Nonaqueous electrolyte secondary battery
By designing a wound electrode body in a lithium-ion secondary battery and setting a spacer on the outermost peripheral surface of the electrode body, the problem of low heat discharge efficiency of the electrode body is solved, the contact between the electrode body and the outer can is improved, and the charging is extended Discharge cycle characteristics.
Patent Information
- Application Number
- CN202380028402.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-29
- Filing Date
- 2023-03-23
- Publication Date
- 2024-11-01
AI Technical Summary
In the lithium-ion secondary battery, the fixing method of the outer peripheral portion of the electrode body causes a decrease in heat discharge efficiency, affecting the charge and discharge cycle characteristics.
A winding electrode body structure is adopted, in which the positive electrode plate and the negative electrode plate are wound by a spacer, and the negative electrode core or the positive electrode core is exposed to the outermost peripheral surface of the electrode body, and a spacer is provided on the outermost peripheral surface to clamp the unfixed belt. The attached part ensures contact with the external can and improve heat discharge efficiency.
Through the design of the spacer, the electrode body can contact the external can more effectively, improve heat discharge efficiency, extend the charge and discharge cycle characteristics, and maintain the heat dissipation performance and insertion smoothness of the electrode body.
Smart Images

Figure CN118891769A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a nonaqueous electrolyte secondary battery. Background Art
[0002] In recent years, non-aqueous electrolyte secondary batteries such as lithium ion secondary batteries have been used as power sources for electric vehicles (EVs), large power storage devices, etc. In this secondary battery, charging and discharging are repeatedly performed. If heat is accumulated in the outer can that contains the electrode body as the power generation element, the durability will tend to decrease. In particular, in order to use lithium ion batteries for purposes such as EVs, it is necessary to be able to withstand use under harsh conditions such as rapid charging and discharging, but it is known that the heat generation of lithium ion batteries increases during rapid charging and discharging. Therefore, in Patent Documents 1 and 2, a technology that can efficiently release the heat generated in the outer can is disclosed.
[0003] Specifically, Patent Document 1 discloses a secondary battery in which a wound electrode body formed by winding a positive electrode plate and a negative electrode plate with a separator interposed therebetween is housed in an outer can. In this secondary battery, the outermost peripheral portion of the electrode body has a single-sided coated portion having a negative electrode mixture layer of the negative electrode plate formed only on one side, and an uncoated portion disposed at a position closer to the winding end side and having both sides of the negative electrode core of the negative electrode plate exposed, and the exposed surfaces of the negative electrode core of the single-sided coated portion and the uncoated portion are in contact with the inner surface of the outer can.
[0004] Patent document 2 discloses a secondary battery in which a negative electrode plate having a negative electrode mixture layer formed on only one side is coated on the outermost periphery of the electrode body, and the exposed surface of the negative electrode core on the opposite side of the negative electrode mixture layer of the single-sided coating portion contacts the inner surface of the outer can.
[0005] Prior Art Literature
[0006] Patent Literature
[0007] Patent Document 1: International Publication No. 2009 / 144919
[0008] Patent Document 2: Japanese Patent Application Publication No. 2013-254561 Summary of the invention
[0009] Patent Documents 1 and 2 do not mention the method for fixing the outer periphery of the electrode body. Generally speaking, in order to maintain the winding structure of the electrode body and to smoothly insert the electrode body into the outer can, the following operation is performed: an insulating tape is attached to the outermost periphery of the electrode body to fix the winding end side end to the outermost periphery. However, since the insulating tape is arranged at the outermost periphery of the electrode body, the contact between the outermost negative electrode core and the inner surface of the outer can may be hindered. As a result, the heat release efficiency of the electrode body in the outer can is reduced, which may cause a decrease in the cycle characteristics during charge and discharge.
[0010] An object of the present disclosure is to improve the efficiency of heat release of an electrode body in a structure in which the outermost periphery of the electrode body is fixed by a tape in a nonaqueous electrolyte secondary battery.
[0011] The non-aqueous electrolyte secondary battery disclosed herein comprises: a wound electrode body, including a strip-shaped positive electrode plate with a positive electrode mixture layer formed on both sides of a positive electrode core body, and a strip-shaped negative electrode plate with a negative electrode mixture layer formed on both sides of a negative electrode core body, and the positive electrode plate and the negative electrode plate are wound with a separator interposed therebetween; and an outer can accommodating the electrode body, wherein the negative electrode core body or the positive electrode core body is exposed to the outermost peripheral surface of the electrode body, and one or more portions of the end portion of the winding termination side of the outermost peripheral surface are fixed by one or more strips, and an area to which one or more strips are attached in the outermost peripheral surface is set as a first area, and an area to which no strips are attached is set as a second area, and when an area overlapping with the second area in the inner surface of the outermost peripheral part of the electrode plate having the outermost peripheral surface among the negative electrode plate and the positive electrode plate is set as a third area, a separator is provided in a part of the third area opposite to the second area and sandwiching the outermost peripheral part.
[0012] According to the non-aqueous electrolyte secondary battery disclosed herein, the portion of the outermost periphery of the electrode body that is not attached with the tape can be squeezed outward by the spacer. Thus, although the outermost periphery of the electrode body is fixed by the tape, the portion of the outermost periphery of the electrode body that is not attached with the tape is also easy to contact the outer can. Therefore, the electrode body can easily dissipate heat through the outer can, thereby improving the heat release efficiency of the electrode body. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 It is a cross-sectional view along the axial direction of a nonaqueous electrolyte secondary battery according to an example of an embodiment.
[0014] Figure 2 It is a perspective view of an electrode body constituting a nonaqueous electrolyte secondary battery according to an example of the embodiment.
[0015] Figure 3 This is a diagram showing the outer surface of the outermost roll in a developed view of a negative electrode plate constituting a nonaqueous electrolyte secondary battery of an example of an embodiment.
[0016] Figure 4 is Figure 3 The unfolded view of the negative electrode plate shows the inner surface of the roll at the outermost peripheral portion.
[0017] Figure 5 yes Figure 2 A cross-sectional view near the outermost periphery of an electrode body.
[0018] Figure 6 This is a perspective view of the electrode body in Example 3.
[0019] Figure 7 This is a perspective view of the electrode body in Comparative Example 1.
[0020] Figure 8 This is a perspective view of the electrode body in Comparative Example 2. DETAILED DESCRIPTION
[0021] Hereinafter, the embodiments of the present invention will be described in detail with reference to the accompanying drawings. In the following description, specific shapes, materials, numbers, numerical values, directions, etc. are examples for making the present invention easy to understand, and can be appropriately changed to match the specifications of the non-aqueous electrolyte secondary battery. In addition, below, regarding the term "substantially", in addition to the completely identical situation, it is also used to include the meaning of the situation that can be regarded as substantially the same. Further, below, in the case of including a plurality of embodiments and variations, it was originally envisioned that their characteristic parts were appropriately combined and used.
[0022] Figure 1 It is a cross-sectional view along the axial direction of the nonaqueous electrolyte secondary battery 10 according to the embodiment. Figure 2 It is a perspective view of the electrode body 14 constituting the nonaqueous electrolyte secondary battery 10 . Figure 3 1 is a diagram showing the outer surface of the outermost rolled portion in a developed view of the negative electrode plate 12 constituting the nonaqueous electrolyte secondary battery 10. Figure 4 1 is a diagram showing the inner surface of the outermost roll in the development view of the negative electrode plate 12. Figures 1 to 4 As shown, the nonaqueous electrolyte secondary battery 10 has a wound electrode body 14, a nonaqueous electrolyte (not shown), an outer can 15 and a sealing body 16. The wound electrode body 14 has a positive electrode plate 11, a negative electrode plate 12 and a separator 13, and the positive electrode plate 11 and the negative electrode plate 12 are wound into a spiral shape across the separator 13. Hereinafter, one axial side of the electrode body 14 is sometimes referred to as "upper" and the other axial side is referred to as "lower". The nonaqueous electrolyte includes a nonaqueous solvent and an electrolyte salt dissolved in the nonaqueous solvent. The nonaqueous electrolyte is not limited to a liquid electrolyte, and may also be a solid electrolyte using a gel polymer or the like.
[0023] The positive electrode tab 19 as a conductive member is joined and electrically connected to the positive electrode plate 11. The positive electrode tab 19 is a conductive member for electrically connecting the positive electrode core body constituting the positive electrode plate 11 to the positive terminal, and extends from the upper end of the positive electrode core body in the electrode body 14 to one side (upper) in the axial direction α. The positive electrode tab 19 is preferably made of a metal with aluminum as the main component. The positive electrode plate 11 has a positive electrode mixture layer formed on the inner surface (radial inner side) and the outer surface (radial outer side) of the positive electrode core body.
[0024] like Figure 3 , Figure 4As shown, the negative electrode plate 12 has a strip-shaped negative electrode core 12a and a negative electrode tab 20 ( Figure 1 , Figure 2 The negative electrode tab 20 is a conductive member for electrically connecting the negative electrode core 12a to the bottom of the outer can 15 described later, and extends from the lower end of the negative electrode core 12a in the electrode body 14 to the axial direction α ( Figure 1 , Figure 2 ) extends from the other side (below). The outer can 15 becomes the negative terminal. The negative electrode contact 20 is, for example, arranged on the inner side portion (inner peripheral side portion) of the roll of the electrode body 14. The negative electrode contact 20 can also be arranged on the outer side portion (outer peripheral side portion) of the roll of the electrode body 14. The negative electrode contact 20 is a strip-shaped conductive member. The constituent material of the negative electrode contact is not particularly limited. The negative electrode contact is preferably composed of a metal with nickel or copper as the main component, or a metal containing both nickel and copper. Furthermore, the negative electrode plate 12 is respectively formed with a negative electrode mixture layer 12b on the inner surface (radial inner side) and the outer surface (radial outer side) of the roll of the negative electrode core 12a.
[0025] Furthermore, if Figure 3 As shown, at the winding end side end of the negative electrode plate 12, no negative electrode mixture layer is formed on the negative electrode core 12a on the outer surface of the winding, so that a core exposed surface 12c where the negative electrode core 12a is exposed is formed.
[0026] As described above, the electrode body 14 has a wound structure in which the positive electrode plate 11 and the negative electrode plate 12 are wound in a spiral shape with the separator 13 interposed therebetween. The positive electrode plate 11, the negative electrode plate 12, and the separator 13 are all formed in a strip shape, and are wound in a spiral shape to form a radial direction β ( Figure 1 In the electrode assembly 14, the electrode plate length direction γ of each electrode plate becomes the winding direction.
[0027] Furthermore, if Figure 2 As shown, the outermost peripheral surface of the electrode body 14 is provided with a core exposed surface 12c where the negative electrode core 12a is exposed as described above. The core exposed surface 12c is connected to the cylindrical portion 15a ( Figure 1 ) to be electrically connected to the outer can 15. The electrical connection between the negative electrode plate 12 and the cylindrical portion 15a of the outer can 15 can ensure better current collection and transfer the heat of the electrode body 14 to the outer can 15 to improve the heat dissipation performance.
[0028] On the other hand, the outermost winding end of the electrode body 14 is fixed by two fixing bands 30. Figure 3In the outer surface of the winding end side end of the outermost circumference of the negative electrode core 12a shown in the figure, two fixing tapes 30 are attached along the length direction γ of the electrode plate at the positions indicated by the oblique lines at both ends of the electrode plate width direction δ. Each fixing tape 30 is an adhesive tape with an adhesive layer provided on one side of the base layer. Figure 2 As shown, in the state where the electrode body 14 is formed, a portion of each fixing tape 30 is attached to Figure 3 The oblique line portion of the negative electrode plate 12 includes a portion of the length direction γ of the winding end side end 12d, and the remaining portion of each fixing tape 30 is wound around the winding end side end 12d in the winding direction. Figure 3 The rest of the slashed part is attached in the same way. Figure 2 As shown, the winding end side end of the electrode body 14 is fixed to the outermost peripheral surface of the electrode body 14 by each fixing tape 30. Figure 2 In FIG. 1 , each fixing belt 30 is shown by a diagonal grid.
[0029] In this way, the fixing tape 30 is provided on a part of the outermost peripheral surface of the electrode body 14, and thus, due to the thickness of the fixing tape 30, a height difference is generated between the attached portion of the fixing tape 30 provided on the outermost peripheral surface of the electrode body and the unattached portion of the fixing tape. Therefore, although the core exposed surface 12c is located on the outermost peripheral surface of the electrode body 14, the contact between the core exposed surface 12c and the outer can 15 may be blocked by the fixing tape 30. In this embodiment, in order to eliminate such an undesirable situation, as described in detail later, a spacer 32 ( Figure 5 ).exist Figure 2 In FIG. 1 , a portion where the separator 32 is provided inside the roll of the negative electrode plate 12 is indicated by a dotted portion.
[0030] exist Figure 1 In the example shown, a metal battery case for accommodating an electrode body 14 and a non-aqueous electrolyte is formed by an outer can 15 and a sealing body 16. Insulating plates 17 and 18 are provided above and below the electrode body 14, respectively. A positive electrode tab 19 extends toward the sealing body 16 through a through hole of the upper insulating plate 17 and is welded to the lower surface of a filter 22 serving as the bottom plate of the sealing body 16. In the non-aqueous electrolyte secondary battery 10, a top plate of the sealing body 16, i.e., a cover 26, which is electrically connected to the filter 22, serves as a positive terminal.
[0031] The outer can 15 is a bottomed cylindrical container having an opening, for example, a metal container having a bottomed cylindrical shape. A gasket 27 is provided between the outer can 15 and the sealing body 16 to ensure the airtightness inside the outer can 15. The outer can 15 has, for example, a groove 21 formed by spinning the side surface from the outside to the radial inside. The groove 21 is preferably formed in an annular shape along the circumference of the outer can 15, and the sealing body 16 is supported by its upper surface. The sealing body 16 seals the opening of the outer can 15.
[0032] The sealing body 16 has a filter 22, a lower valve body 23, an insulating member 24, an upper valve body 25, and a cover 26 stacked in sequence from the electrode body 14 side. The components constituting the sealing body 16 have, for example, a disc shape or a ring shape, and the components except the insulating member 24 are electrically connected to each other. The lower valve body 23 and the upper valve body 25 are connected to each other at their respective central portions, and the insulating member 24 is interposed between their respective peripheral portions. If the internal pressure of the battery rises due to abnormal heat, for example, the lower valve body 23 breaks, whereby the upper valve body 25 expands toward the cover 26 side and separates from the lower valve body 23, thereby cutting off the electrical connection between the two. If the internal pressure rises further, the upper valve body 25 breaks, and gas is discharged from the opening 26a of the cover 26.
[0033] The components of the electrode body 14 and the separator 32 disposed on the inner surface of the roll of the electrode body 14 at the outermost periphery are described in detail. The positive electrode plate 11 has a strip-shaped positive electrode core and a positive electrode mixture layer formed on both sides of the positive electrode core. For the positive electrode core, for example, a foil of a metal such as aluminum, a film obtained by disposing the metal on the surface layer, etc. can be used. A suitable positive electrode core is a foil of a metal having aluminum or an aluminum alloy as a main component. The thickness of the positive electrode core is, for example, 10 μm to 30 μm.
[0034] The positive electrode mixture layer preferably includes a positive electrode active material, a conductive agent, and a binder. A positive electrode mixture slurry including a positive electrode active material, a conductive agent, a binder, and a solvent such as N-methyl-2-pyrrolidone (NMP) is applied to both sides of the positive electrode core, and then dried and compressed to produce the positive electrode plate 11.
[0035] As the positive electrode active material, a lithium-containing transition metal oxide containing transition metal elements such as Co, Mn, and Ni can be exemplified. The lithium-containing transition metal oxide is not particularly limited, but is preferably a general formula Li1+ x A composite oxide represented by MO2 (wherein -0.2<x≤0.2, and M includes at least one of Ni, Co, Mn, and Al).
[0036] As the example of the above-mentioned conductive agent, carbon materials such as carbon black (CB) such as acetylene black (AB), ketjen black, graphite, etc. can be listed. As the example of the above-mentioned binding agent, fluorine resins such as polytetrafluoroethylene (PTFE), polyvinylidene fluoride (PVdF), polyacrylonitrile (PAN), polyimide (PI), acrylic resin, polyolefin resin, etc. can be listed. In addition, these resins and carboxymethyl cellulose (CMC) or its salt, polyethylene oxide (PEO), etc. can also be used in combination. They can both use one kind individually, and two or more combinations can also be used.
[0037] An exposed surface where the surface of the metal constituting the positive electrode core is exposed is formed in a portion of the positive electrode plate 11 in the longitudinal direction of the electrode plate. The exposed surface is a portion connected to the positive electrode tab 19 and is a portion of the surface of the positive electrode core that is not covered by the positive electrode mixture layer.
[0038] The negative electrode plate 12 includes a strip-shaped negative electrode core 12a and negative electrode mixture layers 12b formed on both sides of the negative electrode core 12a. The negative electrode core 12a may be made of, for example, a foil of a metal such as copper or a film having the metal disposed on the surface. The thickness of the negative electrode core 12a is, for example, 5 μm to 30 μm.
[0039] The negative electrode mixture layer 12 b preferably includes a negative electrode active material and a binder. For example, a negative electrode mixture slurry including a negative electrode active material, a binder and water is applied to both surfaces of the negative electrode core 12 a and then dried and compressed to produce the negative electrode plate 12 .
[0040] As the negative electrode active material, as long as it can reversibly absorb and release lithium ions, it is not particularly limited, for example, carbon materials such as natural graphite and artificial graphite, metals such as Si and Sn alloyed with lithium, or alloys and composite oxides containing them can be used. For the binder contained in the negative electrode active material layer, for example, the same resin as that in the case of the positive electrode plate 11 can be used. In the case of using an aqueous solvent to prepare the negative electrode mixture slurry, styrene-butadiene rubber (SBR), CMC or its salt, polyacrylic acid or its salt, polyvinyl alcohol, etc. can be used. They can be used alone or in combination of two or more.
[0041] At the winding end side end of the negative electrode plate 12 in the electrode plate length direction γ, there is formed a single-sided coated portion where the negative electrode mixture layer 12b is formed only on the inner surface of the winding, and an uncoated portion where both sides of the negative electrode core 12a are exposed closer to the winding end side than the single-sided coated portion. Figure 3 , Figure 4 In the embodiment, a single-side coated portion is formed in the range indicated by arrow D1, and an uncoated portion is formed in the range indicated by arrow D2 and coincident with the outermost circumference. Thus, a core exposed surface 12c is formed in the negative electrode plate 12 where the surface of the metal constituting the negative electrode core 12a is exposed.
[0042] Although not shown in the figure, the negative electrode plate 12 also has a core exposed surface formed at the winding start side end, and a negative electrode tab 20 is joined to the core exposed surface. The negative electrode tab 20 passes through the through hole of the lower insulating plate 18 and is welded to the inner surface of the bottom of the outer can 15.
[0043] For the separator 13, a porous sheet having ion permeability and insulation can be used. Specific examples of the porous sheet include microporous films, woven fabrics, non-woven fabrics, etc. As the material of the separator 13, olefin resins such as polyethylene and polypropylene are preferred. The thickness of the separator 13 is, for example, 10μm to 50μm. With the increase in capacity and output of the battery, the separator 13 tends to be thinner. The separator 13 has a melting point of, for example, about 130°C to 180°C.
[0044] Furthermore, two fixing bands 30 are bonded to the outermost peripheral surface of the electrode body 14, i.e., the outermost peripheral surfaces of the axial ends of the negative electrode core 12a of the negative electrode plate 12, so as to fix the winding end side end 12d of the negative electrode plate 12. The fixing bands 30 are made of the same material and have the same thickness, width, and length. The width and length of the fixing bands may be different from each other.
[0045] The fixing tape 30 is, for example, a PP tape having an adhesive layer formed on one surface of a polypropylene (PP) base layer. The base layer of the fixing tape 30 can be made of polyethylene (PE), polyimide (PI), polyethylene terephthalate (PET), or the like.
[0046] The outermost surface of the electrode body 14 is formed by the area where the two fixing tapes 30 are attached. Figure 3 The portion indicated by the oblique grid is defined as the first region A, the region to which the fixing tape 30 is not attached is defined as the second region B1, and the region overlapping the second region B1 on the inner surface of the outermost portion of the negative electrode plate 12 is defined as the third region B2. A spacer 32 ( Figure 2 ).
[0047] like Figure 3 As shown in FIG. 1 , the fixing tapes 30 are attached to the outermost peripheral surface of the negative electrode 12 with gaps between the two ends in the electrode width direction δ. Therefore, the second area B1 is provided in three parts of the outer surface of the roll: the two parts between the end in the electrode width direction δ and the end outside the electrode width direction δ of the attachment part of the fixing tape 30, and the part between the attachment parts of the two fixing tapes 30. Figure 4The negative electrode plate 12 is shown as having an outermost surface of the inner roll, and the separator 32 is attached and arranged in a portion of the third region in the center of the three third regions B2 corresponding to the three second regions B1. The negative electrode plate 12 is the electrode plate having the outermost surface of the electrode body 14 among the negative electrode plate 12 and the positive electrode plate 11.
[0048] Figure 5 : is a cross-sectional view near the outermost periphery of the electrode body 14. The spacer 32 is an elastic material and is the same tape as the fixing tape 30. For example, when the fixing tape 30 is a PP tape, the spacer 32 is also formed of the PP tape. The spacer is preferably a resin tape having an adhesive layer formed on one surface of a base layer, and for the base layer, polyethylene (PE), polyimide (PI), polyethylene terephthalate (PET), etc. can be used in the same manner as the fixing tape 30.
[0049] The spacer 32 is attached to a portion of the third region B2 at the center of the inner surface of the outermost portion of the negative electrode plate 12 along the electrode plate length direction γ. At this time, the spacer 32 does not protrude from both ends of the third region B2 in the electrode plate length direction γ. The presence of the spacer 32 enables the electrode body 14 to be formed, such as Figure 5 As shown, the portion of the negative electrode plate 12 corresponding to the second region B1 sandwiched between the two fixing tapes 30 is pressed outward so as to approach the inner surface of the cylindrical portion 15 a of the outer can 15 .
[0050] The spacer 32 is preferably provided in the central third region B2 at a position equidistant from both ends of the electrode plate in the width direction δ. In addition, in the central third region B2 where the spacer 32 is located, the area ratio of the portion contacted by the spacer 32 is preferably 50% or more, more preferably 80% or more. In addition, the thickness of the spacer 32 is preferably 50% or more and 150% or less of the thickness of the fixing tape 30.
[0051] According to the above-mentioned nonaqueous electrolyte secondary battery 10, the portion of the outermost periphery of the electrode body 14 not attached by the fixing tape 30 can be pressed outward by the spacer 32. Thus, although the outermost periphery of the electrode body 14 is fixed by the fixing tape 30, the portion of the outermost periphery of the electrode body 14 to which the fixing tape 30 is not adhered is also easy to contact the outer can 15. Therefore, the electrode body 14 is easy to dissipate heat through the outer can 15, so that the heat release efficiency of the electrode body 14 can be improved. Therefore, it is possible to take into account the maintenance of the winding structure of the electrode body 14 brought about by the outermost periphery of the electrode body 14 being fixed by the fixing tape 30, the improvement of the productivity when the electrode body 14 is inserted into the outer can 15, and the maintenance of the good contact between the electrode body 14 and the inner surface of the outer can 15. Furthermore, since the heat release efficiency generated in the outer can 15 can be improved, the cycle maintenance rate during charging and discharging can be improved.
[0052] Example
[0053] The inventors of the present disclosure prepared a total of five types of secondary batteries, namely Examples 1 to 3 and Comparative Examples 1 to 2, and charged and discharged them under given conditions, and compared the temperatures at the end of discharge that were substantially consistent with the maximum temperature of the secondary batteries during discharge, thereby confirming the effects of the embodiments.
[0054] [Example 1]
[0055] [Production of positive electrode plate]
[0056] As the positive electrode active material, LiNi 0.88 C0 0.09 Al 0.03 O2-represented lithium nickel oxide containing cobalt and aluminum. Then, 100 parts by mass of LiNi 0.88 Co 0.09 Al 0.03 O2, 1.0 parts by mass of acetylene black and 0.9 parts by mass of polyvinylidene fluoride (PVDF) (binder) are mixed in a solvent of N-methyl-2-pyrrolidone (NMP) to prepare a positive electrode mixture slurry. Next, the positive electrode mixture slurry is evenly applied on both sides of a long positive electrode core composed of an aluminum foil with a thickness of 15 μm, and dried in a dryer at a temperature of 100 to 150°C to remove the NMP. Thereafter, the product after the positive electrode mixture slurry is applied to both sides of the positive electrode core and dried is compressed by a roller press. Furthermore, the product having a positive electrode mixture layer formed on both sides of the positive electrode core after compression processing is cut into a given electrode size to produce a positive electrode plate 11. At this time, the thickness of the positive electrode plate 11 is 0.144 mm, the width is 62.6 mm, and the length is set to 861 mm. An exposed surface of the core body without the mixture layer is formed at one end portion in the longitudinal direction of the positive electrode plate 11 , and an aluminum positive electrode tab 19 is fixed to the exposed surface by welding.
[0057] [Manufacturing of negative electrode plate]
[0058] As the negative electrode active material, a mixture of 95 parts by mass of graphite powder and 5 parts by mass of silicon oxide was used. Then, 100 parts by mass of the negative electrode active material, 1 part by mass of styrene-butadiene rubber (SBR) as a binder, and 1 part by mass of carboxymethyl cellulose (CMC) as a thickener were mixed. Then, the mixed material was dispersed in water to prepare a negative electrode mixture slurry. The negative electrode mixture slurry was applied to both sides of a long strip of negative electrode core composed of a copper foil with a thickness of 8 μμm, dried by a dryer, and compressed with a roller of a roller press so that the thickness of the negative electrode became 0.160 mm, thereby adjusting the thickness of the negative electrode mixture layer. Then, the long strip of negative electrode core with a negative electrode mixture layer formed thereon was cut into a given electrode size, and a negative electrode plate 12 with a negative electrode mixture layer formed on both sides of the negative electrode core was produced. At this time, the width of the negative electrode plate 12 was 64 mm, and the length was set to 959 mm. Then, at one end of the negative electrode plate 12 in the longitudinal direction, located at the winding start side of the electrode body 14, a body exposed surface where no mixture layer exists and the core surface is exposed is provided, and a nickel negative electrode tab 20 is fixedly attached to the core exposed surface by welding. In addition, at the other end of the negative electrode plate 12 in the longitudinal direction, located at the outermost peripheral part of the electrode body 14, a core exposed surface where no mixture layer exists on both sides and the core surface is exposed is formed, and a third region B2 ( Figure 4 ) A separator 32 made of a tape made of polypropylene (PP) was attached to produce a negative electrode plate 12. At this time, the width of the separator 32 was 48 mm, the thickness was 30 μm, and the length was set to 62 mm. In addition, as shown in the column "Ratio of the separator area to the third region" in Table 1, the contact area ratio of the separator 32 to the central third region B2 was set to 80%.
[0059] [Table 1]
[0060]
[0061] [Production of electrode body]
[0062] The positive electrode plate 11 and the negative electrode plate 12 are wound into a spiral shape through a polyethylene separator 13, and a fixing tape 30 made of polypropylene (PP) with a width of 9 mm, a thickness of 30 μm and a length of 62 mm is attached to the two first regions A of the exposed surface of the core body at the outermost periphery. The outermost periphery of the winding end side is fixed by these fixing tapes 30, thereby producing Figure 2 The electrode body 14 shown. At this time, the core body exposed surface is arranged over the entire circumference of the outermost peripheral surface of the electrode body 14 except for the attached portion of the fixing tape 30 .
[0063] [Preparation of non-aqueous electrolyte]
[0064] To 100 parts by mass of a mixed solvent of ethylene carbonate (EC) and dimethyl carbonate (DMC) in a volume ratio of EC:DMC=1:3, 5 parts by mass of vinylene carbonate (VC) was added and dissolved so that LiPF6 became 1.5 mol / L, thereby preparing a non-aqueous electrolyte.
[0065] [Manufacturing of Secondary Batteries]
[0066] The electrode body 14 is contained in a bottomed cylindrical outer can 15, insulating plates 17 and 18 are arranged above and below the electrode body 14, respectively, the negative electrode tab is welded to the bottom of the outer can 15, and the positive electrode tab is welded to the sealing body 16, which is contained inside the outer can 15. After that, after a non-aqueous electrolyte is injected into the inner part of the outer can 15 by decompression, the sealing body 16 is riveted and fixed to the open end of the outer can 15 via a gasket 27, thereby manufacturing a cylindrical non-aqueous electrolyte secondary battery 10. At this time, the battery capacity is 4600 mAh.
[0067] [Example 2]
[0068] In Example 2, the thickness of the PP spacer 32 attached to the third region B2 was set to 15 μm, which was 1 / 2 of the thickness in Example 1. In Example 2, the structure other than this was the same as that in Example 1.
[0069] [Example 3]
[0070] In Example 3, as Figure 6 As shown in the electrode body 14 of the embodiment 1, the width of the PP spacer 32 attached to the third region B2 is set to 30 mm, which is smaller than the width in the case of Example 1. Therefore, as shown in the column "Spacer area ratio to the third region" in Table 1, the contact area ratio of the spacer 32 to the central third region B2 is set to 50%. In Example 3, the structure other than this is the same as that of Example 1.
[0071] [Comparative Example 1]
[0072] In Comparative Example 1, Figure 7 As shown in the electrode body 14a of FIG.
[0073] [Comparative Example 2]
[0074] In Comparative Example 2, Figure 8As shown in the electrode body 14b, a fixing tape 30a made of PP and having a width of 64 mm is attached to the entire outer surface of the exposed surface of the core body at the outermost periphery, and the second area B1 and the third area B2 ( Figure 2 ). In Comparative Example 2, the structure other than this is the same as that of Example 1.
[0075] [Test method]
[0076] In order to evaluate the heat dissipation to the outside of the outer can 15, which has an impact on the cycle characteristics, using the non-aqueous electrolyte secondary batteries of the above-mentioned Examples 1-3 and Comparative Examples 1-2, a comparison was made of the temperature at the end of discharge that was roughly consistent with the highest temperature during discharge. In the test, the manufactured secondary battery was charged with a constant current of 1380mA (0.3It) in an environment of 25°C until the battery voltage reached 4.2V, and then charged with a constant voltage of 4.2V until the current value reached 92mA. Furthermore, after a rest of 20 minutes, a constant current discharge was performed with a discharge current of 4600mA (1.0It), and the temperature of the secondary battery at the end of discharge was measured by a thermocouple installed on the surface of the outer can 15. The electrode body of the secondary battery generates heat during discharge, and its temperature rises toward the end of discharge. Therefore, by measuring the temperature at the end of discharge, a temperature roughly consistent with the highest temperature of the secondary battery during discharge can be obtained.
[0077] [Test results]
[0078] The temperature measurement results of each secondary battery are shown in the column "Discharge end temperature" in Table 1. As shown in Table 1, it can be confirmed that in Examples 1-3, the temperature at the end of discharge can be lowered compared to Comparative Examples 1-2. In addition, in Comparative Example 2, the temperature at the end of discharge becomes very high. The reason for this is believed to be that in Comparative Example 2, the electrode body 14b ( Figure 8 ) is entirely covered by the fixing tape 30a, and the heat conduction from the electrode body 14b to the outer can 15 is hindered by the fixing tape 30a. In addition, in Comparative Example 1, the temperature at the end of discharge decreases compared to Comparative Example 2, but the decrease is not sufficient compared to Examples 1-3. The reason for this is believed to be that in Comparative Example 1, due to the Figure 7 ) is provided at the outermost periphery of the fixing tape 30 and the unattached portion of the fixing tape, thereby preventing the core exposed surface 12c of the outermost periphery of the electrode body 14a from contacting the inner surface of the outer can 15. On the other hand, in Examples 1-3, in the electrode body 14 ( Figure 2 , Figure 6) is provided with a spacer 32 in the third region B2 of the inner surface of the roll at the outermost periphery. As a result, it is considered that the contact between the core exposed surface 12c at the outermost periphery of the electrode body 14 and the inner surface of the outer can 15 is improved, and thus, the temperature rise caused by heat generation can be suppressed by heat dissipation through the outer can 15, and the temperature drops when the discharge is completed.
[0079] Compared with Example 1, the temperature at the end of discharge in Example 2 becomes higher. The reason for this is believed to be that the thickness of the spacer 32 attached to the third area B2 is thin, and the contact between the core exposed surface 12c of the outermost peripheral part of the electrode body 14 and the inner surface of the outer can 15 is insufficient compared with Example 1.
[0080] Compared with Example 1, the temperature at the end of discharge in Example 3 becomes higher. The reason for this is believed to be that the contact area ratio of the spacer 32 relative to the third region B2 is small, and the contact between the core exposed surface 12c of the outermost peripheral part of the electrode body 14 and the inner surface of the outer can 15 is insufficient compared with Example 1.
[0081] In the above-mentioned embodiment, the case where the spacer 32 is an adhesive tape is described, but the spacer may also be an elastic body such as a resin without an adhesive layer. On the other hand, when the spacer is an adhesive tape, the spacer can be easily provided on the inner surface of the roll of the outermost peripheral portion of the negative electrode plate by attaching. Therefore, from the perspective of improving the productivity of the secondary battery, it is preferred that the spacer be an adhesive tape.
[0082] In addition, in the above-mentioned embodiment, as long as one or more portions of the winding end side end of the outermost peripheral surface of the electrode body are fixed by one or more tapes, only one portion of the winding end side end of the outermost peripheral surface of the electrode body may be fixed by one fixing tape. In this case, in the outermost peripheral surface of the electrode body, the area to which one fixing tape is attached becomes the first area, and the area to which the fixing tape is not attached becomes the second area. The separator is provided in a part of the third area overlapping the second area in the inner surface of the outermost peripheral portion of the negative electrode plate having the outermost peripheral surface.
[0083] In addition, in the above-mentioned embodiment, the case where the fixing tape 30 is arranged along the winding direction consistent with the electrode plate length direction of the electrode body is described, but the structure of the present disclosure is not limited to this, and the fixing tape can also be arranged along the axial direction consistent with the electrode plate width direction and the winding end side end of the electrode body is fixed to the outermost peripheral surface. In this case, a spacer is provided in a part of the third area overlapping with the second area other than the first area of the outer surface of the roll to which the fixing tape is attached, in the inner surface of the roll of the outermost peripheral part of the negative electrode plate.
[0084] In addition, in the above-mentioned embodiment, the case where the exposed surface 12c of the core of the negative electrode plate 12 is located on the outermost peripheral surface of the electrode body 14, and the exposed surface 12c of the core is in contact with the inner surface of the outer can 15 is described. On the other hand, the structure of the present disclosure is not limited to this, and it can also be set as a structure where the exposed surface of the core of the positive electrode plate is located on the outermost peripheral surface of the electrode body, and the exposed surface of the core is in contact with the inner surface of the outer can. In this case, the outer can becomes the positive terminal. In addition, the sealing body can be set as the negative terminal by leading the negative electrode tab connected to the negative electrode plate of the electrode body toward the sealing body and connecting it to the sealing body.
[0085] Explanation of symbols
[0086] 10 non-aqueous electrolyte secondary battery; 11 positive electrode plate; 12 negative electrode plate; 12a negative electrode core; 12b negative electrode mixture layer; 12c core exposed surface; 12d winding termination side end; 13 separator; 14, 14a, 14b electrode body; 15 outer can; 15a barrel; 16 sealing body; 17, 18 insulating plates; 19 positive electrode contact; 20 negative electrode contact; 21 slotted portion; 22 filter; 23 lower valve body; 24 insulating member; 25 upper valve body; 26 cover; 26a opening; 27 gasket; 30, 30a fixing belt; 32 spacer.
Claims
1. A non-aqueous electrolyte secondary battery comprising: A wound electrode body, comprising a strip-shaped positive electrode plate having a positive electrode mixture layer formed on both sides of a positive electrode core body, and a strip-shaped negative electrode plate having a negative electrode mixture layer formed on both sides of a negative electrode core body, wherein the positive electrode plate and the negative electrode plate are wound with a separator interposed therebetween; and an outer can accommodating the electrode body, The negative electrode core or the positive electrode core is exposed to the outermost peripheral surface of the electrode body, and one or more portions of the end portion on the winding end side of the outermost peripheral surface are fixed by one or more bands. In the outermost surface, an area to which the one or more tapes are attached is set as the first area, and an area to which the tapes are not attached is set as the second area, and in the inner surface of the outermost roll of the electrode plate having the outermost surface among the negative plate and the positive plate, an area overlapping with the second area is set as the third area, a spacer is provided in a portion of the third area.
2. The nonaqueous electrolyte secondary battery according to claim 1, wherein In the third region where the spacer is located, an area ratio of a portion with which the spacer is in contact is 50% or more.
3. The nonaqueous electrolyte secondary battery according to claim 2, wherein: In the third region where the spacer is located, an area ratio of a portion with which the spacer is in contact is 80% or more.
4. The nonaqueous electrolyte secondary battery according to any one of claims 1 to 3, wherein The thickness of the spacer is 50% or more and 150% or less of the thickness of the tape.
5. The nonaqueous electrolyte secondary battery according to any one of claims 1 to 4, wherein The spacer is the same belt as the belt.