Lens unit, laminate, display body, method for manufacturing display body, and display method
By using a combination of a reflective polarization member, an absorbent polarization member and a lens part in the VR goggles, the problem of afterimage in the VR goggles is solved, and a lightweight and high-refinement display effect is achieved.
Patent Information
- Application Number
- CN202380027570.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-05-10
- Filing Date
- 2023-02-24
- Publication Date
- 2024-11-01
AI Technical Summary
In VR goggles, the use of thin lenses leads to ghost problems in optical components, and it is difficult to achieve a lightweight and highly refined display system.
By adopting a combination of a reflective polarization member, an absorber polarization member, a first lens part, a half mirror and a second λ/4 member, the appearance of afterimage is suppressed through the optical path design and the configuration of the optical axis, and the lightness of the lens part is achieved. Qualification and high refinement.
It effectively suppresses the appearance of afterimage, realizes the lightweight and high-fine display system of VR goggles, and improves display performance.
Smart Images

Figure CN118891568A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a lens portion, a laminate, a display, a method for manufacturing a display, and a display method. Background Art
[0002] Image display devices represented by liquid crystal display devices and electroluminescent (EL) display devices (e.g., organic EL display devices) are rapidly becoming popular. In image display devices, optical components such as polarization components and phase difference components are generally used to realize image display and improve image display performance (e.g., refer to Patent Document 1).
[0003] In recent years, new uses for image display devices have been developed. For example, goggles with displays (VR goggles) for realizing Virtual Reality (VR) have begun to be commercialized. Since the use of VR goggles in various scenarios has been studied, it is expected that they will be lightweight and highly refined. Lightweighting can be achieved, for example, by thinning the lenses used for VR goggles. On the other hand, it is also expected to develop optical components suitable for display systems using thin lenses. In addition, in a VR display system, when using conversion and reflection of circularly polarized light and linearly polarized light, there is a problem of light that should have been reflected passing through and visually recognizing an afterimage (ghost).
[0004] Prior art literature
[0005] Patent Literature
[0006] Patent Document 1: Japanese Patent Application Publication No. 2021-103286 Summary of the invention
[0007] Problems to be solved by the invention
[0008] In view of the above circumstances, a main object of the present invention is to provide a lens unit that can achieve a reduction in weight and a high definition of VR goggles and can suppress afterimages.
[0009] Solutions to the problem
[0010] 1. The lens unit of an embodiment of the present invention is used in a display system for displaying an image to a user. The lens unit includes: a reflective polarization component that reflects light emitted from a display surface of a display element that displays an image and passes through the polarization component and the first λ / 4 component; an absorptive polarization component that is arranged in front of the reflective polarization component; a first lens unit that is arranged on an optical path between the display element and the reflective polarization component; a half mirror that is arranged between the display element and the first lens unit, transmits light emitted from the display element, and reflects light reflected by the reflective polarization component toward the reflective polarization component; and a second λ / 4 component that is arranged on an optical path between the half mirror and the reflective polarization component. The second λ / 4 component is integrated with the reflective polarization component.
[0011] 2. In the lens unit described in 1 above, the reflection axis of the reflective polarization element and the absorption axis of the absorptive polarization element may be arranged parallel to each other.
[0012] 3. In the lens unit described in 1 or 2 above, the first lens unit and the half mirror may be integrated.
[0013] 4. In the lens unit according to any one of 1 to 3 above, the lens unit may include a second lens unit disposed in front of the absorbing polarization element.
[0014] 5. In the lens portion described in any one of 1 to 4 above, the angle formed by the absorption axis of the polarization component contained in the display element and the slow axis of the first λ / 4 component can be 40° to 50°, and the angle formed by the absorption axis of the polarization component contained in the display element and the slow axis of the second λ / 4 component can be 40° to 50°.
[0015] 6. In the lens unit according to any one of 1 to 5 above, the second λ / 4 element, the reflective polarization element, and the absorbing polarization element may be integrated.
[0016] 7. A laminated body according to an embodiment of the present invention is used for the lens unit according to any one of 1 to 6 above, and includes the second λ / 4 member and the reflective polarization member.
[0017] 8. The laminated body described in item 7 above may further include the above-mentioned absorbing polarizing member.
[0018] 9. In the laminated body described in 8 above, the reflection axis of the reflective polarization element and the absorption axis of the absorptive polarization element may be arranged parallel to each other.
[0019] 10. A display according to an embodiment of the present invention includes the lens unit according to any one of 1 to 6 above.
[0020] 11. A method for manufacturing a display according to an embodiment of the present invention is a method for manufacturing a display having the lens unit described in any one of 1 to 6 above.
[0021] 12. The display method of an embodiment of the present invention comprises: a step of causing light of a display image emitted through a polarization component and a 1λ / 4 component to pass through a half-mirror and a first lens portion; a step of causing the light after passing through the half-mirror and the first lens portion to pass through a 2λ / 4 component; a step of causing the light after passing through the 2λ / 4 component to reflect toward the half-mirror at a reflective polarization component; a step of causing the light after being reflected at the reflective polarization component and the half-mirror to pass through the reflective polarization component through the 2λ / 4 component; and a step of causing the light after passing through the reflective polarization component to pass through an absorptive polarization component, wherein the 2λ / 4 component and the reflective polarization component are integrated.
[0022] Effects of the Invention
[0023] According to the lens unit of the embodiment of the present invention, it is possible to achieve a lighter and higher-definition VR goggles, and further, it is possible to suppress afterimages. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 This is a schematic diagram showing a schematic configuration of a display system according to one embodiment of the present invention.
[0025] Figure 2 This is a schematic perspective view showing an example of a multilayer structure included in a reflective polarizing film.
[0026] Explanation of symbols
[0027] 2 Display system
[0028] 4 Lens section
[0029] 12 Display components
[0030] 16. First lens unit
[0031] 18 Half Mirror
[0032] 20 first phase difference member
[0033] 22. Second phase difference member
[0034] 24 Second lens unit
[0035] 32. Reflective polarizing element
[0036] 34 Absorption type polarization element DETAILED DESCRIPTION
[0037] Hereinafter, the embodiments of the present invention will be described with reference to the accompanying drawings, but the present invention is not limited to these embodiments. In addition, in order to explain more clearly, the accompanying drawings sometimes schematically show the width, thickness, shape, etc. of each part compared with the embodiments, but this is only an example and does not limit the interpretation of the present invention.
[0038] (Definition of Terms and Symbols)
[0039] The definitions of terms and symbols in this specification are as follows.
[0040] (1) Refractive index (nx, ny, nz)
[0041] "nx" is the refractive index in the direction where the refractive index in the plane reaches the maximum (ie, the slow axis direction), "ny" is the refractive index in the direction orthogonal to the slow axis in the plane (ie, the fast axis direction), and "nz" is the refractive index in the thickness direction.
[0042] (2) In-plane phase difference (Re)
[0043] "Re(λ)" is the in-plane phase difference measured at 23°C with light of wavelength λnm. For example, "Re(550)" is the in-plane phase difference measured at 23°C with light of wavelength 550nm. When the thickness of the layer (film) is d(nm), Re(λ) can be calculated by the formula: Re(λ) = (nx-ny)×d.
[0044] (3) Retardation in the thickness direction (Rth)
[0045] "Rth(λ)" is the phase difference in the thickness direction measured at 23°C with light of wavelength λnm. For example, "Rth(550)" is the phase difference in the thickness direction measured at 23°C with light of wavelength 550nm. When the thickness of the layer (film) is d(nm), Rth(λ) can be calculated by the formula: Rth(λ) = (nx-nz)×d.
[0046] (4) Nz coefficient
[0047] The Nz coefficient can be calculated by Nz=Rth / Re.
[0048] (5) Angle
[0049] In this specification, when an angle is mentioned, the angle includes both clockwise and counterclockwise angles relative to a reference direction. Therefore, for example, "45°" means ±45°.
[0050] Figure 1 Schematic diagram showing a simplified structure of a display system according to an embodiment of the present invention. Figure 1 , the configuration and shape of each component of the display system 2 are schematically shown. The display system 2 includes a display element 12, a reflective polarization member 32, an absorptive polarization member 34, a first lens unit 16, a half mirror 18, a first phase difference member 20, a second phase difference member 22, and a second lens unit 24. The reflective polarization member 32 is arranged on the display surface 12a side of the display element 12, that is, in front, and can reflect the light emitted from the display element 12. The first lens unit 16 is arranged on the optical path between the display element 12 and the reflective polarization member 32, and the half mirror 18 is arranged between the display element 12 and the first lens unit 16. The first phase difference member 20 is arranged on the optical path between the display element 12 and the half mirror 18, and the second phase difference member 22 is arranged on the optical path between the half mirror 18 and the reflective polarization member 32. The absorptive polarization member 34 can be arranged in front of the reflective polarization member 32. The reflection axis of the reflective polarization element and the absorption axis of the absorptive polarization element can be arranged substantially parallel to each other, and the transmission axis of the reflective polarization element and the absorptive polarization element can be arranged substantially parallel to each other. It should be noted that the reflective polarization element 32 and the absorptive polarization element 34 are sometimes collectively referred to as a reflector.
[0051] In an embodiment of the present invention, the second phase difference member 22 (hereinafter, the second phase difference member is sometimes referred to as the second λ / 4 member) and the reflective polarization member 32 are integrated. In one embodiment, as shown in the figure, the second λ / 4 member 22, the reflective polarization member 32 and the absorption polarization member 34 are integrated. The second λ / 4 member, the reflective polarization member and the absorption polarization member used as needed are integrated (representatively stacked), for example, via an adhesive layer (not shown). If it is such a structure, the second λ / 4 member, the reflective polarization member and the absorption polarization member used as needed are fixed, which can prevent the increase in transmittance caused by the offset of the axis configuration of the optical axis (slow axis, reflection axis and absorption axis) of each member. In particular, the fixation of the second λ / 4 member and the reflective polarization member will be the main reason for such an effect. In addition, it is possible to suppress the adverse effects caused by the air layer that may be formed between the components. As a result, the transmission of light that should be reflected can be suppressed, and the afterimage (ghost) can be well suppressed. The adhesive layer can be formed by an adhesive or an adhesive. The thickness of the adhesive layer is, for example, 0.05 μm to 30 μm, preferably 3 μm to 20 μm, and more preferably 5 μm to 15 μm.
[0052] The components arranged in front of the half mirror (in the illustrated example, the half mirror 18, the first lens unit 16, the second phase difference element 22, the reflective polarization element 32, the absorptive polarization element 34 and the second lens unit 24) are sometimes collectively referred to as a lens unit (lens unit 4).
[0053] The display element 12 is, for example, a liquid crystal display or an organic EL display, and has a display surface 12a for displaying images. Light emitted from the display surface 12a passes through a polarizing member (typically a polarizing film) that may be included in the display element 12 and then emitted as first linearly polarized light.
[0054] The first phase difference member 20 is a λ / 4 member capable of converting the first linearly polarized light incident on the first phase difference member 20 into the first circularly polarized light (hereinafter, the first phase difference member may be referred to as a first λ / 4 member). The first phase difference member 20 may be integrally provided with the display element 12 .
[0055] The half mirror 18 transmits the light emitted from the display element 12 and reflects the light reflected by the reflective polarization member 32 toward the reflective polarization member 32. The half mirror 18 is integrally provided with the first lens portion 16.
[0056] The second phase difference member 22 is a λ / 4 member that allows light reflected by the reflective polarization member 32 and the half mirror 18 to pass through the reflective polarization member 32. The second phase difference member 22 may be integrally provided with the first lens portion 16.
[0057] The first circularly polarized light emitted from the first λ / 4 member 20 passes through the half mirror 18 and the first lens unit 16, and is converted into the second linearly polarized light by the second λ / 4 member 22. The second linearly polarized light emitted from the second λ / 4 member 22 does not pass through the reflective polarization member 32, but is reflected toward the half mirror 18. At this time, the polarization direction of the second linearly polarized light incident on the reflective polarization member 32 is the same direction as the reflection axis of the reflective polarization member. Therefore, the second linearly polarized light incident on the reflective polarization member is reflected by the reflective polarization member.
[0058] The second linear polarized light reflected by the reflective polarization member 32 is converted into the second circular polarized light by the second λ / 4 member 22, and the second circular polarized light emitted from the second λ / 4 member 22 is reflected by the half mirror 18 after passing through the first lens unit 16. The second circular polarized light reflected by the half mirror 18 passes through the first lens unit 16 and is converted into the third linear polarized light by the second λ / 4 member 22. The third linear polarized light is transmitted through the reflective polarization member 32. At this time, the polarization direction of the third linear polarized light incident on the reflective polarization member 32 is the same direction as the transmission axis of the reflective polarization member. Therefore, the third linear polarized light incident on the reflective polarization member 32 is transmitted through the reflective polarization member.
[0059] The light transmitted through the reflective polarizing element 32 passes through the absorptive polarizing element 34 and the second lens unit 24 and enters the user's eye 26. The polarization direction of the third linear polarized light transmitted through the reflective polarizing element 32 is the same as the transmission axis of the absorptive polarizing element.
[0060] For example, the absorption axis of the polarization component included in the display element 12 and the reflection axis of the reflective polarization component 32 can be arranged approximately parallel to each other, or approximately orthogonally. The angle formed by the absorption axis of the polarization component included in the display element 12 and the slow axis of the first phase difference component 20 is, for example, 40° to 50°, 42° to 48°, or approximately 45°. The angle formed by the absorption axis of the polarization component included in the display element 12 and the slow axis of the second phase difference component 22 is, for example, 40° to 50°, 42° to 48°, or approximately 45°. The slow axis of the first phase difference component 20 and the slow axis of the second phase difference component 22 can, for example, be arranged approximately parallel to each other.
[0061] The in-plane phase difference Re (550) of the first phase difference member 20 may be, for example, 100 nm to 190 nm, 110 nm to 180 nm, 130 nm to 160 nm, or 135 nm to 155 nm.
[0062] The first phase difference member 20 preferably exhibits an inverse dispersion wavelength characteristic in which the phase difference value increases with the wavelength of the measured light. The Re(450) / Re(550) of the first phase difference member 20 is, for example, less than 1, may be less than 0.95, further may be less than 0.90, and further may be less than 0.85. The Re(450) / Re(550) of the first phase difference member 20 is, for example, greater than 0.75.
[0063] In one embodiment, the first phase difference member 20 satisfies all of the conditions of Re(400) / Re(550)<0.85, Re(650) / Re(550)>1.03, and Re(750) / Re(550)>1.05. The first phase difference member 20 preferably satisfies at least one selected from 0.65<Re(400) / Re(550)<0.80 (preferably 0.7<Re(400) / Re(550)<0.75), 1.0<Re(650) / Re(550)<1.25 (preferably 1.05<Re(650) / Re(550)<1.20), and 1.05<Re(750) / Re(550)<1.40 (preferably 1.08<Re(750) / Re(550)<1.36), more preferably satisfies at least two, and further preferably satisfies all of them.
[0064] The refractive index characteristics of the first phase difference component 20 preferably show a relationship of nx>ny≥nz. Here, "ny=nz" includes not only the case where ny and nz are completely equal, but also the case where they are substantially equal. Therefore, within the range that does not impair the effect of the present invention, ny<nz may sometimes be satisfied. The Nz coefficient of the first phase difference component 20 is preferably 0.9 to 3, more preferably 0.9 to 2.5, further preferably 0.9 to 1.5, and particularly preferably 0.9 to 1.3.
[0065] The first phase difference member 20 is formed of any appropriate material that can satisfy the above-mentioned characteristics. The first phase difference member 20 may be, for example, a stretched film of a resin film or an alignment fixing layer of a liquid crystal compound.
[0066] As the resin contained in the above-mentioned resin film, there can be cited: polycarbonate resin, polyester carbonate resin, polyester resin, polyvinyl acetal resin, polyarylate resin, cyclic olefin resin, cellulose resin, polyvinyl alcohol resin, polyamide resin, polyimide resin, polyether resin, polystyrene resin, acrylic resin, etc. These resins can be used alone or in combination (for example, blending, copolymerization). In the case where the first phase difference component 20 shows reverse dispersion wavelength characteristics, a resin film containing a polycarbonate resin or a polyester carbonate resin (hereinafter, sometimes referred to as a polycarbonate resin) can be suitably used.
[0067] As the above-mentioned polycarbonate resin, any appropriate polycarbonate resin can be used as long as the effect of the present invention can be obtained. For example, the polycarbonate resin contains structural units derived from fluorene dihydroxy compounds, structural units derived from isosorbide dihydroxy compounds, and structural units derived from at least one dihydroxy compound selected from alicyclic diols, alicyclic dimethanols, di, tri or polyethylene glycols and alkylene glycols or spirodiols. Preferably, the polycarbonate resin contains structural units derived from fluorene dihydroxy compounds, structural units derived from isosorbide dihydroxy compounds, structural units derived from alicyclic dimethanols and / or structural units derived from di, tri or polyethylene glycols; more preferably, it contains structural units derived from fluorene dihydroxy compounds, structural units derived from isosorbide dihydroxy compounds, and structural units derived from di, tri or polyethylene glycols. The polycarbonate resin may also contain structural units derived from other dihydroxy compounds as needed. It should be noted that the details of the polycarbonate resin that can be suitably used for the first phase difference component and the method for forming the first phase difference component are recorded in, for example, Japanese Patent Publication No. 2014-10291, Japanese Patent Publication No. 2014-26266, Japanese Patent Publication No. 2015-212816, Japanese Patent Publication No. 2015-212817, and Japanese Patent Publication No. 2015-212818, and the records in these publications are cited as references in this specification.
[0068] The thickness of the first phase difference member 20 formed of a stretched film of a resin film is, for example, 10 μm to 100 μm, preferably 10 μm to 70 μm, more preferably 10 μm to 40 μm, and further preferably 20 μm to 30 μm.
[0069] The orientation fixing layer of the above-mentioned liquid crystal compound is a layer in which the liquid crystal compound is oriented in a given direction within the layer and its orientation state is fixed. It should be noted that the "orientation fixing layer" is a concept that includes an orientation solidification layer obtained by solidifying the liquid crystal monomer as described later. In the first phase difference component, representatively, the rod-shaped liquid crystal compound is oriented (parallel orientation (homogeneous alignment)) in a state of being arranged along the slow axis direction of the first phase difference component. As rod-shaped liquid crystal compounds, for example, liquid crystal polymers and liquid crystal monomers can be cited. The liquid crystal compound is preferably capable of polymerization. If the liquid crystal compound is capable of polymerization, the orientation state of the liquid crystal compound can be fixed by polymerizing after orienting the liquid crystal compound.
[0070] The orientation fixing layer (liquid crystal orientation fixing layer) of the above-mentioned liquid crystal compound can be formed by the following method: an orientation treatment is applied to the surface of a given substrate, a coating liquid containing a liquid crystal compound is applied to the surface, and the liquid crystal compound is oriented along the direction corresponding to the above-mentioned orientation treatment to fix the orientation state. As an orientation treatment, any appropriate orientation treatment can be adopted. Specifically, mechanical orientation treatment, physical orientation treatment, and chemical orientation treatment can be cited. As specific examples of mechanical orientation treatment, friction treatment and stretching treatment can be cited. As specific examples of physical orientation treatment, magnetic field orientation treatment and electric field orientation treatment can be cited. As specific examples of chemical orientation treatment, inclined evaporation method and optical orientation treatment can be cited. The processing conditions of various orientation treatments can adopt any appropriate conditions according to the purpose.
[0071] The liquid crystal compound can be aligned by treating it at a temperature corresponding to the type of the liquid crystal compound at which it exhibits a liquid crystal phase. By such a temperature treatment, the liquid crystal compound is in a liquid crystal state and is aligned in the alignment treatment direction of the substrate surface.
[0072] In one embodiment, the alignment state is fixed by cooling the aligned liquid crystal compound as described above. When the liquid crystal compound is polymerizable or crosslinkable, the alignment state can be fixed by subjecting the aligned liquid crystal compound to polymerization or crosslinking treatment as described above.
[0073] As the above-mentioned liquid crystal compound, any appropriate liquid crystal polymer and / or liquid crystal monomer can be used. Liquid crystal polymer and liquid crystal monomer can be used alone or in combination. Specific examples of liquid crystal compounds and methods for making liquid crystal orientation fixing layers are described in, for example, Japanese Patent Publication No. 2006-163343, Japanese Patent Publication No. 2006-178389, and International Publication No. 2018 / 123551. The records of these publications are cited as references in this specification.
[0074] The thickness of the first phase difference member 20 composed of the liquid crystal alignment fixing layer is, for example, 1 μm to 10 μm, preferably 1 μm to 8 μm, more preferably 1 μm to 6 μm, and further preferably 1 μm to 4 μm.
[0075] The in-plane phase difference Re(550) of the second phase difference member 22 may be, for example, 100 nm to 190 nm, 110 nm to 180 nm, 130 nm to 160 nm, or 135 nm to 155 nm.
[0076] The second phase difference member 22 preferably exhibits an inverse dispersion wavelength characteristic in which the phase difference value increases with the wavelength of the measured light. The Re(450) / Re(550) of the second phase difference member 22 is, for example, less than 1, may be less than 0.95, further may be less than 0.90, and further may be less than 0.85. The Re(450) / Re(550) of the second phase difference member 22 is, for example, greater than 0.75.
[0077] In one embodiment, the second phase difference member 22 satisfies all of the conditions of Re(400) / Re(550)<0.85, Re(650) / Re(550)>1.03, and Re(750) / Re(550)>1.05. The second phase difference member 22 preferably satisfies at least one selected from 0.65<Re(400) / Re(550)<0.80 (preferably 0.7<Re(400) / Re(550)<0.75), 1.0<Re(650) / Re(550)<1.25 (preferably 1.05<Re(650) / Re(550)<1.20), and 1.05<Re(750) / Re(550)<1.40 (preferably 1.08<Re(750) / Re(550)<1.36), more preferably satisfies at least two, and further preferably satisfies all of them.
[0078] The refractive index characteristics of the second phase difference component 22 preferably show a relationship of nx>ny≥nz. Here, "ny=nz" includes not only the case where ny and nz are completely equal, but also the case where they are substantially equal. Therefore, within the range that does not impair the effect of the present invention, ny<nz may sometimes be achieved. The Nz coefficient of the second phase difference component 22 is preferably 0.9 to 3, more preferably 0.9 to 2.5, further preferably 0.9 to 1.5, and particularly preferably 0.9 to 1.3.
[0079] The second phase difference member 22 is formed of any appropriate material that can satisfy the above characteristics. The second phase difference member 22 can be, for example, a stretched film of a resin film or an orientation fixing layer of a liquid crystal compound. For the second phase difference member 22 composed of a stretched film of a resin film or an orientation fixing layer of a liquid crystal compound, the same description as the first phase difference member 20 can be applied. The first phase difference member 20 and the second phase difference member 22 can be members of the same composition (forming material, thickness, optical properties, etc.), or they can be members of different compositions.
[0080] The above-mentioned reflective polarizing component can transmit polarized light (representatively linear polarized light) parallel to its transmission axis while maintaining its polarization state, and reflect light of other polarization states. As a reflective polarizing component, it is typically composed of a film with a multilayer structure (sometimes referred to as a reflective polarizing film). In this case, the thickness of the reflective polarizing component is, for example, 10 μm to 150 μm, preferably 20 μm to 100 μm, and more preferably 30 μm to 60 μm.
[0081] Figure 2 : is a schematic stereoscopic diagram showing an example of a multilayer structure included in a reflective polarizing film. The multilayer structure 32a alternately comprises a layer A having birefringence and a layer B having substantially no birefringence. The total number of layers constituting the multilayer structure may be 50 to 1000. For example, the refractive index nx of the A layer in the x-axis direction is greater than the refractive index ny in the y-axis direction, the refractive index nx of the B layer in the x-axis direction is substantially the same as the refractive index ny in the y-axis direction, and the refractive index difference between the A layer and the B layer is large in the x-axis direction and substantially zero in the y-axis direction. As a result, the x-axis direction can be made a reflection axis and the y-axis direction can be made a transmission axis. The refractive index difference between the A layer and the B layer in the x-axis direction is preferably 0.2 to 0.3.
[0082] The above-mentioned A layer is typically formed of a material that exhibits birefringence by stretching. Examples of such materials include naphthalene dicarboxylic acid polyesters (e.g., polyethylene naphthalate), polycarbonates, and acrylic resins (e.g., polymethyl methacrylate). The above-mentioned B layer is typically formed of a material that does not substantially exhibit birefringence even when stretched. Examples of such materials include copolyesters of naphthalene dicarboxylic acid and terephthalic acid. The above-mentioned multilayer structure can be formed by combining coextrusion with stretching. For example, after the material constituting the A layer and the material constituting the B layer are extruded, they are multilayered (e.g., using a multiplier). Then, the obtained multilayer laminate is stretched. The x-axis direction of the illustrated example can correspond to the stretching direction.
[0083] Examples of commercially available reflective polarizing films include "DBEF" and "APF" manufactured by 3M Co., Ltd. and "APCF" manufactured by Nitto Denko Corporation.
[0084] The orthogonal transmittance (Tc) of the reflective polarizing component (reflective polarizing film) can be, for example, 0.01% to 3%. The single transmittance (Ts) of the reflective polarizing component (reflective polarizing film) can be, for example, 43% to 49%, and can be preferably 45 to 47%. The polarization degree (P) of the reflective polarizing component (reflective polarizing film) can be, for example, 92% to 99.99%.
[0085] The above-mentioned absorption type polarization component is typically composed of a resin film containing a dichroic substance (sometimes referred to as an absorption type polarization film). In this case, the thickness of the absorption type polarization component is, for example, not less than 1 μm and not more than 20 μm, not less than 2 μm and not more than 15 μm, not more than 12 μm, not more than 10 μm, not more than 8 μm, or not more than 5 μm.
[0086] The above-mentioned absorbing polarizing film may be produced by a single-layer resin film or by using a laminate of two or more layers.
[0087] In the case of a single-layer resin film, for example, a hydrophilic polymer film such as a polyvinyl alcohol (PVA) film, a partially formalized PVA film, or a partially saponified film of an ethylene-vinyl acetate copolymer can be subjected to dyeing treatment using a dichroic substance such as iodine or a dichroic dye, stretching treatment, etc., thereby obtaining an absorbing polarizing film. Among them, an absorbing polarizing film obtained by dyeing a PVA film with iodine and uniaxially stretching the film is preferred.
[0088] The dyeing using iodine can be performed by, for example, immersing the PVA film in an iodine aqueous solution. The stretching ratio of the uniaxial stretching is preferably 3 to 7 times. The stretching can be performed after the dyeing treatment or while dyeing. In addition, the dyeing can also be performed after the stretching. The PVA film can be subjected to swelling treatment, cross-linking treatment, cleaning treatment, drying treatment, etc. as needed.
[0089] As a laminate produced using the above-mentioned two or more layers, there can be cited a laminate of a resin substrate and a PVA-type resin layer (PVA-type resin film) laminated on the resin substrate, or a laminate of a resin substrate and a PVA-type resin layer formed by coating on the resin substrate. The absorption-type polarizing film obtained by using a laminate of a resin substrate and a PVA-type resin layer formed by coating on the resin substrate can be produced by the following method: for example, a PVA-type resin solution is applied to a resin substrate, dried to form a PVA-type resin layer on the resin substrate, and a laminate of the resin substrate and the PVA-type resin layer is obtained; the laminate is stretched and dyed to make the PVA-type resin layer into an absorption-type polarizing film. In this embodiment, it is preferred to form a polyvinyl alcohol-type resin layer containing a halide and a polyvinyl alcohol-type resin on one side of the resin substrate. Stretching typically includes immersing the laminate in a boric acid aqueous solution for stretching. In addition, stretching may further include stretching the laminate in a gas atmosphere at a high temperature (for example, above 95°C) before stretching in a boric acid aqueous solution as needed. In addition, in the present embodiment, it is preferred that the laminate is subjected to a drying shrinkage treatment in which the laminate is shrunk by more than 2% in the width direction by heating while being conveyed in the length direction. Representatively, the manufacturing method of the present embodiment includes sequentially performing an auxiliary stretching treatment in a gas atmosphere, a dyeing treatment, a stretching treatment in an aqueous solution, and a drying shrinkage treatment on the laminate. By introducing the auxiliary stretching, the crystallinity of the PVA can be improved even when the PVA is coated on the thermoplastic resin, and high optical properties can be achieved. In addition, by simultaneously improving the orientation of the PVA in advance, it is possible to prevent problems such as a decrease in orientation and dissolution of the PVA when immersed in water in the subsequent dyeing process and the stretching process, and high optical properties can be achieved. In addition, when the PVA-type resin layer is immersed in a liquid, the orientation disorder of the polyvinyl alcohol molecules and the decrease in orientation can be suppressed compared to the case where the PVA-type resin layer does not contain a halide. As a result, the optical properties of the absorption-type polarizing film obtained by the treatment process of immersing the laminate in a liquid such as a dyeing treatment and a stretching treatment in an aqueous solution can be improved. Furthermore, the optical properties can be improved by shrinking the laminate in the width direction through the drying shrinkage treatment. The obtained laminate of resin substrate / absorption type polarizing film can be used directly (that is, the resin substrate can be used as a protective layer of the absorption type polarizing film), or the resin substrate can be peeled off from the laminate of resin substrate / absorption type polarizing film, and any appropriate protective layer corresponding to the purpose can be laminated on the peeled surface or on the side opposite to the peeled surface. The details of the method for manufacturing such an absorption type polarizing film are described in, for example, Japanese Patent Publication No. 2012-73580 and Japanese Patent No. 6470455. The entire contents of these publications are incorporated into this specification by reference.
[0090] The orthogonal transmittance (Tc) of the absorbing polarizing element (absorbing polarizing film) is preferably 0.5% or less, more preferably 0.1% or less, and further preferably 0.05% or less. The single transmittance (Ts) of the absorbing polarizing element (absorbing polarizing film) is, for example, 41.0% to 45.0%, and preferably 42.0% or more. The polarization degree (P) of the absorbing polarizing element (absorbing polarizing film) is, for example, 99.0% to 99.997%, and preferably 99.9% or more.
[0091] The orthogonal transmittance (Tc) of the reflective portion is preferably 0.5% or less, more preferably 0.1% or less, and further preferably 0.05% or less. By satisfying such an orthogonal transmittance, it is possible to suppress the user's visual recognition of afterimages (ghosts), and to achieve excellent display characteristics. The single-body transmittance (Ts) of the reflective portion is preferably 40.0% to 45.0%, and more preferably 41.0% or more. The polarization degree (P) of the reflective portion is preferably 99.0% to 99.997%, and more preferably 99.9% or more.
[0092] The optical characteristics of the reflective portion may be equivalent to the optical characteristics of the reflective polarization element or the optical characteristics of a laminate of a reflective polarization element and an absorptive polarization element. The optical characteristics can be extremely well achieved by combining an absorptive polarization element with a reflective polarization element.
[0093] As described above, the second phase difference member, the reflective polarization member, and the absorption polarization member used as needed are integrated. The embodiment of the present invention also includes such an integrated product (laminated body). The laminated body can be used, for example, Figure 1 A display system (representatively, its lens portion).
[0094] Example
[0095] The present invention will be described in detail below with reference to examples, but the present invention is not limited to these examples. It should be noted that the thickness is a value measured by the following measurement method.
[0096] <Thickness>
[0097] The thickness of 10 μm or less was measured using a scanning electron microscope (manufactured by JEOL Ltd., product name “JSM-7100F”). The thickness exceeding 10 μm was measured using a digital micrometer (manufactured by Anritsu Co., Ltd., product name “KC-351C”).
[0098] [Manufacturing Example 1: Preparation of Polarizing Plate 1]
[0099] A polyvinyl alcohol film with an average degree of polymerization of 2400, a saponification degree of 99.9 mol%, and a thickness of 30 μm was immersed in warm water at 30°C, and uniaxially stretched the PVA resin film while swelling it so that the length of the film was 2.0 times the original length. Next, it was immersed in a 0.3 wt% (weight ratio: iodine / potassium iodide = 0.5 / 8) iodine solution at 30°C, and uniaxially stretched the PVA resin film so that the length of the film was 3.0 times the original length while dyeing it. Then, in an aqueous solution of 4 wt% boric acid and 5 wt% potassium iodide, the PVA resin film was stretched so that the length of the film was 6 times the original length. Furthermore, after iodine ion impregnation treatment was carried out in an aqueous solution of 3 wt% potassium iodide (iodine impregnation bath), it was dried in an oven at 60°C for 4 minutes to obtain a polarizing film with a thickness of 12 μm.
[0100] On both sides of the polarizing film, a long HC-TAC film and a long acrylic resin film (thickness 20 μm) serving as an inner protective layer were laminated in such a manner that the longitudinal directions thereof were aligned with each other, thereby obtaining a polarizing plate 1. It should be noted that the HC-TAC film is a film having a hard coating (HC) layer (thickness 7 μm) formed on a triacetylcellulose (TAC) film (thickness 25 μm), and the film was laminated in such a manner that the TAC film became the polarizer side.
[0101] [Manufacturing Example 2: Preparation of λ / 4 Member 1]
[0102] In a batch polymerization apparatus consisting of two vertical reactors equipped with stirring blades and a reflux condenser controlled at 100° C., 29.60 parts by weight (0.046 mol) of bis[9-(2-phenoxycarbonylethyl)fluoren-9-yl]methane, 29.21 parts by weight (0.200 mol) of isosorbide (ISB), 42.28 parts by weight (0.139 mol) of spiroglycol (SPG), 63.77 parts by weight (0.298 mol) of diphenyl carbonate (DPC), and 1.19×10-6 parts by weight of calcium acetate monohydrate as a catalyst were charged. -2 Weight parts (6.78×10 -5mol). After the reactor was replaced with nitrogen under reduced pressure, it was heated by a heat medium and stirring was started when the internal temperature reached 100°C. The internal temperature reached 220°C 40 minutes after the start of the temperature rise, and the pressure was reduced while controlling to maintain the temperature, so that it reached 13.3kPa after 90 minutes after reaching 220°C. The phenol vapor produced as a by-product during the polymerization reaction was introduced into a 100°C reflux condenser, so that a certain amount of monomer components contained in the phenol vapor was returned to the reactor, and the uncondensed phenol vapor was introduced into a 45°C condenser for recovery. After nitrogen was introduced into the first reactor to temporarily restore it to atmospheric pressure, the reaction liquid after oligomerization in the first reactor was transferred to the second reactor. Next, the temperature rise and pressure reduction in the second reactor were started, so that it reached an internal temperature of 240°C and a pressure of 0.2kPa after 50 minutes. Then, the polymerization was carried out until the given stirring power was reached. When the predetermined power was reached, nitrogen gas was introduced into the reactor to restore the pressure, and the produced polyester carbonate resin was extruded into water, and the strands were cut to obtain pellets.
[0103] After the obtained polyester carbonate resin (pellets) was vacuum dried at 80°C for 5 hours, a long strip of resin film with a thickness of 130 μm was prepared using a film-making device equipped with a single screw extruder (manufactured by Toshiba Machine Co., Ltd., cylinder setting temperature: 250°C), a T-die (width 200 mm, setting temperature: 250°C), a chilled roll (setting temperature: 120-130°C) and a winder. The obtained long strip of resin film was stretched in the width direction at a stretching temperature of 140°C and a stretching ratio of 2.7 times. Thus, a phase difference film (λ / 4 component 1) with a thickness of 47 μm, a Re (590) of 143 nm, and an Nz coefficient of 1.2 was obtained.
[0104] [Manufacturing Example 3: Preparation of λ / 4 Member 2]
[0105] After adding 55 parts by weight of the compound represented by formula (I), 25 parts by weight of the compound represented by formula (II), and 20 parts by weight of the compound represented by formula (III) to 400 parts by weight of cyclopentanone (CPN), the mixture was heated to 60°C and stirred to dissolve. Then, the solution of the above-mentioned compounds was returned to room temperature, 3 parts by weight of IRGACURE 907 (manufactured by BASF Japan Co., Ltd.), 0.2 parts by weight of MEGAFAC F-554 (manufactured by DIC Corporation), and 0.1 parts by weight of p-methoxyphenol (MEHQ) were added to the solution of the above-mentioned compounds, and the mixture was further stirred. The stirred solution was transparent and uniform. The obtained solution was filtered with a 0.20 μm membrane filter to obtain a polymerizable composition.
[0106] Separately, a polyimide solution for an alignment film was applied to a glass substrate having a thickness of 0.7 mm by spin coating, dried at 100° C. for 10 minutes, and then fired at 200° C. for 60 minutes to obtain a coating film. The obtained coating film was rubbed with a commercially available rubbing device to form an alignment film.
[0107] Next, the polymerizable composition obtained above was applied to a substrate (substantially an alignment film) by spin coating and dried at 100° C. for 2 minutes. After the obtained coating film was cooled to room temperature, a high pressure mercury lamp was used to illuminate the film at 30 mW / cm 2 Thus, a liquid crystal alignment fixing layer (λ / 4 member 2) having a thickness of 1.5 μm, Re (590) of 143 nm, and an Nz coefficient of 1.0 was obtained.
[0108] [Chemical formula 1]
[0109]
[0110] [Chemical formula 2]
[0111]
[0112] [Example 1]
[0113] (Production of Laminated Body 1)
[0114] Polarizer 1 was arranged on a reflective polarizing film ("APCFG4" manufactured by Nitto Denko Corporation) via an adhesive in such a manner that the reflection axis of the reflective polarizing film and the absorption axis of the polarizing film of polarizer 1 were parallel to each other, thereby obtaining a laminate of reflective polarizing film / polarizer 1. Next, the phase difference film 1 (the second λ / 4 component) of manufacturing example 2 was bonded to the surface of the reflective polarizing film on the side where the polarizer was not provided via an adhesive. Among them, the phase difference film 1 was bonded in such a manner that the slow axis of the phase difference film 1 formed an angle of 45° with respect to the reflection axis of the reflective polarizing film and the absorption axis of the polarizing film of the polarizer 1. In this way, a laminate 1 having a structure of (λ / 4) component 1 / reflective polarizing film / polarizer 1 was obtained. The polarizer 1 side of the laminate 1 was bonded to a glass (lens substitute) formed with an anti-reflection layer via an adhesive, thereby obtaining an evaluation sample E1 having a structure of (λ / 4) component 1 / reflective polarizing film / polarizer 1 / glass / anti-reflection layer.
[0115] [Example 2]
[0116] The λ / 4 member 1 side of the laminate 1 obtained in Example 1 was bonded to the same glass as in Example 1 via an adhesive to obtain an evaluation sample E2 having a structure of antireflection layer / glass / (λ / 4) member 1 / reflective polarizing film / polarizer 1.
[0117] [Comparative Example 1]
[0118] A laminate of a reflective polarizing film / polarizer 1 was obtained in the same manner as in Example 1. The polarizer 1 side of the obtained laminate was bonded to the same glass as in Example 1 via an adhesive, and an evaluation sample C1-1 having a structure of a reflective polarizing film / polarizer 1 / glass / anti-reflection layer was obtained. On the other hand, a second λ / 4 member 1 similar to that in Example 1 was bonded to the same glass as in Example 1 via an adhesive, and an evaluation sample C1-2 having a structure of a (λ / 4) member 1 / glass / anti-reflection layer was obtained.
[0119] The evaluation results are shown in Table 1.
[0120] <Evaluation>
[0121] As an evaluation device, an ultraviolet visible spectrophotometer (manufactured by Otsuka Electronics Co., Ltd., "LPF-200") was used. A laminate having the polarizer 1 of manufacturing example 1 and the phase difference film 1 (first λ / 4 component) of manufacturing example 2 in order from the light source side was arranged on the exit side of the light source of the spectrophotometer. Among them, the angle formed by the absorption axis of the polarizing film of the polarizer 1 and the slow axis of the first λ / 4 component 1 was 45°. The evaluation samples of the embodiments and comparative examples were arranged on the exit side of the laminate as described below.
[0122] (Evaluation Sample E1 of Example 1)
[0123] The same glass as the evaluation sample E1 is arranged on the light source side, and the evaluation sample E1 is arranged 1 mm to 3 mm away from the light source side glass in such a way that the second λ / 4 component 1 is opposite to the glass on the light source side. The angle of the optical axis of the evaluation sample E1 and the light source side laminate is as follows. It should be noted that "0°" corresponds to the length direction of the evaluation sample E1, and the angle is the counterclockwise angle relative to the length direction.
[0124] Absorption axis of the absorbing polarizing film of the light source side laminate: 0°
[0125] Slow axis of the first λ / 4 member of the light source side stack: 135°
[0126] Slow axis of the second λ / 4 member in the evaluation sample E1: 45°
[0127] Reflection axis of the reflective polarizing film in the evaluation sample E1: 90°
[0128] Absorption axis of the absorbing polarizing film in the evaluation sample E1: 90°
[0129] (Evaluation Sample E2 of Example 2)
[0130] The evaluation sample E2 was arranged so that the glass was on the light source side, and the same glass as the evaluation sample E2 was arranged on the polarizing plate 1 side of the evaluation sample E2 at a distance of 1 mm to 3 mm from the polarizing plate 1. The angles of the optical axes of the optical members were the same as those in Example 1.
[0131] (Evaluation samples C1-1 and C1-2 of Comparative Example 1)
[0132] The evaluation sample C1-2 was arranged so that the glass was on the light source side, and the evaluation sample C1-1 was arranged on the λ / 4 member 1 side of the evaluation sample C1-2 at a distance of 1 mm to 3 mm from the evaluation sample C1-2 so that the reflective polarizing film was opposite to the second λ / 4 member 1. The angles of the optical axes of the optical members were the same as those in the first embodiment.
[0133] In the above state (this state is referred to as the reference state), the single transmittance of the evaluation sample was measured using an ultraviolet visible spectrophotometer (manufactured by Otsuka Electronics Co., Ltd., "LPF200"). The single transmittance is a Y value obtained by measuring the 2-degree field of view (C light source) of JIS Z8701 and correcting for visibility. Next, the single transmittance was measured in the same manner as above, with the component on the light source side rotated 3° and 10° counterclockwise relative to the reference state. The results are shown in Table 1.
[0134] [Table 1]
[0135]
[0136] As is clear from Table 1, according to the embodiment of the present invention, it is possible to prevent the increase in transmittance caused by the deviation of the axis arrangement of the optical axes (slow axis, reflection axis, and absorption axis) of each member, and thus it is possible to suppress ghosts well. It was confirmed that the same result was obtained even if the λ / 4 member 2 of Manufacturing Example 3 was used instead of the λ / 4 member 1 of Manufacturing Example 2.
[0137] The present invention is not limited to the above-described embodiments, and various modifications are possible. For example, the above-described embodiments may be replaced with substantially the same configuration, a configuration that exhibits the same effects, or a configuration that achieves the same purpose.
[0138] Industrial Applicability
[0139] The lens unit according to the embodiment of the present invention can be used for a display body such as VR goggles, for example.
Claims
1. A lens unit used in a display system for displaying an image to a user, The lens portion comprises: A reflective polarizing member that reflects light emitted forward from a display surface of a display element that displays an image and that passes through the polarizing member and the first λ / 4 member; an absorption-type polarization component, which is arranged in front of the reflection-type polarization component; A first lens portion disposed on an optical path between the display element and the reflective polarization component; a half mirror disposed between the display element and the first lens portion, transmitting light emitted from the display element and reflecting light reflected from the reflective polarizing member toward the reflective polarizing member; as well as a second λ / 4 member disposed on an optical path between the half mirror and the reflective polarization member, The second λ / 4 component and the reflective polarization component are integrated.
2. The lens unit according to claim 1, in, The reflection axis of the reflective polarization element and the absorption axis of the absorptive polarization element are arranged parallel to each other.
3. The lens unit according to claim 1, in, The first lens portion is integral with the half mirror. 4 . The lens unit according to claim 1 , further comprising a second lens unit disposed in front of the absorbing polarization element.
5. The lens portion according to claim 1, in, The angle between the absorption axis of the polarization member included in the display element and the slow axis of the first λ / 4 member is 40° to 50°. The angle formed between the absorption axis of the polarization member included in the display element and the slow axis of the second λ / 4 member is 40° to 50°.
6. The lens portion according to claim 1, in, The second λ / 4 element, the reflective polarization element, and the absorbing polarization element are integrated.
7. A laminated body used for the lens portion according to any one of claims 1 to 6, The stacked body includes the second λ / 4 member and the reflective polarization member. The laminated body according to claim 7 , further comprising the absorbing polarization member.
9. The laminate according to claim 8, in, The reflection axis of the reflective polarization element and the absorption axis of the absorptive polarization element are arranged parallel to each other. 10 . A display body comprising the lens portion according to claim 1 . 11 . A method for producing a display comprising the lens portion according to claim 1 .
12. A display method, comprising: a step of allowing the light of the display image emitted through the polarization element and the first λ / 4 element to pass through the half mirror and the first lens portion; a step of allowing the light that has passed through the half mirror and the first lens portion to pass through a second λ / 4 member; A step of causing the light after passing through the second λ / 4 member to be reflected toward the half mirror by a reflective polarization member; A step of allowing the light reflected by the reflective polarization member and the half mirror to pass through the reflective polarization member via the second λ / 4 member; as well as a step of causing the light transmitted through the reflective polarization member to pass through an absorptive polarization member, The second λ / 4 component and the reflective polarization component are integrated.
Citation Information
Patent Citations
Elliptical polarization plate and picture display device using it
JP2006163343A
Method of producing elliptically polarizing plate and image display using the elliptically polarizing plate
JP2006178389A
Circularly polarizing plate and display device
JP2014010291A
Polarizing plate and organic el panel
JP2014026266A
Retardation film, circularly polarizing plate, and image display device
JP2015212816A