Laminated structure of glass antenna and manufacturing method thereof
Through multi-layer structure design and process optimization, the performance problems of glass antennas in high temperature and electromagnetic interference environments are solved, and efficient signal reception and anti-interference capabilities are achieved, which are suitable for various scenarios such as buildings and automobiles.
Patent Information
- Application Number
- CN202411297672.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-18
- Publication Date
- 2024-11-01
AI Technical Summary
The performance of existing glass antennas is degraded in high temperature and electromagnetic interference environments, especially in sun exposure and multi-signal environments, which is difficult to meet the needs of various usage scenarios such as buildings and automobiles.
Using a multi-layer structure design, including the first glass, the first adhesive layer, the frequency selective surface layer and the second glass, the frequency selective surface layer is composed of polymethyl methacrylate, polydimethylsiloxane and gallium indium alloy liquid It is made of metal, and the bonding strength and signal shielding ability are improved through processes such as roller pressing and laser cutting, and the AF film is coated on the glass surface.
It significantly improves the anti-interference capability and service life of glass antennas, ensures signal transmission and reception performance in high temperature and multi-signal environments, simplifies the manufacturing process, reduces energy consumption and improves product consistency and aesthetics.
Smart Images

Figure CN118889063A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of glass antenna manufacturing, and in particular to a laminated structure of a glass antenna and a manufacturing method thereof. Background Art
[0002] Glass antenna refers to an antenna form that integrates antenna functions on the surface or inside of glass. This antenna technology is mainly used in many fields such as automobiles, construction and telecommunications to meet the communication and signal transmission needs in different scenarios.
[0003] However, problems such as high temperature and electromagnetic interference faced by glass antennas during manufacturing and use will affect the performance of glass antennas. Existing glass antennas experience high temperature environments during the manufacturing process, which causes differences between the antenna line area of the glass antenna and the design, thus affecting the performance of the glass antenna. In addition, when glass antennas are used in certain scenarios, such as when glass antennas are used on glass curtain walls of buildings, the temperature of the glass antenna may be too high under the sun, which will also affect the performance of the glass antenna. In addition, glass antennas are also widely used in the automotive field. Especially with the continuous development of unmanned driving technology, vehicles need to collect a lot of information to drive, including road vehicle information, surrounding traffic information, pedestrian information, etc. However, electromagnetic signals emitted by other vehicles or electronic devices in the environment will interfere with the signal reception of the glass antenna.
[0004] Therefore, designing a glass antenna that has excellent communication performance, can effectively cope with high temperature and electromagnetic interference, has the ability to receive signals at specific angles and frequency bands, and can meet multiple usage scenarios including building glass curtain walls and automobiles is an important challenge in the current field. Summary of the invention
[0005] In order to solve the problems existing in the above background technology, the first aspect of the present invention provides a laminated structure of a glass antenna, which mainly includes: First glass, first adhesive layer, frequency selective surface layer, antenna layer, second glass.
[0006] The first glass comprises a first surface and a second surface, the second surface being used for fixedly connecting the frequency selective surface layer through the first adhesive layer; The frequency selective surface layer is composed of three layers of transparent material, the middle layer of the three layers of transparent material is polymethyl methacrylate, the top layer and the bottom layer of the three layers of transparent material are both polydimethylsiloxane, the top layer and / or the bottom layer are provided with a channel, and the channel is provided with liquid metal; The antenna layer comprises an antenna substrate layer, a metal foil layer, and a second adhesive layer, wherein the second adhesive layer is used to bond the antenna substrate layer and the metal foil layer; The second glass includes a third surface and a fourth surface.
[0007] Furthermore, the thickness of the frequency selective surface layer is ,in The frequency selective surface layer selects the wavelength of the electromagnetic wave to be transmitted. is the dielectric constant of the middle layer, n is a positive integer, The frequency selective surface layer selects the incident angle of the electromagnetic wave to be transmitted.
[0008] Furthermore, projections of the channels of the top layer and the channels of the bottom layer on the frequency selective surface layer are orthogonal to each other.
[0009] Furthermore, the liquid metal is a gallium-indium alloy.
[0010] Furthermore, the mass fraction of gallium in the gallium-indium alloy is 70% to 80%, and the mass fraction of indium is 20% to 30%.
[0011] Furthermore, the cross-sectional shape of the channel is rectangular, the width L of the channel cross-sectional shape is ≥ 0.5 mm, and the height h of the channel cross-sectional shape is ≥ 0.6 mm.
[0012] Furthermore, the second adhesive layer is UV glue.
[0013] Furthermore, the antenna substrate layer and the metal foil layer are rolled and bonded to each other by a rolling mechanism, and the metal foil layer forms an antenna line area on the antenna substrate layer.
[0014] Furthermore, the first surface of the first glass and the surface of the second glass away from the first glass are both provided with AF films.
[0015] Compared with the prior art, the laminated structure of the glass antenna provided in the first aspect of the present invention has the following beneficial effects: The laminated structure of the glass antenna in the first aspect of the present invention mainly includes a first glass, a first adhesive layer, a frequency selective surface layer, an antenna layer, and a second glass. By carefully combining and optimizing the materials of each layer, especially introducing a frequency selective surface layer with unique properties, the various properties of the glass antenna can be greatly improved. Among them, the first glass and the second glass are the inner and outer layers of the laminated structure of the glass antenna, providing the necessary structural support and light transmittance; secondly, the frequency selective surface layer is specifically designed, and the frequency selective surface layer has optical transparency and can selectively transmit or reflect electromagnetic waves of a specific frequency. While maintaining high light transmittance, it also has high-pass filtering properties, can pass through selected electromagnetic wave signals, and can shield other electromagnetic signals, including infrared rays, etc., which can significantly improve the anti-interference ability of the glass antenna and the performance of use under high temperature conditions under sunlight exposure, and significantly improve the service life of the glass antenna; in addition, the design of the antenna layer is closely coordinated with the frequency surface selection layer, thereby ensuring efficient transmission and reception of signals.
[0016] In order to solve the technical problems existing in the background technology, the second aspect of the present invention provides a method for manufacturing a laminated structure of a glass antenna, which is used to manufacture the laminated structure of the glass antenna in the first aspect of the present invention. The method for manufacturing the laminated structure of the glass antenna comprises the following steps: 1) The metal foil layer is arranged on one side of the antenna substrate layer, and a second adhesive layer is applied to the side of the metal foil layer close to the antenna substrate layer according to the shape of the antenna line area, and the metal foil layer is initially cured to the antenna substrate layer by ultraviolet light to form an antenna composite layer; 2) rolling the antenna composite layer by a rolling mechanism, wherein the rolling shape of the rolling mechanism coincides with the shape of the antenna line area, so that the metal foil layer is solidified again on the antenna substrate layer and forms an antenna line area; 3) Performing laser cutting and / or die cutting on the antenna line area and the non-antenna line area on the antenna composite layer, and then separating and recovering the non-antenna line area by negative pressure adsorption using a negative pressure adsorption device, and performing quality inspection on the antenna line area; 4) calculating and designing the thickness of the frequency selective surface layer according to the wavelength of the electromagnetic wave selectively transmitted by the frequency selective surface layer, the incident angle and the dielectric constant of the intermediate layer, and injecting liquid metal into the channel provided in the top layer and / or the bottom layer of the frequency selective surface layer, wherein the liquid metal is a gallium-indium alloy; 5) The first glass, the first adhesive layer, the frequency selective surface layer, the antenna layer, and the second glass are pressed and bonded together by a pressing and bonding device, and an AF film is coated on the first surface of the first glass and the surface of the second glass away from the first glass.
[0017] Compared with the prior art, the method for manufacturing the laminated structure of the glass antenna provided in the second aspect of the present invention has the following beneficial effects: 1) The bonding strength between the antenna substrate layer and the metal foil layer is improved through the preliminary curing of the second adhesive layer and the re-curing by the rolling mechanism. At the same time, the bubbles that may be generated between the antenna substrate layer and the metal foil layer are further eliminated by rolling, thereby avoiding the signal attenuation or connection failure caused by the existence of bubbles; 2) Since the entire process is carried out at room temperature and no high-temperature treatment is required, the process flow is greatly simplified and energy consumption is reduced. At the same time, the influence of high temperature on the plastic antenna substrate layer is avoided, and the antenna substrate layer is prevented from being deformed, so that the shape of the antenna line area formed after the metal foil layer is adhered to the high-temperature substrate layer changes compared with the designed antenna line area shape. ; 3) Through laser cutting and / or die cutting, combined with negative pressure adsorption, the antenna line area and non-antenna line area are accurately and quickly separated, reducing production costs, improving production efficiency and product consistency; 4) Through targeted design and production of frequency selective surface layers, the electromagnetic characteristics of the glass antenna are optimized, the anti-interference ability of the glass antenna is improved, and the signal loss is reduced. At the same time, the impact of sunlight exposure on the performance of the glass antenna is taken into consideration to extend the service life; 5) Through the setting of AF film, an additional protective layer is provided for the glass antenna, maintaining the cleanliness and light transmittance of the glass antenna, and further improving the aesthetics and service life of the glass antenna. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0019] Figure 1 A cross-sectional view of a first implementation of a laminated structure of a glass antenna according to Embodiment 1 of the present invention; Figure 2 A cross-sectional view of a frequency selective surface layer of a laminated structure of a glass antenna according to a first embodiment of the present invention; Figure 3 is a cross-sectional view of a second implementation manner of a laminated structure of a glass antenna according to the first embodiment of the present invention; Figure 4 This is a flow chart of the steps of a method for manufacturing a laminated structure of a glass antenna according to the second embodiment of the present invention.
[0020] Reference numerals: 1. First glass; 2. Frequency selective surface layer; 3. Antenna layer; 4. Second glass; 5. AF film; 21. Top layer; 22. Middle layer; 23. Bottom layer; 24. Channel. DETAILED DESCRIPTION
[0021] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. It should be noted that relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations.
[0022] This embodiment provides a laminated structure of a glass antenna, the specific structure is as follows Figure 1-2 , mainly including: a first glass 1, a first adhesive layer, a frequency selective surface layer 2, an antenna layer 3, and a second glass 4. The first glass 1 includes a first surface and a second surface, and the second surface is used to fix the frequency selective surface layer 2 through the first adhesive layer; the frequency selective surface layer 2 is composed of three layers of transparent materials, the middle layer 22 of the three layers of transparent materials is polymethyl methacrylate, the top layer 21 and the bottom layer 23 of the three layers of transparent materials are both polydimethylsiloxane, and a channel 24 is provided in the top layer 21 and / or the bottom layer 23, and liquid metal is provided in the channel 24; the antenna layer 3 includes an antenna substrate layer, a metal foil layer, and a second adhesive layer, and the second adhesive layer is used to bond the antenna substrate layer and the metal foil layer; the second glass 4 includes a third surface and a fourth surface.
[0023] In this embodiment, the first glass 1 and the second glass 4 can be made of ultra-white glass or low-iron glass, etc. The first glass 1 and the second glass 4 together constitute the main body of the glass antenna, and have good light transmittance and structural strength. The frequency selective surface layer 2 in this embodiment is composed of three layers of transparent materials, especially the top layer 21 and / or the bottom layer 23 are provided with a channel 24, and the channel 24 is provided with liquid metal, which can selectively transmit electromagnetic signals under the condition of achieving optical transparency, and can isolate infrared rays, reduce the temperature rise caused by infrared rays under the condition of sunlight exposure, and thus affect the performance of the glass antenna. In this embodiment, by setting the frequency selective surface layer 2, it can selectively transmit electromagnetic signals, and can isolate infrared rays under the condition of optical transparency, and can isolate other electromagnetic signals, which can not only improve the adaptability of the glass antenna, but also have good signal reception function even on cars or buildings exposed to the sun, and can shield other electromagnetic signals, and improve anti-interference ability. In addition, the materials of the top layer 21 and the bottom layer 23 in this embodiment are polydimethylsiloxane. Due to the inherent elasticity and flexibility of polydimethylsiloxane, polydimethylsiloxane needs to be pasted on a transparent substrate with a certain strength, and polymethyl methacrylate has the advantages of high light transmittance, high strength and low price. Therefore, the frequency selective surface layer 2 in this embodiment is composed of polydimethylsiloxane + polymethyl methacrylate + polydimethylsiloxane, which can improve the performance of the glass antenna and achieve high light transmittance and high strength. In addition, the antenna layer 3 in this embodiment includes an antenna substrate layer, a metal foil layer, a second adhesive layer, and the antenna substrate layer and the metal foil layer are bonded by the second adhesive layer, so that the antenna line area formed by the metal foil layer will not be deformed compared to the designed antenna line area during the production and use process, thereby improving the use effect of the glass antenna.
[0024] In some implementations of this embodiment, Figure 2 As shown, the thickness of the frequency selective surface layer 2 is ,in The frequency selective surface layer 2 selects the wavelength of the electromagnetic wave to be transmitted, is the dielectric constant of the intermediate layer 22, n is a positive integer, such as 1, 2, 3, ..., The incident angle of the electromagnetic wave selected to be transmitted by the frequency selective surface layer 2. Specifically, there are large differences in different radio frequency bands. Therefore, in this embodiment, the thickness d of the frequency selective surface layer 2 is designed and calculated according to the wavelength of the electromagnetic wave selected to be transmitted by the glass antenna, so that electromagnetic waves of other frequencies can be shielded and the anti-interference ability of the glass antenna can be improved. In addition, under normal circumstances, when the glass antenna is used in a car, the front windshield, rear windshield, sunroof and side windows of the car can all use glass antennas. For example, when the glass antenna is applied to the sunroof, the optimal incident angle of the electromagnetic signal transmitted from the satellite is 0°. When the glass antenna is applied to the front windshield, the optimal incident angle of the electromagnetic signal transmitted from the satellite is 30°-60°. For different car models and glass antennas in different use positions (front windshield, rear windshield, sunroof and side windows) of different car models, their specific optimal incident angles are different. Therefore, in this embodiment, the user can perform targeted design calculations based on the specific application location of the glass antenna and the electromagnetic signal selected to be transmitted. By calculating the optimal frequency-selective surface layer 2 thickness and designing the glass antenna accordingly, the performance of the glass antenna in different usage scenarios can be greatly improved, thereby improving the user experience.
[0025] In some implementations of this embodiment, Figure 2 As shown, the channel 24 of the top layer 21 and the bottom layer 23 are both provided with a channel 24, liquid metal is provided in the channel 24, and the projections of the channel 24 of the top layer 21 and the channel 24 of the bottom layer 23 on the frequency selective surface layer 2 are orthogonal to each other. Through the above structure, the shielding performance and optical transparency performance of the frequency selective surface layer 2 can be improved, and the polarization stability can be achieved.
[0026] In some implementations of this embodiment, the liquid metal provided in the channel 24 of the top layer 21 and / or the bottom layer 23 is a eutectic gallium-indium alloy, in which the mass fraction of gallium is 70% to 80% of the mass fraction of gallium, and the mass fraction of indium is 20% to 30%.
[0027] In some implementations of this embodiment, the cross-sectional shape of the channel 24 is rectangular. Based on the processing technology and the viscosity of the selected eutectic gallium-indium alloy, the width L of the cross-sectional shape of the channel 24 is ≥ 0.5 mm, and the height h of the cross-sectional shape of the channel 24 is ≥ 0.6 mm, thereby realizing a high-pass filtering function.
[0028] In some implementations of this embodiment, the second adhesive layer is UV glue, and the second adhesive layer is coated on the side of the metal foil layer close to the antenna substrate layer according to the shape of the antenna line area, and the metal foil layer is initially cured to the antenna substrate layer by ultraviolet light to form an antenna composite layer. In this implementation, ultraviolet light is used to initially cure the metal foil layer to the antenna substrate layer to form an antenna composite layer having the shape of the antenna line area, and the initial curing process can be performed at room temperature, avoiding the risk of deformation of the antenna line area caused by processing the antenna line area under high temperature conditions, and the risk of errors between the antenna line area and the designed antenna line area.
[0029] In some implementations of this embodiment, the antenna substrate layer and the metal foil layer are bonded by the second adhesive layer and initially cured by ultraviolet light, and then rolled and bonded to each other again by a rolling mechanism, wherein the rolling shape of the rolling mechanism coincides with the shape of the antenna line area, so that the metal foil layer is solidified again on the antenna substrate layer, so that the second adhesive layer is in a completely solidified state, and the tightness between the antenna substrate layer and the metal foil is improved. In addition, the rolling of the rolling mechanism can avoid the generation of bubbles at the joint between the antenna substrate layer and the metal foil, and improve the yield rate in the production process of the antenna line area.
[0030] In some embodiments, Figure 3 As shown, an AF film 5 is provided on the first surface of the first glass 1 and the surface of the second glass 4 away from the first glass 1, wherein the AF film 5 has the characteristics of strong anti-fouling ability, easy cleaning, and friction resistance. In this embodiment, by providing the AF film 5 on the first surface of the first glass 1 and the surface of the second glass 4 away from the first glass 1, the glass antenna is easy to clean and the use experience is improved. In addition, when the glass antenna is applied to a car, the outer side of the glass of the car will be exposed to the sun, wind, and rain, and the inner side of the glass of the car may be scratched or stained by the driver or passengers. Therefore, providing the AF film 5 on the first surface of the first glass 1 of the glass antenna and the surface of the second glass 4 away from the first glass 1 can reduce the damage to the glass antenna caused by external factors and improve the service life of the glass antenna.
[0031] Embodiment 2 This embodiment discloses a method for manufacturing a laminated structure of a glass antenna, which is used to manufacture the laminated structure of the glass antenna in the first embodiment, and comprises the following steps: 1) The metal foil layer is arranged on one side of the antenna substrate layer, and a second adhesive layer is applied to the side of the metal foil layer close to the antenna substrate layer according to the shape of the antenna line area, wherein the second adhesive layer is UV glue, and the metal foil layer is initially cured to the antenna substrate layer by ultraviolet light to form an antenna composite layer; 2) rolling the antenna composite layer by a rolling mechanism, wherein the rolling shape of the rolling mechanism coincides with the shape of the antenna line area, so that the metal foil layer is solidified again on the antenna substrate layer and forms the antenna line area; 3) Performing laser cutting and / or die cutting on the antenna line area and the non-antenna line area on the antenna composite layer, and then separating and recovering the non-antenna line area by negative pressure adsorption using a negative pressure adsorption device, and performing quality inspection on the antenna line area; 4) The thickness of the frequency selective surface layer 2 is calculated and designed according to the wavelength of the electromagnetic wave selectively transmitted by the frequency selective surface layer 2, the incident angle, and the dielectric constant of the intermediate layer 22, and liquid metal is injected into the channel 24 provided in the top layer 21 and / or the bottom layer 23 of the frequency selective surface layer 2, wherein the liquid metal is a gallium-indium alloy; 5) The first glass 1, the first adhesive layer, the frequency selective surface layer 2, the antenna layer 3, and the second glass 4 are pressed and bonded together by a pressing and bonding device, and an AF film 5 is coated on the first surface of the first glass 1 and the surface of the second glass 4 away from the first glass 1.
[0032] Specifically, in step 1), a metal foil is disposed on one side of the antenna substrate layer, wherein the metal foil can be aluminum foil, copper foil or other metal materials, and the antenna substrate layer can be a film of plastic material, and a second adhesive layer is coated on a side of the metal foil layer close to the antenna substrate layer in the shape of the antenna line area through a second adhesive layer, wherein the second adhesive layer is UV glue, and a specific bonding method can be achieved by coating the second adhesive layer on the surface of the metal foil facing the antenna substrate layer in the shape of the antenna line area, or by pre-coating the second adhesive layer on the antenna substrate layer in the shape of the antenna line area, and then laminating the metal foil to the antenna substrate layer, and then irradiating the metal foil layer with ultraviolet light to preliminarily cure the metal foil layer to the antenna substrate layer to form an antenna composite layer.
[0033] In step 2), the antenna composite layer is rolled by a rolling mechanism, wherein the rolling shape of the rolling mechanism coincides with the shape of the antenna line area, so that the metal foil layer is solidified again on the antenna substrate layer to form the antenna line area. The antenna composite layer preliminarily solidified in step 1) is solidified again by the rolling mechanism, so that the second adhesive layer is in a completely solidified state, thereby improving the tightness between the antenna substrate layer and the metal foil; and the rolling of the rolling mechanism can avoid the generation of bubbles at the joint between the antenna substrate layer and the metal foil, thereby improving the yield rate in the production process of the antenna line area.
[0034] In step 3), the antenna line area and the non-antenna line area on the antenna composite layer are laser cut and / or die cut to facilitate the waste treatment of the non-antenna line area. After the cutting is completed, the non-antenna line area is separated and recovered by a negative pressure adsorption device using a negative pressure adsorption method, and the antenna line area is quality tested, thereby improving production efficiency and product quality and reducing production costs.
[0035] In step 4), the thickness of the frequency selective surface layer 2 is calculated and designed according to the wavelength of the electromagnetic wave selectively transmitted by the frequency selective surface layer 2, the incident angle and the dielectric constant of the intermediate layer 22. ,in The thickness of surface layer 2 is selected for the frequency, The wavelength of the electromagnetic wave selected to be transmitted by the frequency selective surface layer 2 can be selected and calculated based on the wavelength of the electromagnetic wave selected to be transmitted. is the dielectric constant of the intermediate layer 22, n is a positive integer, such as 1, 2, 3, ..., The incident angle of the electromagnetic wave to be transmitted is selected for the frequency selective surface layer 2. For example, the optimal incident angle of the sunroof glass of a car when receiving satellite signals is 0°. The optimal thickness of the frequency selective surface layer 2 is calculated according to different electromagnetic wave wavelengths and usage scenarios of the glass antenna. A channel 24 is opened in the top layer 21 and / or the bottom layer 23 of the frequency selective surface layer 2, and a gallium-indium alloy is injected into the channel 24, so as to achieve high-pass filtering performance under optical transparency.
[0036] In step 5), the first glass 1, the first adhesive layer, the frequency selective surface layer 2, the antenna layer 3, and the second glass 4 are pressed and bonded together by a pressing and bonding device. After bonding, an AF film 5 is provided on the first surface of the first glass 1 and the surface of the second glass 4 away from the first glass 1. The AF film 5 has the characteristics of strong anti-fouling ability, easy cleaning, and friction resistance, thereby reducing the damage to the glass antenna caused by external factors and increasing the service life of the glass antenna.
[0037] The manufacturing method of the laminated structure of the glass antenna in this embodiment is used to manufacture the laminated structure of the glass antenna in Example 1, which can achieve high-pass filtering under the condition of optical transparency, and can be designed and improved for different usage scenarios, thereby improving the service life of the glass antenna. In addition, each step in the manufacturing process is carried out at room temperature, avoiding the influence of high temperature on the antenna line area, and shielding infrared rays through the frequency selective surface layer 2, reducing the influence of infrared rays on the antenna layer 3 during use, greatly improving the use experience of the glass antenna.
[0038] Although various embodiments of the present disclosure have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and alterations may be made to the embodiments without departing from the principles and spirit of the present disclosure, the scope of which is defined by the claims and their equivalents.
Claims
1. A laminated structure of a glass antenna, characterized in that: comprising a first glass, a first adhesive layer, a frequency selective surface layer, an antenna layer, and a second glass; The first glass comprises a first surface and a second surface arranged opposite to each other, and the second surface is fixedly connected to the frequency selective surface layer through the first adhesive layer; The frequency selective surface layer is composed of three layers of transparent material, the middle layer of the three layers of transparent material is polymethyl methacrylate, the top layer and the bottom layer of the three layers of transparent material are both polydimethylsiloxane, the top layer and / or the bottom layer are provided with a channel, and the channel is provided with liquid metal; The antenna layer comprises an antenna substrate layer, a metal foil layer and a second adhesive layer, wherein the second adhesive layer is used to bond the antenna substrate layer and the metal foil layer; The second glass includes a third surface and a fourth surface which are oppositely arranged.
2. The laminated structure of a glass antenna according to claim 1, characterized in that: The thickness of the frequency selective surface layer is ,in The frequency selective surface layer selects the wavelength of the electromagnetic wave to be transmitted. is the dielectric constant of the middle layer, n is a positive integer, The frequency selective surface layer selects the incident angle of the electromagnetic wave to be transmitted.
3. The laminated structure of a glass antenna according to claim 1, characterized in that: Projections of the channels of the top layer and the channels of the bottom layer on the frequency selective surface layer are orthogonal to each other.
4. The laminated structure of a glass antenna according to claim 1, characterized in that: The liquid metal is a gallium-indium alloy.
5. The laminated structure of a glass antenna according to claim 4, characterized in that: The mass fraction of gallium in the gallium-indium alloy is 70% to 80%, and the mass fraction of indium is 20% to 30%.
6. The laminated structure of a glass antenna according to claim 5, characterized in that: The cross-sectional shape of the channel is rectangular, the width L of the channel cross-sectional shape is ≥ 0.5 mm, and the height h of the channel cross-sectional shape is ≥ 0.6 mm.
7. The laminated structure of a glass antenna according to claim 1, characterized in that: The second adhesive layer is UV glue.
8. The laminated structure of a glass antenna according to claim 7, characterized in that: The antenna substrate layer and the metal foil layer are rolled and bonded to each other by a rolling mechanism, and the metal foil layer forms an antenna line area on the antenna substrate layer.
9. The laminated structure of a glass antenna according to claim 1, characterized in that: The first surface of the first glass and the surface of the second glass away from the first glass are both provided with AF films.
10. A method for manufacturing a laminated structure of a glass antenna, used for manufacturing the laminated structure of a glass antenna as claimed in any one of claims 1 to 9, characterized in that: The following steps are involved: 1) The metal foil layer is arranged on one side of the antenna substrate layer, and a second adhesive layer is applied to the side of the metal foil layer close to the antenna substrate layer according to the shape of the antenna line area, and the metal foil layer is initially cured to the antenna substrate layer by ultraviolet light to form an antenna composite layer; 2) rolling the antenna composite layer by a rolling mechanism, wherein the rolling shape of the rolling mechanism coincides with the shape of the antenna line area, so that the metal foil layer is solidified again on the antenna substrate layer and forms an antenna line area; 3) Performing laser cutting and / or die cutting on the antenna line area and the non-antenna line area on the antenna composite layer, and then separating and recovering the non-antenna line area by negative pressure adsorption using a negative pressure adsorption device, and performing quality inspection on the antenna line area; 4) calculating and designing the thickness of the frequency selective surface layer according to the wavelength of the electromagnetic wave selectively transmitted by the frequency selective surface layer, the incident angle and the dielectric constant of the intermediate layer, and injecting liquid metal into the channels provided in the top layer and / or the bottom layer of the frequency selective surface layer; 5) The first glass, the first adhesive layer, the frequency selective surface layer, the antenna layer, and the second glass are pressed and bonded together by a pressing and bonding device, and an AF film is coated on the first surface of the first glass and the surface of the second glass away from the first glass.