Nonaqueous electrolyte secondary battery

By setting multiple first and second areas on the positive electrode plate of the nonaqueous electrolyte secondary battery, the uniform expansion and contraction of the positive electrode plate is ensured, and the problem of plate deformation caused by uneven expansion and contraction of the positive electrode plate in the battery is solved. , improves the stability and life of the battery.

CN118891780APending Publication Date: 2024-11-01PANASONIC ENERGY CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202380024988.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-11
Filing Date
2023-03-06
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

During the charge and discharge cycle of the nonaqueous electrolyte secondary battery, the plate deforms due to uneven expansion and contraction of the positive electrode plate. Especially when there are more than 4 current collector plates connected to the positive electrode plate, the binding force is insufficient. , easily lead to bending deformation of the plate.

Method used

In the nonaqueous electrolyte secondary battery, a plurality of first regions and second regions are provided in the long side direction of the positive electrode plate, and a positive electrode core is exposed in the first region, while only a positive electrode mixture layer is present in the second region. , ensure that the outer side of the radial direction of the winding start end of the positive electrode plate is uniformly expanded and contracted, and reduce the deformation of the electrode plate.

Benefits of technology

The deformation of the positive electrode plate is effectively suppressed. Although there are multiple positive electrode cores exposed surfaces, the electrode body can be maintained uniformly expanding and contracting during the charge and discharge cycle, and the battery life can be extended.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118891780A_ABST
    Figure CN118891780A_ABST
Patent Text Reader

Abstract

This nonaqueous electrolyte secondary battery is provided with a wound electrode body (14) in which a positive electrode plate (11), which has a positive electrode mixture layer formed on both surfaces of a belt-shaped positive electrode core, and a negative electrode plate (12), which has a negative electrode mixture layer formed on both surfaces of a belt-shaped negative electrode core, are wound with a separator therebetween. A plurality of first regions (A) and a plurality of second regions (B) are present in the longitudinal direction (beta) of the positive electrode plate (11), the exposed surface of the positive electrode core is present in at least a portion of the width direction in the first regions (A), only the portion in which the positive electrode mixture layer is formed in the positive electrode core is present in the second regions (B), and the number of the plurality of first regions (A) is four or more. A collector tab is joined to each of the plurality of first regions (A). In a cross-section of the electrode body (14), only the second region (B) is disposed at a position where a semi-straight line (L1) passing through a winding start end (11e) of the positive electrode plate (11) from the cell center (O) intersects the positive electrode plate (11).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a nonaqueous electrolyte secondary battery. Background Art

[0002] In the past, it is known that there is a non-aqueous electrolyte secondary battery having an electrode body formed by winding a positive electrode plate and a negative electrode plate with a separator and an outer tank for accommodating the electrode body and an electrolyte. In recent years, high input and output of secondary batteries used in electric vehicles and the like are required. Therefore, in non-aqueous electrolyte secondary batteries, it is considered to improve battery characteristics by joining four collector leads (collector tabs) on the exposed surfaces of the four core bodies from which the mixture of the positive electrode plate is stripped, as in the structure described in Patent Document 1.

[0003] Prior Art Literature

[0004] Patent Literature

[0005] Patent Document 1: Japanese Patent Application Publication No. 2000-243376 Summary of the invention

[0006] However, the electrode body of the non-aqueous electrolyte secondary battery expands / contracts with the charge and discharge cycle, and in this cycle, the electrode plate deformation that bends the electrode plate constituting the electrode body sometimes occurs. In particular, at the winding starting end of the positive electrode plate and the negative electrode plate on the inner side of the winding, the restraining force cannot fully work, so it is easy to produce electrode plate deformation. Furthermore, the negative electrode plate on the inner side of the winding starting end of the positive electrode plate is prone to height difference depending on the difference in the presence or absence of the positive electrode plate on the outer side of the winding. Moreover, when the part of the radially outer side of the winding starting end of the positive electrode plate expands and contracts unevenly, it is easy to produce electrode plate deformation, especially, it is easy to produce electrode plate deformation of the positive electrode plate and the negative electrode plate near the winding starting end of the positive electrode plate.

[0007] In the case where the positive plate is joined with more than 4 current collector tabs, it is necessary to set the core exposed surface at more than 4 positions in the long side direction of the positive plate, but each core exposed surface and the negative plate opposite to the surface separated by the separator are not charged and discharged. Therefore, in the case where there are both a part of the positive plate with the core exposed surface and a part without the positive core exposed surface on the radial outside of the winding start end of the positive plate, the part of the positive plate on the radial outside of the winding start end will not expand and shrink evenly, so it is easy to cause plate deformation. In addition, in the case where there is a boundary between the core exposed surface and the mixture layer in a part of the width direction of the positive plate, the expansion / contraction will also become uneven in the width direction of the positive plate, so it is more likely to cause the above-mentioned plate deformation.

[0008] An object of the present disclosure is to suppress deformation of an electrode plate in a nonaqueous electrolyte secondary battery in which four or more current collecting tabs are joined to a positive electrode plate.

[0009] The non-aqueous electrolyte secondary battery disclosed herein comprises: a wound electrode body, in which a positive electrode plate having a positive electrode mixture layer formed on both sides of a strip-shaped positive electrode core and a negative electrode plate having a negative electrode mixture layer formed on both sides of a strip-shaped negative electrode core are wound together with an isolating member; and a cylindrical outer can, which accommodates the electrode body, wherein in the long side direction of the positive electrode plate, there are a plurality of first regions and a plurality of second regions, in the first region, an exposed surface of the positive electrode core exists in at least a portion in the width direction, in the second region, only a portion where the positive electrode mixture layer is formed on the positive electrode core exists, and the number of the plurality of first regions is 4 or more, current collecting tabs are respectively joined to the plurality of first regions, and in the cross section of the electrode body, only the second region is arranged at a position where a half straight line passing through the winding starting end of the positive electrode plate from the center of the battery intersects with the positive electrode plate.

[0010] According to the non-aqueous electrolyte secondary battery involved in the present disclosure, in a structure in which the positive electrode plate is joined with more than four current collector tabs, only the second region is arranged at the position where the half straight line from the center of the battery through the winding start end of the positive electrode plate and the positive electrode plate intersect. The second region is a region where only the portion where the positive electrode mixture layer is formed on the positive electrode core body exists. As a result, the radially outer portion of the winding start end of the positive electrode plate expands / contracts uniformly, so that even if the number of the first regions of the exposed surface of the positive electrode core body is as many as four or more, the deformation of the electrode plate can be suppressed. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is a cross-sectional view along the axial direction of a nonaqueous electrolyte secondary battery according to an example of an embodiment.

[0012] Figure 2 It is a perspective view of an electrode body constituting a nonaqueous electrolyte secondary battery according to an example of an embodiment.

[0013] Figure 3 It is a schematic development view of a positive electrode plate in an example of an embodiment.

[0014] Figure 4A FIG. 1 is a schematic diagram of a cross section perpendicular to the axial direction of a nonaqueous electrolyte secondary battery in one example of an embodiment.

[0015] Figure 4B is Figure 4A 1 and 2 are diagrams showing only the plurality of first regions and the outer shape of the outer can, and illustrating the central angles θ1 to θ4 of the respective first regions.

[0016] Figure 54 and graphs showing the results of electrode plate deformation in Example 1 and Comparative Examples 1 to 4 of the nonaqueous electrolyte secondary battery.

[0017] Figure 6 The cross-sectional view perpendicular to the axial direction of the battery shows two electrode plate deformation levels used in the evaluation of the experimental results for confirming the electrode plate deformation of the electrode assembly. DETAILED DESCRIPTION

[0018] Hereinafter, the embodiments of the present invention will be described in detail with reference to the accompanying drawings. In the following description, specific shapes, materials, numerical values, directions, etc. are examples for making the present invention easy to understand, and can be appropriately changed to match the specifications of the non-aqueous electrolyte secondary battery. In addition, below, regarding the term "substantially", in addition to the completely identical situation, it is also used as a meaning including situations that can be regarded as substantially the same. Further, below, in the case of including a plurality of embodiments and variations, it was originally envisioned that their characteristic parts would be appropriately combined for use.

[0019] Figure 1 1 is a cross-sectional view of the nonaqueous electrolyte secondary battery 10 according to the embodiment, taken along the axial direction. Figure 2 It is a perspective view of the electrode body 14 constituting the nonaqueous electrolyte secondary battery 10 . Figure 3 It is a schematic development view of the positive electrode plate 11 . Figure 4A 1 is a schematic diagram of a cross section perpendicular to the axial direction of the nonaqueous electrolyte secondary battery 10 . Figure 4B is Figure 4A In the figure, only the first regions and the outer shape of the outer can 15 are shown to show the central angles θ1 to θ4 of each first region. Figures 1 to 4B As shown in the example, the nonaqueous electrolyte secondary battery 10 includes a wound electrode body 14, a nonaqueous electrolyte (not shown), an outer can 15, and a sealing body 16. The wound electrode body 14 includes a positive electrode plate 11, a negative electrode plate 12, and a separator 13, as described later. Figure 2 As shown, the positive electrode plate 11 and the negative electrode plate 12 are wound into a spiral shape with the separator 13 interposed therebetween. Hereinafter, one axial side of the electrode body 14 is sometimes referred to as "upper", and the other axial side is sometimes referred to as "lower". The nonaqueous electrolyte includes a nonaqueous solvent and an electrolyte salt dissolved in the nonaqueous solvent. The nonaqueous electrolyte is not limited to a liquid electrolyte, and may also be a solid electrolyte using a gel polymer or the like.

[0020] like Figure 2 As shown in FIG. 1 , four positive electrode tabs 20 as current collecting tabs are joined and electrically connected to the positive electrode plate 11. Each positive electrode tab 20 is used to connect the positive electrode core 11a ( Figure 3)A conductive member electrically connected to the positive terminal extends upward (to one side in the axial direction α) from the upper end of the positive electrode core 11a among the electrode bodies 14.

[0021] Two negative electrode connection tabs 21a and 21b are joined and electrically connected to the negative electrode plate 12. Each of the negative electrode connection tabs 21a and 21b is a conductive member for electrically connecting the negative electrode core constituting the negative electrode plate 12 to the negative terminal, and extends downward (to the other side in the axial direction α) from the lower end of the negative electrode core of the electrode body 14. One negative electrode connection tab 21a is joined to the winding start side end of the negative electrode plate 12, and the other negative electrode connection tab 21b is joined to the winding end side end of the negative electrode plate 12. One of the two negative electrode connection tabs 21a and 21b may be omitted.

[0022] In order to suppress the precipitation of lithium, the negative electrode plate 12 is formed to be one size larger in circumference than the positive electrode plate 11, and is formed longer than the positive electrode plate 11 in the longitudinal direction and the width direction (short side direction). In addition, two separator members 13 are formed to be at least one size larger in circumference than the positive electrode plate 11, and are arranged to sandwich the positive electrode plate 11.

[0023] Refer to Figure 3 , the positive electrode plate 11 has a strip-shaped positive electrode core 11a and positive electrode mixture layers 11b formed on both surfaces of the positive electrode core 11a. For the positive electrode core 11a, for example, a foil of a metal such as aluminum, a film having the metal disposed on the surface layer, etc. can be used. A suitable positive electrode core 11a is a foil of a metal mainly composed of aluminum or an aluminum alloy. The thickness of the positive electrode core 11a is, for example, 10 μm to 30 μm.

[0024] The positive electrode mixture layer 11b preferably includes a positive electrode active material, a conductive agent, and a binder. After applying a positive electrode mixture slurry containing a positive electrode active material, a conductive agent, a binder, and a solvent such as N-methyl-2-pyrrolidone (NMP) to both surfaces of the positive electrode core 11a, drying and pressing are performed, whereby the positive electrode plate 11 is manufactured.

[0025] As the positive electrode active material, a lithium-containing transition metal oxide containing transition metal elements such as Co, Mn, and Ni can be exemplified. The lithium-containing transition metal oxide is not particularly limited, but is preferably a composite oxide represented by the general formula Li1+ x MO2 (wherein, -0.2 < x ≤ 0.2, and M includes at least one of Ni, Co, Mn, and Al).

[0026] As the example of the above-mentioned conductive agent, carbon materials such as carbon black (CB) such as acetylene black (AB), ketjen black, graphite, etc. can be listed. As the example of the above-mentioned binding agent, fluorine resins such as polytetrafluoroethylene (PTFE), polyvinylidene fluoride (PVdF), polyacrylonitrile (PAN), polyimide (PI), acrylic resin, polyolefin resin, etc. can be listed. In addition, these resins and carboxymethyl cellulose (CMC) or its salt, polyethylene oxide (PEO), etc. can also be used in combination. They can both use one kind individually, and two or more combinations can also be used.

[0027] like Figure 3 As shown, there are four first regions A and five second regions B in the longitudinal direction β of the positive electrode plate 11. In the first region A, at least a portion of the width direction γ has an exposed surface 11c where the surface of the metal constituting the positive electrode core 11a is exposed. In the second region B, only a portion of the positive electrode core 11a is formed with the positive electrode mixture layer 11b. The width direction γ of the positive electrode plate 11 is parallel to the axial direction α in the wound state ( Figure 1 ). The first region A and the second region B are alternately arranged along the long side direction of the positive electrode plate 11. The exposed surface 11c is the portion connected to the positive electrode tab 20 and is the portion of the surface of the positive electrode core 11a that is not covered by the positive electrode mixture layer. Figure 3 In the figure, the positive electrode mixture layer 11b is shown by the oblique line. The four positive electrode tabs 20 are connected to the four exposed surfaces 11c by, for example, ultrasonic welding. The positive electrode tabs 20 are covered with an insulating tape 24, and as a result, a short circuit between the positive electrode plate 11 and the negative electrode plate 12 is prevented. Figure 3 As shown, the insulating tape 24 preferably covers the entire exposed surface 11 c of the positive electrode substrate 11 a .

[0028] exist Figure 3 In the example of , in each first region A, the exposed surface 11c is provided only at one end portion in the width direction which is the upper end portion of the positive electrode plate 11, and the portion of each first region A other than the exposed surface 11c is covered by the positive electrode mixture layer 11b. The structural material of the positive electrode tab 20 is not particularly limited. The positive electrode tab 20 is preferably made of a metal having aluminum as a main component.

[0029] In addition, Figure 3 In FIG. 1 , it is shown that in the long side direction β of the positive electrode plate 11, the lengths of the four first regions A are substantially equal. In fact, Figure 4A , Figure 4B As shown, the lengths of the long sides β of the first regions A are different from each other, and the lengths increase from the inner side of the winding to the outer side of the winding. Moreover, the total of the central angles θ1, θ2, θ3, and θ4 of the four first regions A with respect to the center of the battery, i.e., the center O of the outer can 15, is greater than 360 degrees. Figure 4AIn FIG. 1 , the first region A of the positive electrode plate 11 is indicated by the thickest thick line, the second region B is indicated by the thin line, and the negative electrode plate 12 is indicated by a line of an intermediate thickness between the regions A and B. FIG.

[0030] The winding start end 12a of the negative electrode plate 12 is located at a position closer to the inner side of the winding start end 11d of the positive electrode plate 11 and extends toward the winding start side. The winding end end 12b of the negative electrode plate 12 is located at a position closer to the outer side of the winding end end 11e of the positive electrode plate 11 and extends toward the winding end side. Figure 3 The illustration of the isolator is omitted. Figure 1 , Figure 4A Compared with the situation shown in FIG. 1 , the actual number of windings of the positive electrode plate 11 and the negative electrode plate 12 is much greater.

[0031] Further, in Figure 4A In the cross section of the electrode body 14 shown in FIG. 4 , only the second region B is arranged at the position where the half straight line (the line indicated by the dotted line L1 in FIG. 4 ) passing through the winding start end 11d of the positive electrode plate 11 from the battery center O intersects with the positive electrode plate 11, that is, only the region where only the portion where the positive electrode mixture layer 11b is formed on the positive electrode core 11a is arranged. In other words, the exposed surface 11c of the positive electrode core 11a does not exist on the above-mentioned half straight line. As described later, the deformation of the electrode plate in the structure in which four or more positive electrode tabs 20 are joined to the positive electrode plate 11 can be suppressed.

[0032] The negative electrode plate 12 has a strip-shaped negative electrode core and negative electrode mixture layers formed on both sides of the negative electrode core. The negative electrode core can be made of, for example, a foil of a metal such as copper or a film having the metal disposed on the surface. The thickness of the negative electrode core is, for example, 5 μm to 30 μm.

[0033] The negative electrode mixture layer preferably contains a negative electrode active material and a binder. For example, a negative electrode mixture slurry containing a negative electrode active material, a binder, and water is applied to both sides of a negative electrode core, followed by drying and pressing to produce the negative electrode plate 12 .

[0034] As the negative electrode active material, as long as it can reversibly absorb and release lithium ions, it is not particularly limited, for example, carbon materials such as natural graphite and artificial graphite, metals such as Si and Sn alloyed with lithium, or alloys and composite oxides containing them can be used. For the binder contained in the negative electrode active material layer, for example, the same resin as that in the case of the positive electrode plate 11 can be used. In the case of using an aqueous solvent to prepare the negative electrode mixture slurry, styrene-butadiene rubber (SBR), CMC or its salt, polyacrylic acid or its salt, polyvinyl alcohol, etc. can be used. They can be used alone or in combination of two or more.

[0035] For the spacer 13 ( Figure 1-2), a porous sheet with ion permeability and insulation can be used. Specific examples of porous sheets include microporous films, woven fabrics, non-woven fabrics, etc. The material of the separator 13 is preferably an olefin resin such as polyethylene and polypropylene. The thickness of the separator 13 is, for example, 10μm to 50μm. With the increase in capacity and output of the battery, the separator 13 tends to be thinner. The separator 13 has a melting point of, for example, about 130°C to 180°C.

[0036] Furthermore, a tape (not shown) is attached to the outermost peripheral surface of the separator so that the winding end E of the separator 13 is fixed to the outermost peripheral surface of the electrode body 14 , that is, the outermost peripheral surface of the separator 13 .

[0037] exist Figure 1 In the example shown, the metal battery case containing the electrode body 14 and the non-aqueous electrolyte is formed by the outer can 15 and the sealing body 16. The metal terminal cover, i.e., the sealing plate 17 on the upper side and the metal collector plate 18 on the lower side having the through hole 18a, sandwich the metal plate 19 between the two and overlap in the up-down direction, thereby forming the sealing body 16. The sealing plate 17 is a hat-shaped having a short cylindrical portion 17a with a bottomed cylindrical shape that is bulged upward at the center. The outer can 15 is recessed radially inwardly over the entire circumference at the upper end of the cylindrical portion 15a, thereby forming an annular groove portion 15b. In a state where the sealing body 16 is embedded inwardly from the opening of the upper end of the cylindrical portion 15a through the gasket 27 and is locked on the upper surface of the groove portion 15b, the upper end of the cylindrical portion 15a is riveted radially inward. Thus, the sealing body 16 is fixed to the inner side of the opening end of the outer can 15 by caulking via the gasket 27 on the outer peripheral side.

[0038] Insulating plates 28 and 29 are provided above and below the electrode body 14, respectively. Four positive electrode tabs 20 extend toward the sealing body 16 through the through holes of the upper insulating plate 28, pass through the through holes 18a of the current collector plate 18, and are sandwiched and joined by the outer peripheral parts of the current collector plate 18 and the metal plate 19. In the non-aqueous electrolyte secondary battery 10, the sealing plate 17 electrically connected to the current collector plate 18 and the metal plate 19 serves as a positive terminal.

[0039] One of the two negative electrode tabs 21a and 21b, which is joined to the end of the winding start side of the negative electrode plate 12, passes through the through hole of the lower insulating plate 29, is bent at a substantially right angle toward the battery center O, and extends toward the opposite side with respect to the battery center O. The other of the two negative electrode tabs 21a and 21b, which is joined to the end of the winding end side of the negative electrode plate 12, passes through the outside of the insulating plate 29, and is bent so as to overlap with the one negative electrode tab 21a. The overlapping portion of each negative electrode tab 21a and 21b is joined to the inner surface of the bottom of the outer can 15. Thus, each negative electrode tab 21a and 21b is electrically connected to the outer can 15 serving as a negative terminal.

[0040] According to the above-mentioned nonaqueous electrolyte secondary battery 10, in the structure where four positive electrode tabs 20 are joined to the positive electrode plate 11, only the second region B is arranged at the position where the half-line passing through the winding start end 11d of the positive electrode plate 11 from the battery center O intersects with the positive electrode plate 11. Therefore, in the secondary battery 10, although the number of the first regions A where the exposed surface 11c of the positive electrode core 11a exists is as many as four or more, the exposed surface 11c of the positive electrode core 11a does not exist at the position where the above-mentioned half-line and the positive electrode plate 11 intersect, in other words, only the mixture layer forming part of the positive electrode plate 11 exists at this position. Therefore, on the radial outer side of the winding start end 11d of the positive electrode plate 11 in the battery, it becomes easy for the positive electrode plate 11 and the negative electrode plate 12 to expand and contract evenly. Therefore, even though many positive electrode tabs 20 are joined to the positive electrode plate 11, it is possible to suppress deformation of the electrode plate.

[0041] In addition, according to the above-mentioned non-aqueous electrolyte secondary battery 10, although the total of the central angles of each of the multiple first regions A with respect to the battery center O is greater than 360 degrees, since only the second region B is arranged radially outside the winding starting end 11d of the positive electrode plate 11, the effect of suppressing plate deformation will also become significant.

[0042] Furthermore, according to the above-described nonaqueous electrolyte secondary battery 10, in at least a portion of the first region A, the exposed surface 11c exists only on one side in the width direction of the positive electrode plate 11, so that even though the expansion / contraction in the width direction of the positive electrode plate becomes uneven, the effect of suppressing plate deformation becomes significant.

[0043] <Example>

[0044] The inventor of the present disclosure Figure 5 Under the conditions shown, a total of 5 secondary batteries, namely Example 1 and Comparative Examples 1-4, were manufactured, and charged and discharged under the given conditions to confirm the degree of plate deformation. Figure 5 , the cross-section of each secondary battery and the results (levels) of plate deformation are shown.

[0045] Example

[0046] [Example 1]

[0047] [Production of positive electrode plate]

[0048] As the positive electrode active material, LiNi 0.88 Co 0.09 Al 0.03 O2 represents aluminum-containing lithium nickel cobalt oxide. Then, 100 parts by mass of LiNi 0.88 Co 0.09 Al 0.03 O2, 1 part by mass of acetylene black and 0.9 parts by mass of polyvinylidene fluoride (PVDF) (binder) are mixed, and N-methyl-2-pyrrolidone (NMP) is further added in an appropriate amount to prepare a positive electrode mixture slurry. Next, the positive electrode mixture slurry in a paste state is applied to both sides of a long positive electrode core body composed of an aluminum foil with a thickness of 15 μm in such a way as to form four exposed surfaces of the core body for welding the positive electrode tabs 20, and is dried with a dryer. After that, the product after the positive electrode mixture slurry is applied to the positive electrode core body 11a and dried is cut into a given electrode size, and a roller is used for pressing to produce a positive electrode plate 11 having a positive electrode mixture layer 11b formed on both sides of the positive electrode core body 11a. At this time, the thickness of the positive electrode plate 11 is 0.144 mm, the width is 62.6 mm, and the length is set to 861 mm. Aluminum positive electrode tabs 20 are fixed by welding to all of the exposed surfaces 11 c of the core at four locations in the longitudinal direction of the positive electrode plate 11 .

[0049] [Manufacturing of negative electrode plate]

[0050] As the negative electrode active material, a negative electrode active material obtained by mixing 95 parts by mass of graphite powder and 5 parts by mass of silicon oxide was used. Then, 100 parts by mass of the negative electrode active material, 1 part by mass of styrene-butadiene rubber (SBR) as a binder, and 1 part by mass of carboxymethyl cellulose (CMC) as a thickener were mixed. Then, the mixed product was dispersed in water to prepare a negative electrode mixture slurry. The negative electrode mixture slurry was applied to both sides of a negative electrode core composed of a copper foil having a thickness of 8 μm, dried by a dryer, and compressed with a roller of a roller press to a given thickness. Then, the long strip of negative electrode core formed with a negative electrode mixture layer was cut into a given electrode size, thereby producing a negative electrode plate 12 having a negative electrode mixture layer formed on both sides of the negative electrode core. At this time, the thickness of the negative electrode plate 12 was 0.160 mm, the width was 64.2 mm, and the length was 959 mm. An exposed portion where no mixture layer exists and the collector surface is exposed is provided at one end of the negative electrode plate 12 in the longitudinal direction and located at the winding end side of the electrode body 14. A negative electrode tab 21b made of nickel is fixedly mounted on the exposed portion by welding.

[0051] [Production of electrode body]

[0052] The produced positive electrode plate 11 and negative electrode plate 12 are wound in a spiral shape with a separator 13 composed of a polyethylene microporous film interposed therebetween to produce a wound electrode body 14 , and the winding end is fixed by a tape.

[0053] [Preparation of non-aqueous electrolyte]

[0054] To 100 parts by mass of a mixed solvent of ethylene carbonate (EC) and dimethyl carbonate (DMC) in a volume ratio of EC:DMC=1:3, 5 parts by mass of vinylene carbonate (VC) was added and dissolved so that LiPF6 became 1.5 mol / L, thereby preparing a non-aqueous electrolyte.

[0055] [Manufacturing of Secondary Batteries]

[0056] The electrode body 14 is contained in a bottomed cylindrical outer can 15, insulating plates 28 and 29 are respectively arranged above and below the electrode body 14, and a non-aqueous electrolyte is injected into the outer can 15 by decompression. After that, the sealing body 16 is riveted and fixed to the open end of the outer can 15 via a gasket 27, thereby manufacturing a cylindrical non-aqueous electrolyte secondary battery 10. At this time, the battery capacity is 4600 mAh.

[0057] In addition, in Example 1, Figure 5As shown, in the cross section of the battery, only the second region B is arranged at the position where the half straight line L1 from the battery center O through the winding start end 11d of the positive electrode plate 11 intersects the positive electrode plate 11. Figure 5 In FIG. 1 , the winding start end 11d is shown by a black circle.

[0058] [Comparative Example 1]

[0059] like Figure 5 As shown, in the cross section of the battery of Comparative Example 1, all of the four first regions A are arranged at the intersection of the half straight line L1 from the battery center O through the winding start end 11d of the positive electrode plate 11 and the positive electrode plate 11. Figure 5 In the figure, the winding number is shown to be smaller than the actual number, so it is not shown in the figure, but in fact, on the half line L1, there are not only the first area A but also a plurality of second areas B. In Comparative Example 1, the structure other than this is the same as that of Example 1.

[0060] [Comparative Example 2]

[0061] like Figure 5 As shown, in the cross section of the battery of Comparative Example 2, three first regions A are arranged at the intersection of the half straight line L1 from the battery center O through the winding start end 11d of the positive electrode plate 11 and the positive electrode plate 11. Figure 5 In the embodiment, in fact, a plurality of second regions B exist on the half-line L1, which is the same as in Comparative Example 1. In Comparative Example 2, the other configurations are the same as in Example 1.

[0062] [Comparative Example 3]

[0063] like Figure 5 As shown, in the cross section of the battery of Comparative Example 3, two first regions A are arranged at the intersection of the half straight line L1 from the battery center O through the winding start end 11d of the positive electrode plate 11 and the positive electrode plate 11. Figure 5 In the embodiment, in fact, a plurality of second regions B exist on the half straight line L1, which is the same as in Comparative Example 1. In Comparative Example 3, the other structures are the same as those of Example 1.

[0064] [Comparative Example 4]

[0065] like Figure 5 As shown, in the cross section of the battery of Comparative Example 4, a first region A is arranged at the intersection of the half straight line L1 from the battery center O through the winding start end 11d of the positive electrode plate 11 and the positive electrode plate 11. Figure 5 In the embodiment, in fact, a plurality of second regions B exist on the half-line L1, which is the same as in Comparative Example 1. In Comparative Example 4, the other structures are the same as those of Example 1.

[0066] [Test method]

[0067] Using the non-aqueous electrolyte secondary batteries of the above-mentioned Example 1 and Comparative Examples 1-4, constant current charging (CC) was performed at a current of 1380mA (0.3It) in an environment of 25°C until the battery voltage reached 4.2V, and then constant voltage charging (CV) was performed at a battery voltage of 4.2V until the current value reached 92mA. Furthermore, after a rest of 20 minutes, constant current discharge was performed at a discharge current of 2300mA (0.5It), and then a rest of 20 minutes was performed, which was set as a charge and discharge cycle. In the battery after repeating such a charge and discharge cycle for 1000 cycles, after the battery voltage reached 4.2V by constant current charging at 1380mA (0.3It), constant voltage charging with a termination current of 92mA was performed at a battery voltage of 4.2V. Afterwards, an X-ray CT device was used to perform cross-sectional observation of the position where the exposed surface 11c of the positive electrode core 11a of the electrode body 14 was located on the above-mentioned battery. Figure 5 The column of plate deformation results shows the level of plate deformation in two stages.

[0068] Figure 6 The figure shows two levels of plate deformation used to evaluate the experimental results for confirming the plate deformation in the electrode body 14, and is a cross-sectional view perpendicular to the axial direction of the electrode body 14. Level 1 of the plate deformation has a small deformation degree among the two levels, and the plate deformation with bending occurs only in the innermost circumference of the electrode body 14. Level 2 has a large deformation degree among the two levels, and the plate deformation with bending occurs in at least three circumferences including the innermost circumference of the electrode body 14. Figure 6 In FIG. 1 , the outermost circle represents the outer can 15 , and the solid line curve inside the circle represents the negative electrode plate 12 . In addition, the thin solid line curve represents the positive electrode plate 11 .

[0069] [Test results]

[0070] like Figure 5 As shown, in Example 1, no plate deformation was found. In addition, the plate deformation of Comparative Examples 1 and 2 was level 2, and the plate deformation of Comparative Examples 3 and 4 was level 1. Therefore, as in Example 1, when only the second region B is arranged at the position intersecting the half straight line L1 and the positive electrode plate 11, that is, only the portion where the positive electrode mixture layer 11b is formed on the positive electrode core 11a, no plate deformation is found, and the effect of the embodiment can be confirmed.

[0071] In addition, as is clear from the test results of Comparative Examples 1 to 4, it can be confirmed that even when there is one first region A on the half-line L1, the electrode plate is deformed. In the case of Comparative Examples 1 and 2 where the number of first regions A on the half-line L1 is three or more, the degree of deformation of the electrode plate is greater.

[0072] In the above-described embodiment, the case where the number of first regions A in the longitudinal direction of the positive electrode plate is four or more is described. However, the structure of the present disclosure can also be applied to a structure where the number of first regions A is five or more.

[0073] Explanation of symbols

[0074] 10 non-aqueous electrolyte secondary battery; 11 positive electrode plate; 11a positive electrode core; 11b positive electrode mixture layer; 11c exposed surface; 11d winding start end; 11e winding end end; 12 negative electrode plate; 12a winding start end; 12b winding end end; 13 separator; 14 electrode body; 15 outer can; 16 sealing body; 17 sealing plate; 17a short cylinder; 18 collector plate; 19 metal plate; 20 positive electrode tab; 21a, 21b negative electrode tab; 24 insulating tape; 27 gasket; 28, 29 insulating plates; A first region; B second region.

Claims

1. A non-aqueous electrolyte secondary battery comprising: A wound electrode body is formed by winding a positive electrode plate having a positive electrode mixture layer formed on both sides of a strip-shaped positive electrode core and a negative electrode plate having a negative electrode mixture layer formed on both sides of a strip-shaped negative electrode core through a separator; and A cylindrical outer can accommodates the electrode body. In the long side direction of the positive electrode plate, there are a plurality of first regions and a plurality of second regions, in the first region, the exposed surface of the positive electrode core body exists in at least a portion in the width direction, in the second region, only a portion where the positive electrode mixture layer is formed on the positive electrode core body exists, and the number of the plurality of first regions is 4 or more, A current collecting tab is connected to each of the plurality of first regions. In the cross section of the electrode body, only the second region is arranged at a position where a half straight line passing through the winding start end of the positive electrode plate from the center of the battery intersects the positive electrode plate.

2. The nonaqueous electrolyte secondary battery according to claim 1, in, The total of the central angles of each of the plurality of first regions with respect to the battery center is greater than or equal to 360 degrees.

3. The nonaqueous electrolyte secondary battery according to claim 1 or 2, in, In at least a portion of the first region, the exposed surface exists only on one side in the width direction of the positive electrode plate.

Citation Information

Patent Citations

  • Lithium secondary battery

    JP2000243376A