness of the shielding layer is 0.06 mm to 0.2 mm; when the microstructure unit array is arranged inside the shielding layer, the thickness of the shielding layer is ≥ the maximum size of the microstructure unit.

6. A fully flexible solar cell array suitable for low temperature and low light intensity environments according to claim 1, Features The solar cell has the same shape and size as the focusing center point.

7. A fully flexible solar cell array suitable for low temperature and low light intensity environments according to claim 1, Features When the microstructure unit array is arranged on the surface of the shielding layer, the microstructure unit is bonded to the surface of the shielding layer by an adhesive and then combined by a lamination process; the lamination process is specifically carried out in the following steps: applying pressure on both the upper and lower sides, and at a vacuum degree of 1×10 -3 Pa~1×10 -4 Pa, room temperature, upper pressure of 50kPa ~ 150kPa and lower pressure of 50kPa ~ 150kPa, lamination for 30min ~ 60min, after lamination at room temperature and vacuum degree of 1×10 -3 Pa~1×10 -4 Pa, and cure for 36 to 72 hours.

8. A fully flexible solar cell array suitable for low temperature and low light intensity environments according to claim 1, Features The solar cell is bonded to the substrate by adhesive and then combined by lamination process; the lamination process is specifically carried out in the following steps: ① Apply pressure on both the upper and lower sides, and at a vacuum degree of 1×10 -3 Pa~1×10 -4 Pa, the first lamination temperature is 50℃~150℃, the upper pressure is 30kPa~150kPa and the lower pressure is 30kPa~150kPa, and the lamination is performed for 45min~60min; ② Wait until the temperature drops to room temperature for the second lamination, apply pressure on the upper side, and keep the vacuum at 1×10 -3 Pa~1×10 -4 Pa, room temperature and upper pressure of 50kPa to 100kPa, lamination for 15min to 30min; ③ Apply pressure on the lower side and keep the vacuum at 1×10 -3 Pa~1×10 -4 Pa, room temperature and lower side pressure of 50kPa ~ 100kPa, lamination for 15min ~ 30min; ④ After lamination, at room temperature and vacuum degree of 1×10 -3 Pa~1×10 -4 Pa, curing time is 48h to 96h.

9. A fully flexible solar cell array suitable for low temperature and low light intensity environments according to claim 1, Features The shielding layer of the micro-concentrating structure layer is bonded to the surface of one side of the solar cell of the solar cell array module by an adhesive, and then combined by a lamination process; the lamination process is specifically carried out in the following steps: applying pressure on both the upper and lower sides, and in a vacuum degree of 1×10 -3 Pa~1×10 -4 Pa, lamination temperature of 50 ℃ ~ 150 ℃, upper pressure of 30 kPa ~ 150 kPa and lower pressure of 30 kPa ~ 150 kPa, lamination for 30 min ~ 120 min, after lamination at room temperature and vacuum degree of 1 × 10 -3 Pa~1×10 -4 Pa, and cure for 36 to 72 hours.

10. A fully flexible solar cell array suitable for low temperature and low light intensity environments according to claim 7, 8 or 9, Features The adhesive is silicone rubber, resin glue, polytetrafluoroethylene glue, transparent polyimide glue or EVA glue.