High-efficiency single-crystal PERC battery and preparation process thereof

By introducing multi-layer heterojunction structures, including photonic crystal layer, transparent conductive oxide layer and quantum well structure, the problem of insufficient photo utilization and stability of existing batteries is solved, and the photoelectric conversion efficiency is significantly improved and Overall performance.

CN118899348APending Publication Date: 2024-11-05CECEP SOLAR ENERGY TECH (ZHENJIANG) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410944291.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-15
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

Existing PERC batteries still have room for improvement in light utilization and stability, especially in the context of growing demands for cost control and efficiency improvement.

Method used

High-efficiency single crystal PERC cell design with multi-layer heterojunction structure includes adding a photonic crystal layer composed of nanomaterials between the silicon wafer and the silicon nitride anti-reflection film, and adding a transparent conductive oxide layer to improve ohmic contact and light reflection. And a quantum well structure is provided at the edge of the battery to reduce edge leakage.

Benefits of technology

Significantly improves light utilization efficiency and battery performance, by enhancing the absorption and scattering of light at specific wavelengths, the secondary absorption opportunity of light is increased, ohmic contact and current transmission is improved, edge leakage is reduced, and overall performance and output efficiency is improved. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118899348A_ABST
    Figure CN118899348A_ABST
Patent Text Reader

Abstract

The high-efficiency single-crystal PERC battery comprises a silicon wafer, a silicon nitride antireflection film and a metal electrode, a photonic crystal layer made of nanometer materials is arranged between the silicon wafer and the front silicon nitride antireflection film, a transparent conductive oxide layer is arranged on the contact surface of the metal electrode, and a quantum well structure is arranged on the edge of the battery. Compared with the existing cell structure and preparation mode, the scheme can significantly improve the utilization efficiency of sunlight, and the photonic crystal layer can enhance the absorption and scattering of light with specific wavelength, so that more light energy can be effectively utilized, thereby improving the photoelectric conversion efficiency of the cell. And meanwhile, secondary absorption is increased, the transparent conductive oxide layer on the back side reflects the light which is not absorbed and returns to the interior of the cell, and the utilization rate of the light is further improved. In addition, ohmic contact is improved, the transparent conductive oxide layer and the metal electrode form good ohmic contact, and current transmission is facilitated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This article relates to a high-efficiency single-crystal PERC battery and its preparation process. Background Art

[0002] Traditional solar cell structures have some efficiency limitations, such as incomplete light absorption, high carrier recombination rate, etc. In order to improve efficiency, people are constantly exploring new technical approaches.

[0003] Before PERC technology, there may be some relatively simple battery structures, but they have room for improvement in conversion efficiency, etc. With the development of technology, PERC technology has effectively reduced carrier recombination and increased the open circuit voltage and short circuit current of the battery by adding a passivation layer on the back of the battery, thereby improving the overall efficiency.

[0004] However, with the continuous improvement of requirements and the continuous control of costs, the light utilization rate and stability of existing PERC cells need to be further enhanced. Summary of the invention

[0005] In order to solve the above problems, the present invention provides a high-efficiency single crystal PERC cell structure with a multi-layer heterojunction structure.

[0006] This type of cell structure adds some special interlayers on the basis of the conventional PERC cell structure. A photonic crystal layer made of nanomaterials is added between the silicon wafer and the front silicon nitride anti-reflection film to enhance the absorption and scattering of light of a specific wavelength and improve the light utilization efficiency; a transparent conductive oxide layer is added on the back to form a good ohmic contact with the metal electrode. At the same time, this layer also has a certain light reflection function, reflecting the unabsorbed light back into the cell for secondary absorption; a circle of quantum well structure is set at the edge of the cell to reduce edge leakage and improve the overall performance of the cell.

[0007] A high-efficiency single-crystal PERC battery comprises a silicon wafer, a silicon nitride anti-reflection film, and a metal electrode. A photonic crystal layer made of nanomaterials is provided between the silicon wafer and the front silicon nitride anti-reflection film, a transparent conductive oxide layer is provided on the contact surface of the metal electrode, and a quantum well structure is provided at the edge of the battery.

[0008] Furthermore, the photonic crystal layer is composed of a plurality of zinc oxide nanoparticles arranged in a periodic manner.

[0009] Furthermore, the conductive oxide layer is a transparent layer with a certain thickness formed by depositing transparent conductive oxide by magnetron sputtering.

[0010] A preparation process of a high-efficiency single crystal PERC cell comprises the following steps:

[0011] S1. Silicon wafer processing:

[0012] Cleaning and texturing of single crystal silicon wafers;

[0013] S2. Preparation of photonic crystal layer:

[0014] A high-refractive-index nanomaterial colloidal solution is prepared by chemical synthesis, and then evenly coated on a silicon wafer by spin coating or spray coating, and then dried and heat treated to form a photonic crystal layer;

[0015] S3, Silicon nitride anti-reflection film deposition:

[0016] Depositing a silicon nitride anti-reflection film on the photonic crystal layer by plasma enhanced chemical vapor deposition;

[0017] S4. Preparation of transparent conductive oxide layer:

[0018] Depositing a transparent conductive oxide by magnetron sputtering to form the layer on the contact surface of the metal electrode;

[0019] S5. Preparation of quantum well structure:

[0020] Using techniques such as molecular beam epitaxy or metal organic chemical vapor deposition, semiconductor material layers with different energy band structures are alternately grown at the edge of the battery to construct a quantum well structure, during which the growth conditions and thickness of each layer are controlled;

[0021] S6. Metal electrode production:

[0022] Finally, the metal electrodes were made by screen printing.

[0023] In order to improve the coating strength of the photonic crystal layer, the preparation method of the photonic crystal layer includes the following steps:

[0024] S11, preparing zinc oxide nanoparticles by chemical synthesis method;

[0025] S12, using self-assembly technology, uniformly dispersing zinc oxide nanoparticles in a solvent to form a colloidal solution;

[0026] S13, coating the colloidal solution uniformly on the surface of the battery by spin coating or spray coating;

[0027] S14, after steps such as drying and heat treatment, the nanoparticles are made to form a stable periodic nanocolumn structure photonic crystal layer.

[0028] In order to improve the contact strength and stability of the conductive oxide layer, the preparation method of the conductive oxide layer includes the following:

[0029] S21. Construct the basic environment of physical vapor deposition such as magnetron sputtering;

[0030] S22, placing an indium tin oxide target into a vacuum chamber for sputtering deposition to form a uniform, transparent conductive layer;

[0031] S23, placing the conductive layer in a reaction chamber, alternately introducing a precursor containing aluminum elements and a reaction gas, and depositing a thin and uniform aluminum oxide layer as a protective layer;

[0032] The preparation steps of the quantum well structure include the following steps:

[0033] S31, alternately growing narrow bandgap materials and wide bandgap materials on the edge of the battery to form a multilayer structure;

[0034] S32, controlling the thickness of each layer;

[0035] S33. After the growth is completed, heat treatment is performed to remove the residual internal stress.

[0036] In step S33, the specific order of heat treatment is: put the battery with quantum well structure into the heat treatment furnace, increase the temperature to 500°C at a heating rate of 5-10°C / min, and keep it at this temperature for 30 minutes, then cool it down at 2-5°C / min until it cools to room temperature. During the heat treatment, the protective atmosphere is nitrogen. The narrow bandgap material and the wide bandgap material are GaN and InN respectively.

[0037] Beneficial effects:

[0038] Compared with the existing battery structure and preparation method, this solution can significantly improve the light utilization efficiency. The photonic crystal layer can enhance the absorption and scattering of light of a specific wavelength, so that more light energy can be effectively utilized, thereby improving the photoelectric conversion efficiency of the battery. At the same time, it increases the opportunity for secondary absorption, and the transparent conductive oxide layer on the back reflects the unabsorbed light back into the battery, further improving the utilization rate of light. It also improves the ohmic contact, in which the transparent conductive oxide layer forms a good ohmic contact with the metal electrode, which is conducive to current transmission.

[0039] Moreover, the edge quantum well structure can reduce edge leakage, improve the overall performance and stability of the battery, and ultimately significantly improve the overall performance and output efficiency of the monocrystalline PERC battery. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] Figure 1 It is a preparation flow chart of a high-efficiency single-crystal PERC battery. DETAILED DESCRIPTION

[0041] In order to deepen the understanding of the present invention, the present invention will be further described in detail below with reference to embodiments and drawings. The embodiments are only used to explain the present invention and do not constitute a limitation on the protection scope of the present invention.

[0042] Embodiment 1:

[0043] A high-efficiency single-crystal PERC battery comprises a silicon wafer, a silicon nitride anti-reflection film, and a metal electrode. A photonic crystal layer made of nanomaterials is provided between the silicon wafer and the front silicon nitride anti-reflection film, a transparent conductive oxide layer is provided on the contact surface of the metal electrode, and a quantum well structure is provided at the edge of the battery.

[0044] The preparation process comprises the following steps:

[0045] S1. Silicon wafer processing:

[0046] The monocrystalline silicon wafers were cleaned and textured, wherein deionized water was used for multiple cleanings during the cleaning process, and sodium hydroxide solution was used for treatment at 80° C. for 30 minutes during the texturing.

[0047] S2. Preparation of photonic crystal layer:

[0048] S21. Select zinc oxide as a precursor, use distilled water to dissolve the precursor, and adjust it by adding ammonia water and dilute acid at 90 degrees Celsius, and slowly add a precipitant under stirring to make the zinc ions in the solution react with the hydroxide ions to precipitate. After maintaining for a period of time, control the crystal growth and obtain a sediment, and then calcine the sediment to obtain zinc oxide nanoparticles of a certain particle size, wherein the diameter of the particles is controlled to be about 50 nanometers.

[0049] S22. Using self-assembly technology, zinc oxide nanoparticles are evenly dispersed in a solvent to form a colloidal solution.

[0050] S23, uniformly dispersing the particles in an ethanol solvent to form a colloidal solution, and uniformly coating the colloidal solution on the battery surface by spin coating at a rotation speed of 3000 rpm;

[0051] S24, after steps such as drying and heat treatment, the nanoparticles are made to form a stable periodic nanocolumn structure photonic crystal layer.

[0052] S3, Silicon nitride anti-reflection film deposition:

[0053] Establish a vacuum state, control the temperature within 350-400 degrees Celsius, and adjust the flow ratio of silane (SiH4) and ammonia (NH3) according to the required silicon nitride film properties. Set the SiH4 flow rate to 100 sccm (standard cubic centimeters per minute) and the NH3 flow rate to 300 sccm. Set the RF generator output power to 500W to 1000W to generate a stable plasma. Deposit a silicon nitride anti-reflection film on the photonic crystal layer;

[0054] S4. Preparation of transparent conductive oxide layer:

[0055] S41. Construct a basic environment for physical vapor deposition such as magnetron sputtering, where the vacuum degree is 10 -6 to 10 -7 Preheat to 200 degrees Celsius.

[0056] S42, placing an indium tin oxide target into a vacuum chamber for sputtering deposition to form a uniform, transparent conductive layer, wherein the protective atmosphere is argon gas, the gas flow rate is 50 sccm, and the DC power supply power is 5KW.

[0057] S43, placing the conductive layer in a reaction chamber, and alternately introducing a precursor containing aluminum elements and a reaction gas at 82 degrees Celsius to deposit a thin and uniform aluminum oxide layer as a protective layer;

[0058] S5. Preparation of quantum well structure:

[0059] S51, alternately growing narrow bandgap materials and wide bandgap materials on the edge of the battery to form a multilayer structure;

[0060] S52, controlling the thickness of each layer;

[0061] S53. After the growth is completed, the battery with the quantum well structure is placed in a heat treatment furnace, and the temperature is raised to 500°C at a heating rate of 6°C / min, and maintained at this temperature for 30 minutes, and then cooled at 2°C / min until it cools to room temperature. During the process, the protective atmosphere is nitrogen. The narrow bandgap material and the wide bandgap material are GaN and InN respectively.

[0062] S6. Metal electrode production:

[0063] Finally, the metal electrodes were made by screen printing.

[0064] Embodiment 2:

[0065] A high-efficiency single-crystal PERC battery comprises a silicon wafer, a silicon nitride anti-reflection film, and a metal electrode. A photonic crystal layer made of nanomaterials is provided between the silicon wafer and the front silicon nitride anti-reflection film, a transparent conductive oxide layer is provided on the contact surface of the metal electrode, and a quantum well structure is provided at the edge of the battery.

[0066] The preparation process comprises the following steps:

[0067] S1. Silicon wafer processing:

[0068] The single crystal silicon wafer is cleaned and textured. During the cleaning process, an acidic solution is first used to remove the oxide layer on the surface, and then deionized water is used for multiple cleanings. During the texturing process, a sodium hydroxide solution is used at 80°C for 30 minutes.

[0069] S2. Preparation of photonic crystal layer:

[0070] S21. Select zinc oxide as a precursor, use distilled water to dissolve the precursor, and adjust it by adding ammonia water and dilute acid at 90 degrees Celsius, slowly add a precipitant under stirring, so that the zinc ions in the solution react with the hydroxide ions to precipitate, keep it for a period of time, control the crystal growth, and obtain a sediment, and then calcine the sediment to obtain zinc oxide nanoparticles of a certain particle size, wherein the diameter of the particles is controlled to be about 40 nanometers.

[0071] S22. Using self-assembly technology, zinc oxide nanoparticles are evenly dispersed in a solvent to form a colloidal solution.

[0072] S23, uniformly dispersing the particles in an ethanol solvent to form a colloidal solution, and uniformly coating the colloidal solution on the battery surface by spraying, controlling the spraying to be uniform;

[0073] S24, after steps such as drying and heat treatment, the nanoparticles are made to form a stable periodic nanocolumn structure photonic crystal layer.

[0074] S3, Silicon nitride anti-reflection film deposition:

[0075] Establish a vacuum state, control the temperature within 360-380 degrees Celsius, and adjust the flow ratio of silane (SiH4) and ammonia (NH3) according to the required silicon nitride film properties. Set the SiH4 flow rate to 100 sccm (standard cubic centimeters per minute) and the NH3 flow rate to 300 sccm. Set the RF generator output power to 600W to 800W to generate a stable plasma. Deposit a silicon nitride anti-reflection film on the photonic crystal layer;

[0076] S4. Preparation of transparent conductive oxide layer:

[0077] S41. Construct a basic environment for physical vapor deposition such as magnetron sputtering, where the vacuum degree is 10 -6 to 10 -7 Preheat to 200 degrees Celsius.

[0078] S42, placing an indium tin oxide target into a vacuum chamber for sputtering deposition to form a uniform, transparent conductive layer, wherein the protective atmosphere is argon gas, the gas flow rate is 50 sccm, and the DC power supply power is 5KW.

[0079] S43, placing the conductive layer in a reaction chamber, and alternately introducing a precursor containing aluminum elements and a reaction gas at 82 degrees Celsius to deposit a thin and uniform aluminum oxide layer as a protective layer;

[0080] S5. Preparation of quantum well structure:

[0081] S51, alternately growing narrow bandgap materials and wide bandgap materials on the edge of the battery to form a multilayer structure;

[0082] S52, controlling the thickness of each layer;

[0083] S53. After the growth is completed, the battery with the quantum well structure is placed in a heat treatment furnace, and the temperature is raised to 500°C at a heating rate of 5°C / min, and maintained at this temperature for 30 minutes, and then cooled at 3°C / min until it cools to room temperature. During the process, the protective atmosphere is nitrogen. The narrow bandgap material and the wide bandgap material are GaN and InN respectively.

[0084] S6. Metal electrode production:

[0085] Finally, the metal electrodes were made by screen printing.

[0086] Compared with the existing single-crystal PERC cells, the light utilization rate of the bifacial PERC cells in this solution is greatly improved, and can be used in low-light environments, especially when used in areas with insufficient light. It can make greater use of local light and thus obtain higher power conversion efficiency.

[0087] Specifically, the conversion efficiency in Example 1 and Example 2 can reach 26%-27%, with Voc increased to more than 720mV and Jsc exceeding 40A / m2. Under ideal conditions of use, FF may be close to 90% or higher. Compared with traditional products, the attenuation in the first year is controlled to no more than 2%, and the attenuation in subsequent years is ensured to be less than 0.7%.

[0088] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A high-efficiency single crystal PERC cell, comprising a silicon wafer, a silicon nitride anti-reflection film, and a metal electrode, characterized in that: A photonic crystal layer made of nanomaterials is provided between the silicon wafer and the front silicon nitride anti-reflection film, a transparent conductive oxide layer is provided on the contact surface of the metal electrode, and a quantum well structure is provided at the edge of the battery.

2. A high-efficiency single crystal PERC cell according to claim 1, characterized in that: The photonic crystal layer is composed of a plurality of zinc oxide nanoparticles arranged in a periodic manner.

3. A high-efficiency single crystal PERC cell according to claim 1, characterized in that: The conductive oxide layer is a transparent layer with a certain thickness formed by depositing transparent conductive oxide by magnetron sputtering.

4. A process for preparing a high-efficiency single crystal PERC cell, characterized in that: The following steps are involved: S1. Silicon wafer processing: Cleaning and texturing of single crystal silicon wafers; S2. Preparation of photonic crystal layer: A high-refractive-index nanomaterial colloidal solution is prepared by chemical synthesis, and then evenly coated on a silicon wafer by spin coating or spray coating, and then dried and heat treated to form a photonic crystal layer; S3, Silicon nitride anti-reflection film deposition: Depositing a silicon nitride anti-reflection film on the photonic crystal layer by plasma enhanced chemical vapor deposition; S4. Preparation of transparent conductive oxide layer: Depositing a transparent conductive oxide by magnetron sputtering to form the layer on the contact surface of the metal electrode; S5. Preparation of quantum well structure: Using techniques such as molecular beam epitaxy or metal organic chemical vapor deposition, semiconductor material layers with different energy band structures are alternately grown at the edge of the battery to construct a quantum well structure, during which the growth conditions and thickness of each layer are controlled; S6. Metal electrode production: Finally, the metal electrodes were made by screen printing.

5. The process for preparing a high-efficiency single crystal PERC cell according to claim 4, characterized in that: The method for preparing the photonic crystal layer comprises: the following: S11, preparing zinc oxide nanoparticles by chemical synthesis method; S12, using self-assembly technology, uniformly dispersing zinc oxide nanoparticles in a solvent to form a colloidal solution; S13, coating the colloidal solution uniformly on the surface of the battery by spin coating or spray coating; S14, after steps such as drying and heat treatment, the nanoparticles are made to form a stable periodic nanocolumn structure photonic crystal layer.

6. The process for preparing a high-efficiency single crystal PERC cell according to claim 4, characterized in that: The method for preparing the conductive oxide layer comprises the following steps: S21. Construct the basic environment of physical vapor deposition such as magnetron sputtering; S22, placing an indium tin oxide target into a vacuum chamber for sputtering deposition to form a uniform, transparent conductive layer; S23, placing the conductive layer into a reaction chamber, alternately introducing a precursor containing aluminum elements and a reaction gas, and depositing a thin and uniform aluminum oxide layer as a protective layer.

7. A process for preparing a high-efficiency single crystal PERC cell according to any one of claims 4 to 6, characterized in that: The preparation steps of the quantum well structure include the following steps: S31, alternately growing narrow bandgap materials and wide bandgap materials on the edge of the battery to form a multilayer structure; S32, controlling the thickness of each layer; S33. After the growth is completed, heat treatment is performed to remove the residual internal stress.

8. The process for preparing a high-efficiency single crystal PERC cell according to claim 7, characterized in that: In step S33, the specific order of heat treatment is: put the battery with quantum well structure into the heat treatment furnace, increase the temperature to 500°C at a heating rate of 5-10°C / min, and keep it at this temperature for 30 minutes, then cool it down at 2-5°C / min until it cools to room temperature.

9. A process for preparing a high-efficiency single crystal PERC cell according to claim 8, characterized in that: During the heat treatment, the protective atmosphere was nitrogen.

10. The process for preparing a high-efficiency single crystal PERC cell according to claim 7, characterized in that: The narrow bandgap material and the wide bandgap material are GaN and InN respectively.