Manufacturing method of light-emitting device
By processing the organic compound layer by photolithography, the moisture in the intermediate layer is removed, and the driving voltage rise and current efficiency decrease caused by the alkali metal or alkali metal compound layer in the photolithography process is solved, thus achieving high efficiency Light emitting device manufacturing, suitable for high-definition display devices.
Patent Information
- Application Number
- CN202380027960.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-31
- Filing Date
- 2023-03-20
- Publication Date
- 2024-11-01
AI Technical Summary
Prior Art When manufacturing a light emitting device containing an organic semiconductor layer containing an alkali metal or alkali metal compound, it is susceptible to oxygen or water in the atmosphere, resulting in an increase in driving voltage and a decrease in current efficiency, especially in the middle exposed in the photolithography process. Layer causes feature degradation problems.
After the organic compound layer is processed by a photolithography method, the organic compound layer is subjected to heat treatment to remove moisture in the intermediate layer and prevent water adsorption, thereby suppressing the increase of the driving voltage and the decrease in current efficiency.
Through heating treatment, a series-type light emitting device with good characteristics can be manufactured, avoiding a significant increase in driving voltage and a significant decrease in current efficiency, and is suitable for high-definition display devices such as VR and AR.
Smart Images

Figure CN118891970A_ABST
Abstract
Description
Technical Field
[0001] One embodiment of the present invention relates to a method for manufacturing a light-emitting device.
[0002] Note that one embodiment of the present invention is not limited to the above-mentioned technical field. As an example of the technical field of one embodiment of the present invention, a light-emitting device, a semiconductor device, a display device, a display module, a light-emitting device, a power storage device, a storage device, an electronic device, a lighting device, an input device (e.g., a touch sensor), an input-output device (e.g., a touch panel), and a driving method or a manufacturing method of the above-mentioned device can be cited. Background Art
[0003] In recent years, display devices are expected to be used in various applications. For example, large display devices can be used in home television devices (also called televisions or television receivers), digital signage, and public information displays (PID). In addition, as portable information terminals, research and development of smartphones and tablet terminals equipped with touch panels is underway.
[0004] In addition, there is a demand for higher-definition display devices. As devices requiring high-definition display devices, for example, devices for virtual reality (VR), augmented reality (AR), alternative reality (SR), and mixed reality (MR) are being actively developed.
[0005] As a display device, for example, a light-emitting device including a light-emitting device (also referred to as a light-emitting element) has been developed. A light-emitting device (also referred to as an "EL device" or "EL element") utilizing the electroluminescence (hereinafter referred to as EL) phenomenon has the characteristics of being easy to achieve thinness and lightness; being able to respond to input signals at high speed; and being able to be driven using a DC constant voltage power supply, etc., and has been applied to display devices.
[0006] Patent document 1 discloses a display device for VR using an organic EL device (also referred to as an organic EL element). Patent document 2 discloses a light-emitting device having a low driving voltage and good reliability, using a mixed film of an organic compound containing a transition metal and a non-shared electron pair as an electron injection layer. [Prior technical literature] [Patent Document]
[0007] [Patent Document 1] International Patent Application Publication No. 2018 / 087625 [Patent Document 2] Japanese Patent Application Publication No. 2018-201012 Summary of the invention Technical problem to be solved by the invention
[0008] One of the purposes of one embodiment of the present invention is to provide a method for manufacturing a light-emitting device that can be used for a display device with high display quality. Another purpose of one embodiment of the present invention is to provide a method for manufacturing a light-emitting device that can be used for a high-definition display device. Another purpose of one embodiment of the present invention is to provide a method for manufacturing a light-emitting device that can be used for a high-resolution display device. Another purpose of one embodiment of the present invention is to provide a method for manufacturing a light-emitting device that can be used for a display device with high reliability. Another purpose of one embodiment of the present invention is to provide a method for manufacturing a light-emitting device that can be used for a novel display device with excellent convenience, practicality or reliability. Another purpose of one embodiment of the present invention is to provide a method for manufacturing a novel display module with excellent convenience, practicality or reliability. Another purpose of one embodiment of the present invention is to provide a method for manufacturing a novel electronic device with excellent convenience, practicality or reliability. Another purpose of one embodiment of the present invention is to provide a method for manufacturing a novel light-emitting device, a display device, a novel display module, a novel electronic device or a novel semiconductor device.
[0009] Note that the description of these objectives does not prevent the existence of other objectives. One embodiment of the present invention does not need to achieve all of the above objectives. Objectives other than the above objectives can be extracted from the description of the specification, drawings, and claims. Solutions to technical problems
[0010] One embodiment of the present invention is a method for manufacturing a light-emitting device, comprising the following steps: forming a first electrode; forming an organic compound layer on the first electrode including an intermediate layer containing an alkali metal or an alkali metal compound between a first light-emitting layer and a second light-emitting layer; processing the organic compound layer by photolithography; performing heat treatment; and forming a second electrode in a manner covering the first electrode and the organic compound layer.
[0011] In addition, one embodiment of the present invention is a method for manufacturing a light-emitting device, comprising the following steps: forming a first electrode; forming an organic compound layer on the first electrode including an intermediate layer containing an alkali metal or an alkali metal compound between a first light-emitting layer and a second light-emitting layer; forming a sacrificial layer on the organic compound layer; forming a mask from a resist on the sacrificial layer; processing the organic compound layer by photolithography; removing at least a portion of the sacrificial layer; performing heat treatment; and forming a second electrode in a manner covering the first electrode and the organic compound layer.
[0012] In addition, one embodiment of the present invention is a method for manufacturing a light-emitting device, comprising the following steps: forming a first electrode; forming an organic compound layer including an intermediate layer containing an alkali metal or an alkali metal compound between a first light-emitting layer and a second light-emitting layer on the first electrode; forming a sacrificial layer on the organic compound layer; forming a mask from a resist on the sacrificial layer; processing the organic compound layer by photolithography; forming an insulating layer covering the side of the organic compound layer; removing at least a portion of the sacrificial layer and performing heat treatment; forming a second electrode in a manner covering the first electrode and the organic compound layer.
[0013] In addition, one embodiment of the present invention is a method for manufacturing a light emitting device, wherein the heat treatment is performed at a temperature of 100° C. or higher in each of the above structures.
[0014] In addition, one embodiment of the present invention is a method for manufacturing a light emitting device, wherein the heat treatment is performed at a temperature of 100° C. or higher and 120° C. or lower in each of the above structures.
[0015] In addition, one embodiment of the present invention is a method for manufacturing a light emitting device, wherein in each of the above structures, the heat treatment is performed at a temperature of 100° C. or higher and lower than a glass transition temperature of an organic compound included in a top surface of the organic compound layer. Effects of the Invention
[0016] One embodiment of the present invention may provide a method for manufacturing a light-emitting device that can be used in a display device with high display quality. In addition, one embodiment of the present invention may provide a method for manufacturing a light-emitting device that can be used in a high-definition display device. In addition, one embodiment of the present invention may provide a method for manufacturing a light-emitting device that can be used in a high-resolution display device. In addition, one embodiment of the present invention may provide a method for manufacturing a light-emitting device that can be used in a display device with high reliability. In addition, one embodiment of the present invention may provide a method for manufacturing a light-emitting device that can be used in a novel display device with excellent convenience, practicality or reliability. In addition, one embodiment of the present invention may provide a method for manufacturing a novel display module with excellent convenience, practicality or reliability. In addition, a method for manufacturing a novel electronic device with excellent convenience, practicality or reliability may be provided. In addition, a method for manufacturing a light-emitting device that can be used in a novel display device, a novel display module, a novel electronic device or a novel semiconductor device may be provided.
[0017] Note that the description of these effects does not prevent the existence of other effects. One embodiment of the present invention does not necessarily have all of the above effects. Effects other than the above effects can be extracted from the description of the specification, drawings, and claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1A and Figure 1B is a diagram showing a light emitting device. FIG. 2A to FIG. 2D is a cross-sectional view showing an example of a method for manufacturing a light emitting device. FIG. 3A to FIG. 3D is a cross-sectional view showing an example of a method for manufacturing a light emitting device. FIG. 4A to FIG. 4D is a cross-sectional view showing an example of a method for manufacturing a light emitting device. FIG. 5A to FIG. 5C is a cross-sectional view showing an example of a method for manufacturing a light emitting device. Fig. 6A and Figure 6B 1 and 2 are a top view and a cross-sectional view of the light emitting device. FIG. 7A to FIG. 7D is a diagram showing a light emitting device. FIG. 8A to FIG. 8E This is a cross-sectional view showing an example of a method for manufacturing a display device. 9A to 9D This is a cross-sectional view showing an example of a method for manufacturing a display device. FIG. 10A to FIG. 10D This is a cross-sectional view showing an example of a method for manufacturing a display device. FIG. 11A to FIG. 11C This is a cross-sectional view showing an example of a method for manufacturing a display device. FIG. 12A to FIG. 12C This is a cross-sectional view showing an example of a method for manufacturing a display device. FIG. 13A to FIG. 13C This is a cross-sectional view showing an example of a method for manufacturing a display device. Fig.14A and Fig. 14B is a perspective view showing a structural example of a display module. Fig.15A and Fig. 15B is a cross-sectional view showing a structural example of a display device. FIG. 16A to FIG. 16D is a diagram showing an example of an electronic device. FIG. 17A to FIG. 17F is a diagram showing an example of an electronic device. Fig.18 1 is a graph showing the luminance-current density characteristics of the light emitting device 1 and the comparative light emitting device 2. Fig.19 is a graph showing the luminance-voltage characteristics of the light emitting device 1 and the comparative light emitting device 2 . Fig. 20 1 is a graph showing current efficiency-luminance characteristics of the light emitting device 1 and the comparative light emitting device 2 . Fig.213 is a graph showing current density-voltage characteristics of the light emitting device 1 and the comparative light emitting device 2. Fig. 22 1 is a graph showing current efficiency-current density characteristics of the light emitting device 1 and the comparative light emitting device 2 . Fig.23 1 is a diagram showing emission spectra of the light-emitting device 1 and the comparative light-emitting device 2. Fig.24 is a graph showing the luminance-current density characteristics of the reference light-emitting device 3 and the comparative light-emitting device 4 . Fig.25 3 is a graph showing the luminance-voltage characteristics of the reference light-emitting device 3 and the comparative light-emitting device 4. Fig.26 3 is a graph showing current efficiency-luminance characteristics of the reference light-emitting device 3 and the comparative light-emitting device 4. Fig. 27 is a graph showing current density-voltage characteristics of the reference light-emitting device 3 and the comparative light-emitting device 4. Fig.28 1 is a diagram showing emission spectra of the reference light-emitting device 3 and the comparative light-emitting device 4 . Fig.29 3 is a graph showing the TDS analysis results of Sample 1. Fig.30 3 is a graph showing the TDS analysis results of Comparative Sample 2. Fig.31 3 is a graph showing the TDS analysis results of Comparative Sample 3. Modes for Carrying Out the Invention
[0019] The embodiments are described in detail with reference to the accompanying drawings. Note that the present invention is not limited to the following description, and a person skilled in the art can easily understand that the method and details can be transformed into various forms without departing from the purpose and scope of the present invention. Therefore, the present invention should not be interpreted as being limited to the contents described in the embodiments shown below.
[0020] Note that in the structure of the invention described below, the same reference numerals are used in common between different drawings to represent the same parts or parts with the same function, and their repeated descriptions are omitted. In addition, when representing parts with the same function, the same hatching is sometimes used without adding a reference numeral in particular.
[0021] In addition, for ease of understanding, the positions, sizes, and ranges of various components shown in the drawings may not represent their actual positions, sizes, and ranges. Therefore, the disclosed invention is not necessarily limited to the positions, sizes, and ranges disclosed in the drawings.
[0022] In addition, depending on the situation or state, the "film" and the "layer" may be interchanged. For example, the "conductive layer" may be replaced with the "conductive film". Also, the "insulating film" may be replaced with the "insulating layer".
[0023] Note that in this specification, etc., a device manufactured using a metal mask or FMM (Fine Metal Mask) is sometimes referred to as a device having an MM (Metal Mask) structure. In addition, in this specification, etc., a device manufactured without using a metal mask or FMM is sometimes referred to as a device having an MML (Metal Mask Less) structure.
[0024] In this specification, holes or electrons are sometimes referred to as "carriers". Specifically, a hole injection layer or an electron injection layer is sometimes referred to as a "carrier injection layer", a hole transport layer or an electron transport layer is sometimes referred to as a "carrier transport layer", and a hole blocking layer or an electron blocking layer is sometimes referred to as a "carrier blocking layer". Note that the above-mentioned carrier injection layer, carrier transport layer, and carrier blocking layer are sometimes not clearly distinguishable based on cross-sectional shapes or characteristics. In addition, sometimes one layer has the functions of two or three of a carrier injection layer, a carrier transport layer, and a carrier blocking layer.
[0025] In this specification, etc., a light-emitting device (also referred to as a light-emitting element) includes an EL layer between a pair of electrodes. The EL layer includes at least a light-emitting layer. In this specification, etc., a light-receiving device (also referred to as a light-receiving element) includes at least an active layer used as a photoelectric conversion layer between a pair of electrodes. In this specification, etc., one of a pair of electrodes is sometimes referred to as a pixel electrode and the other as a common electrode.
[0026] In this specification, etc., a tapered shape refers to a shape in which at least a portion of the side surface of a constituent element is disposed obliquely relative to the substrate surface. For example, it is preferred to have an area where the inclined side surface and the substrate surface (also referred to as a taper angle) are less than 90°. Note that the side surface and the substrate surface of a constituent element do not necessarily have to be completely flat, and may be a substantially planar shape with a slight curvature or a substantially planar shape with fine concave and convex shapes.
[0027] (Implementation Method 1) As one of the methods for manufacturing an organic semiconductor film into a prescribed shape, a vacuum evaporation method (mask evaporation) using a metal mask is widely used. However, recently, with the progress of high density and high definition, due to various reasons represented by the problem of position alignment accuracy and the configuration interval with the substrate, the further high definition of mask evaporation is approaching the limit. On the other hand, by processing the shape of the organic semiconductor film using photolithography, a denser pattern can be formed. In addition, since the above method is easy to achieve large area, research on the processing of organic semiconductor films using photolithography has been conducted.
[0028] The organic EL element includes an organic compound layer (equivalent to the above-mentioned organic semiconductor film) containing a light-emitting substance between electrodes (between the first electrode and the second electrode) and has a structure that obtains light emission by energy generated by recombination of carriers (holes and electrons) injected from the electrodes into the organic compound layer.
[0029] Here, since it is difficult for current to flow through the organic compound layer and the energy barrier is large, a high voltage is basically required when injecting carriers, especially electrons. Therefore, currently, an alkali metal such as lithium (Li) or a compound of the alkali metal is used as an electron injection layer in contact with the cathode to achieve low voltage.
[0030] However, when using the above-mentioned photolithography method to manufacture a light-emitting device including the above-mentioned organic semiconductor layer containing an alkali metal or an alkali metal compound, there are problems such as a significant increase in driving voltage or a significant decrease in current efficiency due to the influence of oxygen or water in the atmosphere or chemical solutions or water in the process.
[0031] As one of the means to solve the above-mentioned problem, there is a method of performing a photolithography process in the middle of forming an organic compound layer of a light-emitting device (before forming a layer containing an alkali metal or an alkali metal compound). That is, when this method is adopted, the organic compound layer is processed by photolithography at a stage before forming an electron injection layer, and then the process of forming the electron injection layer and subsequent processes are performed, thereby avoiding degradation of characteristics.
[0032] However, the above-mentioned avoidance method cannot be applied to the tandem light-emitting device, and a significant degradation of characteristics due to the photolithography process cannot be avoided.
[0033] This is because: the tandem light-emitting device includes an organic semiconductor layer having a structure in which a plurality of light-emitting layers are stacked in series via an intermediate layer, and the intermediate layer includes a layer containing an alkali metal or an alkali metal compound to inject electrons into the light-emitting layer on the anode side. The intermediate layer exists between the light-emitting layers, so when the light-emitting layer is processed by photolithography, the intermediate layer must also be exposed to the photolithography process.
[0034] Therefore, exposure of the layer containing an alkali metal or an alkali metal compound in the intermediate layer to the photolithography process causes a significant increase in the driving voltage of the light-emitting device and a significant decrease in the current efficiency, similar to the case where the electron injection layer is exposed to the photolithography process.
[0035] The present inventors have discovered that a layer containing an alkali metal or an alkali metal compound has the property of easily adsorbing water in the atmosphere. This is the reason why the driving voltage of the light-emitting device increases significantly and the current efficiency decreases significantly when the layer is exposed to a photolithography process. Furthermore, by performing a process for sufficiently removing water from the layer, a tandem light-emitting device with good characteristics can be manufactured even if the layer is exposed to a photolithography process.
[0036] Therefore, in the method for manufacturing a light-emitting device according to one embodiment of the present invention, the heat treatment is performed after the step of processing the organic compound layer containing an alkali metal or an alkali metal compound by photolithography.
[0037] By manufacturing a light-emitting device using this method, water can be fully removed from the organic compound layer containing an alkali metal or an alkali metal compound. Therefore, a substantial increase in the driving voltage of the light-emitting device can be suppressed, and a decrease in current efficiency can be prevented. As a result, a light-emitting device with good characteristics can be obtained. In addition, a display device capable of high-definition display sufficient for VR, AR, etc. and having good characteristics can be provided.
[0038] Figure 1A A light-emitting device 130 is shown as an example of a light-emitting device that can be manufactured using a method for manufacturing a light-emitting device according to one embodiment of the present invention. The light-emitting device 130 is a tandem light-emitting device including an organic compound layer 103 having a plurality of light-emitting units between a first electrode 101 including an anode and a second electrode 102 including a cathode. In the light-emitting device 130, the organic compound layer 103 includes a first light-emitting unit 501 including a first light-emitting layer 113_1, a second light-emitting unit 502 including a second light-emitting layer 113_2, and an intermediate layer 116.
[0039] Note that in this embodiment, a light-emitting device including one intermediate layer 116 and two light-emitting units as an organic compound layer 103 is used as an example to describe a method for manufacturing a light-emitting device according to one embodiment of the present invention. However, a light-emitting device including n (n is an integer greater than or equal to 1) intermediate layers (also referred to as charge generation layers) and n+1 light-emitting units as an organic compound layer 103 can also be manufactured by the method for manufacturing a light-emitting device according to one embodiment of the present invention. For example, Figure 1B The light-emitting device 130 shown is an example of a tandem light-emitting device, wherein n is 2, and as the organic compound layer 103, includes a first light-emitting unit 501, a first intermediate layer 116_1, a second light-emitting unit 502, a second intermediate layer 116_2, and a third light-emitting unit 503. The color gamut of light presented by the light-emitting layer in each light-emitting unit can be the same or different. In addition, the light-emitting layer can have both a single layer and a stacked structure. For example, by adopting a structure in which the first light-emitting unit and the third light-emitting unit present light in the blue region and the light-emitting layer having a stacked structure in the second light-emitting unit presents light in the red region and light in the green region, white light emission can be obtained.
[0040] In addition, the light-emitting device 130 is a light-emitting device manufactured by a method for manufacturing a light-emitting device of one embodiment of the present invention using photolithography, and at least the second light-emitting layer 113_2 in the organic compound layer 103 and each layer closer to the first electrode 101 than the second light-emitting layer 113_2 are processed simultaneously, so that their ends are roughly aligned in the vertical direction.
[0041] In addition, in the light-emitting device 130, the intermediate layer 116 contains at least an alkali metal or an alkali metal compound. More specifically, the intermediate layer 116 is a layer including an N-type layer 119 and a P-type layer 117, and the N-type layer 119 preferably contains an alkali metal or an alkali metal compound. Specific examples of alkali metals include lithium, sodium, potassium, rubidium, cesium, francium, etc. Specific examples of alkali metal compounds include compounds of the above-mentioned alkali metals, for example, lithium compounds such as lithium oxide. In addition, in addition to alkali metals or alkali metal compounds, the N-type layer 119 may also include an organic compound having electron transport properties.
[0042] The P-type layer 117 is closer to the second electrode 102 than the N-type layer 119. In addition, an electron relay layer 118 may be provided between the N-type layer 119 and the P-type layer 117 to facilitate electron transfer between the two layers.
[0043] In addition, the first light-emitting unit 501 and the second light-emitting unit 502 may also include other functional layers in addition to the light-emitting layer. Figure 1A In the embodiment, the first light-emitting unit 501 is provided with a hole injection layer 111, a first hole transport layer 112_1 and a first electron transport layer 114_1 in addition to the first light-emitting layer 113_1, and the second light-emitting unit 502 is provided with a second hole transport layer 112_2, a second electron transport layer 114_2 and an electron injection layer 115 in addition to the second light-emitting layer 113_2, but the structure of the organic compound layer 103 of the present invention is not limited thereto, and any of the above layers may not be provided, and other layers may be provided. As other layers, typically there are carrier blocking layers, exciton blocking layers, etc.
[0044] In addition, the intermediate layer 116 includes an N-type layer 119, so the N-type layer 119 is used as an electron injection layer in the light-emitting unit on the anode side. Figure 1A The first light-emitting unit 501 in the cathode side may include or not include an electron injection layer. In addition, similarly, the intermediate layer 116 includes a P-type layer 117, so the P-type layer 117 is used as a hole injection layer in the light-emitting unit on the cathode side. Therefore, the light-emitting unit on the cathode side ( Figure 1A The second light emitting unit 502) in the embodiment may include or may not include a hole injection layer.
[0045] Next, a method for manufacturing a light emitting device according to one embodiment of the present invention will be described with reference to FIGS. 2 to 5 .
[0046] First, if Figure 2A As shown, a first electrode 101 is formed on a substrate 105 .
[0047] The first electrode 101 may be formed, for example, by photolithography. Specifically, after a resist mask is formed on the conductive film formed on the substrate 105, a portion of the conductive film is removed by etching. For example, a portion of the conductive film may be removed by wet etching. In addition, a portion of the conductive film may also be removed by dry etching.
[0048] Then, if Figure 2B As shown, an organic compound film 103f which will later become the organic compound layer 103 is formed on the substrate 105 and the first electrode 101. Note that in FIGS. 2 to 5, for the sake of simplicity, only the organic compound film 501f, the intermediate film 116f, and the organic compound film 502f are shown among the films included in the organic compound film 103f. Note that the organic compound film 501f is a film which will later become the first light-emitting unit 501, the intermediate film 116f is a film which will later become the intermediate layer 116, and the organic compound film 502f is a film which will later become the second light-emitting unit 502.
[0049] The intermediate film 116f included in the organic compound film 103f contains at least an alkali metal or an alkali metal compound. More specifically, the intermediate film 116f is a film including an N-type film and a P-type film, and the N-type film preferably contains an alkali metal or an alkali metal compound. Specific examples of alkali metals include lithium, sodium, potassium, rubidium, cesium, francium, etc. Specific examples of alkali metal compounds include compounds of the above-mentioned alkali metals, for example, lithium compounds such as lithium oxide. In addition, in addition to alkali metals or alkali metal compounds, the N-type film may also contain an organic compound having electron transport properties.
[0050] The organic compound film 103f can be formed by, for example, an evaporation method, specifically, a vacuum evaporation method. Alternatively, the organic compound film 103f can be formed by a transfer method, a printing method, an inkjet method, a coating method, or the like.
[0051] Then, if Figure 2C As shown, a sacrificial film 158f, which will later become a sacrificial layer 158, and a mask film 159f, which will later become a mask layer 159, are sequentially formed on the organic compound film 103f. For a specific example of a method for forming the sacrificial film 158f and the mask film 159f, reference can be made to a method for forming the sacrificial film 158Rf and the mask film 159Rf described in detail in a later embodiment.
[0052] Then, if Figure 2D As shown, a resist mask 190 is formed on the mask film 159f at a position overlapping the first electrode 101. The resist mask 190 can be formed by applying a photosensitive resin (photoresist), exposing and developing. The resist mask 190 can also be made of a positive resist material or a negative resist material.
[0053] Next, a portion of the mask film 159f is removed using the resist mask 190 to form the mask layer 159. Then, the resist mask 190 is removed. Next, a portion of the sacrificial film 158f is removed using the mask layer 159 as a mask (also referred to as a hard mask) to form the sacrificial layer 158 (see FIG. 1 ). Figure 3A ).
[0054] Note that the specific processing method of the sacrificial film 158f and the mask film 159f can refer to the processing method of the sacrificial film 158Rf and the mask film 159Rf described in detail in the following embodiments. Regarding the specific removal method of the resist mask 190R, refer to the removal method of the resist mask 190R described in detail in the following embodiments.
[0055] Then, if Figure 3B As shown, the organic compound film 103f (the organic compound film 501f, the intermediate film 116f, and the organic compound film 502f) is processed to form the organic compound layer 103 (the first light-emitting unit 501, the intermediate layer 116, and the second light-emitting unit 502). For example, the mask layer 159 and the sacrificial layer 158 are used as a hard mask to remove a portion of the organic compound film 103f, thereby forming the organic compound layer 103. For a specific method of processing the organic compound film 103f, reference can be made to the method of processing the organic compound film 103Rf described in detail in the later embodiment.
[0056] As described above, in one embodiment of the present invention, the mask layer 159 is formed by forming the resist mask 190 on the mask film 159f and removing a portion of the mask film 159f using the resist mask 190. Then, the organic compound layer 103 is formed by removing a portion of the organic compound film 103f using the mask layer 159 as a mask. Therefore, it can be said that the organic compound layer 103 is formed by processing the organic compound film 103f using the photolithography method. In addition, the organic compound film 103f includes the intermediate film 116f, and the intermediate film 116f contains at least an alkali metal or an alkali metal compound. Therefore, it can be said that the organic compound layer 103 containing an alkali metal or an alkali metal compound is formed by processing the organic compound film 103f containing an alkali metal or an alkali metal compound using the photolithography method. In addition, a portion of the organic compound film 103f can also be removed using the resist mask 190. Then, the resist mask 190 can also be removed.
[0057] Then, if Figure 3C As shown, it is preferable to remove the mask layer 159. In the process of removing the mask layer 159, the same method as the process of processing the mask film 159f can be used. The method of removing the mask layer 159 will be described in detail in the following embodiment.
[0058] After removing the mask layer, heat treatment may be performed. For example, heat treatment may be performed in an inert gas atmosphere or a reduced pressure atmosphere. Heat treatment may be performed at a substrate temperature of 50°C to 200°C, preferably 60°C to 150°C, and more preferably 70°C to 120°C. By adopting a reduced pressure atmosphere, drying can be performed at a lower temperature, so it is preferred.
[0059] By this heat treatment, water contained in the organic compound layer 103 and water adsorbed on the surface of the organic compound layer 103, in particular, water contained in the intermediate layer 116 of the layer containing an alkali metal or an alkali metal compound can be removed. Thus, even if a manufacturing method is adopted in which the intermediate layer 116 of the layer containing an alkali metal or an alkali metal compound is exposed to a photolithography process, a significant increase in the driving voltage of the light-emitting device and a significant decrease in the current efficiency can be prevented.
[0060] Then, if Figure 3D As shown, an inorganic insulating film 125f, which will later become the inorganic insulating layer 125, is formed to cover the organic compound layer 103 and the sacrificial layer 158. A specific method of depositing the inorganic insulating film 125f will be described in detail in the following embodiment.
[0061] Then, if Figure 4A As shown, an insulating film 127f, which will later become an insulating layer 127, is formed on the inorganic insulating film 125f. The insulating film 127f is preferably formed using a photosensitive material by spin coating, for example, and more specifically, is preferably formed using a photosensitive resin composition containing an acrylic resin. A specific deposition method of the insulating film 127f will be described in detail in the following embodiment.
[0062] Next, exposure is performed to sensitize a portion of the insulating film 127f with visible light or ultraviolet light. Here, when a positive photosensitive resin composition containing an acrylic resin is used for the insulating film 127f, visible light or ultraviolet light is irradiated onto the first electrode 101 in a region where the insulating layer 127 is not formed in a later process. Note that, when a negative photosensitive material is used for the insulating film 127f, visible light or ultraviolet light is irradiated onto a region where the insulating layer 127 is to be formed. A specific method of exposing the insulating film 127f will be described in detail in the following embodiment.
[0063] Then, if Figure 4BAs shown, a part of the insulating film 127f is removed by development to form an insulating layer 127a. The insulating layer 127a is formed in a region that does not overlap with the first electrode 101. A specific method of forming the insulating layer 127a will be described in detail in the following embodiments.
[0064] Then, if Figure 4C As shown, etching is performed using the insulating layer 127a as a mask to remove a portion of the inorganic insulating film 125f, thereby reducing the thickness of a portion of the sacrificial layer 158. Thus, the inorganic insulating layer 125 is formed under the insulating layer 127a. In addition, the surface of the thin portion of the sacrificial layer 158 is exposed. In this way, by leaving the sacrificial layer 158 on the organic compound layer 103, the organic compound layer 103 can be prevented from being damaged in the processing of the subsequent steps. Thus, a light-emitting device with high reliability can be manufactured.
[0065] A specific method of etching using the insulating layer 127a as a mask will be described in detail in a later embodiment. In addition, the effect of the remaining sacrificial layer 158 will be described in detail in a later embodiment.
[0066] Next, heat treatment is performed. By performing heat treatment, the shape of the insulating layer 127a can be deformed so that its side has a tapered shape, thereby forming the insulating layer 127 ( Figure 4D ). The heat treatment is performed at a temperature lower than the heat resistance temperature of the organic compound layer. The heat treatment can be performed at a substrate temperature of 50°C to 200°C, preferably 60°C to 150°C, and more preferably 70°C to 130°C. The heating atmosphere may be either an air atmosphere or an inert gas atmosphere. In addition, the heating atmosphere may be either an air atmosphere or a reduced pressure atmosphere. The details of the heat treatment after the etching process using the insulating layer 127a as a mask are described in detail in the following embodiments.
[0067] Then, if Figure 5A As shown, etching is performed using the insulating layer 127 as a mask to remove a portion of the sacrificial layer 158 (or a portion where the thickness of the sacrificial layer 158 is relatively thin). Note that a portion of the inorganic insulating layer 125 may also be removed. As a result, an opening is formed in the sacrificial layer 158, and a portion of the top surface of the organic compound layer 103 is exposed.
[0068] Removal of a portion of the sacrificial layer 158 by etching using the insulating layer 127 as a mask is performed by wet etching. By using the wet etching method, damage to the organic compound layer 103 can be reduced compared to the case of using the dry etching method. A specific method of removing a portion of the sacrificial layer 158 by etching using the insulating layer 127 as a mask is described in detail in the following embodiment.
[0069] In addition, after a portion of the top surface of the organic compound layer 103 is exposed, heat treatment is further performed. By this heat treatment, water contained in the organic compound layer 103, water adsorbed on the surface of the organic compound layer 103, and water contained in the intermediate layer 116 which is a layer containing an alkali metal or an alkali metal compound, etc. can be removed. In addition, the shape of the insulating layer 127 may change due to this heat treatment. Specifically, the insulating layer 127 may expand so as to cover at least one of the end of the inorganic insulating layer 125, the end of the sacrificial layer 158, and the top surface of the organic compound layer 103.
[0070] If the temperature of the heat treatment is too low, water contained in the organic compound layer 103, water adsorbed on the surface of the organic compound layer 103, and water contained in the intermediate layer 116 which is a layer containing an alkali metal or an alkali metal compound cannot be sufficiently removed. If the temperature of the heat treatment is too high, the organic compound layer 103 may be degraded or the shape of the insulating layer 127 may be excessively changed. Therefore, the heat treatment temperature is preferably higher than the temperature at which water is desorbed from the organic compound layer 103 and lower than the glass transition temperature of the organic compound contained in the organic compound layer 103, and is preferably lower than the glass transition temperature of the organic compound contained in the top surface of the organic compound layer 103. Specifically, the substrate temperature is preferably 80° C. to 130° C., more preferably 90° C. to 120° C., further preferably 100° C. to 120° C., and further preferably 100° C. to 110° C. The heating atmosphere may be either an air atmosphere or an inert gas atmosphere. Note that the heating atmosphere may be an atmospheric pressure atmosphere or a reduced pressure atmosphere, and a reduced pressure atmosphere is preferably used to prevent water desorbed from the organic compound layer 103 from being re-adsorbed.
[0071] By this heat treatment, water contained in the organic compound layer 103, water adsorbed on the surface of the organic compound layer 103, and water contained in the intermediate layer 116 which is a layer containing an alkali metal or an alkali metal compound can be sufficiently removed without causing degradation of the organic compound layer 103 and excessive change in the shape of the insulating layer 127. Thus, even when a manufacturing method is adopted in which the intermediate layer 116 which is a layer containing an alkali metal or an alkali metal compound is exposed to a photolithography process, a significant increase in the driving voltage of the light-emitting device and a significant decrease in the current efficiency can be prevented.
[0072] Then, if Figure 5B As shown in FIG. 1 , the second electrode 102 is formed over the organic compound layer 103 and the insulating layer 127. The second electrode 102 can be formed by a method such as sputtering or vacuum evaporation. Alternatively, the second electrode 102 can be formed by stacking a film formed by evaporation and a film formed by sputtering.
[0073] Through the above-mentioned processes, the light emitting device 130 can be manufactured.
[0074] In addition, after the heat treatment, Figure 5C As shown, the organic compound layer 502b and the second electrode 102 may be formed over the organic compound layer 103. Since the organic compound layer 502b is deposited after the photolithography step, a material with low heat resistance can be selected as a material that can be used for the organic compound layer 502b, thereby expanding the range of material selection.
[0075] In the light-emitting device 130, the organic compound layer 502b can use a material used as an electron injection layer, for example. Specifically, as the organic compound layer 502b, a layer containing an alkali metal or an alkali metal compound can be formed. By forming a layer containing an alkali metal or an alkali metal compound after a photolithography process, a significant increase in the driving voltage of the light-emitting device or a significant decrease in the current efficiency can be prevented. In addition, when the organic compound layer 502b is provided, the stacked structure of the organic compound layer 103 and the organic compound layer 502b is equivalent to the organic compound layer 103 in Embodiment 1.
[0076] As described above, in the method for manufacturing a light-emitting device according to one embodiment of the present invention, the island-shaped organic compound layer 103 is not formed using a high-precision metal mask but is formed by depositing a film on one surface and then processing it, so that the island-shaped layer can be formed with a uniform thickness. In addition, a light-emitting device that realizes a high-definition display device or a display device with a high aperture ratio can be manufactured. In addition, even a tandem light-emitting device manufactured by photolithography can provide a light-emitting device with good characteristics.
[0077] This embodiment mode can be combined with other embodiment modes or examples as appropriate. In addition, in this specification, when a plurality of configuration examples are shown in one embodiment mode, the configuration examples can be combined as appropriate.
[0078] (Implementation Method 2) In this embodiment, materials that can be used for each layer of the light-emitting device 130 described in Embodiment 1 are described.
[0079] First, the materials that can be used for the intermediate layer 116 are described. The intermediate film 116f is a film that contains at least an alkali metal or an alkali metal compound. More specifically, the intermediate film 116f is a film that includes an N-type film and a P-type film, and the N-type film preferably contains an alkali metal or an alkali metal compound. Specific examples of alkali metals include lithium, sodium, potassium, rubidium, cesium, francium, etc. Specific examples of alkali metal compounds include compounds of the above-mentioned alkali metals, for example, lithium compounds such as lithium oxide. In addition, in addition to alkali metals or alkali metal compounds, the N-type film may also contain organic compounds with electron transport properties.
[0080] As the alkali metal or alkali metal compound, lithium or a lithium compound is more preferably used, and specifically, lithium, a lithium complex, a lithium compound, a lithium alloy, etc. can be used. Specifically, lithium, lithium oxide, lithium nitride, lithium carbonate, lithium fluoride, 8-hydroxyquinoline-lithium (abbreviated as: Liq), 2-methyl-8-hydroxyquinoline-lithium (abbreviated as: Li-mq) and the like lithium complex containing an alkyl group can be cited.
[0081] As an organic compound having an electron-transporting property that can be used for the N-type layer 119, it is preferable to use an organic compound having an electron mobility of 1×10 -7 cm 2 / Vs or more, preferably 1×10 -6 cm 2 In addition, any substance other than the above may be used as long as it has a higher electron-transporting property than a hole-transporting property.
[0082] As the above-mentioned organic compound, an organic compound containing a π-electron-deficient heteroaromatic ring is preferably used. As the organic compound containing a π-electron-deficient heteroaromatic ring, for example, any one or more of an organic compound containing a heteroaromatic ring having a polyazole skeleton, an organic compound containing a heteroaromatic ring having a pyridine skeleton, an organic compound containing a heteroaromatic ring having a diazine skeleton, and an organic compound containing a heteroaromatic ring having a triazine skeleton is preferably used.
[0083] As the organic compound with electron transport property that can be used for the N-type layer 119, specifically, there can be mentioned: 2-(4-biphenylyl)-5-(4-tert-butylphenyl)-1,3,4-oxadiazole (abbreviated as: PBD), 3-(4-biphenylyl)-4-phenyl-5-(4-tert-butylphenyl)-1,2,4-triazole (abbreviated as: TAZ), 1,3-bis[5-(p-tert-butylphenyl)-1,3,4-oxadiazol-2-yl]benzene (abbreviated as: OXD-7), 9-[4-(5-phenyl-1,3,4-oxadiazol-2-yl)phenyl]-9H-carbazole (abbreviated as: CO11), 2,2',2"-(1,3,5-phenyltriyl)tris(1-phenyl-1H- organic compounds having an azole skeleton, such as benzoimidazole (abbreviated as TPBI), 2-[3-(dibenzothiophene-4-yl)phenyl]-1-phenyl-1H-benzimidazole (abbreviated as mDBTBIm-II), 4,4'-bis(5-methylbenzoxazol-2-yl)stilbene (abbreviated as BzOs); 3,5-bis[3-(9H-carbazole-9-yl)phenyl]pyridine (abbreviated as 35DCzPPy), 1,3,5-tris[3-(3-pyridyl)phenyl]benzene (abbreviated as TmPyPB), bathophenanthroline (abbreviated as Bphen), bathocuproin (abbreviated as BCP), 2,9-bis(naphthalene-2-yl)-4,7-diphenyl-1,10-phenanthroline (abbreviated as BCP), organic compounds containing a heteroaromatic ring having a pyridine skeleton, such as 2,2'-(1,3-phenylene)bis(9-phenyl-1,10-phenanthroline) (abbreviated as mPPhen2P); 2-[3-(dibenzothiophene-4-yl)phenyl]dibenzo[f,h]quinoxaline (abbreviated as 2mDBTPDBq-II), 2-[3-(3'-(dibenzothiophene-4-yl)biphenyl]dibenzo[f,h]quinoxaline (abbreviated as 2mDBTBPDBq-II), 2-[3'-(9H-carbazole-9-yl)biphenyl-3-yl]dibenzo[f,h]quinoxaline (abbreviated as 2mCzBPDBq), 2-[4'-(9-phenyl-9H- carbazole-3-yl)-3,1'-biphenyl-1-yl]dibenzo[f,h]quinoxaline (abbreviation: 2mpPCBPDBq), 2-[4-(3,6-diphenyl-9H-carbazole-9-yl)phenyl]dibenzo[f,h]quinoxaline (abbreviation: 2CzPDBq-Ⅲ), 7-[3-(dibenzothiophene-4-yl)phenyl]dibenzo[f,h]quinoxaline (abbreviation: 7mDBTPDBq-II), 6-[3-(dibenzothiophene-4-yl)phenyl]dibenzo[f,h]quinoxaline (abbreviation: 6mDBTPDBq-Ⅱ), 9-[(3'-dibenzothiophene-4-yl)biphenyl-3-yl]naphtho[1',2':4,5]furo[2,3-b]pyrazine (abbreviation: 9mDBtBPNfpr), 9-[(3'-dibenzothiophene-4-yl)biphenyl-4-yl]naphtho[1',2':4,5]furo[2,3-b]pyrazine (abbreviation: 9pmDBtBPNfpr), 4,6-bis[3-(phenanthrene-9-yl)phenyl]pyrimidine (abbreviation: 4,6mPnP2Pm), 4,6-bis[3-(4-dibenzothiophene-yl)phenyl]pyrimidine (abbreviation: 4,6mDBTP2Pm-II), 4,6-bis[3-(9H-carbazole-9-yl)phenyl]pyrimidine (abbreviation: 4,6mCzP2Pm), 9,9'-[pyrimidine-4,6-diylbis(biphenyl-3,3'-diyl)]bis(9H-carbazole) (abbreviation: 4,6mCzBP2Pm), 8-(1,1'-biphenyl-4-yl)-4-[3-(dibenzothiophen-4-yl)phenyl]-[1]benzofurano[3,2-d]pyrimidine (abbreviation: 8BP-4mDBtPBfpm), 3,8-bis[3-(dibenzothiophen-4-yl)phenyl]benzofurano[2,3-b]pyrazine (abbreviation: 3,8mDBtP2Bfpr), 4,8-bis[3-(dibenzothiophen-4-yl)phenyl]-[1]benzofurano[3,2-d]pyrimidine (abbreviation: 4,8mDBtP2Bfpm), 8-[3'-(dibenzothiophen-4-yl)biphenyl-3-yl]naphtho[1',2':4,5]furano[3, 2-d]pyrimidine (abbreviation: 8mDBtBPNfpm), 8-[(2,2'-binaphthyl)-6-yl]-4-[3-(dibenzothiophen-4-yl)phenyl]-[1]benzofurano[3,2-d]pyrimidine (abbreviation: 8(βN2)-4mDBtPBfpm), 2,2'-(pyridine-2,6-diyl)bis(4-phenylbenzo[h]quinazoline) (abbreviation: 2,6(P-Bqn)2Py), 2,2'-(pyridine-2,6-diyl)bis{4-[4-(2-naphthyl)phenyl]-6-phenylpyrimidine} (abbreviation: 2,6(NP-PPm)2Py), 6-(biphenyl-3-yl)-4-[3,5-bis(9H-carbazole-9-yl)phenyl]-2 -phenylpyrimidine (abbreviation: 6mBP-4Cz2PPm), 2,6-bis(4-naphthylphenyl)-4-[4-(3-pyridyl)phenyl]pyrimidine (abbreviation: 2,4NP-6PyPPm), 4-[3,5-bis(9H-carbazol-9-yl)phenyl]-2-phenyl-6-(biphenyl-4-yl)pyrimidine (abbreviation: 6BP-4Cz2PPm), 7-[4-(9-phenyl-9H-carbazol-2-yl)quinazolin-2-yl]-7H-dibenzo[c,g]carbazole (abbreviation: PC-cgDBCzQz), etc.; 2-(biphenyl-4-yl)-4-phenyl-6-(9,9'-spirobi[9H-fluorene]-2-yl)-1,3,5-triazine (abbreviation: BP-SFTzn), 2-{3-[3-(benzo[b]naphtho[1,2-d]furan-8-yl)phenyl]phenyl}-4,6-diphenyl-1,3,5-triazine (abbreviation: mBnfBPTzn), 2-{3-[3-(benzo[b]naphtho[1,2-d]furan-6-yl)phenyl]phenyl}-4,6-diphenyl-1,3,5-triazine (abbreviation: mBnfBPTzn-02), 2-{4-[3-(N-phenyl-9H-carbazole-3-yl)-9H-carbazole-9-yl]phenyl}-4,6-diphenyl-1,3,5-triazine (abbreviation: PCCzPTzn), 9-[3-(4,6-diphenyl-1,3, 5-triazine-2-yl)phenyl]-9'-phenyl-2,3'-bi-9H-carbazole (abbreviated as mPCCzPTzn-02), 2-[3'-(9,9-dimethyl-9H-fluorene-2-yl)biphenyl-3-yl]-4,6-diphenyl-1,3,5-triazine (abbreviated as mFBPTzn), 5-[3-(4,6-diphenyl-1,3,5-triazine-2-yl)phenyl]-7,7-dimethyl-5H,7H-indeno[2,1-b]carbazole (abbreviated as mINc(II)PTzn), 2-{3-[3-(dibenzothiophen-4-yl)phenyl]phenyl}-4,6-diphenyl-1,3,5-triazine (abbreviated as mDBtBPTzn), 2,4 , 6-tris(3'-(pyridin-3-yl)biphenyl-3-yl)-1,3,5-triazine (abbreviated as: TmPPPyTz), 2-[3-(2,6-dimethyl-3-pyridinyl)-5-(9-phenanthrenyl)phenyl]-4,6-diphenyl-1,3,5-triazine (abbreviated as: mPn-mDMePyPTzn), 11-[4-(biphenyl-4-yl)-6-phenyl-1,3,5-triazine-2-yl]-11,12-dihydro-12-phenylindole[2,3-a]carbazole (abbreviated as: BP-Icz(II)Tzn), 2-[3'-(triphenylene-2-yl)biphenyl-3-yl]-4,6-diphenyl-1,3,5-triazine (abbreviated as: mTpBPTzn ), 3-[9-(4,6-diphenyl-1,3,5-triazine-2-yl)-2-dibenzothienyl]-9-phenyl-9H-carbazole (abbreviated as PCDBfTzn), 2-(biphenyl-3-yl)-4-phenyl-6-{8-[(1,1':4',1"-terphenyl)-4-yl-1-dibenzofuranyl}-1,3,5-triazine (abbreviated as mBP-TPDBfTzn), etc. having a triazine skeleton. In particular, it is preferred to use an organic compound having a phenanthroline skeleton such as Bphen, BCP, NBphen and mPPhen2P. Organic compounds having a phenanthroline dimer structure such as mPPhen2P have good stability and are therefore more preferred.
[0084] In addition, the P-type layer 117 used as the charge generation layer is preferably composed of a composite material containing a material having an acceptor property and an organic compound having a hole transport property. As the organic compound having a hole transport property used in the composite material, various organic compounds such as aromatic amine compounds, heteroaromatic compounds, aromatic hydrocarbons, high molecular weight compounds (oligomers, dendrimers, polymers, etc.) can be used. As the organic compound having a hole transport property used in the composite material, it is preferred to use an organic compound having a hole mobility of 1×10 -6 cm 2 / Vs or more organic compound. The organic compound with hole transport properties used in the composite material is preferably a compound containing a fused aromatic hydrocarbon ring or a π-electron-rich heteroaromatic ring. As the fused aromatic hydrocarbon ring, an anthracene ring, a naphthalene ring, etc. are preferred. In addition, as the π-electron-rich heteroaromatic ring, a fused aromatic ring containing at least one of a pyrrole skeleton, a furan skeleton, and a thiophene skeleton is preferred, specifically, a carbazole ring, a dibenzothiophene ring, or a ring in which these rings are also fused with an aromatic ring or a heteroaromatic ring.
[0085] These organic compounds having hole transport properties preferably have any one of a carbazole skeleton, a dibenzofuran skeleton, a dibenzothiophene skeleton, and an anthracene skeleton. In particular, it can be an aromatic amine having a substituent containing a dibenzofuran ring or a dibenzothiophene ring, an aromatic monoamine containing a naphthalene ring, or an aromatic monoamine in which a 9-fluorenyl group is bonded to the nitrogen of the amine through an arylene group. Note that when these organic compounds having hole transport properties are substances including N, N-bis(4-biphenyl)amino groups, a light-emitting device with a long life can be manufactured, so it is preferred.
[0086] Specific examples of the organic compound having a hole transport property include N-(4-biphenyl)-6,N-diphenylbenzo[b]naphtho[1,2-d]furan-8-amine (abbreviated as BnfABP), N,N-bis(4-biphenyl)-6-phenylbenzo[b]naphtho[1,2-d]furan-8-amine (abbreviated as BBABnf), 4,4'-bis(6-phenylbenzo[b]naphtho[1,2-d]furan-8-yl)-4"-phenyltriphenylamine (abbreviated as BnfBB1BP), N,N-bis(4-biphenyl)benzo[b]naphtho[1,2-d]furan-6-amine (abbreviated as BBABnf(6)), N,N-bis(4-biphenyl)benzo[b]naphtho[1,2-d]furan-8-amine (abbreviated as BBABnf(6)), furan-8-amine (abbreviation: BBABnf(8)), N,N-bis(4-biphenyl)benzo[b]naphtho[2,3-d]furan-4-amine (abbreviation: BBABnf(II)(4)), N,N-bis[4-(dibenzofuran-4-yl)phenyl]-4-amino-p-terphenyl (abbreviation: DBfBB1TP), N-[4-(dibenzothiophen-4-yl)phenyl]-N-phenyl-4-benzidine (abbreviation: ThBA1BP), 4-(2-naphthyl)-4',4"-diphenyltriphenylamine (abbreviation: BBAβNB), 4-[4-(2-naphthyl)phenyl]-4',4"-diphenyltriphenylamine (abbreviation: BBAβNBi), 4,4'-diphenyl-4"-(6; 1'-binaphthyl-2-yl) triphenylamine (abbreviation: BBAαNβNB), 4,4'-diphenyl-4"-(7;1'-binaphthyl-2-yl) triphenylamine (abbreviation: BBAαNβNB-03), 4,4'-diphenyl-4"-(7-phenyl)naphthyl-2-yl triphenylamine (abbreviation: BBAPβNB-03), 4,4'-diphenyl-4"-(6;2'-binaphthyl-2-yl) triphenylamine (abbreviation: BBA(βN2)B), 4,4'-diphenyl-4"-(7;2'-binaphthyl-2-yl)-triphenylamine (abbreviation: BBA(βN2)B-03), 4,4'-diphenyl-4"-(4;2'-binaphthyl-1-yl) triphenylamine (abbreviation: BBAβNαN B), 4,4'-diphenyl-4"-(5;2'-binaphthyl-1-yl)triphenylamine (abbreviated as: BBAβNαNB-02), 4-(4-biphenyl)-4'-(2-naphthyl)-4"-phenyltriphenylamine (abbreviated as: TPBiAβNB), 4-(3-biphenyl)-4'-[4-(2-naphthyl)phenyl]-4"-phenyltriphenylamine (abbreviated as: mTPBiAβNBi), 4-(4-biphenyl)-4'-[4-(2-naphthyl)phenyl]-4"-phenyltriphenylamine (abbreviated as: TPBiAβNBi), 4-phenyl-4'-(1-naphthyl)triphenylamine (abbreviated as: αNBA1BP), 4,4'-bis(1-naphthyl)triphenylamine (abbreviated as: αNBB1BP), 4,4'-Diphenyl-4"-[4'-(carbazol-9-yl)biphenyl-4-yl]triphenylamine (abbreviation: YGTBi1BP), 4'-[4-(3-phenyl-9H-carbazol-9-yl)phenyl]tri(biphenyl-4-yl)amine (abbreviation: YGTBi1BP-02), 4-[4'-(carbazol-9-yl)biphenyl-4-yl]-4'-(2-naphthyl)-4"-phenyltriphenylamine (abbreviation: YGTBiβNB), N-[4-(9-phenyl-9H-carbazol-3-yl)phenyl]-N-[4-(1-naphthyl)phenyl]-9,9'-spirobi[9H-fluorene]-2-amine (abbreviation: PCBNBSF), N,N-bis(-biphenyl-4-yl)-9,9'-spirobi[9H-fluorene]-2-amine (abbreviation: PCBNBSF), ]-2-amine (abbreviation: BBASF), N,N-bis(biphenyl-4-yl)-9,9'-spirobi[9H-fluorene]-4-amine (abbreviation: BBASF(4)), N-(biphenyl-2-yl)-N-(9,9-dimethyl-9H-fluorene-2-yl)-9,9'-spirobi[9H-fluorene]-4-amine (abbreviation: oFBiSF), N-(biphenyl-4-yl)-N-(9,9-dimethyl-9H-fluorene-2-yl)dibenzofuran-4-amine (abbreviation: FrBiF), N-[4-(1-naphthyl)phenyl]-N-[3-(6-phenyldibenzofuran-4-yl)phenyl]-1-naphthylamine (abbreviation: mPDBfBNBN), 4-phenyl-4'-(9-phenylfluorene-9- triphenylamine (abbreviation: BPAFLP), 4-phenyl-3'-(9-phenylfluoren-9-yl)triphenylamine (abbreviation: mBPAFLP), 4-phenyl-4'-[4-(9-phenylfluoren-9-yl)phenyl]triphenylamine (abbreviation: BPAFLBi), 4-phenyl-4'-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBA1BP), 4,4'-diphenyl-4"-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBBi1BP), 4-(1-naphthyl)-4'-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBANB), 4,4'-di(1-naphthyl)-4"-(9-phenyl-9H-carbazole- 3-yl) triphenylamine (abbreviation: PCBNBB), N-phenyl-N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]-9,9'-spirobi[9H-fluorene]-2-amine (abbreviation: PCBASF), N-(biphenyl-4-yl)-N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]-9,9-dimethyl-9H-fluorene-2-amine (abbreviation: PCBBiF), N,N-bis(9,9-dimethyl-9H-fluorene-2-yl)-9,9'-spirobi-9H-fluorene-4-amine, N,N-bis(9,9-dimethyl-9H-fluorene-2-yl)-9,9'-spirobi-9H-fluorene-3-amine, N,N-bis(9,9-dimethyl-9H-fluorene-2-yl)-9,9'-spirodi-9H-fluorene-2-amine, N,N-bis(9,9-dimethyl-9H-fluorene-2-yl)-9,9'-spirodi-9H-fluorene-1-amine, etc.
[0087] In addition, as materials with hole transport properties, the following aromatic amine compounds can also be used: N,N'-di(p-tolyl)-N,N'-diphenyl-p-phenylenediamine (abbreviation: DTDPPA), 4,4'-bis[N-(4-diphenylaminophenyl)-N-phenylamino]biphenyl (abbreviation: DPAB), 4,4'-bis(N-{4-[N'-(3-methylphenyl)-N'-phenylamino]phenyl}-N-phenylamino)biphenyl (abbreviation: DNTPD), 1,3,5-tris[N-(4-diphenylaminophenyl)-N-phenylamino]benzene (abbreviation: DPA3B), etc.
[0088] As the acceptor substance contained in the P-type layer 117, an organic compound having an electron-withdrawing group (halogen group, cyano group, etc.) can be used, and examples thereof include 7,7,8,8-tetracyano-2,3,5,6-tetrafluoroquinodimethane (abbreviation: F4-TCNQ), chloranil, 2,3,6,7,10,11-hexacyano-1,4,5,8,9,12-hexaazatriphenylene (abbreviation: HAT-CN), 1,3,4,5,7,8-hexafluorotetracyano-naphthoquinodimethane (abbreviation: F6-TCNNQ), 2-(7-dicyano-1,3,4,5,6,8,9,10-octafluoro-7H-pyrene-2-ylidene)malononitrile, etc. In particular, compounds such as HAT-CN in which electron-withdrawing groups are bonded to fused aromatic rings having multiple heteroatoms are thermally stable and therefore are preferred. In addition, [3] axial ene derivatives having electron-withdrawing groups (especially halogen groups such as fluorine groups and cyano groups) are particularly preferred because their electron acceptability is very high. Specifically, examples include: α, α', α"-1,2,3-cyclopropane tris(ylidene) tris[4-cyano-2,3,5,6-tetrafluorophenylacetonitrile], α, α', α"-1,2,3-cyclopropane tris[2,6-dichloro-3,5-difluoro-4-(trifluoromethyl)phenylacetonitrile], α, α', α"-1,2,3-cyclopropane tris[2,3,4,5,6-pentafluorophenylacetonitrile], etc. As acceptor-capable substances, in addition to the above-mentioned organic compounds, transition metal oxides such as molybdenum oxide, vanadium oxide, ruthenium oxide, tungsten oxide, and manganese oxide can also be used.
[0089] The electron relay layer 118 contains a substance having electron transport properties, and can prevent the interaction between the N-type layer 119 and the P-type layer 117, and smoothly transfer electrons. The LUMO (Lowest Unoccupied Molecular Orbital) energy level of the substance having electron transport properties contained in the electron relay layer 118 is preferably between the LUMO energy level of the acceptor substance in the P-type layer 117 and the LUMO energy level of the layer ( Figure 1A Specifically, the LUMO energy level of the substance having electron transport properties in the electron relay layer 118 is preferably above -5.0 eV, more preferably above -5.0 eV and below -3.0 eV. In addition, as the substance having electron transport properties in the electron relay layer 118, a phthalocyanine material or a metal complex having a metal-oxygen bond and an aromatic ligand is preferably used.
[0090] Next, the structure of the light emitting device 130 other than the intermediate layer 116 will be described.
[0091] The first electrode 101 is an electrode including an anode. The first electrode 101 may also have a stacked structure, in which case the layer in contact with the organic compound layer 103 is used as an anode. The anode is preferably formed using a metal, an alloy, a conductive compound, and a mixture thereof having a large work function (specifically, 4.0 eV or more). Specifically, for example, indium oxide-tin oxide (ITO: Indium Tin Oxide), indium oxide-tin oxide containing silicon or silicon oxide, indium oxide-zinc oxide, indium oxide containing tungsten oxide and zinc oxide (IWZO), etc. may be cited. Although these conductive metal oxide films are usually deposited by sputtering, they can also be formed by applying a sol-gel method, etc. As an example of a formation method, a method of forming indium oxide-zinc oxide by sputtering using a target material having 1wt% to 20wt% of zinc oxide added to indium oxide may be cited. In addition, indium oxide (IWZO) containing tungsten oxide and zinc oxide can also be formed by sputtering using a target material in which 0.5wt% to 5wt% of tungsten oxide and 0.1wt% to 1wt% of zinc oxide are added to indium oxide. In addition, as materials for the anode, for example, gold (Au), platinum (Pt), nickel (Ni), tungsten (W), chromium (Cr), molybdenum (Mo), iron (Fe), cobalt (Co), copper (Cu), palladium (Pd) or nitrides of metal materials (for example, titanium nitride) can be cited. In addition, graphene can also be used as a material for the anode. In addition, by using the composite material constituting the P-type layer 117 in the above-mentioned intermediate layer 116 for the layer in contact with the anode (typically a hole injection layer), it is possible to select the electrode material without taking into account the work function.
[0092] The organic compound layer 103 has a stacked-layer structure. Figure 1A In the figure, as the stacked structure, a structure including a first light-emitting unit 501 having a first light-emitting layer 113_1, an intermediate layer 116, and a second light-emitting unit 502 having a second light-emitting layer 113_2 is shown. Note that a structure in which two light-emitting units are stacked with an intermediate layer is shown here, but a structure in which three or more light-emitting units are stacked can also be used. In this case, an intermediate layer is provided between the light-emitting units. Each light-emitting unit also has a stacked structure. The structure of the light-emitting unit is not limited to Figure 1A The structure shown can be constituted by using various functional layers such as a hole injection layer, a hole transport layer, an electron transport layer, an electron injection layer, a carrier blocking layer (hole blocking layer, electron blocking layer), and an exciton blocking layer as appropriate.
[0093] The hole injection layer 111 is in contact with the anode and has the function of making holes easily injected into the organic compound layer 103 (the first light-emitting unit 501). The hole injection layer 111 can be formed using phthalocyanine compounds such as phthalocyanine (abbreviated as H2Pc); phthalocyanine complex compounds such as copper phthalocyanine (abbreviated as CuPc); aromatic amine compounds such as 4,4'-bis[N-(4-diphenylaminophenyl)-N-phenylamino]biphenyl (abbreviated as DPAB), 4,4'-bis(N-{4-[N'-(3-methylphenyl)-N'-phenylamino]phenyl}-N-phenylamino)biphenyl (abbreviated as DNTPD); or polymers such as poly(3,4-ethylenedioxythiophene) / (polystyrenesulfonic acid) (abbreviated as PEDOT / PSS).
[0094] The hole injection layer 111 may also be formed of a substance having electron accepting properties. As the substance having electron accepting properties, the substances listed above as the accepting substances of the composite material constituting the P-type layer 117 in the intermediate layer 116 can be used in the same manner.
[0095] Similarly, the hole injection layer 111 may also be formed using the composite material constituting the P-type layer 117 in the intermediate layer 116 described above.
[0096] Note that in the hole injection layer 111, the organic compound with hole transport properties used in the composite material is more preferably a substance with a deeper HOMO energy level of -5.7 eV or higher and -5.4 eV or lower. When the organic compound with hole transport properties used in the composite material has a deeper HOMO energy level, holes are easily injected into the hole transport layer, and a light-emitting device with a long life can be easily obtained. In addition, when the organic compound with hole transport properties used in the composite material is a substance with a deeper HOMO energy level, the induction of holes is appropriately suppressed, so a light-emitting device with a longer life can be achieved.
[0097] By forming the hole injection layer 111, hole injection properties can be improved, so that a light-emitting device with a low driving voltage can be obtained.
[0098] Furthermore, among substances having acceptor properties, organic compounds having acceptor properties can be easily formed by vapor deposition and are therefore easy-to-use materials.
[0099] In addition, since the P-type layer 117 in the intermediate layer 116 is used as a hole injection layer, the second light emitting unit 502 is not provided with a hole injection layer, but the second light emitting unit may also be provided with a hole injection layer.
[0100] The hole transport layer (the first hole transport layer 112_1 and the second hole transport layer 112_2) is formed by including an organic compound having a hole transport property. The organic compound having a hole transport property preferably has a 1×10 -6 cm 2 / Vs and above hole mobility.
[0101] Examples of the hole-transporting material include 4,4'-bis[N-(1-naphthyl)-N-phenylamino]biphenyl (abbreviated as NPB), N,N'-diphenyl-N,N'-bis(3-methylphenyl)4,4'-diaminobiphenyl (abbreviated as TPD), N,N'-bis(9,9'spirobi[9H-fluorene]-2-yl)-N,N'-diphenyl-4,4'-diaminobiphenyl (abbreviated as BSPB), 4-phenyl-4'-(9-phenylfluorene-9-yl)triphenylamine (abbreviated as BPAFLP), 4-phenyl-3'-(9-phenylfluorene-9-yl)triphenylamine (abbreviated as mBPAFLP), 4-phenyl-4'-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviated as PCBA1BP), Compounds having an aromatic amine skeleton such as 4,4'-diphenyl-4"-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviated as PCBBi1BP), 4-(1-naphthyl)-4'-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviated as PCBANB), 4,4'-di(1-naphthyl)-4"-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviated as PCNBB), 9,9-dimethyl-N-phenyl-N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]fluorene-2-amine (abbreviated as PCBAF), and N-phenyl-N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]-9,9'-spirobi[9H-fluorene]-2-amine (abbreviated as PCBASF);1,3-Bis(N-carbazolyl)benzene (abbreviated as mCP), 4,4'-bis(N-carbazolyl)biphenyl (abbreviated as CBP), 3,6-bis(3,5-diphenylphenyl)-9-phenylcarbazole (abbreviated as CzTP), 3,3'-bis(9-phenyl-9H-carbazole) (abbreviated as PCCP), 9,9'-bis(biphenyl-4-yl)-3,3'-bi-9H-carbazole (abbreviated as BisBPCz), 9,9'-bis(1,1'-biphenyl-3-yl)-3,3'-bi-9H-carbazole (abbreviated as BismBPCz), 9-(1,1'-biphenyl-3-yl)-9'-(1,1'-biphenyl- 4-yl)-9H,9'H-3,3'-bicarbazole (abbreviated as mBPCCBP), 9-(2-naphthyl)-9'-phenyl-9H,9'H-3,3'-bicarbazole (abbreviated as βNCCP), 9-(3-biphenyl)-9'-(2-naphthyl)-3,3'-bi-9H-carbazole (abbreviated as βNCCmBP), 9-(4-biphenyl)-9'-(2-naphthyl)-3,3'-bi-9H-carbazole (abbreviated as βNCCBP), 9,9'-di-2-naphthyl-3,3'-9H,9'H-bicarbazole (abbreviated as BisβNCz), 9-(2-naphthyl)-9'-[1,1':4' ,1"-terphenyl]-3-yl-3,3'-9H,9'H-bicarbazole, 9-(2-naphthyl)-9'-[1,1':3',1"-terphenyl]-3-yl-3,3'-9H,9'H-bicarbazole, 9-(2-naphthyl)-9'-[1,1':3',1"-terphenyl]-5'-yl-3,3'-9H,9'H-bicarbazole, 9-(2-naphthyl)-9'-[1,1':3',1"-terphenyl]-4-yl-3,3'-9H,9'H-bicarbazole, 9-(2-naphthyl)-9'-[1,1':3',1"-terphenyl]-4-yl-3,3'-9H,9'H -bicarbazole, 9-(2-naphthyl)-9'-(triphenyl-2-yl)-3,3'-9H,9'H-bicarbazole, 9-phenyl-9'-(triphenyl-2-yl)-3,3'-9H,9'H-bicarbazole (abbreviated as: PCCzTp), 9,9'-bi(triphenyl-2-yl)-3,3'-9H,9'H-bicarbazole, 9-(4-biphenyl)-9'-(triphenyl-2-yl)-3,3'-9H,9'H-bicarbazole, 9-(triphenyl-2-yl)-9'-[1,1':3',1"-terphenyl]-4-yl-3,3'-9H,9'H-bicarbazole, etc.;Compounds having a thiophene skeleton, such as 4,4',4"-(benzene-1,3,5-triyl)tri(dibenzothiophene) (abbreviation: DBT3P-II), 2,8-diphenyl-4-[4-(9-phenyl-9H-fluorene-9-yl)phenyl]dibenzothiophene (abbreviation: DBTFLP-III), and 4-[4-(9-phenyl-9H-fluorene-9-yl)phenyl]-6-phenyldibenzothiophene (abbreviation: DBTFLP-IV); and compounds having a furan skeleton, such as 4,4',4"-(benzene-1,3,5-triyl)tri(dibenzofuran) (abbreviation: DBF3P-II), and 4-{3-[3-(9-phenyl-9H-fluorene-9-yl)phenyl]phenyl}dibenzofuran (abbreviation: mmDBFFLBi-II). Among them, compounds having an aromatic amine skeleton and compounds having a carbazole skeleton are preferred because they have good reliability and high hole transport properties and contribute to lowering the driving voltage. In addition, the materials listed as the materials having hole transport properties for the composite material used for the hole injection layer 111 can also be appropriately used as the materials constituting the hole transport layer. ;
[0102] The light-emitting layer (the first light-emitting layer 113_1 and the second light-emitting layer 113_2) preferably contains a light-emitting substance and a host material. Note that the light-emitting layer may also contain other materials. Alternatively, two layers having different compositions may be stacked.
[0103] The light-emitting substance may be a fluorescent substance, a phosphorescent substance, a substance exhibiting thermally activated delayed fluorescence (TADF), or other light-emitting substances.
[0104] In the light-emitting layer, materials that can be used as the fluorescent substance include, for example, the following substances. Note that other fluorescent substances can also be used.
[0105] Examples thereof include 5,6-bis[4-(10-phenyl-9-anthracenyl)phenyl]-2,2'-bipyridine (abbreviation: PAP2BPy), 5,6-bis[4'-(10-phenyl-9-anthracenyl)biphenyl-4-yl]-2,2'-bipyridine (abbreviation: PAPP2BPy), N,N'-diphenyl-N,N'-bis[4-(9-phenyl-9H-fluoren-9-yl)phenyl]pyrene-1,6-diamine (abbreviation: 1,6FLPAPrn), N,N'-bis(3-methylphenyl)-N, N'-bis[3-(9-phenyl-9H-fluorene-9-yl)phenyl]pyrene-1,6-diamine (abbreviated as: 1,6mMemFLPAPrn), N,N'-bis[4-(9H-carbazol-9-yl)phenyl]-N,N'-diphenylstilbene-4,4'-diamine (abbreviated as: YGA2S), 4-(9H-carbazol-9-yl)-4'-(10-phenyl-9-anthracenyl)triphenylamine (abbreviated as: YGAPA), 4-(9H-carbazol-9-yl)-4'-(9,10-diphenyl -2-anthryl)triphenylamine (abbreviation: 2YGAPPA), N,9-diphenyl-N-[4-(10-phenyl-9-anthryl)phenyl]-9H-carbazole-3-amine (abbreviation: PCAPA), perylene, 2,5,8,11-tetra-tert-butylperylene (abbreviation: TBP), 4-(10-phenyl-9-anthryl)-4'-(9-phenyl-9H-carbazole-3-yl)triphenylamine (abbreviation: PCBAPA), N,N"-(2-tert-butylanthracene-9,10-diyldi-4,1-phenylene)bis(2-tert-butylanthracene-9,10-diyldi-4,1-phenylene)bis(2-tert-butylanthracene-9,10-diyldi-4,1-phenylene)bis(2-tert-butylanthracene-9,10-diyldi-4,1-phenylene)bis(2-tert-butylanthracene-9,10-diyldi-4,1-phenylene)bis(2-tert-butylanthracene-1 (N,N',N'-triphenyl-1,4-phenylenediamine) (abbreviation: DPABPA), N,9-diphenyl-N-[4-(9,10-diphenyl-2-anthryl)phenyl]-9H-carbazole-3-amine (abbreviation: 2PCAPPA), N-[4-(9,10-diphenyl-2-anthryl)phenyl]-N,N',N'-triphenyl-1,4-phenylenediamine (abbreviation: 2DPAPPA), N,N,N',N',N",N",N"',N"'-octaphenyldibenzo[g,p] -2,7,10,15-tetramine (abbreviation: DBC1), coumarin 30, N-(9,10-diphenyl-2-anthracenyl)-N,9-diphenyl-9H-carbazole-3-amine (abbreviation: 2PCAPA), N-[9,10-bis(biphenyl-2-yl)-2-anthracenyl]-N,9-diphenyl-9H-carbazole-3-amine (abbreviation: 2PCABPhA), N-(9,10-diphenyl-2-anthracenyl)-N,N',N'-triphenyl-1,4-phenylenediamine (abbreviation: 2DPAPA), N-[9,10-bis(biphenyl-2-yl)-2-anthracenyl]-N,N',N'-triphenyl-1,4-phenylenediamine (abbreviation: 2DPABPhA), 9,10-bis(biphenyl- 2-{2-[4-(9H-carbazole-9-yl)phenyl]-N-phenylanthracen-2-amine (abbreviation: 2YGABPhA), N,N,9-triphenylanthracen-9-amine (abbreviation: DPhAPhA), coumarin 545T, N,N'-diphenylquinacridone (abbreviation: DPQd), rubrene, 5,12-bis(1,1'-biphenyl-4-yl)-6,11-diphenylnaphthacene (abbreviation: BPT), 2-(2-{2-[4-(dimethylamino)phenyl]vinyl}-6-methyl-4H-pyran-4-ylidene)malononitrile (abbreviation: DCM1), 2-{2-methyl-6-[2-(2,3,6,7-tetrahydro-1H,5H-benzo[ij]quinolizin-9-yl)ethyl 1-[4-[(4-methylphenyl)acenaphtho[1,2-a]fluoranthene-3,10-diamine (abbreviated as p-mPhAFD), 2-{2-isopropyl-6-[2-(1,1,7,7-tetramethyl-2,3,6,7-tetrahydro-1H,5H-benzo[ij]quinolizin-9-yl)vinyl]-4H-pyran-4-ylidene}malononitrile (abbreviated as DCJTI), 2-{2-tert-butyl-6-[2-(1,1,7,7-tetramethyl-2 ,3,6,7-tetrahydro-1H,5H-benzo[ij]quinolizin-9-yl)vinyl]-4H-pyran-4-ylidene}malononitrile (abbreviated as: DCJTB), 2-(2,6-bis{2-[4-(dimethylamino)phenyl]vinyl}-4H-pyran-4-ylidene)malononitrile (abbreviated as: BisDCM), 2-{2,6-bis[2-(8-methoxy-1,1,7,7-tetramethyl-2,3,6,7-tetrahydro-1H,5H-benzo[ij]quinolizin-9-yl)vinyl]-4H-pyran-4-ylidene}malononitrile (abbreviated as: BisDCJTM), N,N'-diphenyl-N,N'-(1,6-pyrene-diyl)bis[(6-phenylbenzo[b]naphtho[1,2-d] furan)-8-amine] (abbreviation: 1,6BnfAPrn-03), 3,10-bis[N-(9-phenyl-9H-carbazole-2-yl)-N-phenylamino] naphtho[2,3-b;6,7-b']bisbenzofuran (abbreviation: 3,10PCA2Nbf(IV)-02), 3,10-bis[N-(dibenzofuran-3-yl)-N-phenylamino] naphtho[2,3-b;6,7-b']bisbenzofuran (abbreviation: 3,10FrA2Nbf(IV)-02), etc. In particular, condensed aromatic diamine compounds represented by pyrene diamine compounds such as 1,6FLPAPrn, 1,6mMemFLPAPrn, and 1,6BnfAPrn-03 are preferred because they have good hole-trapping properties and high luminous efficiency or good reliability. ,
[0106] When a phosphorescent substance is used as a light-emitting substance in the light-emitting layer, examples of usable materials include the following substances.
[0107] Examples include organometallic iridium complexes having a 4H-triazole skeleton, such as tris{2-[5-(2-methylphenyl)-4-(2,6-dimethylphenyl)-4H-1,2,4-triazol-3-yl-κN2]phenyl-κC}iridium(III) (abbreviated as [Ir(mpptz-dmp)3]), tris(5-methyl-3,4-diphenyl-4H-1,2,4-triazole)iridium(III) (abbreviated as [Ir(Mptz)3]), and tris[4-(3-biphenyl)-5-isopropyl-3-phenyl-4H-1,2,4-triazole]iridium(III) (abbreviated as [Ir(iPrptz-3b)3]); tris[3-methyl-1-(2-methylphenyl)-5-phenyl-1H-1,2,4-triazole]iridium(III) (abbreviated as [Ir [Mptz1-mp)3]), tris(1-methyl-5-phenyl-3-propyl-1H-1,2,4-triazole)iridium(III) (abbreviated as [Ir(Prptz1-Me)3]), etc. having an organometallic iridium complex with a 1H-triazole skeleton; fac-tris[1-(2,6-diisopropylphenyl)-2-phenyl-1H-imidazole]iridium(III) (abbreviated as [Ir(iPrpim)3]), tris[3-(2,6-dimethylphenyl)-7-methylimidazo[1,2-f]phenanthridinato]iridium(III) (abbreviated as [Ir(dmpimpt-Me)3]), etc. having an imidazole skeleton; and bis[2-(4',6'-difluorophenyl)pyridinium-N,C 2’ ]iridium(III)tetrakis(1-pyrazolyl)borate (abbreviated as FIr6), bis[2-(4',6'-difluorophenyl)pyridinium-N,C 2’] iridium (III) picolinate (FIrpic), bis {2-[3', 5'-bis (trifluoromethyl) phenyl] pyridinium-N, C 2’ Iridium(III) picolinate (abbreviated as [Ir(CF3ppy)2(pic)]), bis[2-(4',6'-difluorophenyl)pyridinium-N,C 2’ ] Iridium (III) acetylacetonate (abbreviated as FIracac) and other organic metal iridium complexes with phenylpyridine derivatives having electron-withdrawing groups as ligands. The above substances are compounds that emit blue phosphorescence and have a luminescence peak in the wavelength region of 450nm to 520nm.
[0108] In addition, tris(4-methyl-6-phenylpyrimidinyl)iridium(III) (abbreviation: [Ir(mppm)3]), tris(4-tert-butyl-6-phenylpyrimidinyl)iridium(III) (abbreviation: [Ir(tBuppm)3]), (acetylacetonate)bis(6-methyl-4-phenylpyrimidinyl)iridium(III) (abbreviation: [Ir(mppm)2(acac)]), (acetylacetonate)bis(6-tert-butyl-4-phenylpyrimidinyl)iridium(III) (abbreviation: [Ir(tBuppm)2(acac)]), (acetylacetonate)bis(6-tert-butyl-4-phenylpyrimidinyl)iridium(III) (abbreviation: [Ir(tBuppm)2(acac)]), (acetylacetonate)bis[6-(2-norbornyl)-4-phenylpyrimidinyl]iridium(III) (abbreviation: [Ir(nbppm)2(acac)]), (acetylacetonate)bis[5-methyl [Ir(mppr-iPr)2(acac)]) and other organic metal iridium complexes with a pyrimidine skeleton, such as (acetylacetonato)bis(3,5-dimethyl-2-phenylpyrazine)iridium(III) (abbreviated as [Ir(mppr-Me)2(acac)] and (acetylacetonato)bis(5-isopropyl-3-methyl-2-phenylpyrazine)iridium(III) (abbreviated as [Ir(mppr-iPr)2(acac)]; [Ir(mppr-iPr)2(acac)] and other organic metal iridium complexes with a pyrazine skeleton, such as tris(2-phenylpyridinium-N,C 2’ )iridium(III) (abbreviation: [Ir(ppy)3]), bis(2-phenylpyridinium-N,C 2’ )iridium(III)acetylacetonate (abbreviated as [Ir(ppy)2(acac)]), bis(benzo[h]quinoline)iridium(III)acetylacetonate (abbreviated as [Ir(bzq)2(acac)]), tris(benzo[h]quinoline)iridium(III) (abbreviated as [Ir(bzq)3]), tris(2-phenylquinoline-N,C 2’)iridium(III) (abbreviation: [Ir(pq)3]), bis(2-phenylquinoline-N,C 2’ )iridium(III) acetylacetonate (abbreviation: [Ir(pq)2(acac)]), [2-d3-methyl-8-(2-pyridyl-κN)benzofurano[2,3-b]pyridine-κC]bis[2-(5-d3-methyl-2-pyridyl-κN2)phenyl-κC]iridium(III) (abbreviation: [Ir(5mppy-d3)2(mbfpypy-d3)), {2-(methyl-d3)-8-[4-(1-methylethyl-1-d)-2-pyridyl-κN]benzofurano[2,3-b]pyridin-7-yl-κC}bis{5-(methyl-d3)-2-[5-(methyl-d3)-2-pyridyl-κN]phenyl-κC}iridium(III) (abbreviation: Ir(5mtpy-d3)2(mbfpypy-d3)), Organometallic iridium complexes having a pyridine skeleton, such as [2-d3-methyl-(2-pyridyl-κN)benzofurano[2,3-b]pyridine-κC]bis[2-(2-pyridyl-κN)phenyl-κC]iridium(III) (abbreviated as [Ir(ppy)2(mbfpypy-d3)), [2-(4-methyl-5-phenyl-2-pyridyl-κN)phenyl-κC]bis[2-(2-pyridyl-κN)phenyl-κC]iridium(III) (abbreviated as Ir(ppy)2(mdppy)); and rare earth metal complexes such as tris(acetylacetonato)(monophenanthroline)terbium(III) (abbreviated as [Tb(acac)3(Phen)]). The above substances are mainly compounds that exhibit green phosphorescence and have a luminescence peak in the wavelength region of 500nm to 600nm. In addition, an organometallic iridium complex having a pyrimidine skeleton is particularly preferred because it has particularly excellent reliability and luminous efficiency.
[0109] In addition, organic metal iridium complexes having a pyrimidine skeleton include: (diisobutyrylmethane)bis[4,6-bis(3-methylphenyl)pyrimidinyl]iridium(III) (abbreviation: [Ir(5mdppm)2(dibm)]), bis[4,6-bis(3-methylphenyl)pyrimidinyl](dipivaloylmethanyl)iridium(III) (abbreviation: [Ir(5mdppm)2(dpm)]), bis[4,6-di(naphthalene-1-yl)pyrimidinyl](dipivaloylmethanyl)iridium(III) (abbreviation: [Ir(d1npm)2(dpm)]); Organometallic iridium complexes having a pyrazine skeleton, such as (acetylacetonato)bis(2,3,5-triphenylpyrazine)iridium(III) (abbreviated as [Ir(tppr)2(acac)]), bis(2,3,5-triphenylpyrazine)(dipivaloylmethano)iridium(III) (abbreviated as [Ir(tppr)2(dpm)]), (acetylacetonato)bis[2,3-bis(4-fluorophenyl)quinoxalinato]iridium(III) (abbreviated as [Ir(Fdpq)2(acac)]); tris(1-phenylisoquinoline-N,C 2’ )iridium(III) (abbreviated as [Ir(piq)3]), bis(1-phenylisoquinoline-N,C 2’ ) iridium (III) acetylacetonate (abbreviation: [Ir(piq)2(acac)]) and other organic metal iridium complexes having a pyridine skeleton; 2,3,7,8,12,13,17,18-octaethyl-21H,23H-porphyrin platinum (II) (abbreviation: PtOEP) and other platinum complexes; and tris (1,3-diphenyl-1,3-propanedionato) (monophenanthroline) europium (III) (abbreviation: [Eu(DBM)3(Phen)]), tris [1-(2-thenoyl) -3,3,3-trifluoroacetonato] (monophenanthroline) europium (III) (abbreviation: [Eu(TTA)3(Phen)] and other rare earth metal complexes. The above substances are compounds that exhibit red phosphorescence and have a luminescence peak in the wavelength region of 600nm to 700nm. In addition, organometallic iridium complexes with a pyrazine skeleton can obtain red luminescence with good chromaticity.
[0110] Furthermore, in addition to the above-mentioned phosphorescent compounds, known phosphorescent compounds may be selected and used.
[0111] As TADF materials, fullerene and its derivatives, acridine and its derivatives, and eosin derivatives can be used. In addition, metal-containing porphyrins containing magnesium (Mg), zinc (Zn), cadmium (Cd), tin (Sn), platinum (Pt), indium (In), or palladium (Pd) can also be mentioned. As the metal-containing porphyrin, for example, there can be mentioned protoporphyrin-tin fluoride complex (SnF2(Proto IX)), mesoporphyrin-tin fluoride complex (SnF2(Meso IX)), hematoporphyrin-tin fluoride complex (SnF2(Hemato IX)), coproporphyrin tetramethyl ester-tin fluoride complex (SnF2(Copro III-4Me), octaethylporphyrin-tin fluoride complex (SnF2(OEP)), protoporphyrin-tin fluoride complex (SnF2(Etio I)) and octaethylporphyrin-platinum chloride complex (PtCl2OEP) etc. represented by the following structural formula.
[0112] [Chemical formula 1]
[0113] In addition, 2-(biphenyl-4-yl)-4,6-bis(12-phenylindol[2,3-a]carbazole-11-yl)-1,3,5-triazine (abbreviation: PIC-TRZ), 9-(4,6-diphenyl-1,3,5-triazine-2-yl)-9'-phenyl-9H,9'H-3,3'-bicarbazole (abbreviation: PCCzTzn), 2-{4-[3-(N-phenyl-9H-carbazole-3-yl)-9H-carbazole-9-yl]phenyl}-4,6-diphenyl-1,3,5-triazine (abbreviation: PCCzPTzn), 2-[4-(10H-phenoxazine-10-yl)phenyl]-4,6-diphenyl-1,3,5-triazine (abbreviation: PCCzPTzn), and 2-[4-(10H-phenoxazine-10-yl)phenyl]-4,6-diphenyl-1,3,5-triazine (abbreviation: PCCzPTzn) represented by the following structural formula can also be used. Heterocyclic compounds having one or both of a π-electron-rich heteroaromatic ring and a π-electron-deficient heteroaromatic ring, such as 5-triazine (abbreviation: PXZ-TRZ), 3-[4-(5-phenyl-5,10-dihydrophenazine-10-yl)phenyl]-4,5-diphenyl-1,2,4-triazole (abbreviation: PPZ-3TPT), 3-(9,9-dimethyl-9H-acridin-10-yl)-9H-oxanthene-9-one (abbreviation: ACRXTN), bis[4-(9,9-dimethyl-9,10-dihydroacridinium)phenyl]sulfone (abbreviation: DMAC-DPS), and 10-phenyl-10H,10'H-spiro[acridine-9,9'-anthracene]-10'-one (abbreviation: ACRSA). The heterocyclic compound has a π-electron-rich heteroaromatic ring and a π-electron-deficient heteroaromatic ring, and both electron transport and hole transport are high, so it is preferred. Among them, in the skeleton with a π-electron-deficient heteroaromatic ring, a pyridine skeleton, a diazine skeleton (pyrimidine skeleton, pyrazine skeleton, pyridazine skeleton) and a triazine skeleton are stable and have good reliability, so it is preferred. In particular, the acceptor of the benzofuran pyrimidine skeleton, the benzothiophene pyrimidine skeleton, the benzofuran pyrazine skeleton, and the benzothiophene pyrazine skeleton is high and has good reliability, so it is preferred. In addition, in the skeleton with a π-type electron-rich heteroaromatic ring, an acridine skeleton, a phenoxazine skeleton, a phenothiazine skeleton, a furan skeleton, a thiophene skeleton and a pyrrole skeleton are stable and have good reliability, so it is preferred to have at least one of the above skeletons. In addition, a dibenzofuran skeleton is preferably used as a furan skeleton, and a dibenzothiophene skeleton is preferably used as a thiophene skeleton. As the pyrrole skeleton, it is particularly preferred to use an indole skeleton, a carbazole skeleton, an indolecarbazole skeleton, a bicarbazole skeleton, and a 3-(9-phenyl-9H-carbazole-3-yl)-9H-carbazole skeleton. In a substance in which a π-electron-rich heteroaromatic ring and a π-electron-deficient heteroaromatic ring are directly bonded, the electron donation property of the π-electron-rich heteroaromatic ring and the electron acceptance property of the π-electron-deficient heteroaromatic ring are both high, and the energy difference between the S1 energy level and the T1 energy level becomes small, so that thermally activated delayed fluorescence can be efficiently obtained, so it is particularly preferred. Note that an aromatic ring bonded with an electron-withdrawing group such as a cyano group can also be used instead of a π-electron-deficient heteroaromatic ring. In addition, as a π-electron-rich skeleton, an aromatic amine skeleton, a phenazine skeleton, etc. can be used.In addition, as the π-electron-deficient skeleton, a xanthene skeleton, a thioxanthene dioxide skeleton, an oxadiazole skeleton, a triazole skeleton, an imidazole skeleton, an anthraquinone skeleton, a boron-containing skeleton such as phenylborane and boranthrene, an aromatic ring having a nitrile group or a cyano group such as benzonitrile or cyanophenyl, a heteroaromatic ring, a carbonyl skeleton such as benzophenone, a phosphine oxide skeleton, a sulfone skeleton, etc. can be used. In this way, a π-electron-deficient skeleton and a π-electron-rich skeleton can be used to replace at least one of the π-electron-deficient heteroaromatic ring and the π-electron-rich heteroaromatic ring.
[0114] [Chemical formula 2]
[0115] In addition, as a TADF material, a TADF material in which a singlet excited state and a triplet excited state are in thermal equilibrium can also be used. Since such a TADF material has a short luminescence lifetime (excitation lifetime), it can suppress the reduction in efficiency in the high brightness area of the light-emitting device. Specifically, materials having the following molecular structures can be cited.
[0116] [Chemical formula 3]
[0117] TADF materials refer to materials with a small difference between the S1 energy level and the T1 energy level and the function of converting triplet excitation energy into singlet excitation energy through anti-intersystem crossing. Therefore, it is possible to up-convert triplet excitation energy into singlet excitation energy (anti-intersystem crossing) through tiny thermal energy and efficiently generate singlet excited states. In addition, triplet excitation energy can be converted into luminescence.
[0118] The exciplex formed by two substances in an excited state has the function of a TADF material that can convert triplet excitation energy into singlet excitation energy because the difference between the S1 energy level and the T1 energy level is extremely small.
[0119] Note that as an indicator of the T1 level, a phosphorescence spectrum observed at a low temperature (e.g., 77 K to 10 K) can be used. With respect to the TADF material, when the wavelength energy of an extrapolated line obtained by cutting a line at the tail of the short wavelength side of the fluorescence spectrum is taken as the S1 level and the wavelength energy of an extrapolated line obtained by cutting a line at the tail of the short wavelength side of the phosphorescence spectrum is taken as the T1 level, it is preferred that the difference between S1 and T1 is 0.3 eV or less, more preferably 0.2 eV or less.
[0120] In addition, when a TADF material is used as a light-emitting substance, the S1 energy level of the host material is preferably higher than the S1 energy level of the TADF material. In addition, the T1 energy level of the host material is preferably higher than the T1 energy level of the TADF material.
[0121] As the host material of the light-emitting layer, various carrier transport materials such as a material having an electron transport property and / or a material having a hole transport property, and the above-mentioned TADF material can be used.
[0122] As the material having a hole transporting property, the above-mentioned materials having a hole transporting property can be used in the same manner.
[0123] As the material having an electron-transporting property, the above-mentioned materials having an electron-transporting property can be used in the same manner.
[0124] As a TADF material that can be used as a host material, the same material as the material cited above as a TADF material can be used. When a TADF material is used as a host material, the triplet excitation energy generated by the TADF material is converted into singlet excitation energy through anti-intersystem crossing and further energy is transferred to the luminescent material, thereby improving the luminous efficiency of the light-emitting device. At this time, the TADF material is used as an energy donor and the luminescent material is used as an energy acceptor.
[0125] This is very effective when the above-mentioned luminescent material is a fluorescent luminescent material. In addition, at this time, in order to obtain high luminous efficiency, the S1 energy level of the TADF material is preferably higher than the S1 energy level of the fluorescent luminescent material. In addition, the T1 energy level of the TADF material is preferably higher than the S1 energy level of the fluorescent luminescent material. Therefore, the T1 energy level of the TADF material is preferably higher than the T1 energy level of the fluorescent luminescent material.
[0126] In addition, it is preferable to use a TADF material that emits light at a wavelength overlapping with the absorption band on the lowest energy side of the fluorescent material. This is preferable because the excitation energy is smoothly transferred from the TADF material to the fluorescent material, and light emission can be obtained efficiently.
[0127] In order to efficiently generate singlet excitation energy from triplet excitation energy by anti-intersystem crossing, carrier recombination is preferably generated in TADF material. In addition, it is preferred that the triplet excitation energy generated in TADF material is not transferred to the triplet excitation energy of fluorescent material. For this reason, the fluorescent material preferably has a protecting group around the luminophore (the skeleton that becomes the cause of luminescence) possessed by the fluorescent material. As the protecting group, it is preferably a substituent without a π bond, preferably a saturated hydrocarbon, specifically, an alkyl group having a carbon number of more than 3 and less than 10, a substituted or unsubstituted cycloalkyl group having a carbon number of more than 3 and less than 10, and a trialkylsilyl group having a carbon number of more than 3 and less than 10, more preferably having a plurality of protecting groups. Substituents without π bonds have almost no function of transmitting carriers, so there is almost no effect on carrier transmission or carrier recombination, and the luminophore of the TADF material and the fluorescent material can be kept away from each other. Here, the luminophore refers to the atomic group (skeleton) that becomes the cause of luminescence in the fluorescent material. The luminophore preferably has a π-bond skeleton, preferably contains an aromatic ring, and preferably has a condensed aromatic ring or a condensed heteroaromatic ring. Examples of the condensed aromatic ring or the condensed heteroaromatic ring include a phenanthrene skeleton, a stilbene skeleton, an acridone skeleton, a phenoxazine skeleton, a phenothiazine skeleton, and the like. In particular, luminophores having a naphthalene skeleton, an anthracene skeleton, a fluorene skeleton, Fluorescent substances having a chrysene skeleton, a triphenylene skeleton, a tetracene skeleton, a pyrene skeleton, a perylene skeleton, a coumarin skeleton, a quinacridone skeleton, or a naphthobisbenzofuran skeleton are preferred because they have high fluorescence quantum yields.
[0128] In the case where a fluorescent luminescent substance is used as a luminescent substance, a material having an anthracene skeleton is preferably used as a host material. By using a substance having an anthracene skeleton as a host material of a fluorescent luminescent substance, a light-emitting layer having high luminous efficiency and durability can be achieved. Among the substances having an anthracene skeleton used as a host material, substances having a diphenylanthracene skeleton (especially a 9,10-diphenylanthracene skeleton) are chemically stable, so they are preferred. In addition, in the case where the host material has a carbazole skeleton, the injection / transport properties of holes are improved, so it is preferred. In the case of a benzocarbazole skeleton having a benzene ring fused to carbazole, its HOMO energy level is about 0.1eV shallower than carbazole, and holes are easily injected, so it is more preferred. In particular, in the case where the host material has a dibenzocarbazole skeleton, its HOMO energy level is about 0.1eV shallower than carbazole, and not only holes are easily injected, but also hole transport and heat resistance are improved, so it is preferred. Therefore, a more preferred host material is one having a 9,10-diphenylanthracene skeleton and a carbazole skeleton (or a benzocarbazole skeleton or a dibenzocarbazole skeleton). Note that from the viewpoint of the hole injection / transport property, a benzofluorene skeleton or a dibenzofluorene skeleton may be used instead of the carbazole skeleton. Examples of such substances include 9-phenyl-3-[4-(10-phenyl-9-anthracenyl)phenyl]-9H-carbazole (abbreviated as PCzPA), 3-[4-(1-naphthyl)phenyl]-9-phenyl-9H-carbazole (abbreviated as PCPN), 9-[4-(10-phenyl-9-anthracenyl)phenyl]-9H-carbazole (abbreviated as CzPA), 7-[4-(10-phenyl-9-anthracenyl)phenyl]-7H-dibenzo[c,g]carbazole (abbreviated as cgDBCzPA), 6-[3-(9,10-diphenyl-2-anthracenyl)phenyl]benzo[b]naphtho[1,2-d]furan (abbreviated as 2mBnfPPA), 9-phenyl-10-[4′-(9-phenyl-9H-fluoren-9-yl)phenyl]-9H-carbazole (abbreviated as PCPN), -biphenyl-4-yl]anthracene (abbreviation: FLPPA), 9-(1-naphthyl)-10-[4-(2-naphthyl)phenyl]anthracene (abbreviation: αN-βNPAnth), 9-(1-naphthyl)-10-(2-naphthyl)anthracene (abbreviation: α, βADN), 2-(10-phenylanthracene-9-yl)dibenzofuran, 2-(10-phenyl-9-anthracenyl)benzo[b]naphtho[2,3-d]furan (abbreviation: Bnf(II)PhA), 9-(2-naphthyl)-10-[3-(2-naphthyl)phenyl]anthracene (abbreviation: βN-mβNPAnth), 1-[4-(10-(biphenyl-4-yl)-9-anthracenyl)phenyl]-2-ethyl-1H-benzimidazole (abbreviation: EtBImPBPhA), etc. In particular, CzPA, cgDBCzPA, 2mBnfPPA, and PCzPA are preferred because they exhibit very good properties.
[0129] In addition, the host material may also be a material mixed with multiple substances. When a mixed host material is used, it is preferred to mix a material having electron transport properties and a material having hole transport properties. By mixing a material having electron transport properties and a material having hole transport properties, it is easier to adjust the transport properties of the light-emitting layer 113, and it is also easier to control the recombination area. The weight ratio of the content of the material having hole transport properties to the content of the material having electron transport properties is 1:19 to 19:1.
[0130] Note that as part of the above mixed material, a phosphorescent substance may be used. When a fluorescent substance is used as a light-emitting substance, the phosphorescent substance may be used as an energy donor for supplying excitation energy to the fluorescent substance.
[0131] In addition, these mixed materials can also be used to form an exciplex. By selecting the mixed material in a manner to form an exciplex that exhibits light overlapping with the wavelength of the absorption band on the lowest energy side of the luminescent substance, energy transfer can be smoothed, thereby efficiently obtaining luminescence, so it is preferred. In addition, by adopting this structure, the driving voltage can be reduced, so it is preferred.
[0132] Note that at least one of the materials forming the exciplex may be a phosphorescent substance. In this way, triplet excitation energy can be efficiently converted into singlet excitation energy via anti-intersystem crossing.
[0133] Regarding the combination of materials that efficiently form an exciplex, the HOMO energy level of the material having hole transport properties is preferably higher than the HOMO energy level of the material having electron transport properties. In addition, the LUMO energy level of the material having hole transport properties is preferably higher than the LUMO energy level of the material having electron transport properties. Note that the LUMO energy level and HOMO energy level of the material can be obtained from the electrochemical properties (reduction potential and oxidation potential) of the material measured by cyclic voltammetry (CV) measurement.
[0134] Note that the formation of an exciplex can be confirmed, for example, by comparing the emission spectra of a material having hole transport properties, the emission spectra of a material having electron transport properties, and the emission spectra of a mixed film formed by mixing these materials. When the emission spectrum of the mixed film is observed to drift toward the long wavelength side compared to the emission spectrum of each material (or to have a new peak on the long wavelength side), it indicates that an exciplex has been formed. Alternatively, the transient photoluminescence (PL) of a material having hole transport properties, the transient PL of a material having electron transport properties, and the transient PL of a mixed film formed by mixing these materials are compared. When the transient response is different, such as the ratio of the transient PL lifetime of the mixed film to the transient PL lifetime of each material having a long-life component or a delayed component becomes larger, it indicates that an exciplex has been formed. In addition, the above-mentioned transient PL can be referred to as transient electroluminescence (EL). In other words, the formation of an exciplex can be confirmed by comparing the transient EL of a material having hole transport properties, the transient EL of a material having electron transport properties, and the transient EL of a mixed film of these materials and observing the difference in transient response.
[0135] The electron transport layer (first electron transport layer 114_1, second electron transport layer 114_2) is a layer containing a substance having an electron transport property. As the material having an electron transport property, it is preferable to use a material having an electron mobility of 1×10 -7 cm 2 / Vs or more, preferably 1×10 -6 cm 2 / Vs or more. In addition, as long as the electron transport property is higher than the hole transport property, substances other than the above can be used. As the above-mentioned organic compound, it is preferred to use an organic compound containing a π-electron-deficient heteroaromatic ring. As an organic compound containing a π-electron-deficient heteroaromatic ring, for example, it is preferred to use any one or more of an organic compound containing a heteroaromatic ring having a polyazole skeleton, an organic compound containing a heteroaromatic ring having a pyridine skeleton, an organic compound containing a heteroaromatic ring having a diazine skeleton, and an organic compound containing a heteroaromatic ring having a triazine skeleton.
[0136] As the above-mentioned organic compound with electron transport properties that can be used for the electron transport layer, an organic compound that can be used as the organic compound with electron transport properties in the N-type layer of the above-mentioned intermediate layer 116 can be used in the same manner. Among them, an organic compound containing a heteroaromatic ring having a diazine skeleton, an organic compound containing a heteroaromatic ring having a pyridine skeleton, or an organic compound containing a heteroaromatic ring having a triazine skeleton has good reliability, so it is preferred. In particular, an organic compound containing a heteroaromatic ring having a diazine (pyrimidine or pyrazine) skeleton and an organic compound containing a heteroaromatic ring having a triazine skeleton have high electron transport properties, which helps to reduce the driving voltage.
[0137] In addition, the electron transport layer preferably has an electron mobility of 1×10 -7 cm 2 / Vs or above and 5×10 -5 cm 2 / Vs or less. By reducing the transportability of electrons in the electron transport layer, the amount of electrons injected into the light-emitting layer can be controlled, thereby preventing the light-emitting layer from becoming in a state with too many electrons. When the hole injection layer is formed using a composite material and the HOMO energy level of the material with hole transport properties in the composite material is a deeper HOMO energy level of more than -5.7eV and less than -5.4eV, a long life can be obtained, so it is particularly preferred. Note that at this time, the HOMO energy level of the material with electron transport properties is preferably above -6.0eV.
[0138] As the electron injection layer 115, a layer containing an alkali metal, alkaline earth metal, rare earth metal or a compound or complex thereof such as lithium fluoride (LiF), cesium fluoride (CsF), calcium fluoride (CaF2), 8-hydroxyquinoline-lithium (abbreviated as: Liq), ytterbium (Yb), etc., or a layer containing an alkali metal, alkaline earth metal or a rare earth metal or a compound thereof or a complex thereof may be provided. The electron injection layer 115 may use a layer or an electron compound (electride) in which an alkali metal, alkaline earth metal or a compound thereof is contained in a layer composed of a substance having electron transport properties. As the electron compound, for example, a substance in which electrons are added to a mixed oxide of calcium and aluminum at a high concentration may be cited.
[0139] Note that a layer containing a fluoride of an alkali metal or alkaline earth metal in a microcrystalline state at a concentration of 50 wt % or more may be used as the electron injection layer 115. Since this layer has a low refractive index, a light-emitting device with better external quantum efficiency can be provided.
[0140] The second electrode 102 is an electrode including a cathode. The second electrode 102 may also have a laminated structure, in which case the layer in contact with the organic compound layer 103 is used as a cathode. As a material forming the cathode, metals, alloys, conductive compounds, and mixtures thereof with a small work function (specifically less than 3.8 eV) may be used. As specific examples of such cathode materials, elements belonging to Group 1 or Group 2 in the periodic table, alloys containing them (MgAg, AlLi), europium (Eu), rare earth metals such as ytterbium (Yb), and alloys containing them may be cited. However, by providing an electron injection layer between the second electrode 102 and the electron transport layer, various conductive materials such as Al, Ag, ITO, indium oxide-tin oxide containing silicon or silicon oxide, etc. may be used as cathodes regardless of the size of the work function.
[0141] In the case where the second electrode 102 is formed of a material having a property of transmitting visible light, a light-emitting device that emits light from the second electrode 102 side can be formed.
[0142] These conductive materials can be deposited by a dry method such as vacuum evaporation or sputtering, an inkjet method, a spin coating method, etc. Alternatively, they can be formed by a wet method such as a sol-gel method or a wet method using a paste of a metal material.
[0143] The organic compound layer 103 can be formed by any of a variety of methods, whether dry or wet. For example, vacuum deposition, gravure printing, offset printing, screen printing, inkjet printing, or spin coating can be used.
[0144] In addition, the above-mentioned electrodes or layers may also be formed by using different deposition methods.
[0145] This embodiment mode can be combined with other embodiment modes or examples as appropriate. In addition, in this specification, when a plurality of configuration examples are shown in one embodiment mode, the configuration examples can be combined as appropriate.
[0146] (Implementation method 3) like Fig. 6A and Figure 6B As shown in FIG. 1 , a plurality of light emitting devices 130 are formed on an insulating layer 175 to form a display device. In this embodiment, a display device according to one embodiment of the present invention is described in detail.
[0147] The display device 100 includes a pixel portion 177 in which a plurality of pixels 178 are arranged in a matrix. The pixel 178 includes a sub-pixel 110R, a sub-pixel 110G, and a sub-pixel 110B.
[0148] In this specification, for example, the sub-pixel 110 may be used to describe the common contents among the sub-pixel 110R, the sub-pixel 110G, and the sub-pixel 110B. In addition, for other components distinguished by letters, reference numerals without letters may be used to describe the common contents among the components.
[0149] Sub-pixel 110R presents red light, sub-pixel 110G presents green light, and sub-pixel 110B presents blue light. Thus, an image can be displayed on the pixel portion 177. Note that in this embodiment, sub-pixels of three colors, red (R), green (G), and blue (B), are used as examples for explanation, and sub-pixels of other colors may also be combined. In addition, the number of sub-pixels is not limited to three, but may be four or more. As four sub-pixels, for example, there may be: sub-pixels of four colors, R, G, B, and white (W); sub-pixels of four colors, R, G, B, and Y; and sub-pixels of four colors, R, G, B, and infrared light (IR); and the like.
[0150] In this specification and the like, the row direction may be referred to as the X direction and the column direction may be referred to as the Y direction. The X direction and the Y direction intersect, for example, perpendicularly intersect.
[0151] exist Fig. 6A In the example shown, sub-pixels of different colors are arranged in the X direction, and sub-pixels of the same color are arranged in the Y direction. Note that sub-pixels of different colors may be arranged in the Y direction, and sub-pixels of the same color may be arranged in the X direction.
[0152] The connection portion 140 and the region 141 may be provided outside the pixel portion 177. For example, the region 141 is provided between the pixel portion 177 and the connection portion 140. The organic compound layer 103 is provided in the region 141. In addition, the connection portion 140 is provided with the conductive layer 151C.
[0153] exist Fig. 6A In the example shown, the connection portion 140 and the region 141 are located on the right side of the pixel portion 177, but there is no particular limitation on the positions of the connection portion 140 and the region 141. In addition, the connection portion 140 and the region 141 may be one or more.
[0154] Figure 6B is along Fig. 6A An example of a cross-sectional view along the dot-dash line A1-A2 in FIG. Figure 6BAs shown, the display device 100 includes an insulating layer 171, a conductive layer 172 on the insulating layer 171, an insulating layer 173 on the insulating layer 171 and the conductive layer 172, an insulating layer 174 on the insulating layer 173, and an insulating layer 175 on the insulating layer 174. The insulating layer 171 is disposed on a substrate (not shown). The insulating layer 175, the insulating layer 174, and the insulating layer 173 are provided with openings that reach the conductive layer 172, and a plug 176 is provided in a manner of being embedded in the opening.
[0155] In the pixel portion 177, the light emitting device 130 is provided on the insulating layer 175 and the plug 176. The protective layer 131 is provided so as to cover the light emitting device 130. The substrate 120 is bonded to the protective layer 131 via the resin layer 122. In addition, the inorganic insulating layer 125 and the insulating layer 127 on the inorganic insulating layer 125 are preferably provided between adjacent light emitting devices 130.
[0156] Figure 6B Although the cross sections of the plurality of inorganic insulating layers 125 and the plurality of insulating layers 127 are shown, the inorganic insulating layers 125 and the insulating layers 127 are preferably formed as a continuous layer in a plan view of the display device 100. That is, the insulating layer 127 is preferably an insulating layer having an opening on the first electrode.
[0157] Figure 6B As the light emitting device 130, a light emitting device 130R, a light emitting device 130G, and a light emitting device 130B are shown. The light emitting device 130R, the light emitting device 130G, and the light emitting device 130B emit light of different colors. For example, the light emitting device 130R may emit red light, the light emitting device 130G may emit green light, and the light emitting device 130B may emit blue light. In addition, the light emitting device 130R, the light emitting device 130G, or the light emitting device 130B may also emit other visible light or infrared light.
[0158] The display device of one embodiment of the present invention may have, for example, a top emission structure that emits light in a direction opposite to a substrate on which a light-emitting device is formed. Alternatively, the display device of one embodiment of the present invention may have a bottom emission structure.
[0159] Examples of the light-emitting material contained in the light-emitting device 130 include organic compounds or organometallic complexes such as materials that emit fluorescence (fluorescent materials), materials that emit phosphorescence (phosphorescent materials), and materials that exhibit thermally activated delayed fluorescence (TADF materials). Inorganic compounds such as quantum dots may also be used.
[0160] The light-emitting device 130R has the structure shown in Embodiment 1, and includes a first electrode (pixel electrode) composed of a conductive layer 151R and a conductive layer 152R, an organic compound layer 103R on the first electrode, a common layer 104 on the organic compound layer 103R, and a second electrode (common electrode) 102 on the common layer 104. The common layer 104 may or may not be provided, but when the common layer 104 is provided, damage to the organic compound layer 103R during processing can be reduced, so it is preferred. When the common layer 104 is provided, the common layer 104 is preferably an electron injection layer. In addition, when the common layer 104 is provided, the stacked structure of the organic compound layer 103R and the common layer 104 is equivalent to the organic compound layer 103 in Embodiment 1.
[0161] The light-emitting device 130G has a structure as described in Embodiment 1, including a first electrode (pixel electrode) composed of a conductive layer 151G and a conductive layer 152G, an organic compound layer 103G on the first electrode, a common layer 104 on the organic compound layer 103G, and a second electrode (common electrode) 102 on the common layer 104. The common layer 104 may or may not be provided, but when the common layer 104 is provided, damage to the organic compound layer 103G during processing can be reduced, so it is preferred. When the common layer 104 is provided, the common layer 104 is preferably an electron injection layer. In addition, when the common layer 104 is provided, the stacked structure of the organic compound layer 103G and the common layer 104 is equivalent to the organic compound layer 103 in Embodiment 1.
[0162] The light-emitting device 130B has a structure as described in Embodiment 1, including a first electrode (pixel electrode) composed of a conductive layer 151B and a conductive layer 152B, an organic compound layer 103B on the first electrode, a common layer 104 on the organic compound layer 103B, and a second electrode (common electrode) 102 on the common layer 104. The common layer 104 may or may not be provided, but when the common layer 104 is provided, damage to the organic compound layer 103B during processing can be reduced, so it is preferred. When the common layer 104 is provided, the common layer 104 is preferably an electron injection layer. In addition, when the common layer 104 is provided, the stacked structure of the organic compound layer 103B and the common layer 104 is equivalent to the organic compound layer 103 in Embodiment 1.
[0163] One of the pixel electrode and the common electrode included in the light emitting device is used as an anode, and the other is used as a cathode. Unless otherwise specified, the following description is based on the premise that the pixel electrode is used as an anode and the common electrode is used as a cathode.
[0164] The organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B are each formed in an island shape or independently for each light-emitting color. By providing the organic compound layer 103 in an island shape for each light-emitting device 130, leakage current between adjacent light-emitting devices 130 can be suppressed in a high-definition display device. As a result, crosstalk can be suppressed, and a light-emitting device with extremely high contrast can be realized. In particular, a display device with high current efficiency at low brightness can be realized.
[0165] The island-shaped organic compound layer 103 is formed by depositing an EL film and processing the EL film using a photolithography method.
[0166] The organic compound layer 103 is preferably provided in a manner covering the top surface and the side surface of the first electrode (pixel electrode) of the light-emitting device 130. Thus, it is easier to increase the aperture ratio of the display device 100 than in a structure in which the end of the organic compound layer 103 is located on the inner side of the end of the pixel electrode. In addition, by covering the side surface of the pixel electrode of the light-emitting device 130 with the organic compound layer 103, it is possible to suppress the contact between the pixel electrode and the second electrode 102, thereby suppressing the short circuit of the light-emitting device 130. In addition, the distance between the light-emitting region of the organic compound layer 103 (i.e., the region overlapping with the pixel electrode) and the end of the organic compound layer 103 can be increased. In addition, since the end of the organic compound layer 103 may be damaged by processing, by using the region away from the end of the organic compound layer 103 as the light-emitting region, the reliability of the light-emitting device 130 can be improved.
[0167] In the display device of one embodiment of the present invention, the first electrode (pixel electrode) of the light-emitting device preferably has a stacked structure. Figure 6B In the example shown, the first electrode of the light-emitting device 130 has a stacked structure of a conductive layer 151 and a conductive layer 152. For example, when the display device 100 has a top emission structure and the pixel electrode of the light-emitting device 130 is used as an anode, it is preferred that the conductive layer 151 is a layer with a high visible light reflectivity, and the conductive layer 152 is, for example, a layer with visible light transmittance and a large work function. When the display device 100 has a top emission structure, the higher the visible light reflectivity of the pixel electrode, the higher the light extraction efficiency emitted by the organic compound layer 103 can be improved. In addition, when the pixel electrode is used as an anode, the larger the work function of the pixel electrode, the easier it is to inject holes into the organic compound layer 103. Thus, by having the pixel electrode of the light-emitting device 130 have a stacked structure of a conductive layer 151 with a high visible light reflectivity and a conductive layer 152 with a large work function, the light-emitting device 130 can be a light-emitting element with high light extraction efficiency and low driving voltage.
[0168] When the conductive layer 151 is a layer having a high visible light reflectivity, the visible light reflectivity of the conductive layer 151 is preferably, for example, 40% to 100%, more preferably 70% to 100%. When the conductive layer 152 is an electrode having visible light transmittance, the visible light transmittance is preferably, for example, 40% or more.
[0169] Here, when the pixel electrode has a multi-layer stacked structure, the pixel electrode is degraded by, for example, a reaction between the multiple layers. For example, when a film formed after forming the pixel electrode is removed by wet etching, galvanic corrosion occurs due to the contact of a chemical solution with the pixel electrode.
[0170] In view of this, in the display device 100 of the present embodiment, the conductive layer 152 is formed in a manner covering the top surface and the side surface of the conductive layer 151. Thus, for example, when a film formed after forming a pixel electrode including the conductive layer 151 and the conductive layer 152 is removed by a wet etching method, it is also possible to suppress the contact of the chemical solution with the conductive layer 151. Therefore, for example, galvanic corrosion can be suppressed in the pixel electrode. Therefore, the display device 100 can be manufactured by a method with a high yield rate, so that an inexpensive display device can be realized. In addition, it is possible to suppress the occurrence of defects in the display device 100, so the display device 100 can be a display device with high reliability.
[0171] For example, a metal material can be used as the conductive layer 151. Specifically, for example, metals such as aluminum (Al), titanium (Ti), chromium (Cr), manganese (Mn), iron (Fe), cobalt (Co), nickel (Ni), copper (Cu), gallium (Ga), zinc (Zn), indium (In), tin (Sn), molybdenum (Mo), tantalum (Ta), tungsten (W), palladium (Pd), gold (Au), platinum (Pt), silver (Ag), yttrium (Y), neodymium (Nd), and alloys obtained by appropriately combining these metals can be used.
[0172] As the conductive layer 152, an oxide containing any one or more selected from indium, tin, zinc, gallium, titanium, aluminum, and silicon can be used. For example, a conductive oxide containing any one or more of indium oxide, indium tin oxide, indium zinc oxide, zinc oxide, zinc oxide containing gallium, titanium oxide, indium zinc oxide containing gallium, indium zinc oxide containing aluminum, indium tin oxide containing silicon, and indium zinc oxide containing silicon is preferably used. In particular, indium tin oxide containing silicon has a large work function, for example, 4.0 eV or more, and can be preferably used as the conductive layer 152.
[0173] Each of the conductive layer 151 and the conductive layer 152 may have a stacked-layer structure including a plurality of layers of different materials. In this case, the conductive layer 151 may include a layer using a material that can be used for the conductive layer 152, such as a conductive oxide, and the conductive layer 152 may include a layer using a material that can be used for the conductive layer 151, such as a metal material. For example, when the conductive layer 151 has a stacked-layer structure of two or more layers, the layer in contact with the conductive layer 152 may be a layer using a material that can be used for the conductive layer 152.
[0174] The side surface of the conductive layer 151 preferably has a tapered shape. Specifically, the side surface of the conductive layer 151 preferably has a tapered shape with a taper angle of less than 90°. In this case, the conductive layer 152 provided along the side surface of the conductive layer 151 also has a tapered shape. By making the side surface of the conductive layer 152 have a tapered shape, the coverage of the organic compound layer 103 provided along the side surface of the conductive layer 152 can be improved.
[0175] Fig. 7A 1 is a diagram when the conductive layer 151 has a stacked structure of a plurality of layers including different materials. Fig. 7A As shown, the conductive layer 151 includes a conductive layer 151a, a conductive layer 151b on the conductive layer 151a, and a conductive layer 151c on the conductive layer 151b. That is, Fig. 7A The conductive layer 151 shown has a three-layer stacked structure. In this way, when the conductive layer 151 has a multi-layer stacked structure, the visible light reflectance of at least one of the layers constituting the conductive layer 151 may be higher than the visible light reflectance of the conductive layer 152 .
[0176] exist Fig. 7A In the example shown, the conductive layer 151b is sandwiched between the conductive layer 151a and the conductive layer 151c. The conductive layer 151a and the conductive layer 151c can use a material that is less likely to deteriorate than the conductive layer 151b. For example, the conductive layer 151a can use a material that is less likely to migrate due to contact with the insulating layer 175 than the conductive layer 151b. In addition, the conductive layer 151c can use a material that is less likely to be oxidized than the conductive layer 151b and whose oxide has a lower resistivity than the oxide of the material used for the conductive layer 151b.
[0177] In this way, by adopting a structure in which the conductive layer 151b is sandwiched between the conductive layer 151a and the conductive layer 151c, the range of choices for the material of the conductive layer 151b can be expanded. Thus, for example, the conductive layer 151b can be made into a layer whose visible light reflectance is higher than that of at least one of the conductive layer 151a and the conductive layer 151c. For example, aluminum can be used as the conductive layer 151b. In addition, an alloy containing aluminum can also be used as the conductive layer 151b. In addition, titanium can be used as the conductive layer 151a. Although titanium has a lower visible light reflectance than aluminum, it is less likely to migrate than aluminum even when it contacts the insulating layer 175. In addition, titanium can be used as the conductive layer 151c. Although titanium has a lower visible light reflectance than aluminum, it is less likely to be oxidized than aluminum and the resistivity of oxide is lower than that of aluminum oxide.
[0178] In addition, silver or an alloy containing silver may be used as the conductive layer 151c. Silver has the characteristic of having a higher visible light reflectivity than titanium. Furthermore, silver is less easily oxidized than aluminum, and the resistivity of silver oxide is lower than that of aluminum oxide. Therefore, when silver or an alloy containing silver is used as the conductive layer 151c, the visible light reflectivity of the conductive layer 151 can be appropriately improved while suppressing the increase in resistance of the pixel electrode caused by the oxidation of the conductive layer 151b. Here, as the silver-containing alloy, for example, an alloy of silver, palladium and copper (Ag-Pd-Cu, also referred to as APC) can be used. In addition, when silver or an alloy containing silver is used as the conductive layer 151c and aluminum is used as the conductive layer 151b, the visible light reflectivity of the conductive layer 151c can be improved compared to the visible light reflectivity of the conductive layer 151b. Here, silver or an alloy containing silver may also be used as the conductive layer 151b. In addition, silver or an alloy containing silver may also be used as the conductive layer 151a.
[0179] On the other hand, a film made of titanium has better etching processability than a film made of silver. Therefore, by using titanium as the conductive layer 151c, the conductive layer 151c can be easily formed. In addition, a film made of aluminum also has better etching processability than a film made of silver.
[0180] By making the conductive layer 151 have a stacked structure of a plurality of layers in this manner, the characteristics of the display device can be improved. For example, the display device 100 can be made to have high light extraction efficiency and high reliability.
[0181] Here, when the light emitting device 130 adopts a microcavity structure, by using silver or an alloy containing silver, which is a material with high visible light reflectivity, as the conductive layer 151 c , the light extraction efficiency of the display device 100 can be appropriately improved.
[0182] As described above, the side surface of the conductive layer 151 preferably has a tapered shape. Specifically, the side surface of the conductive layer 151 preferably has a tapered shape with a taper angle less than 90°. Fig. 7A In the conductive layer 151 of the structure shown, it is preferable that a side surface of at least one of the conductive layer 151a, the conductive layer 151b, and the conductive layer 151c has a tapered shape.
[0183] Fig. 7A The conductive layer 151 shown can be formed by photolithography. Specifically, first, a conductive film to become the conductive layer 151a, a conductive film to become the conductive layer 151b, and a conductive film to become the conductive layer 151c are deposited in sequence. Next, a resist mask is formed on the conductive film to become the conductive layer 151c. Then, the conductive film in the area that does not overlap with the resist mask is removed, for example, by etching. Here, by processing the conductive film under conditions in which the resist mask is easier to retreat (shrink) than in the case where the conductive layer 151 is formed in a manner in which the side does not have a tapered shape (i.e., the side is vertical), a conductive layer 151 having a tapered shape on the side can be formed.
[0184] Here, when the conductive film is processed under the condition that the resist mask easily retreats (shrinks), the conductive film may be easily processed in the horizontal direction. In other words, the isotropy of etching may become higher than when the conductive layer 151 is formed so that the side surface is vertical.
[0185] When the conductive layer 151 has a stacked structure of a plurality of layers made of different materials, the plurality of layers may have different eases of processing in the horizontal direction. For example, the conductive layer 151a, the conductive layer 151b, and the conductive layer 151c may have different eases of processing in the horizontal direction.
[0186] In this case, sometimes after processing the conductive film, Fig. 7A As shown, the side surface of the conductive layer 151b is located inside the side surfaces of the conductive layer 151a and the conductive layer 151c to form a protrusion. This may reduce the coverage of the conductive layer 152 with respect to the conductive layer 151 and cause disconnection of the conductive layer 152.
[0187] In view of this, it is preferred Fig. 7A The insulating layer 156 is provided in this manner. Fig. 7A An example is shown in which insulating layer 156 is provided on conductive layer 151a so as to have a region overlapping with the side surface of conductive layer 151b. This can suppress disconnection or thinning of conductive layer 152 due to the protrusion, thereby suppressing poor connection and increase in driving voltage.
[0188] Note that although Fig. 7AAlthough the structure in which the entire side surface of the conductive layer 151b is covered by the insulating layer 156 is shown, a part of the side surface of the conductive layer 151b may not be covered by the insulating layer 156. Similarly, in the pixel electrode having the structure shown below, a part of the side surface of the conductive layer 151b may not be covered by the insulating layer 156.
[0189] The conductive layer 151 has Fig. 7A In the structure shown in the figure, the conductive layer 152 covers the conductive layer 151a, the conductive layer 151b, the conductive layer 151c and the insulating layer 156 and is electrically connected to the conductive layer 151a, the conductive layer 151b and the conductive layer 151c. Therefore, when removing a film deposited after the conductive layer 152 is formed by a wet etching method, for example, the chemical solution does not need to contact the conductive layer 151a, the conductive layer 151b and the conductive layer 151c. Therefore, corrosion in the conductive layer 151a, the conductive layer 151b and the conductive layer 151c can be suppressed. Therefore, the display device 100 can be manufactured by a method with a high yield. In addition, the occurrence of defects can be suppressed, thereby realizing a display device 100 with high reliability.
[0190] Here, if Fig. 7A As shown, the insulating layer 156 preferably has a curved surface. Thus, for example, compared with a case where the side surface of the insulating layer 156 is perpendicular (parallel to the Z direction), the occurrence of disconnection in the conductive layer 152 covering the insulating layer 156 can be suppressed. In addition, when the side surface of the insulating layer 156 has a tapered shape, specifically a tapered shape with a taper angle of less than 90°, for example, compared with a case where the side surface of the insulating layer 156 is perpendicular, the occurrence of disconnection in the conductive layer 152 covering the insulating layer 156 can be suppressed. Thus, the display device 100 can be manufactured by a method with a high yield. In addition, the occurrence of defects is suppressed, and the display device 100 can be made into a display device with high reliability.
[0191] Notice, Fig. 7A Although the structure in which the side surface of the conductive layer 151b is located inside the side surface of the conductive layer 151a and the side surface of the conductive layer 151c is shown, one embodiment of the present invention is not limited to this. For example, the side surface of the conductive layer 151b may be located outside the side surface of the conductive layer 151a. In addition, the side surface of the conductive layer 151b may be located outside the side surface of the conductive layer 151c.
[0192] FIG. 7B to FIG. 7D Other structures of the first electrode 101 are shown. Figure 7B 1 shows a structure in which the insulating layer 156 covers the side surfaces of the conductive layer 151a, the conductive layer 151b, and the conductive layer 151c in addition to the side surface of the conductive layer 151b in the first electrode 101 of FIG.
[0193] Figure 7CThe structure in which the insulating layer 156 is not provided in the first electrode 101 of FIG. 1 is shown.
[0194] Fig.7D The following structure is shown: in the first electrode 101 of FIG. 1 , the conductive layer 151 does not have a stacked-layer structure and the conductive layer 152 has a stacked-layer structure.
[0195] The conductive layer 152a is a layer having a higher adhesion to the conductive layer 152b than the insulating layer 175, for example. As the conductive layer 152a, for example, an oxide containing any one or more selected from indium, tin, zinc, gallium, titanium, aluminum, and silicon can be used. For example, it is preferable to use a conductive oxide containing any one or more of indium oxide, indium tin oxide, indium zinc oxide, zinc oxide, zinc oxide containing gallium, titanium oxide, indium titanium oxide, zinc titanate, aluminum zinc oxide, indium zinc oxide containing gallium, indium zinc oxide containing aluminum, indium tin oxide containing silicon, and indium zinc oxide containing silicon. Thus, film peeling of the conductive layer 152b can be suppressed. In addition, the conductive layer 152b can be prevented from contacting the insulating layer 175.
[0196] The conductive layer 152b is a layer with a higher visible light reflectivity (for example, reflectivity for light of a specified wavelength in the range of 400 nm to less than 750 nm) than the conductive layer 151, the conductive layer 152a, and the conductive layer 152c. The visible light reflectivity of the conductive layer 152b can be, for example, 70% to 100%, preferably 80% to 100%, and more preferably 90% to 100%. In addition, as the conductive layer 152b, for example, a material having a higher visible light reflectivity than aluminum can be used. Specifically, for example, silver or an alloy containing silver can be used as the conductive layer 152b. As an example of an alloy containing silver, an alloy of silver, palladium, and copper (APC) can be cited. As a result, the display device 100 can be made into a display device with high light extraction efficiency. Note that a metal other than silver can also be used as the conductive layer 152b.
[0197] When the conductive layer 151 and the conductive layer 152 are used as an anode, the conductive layer 152c is preferably a layer having a large work function. The conductive layer 152c is, for example, a layer having a larger work function than the conductive layer 152b. As the conductive layer 152c, for example, the same material as that which can be used for the conductive layer 152a can be used. For example, the same material can be used for the conductive layer 152a and the conductive layer 152c. For example, when indium tin oxide is used for the conductive layer 152a, indium tin oxide can also be used for the conductive layer 152c.
[0198] Note that when the conductive layer 151 and the conductive layer 152 are used as a cathode, the conductive layer 152c is preferably a layer with a small work function. For example, the conductive layer 152c is a layer with a smaller work function than the conductive layer 152b.
[0199] In addition, the conductive layer 152c is preferably a layer with high visible light transmittance (for example, transmittance to light of a specified wavelength in the range of greater than 400 nm and less than 750 nm). For example, the visible light transmittance of the conductive layer 152c is preferably higher than the visible light transmittance of the conductive layer 151 and the conductive layer 152b. For example, the visible light transmittance of the conductive layer 152c can be greater than 60% and less than 100%, preferably greater than 70% and less than 100%, and more preferably greater than 80% and less than 100%. Thereby, the light absorbed by the conductive layer 152c in the light emitted by the organic compound layer 103 can be reduced. In addition, as described above, the conductive layer 152b under the conductive layer 152c can be a layer with high visible light reflectance. Therefore, the display device 100 can be made into a display device with high light extraction efficiency.
[0200] Next, the method having the Fig. 6A An example of a method for manufacturing the display device 100 having the structure shown is shown.
[0201] [Manufacturing method example] The thin film (insulating film, semiconductor film, conductive film, etc.) constituting the display device can be formed by sputtering, chemical vapor deposition (CVD: Chemical Vapor Deposition) method, vacuum evaporation method, pulsed laser deposition (PLD: Pulsed Laser Deposition) method or atomic layer deposition (ALD: Atomic Layer Deposition) method, etc. As CVD methods, there are plasma enhanced chemical vapor deposition (PECVD: Plasma Enhanced CVD) method and thermal CVD method, etc. In addition, as one of the thermal CVD methods, there is metal organic chemical vapor deposition (MOCVD: Metal Organic CVD) method.
[0202] In addition, thin films (insulating films, semiconductor films, conductive films, etc.) that constitute the display device can be formed using a wet deposition method such as spin coating, dipping, spraying, inkjet, dispenser, screen printing, offset printing, doctor knife, slit coating, roll coating, curtain coating or doctor knife coating.
[0203] In particular, when manufacturing a light-emitting device, a vacuum process such as evaporation and a solution process such as spin coating and inkjet can be used. As an evaporation method, physical evaporation methods (PVD methods) such as sputtering, ion plating, ion beam evaporation, molecular beam evaporation, vacuum evaporation, and chemical vapor deposition (CVD methods) can be cited. In particular, the functional layer (hole injection layer, hole transport layer, hole blocking layer, light-emitting layer, electron blocking layer, electron transport layer, and electron injection layer, etc.) included in the organic compound layer can be formed by methods such as evaporation (vacuum evaporation, etc.), coating (dip coating, dye coating, rod coating, spin coating, spray coating), printing (inkjet, screen printing (porcelain printing), offset printing (lithography), flexographic printing (relief printing), gravure printing, or micro-contact printing, etc.).
[0204] In addition, when processing the thin film constituting the display device, for example, photolithography can be used for processing. Alternatively, the thin film can also be processed by nanoimprinting, sandblasting, lift-off, etc. In addition, an island-shaped thin film can also be directly formed by a deposition method using a shielding mask such as a metal mask.
[0205] There are two typical methods of photolithography. One is to form a resist mask on a thin film to be processed, process the thin film by etching, and then remove the resist mask. The other is to form a photosensitive thin film, then expose and develop it, and process the thin film into a desired shape.
[0206] In the photolithography method, as the light used for exposure, for example, i-line (wavelength of 365nm), g-line (wavelength of 436nm), h-line (wavelength of 405nm) or a mixture of these lights can be used. In addition, ultraviolet rays, KrF lasers or ArF lasers can also be used. In addition, liquid immersion exposure technology can also be used for exposure. In addition, as the light used for exposure, extreme ultraviolet (EUV: Extreme Ultra-Violet) light or X-rays can also be used. In addition, instead of the light used for exposure, an electron beam can also be used. When extreme ultraviolet light, X-rays or electron beams are used, extremely fine processing can be performed, so it is preferred. In addition, when exposure is performed by scanning a light beam such as an electron beam, a photomask is not required.
[0207] For etching of the thin film, dry etching, wet etching, sand blasting, or the like can be used.
[0208] First, if Fig. 8AAs shown, an insulating layer 171 is formed on a substrate (not shown). Then, a conductive layer 172 and a conductive layer 179 are formed on the insulating layer 171, and an insulating layer 173 is formed on the insulating layer 171 to cover the conductive layer 172 and the conductive layer 179. Then, an insulating layer 174 is formed on the insulating layer 173, and an insulating layer 175 is formed on the insulating layer 174.
[0209] As the substrate, a substrate having heat resistance at least enough to withstand the subsequent heat treatment can be used. In the case of using an insulating substrate as the substrate, a glass substrate, a quartz substrate, a sapphire substrate, a ceramic substrate, or an organic resin substrate can be used. In addition, a semiconductor substrate such as a single crystal semiconductor substrate or a polycrystalline semiconductor substrate made of silicon or silicon carbide, a compound semiconductor substrate made of silicon germanium, or an SOI substrate can also be used.
[0210] Then, if Fig. 8A As shown in FIG. 1 , openings reaching the conductive layer 172 are formed in the insulating layer 175, the insulating layer 174, and the insulating layer 173. Next, the plug 176 is formed so as to be embedded in the opening.
[0211] Then, if Fig. 8A As shown, a conductive film 151f, which will later become the conductive layer 151R, the conductive layer 151G, the conductive layer 151B, and the conductive layer 151C, is formed on the plug 176 and the insulating layer 175. The conductive film 151f can be formed by, for example, sputtering or vacuum deposition. In addition, as the conductive film 151f, for example, a metal material can be used.
[0212] Then, if Fig. 8A As shown in FIG. 1 , a resist mask 191 is formed on the conductive film 151f. The resist mask 191 can be formed by applying a photosensitive material (photoresist), exposing it to light, and developing it.
[0213] Then, if Figure 8B As shown, for example, the conductive film 151f in the region that does not overlap with the resist mask 191 is removed by etching, specifically, by dry etching. Note that when the conductive film 151f includes a layer made of a conductive oxide such as indium tin oxide, the layer may be removed by wet etching. Thus, the conductive layer 151 is formed. Note that, for example, when a portion of the conductive film 151f is removed by dry etching, a recessed portion may be formed in a region of the insulating layer 175 that does not overlap with the conductive layer 151.
[0214] Then, if Figure 8CAs shown, the resist mask 191 is removed. The resist mask 191 can be removed, for example, by ashing using oxygen plasma. Alternatively, oxygen gas and CF4, C4F8, SF6, CHF3, Cl2, H2O, BCl3 or Group 18 elements such as He can also be used. Alternatively, the resist mask 191 can also be removed by wet etching.
[0215] Then, if Fig.8D As shown in FIG. 1 , an insulating film 156f, which will later become insulating layers 156R, 156G, 156B, and 156C, is formed on the conductive layers 151R, 151G, 151B, 151C, and the insulating layer 175. The insulating film 156f can be formed by, for example, CVD, ALD, sputtering, or vacuum evaporation.
[0216] The insulating film 156f may be made of an inorganic material. As the insulating film 156f, for example, an inorganic insulating film such as an oxide insulating film, a nitride insulating film, an oxynitride insulating film, or a nitride oxide insulating film may be used. For example, as the insulating film 156f, an oxide insulating film, a nitride insulating film, an oxynitride insulating film, or a nitride oxide insulating film containing silicon may be used. For example, as the insulating film 156f, silicon oxynitride may be used.
[0217] Then, if Fig. 8E As shown, the insulating film 156f is processed to form the insulating layer 156R, the insulating layer 156G, the insulating layer 156B, and the insulating layer 156C. For example, the top surface of the insulating film 156f is etched roughly uniformly, thereby forming the insulating layer 156. Such a process of etching uniformly to flatten is also called an etch-back process. Alternatively, the insulating layer 156 may be formed by photolithography.
[0218] Then, if Fig. 9A As shown in FIG. 1 , a conductive film 152f, which will later become the conductive layer 152R, the conductive layer 152G, the conductive layer 152B, and the conductive layer 152C, is formed on the conductive layer 151R, the conductive layer 151G, the conductive layer 151B, the conductive layer 151C, the insulating layer 156R, the insulating layer 156G, the insulating layer 156B, the insulating layer 156C, and the insulating layer 175. Specifically, for example, the conductive film 152f is formed so as to cover the conductive layer 151R, the conductive layer 151G, the conductive layer 151B, the conductive layer 151C, the insulating layer 156R, the insulating layer 156G, the insulating layer 156B, and the insulating layer 156C.
[0219] The conductive film 152f can be formed by, for example, a sputtering method or a vacuum evaporation method. In addition, as the conductive film 152f, for example, a conductive oxide can be used. Alternatively, as the conductive film 152f, a laminated structure of a film using a metal material and a film using a conductive oxide on the film can be used. For example, as the conductive film 152f, a laminated structure of a film using titanium, silver, or an alloy containing silver and a film using a conductive oxide on the film can be used.
[0220] In addition, the conductive film 152f can be formed using the ALD method. Here, as the conductive film 152f, an oxide containing any one or more selected from indium, tin, zinc, gallium, titanium, aluminum and silicon can be used. At this time, by introducing a precursor (generally sometimes referred to as a precursor or a metal precursor, etc.), purging the precursor, introducing an oxidant (generally sometimes referred to as a reactant, reactant or non-metal precursor, etc.) and purging the oxidant as one cycle, the conductive film 152f can be formed by repeating the cycle. Here, when an oxide film containing multiple metals such as indium tin oxide is formed as the conductive film 152f, the metal composition can be controlled by changing the number of cycles according to the type of precursor.
[0221] For example, when an indium tin oxide film is deposited as the conductive film 152f, an In-O film is formed by introducing a precursor containing indium, purging the precursor, and introducing an oxidant, and then a Sn-O film is formed by introducing a precursor containing tin, purging the precursor, and introducing an oxidant. Here, by making the number of cycles when forming the In-O film greater than the number of cycles when forming the Sn-O film, the number of In atoms contained in the conductive film 152f can be greater than the number of Sn atoms.
[0222] In addition, for example, in the case where a zinc oxide film is deposited as the conductive film 152f, a Zn-O film is formed by the above process. In addition, for example, in the case where an aluminum zinc oxide film is deposited as the conductive film 152f, a Zn-O film and an Al-O film are formed by the above process. In addition, for example, in the case where a titanium oxide film is deposited as the conductive film 152f, a Ti-O film is formed by the above process. In addition, for example, in the case where an indium tin oxide film containing silicon is deposited as the conductive film 152f, an In-O film, a Sn-O film, and a Si-O film are formed by the above process. In addition, for example, in the case where a zinc oxide film containing gallium is deposited, a Ga-O film and a Zn-O film are formed by the above process.
[0223] As a precursor containing indium, for example, triethylindium, trimethylindium or [1,1,1-trimethyl-N-(trimethylsilyl)amide]-indium can be used. As a precursor containing tin, for example, tin chloride or tetrakis(dimethylamide)tin can be used. As a precursor containing zinc, for example, diethylzinc or dimethylzinc can be used. As a precursor containing gallium, for example, triethylgallium can be used. As a precursor containing titanium, for example, titanium chloride, tetrakis(dimethylamide)titanium or tetraisopropyl titanate can be used. As a precursor containing aluminum, for example, aluminum chloride or trimethylaluminum can be used. As a precursor containing silicon, for example, trisilylamine, bis(diethylamino)silane, tris(dimethylamino)silane, bis(tert-butylamino)silane or bis(ethylmethylamino)silane can be used. In addition, as an oxidant, water vapor, oxygen plasma or ozone gas can be used.
[0224] Then, if Fig. 9B As shown in the figure, the conductive film 152f is processed by, for example, photolithography, thereby forming the conductive layer 152R, the conductive layer 152G, the conductive layer 152B, and the conductive layer 152C. Specifically, for example, after forming a resist mask, a portion of the conductive film 152f is removed by etching. For example, the conductive film 152f can be removed by wet etching. Note that the conductive film 152f can also be removed by dry etching. Thus, the pixel electrode including the conductive layer 151 and the conductive layer 152 is formed.
[0225] Next, the conductive layer 152 is preferably subjected to a hydrophobic treatment. Through the hydrophobic treatment, the surface state of the treatment object can be changed from hydrophilic to hydrophobic, or the hydrophobicity of the surface of the treatment object can be improved. By performing the hydrophobic treatment on the conductive layer 152, the adhesion between the conductive layer 152 and the organic compound layer 103 to be formed in the subsequent process can be improved to suppress film peeling. Note that the hydrophobic treatment may not be performed.
[0226] Then, if Fig. 9C As shown in FIG. 1 , an organic compound film 103Rf which will later become the organic compound layer 103R is formed over the conductive layer 152R, the conductive layer 152G, the conductive layer 152B, and the insulating layer 175 .
[0227] like Fig. 9C As shown, the organic compound film 103Rf is not formed on the conductive layer 152C. For example, by using a mask for defining a deposition range (also referred to as an area mask or a rough metal mask, etc., to distinguish it from a high-definition metal mask), the organic compound film 103Rf can be deposited only in a desired area. By adopting a deposition process using an area mask and a processing process using a resist mask, a light-emitting device can be manufactured with a relatively simple process.
[0228] The organic compound film 103Rf can be formed by, for example, a vapor deposition method, specifically, a vacuum vapor deposition method. Alternatively, the organic compound film 103Rf can be formed by a transfer method, a printing method, an inkjet method, a coating method, or the like.
[0229] Then, if Fig. 9C As shown in FIG. 1 , a sacrificial film 158Rf which will later become a sacrificial layer 158R and a mask film 159Rf which will later become a mask layer 159R are sequentially formed on the organic compound film 103Rf, the conductive layer 152C, and the insulating layer 175 .
[0230] Note that in this embodiment, an example is shown in which the mask film has a two-layer structure of the sacrificial film 158Rf and the mask film 159Rf, but the mask film may have a single-layer structure or a stacked-layer structure of three or more layers.
[0231] By providing a sacrificial layer on the organic compound film 103Rf, damage to the organic compound film 103Rf during the manufacturing process of the display device can be reduced, and the reliability of the light-emitting device can be improved.
[0232] The sacrificial film 158Rf is a film having high resistance to the processing conditions of the organic compound film 103Rf, specifically, a film having a large etching selectivity ratio with the organic compound film 103Rf. The mask film 159Rf is a film having a large etching selectivity ratio with the sacrificial film 158Rf.
[0233] In addition, the sacrificial film 158Rf and the mask film 159Rf are formed at a temperature lower than the heat resistance temperature of the organic compound film 103Rf. The substrate temperature when forming the sacrificial film 158Rf and the sacrificial film 159Rf is typically 200° C. or less, preferably 150° C. or less, more preferably 120° C. or less, further preferably 100° C. or less, and further preferably 80° C. or less.
[0234] The sacrificial film 158Rf and the mask film 159Rf are preferably films that can be removed by wet etching. By using wet etching, damage to the organic compound film 103Rf during processing of the sacrificial film 158Rf and the mask film 159Rf can be reduced compared to the case of using dry etching.
[0235] The sacrificial film 158Rf and the mask film 159Rf can be formed by, for example, sputtering, ALD (thermal ALD, PEALD), CVD, or vacuum deposition. Alternatively, they can be formed by the wet deposition method described above.
[0236] The sacrificial film 158Rf formed in contact with the organic compound film 103Rf is preferably formed by a formation method that causes less damage to the organic compound film 103Rf than when the mask film 159Rf is formed. For example, the sacrificial film 158Rf is preferably formed by ALD or vacuum deposition rather than sputtering.
[0237] As the sacrificial film 158Rf and the mask film 159Rf, for example, one or more of a metal film, an alloy film, a metal oxide film, a semiconductor film, an organic insulating film, and an inorganic insulating film can be used.
[0238] As the sacrificial film 158Rf and the mask film 159Rf, for example, metal materials such as gold, silver, platinum, magnesium, nickel, tungsten, chromium, molybdenum, iron, cobalt, copper, palladium, titanium, aluminum, yttrium, zirconium, and tantalum, or alloy materials containing the metal materials can be used. In particular, low melting point materials such as aluminum and silver are preferably used. By using a metal material that can shield ultraviolet rays as one or both of the sacrificial film 158Rf and the mask film 159Rf, it is possible to suppress ultraviolet rays from irradiating the organic compound film 103Rf and suppress the degradation of the organic compound film 103Rf, which is preferred.
[0239] In addition, as the sacrificial film 158Rf and the mask film 159Rf, metal oxides such as In-Ga-Zn oxide, indium oxide, In-Zn oxide, In-Sn oxide, indium titanium oxide (In-Ti oxide), indium tin zinc oxide (In-Sn-Zn oxide), indium titanium zinc oxide (In-Ti-Zn oxide), indium gallium tin zinc oxide (In-Ga-Sn-Zn oxide) or indium tin oxide containing silicon can be used respectively.
[0240] Note that element M (M is one or more of aluminum, silicon, boron, yttrium, copper, vanadium, beryllium, titanium, iron, nickel, germanium, zirconium, molybdenum, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, and magnesium) may be used instead of the above-mentioned gallium.
[0241] In addition, as the sacrificial film and the mask film, a film containing a material having light-shielding properties, especially ultraviolet light-shielding properties, is preferably used. As the material having light-shielding properties, various materials such as metals, insulators, semiconductors, and semimetals having ultraviolet light-shielding properties can be used. Since part or all of the sacrificial film and the mask film will be removed in the subsequent process, the sacrificial film and the mask film are preferably films that can be processed by etching, and are particularly preferably films with good processability.
[0242] As sacrificial films and mask films, semiconductor materials such as silicon or germanium are used, which have high affinity with the semiconductor manufacturing process and are therefore preferred. Alternatively, oxides or nitrides of the above semiconductor materials can be used. Alternatively, non-metallic materials such as carbon or their compounds can be used. In addition, metals such as titanium, tantalum, tungsten, chromium, aluminum, or alloys containing one or more of them can be used. In addition, oxides containing the above metals such as titanium oxide or chromium oxide, or nitrides such as titanium nitride, chromium nitride, or tantalum nitride can be used.
[0243] In addition, by using a film of a material having ultraviolet light shielding properties as a sacrificial film or a mask film, it is possible to prevent ultraviolet rays from irradiating the organic compound layer during, for example, an exposure process. By preventing ultraviolet rays from damaging the organic compound layer, the reliability of the light-emitting device can be improved.
[0244] Note that the film containing a material having ultraviolet light shielding properties also exhibits the same effect when used as a material for the inorganic insulating film 125f described later.
[0245] In addition, various inorganic insulating films can be used as the sacrificial film 158Rf and the mask film 159Rf. In particular, the oxide insulating film has a higher adhesion to the organic compound film 103Rf than the nitride insulating film, so it is preferred. For example, inorganic insulating materials such as aluminum oxide, hafnium oxide or silicon oxide can be used for the sacrificial film 158Rf and the mask film 159Rf. As the sacrificial film 158Rf and the mask film 159Rf, for example, an aluminum oxide film can be formed by the ALD method. By using the ALD method, the damage to the substrate (especially the organic compound layer) can be reduced, so it is preferred.
[0246] For example, an inorganic insulating film (e.g., an aluminum oxide film) formed using an ALD method can be used as the sacrificial film 158Rf, and an inorganic film (e.g., an In—Ga—Zn oxide film, an aluminum film, or a tungsten film) formed using a sputtering method can be used as the mask film 159Rf.
[0247] In addition, the same inorganic insulating film can be used for both the sacrificial layer 158Rf and the inorganic insulating layer 125 to be formed later. For example, an aluminum oxide film formed using the ALD method can be used for both the sacrificial layer 158Rf and the inorganic insulating layer 125. Here, the sacrificial layer 158Rf and the inorganic insulating layer 125 can be deposited under the same deposition conditions or different deposition conditions. For example, by depositing the sacrificial film 158Rf under the same conditions as the inorganic insulating layer 125, the sacrificial film 158Rf can be formed as an insulating layer with high barrier properties to at least one of water and oxygen. On the other hand, the sacrificial film 158Rf is a layer that will be mostly or entirely removed in a subsequent process, so it is preferably easy to process. Therefore, the sacrificial layer 158Rf is preferably deposited under conditions where the substrate temperature is lower than that of the inorganic insulating layer 125 during deposition.
[0248] An organic material may be used as one or both of the sacrificial film 158Rf and the mask film 159Rf. For example, as the organic material, a material that is soluble in a solvent that is chemically stable to at least the film located at the uppermost portion of the organic compound film 103Rf may be used. In particular, a material that is soluble in water or alcohol may be used appropriately. When depositing the above-mentioned material, it is preferred that the material is applied by a wet deposition method in a state where the material is dissolved in a solvent such as water or alcohol, and then a heat treatment is performed to evaporate the solvent. At this time, it is preferred to perform the heat treatment in a reduced pressure atmosphere, thereby removing the solvent at a low temperature and in a short time, and reducing the thermal damage to the organic compound film 103Rf.
[0249] The sacrificial film 158Rf and the mask film 159Rf may each be made of an organic resin such as polyvinyl alcohol (PVA), polyvinyl butyral, polyvinyl pyrrolidone, polyethylene glycol, polyglycerol, pullulan, water-soluble cellulose, alcohol-soluble polyamide resin, or fluororesin such as perfluoropolymer.
[0250] For example, an organic film (eg, a PVA film) formed by any of the evaporation method and the above-described wet deposition method may be used as the sacrificial film 158Rf, and an inorganic film (eg, a silicon nitride film) formed by sputtering may be used as the mask film 159Rf.
[0251] Then, if Fig. 9C As shown in FIG. 1 , a resist mask 190R is formed on the mask film 159Rf. The resist mask 190R can be formed by applying a photosensitive resin (photoresist), exposing it to light, and developing it.
[0252] The resist mask 190R may use a positive resist material or a negative resist material.
[0253] The resist mask 190R is provided at a position overlapping with the conductive layer 152R. The resist mask 190R is preferably also provided at a position overlapping with the conductive layer 152C. This can prevent the conductive layer 152C from being damaged during the manufacturing process of the display device. Note that the resist mask 190R may not be provided on the conductive layer 152C. Fig. 9C As shown in the cross-sectional view taken along B1 - B2 in FIG. 1 , the resist mask 190R is preferably provided so as to cover from the end of the organic compound film 103Rf to the end of the conductive layer 152C (the end on the organic compound film 103Rf side).
[0254] Then, if Fig.9D As shown, a portion of the mask film 159Rf is removed using the resist mask 190R to form a mask layer 159R. The mask layer 159R remains on the conductive layer 152R and the conductive layer 152C. Then, the resist mask 190R is removed. Next, a portion of the sacrificial film 158Rf is removed using the mask layer 159R as a mask (also referred to as a hard mask) to form a sacrificial layer 158R.
[0255] The sacrificial film 158Rf and the mask film 159Rf can be processed by wet etching or dry etching, respectively. The sacrificial film 158Rf and the mask film 159Rf are preferably processed by isotropic etching.
[0256] By using the wet etching method, the damage to the organic compound film 103Rf during the processing of the sacrificial film 158Rf and the mask film 159Rf can be reduced compared to the case of using the dry etching method. When the wet etching method is used, for example, a developer, a tetramethylammonium hydroxide aqueous solution (TMAH), dilute hydrofluoric acid, oxalic acid, phosphoric acid, acetic acid, nitric acid, or a mixed liquid thereof is preferably used.
[0257] Since the organic compound film 103Rf is not exposed when processing the mask film 159Rf, the range of processing methods is wider than when processing the sacrificial film 158Rf. Specifically, when processing the mask film 159Rf, even if an oxygen-containing gas is used as an etching gas, degradation of the organic compound film 103Rf can be suppressed.
[0258] In addition, when dry etching is used in processing the sacrificial film 158Rf, degradation of the organic compound film 103Rf can be suppressed by not using an oxygen-containing gas as an etching gas. In the case of dry etching, for example, a gas containing CF4, C4F8, SF6, CHF3, Cl2, H2O, BCl3 or a Group 18 element such as He is preferably used as an etching gas.
[0259] For example, when an aluminum oxide film formed by an ALD method is used as the sacrificial film 158Rf, a portion of the sacrificial film 158Rf can be removed by dry etching using CHF3 and He or CHF3, He and CH4. In addition, when an In-Ga-Zn oxide film formed by a sputtering method is used as the mask film 159Rf, a portion of the mask film 159Rf can be removed by a wet etching method using dilute phosphoric acid. Alternatively, a portion of the mask film 159Rf can be removed by dry etching using CH4 and Ar. Alternatively, a portion of the mask film 159Rf can be removed by wet etching using dilute phosphoric acid. In addition, when a tungsten film formed by a sputtering method is used as the mask film 159Rf, a portion of the mask film 159Rf can be removed by dry etching using SF6, CF4 and O2 or CF4, Cl2 and O2.
[0260] The resist mask 190R can be removed by the same method as the resist mask 191. The resist mask 190R can be removed, for example, by ashing using oxygen plasma. Alternatively, oxygen gas and CF4, C4F8, SF6, CHF3, Cl2, H2O, BCl3 or Group 18 elements such as He can be used. Alternatively, the resist mask 190R can be removed by wet etching. At this time, the sacrificial film 158Rf is located at the uppermost surface and the organic compound film 103Rf is not exposed, so that the organic compound film 103Rf can be prevented from being damaged in the removal process of the resist mask 190R. In addition, the range of selection of the removal method of the resist mask 190R can be expanded.
[0261] Then, if Fig.9D As shown, the organic compound film 103Rf is processed to form the organic compound layer 103R. For example, the organic compound layer 103R is formed by removing a portion of the organic compound film 103Rf using the mask layer 159R and the sacrifice layer 158R as a hard mask.
[0262] Therefore, if Fig.9D As shown in FIG. 1 , the stacked structure of the organic compound layer 103R, the sacrificial layer 158R, and the mask layer 159R remains on the conductive layer 152R. In addition, the conductive layer 152G and the conductive layer 152B are exposed.
[0263] Fig.9D 103R is located outside the end of the conductive layer 152R. By adopting this structure, the pixel aperture ratio can be improved. Fig.9D Although not shown in the figure, a recessed portion may be formed in a region of the insulating layer 175 that does not overlap with the organic compound layer 103R due to the etching process described above.
[0264] In addition, since the organic compound layer 103R covers the top surface and the side surface of the conductive layer 152R, the subsequent process can be performed in a manner that does not expose the conductive layer 152R. When the end of the conductive layer 152R is exposed, corrosion may occur in an etching process, for example. The product caused by the corrosion of the conductive layer 152R is sometimes unstable. For example, the product may be dissolved in a solution in wet etching, and the product may be scattered in the atmosphere in dry etching. When the product is dissolved in a solution or scattered in the atmosphere, for example, the product may adhere to the processed surface and the side surface of the organic compound layer 103R, etc., and have an adverse effect on the characteristics of the light-emitting device or may cause a leakage path to be formed between multiple light-emitting devices. In addition, in the region where the end of the conductive layer 152R is exposed, the adhesion of the layers in contact with each other may be reduced, and film peeling of the organic compound layer 103R or the conductive layer 152R may be easily caused.
[0265] Therefore, by adopting a structure in which the organic compound layer 103R covers the top surface and the side surfaces of the conductive layer 152R, for example, the yield and characteristics of the light-emitting device can be improved.
[0266] As described above, the resist mask 190R is preferably provided so as to cover from the end of the organic compound layer 103R to the end of the conductive layer 152C (the end on the organic compound layer 103R side) between B1 and B2. Fig.9D As shown, the sacrificial layer 158R and the mask layer 159R are provided between the dotted line B1-B2 in a manner covering the end of the organic compound layer 103R to the end of the conductive layer 152C (the end on one side of the organic compound layer 103R). Therefore, for example, the insulating layer 175 can be prevented from being exposed between B1-B2. Thus, the insulating layer 175, the insulating layer 174, and a portion of the insulating layer 173 can be prevented from being removed by etching or the like, resulting in the conductive layer 179 being exposed. Therefore, the conductive layer 179 can be prevented from being unintentionally electrically connected to other conductive layers. For example, a short circuit between the conductive layer 179 and the common electrode 155 to be formed in a later process can be prevented.
[0267] The organic compound film 103Rf is preferably processed by anisotropic etching. Anisotropic dry etching is particularly preferred. Alternatively, wet etching may be used.
[0268] When the dry etching method is used, by not using an oxygen-containing gas as an etching gas, degradation of the organic compound film 103Rf can be suppressed.
[0269] In addition, an oxygen-containing gas may be used as the etching gas. When the etching gas contains oxygen, the etching rate can be increased. Therefore, etching can be performed under low power conditions while maintaining a sufficient etching rate. Therefore, damage to the organic compound film 103Rf can be suppressed. In addition, defects such as adhesion of reaction products generated during etching can be suppressed.
[0270] When using the dry etching method, for example, it is preferred to use a gas containing H2, CF4, C4F8, SF6, CHF3, Cl2, H2O, BCl3 and one or more of the 18th group elements such as He or Ar as the etching gas. Alternatively, it is preferred to use a gas containing one or more of the above gases and oxygen as the etching gas. Alternatively, oxygen gas can also be used as the etching gas. Specifically, for example, a gas containing H2 and Ar or a gas containing CF4 and He can be used as the etching gas. In addition, for example, a gas containing CF4, He and oxygen can be used as the etching gas. In addition, for example, a gas containing H2 and Ar and an oxygen-containing gas can be used as the etching gas.
[0271] As described above, in one embodiment of the present invention, the mask layer 159R is formed by forming the resist mask 190R on the mask film 159Rf and removing a portion of the mask film 159Rf using the resist mask 190R. Then, the organic compound layer 103R is formed by removing a portion of the organic compound film 103Rf using the mask layer 159R as a mask. Therefore, it can be said that the organic compound layer 103R is formed by processing the organic compound film 103Rf using the photolithography method. In addition, a portion of the organic compound film 103Rf may be removed using the resist mask 190R. Then, the resist mask 190R may also be removed.
[0272] Next, for example, the conductive layer 152G is preferably subjected to a hydrophobic treatment. When the organic compound film 103Rf is processed, for example, the surface state of the conductive layer 152G sometimes becomes hydrophilic. By performing a hydrophobic treatment on the conductive layer 152G, for example, the adhesion between the conductive layer 152G and a layer to be formed in a subsequent process (here, the organic compound layer 103G) can be improved to suppress film peeling. Note that the hydrophobic treatment may not be performed.
[0273] Then, if Fig. 10A As shown in FIG. 1 , an organic compound film 103Gf which will later become the organic compound layer 103G is formed over the conductive layer 152G, the conductive layer 152B, the mask layer 159R, and the insulating layer 175 .
[0274] The organic compound film 103Gf can be formed by the same method as that used in forming the organic compound film 103Rf. In addition, the organic compound film 103Gf can have the same structure as that of the organic compound film 103Rf.
[0275] Then, if Fig. 10A As shown, a sacrificial film 158Gf, which will later become a sacrificial layer 158G, and a mask film 159Gf, which will later become a mask layer 159G, are sequentially formed on the organic compound film 103Gf and the mask layer 159R. Then, a resist mask 190G is formed. The materials and forming methods of the sacrificial film 158Gf and the mask film 159Gf are the same as those that can be applied to the sacrificial film 158Rf and the mask film 159Rf. The materials and forming methods of the resist mask 190G are the same as those that can be applied to the resist mask 190R.
[0276] The resist mask 190G is provided at a position overlapping with the conductive layer 152G.
[0277] Then, if Fig. 10B As shown, a portion of the mask film 159Gf is removed using the resist mask 190G to form the mask layer 159G. The mask layer 159G remains on the conductive layer 152G. Then, the resist mask 190G is removed. Next, a portion of the sacrificial film 158Gf is removed using the mask layer 159G as a mask to form the sacrificial layer 158G. Next, the organic compound film 103Gf is processed to form the organic compound layer 103G. For example, a portion of the organic compound film 103Gf is removed using the mask layer 159G and the sacrificial layer 158G as a hard mask to form the organic compound layer 103G.
[0278] Therefore, if Fig. 10B As shown in FIG. 1 , a stacked structure of the organic compound layer 103G, the sacrificial layer 158G, and the mask layer 159G remains on the conductive layer 152G. In addition, the mask layer 159R and the conductive layer 152B are exposed.
[0279] Next, for example, the conductive layer 152B is preferably subjected to a hydrophobic treatment. When processing the organic compound film 103Gf, for example, the surface state of the conductive layer 152B sometimes becomes hydrophilic. By conducting a hydrophobic treatment on the conductive layer 152B, for example, the adhesion between the conductive layer 152B and a layer to be formed in a subsequent process (here, the organic compound layer 103B) can be improved to suppress film peeling. Note that the hydrophobic treatment may not be performed.
[0280] Then, if Fig. 10C As shown in FIG. 1 , an organic compound film 103Bf which will later become the organic compound layer 103B is formed over the conductive layer 152B, the mask layer 159R, the mask layer 159G, and the insulating layer 175 .
[0281] The organic compound film 103Bf can be formed by the same method as that used to form the organic compound film 103Rf. In addition, the organic compound film 103Bf can have the same structure as that of the organic compound film 103Rf.
[0282] Then, if Fig. 10C As shown, a sacrificial film 158Bf, which will later become a sacrificial layer 158B, and a mask film 159Bf, which will later become a mask layer 159B, are sequentially formed on the organic compound film 103Bf and the mask layer 159R. Then, a resist mask 190B is formed. The materials and forming methods of the sacrificial film 158Bf and the mask film 159Bf are the same as those that can be applied to the sacrificial film 158Rf and the mask film 159Rf. The materials and forming methods of the resist mask 190B are the same as those that can be applied to the resist mask 190R.
[0283] The resist mask 190B is provided at a position overlapping with the conductive layer 152B.
[0284] Then, if Fig. 10D As shown, a portion of the mask film 159Bf is removed using the resist mask 190B to form the mask layer 159B. The mask layer 159B remains on the conductive layer 152B. Then, the resist mask 190B is removed. Next, a portion of the sacrificial film 158Bf is removed using the mask layer 159B as a mask to form the sacrificial layer 158B. Next, the organic compound film 103Bf is processed to form the organic compound layer 103B. For example, a portion of the organic compound film 103Bf is removed using the mask layer 159B and the sacrificial layer 158B as a hard mask to form the organic compound layer 103B.
[0285] Therefore, if Fig. 10D As shown in FIG. 1 , a stacked structure of the organic compound layer 103B, the sacrificial layer 158B, and the mask layer 159B remains on the conductive layer 152B. In addition, the mask layer 159R and the mask layer 159G are exposed.
[0286] Note that the side surfaces of the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B are each preferably perpendicular or substantially perpendicular to the formed surface. For example, the angle formed by the formed surface and these side surfaces is preferably not less than 60 degrees and not more than 90 degrees.
[0287] As described above, the distance between two adjacent organic compound layers in the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B formed using the photolithography method can be reduced to less than 8 μm, less than 5 μm, less than 3 μm, less than 2 μm, or less than 1 μm. Here, for example, the distance can be specified according to the distance between the opposite ends of the two adjacent organic compound layers in the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B. In this way, by reducing the distance between the island-shaped organic compound layers, a display device with high clarity and a large aperture ratio can be provided. In addition, the distance between the first electrodes of adjacent light-emitting devices can also be reduced, for example, to less than 10 μm, less than 8 μm, less than 5 μm, less than 3 μm, or less than 2 μm. In addition, the distance between the first electrodes of adjacent light-emitting devices is preferably greater than 2 μm and less than 5 μm.
[0288] Then, if Fig.11A As shown, it is preferred to remove the mask layer 159R, the mask layer 159G, and the mask layer 159B. Depending on the subsequent process, the sacrificial layer 158R, the sacrificial layer 158G, the sacrificial layer 158B, the mask layer 159R, the mask layer 159G, and the mask layer 159B may remain in the display device. By removing the mask layer 159R, the mask layer 159G, and the mask layer 159B at this stage, it is possible to suppress the mask layer 159R, the mask layer 159G, and the mask layer 159B from remaining in the display device. For example, in the case where a conductive material is used for the mask layer 159R, the mask layer 159G, and the mask layer 159B, by removing the mask layer 159R, the mask layer 159G, and the mask layer 159B in advance, it is possible to suppress the generation of leakage current and the formation of capacitance due to the remaining mask layer 159R, the mask layer 159G, and the mask layer 159B.
[0289] Note that, although the present embodiment describes the case where the mask layers 159R, 159G, and 159B are removed as an example, the mask layers 159R, 159G, and 159B may not be removed. For example, when the mask layers 159R, 159G, and 159B include the above-mentioned material having ultraviolet light shielding properties, it is preferable to proceed to the next step without removing the mask layers because the organic compound layer can be protected from ultraviolet rays.
[0290] The mask layer removal process can use the same method as the mask layer processing process. By using the wet etching method, compared with the case of using the dry etching method, the damage to the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B when removing the mask layer can be reduced.
[0291] Alternatively, the mask layer may be removed by dissolving it in a solvent such as water or alcohol. Examples of the alcohol include ethanol, methanol, isopropyl alcohol (IPA), and glycerin.
[0292] After removing the mask layer, a drying treatment may be performed to remove water contained in the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B and water adsorbed on the surfaces of the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B. For example, a heat treatment may be performed in an inert gas atmosphere or a reduced pressure atmosphere. The heat treatment may be performed at a substrate temperature of 50° C. to 200° C., preferably 60° C. to 150° C., and more preferably 70° C. to 120° C. The use of a reduced pressure atmosphere is preferred because drying can be performed at a lower temperature.
[0293] Then, if Fig. 11B As shown, an inorganic insulating film 125f, which will later become the inorganic insulating layer 125, is formed to cover the organic compound layer 103R, the organic compound layer 103G, the organic compound layer 103B, the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B.
[0294] As described later, an insulating film that will become an insulating layer 127 later is formed in a manner that contacts the top surface of the inorganic insulating film 125f. Therefore, the top surface of the inorganic insulating film 125f preferably has a high affinity with the material (e.g., a photosensitive resin composition containing acrylic resin) used for the insulating film. In order to improve this affinity, surface treatment can also be performed to hydrophobize the top surface of the inorganic insulating film 125f (or improve its hydrophobicity). For example, it is preferably processed using a silanizing agent such as hexamethyldisilazane (HMDS). By making the top surface of the inorganic insulating film 125f hydrophobic in this way, the above-mentioned insulating film can be formed with high adhesion. In addition, as a surface treatment, the above-mentioned hydrophobization treatment can also be performed.
[0295] Then, if Fig. 11C As shown in FIG. 1 , an insulating film 127 f which will later become an insulating layer 127 is formed on the inorganic insulating film 125 f.
[0296] The inorganic insulating film 125f and the insulating film 127f are preferably deposited by a formation method that causes less damage to the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B. In particular, since the inorganic insulating film 125f is formed in contact with the side surfaces of the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B, the inorganic insulating film 125f is preferably deposited by a formation method that causes less damage to the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B than when the insulating film 127f is deposited.
[0297] In addition, the inorganic insulating film 125f and the insulating film 127f are each formed at a temperature lower than the heat resistance temperature of the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B. By increasing the substrate temperature during deposition, the inorganic insulating film 125f having a low impurity concentration and high barrier properties against at least one of water and oxygen can be formed even if the thickness is thin.
[0298] The substrate temperature when forming the inorganic insulating film 125f and the insulating film 127f is preferably 60°C or higher, 80°C or higher, 100°C or higher, or 120°C or higher and 200°C or lower, 180°C or lower, 160°C or lower, 150°C or lower, or 140°C or lower.
[0299] As the inorganic insulating film 125f, it is preferable to form an insulating film with a thickness of 3 nm, 5 nm or 10 nm and 200 nm, 150 nm, 100 nm or 50 nm within the above-mentioned substrate temperature range.
[0300] The inorganic insulating film 125f is preferably formed by, for example, the ALD method. The ALD method is preferred because it can reduce deposition damage and deposit a film with high coverage. As the inorganic insulating film 125f, for example, an aluminum oxide film is preferably formed by the ALD method.
[0301] In addition, the inorganic insulating film 125f may be formed by a sputtering method, a CVD method, or a PECVD method having a higher deposition rate than the ALD method. Thus, a display device with high reliability can be manufactured with high productivity.
[0302] The insulating film 127f is preferably formed by the wet deposition method described above. The insulating film 127f is preferably formed by, for example, a photosensitive material by spin coating, and more specifically, is preferably formed by using a photosensitive resin composition containing an acrylic resin.
[0303] For example, it is preferred to use a resin composition containing a polymer, an acid generator and a solvent to form the insulating film 127f. The polymer is formed using one or more monomers and has a structure in which one or more structural units (also referred to as constituent units) are regularly or irregularly repeated. As an acid generator, one or both of a compound that generates an acid by irradiating light and a compound that generates an acid by heating can be used. The resin composition may also contain one or more of a photosensitizer, a sensitizer, a catalyst, an adhesive aid, a surfactant and an antioxidant.
[0304] In addition, it is preferable to perform heat treatment (also referred to as pre-baking) after forming the insulating film 127f. The heat treatment is performed at a temperature lower than the heat resistance temperature of the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B. The substrate temperature during the heat treatment is preferably 50° C. to 200° C., more preferably 60° C. to 150° C., and further preferably 70° C. to 120° C. In this way, the solvent in the insulating film 127f can be removed.
[0305] Next, exposure is performed to expose a portion of the insulating film 127f to visible light or ultraviolet light. Here, in the case where a positive photosensitive resin composition containing an acrylic resin is used for the insulating film 127f, visible light or ultraviolet light is irradiated to a region where the insulating layer 127 is not formed in a later process. The insulating layer 127 is formed in a region sandwiched by any two of the conductive layer 152R, the conductive layer 152G, and the conductive layer 152B, and around the conductive layer 152C. Therefore, visible light or ultraviolet light is irradiated to the conductive layer 152R, the conductive layer 152G, the conductive layer 152B, and the conductive layer 152C. Note that in the case where a negative photosensitive material is used for the insulating film 127f, visible light or ultraviolet light is irradiated to a region where the insulating layer 127 is to be formed.
[0306] The width of the insulating layer 127 to be formed later can be controlled by the region in which the insulating film 127f is exposed. In this embodiment, the insulating layer 127 is processed so that the insulating layer 127 has a portion overlapping with the top surface of the conductive layer 151.
[0307] The light used for exposure preferably includes i-line (wavelength: 365 nm). Alternatively, the light used for exposure may include at least one of g-line (wavelength: 436 nm) and h-line (wavelength: 405 nm).
[0308] Here, by providing an oxygen blocking insulating layer (e.g., an aluminum oxide film) as one or both of the sacrificial layer 158 (sacrificial layer 158R, sacrificial layer 158G, and sacrificial layer 158B) and the inorganic insulating film 125f, diffusion of oxygen into the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B can be suppressed. When light (visible light or ultraviolet light) is irradiated to the organic compound layer, the organic compound contained in the organic compound layer sometimes becomes excited and promotes reaction with oxygen in the atmosphere. Specifically, when light (visible light or ultraviolet light) is irradiated to the organic compound layer in an oxygen-containing atmosphere, oxygen may be bonded to the organic compound contained in the organic compound layer. By providing the sacrificial layer 158 and the inorganic insulating film 125f on the island-shaped organic compound layer, bonding of oxygen in the atmosphere to the organic compound contained in the organic compound layer can be suppressed.
[0309] Then, if Fig. 12AAs shown, the exposed area in the insulating film 127f is removed by development to form the insulating layer 127a. The insulating layer 127a is formed in the area sandwiched by any two of the conductive layer 152R, the conductive layer 152G, and the conductive layer 152B and the area surrounding the conductive layer 152C. Here, in the case of using an acrylic resin for the insulating film 127f, an alkaline solution, such as TMAH, can be used as a developer.
[0310] Next, residues left during development (so-called scum) may be removed. For example, the residues may be removed by ashing using oxygen plasma.
[0311] In addition, etching may be performed to adjust the height of the surface of the insulating layer 127a. The insulating layer 127a may be processed by, for example, ashing using oxygen plasma. In addition, when a non-photosensitive material is used as the insulating film 127f, the height of the surface of the insulating film 127f may also be adjusted by, for example, ashing.
[0312] Then, if Fig. 12B As shown, the insulating layer 127a is used as a mask to perform etching to remove a portion of the inorganic insulating film 125f, thereby reducing the thickness of a portion of the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B. As a result, the inorganic insulating layer 125 is formed under the insulating layer 127a. In addition, the surface of the thinner portion of the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B is exposed. Hereinafter, the etching process using the insulating layer 127a as a mask is sometimes referred to as the first etching process.
[0313] The first etching process can be performed by dry etching or wet etching. When the inorganic insulating film 125f is deposited using the same material as the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B, the first etching process can be performed at once, which is preferable.
[0314] By using the insulating layer 127 a having tapered side surfaces as a mask for etching, the side surfaces of the inorganic insulating layer 125 and the upper end portions of the side surfaces of the sacrificial layers 158R, 158G, and 158B can be easily tapered.
[0315] When dry etching is performed, chlorine-based gas is preferably used. As the chlorine-based gas, one gas selected from Cl2, BCl3, SiCl4, and CCl4, or a mixture of two or more of the above gases, can be used. In addition, one gas selected from oxygen gas, hydrogen gas, helium gas, and argon gas, or a mixture of two or more of the above gases can be appropriately added to the above chlorine-based gas. By utilizing dry etching, thin regions of the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B can be formed with excellent in-plane uniformity.
[0316] As a dry etching device, a dry etching device having a high-density plasma source can be used. For example, as a dry etching device having a high-density plasma source, for example, an inductively coupled plasma (ICP: Inductively Coupled Plasma) etching device can be used. Alternatively, a capacitively coupled plasma (CCP: Capacitively Coupled Plasma) etching device including parallel plate electrodes can be used. The capacitively coupled plasma etching device including parallel plate electrodes can also adopt a structure in which a high-frequency voltage is applied to one of the parallel plate electrodes. Alternatively, a structure in which multiple different high-frequency voltages are applied to one of the parallel plate electrodes can also be adopted. Alternatively, a structure in which a high-frequency voltage with the same frequency is applied to each of the parallel plate electrodes can also be adopted. Alternatively, a structure in which high-frequency voltages with different frequencies are applied to each of the parallel plate electrodes can also be adopted.
[0317] In addition, when dry etching is performed, byproducts generated during dry etching may be deposited on the top surface and side surfaces of the insulating layer 127a. As a result, components in the etching gas, components in the inorganic insulating film 125f, components in the sacrificial layers 158R, 158G, and 158B may be included in the insulating layer 127 after the display device is completed.
[0318] In addition, it is preferred to perform the first etching process using wet etching. By using the wet etching method, the damage to the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B can be further reduced compared to the case of using the dry etching method. For example, wet etching can be performed using an alkaline solution. For example, TMAH, an alkaline solution, can be used in the wet etching of the aluminum oxide film. At this time, wet etching can be performed in a glue coating manner. When the inorganic insulating film 125f is deposited using the same material as the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B, the above-mentioned etching process can be performed at one time, so it is preferred.
[0319] In the first etching process, the sacrificial layers 158R, 158G, and 158B are not completely removed, and the etching process is stopped in a state where the thickness is reduced. In this way, by leaving the corresponding sacrificial layers 158R, 158G, and 158B on the organic compound layers 103R, 103G, and 103B, the organic compound layers 103R, 103G, and 103B can be prevented from being damaged in the subsequent process.
[0320] Next, the entire substrate is preferably exposed to visible light or ultraviolet light to irradiate the insulating layer 127a. The energy density of this exposure is preferably greater than 0 mJ / cm 2And 800mJ / cm 2 Below, more preferably greater than 0 mJ / cm 2 And 500mJ / cm 2 By performing such exposure after development, the transparency of the insulating layer 127a can be improved. In addition, the substrate temperature required for heat treatment in a later step for deforming the insulating layer 127a into a tapered shape can be reduced.
[0321] Here, by providing an oxygen blocking insulating layer (e.g., an aluminum oxide film) as the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B, it is possible to suppress the diffusion of oxygen into the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B. When light (visible light or ultraviolet light) is irradiated to the organic compound layer, sometimes the organic compound contained in the organic compound layer becomes excited and promotes the reaction with oxygen in the atmosphere. Specifically, when light (visible light or ultraviolet light) is irradiated to the organic compound layer in an oxygen-containing atmosphere, oxygen may be bonded to the organic compound contained in the organic compound layer. By providing the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B on the island-shaped organic compound layer, it is possible to suppress the oxygen in the atmosphere from bonding to the organic compound contained in the organic compound layer.
[0322] Next, a heat treatment (also called post-baking) is performed. By performing the heat treatment, the insulating layer 127a can be deformed into an insulating layer 127 having a tapered shape on its side. Fig. 12C ). The heat treatment is performed at a temperature lower than the heat resistance temperature of the organic compound layer. The heat treatment can be performed at a substrate temperature of 50°C to 200°C, preferably 60°C to 150°C, and more preferably 70°C to 130°C. The heating atmosphere can be either an air atmosphere or an inert gas. In addition, the heating atmosphere can be either an air atmosphere or a reduced pressure atmosphere. In the heat treatment of this step, it is preferred to increase the substrate temperature compared to the heat treatment (pre-baking) after the insulating film 127f is formed. Thereby, the adhesion between the insulating layer 127 and the inorganic insulating layer 125 can be improved, and the corrosion resistance of the insulating layer 127 can also be improved.
[0323] In the first etching process, the sacrificial layers 158R, 158G, and 158B are not completely removed, but the sacrificial layers 158R, 158G, and 158B are left in a thin state, so that the organic compound layers 103R, 103G, and 103B can be prevented from being damaged and deteriorated during the heat treatment. Thus, the reliability of the light-emitting device can be improved.
[0324] Note that the side surface of the insulating layer 127 may have a concave curved surface shape depending on the material of the insulating layer 127 and the temperature, time, and atmosphere of the post-bake. For example, as the temperature in the post-bake conditions increases or the time increases, the shape of the insulating layer 127 is more likely to change, and thus a concave curved surface shape may be formed.
[0325] Then, if Fig.13A As shown in FIG. 1 , etching is performed using the insulating layer 127 as a mask to remove a portion of the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B. Note that a portion of the inorganic insulating layer 125 is sometimes removed. As a result, openings are formed in the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B, respectively, and the top surfaces of the organic compound layer 103R, the organic compound layer 103G, the organic compound layer 103B, and the conductive layer 152C are exposed. Hereinafter, the etching process using the insulating layer 127 as a mask is sometimes referred to as a second etching process.
[0326] The end of the inorganic insulating layer 125 is covered with the insulating layer 127. Fig.13A An example is shown in which a portion of the end portion of the sacrificial layer 158G (specifically, the tapered portion formed by the first etching process) is covered with the insulating layer 127 and the tapered portion formed by the second etching process is exposed.
[0327] When the inorganic insulating layer 125 and the sacrificial layer are etched at one time without the first etching process and after post-baking, sometimes the inorganic insulating layer 125, the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B below the end of the insulating layer 127 disappear due to side etching, forming a cavity. Due to the cavity, the surface on which the common electrode 155 is formed is uneven, and disconnection is likely to occur in the common electrode 155. Even if the inorganic insulating layer 125, the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B are side-etched to form a cavity after the first etching process, the cavity can be filled by the insulating layer 127 through the post-baking performed thereafter. Then, in the second etching process, the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B whose thickness is further reduced are etched, so the amount of side etching is small, it is not easy to form a cavity, and the cavity that can be formed can also be extremely small. Therefore, the surface on which the common electrode 155 is formed can be made flatter.
[0328] The insulating layer 127 may cover the entire end of the sacrificial layer 158G. For example, the end of the insulating layer 127 may sag and cover the end of the sacrificial layer 158G. In addition, for example, the end of the insulating layer 127 may contact the top surface of at least one of the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B. As described above, when the insulating layer 127a after development is not exposed, the shape of the insulating layer 127 may be easily changed.
[0329] The second etching process is performed by wet etching. By using the wet etching method, damage to the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B can be reduced compared with the case of using the dry etching method. Wet etching can be performed using an alkaline solution such as TMAH.
[0330] On the other hand, when the second etching process is performed by wet etching, if there is a gap at the interface between the organic compound layer 103 and the sacrificial layer 158, between the organic compound layer 103 and the inorganic insulating layer 125, and between the organic compound layer 103 and the insulating layer 175 due to problems such as the adhesion between the organic compound layer 103 and other layers, the chemical solution used in the second etching process sometimes enters the gap and contacts the pixel electrode. Here, when the chemical solution contacts both the conductive layer 151 and the conductive layer 152, the conductive layer with a lower natural potential among the conductive layers 151 and 152 is sometimes corroded due to galvanic corrosion. For example, when aluminum is used as the conductive layer 151 and indium tin oxide is used as the conductive layer 152, the conductive layer 152 is sometimes corroded. As a result, the yield of the display device is sometimes reduced. In addition, the reliability of the display device is sometimes reduced.
[0331] As described above, when the conductive layer 152 is formed so as to cover the top surface and the side surfaces of the conductive layer 151, even if there is a gap between the organic compound layer 103 and the sacrificial layer 158, between the organic compound layer 103 and the inorganic insulating layer 125, and between the organic compound layer 103 and the insulating layer 175, the chemical solution can be prevented from contacting the conductive layer 151 in the second etching process. Thus, corrosion of the pixel electrode such as the conductive layer 152 can be prevented.
[0332] Furthermore, since the insulating layer 156 is formed to have a region overlapping the side surface of the conductive layer 151 and the conductive layer 152 is formed to cover the conductive layer 151 and the insulating layer 156, disconnection of the conductive layer 152 can be prevented, and thus, for example, the chemical solution can be prevented from contacting the conductive layer 151 in the second etching process. Thus, corrosion of the pixel electrode such as the conductive layer 152 can be prevented.
[0333] As described above, by providing the insulating layer 127, the inorganic insulating layer 125, the sacrificial layer 158R, the sacrificial layer 158G, and the sacrificial layer 158B, it is possible to suppress the occurrence of poor connection due to disconnected portions and resistance increase due to locally thin portions in the common electrode 155 between the light-emitting devices. Thus, the display device of one embodiment of the present invention can improve display quality.
[0334] In addition, after a portion of the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B is exposed, a heat treatment may be further performed. By this heat treatment, water contained in each organic compound layer and water adsorbed on the surface of each organic compound layer may be removed. In addition, water contained in an intermediate layer of an intermediate layer containing an alkali metal or an alkali metal compound included in each organic compound layer may be removed. In addition, the shape of the insulating layer 127 may sometimes change due to the heat treatment. Specifically, the insulating layer 127 may sometimes expand in a manner covering at least one of the end of the inorganic insulating layer 125, the end of the sacrificial layer 158R, the sacrificial layer 158G, and the top surface of the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B.
[0335] When the temperature of the heat treatment is too low, water contained in each organic compound layer, water adsorbed on the surface of each organic compound layer, and water contained in the intermediate layer containing an alkali metal or an alkali metal compound cannot be sufficiently removed. In addition, when the temperature of the heat treatment is too high, degradation of the organic compound layer 103 and excessive change in the shape of the insulating layer 127 may occur. Therefore, the heat treatment temperature is preferably higher than the temperature at which water is separated from the organic compound layer 103 and lower than the glass transition temperature of the organic compound contained in the organic compound layer 103, and is preferably lower than the glass transition temperature of the organic compound contained in the top surface of the organic compound layer 103. Specifically, the substrate temperature is preferably 80° C. to 130° C., more preferably 90° C. to 120° C., further preferably 100° C. to 120° C., and further preferably 100° C. to 110° C. The heating atmosphere may be either an air atmosphere or an inert gas atmosphere. Note that the heating atmosphere may be an atmospheric pressure atmosphere or a reduced pressure atmosphere, and a reduced pressure atmosphere is preferably used to prevent water separated from the organic compound layer 103 from being re-adsorbed.
[0336] By this heat treatment, water contained in each organic compound layer, water adsorbed on the surface of each organic compound layer, and water contained in the intermediate layer containing an alkali metal or an alkali metal compound can be sufficiently removed without causing degradation of the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B and excessive change in the shape of the insulating layer 127. Thus, even when a manufacturing method is adopted in which an intermediate layer containing an alkali metal or an alkali metal compound is exposed to a photolithography process, a significant increase in the driving voltage of the light-emitting device and a significant decrease in the current efficiency can be prevented.
[0337] Then, if Fig. 13BAs shown, a common layer 104 and a common electrode 155 are formed on the organic compound layer 103R, the organic compound layer 103G, the organic compound layer 103B, the conductive layer 152C, and the insulating layer 127. The common layer 104 and the common electrode 155 can be formed by a method such as a sputtering method or a vacuum evaporation method. Alternatively, the common layer 104 can be formed by an evaporation method and the common electrode 155 can be formed by a sputtering method.
[0338] Then, if Fig. 13C As shown, a protective layer 131 is formed on the common electrode 155. The protective layer 131 can be formed by vacuum evaporation, sputtering, CVD, ALD or the like.
[0339] Next, the substrate 120 is bonded to the protective layer 131 using the resin layer 122, whereby a display device can be manufactured. As described above, in the method for manufacturing a display device according to one embodiment of the present invention, the insulating layer 156 is provided so as to have a region overlapping with the side surface of the conductive layer 151, and the conductive layer 152 is formed so as to cover the conductive layer 151 and the insulating layer 156. Thus, the yield of the display device can be improved, and the occurrence of defects can be suppressed.
[0340] As described above, in a method for manufacturing a display device of one embodiment of the present invention, the island-shaped organic compound layer 103R, the island-shaped organic compound layer 103G, and the island-shaped organic compound layer 103B are not formed using a high-precision metal mask but are formed by depositing a film on one surface and then processing it, so that the island layer can be formed with a uniform thickness. In addition, a high-definition display device or a display device with a high aperture ratio can be realized. In addition, even if the clarity or aperture ratio is high and the distance between sub-pixels is extremely short, the organic compound layer 103R, the organic compound layer 103G, and the organic compound layer 103B in adjacent sub-pixels can be prevented from contacting each other. Therefore, leakage current can be suppressed between sub-pixels. Thus, crosstalk can be prevented and a display device with extremely high contrast can be realized. In addition, a display device having good characteristics even if it includes a tandem light-emitting device manufactured by photolithography can be provided.
[0341] (Implementation 4) In this embodiment, a display device which is one embodiment of the present invention is described.
[0342] The display device of this embodiment can be a high-definition display device. Therefore, for example, the display device of this embodiment can be used for the display portion of information terminal devices (wearable devices) such as watch-type and bracelet-type devices, and the display portion of wearable devices that can be worn on the head such as VR devices such as head-mounted displays (HMDs) and glasses-type AR devices.
[0343] In addition, the display device of this embodiment can be a high-resolution display device or a large display device. Therefore, for example, the display device of this embodiment can be used for the display portion of the following devices: electronic devices with large screens such as television devices, desktop or notebook personal computers, displays for computers, etc., digital signage and large game machines such as pinball machines, etc.; digital cameras; digital video cameras; digital photo frames; mobile phones; portable game consoles; portable information terminals; and sound reproduction devices.
[0344] [Display module] Fig.14A The display module 280 is a perspective view showing the display module 280. The display module 280 includes a light emitting device 100A and an FPC 290.
[0345] The display module 280 includes a substrate 291 and a substrate 292. The display module 280 includes a display portion 281. The display portion 281 is an image display region in the display module 280, and light from each pixel provided in a pixel portion 284 described below can be viewed.
[0346] Fig. 14B 2 is a perspective view schematically showing a structure on one side of a substrate 291. A circuit portion 282, a pixel circuit portion 283 on the circuit portion 282, and a pixel portion 284 on the pixel circuit portion 283 are stacked on the substrate 291. In addition, a terminal portion 285 for connecting to the FPC 290 is provided on a portion of the substrate 291 that is not overlapped by the pixel portion 284. The terminal portion 285 is electrically connected to the circuit portion 282 via a wiring portion 286 composed of a plurality of wirings.
[0347] The pixel portion 284 includes a plurality of pixels 284 a arranged periodically. Fig. 14B An enlarged view of one pixel 284a is shown on the right side of FIG. The pixel 284a can adopt the various structures described in the above embodiment. Fig. 14B An example is shown in which the pixel 284 a has the same structure as the pixel 178 shown in FIG. 6 .
[0348] The pixel circuit portion 283 includes a plurality of pixel circuits 283 a arranged periodically.
[0349] One pixel circuit 283a controls the driving of multiple devices included in one pixel 284a. Three circuits for controlling the light emission of one light emitting device may be provided in one pixel circuit 283a. For example, the pixel circuit 283a may adopt a structure including at least one selection transistor, one current control transistor (driving transistor) and a capacitor for one light emitting device. At this time, a gate signal is input to the gate of the selection transistor, and a video signal is input to the source or drain. Thus, an active matrix display device is realized.
[0350] The circuit unit 282 includes a circuit for driving each pixel circuit 283a of the pixel circuit unit 283. For example, it preferably includes one or both of a gate line driving circuit and a source line driving circuit. In addition, it may include at least one of a calculation circuit, a storage circuit, and a power supply circuit.
[0351] The FPC 290 is used as wiring for supplying video signals, power supply potential, and the like from the outside to the circuit portion 282. Alternatively, an IC may be mounted on the FPC 290.
[0352] The display module 280 can adopt a structure in which one or both of the pixel circuit unit 283 and the circuit unit 282 are stacked on the lower side of the pixel unit 284, so that the display unit 281 can have an extremely high aperture ratio (effective display area ratio). For example, the aperture ratio of the display unit 281 can be 40% or more and less than 100%, preferably 50% or more and 95% or less, and more preferably 60% or more and 95% or less. In addition, the pixels 284a can be arranged at an extremely high density, thereby making the display unit 281 have an extremely high definition. For example, the display unit 281 preferably arranges the pixels 284a at a definition of less than 20,000 ppi or less than 30,000 ppi and more than 2,000 ppi, more preferably more than 3,000 ppi, further preferably more than 5,000 ppi, and further preferably more than 6,000 ppi.
[0353] Due to its extremely high definition, the display module 280 can be suitable for use in VR devices such as HMD or glasses-type AR devices. For example, because the display module 280 has an extremely high-definition display unit 281, in the structure of viewing the display unit of the display module 280 through a lens, even if the display unit is magnified by a lens, the user cannot see the pixels, thereby achieving a highly immersive display. In addition, without limitation to this, the display module 280 can also be applied to electronic devices with a relatively small display unit. For example, it is suitable for use in the display unit of wearable electronic devices such as watch-type devices.
[0354] [Display device 100A] Fig.15A The display device 100A shown includes a substrate 301 , a light emitting device 130R, a light emitting device 130G, a light emitting device 130B, a capacitor 240 , and a transistor 310 .
[0355] Substrate 301 is equivalent to Fig.14A and Fig. 14BThe transistor 310 is a transistor having a channel formation region in the substrate 301. As the substrate 301, for example, a semiconductor substrate such as a single crystal silicon substrate can be used. The transistor 310 includes a portion of the substrate 301, a conductive layer 311, a low resistance region 312, an insulating layer 313 and an insulating layer 314. The conductive layer 311 is used as a gate electrode. The insulating layer 313 is located between the substrate 301 and the conductive layer 311 and is used as a gate insulating layer. The low resistance region 312 is a region doped with impurities in the substrate 301 and is used as a source or a drain. The insulating layer 314 covers the side of the conductive layer 311.
[0356] Furthermore, an element isolation layer 315 is provided between two adjacent transistors 310 so as to be embedded in the substrate 301 .
[0357] In addition, an insulating layer 261 is provided to cover the transistor 310 , and the capacitor 240 is provided over the insulating layer 261 .
[0358] The capacitor 240 includes a conductive layer 241, a conductive layer 245, and an insulating layer 243 therebetween. The conductive layer 241 is used as one electrode in the capacitor 240, the conductive layer 245 is used as the other electrode in the capacitor 240, and the insulating layer 243 is used as a dielectric of the capacitor 240.
[0359] The conductive layer 241 is provided on the insulating layer 261 and embedded in the insulating layer 254. The conductive layer 241 is electrically connected to one of the source and the drain of the transistor 310 through the plug 271 embedded in the insulating layer 261. The insulating layer 243 is provided in a manner covering the conductive layer 241. The conductive layer 245 is provided in a region overlapping with the conductive layer 241 via the insulating layer 243.
[0360] An insulating layer 255 is provided to cover the capacitor 240, an insulating layer 174 is provided on the insulating layer 255, and an insulating layer 175 is provided on the insulating layer 174. On the insulating layer 175, the light emitting devices 130R, 130G, and 130B are provided. Fig.15A The light emitting device 130R, the light emitting device 130G and the light emitting device 130B are shown to have Fig. 9A An example of a stacked structure is shown. An insulating material is provided in the region between adjacent light emitting devices. Fig.15A In the embodiment, an inorganic insulating layer 125 and an insulating layer 127 on the inorganic insulating layer 125 are provided in the region.
[0361] The insulating layer 156R is provided so as to have a region overlapping with the side surface of the conductive layer 151R included in the light emitting device 130R, the insulating layer 156G is provided so as to have a region overlapping with the side surface of the conductive layer 151G included in the light emitting device 130G, and the insulating layer 156B is provided so as to have a region overlapping with the side surface of the conductive layer 151B included in the light emitting device 130B. In addition, the conductive layer 152R is provided so as to cover the conductive layer 151R and the insulating layer 156R, the conductive layer 152G is provided so as to cover the conductive layer 151G and the insulating layer 156G, and the conductive layer 152B is provided so as to cover the conductive layer 151B and the insulating layer 156B. Furthermore, the sacrificial layer 158R is located on the organic compound layer 103R included in the light emitting device 130R, the sacrificial layer 158G is located on the organic compound layer 103G included in the light emitting device 130G, and the sacrificial layer 158B is located on the organic compound layer 103B included in the light emitting device 130B.
[0362] Conductive layer 151R, conductive layer 151G, and conductive layer 151B are electrically connected to one of the source and drain of transistor 310 via plug 256 embedded in insulating layer 243, insulating layer 255, insulating layer 174, and insulating layer 175, conductive layer 241 embedded in insulating layer 254, and plug 271 embedded in insulating layer 261. The height of the top surface of insulating layer 175 is equal to or substantially equal to the height of the top surface of plug 256. Various conductive materials can be used for the plug.
[0363] In addition, a protective layer 131 is provided on the light emitting device 130R, the light emitting device 130G, and the light emitting device 130B. The substrate 120 is bonded to the protective layer 131 via a resin layer 122. The details of the components of the light emitting device 130 to the substrate 120 can be referred to Embodiment 3. The substrate 120 corresponds to Fig.14A substrate 292.
[0364] Fig. 15B Show Fig.15A A modified example of the display device 100A shown. Fig. 15B The display device shown includes a coloring layer 132R, a coloring layer 132G, and a coloring layer 132B, and the light emitting device 130 has a region overlapping one of the coloring layer 132R, the coloring layer 132G, and the coloring layer 132B. Fig. 15B In the light-emitting device shown, the light-emitting device 130 can emit white light, for example. In addition, for example, the coloring layer 132R, the coloring layer 132G, and the coloring layer 132B can transmit red light, green light, and blue light, respectively. In this way, in a display device using a coloring layer, only light-emitting devices that emit white light need to be manufactured in the manufacture of a display device that is required to display in full color, so the manufacturing method of the above-mentioned display device can be simplified.
[0365] This embodiment mode can be combined with other embodiment modes or examples as appropriate. In addition, in this specification, when a plurality of configuration examples are shown in one embodiment mode, the configuration examples can be combined as appropriate.
[0366] (Implementation 5) In this embodiment, an electronic device which is one embodiment of the present invention is described.
[0367] The electronic device of this embodiment includes a display device of one embodiment of the present invention in a display portion. The display device of one embodiment of the present invention has high reliability and can easily achieve high definition and high resolution. Therefore, it can be used in the display portion of various electronic devices.
[0368] Electronic devices include, for example, television sets, desktop or notebook personal computers, displays for computers, etc., digital signage, large-scale game consoles such as pinball machines, and other electronic devices with larger screens, as well as digital cameras, digital video cameras, digital photo frames, mobile phones, portable game consoles, portable information terminals, sound reproduction devices, and the like.
[0369] In particular, since the display device of one embodiment of the present invention can improve the clarity, it can be appropriately used in electronic devices including a smaller display unit. Examples of such electronic devices include watch-type and bracelet-type information terminal devices (wearable devices), wearable devices that can be worn on the head, VR devices such as head-mounted displays, glasses-type AR devices, and MR devices.
[0370] A display device according to one embodiment of the present invention preferably has an extremely high resolution such as HD (1280×720 pixels), FHD (1920×1080 pixels), WQHD (2560×1440 pixels), WQXGA (2560×1600 pixels), 4K (3840×2160 pixels), 8K (7680×4320 pixels), etc. In particular, the resolution is preferably set to 4K, 8K or above. In addition, the pixel density (clarity) of a display device according to one embodiment of the present invention is preferably 100 ppi or more, preferably 300 ppi or more, more preferably 500 ppi or more, further preferably 1000 ppi or more, further preferably 2000 ppi or more, further preferably 3000 ppi or more, further preferably 5000 ppi or more, further preferably 7000 ppi or more. By using a display device having one or both of high resolution and high definition, the sense of reality and depth can be further improved in electronic devices for personal use such as portable or home use. In addition, there is no particular limitation on the screen ratio (aspect ratio) of the display device of one embodiment of the present invention. For example, the display device can adapt to various screen ratios such as 1:1 (square), 4:3, 16:9 and 16:10.
[0371] The electronic device of this embodiment may also include a sensor (the sensor has the function of measuring the following factors: force, displacement, position, speed, acceleration, angular velocity, rotation speed, distance, light, liquid, magnetism, temperature, chemical substance, sound, time, hardness, electric field, current, voltage, electricity, radiation, flow, humidity, inclination, vibration, smell or infrared).
[0372] The electronic device of this embodiment may have various functions. For example, it may have the following functions: a function of displaying various information (static images, dynamic images, text images, etc.) on a display unit; a function of a touch panel; a function of displaying a calendar, date, or time, etc.; a function of executing various software (programs); a function of wireless communication; a function of reading programs or data stored in a storage medium; etc.
[0373] use FIG. 16A to FIG. 16D An example of a wearable device that can be worn on the head is described. These wearable devices have at least one of a function of displaying AR content, a function of displaying VR content, a function of displaying SR content, and a function of displaying MR content. When an electronic device has a function of displaying at least one of AR, VR, SR, and MR, the user's sense of immersion can be improved.
[0374] Fig.16A The electronic device 700A shown and Fig. 16BThe electronic devices 700B shown include a pair of display panels 751, a pair of frames 721, a communication unit (not shown), a pair of mounting units 723, a control unit (not shown), an imaging unit (not shown), a pair of optical components 753, a frame 757 and a pair of nose pads 758.
[0375] The display device of one embodiment of the present invention can be applied to the display panel 751. Thus, a highly reliable electronic device can be realized.
[0376] Both the electronic device 700A and the electronic device 700B can project the image displayed by the display panel 751 onto the display area 756 in the optical member 753. Since the optical member 753 is light-transmissive, the user can see the image displayed in the display area overlapping with the transmitted image seen through the optical member 753. Therefore, both the electronic device 700A and the electronic device 700B are electronic devices capable of AR display.
[0377] The electronic device 700A and the electronic device 700B may also be provided with a camera capable of photographing the front as an imaging unit. In addition, by providing an acceleration sensor such as a gyro sensor on the electronic device 700A and the electronic device 700B, the user's head orientation can be detected and an image corresponding to the direction can be displayed on the display area 756.
[0378] The communication unit includes a wireless communication device, through which, for example, a video signal can be supplied. In addition, the communication unit may include a connector to which a cable for supplying the video signal and the power supply potential can be connected, instead of or in addition to the wireless communication device.
[0379] Furthermore, electronic device 700A and electronic device 700B are provided with batteries, and can be charged wirelessly or by wire, or both.
[0380] The frame 721 may also be provided with a touch sensor module. The touch sensor module has a function of detecting whether the outer surface of the frame 721 is touched. Through the touch sensor module, various processes can be performed by detecting a user's tapping operation or sliding operation. For example, a process such as temporarily stopping or restarting a dynamic image can be performed through a tapping operation, and a process such as fast forwarding or rewinding can be performed through a sliding operation. In addition, by providing a touch sensor module in each of the two frames 721, the operating range can be expanded.
[0381] As the touch sensor module, various touch sensors can be used. For example, various methods such as electrostatic capacitance, resistance film, infrared, electromagnetic induction, surface acoustic wave, and optical can be used. In particular, it is preferred to use electrostatic capacitance or optical sensors in the touch sensor module.
[0382] When an optical touch sensor is used, a photoelectric conversion device (also referred to as a photoelectric conversion element) can be used as a light receiving device. Inorganic semiconductors and organic semiconductors or both can be used in the active layer of the photoelectric conversion device.
[0383] Fig. 16C The electronic device 800A shown and Fig.16D The electronic devices 800B shown each include a pair of display portions 820 , a housing 821 , a communication portion 822 , a pair of mounting portions 823 , a control portion 824 , a pair of imaging portions 825 , and a pair of lenses 832 .
[0384] The display device of one embodiment of the present invention can be applied to the display portion 820. Thus, an electronic device with high reliability can be realized.
[0385] The display unit 820 is provided at a position visible through the lens 832 inside the housing 821. In addition, by displaying different images on each of the pair of display units 820, three-dimensional display using parallax can be performed.
[0386] The electronic device 800A and the electronic device 800B can both be referred to as VR-oriented electronic devices. A user who wears the electronic device 800A or the electronic device 800B can see the image displayed on the display unit 820 through the lens 832 .
[0387] The electronic device 800A and the electronic device 800B preferably have a mechanism in which the left and right positions of the lens 832 and the display unit 820 can be adjusted so that the lens 832 and the display unit 820 are located at the most suitable position according to the position of the user's eyes. In addition, it is preferable to have a mechanism in which the focus is adjusted by changing the distance between the lens 832 and the display unit 820.
[0388] The user can use the mounting portion 823 to mount the electronic device 800A or the electronic device 800B on the head. Fig. 16C In the embodiment, the mounting portion 823 has a shape such as the temples of glasses (also referred to as hinges or temples, etc.), but is not limited thereto. As long as the user can fit it, the mounting portion 823 may have a helmet-type or belt-type shape, for example.
[0389] The imaging unit 825 has a function of acquiring external information. The data acquired by the imaging unit 825 can be output to the display unit 820. An image sensor can be used in the imaging unit 825. In addition, a plurality of cameras can be provided to be able to correspond to various viewing angles such as telephoto and wide angle.
[0390] Note that the example including the imaging unit 825 is shown here, and a distance measuring sensor (hereinafter, also referred to as a detection unit) capable of measuring the distance to the object may be provided. In other words, the imaging unit 825 is a form of a detection unit. As the detection unit, for example, an image sensor or a distance image sensor such as a laser radar (LIDAR: Light Detection and Ranging) may be used. By using the image obtained by the camera and the image obtained by the distance image sensor, more information can be obtained, and a more accurate gesture operation can be achieved.
[0391] The electronic device 800A may also include a vibration mechanism used as a bone conduction headset. For example, any one or more of the display unit 820, the frame 821, and the mounting unit 823 may adopt a structure including the vibration mechanism. Thus, there is no need to separately provide audio equipment such as headphones, earphones, or speakers, and the user can enjoy images and sounds by simply installing the electronic device 800A.
[0392] Electronic device 800A and electronic device 800B may both include input terminals. For example, a cable for supplying a video signal from a video output device or the like and power for charging a battery provided in the electronic device may be connected to the input terminal.
[0393] An electronic device according to one embodiment of the present invention may also have a function of wirelessly communicating with earphone 750. Earphone 750 includes a communication unit (not shown) and has a wireless communication function. Earphone 750 can receive information (such as sound data) from the electronic device through the wireless communication function. For example, Fig.16A The electronic device 700A shown has a function of transmitting information to the headset 750 through a wireless communication function. In addition, for example Fig. 16C The electronic device 800A shown has a function of transmitting information to the headset 750 through a wireless communication function.
[0394] In addition, the electronic device may include an earphone unit. Fig. 16B The electronic device 700B shown includes an earphone unit 727. For example, a structure in which the earphone unit 727 and the control unit are connected in a wired manner may be adopted. A part of the wiring connecting the earphone unit 727 and the control unit may also be arranged inside the frame 721 or the mounting portion 723.
[0395] same, Fig.16DThe electronic device 800B shown includes an earphone unit 827. For example, a structure in which the earphone unit 827 and the control unit 824 are connected in a wired manner may be adopted. A part of the wiring connecting the earphone unit 827 and the control unit 824 may also be arranged inside the frame 821 or the mounting portion 823. In addition, the earphone unit 827 and the mounting portion 823 may also include magnets. Thus, the earphone unit 827 can be fixed to the mounting portion 823 by magnetic force, and storage becomes easy, which is preferred.
[0396] The electronic device may also include a sound output terminal that can be connected to earphones or headphones. In addition, the electronic device may also include one or both of a sound input terminal and a sound input mechanism. As the sound input mechanism, for example, a sound receiving device such as a microphone may be used. By providing the sound input mechanism to the electronic device, the electronic device can have the so-called earphone function.
[0397] As described above, as electronic devices according to one embodiment of the present invention, both glasses-type (electronic devices 700A and 700B, etc.) and goggles-type (electronic devices 800A and 800B, etc.) are preferable.
[0398] In addition, the electronic device according to one embodiment of the present invention can transmit information to the headset in a wired or wireless manner.
[0399] Fig.17A The electronic device 6500 shown is a portable information terminal device that can be used as a smartphone.
[0400] The electronic device 6500 includes a housing 6501, a display portion 6502, a power button 6503, a button 6504, a speaker 6505, a microphone 6506, a camera 6507, a light source 6508, and the like. The display portion 6502 has a touch panel function.
[0401] The display device of one embodiment of the present invention can be used as the display portion 6502. Thus, a highly reliable electronic device can be achieved.
[0402] Fig. 17B 6506 is a schematic cross-sectional view of an end portion of a housing 6501 on the microphone 6506 side.
[0403] A light-transmitting protective component 6510 is provided on one side of the display surface of the frame 6501, and a display panel 6511, an optical component 6512, a touch sensor panel 6513, a printed circuit board 6517, a battery 6518, etc. are provided in the space surrounded by the frame 6501 and the protective component 6510.
[0404] The display panel 6511 , the optical member 6512 , and the touch sensor panel 6513 are fixed to the protective member 6510 using an adhesive layer (not shown).
[0405] In a region outside the display portion 6502, a portion of the display panel 6511 is folded back, and the folded back portion is connected to an FPC 6515. An IC 6516 is mounted on the FPC 6515. The FPC 6515 is connected to a terminal provided on a printed circuit board 6517.
[0406] The display panel 6511 can use a display device of one embodiment of the present invention. Thus, an extremely lightweight electronic device can be realized. In addition, since the display panel 6511 is extremely thin, a large-capacity battery 6518 can be installed while suppressing the thickness of the electronic device. In addition, by folding a portion of the display panel 6511 to provide a connection portion with the FPC 6515 on the back of the pixel portion, an electronic device with a narrow frame can be realized.
[0407] Fig. 17C An example of a television set is shown. In a television set 7100, a display portion 7000 is incorporated in a housing 7171. Here, a structure in which the housing 7171 is supported by a stand 7173 is shown.
[0408] The light-emitting device of one embodiment of the present invention can be used as the display portion 7000. Thus, a highly reliable electronic device can be realized.
[0409] The operation can be performed by using the operation switch provided in the frame 7171 and the remote control operation machine 7151 provided separately. Fig. 17C Alternatively, the display unit 7000 may be provided with a touch sensor, and the television unit 7100 may be operated by touching the display unit 7000 with a finger or the like. In addition, the remote control unit 7151 may be provided with a display unit that displays information output from the remote control unit 7151. By using the operation keys or the touch panel provided in the remote control unit 7151, the channel and volume can be operated, and the image displayed on the display unit 7000 can be operated.
[0410] In addition, the television device 7100 includes a receiver and a modem. The receiver can receive general television broadcasts. Furthermore, the modem can be connected to a wired or wireless communication network to perform one-way (from a sender to a receiver) or two-way (between a sender and a receiver or between receivers, etc.) information communication.
[0411] Fig.17D 1 shows an example of a notebook personal computer. The notebook personal computer 7200 includes a housing 7211 , a keyboard 7212 , a pointing device 7213 , an external connection port 7214 , and the like. A display portion 7000 is incorporated in the housing 7211 .
[0412] The light-emitting device of one embodiment of the present invention can be used as the display portion 7000. Thus, a highly reliable electronic device can be realized.
[0413] Fig.17E and Fig.17F An example of digital signage is shown.
[0414] Fig.17E The digital signage 7300 shown includes a housing 7301, a display portion 7000, a speaker 7303, etc. In addition, an LED lamp, operation keys (including a power switch or an operation switch), a connection terminal, various sensors, a microphone, etc. may be included.
[0415] Fig.17F The digital signage 7400 is shown to be disposed on a cylindrical pillar 7401. The digital signage 7400 includes a display unit 7000 disposed along a curved surface of the pillar 7401.
[0416] exist Fig.17E and Fig.17F In the embodiment of the present invention, the display device according to one embodiment of the present invention can be used for the display portion 7000. Thus, a highly reliable electronic device can be achieved.
[0417] The larger the display unit 7000 is, the more information can be provided at one time. The larger the display unit 7000 is, the easier it is to attract people's attention, for example, the advertising effect can be improved.
[0418] By using a touch panel for the display unit 7000, not only can a static image or a dynamic image be displayed on the display unit 7000, but the user can also intuitively operate it, which is preferred. In addition, when used for providing information such as route information or traffic information, the ease of use can be improved through intuitive operation.
[0419] like Fig.17E and Fig.17F As shown, the digital signage 7300 or the digital signage 7400 can preferably be linked with the information terminal device 7311 or the information terminal device 7411 such as a smartphone carried by the user through wireless communication. For example, the advertising information displayed on the display unit 7000 can be displayed on the screen of the information terminal device 7311 or the information terminal device 7411. In addition, by operating the information terminal device 7311 or the information terminal device 7411, the display of the display unit 7000 can be switched.
[0420] Furthermore, the game can be executed on the digital signage 7300 or the digital signage 7400 using the screen of the information terminal device 7311 or the information terminal device 7411 as an operation unit (controller). Thus, an unspecified number of users can participate in the game at the same time and enjoy the game.
[0421] This embodiment mode can be combined with other embodiment modes or examples as appropriate. In addition, in this specification, when a plurality of configuration examples are shown in one embodiment mode, the configuration examples can be combined as appropriate. [Example 1]
[0422] In this example, characteristics of a tandem light-emitting device obtained by a method for manufacturing a light-emitting device according to one embodiment of the present invention are described by comparing light-emitting devices 1 to 4 and comparative light-emitting device 5. Structural formulas of organic compounds used in this example are shown below.
[0423] [Chemical formula 4]
[0424] (Method for Manufacturing Light Emitting Device 1) First, an alloy containing silver (Ag), palladium (Pd) and copper (Cu) (APC for short) is deposited on a glass substrate as a reflective electrode with a thickness of 100 nm by sputtering, and then indium tin oxide (ITSO) containing silicon oxide is deposited as a transparent electrode with a thickness of 100 nm by sputtering to form a first electrode 101. The electrode area is 4 mm 2 (2 mm×2 mm) In addition, the transparent electrode is used as an anode, and can be considered as the first electrode 101 in combination with the above-mentioned reflective electrode.
[0425] Next, as a pretreatment for forming a light-emitting device on the substrate, the substrate surface was washed with water, baked at 200° C. for 1 hour, and then subjected to UV ozone treatment for 370 seconds.
[0426] Then, the substrate is placed inside the chamber and the pressure is reduced to 10 -4 Pa in a vacuum evaporation device, and in a heating chamber in the vacuum evaporation device, heat treatment is performed at a temperature of 170° C. for 30 minutes, and then the substrate is cooled for about 30 minutes.
[0427] Next, the substrate is fixed on a bracket provided in a vacuum evaporation device in a manner such that the surface on which the first electrode 101 is formed faces downward, and N-(biphenyl-4-yl)-N-[4-(9-phenyl-9H-carbazole-3-yl)phenyl]-9,9-dimethyl-9H-fluorene-2-amine (abbreviated as: PCBBiF) represented by the above structural formula (i) and an electron acceptor material containing fluorine with a molecular weight of 672 (OCHD-003) are co-evaporated on the first electrode 101 by a method of evaporation in a weight ratio of 1:0.03 (=PCBBiF:OCHD-003) and a thickness of 10 nm, thereby forming a hole injection layer.
[0428] PCBBiF was evaporated on the hole injection layer to a thickness of 70 nm, thereby forming a first hole transport layer.
[0429] Next, 4,8-bis[3-(dibenzothiophene-4-yl)phenyl]-[1]benzofurano[3,2-d]pyrimidine (abbreviated as 4,8mDBtP2Bfpm) represented by the above structural formula (ii), 9-(2-naphthyl)-9'-phenyl-9H,9'H-3,3'-bicarbazole (abbreviated as βNCCP) represented by the above structural formula (iii) and [2-d3-methyl-( The first light-emitting layer is formed by co-evaporation in a weight ratio of 0.5:0.5:0.1 (=4,8mDBtP2Bfpm:βNCCP:Ir(ppy)2(mbfpypy-d3)) and a thickness of 40nm.
[0430] Next, 2-{3-[3-(N-phenyl-9H-carbazole-3-yl)-9H-carbazole-9-yl]phenyl}dibenzo[f,h]quinoxaline (abbreviation: 2mPCCzPDBq) represented by the above structural formula (v) was evaporated in a thickness of 10 nm to form a first electron transport layer.
[0431] After forming the first electron transport layer, 2,2'-(1,3-phenylene)bis(9-phenyl-1,10-phenanthroline) (abbreviated as mPPhen2P) represented by the above structural formula (vi) is evaporated in a thickness of 20 nm, and then lithium oxide (Li2O) is evaporated in a thickness of 0.3 nm, thereby forming an N-type layer. Next, copper phthalocyanine (abbreviated as CuPc) represented by the above structural formula (vii) is deposited in a thickness of 2 nm to form an electron relay layer (ER layer). And, PCBBiF and OCHD-003 are co-evaporated in a weight ratio of 1:0.15 (PCBBiF:OCHD-003) and a thickness of 10 nm to form a P-type layer, thereby forming an intermediate layer including an N-type layer, an ER layer and a P-type layer.
[0432] PCBBiF was evaporated on the intermediate layer to a thickness of 40 nm, thereby forming a second hole transport layer.
[0433] On the second hole transport layer, 4,8mDBtP2Bfpm, βNCCP and Ir(ppy)2(mbfpypy-d3) were co-evaporated in a weight ratio of 0.5:0.5:0.1 (=4,8mDBtP2Bfpm:βNCCP:Ir(ppy)2(mbfpypy-d3)) and a thickness of 40nm to form a second light-emitting layer.
[0434] Then, after 2mPCCzPDBq was evaporated in a thickness of 20 nm and mPPhen2P was evaporated in a thickness of 20 nm to form a second electron transport layer, the formed organic compound layers (hole injection layer, first hole transport layer, first light-emitting layer, first electron transport layer, intermediate layer, second hole transport layer, second light-emitting layer and second electron transport layer) were processed by photolithography.
[0435] <<Processing by Photolithography>> First, the substrate was taken out of the vacuum deposition device and exposed to the atmosphere, and then aluminum oxide was deposited to a thickness of 30 nm by the ALD method using trimethylaluminum (TMA) as a precursor and water vapor as an oxidant, thereby forming a first sacrificial layer.
[0436] Then, a composite oxide containing indium, gallium, zinc, and oxygen (abbreviated as IGZO) was deposited on the first sacrificial layer by a sputtering method to a thickness of 50 nm, thereby forming a second sacrificial layer.
[0437] Next, a resist was formed on the second sacrificial layer using a photoresist, and processing was performed by photolithography so as to form a slit with a width of 3 μm at a position 3.5 μm away from the end of the first electrode.
[0438] Specifically, the second sacrificial layer is processed using a solution containing phosphoric acid with a resist as a mask, and then the first sacrificial layer is processed using an etching gas containing trifluoromethane (CHF3) and helium (He) at a flow ratio of CHF3:He=1:9. Then, the second electron transport layer, the second light-emitting layer, the second hole transport layer, the intermediate layer, the first electron transport layer, the first light-emitting layer, the first hole transport layer, and the hole injection layer are processed using an etching gas containing oxygen (O2). The above is a processing step using photolithography. After the processing, the second sacrificial layer and the first sacrificial layer are removed using a chemical solution to expose the second electron transport layer.
[0439] <<Heat Treatment>> After the second electron transport layer is exposed, the substrate is placed inside the decompression to 10 -4 Pa in a vacuum deposition device, and heat treatment was performed at 80° C. for 1 hour in a heating chamber in the vacuum deposition device.
[0440] After cooling, the sample is placed back into the vacuum evaporation device, and lithium fluoride (LiF) and ytterbium (Yb) are co-evaporated on the second electron transport layer in a volume ratio of 1:1 (=LiF:Yb) to form an electron injection layer 115, and finally silver (Ag) and magnesium (Mg) are co-evaporated in a volume ratio of 1:0.1 and a thickness of 15 nm to form a second electrode 102, thereby manufacturing a light-emitting device 1.
[0441] The second electrode 102 is a semi-transmissive-semi-reflective electrode having a function of reflecting light and a function of transmitting light. The light-emitting device of this embodiment is a tandem light-emitting device having a top emission structure for extracting light from the second electrode 102. In addition, 4,4',4"-(benzene-1,3,5-triyl)tris(dibenzothiophene) (abbreviated as DBT3P-II) represented by the above structural formula (viii) is evaporated on the second electrode 102 as a cap layer with a thickness of 70 nm to improve the light extraction efficiency.
[0442] (Method of Manufacturing Light Emitting Devices 2 to 4) The temperature of the heat treatment after exposing the second electron transport layer after the processing step using the photolithography method was 100° C. for the light emitting device 2, 110° C. for the light emitting device 3, and 120° C. for the light emitting device 4. The light emitting devices 2 to 4 were manufactured in the same manner as the light emitting device 1 except for the temperature of the heat treatment.
[0443] Note that a light-emitting device whose temperature is 80°C after the second sacrificial layer and the first sacrificial layer are removed and the second electron transport layer is exposed is sometimes referred to as a light-emitting device 1 (80°C), a light-emitting device whose temperature is 100°C is referred to as a light-emitting device 2 (100°C), a light-emitting device whose temperature is 110°C is referred to as a light-emitting device 3 (110°C), and a light-emitting device whose temperature is 120°C is referred to as a light-emitting device 4 (120°C).
[0444] (Manufacturing Method of Comparative Light Emitting Device 5) The difference between the comparative light-emitting device 5 and the light-emitting devices 1 to 4 is that in the comparative light-emitting device 5, after the second electron transport layer is formed without performing the processing step using the photolithography method in the light-emitting device 1, the electron injection layer is directly formed, and then the cap layer is formed. That is, the comparative light-emitting device 5 is a light-emitting device manufactured by a continuous vacuum process. Other than this, it is manufactured in the same manner as the light-emitting devices 1 to 4.
[0445] The device structures of light-emitting devices 1 to 4 and comparative light-emitting device 5 are shown in the following table.
[0446] [Table 1]
[0447] In a glove box with a nitrogen atmosphere, the light-emitting devices 1 to 4 and the comparison light-emitting device 5 are sealed using a glass substrate without exposing them to the atmosphere (UV-curing sealing material is applied around the device, and only the sealing material is irradiated with UV without irradiating the light-emitting device, and heat-treated at 80°C for 1 hour under atmospheric pressure), and then the initial characteristics of each light-emitting device are measured.
[0448] Fig.18 The luminance-current density characteristics of the light emitting devices 1 to 4 and the comparative light emitting device 5 are shown. Fig.19 The brightness-voltage characteristics are shown. Fig. 20 The current efficiency-brightness characteristics are shown. Fig.21 The current density-voltage characteristics are shown. Fig. 22 The current efficiency-current density characteristics are shown. Fig.23 The emission spectrum is shown below. In addition, the current density is 50 mA / cm 2 Note that the brightness, CIE chromaticity, and emission spectrum were measured at room temperature using a spectroradiometer (SR-UL1R manufactured by Topcon).
[0449] [Table 2]
[0450] Depend on Figures 18 to 23 It can be seen that the comparative light-emitting device 5, which is a light-emitting device manufactured by a continuous vacuum process without a processing step using photolithography, is a light-emitting device that exhibits good characteristics.
[0451] On the other hand, from Fig. 20 , Fig. 22 As can be seen from the above table, the current efficiency of the light-emitting device 1 (80°C), which is a light-emitting device that has undergone a processing step using photolithography, is lower than that of the comparative light-emitting device 5. In addition, it can be seen that the current efficiency of the light-emitting device 2 (100°C), the light-emitting device 3 (110°C), and the light-emitting device 4 (120°C) is higher than that of the light-emitting device 1 (80°C). Therefore, the temperature of the heat treatment after exposing the second electron transport layer is preferably 100°C or more, and more preferably 100°C or more and 120°C or less.
[0452] In addition, during the heat treatment, the second electron transport layer is exposed. Therefore, in order to suppress damage to the organic compound contained in the second electron transport layer, the temperature of the heat treatment is preferably 100°C or more and lower than the glass transition temperature of the organic compound contained in the second electron transport layer. In addition, the glass transition temperature of mPPhen2P of the organic compound contained in the second electron transport layer was measured by differential scanning calorimetry using DSC8500 manufactured by PerkinElmer, Inc., and the result was 135°C.
[0453] The reason for the low current efficiency of light-emitting device 1 (80°C) is that the organic compound layer containing alkali metals or their compounds is exposed to water, oxygen, etc. in the atmosphere. However, by performing a heating treatment at a temperature above 100°C in light-emitting device 2 (100°C), light-emitting device 3 (110°C), and light-emitting device 4 (120°C), water, oxygen, etc. in the organic compound layer containing alkali metals or their compounds are removed, and the current efficiency is improved.
[0454] Note that when comparing light-emitting device 2 (100°C), light-emitting device 3 (110°C), and light-emitting device 4 (120°C), light-emitting device 2 (100°C) has the highest current efficiency, followed by light-emitting device 3 (110°C) which has the second highest current efficiency. Therefore, it can be said that the temperature of the heat treatment after exposing the second electron transport layer is preferably 100°C or more and 110°C or less.
[0455] In addition, from Fig.19 , Fig.21 As can be seen from the above table, the driving voltage of light-emitting device 1 (80°C) and light-emitting device 2 (100°C), which are light-emitting devices that have undergone a processing step using photolithography, is higher than that of comparative light-emitting device 5. On the other hand, it can be seen that the driving voltage of light-emitting device 3 (110°C) and light-emitting device 4 (120°C) is reduced compared with light-emitting device 1 (80°C) and light-emitting device 2 (100°C). Therefore, it can also be said that the temperature of the heat treatment after exposing the second electron transport layer is preferably above 110°C and below 120°C.
[0456] The reason why the driving voltage of light-emitting device 1 (80°C) and light-emitting device 2 (100°C) increases compared to comparison light-emitting device 5 is that the organic compound layer containing alkali metals or their compounds is exposed to the influence of water, oxygen, etc. in the atmosphere and is heated during the processing step of photolithography. By performing a heating treatment at 110°C or above in light-emitting device 3 (110°C) and light-emitting device 4 (120°C), water, oxygen, etc. in the organic compound layer containing alkali metals or their compounds are removed, thereby suppressing the increase in driving voltage.
[0457] In this way, it can be confirmed that even after a manufacturing method using photolithography, a method for manufacturing a light-emitting device of one embodiment of the present invention, which removes the second sacrificial layer and the first sacrificial layer and exposes the second electron transport layer, and then performs a heat treatment at a temperature of 100°C or above, more preferably 100°C or above and 120°C or below, or 110°C or above and 120°C, can manufacture a light-emitting device that shows high current efficiency and has a suppressed increase in driving voltage. [Example 2]
[0458] In this example, characteristics of a reference light-emitting device 6 and a comparative device 7, which are single-type light-emitting devices manufactured to illustrate a method for manufacturing a light-emitting device according to one embodiment of the present invention, are described. Structural formulas of organic compounds used in this example are shown below.
[0459] [Chemical formula 5]
[0460] (Method for manufacturing reference light emitting device 6) Reference light-emitting device 6 is a single-type light-emitting device, which includes a hole transport layer (thickness of 50 nm), a light-emitting layer, and an electron transport layer (total thickness of 30 nm) instead of the first hole transport layer (thickness of 70 nm), the first light-emitting layer, and the second electron transport layer (total thickness of 40 nm) in light-emitting device 1, and does not include the first electron transport layer, the intermediate layer, the second hole transport layer, and the second light-emitting layer, and [2-d3-methyl-8-(2-pyridyl-κN)benzofurano[2,3-b]pyridine-κC]bis[2-(5-d3-methyl-2-pyridyl-κN2)phenyl-κC]iridium (III) (abbreviated as: Ir(5mppy-d3)2(mbfpypy-d3)) represented by the above structural formula (ix) is used for the light-emitting layer instead of Ir(ppy)2(mbfpypy-d3) used for the first light-emitting layer in light-emitting device 1. Other than that, it is manufactured in the same manner as light-emitting device 1. In addition, the temperature of the heat treatment after removing the second sacrificial layer and the first sacrificial layer to expose the electron transport layer was 80°C.
[0461] (Manufacturing Method of Comparative Light Emitting Device 7) The difference between the comparative light-emitting device 7 and the reference light-emitting device 6 is that the comparative light-emitting device 7 does not perform the processing using the photolithography method in the reference light-emitting device 6, and the electron injection layer is directly formed after the electron transport layer is formed, and then the cap layer is formed. That is, the comparative light-emitting device 7 is a light-emitting device manufactured by a continuous vacuum process. Other than this, it is manufactured in the same manner as the reference light-emitting device 6.
[0462] The device structures of the reference light emitting device 6 and the comparative light emitting device 7 are shown in the following table.
[0463] [Table 3]
[0464] In a glove box with a nitrogen atmosphere, a sealing treatment is performed using a glass substrate in such a manner that the reference light-emitting device 6 and the comparison light-emitting device 7 are not exposed to the atmosphere (a UV-curable sealing material is applied around the device, and only the sealing material is irradiated with UV without irradiating the light-emitting device, and heat-treated at 80°C for 1 hour under atmospheric pressure), and then the initial characteristics of each light-emitting device are measured.
[0465] Fig.24 The brightness-current density characteristics of the light emitting device 6 and the comparative light emitting device 7 are shown. Fig.25 The brightness-voltage characteristics are shown. Fig.26 The current efficiency-brightness characteristics are shown. Fig. 27 The current density-voltage characteristics are shown. Fig.28 The emission spectrum is shown below. In addition, the current density is 50 mA / cm 2 Note that the brightness, CIE chromaticity, and emission spectrum were measured at room temperature using a spectroradiometer (SR-UL1R manufactured by Topcon).
[0466] [Table 4]
[0467] Depend on Figures 24 to 28 As can be seen from the above table, both the reference light-emitting device 6 and the comparative light-emitting device 7 are light-emitting devices exhibiting good characteristics.
[0468] Although the characteristics of the light emitting device 1 (80°C) of the tandem light emitting device subjected to the processing steps using the photolithography method shown in Example 1 are lower than those of the comparative light emitting device 5, the characteristics of the reference light emitting device 6 (80°C) of the single-type light emitting device subjected to the processing steps using the photolithography method manufactured in this example are not changed compared with the comparative light emitting device 7. Therefore, since the influence of water, oxygen, etc. is small in the single-type device not including the layer containing the alkali metal or its compound as the intermediate layer, the characteristics are not easily degraded even if the heat treatment at 100°C or more is not performed after the electron transport layer is exposed.
[0469] This shows that in the method for manufacturing a light-emitting device according to one embodiment of the present invention, the step of exposing the electron transport layer after processing by photolithography and performing heat treatment at 100° C. or higher is particularly effective in the case of a tandem device. [Example 3]
[0470] In this embodiment, in order to illustrate a method for manufacturing a light-emitting device according to one embodiment of the present invention, results of TDS (Thermal Desorption Spectroscopy) analysis tests on Sample 1, Comparative Sample 2, and Comparative Sample 3, each of which has an organic compound layer formed on a glass substrate, are shown.
[0471] Note that the organic compound used for Sample 1, Comparative Sample 2, and Comparative Sample 3 in this embodiment is the same as the organic compound used for the light-emitting device in Embodiment 1, so the structural formula is omitted in this embodiment.
[0472] (Manufacturing method of sample 1) Sample 1 is a sample in which an organic compound layer similar to that of the light-emitting device 1 is formed on a glass substrate, that is, a sample imitating an organic compound layer of a tandem light-emitting device containing an alkali metal or an alkali metal compound as an intermediate layer. Note that the thickness of a part of the layer is different from that of the light-emitting device 1. In addition, in Sample 1, no processing step using photolithography is performed.
[0473] (Comparison sample 2) Comparative Sample 2 is a sample that does not include Li2O and the ER layer as part of the N-type layer in Sample 1. The other parts are manufactured in the same manner as Sample 1. That is, Comparative Sample 2 is a sample that simulates a structure in which a layer containing an alkali metal or an alkali metal compound is removed from the organic compound layer of a tandem light-emitting device.
[0474] (Manufacturing method of comparative sample 3) Comparative sample 3 is a sample that does not include the first electron transport layer, the intermediate layer, the second hole transport layer, and the second light-emitting layer in sample 1, that is, a sample that simulates the organic compound layer of a single-type light-emitting device.
[0475] The structures of the organic compound layers of Sample 1, Comparative Sample 2, Sample 3, and Sample 4 are shown below.
[0476] [Table 5]
[0477] TDS analysis was performed on the above-mentioned sample 1, comparative sample 2, sample 3 and sample 4. TDS is an analysis device in which a quadrupole mass analyzer (quadrupole mass spectrometer) is used to detect and identify gas components that are separated and generated when the sample is heated in a high vacuum and the temperature of the sample is increased, and when TDS is used, gases and molecules separated from the surface and inside of the sample can be observed. TDS manufactured by Electronic Science Co., Ltd. (product name: EMD-WA1000S) was used, and the measurement conditions were a temperature increase of about 5°C / min.
[0478] Figure 29 to Figure 31 The TDS analysis results of Sample 1, Comparative Sample 2, and Comparative Sample 3 are shown. Figure 29 to Figure 31 The results are shown when the mass-to-charge ratio (M / z) corresponding to water molecules is 18. In each figure, the horizontal axis represents the substrate temperature, and the vertical axis represents the detection intensity.
[0479] Depend on Fig.29 and Fig.30It can be seen that peaks appear near 60°C and 100°C in Sample 1, but the peaks are smaller in all temperature ranges in Comparative Sample 2. This shows that the organic compound layer of Sample 1 including the layer including the alkali metal or the alkali metal compound absorbs more water than the organic compound layer of Comparative Sample 2 not including the layer including the alkali metal or the alkali metal compound.
[0480] In addition, by Fig.29 and Fig.31 It can be seen that peaks appear near 60°C and 100°C in Comparative Sample 3, but the detection intensity of Sample 1 at these temperatures is stronger than that of Sample 1. This shows that the organic compound layer of Sample 1, which simulates a tandem light-emitting device containing an alkali metal or an alkali metal compound as an intermediate layer, adsorbs more water than the organic compound layer of Comparative Sample 3, which simulates a single-type light-emitting device without an intermediate layer.
[0481] The above results show that the tandem organic compound layer having a layer containing an alkali metal or its compound as an intermediate layer easily absorbs water. It is therefore known that the step of removing water from the organic compound layer according to the method for manufacturing a light-emitting device of one embodiment of the present invention is particularly effective in a tandem light-emitting device having a layer containing an alkali metal or its compound as an intermediate layer.
[0482] In addition, from this result, it can be seen that in the tandem light-emitting device, water can be removed by performing a heat treatment at 100° C. to 120° C. after exposing the second electron transport layer. Therefore, it can be seen that the temperature of the heat treatment after exposing the second electron transport layer is preferably 100° C. to 120° C. [Explanation of symbols]
[0483] 100A: display device, 100: display device, 101: first electrode, 102: second electrode, 103: organic compound layer, 103f: organic compound film, 103B: organic compound layer, 103Bf: organic compound film, 103G: organic compound layer, 103Gf: organic compound film, 103R: organic compound layer, 103Rf: organic compound film, 104: common layer, 105: substrate, 110B: sub-pixel, 110G: sub-pixel, 110R: sub-pixel, 110: sub-pixel, 111: hole injection layer, 112_1: first hole transport layer, 112_2: second hole transport layer, 113_1: first light-emitting layer, 113_2: second light-emitting layer, 1 13: light-emitting layer, 114_1: first electron transport layer, 114_2: second electron transport layer, 115: electron injection layer, 116_1: first intermediate layer, 116_2: second intermediate layer, 116: intermediate layer, 117: P-type layer, 118: electron relay layer, 119: N-type layer, 120: substrate, 122: resin layer, 125f: inorganic insulating film, 125: inorganic insulating layer, 127a: insulating layer, 127f: insulating film, 127: insulating layer, 130B: light-emitting device, 130G: light-emitting device, 130R: light-emitting device, 130: light-emitting device, 131: protective layer, 132B: coloring layer, 132G: coloring layer, 132R: coloring layer, 140: connecting portion, 14 1: region, 151a: conductive layer, 151B: conductive layer, 151b: conductive layer, 151C: conductive layer, 151c: conductive layer, 151f: conductive film, 151G: conductive layer, 151R: conductive layer, 151: conductive layer, 152a: conductive layer, 152B: conductive layer, 152b: conductive layer, 152C: conductive layer, 152c: conductive layer, 152f: conductive film, 152G: conductive layer, 152R: conductive layer, 152: conductive layer, 155: common electrode, 156B: insulating layer, 156C: insulating layer, 156f: insulating film, 156G: insulating layer, 156R: insulating layer, 156: insulating layer, 158: sacrificial layer, 158f: sacrificial film, 158B: Sacrificial layer, 158Bf: sacrificial film, 158G: sacrificial layer, 158Gf: sacrificial film, 158R: sacrificial layer, 158Rf: sacrificial film, 159: mask layer, 159f: mask film, 159B: mask layer, 159Bf: mask film, 159G: mask layer, 159Gf: mask film, 159R: mask layer, 159Rf: mask film, 171: insulating layer, 172: conductive layer, 173: insulating layer, 174: insulating layer, 175: insulating layer, 176: plug, 177: pixel portion, 178: pixel, 179: conductive layer, 190: resist mask, 190B: resist mask, 190G: resist mask, 190R: resist mask, 191: resist mask,240: capacitor, 241: conductive layer, 243: insulating layer, 245: conductive layer, 254: insulating layer, 255: insulating layer, 256: plug, 261: insulating layer, 271: plug, 280: display module, 281: display unit, 282: circuit unit, 283a: pixel circuit, 283: pixel circuit unit, 284a: pixel, 284: pixel unit, 285: terminal unit, 286: wiring unit, 290: FPC, 291: substrate, 292: substrate, 301: substrate, 310: transistor, 311: conductive layer, 312: low resistance region, 313: insulating layer, 314: insulating layer, 315: element separation layer, 501: first light-emitting unit, 501f: organic compound film, 502b: organic compound layer, 502: second light-emitting unit, 502f: organic compound film, 503: third light-emitting unit, 700A: electronic device, 700B: electronic device, 721: frame, 723: mounting portion, 727: earphone portion, 750: earphone, 751: display panel, 753: optical member, 756: display region, 757: frame, 758: nose pad, 800A: electronic device, 800B: electronic device, 820: display unit, 821: housing, 822: communication unit, 823: mounting unit, 824: control unit, 825: imaging unit, 827: earphone unit, 832: lens, 6500: electronic device, 6501: housing, 6502: display unit, 6503: power button, 6504: button, 6505: speaker, 6506: microphone, 6507: camera, 6508: light source, 6510: protection member, 6511: display panel, 6512: optical member, 6513: touch sensor panel, 6515: touch sensor panel, 6516: touch sensor panel, 6517: touch sensor panel, 6518: touch sensor panel, 6519: touch sensor panel, 6520: touch sensor panel, 6521: touch sensor panel, 6523: touch sensor panel, 6524: touch sensor panel, 6525: touch sensor panel, 6526: touch sensor panel, 6527: touch sensor panel, 6528: touch sensor panel, 6529: touch sensor panel, 6530: touch sensor panel, 6531: touch sensor panel, 6532: touch sensor panel, 6533: touch sensor panel, 6534: touch sensor panel, 6535: touch sensor panel, 6536: touch sensor panel, 6537: touch sensor panel, 6538: touch sensor panel, 6539: touch sensor panel, 6540: touch sensor panel, 6541: touch sensor panel, 6542: touch sensor panel, 6543: touch sensor panel, 6544: touch sensor panel, 6545: touch sensor panel, 6546: touch sensor panel, 6547: touch sensor panel, 6548: :FPC、6516:IC、6517:Printed circuit board、6518:Battery、7000:Display unit、7100:TV device、7151:Remote control unit、7171:Frame、7173:Stand、7200:Notebook personal computer、7211:Frame、7212:Keyboard、7213:Pointing device、7214:External connection port、7300:Digital signage、7301:Frame、7303:Speaker、7311:Information terminal equipment、7400:Digital signage、7401:Pillar、7411:Information terminal equipment、
Claims
1. A method for manufacturing a light emitting device, comprising the following steps: forming a first electrode; forming an organic compound layer including an intermediate layer including an alkali metal or an alkali metal compound between the first light-emitting layer and the second light-emitting layer on the first electrode; Processing the organic compound layer by photolithography; performing a heat treatment; and A second electrode is formed so as to cover the first electrode and the organic compound layer.
2. A method for manufacturing a light emitting device, comprising the following steps: forming a first electrode; forming an organic compound layer including an intermediate layer including an alkali metal or an alkali metal compound between the first light-emitting layer and the second light-emitting layer on the first electrode; forming a sacrificial layer on the organic compound layer; forming a mask from a resist on the sacrificial layer; processing the organic compound layer by photolithography; removing at least a portion of the sacrificial layer and performing a heat treatment; as well as A second electrode is formed so as to cover the first electrode and the organic compound layer.
3. A method for manufacturing a light emitting device, comprising the following steps: forming a first electrode; forming an organic compound layer including an intermediate layer including an alkali metal or an alkali metal compound between the first light-emitting layer and the second light-emitting layer on the first electrode; forming a sacrificial layer on the organic compound layer; forming a mask from a resist on the sacrificial layer; processing the organic compound layer by photolithography; forming an insulating layer covering the side surfaces of the organic compound layer; removing at least a portion of the sacrificial layer and performing a heat treatment; as well as A second electrode is formed so as to cover the first electrode and the organic compound layer.
4. A method for manufacturing a light emitting device according to any one of claims 1 to 3, The heating treatment is performed at a temperature of 100° C. or higher.
5. A method for manufacturing a light emitting device according to any one of claims 1 to 3, The heating treatment is performed at a temperature of 100° C. or higher and 120° C. or lower.
6. A method for manufacturing a light emitting device according to any one of claims 1 to 3, The heat treatment is performed at a temperature of 100° C. or higher and lower than a glass transition temperature of an organic compound contained on a top surface of the organic compound layer.