Ultra-narrow line width CF manufacturing method and liquid crystal display device
By irradiating UV light on the negative photoresist of the CF substrate and exposing and developing high-temperature main curing in the liquid crystal display process, the problem of negative photoresist residue is solved, and line width narrowing and transmittance increase is achieved.
Patent Information
- Application Number
- CN202411353134.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-26
- Publication Date
- 2024-11-08
AI Technical Summary
In the existing liquid crystal display process, negative photoresist can easily form a positive trapezoidal shape after curing, resulting in a small slope angle on both sides of the line width, forming a BM photoresist residue, affecting transmittance.
The negative photoresist of the CF substrate is exposed to UV light and developed, which prompts the surface curing reaction again, maintains the original shape of the line width pattern, and performs main curing in high-temperature equipment to avoid deformation or collapse, thereby reducing BM glue residue , increase the slope angle.
The line width is narrowed, the transmittance of the LCD display is improved, and the market demand for high-precision products is met.
Smart Images

Figure CN118915404A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of display panel manufacturing, and in particular to a method for manufacturing a CF with an ultra-narrow line width and a liquid crystal display device. Background Art
[0002] With the development of display technology, flat display devices such as liquid crystal displays (LCD) have been widely used in various consumer electronic products such as mobile phones, televisions, personal digital assistants, digital cameras, laptops, desktop computers, etc. due to their advantages of high image quality, power saving, thin body and wide application range, becoming the mainstream of display devices.
[0003] Currently, the quality requirements for LCD displays are getting higher and higher, such as high resolution, high contrast, ultra-wide viewing angle, etc. At the same time, the industry development is also constantly expanding, not only involving mobile phones and TV displays, but also including many wearable device displays, such as AR displays.
[0004] As the quality requirements for LCDs become increasingly stringent, the precision requirements for production equipment and product materials also increase accordingly, so the investment and production costs of LCD products continue to increase, but the current equipment or process status can no longer meet the market's requirements for products, mainly in the curing process of negative photoresist. After the main curing, the negative photoresist is in a positive trapezoidal shape with a small slope angle on both sides of the line width, forming a layer of BM photoresist residue on the surface of the glass substrate, which will affect the transmittance of this area. If the equipment and process are not optimized, the market opportunity for high-precision products will be lost first. Summary of the invention
[0005] In the existing LCD process, when curing the photoresist, BM photoresist residues are present, resulting in reduced transmittance of the LCD.
[0006] In view of the above problems, a method for manufacturing CF with ultra-narrow line width and a liquid crystal display device are proposed. After the negative photoresist on the CF substrate is exposed and developed by UV light, a surface curing reaction occurs again, so that the line width pattern maintains its original state after exposure and development. When the main curing is performed and the negative photoresist material is baked in a high-temperature device, it is no longer prone to deformation or collapse, so that there is no BM glue residue at the bottom of the line width and the slope angle becomes larger, thereby achieving the product requirement of narrowing the line width based on the original process equipment.
[0007] In a first aspect, a method for manufacturing a CF with an ultra-narrow line width includes: Step 100, cleaning the white glass substrate and then applying glue to obtain a first CF substrate, and pre-curing the first CF substrate to obtain a second CF substrate; Step 200, sequentially performing exposure processing and development processing on the second CF substrate to obtain a third CF substrate; Step 300, irradiating UV light uniformly on the third CF substrate to perform UV curing to obtain a fourth CF substrate; Step 400: perform leveling treatment on the fourth CF substrate, and then place the fourth CF substrate into a preheated oven for primary curing to obtain a final CF substrate.
[0008] In conjunction with the method for manufacturing a CF with an ultra-narrow line width according to the first aspect of the present invention, in a first possible implementation manner, step 100 includes: Step 110, performing UV cleaning on the white glass substrate; Step 120 , the white glass substrate after UV cleaning is washed with DI water, and then coated with photoresist.
[0009] In combination with the first possible implementation manner of the first aspect of the present invention, in a second possible implementation manner, step 110 includes: Step 111, placing the white glass substrate on a transmission table of a UV cleaning device; Step 112: Use ultraviolet rays emitted by the UV light source of the UV cleaning equipment to irradiate the surface of the white glass substrate to decompose organic matter and perform UV cleaning.
[0010] In combination with the second possible implementation manner of the first aspect of the present invention, in a third possible implementation manner, step 200 includes: Step 210: making a mask plate, and placing the mask plate and the second CF substrate into an exposure machine for exposure; Step 220: placing the exposed second CF substrate into a developer for development.
[0011] In combination with the third possible implementation manner of the first aspect of the present invention, in a fourth possible implementation manner, step 210 includes: Step 211, manufacturing a mask plate according to the CF substrate pattern, and designing a light-transmitting area and a light-shielding area corresponding to the pattern on the mask plate; Step 212: accurately align the mask plate and the second CF substrate, and then place them in an exposure machine for exposure.
[0012] In combination with the fourth possible implementation manner of the first aspect of the present invention, in a fifth possible implementation manner, step 300 includes: Step 310, coating the pattern of the third CF substrate with UV glue; Step 320: Place the third CF substrate coated with UV glue into a UV curing device for UV curing.
[0013] In combination with the fifth possible implementation manner of the first aspect of the present invention, in a sixth possible implementation manner, step 310 includes: Step 311, uniformly coating the UV glue on the pattern of the third CF substrate; Step 312: performing a leveling process on the third CF substrate coated with UV glue.
[0014] In combination with the sixth possible implementation manner of the first aspect of the present invention, in a seventh possible implementation manner, step 320 includes: Step 321, positioning the third CF substrate after being placed in the UV curing device; Step 322: Evenly irradiate the UV light source onto the UV glue pattern to perform UV curing.
[0015] In combination with the seventh possible implementation manner of the first aspect of the present invention, in an eighth possible implementation manner, step 400 includes: Step 410, adjusting the position and spacing of the fourth CF substrate in the oven so that the pattern of the fourth CF substrate is fully cured; Step 420: The solidified fourth CF substrate is taken out and cooled to obtain the final CF substrate.
[0016] In a second aspect, a liquid crystal display device is provided, comprising a CF substrate manufactured by the ultra-narrow linewidth CF manufacturing method described in the first aspect.
[0017] The ultra-narrow line width CF manufacturing method and liquid crystal display device described in the present invention are implemented. After the negative photoresist on the CF substrate is exposed and developed by UV light, a surface curing reaction occurs again, so that the line width pattern maintains its original state after exposure and development. When the main curing is performed and the negative photoresist material is baked in a high-temperature device, it is no longer prone to deformation or collapse, so that there is no BM glue residue at the bottom of the line width, the slope angle becomes larger, and the product requirement of narrowing the line width is achieved based on the original process equipment. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0019] Figure 1 is a schematic diagram of the line width of black photoresist in the prior art; Figure 2 Schematic diagram of the UV curing process in the present invention; Figure 3 Schematic diagram of the line width of the black photoresist in the present invention; Figure 4 It is a first schematic diagram of the method for manufacturing a CF with ultra-narrow line width in the present invention; Figure 5 It is a second schematic diagram of the method for manufacturing a CF with ultra-narrow line width in the present invention; Figure 6 It is a third schematic diagram of the method for manufacturing a CF with ultra-narrow line width in the present invention; Figure 7 A fourth schematic diagram of the method for manufacturing a CF with an ultra-narrow line width in the present invention; Figure 8 It is a fifth schematic diagram of the method for manufacturing a CF with an ultra-narrow line width in the present invention; Fig. 9 It is a sixth schematic diagram of the method for manufacturing a CF with an ultra-narrow line width in the present invention; Fig.10 It is the seventh schematic diagram of the method for manufacturing a CF with ultra-narrow line width in the present invention; Fig.11 The eighth schematic diagram of the method for manufacturing a CF with ultra-narrow line width in the present invention; Fig.12 This is the ninth schematic diagram of the method for manufacturing a CF with an ultra-narrow line width in the present invention. DETAILED DESCRIPTION
[0020] The following will be combined with the accompanying drawings in the invention to clearly and completely describe the technical solutions in the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments in the present invention, other embodiments obtained by ordinary technicians in this field without creative work are all within the scope of protection of the present invention.
[0021] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.
[0022] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it can be directly on the other element or indirectly on the other element. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.
[0023] It should be understood that the orientation or position relationship indicated by terms such as "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0024] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0025] Glossary UV: Ultraviolet light, wavelength 365nm CF:Color Filter BM: High impedance photoresist material OVEN: Main curing 230℃ / 30min Tape: Slope Angle Glass: White glass, thickness 0.5mm In the existing LCD process, when curing the photoresist, BM photoresist residues are present, resulting in reduced transmittance of the LCD.
[0026] In view of the above problems, a method for manufacturing a CF with an ultra-narrow line width and a liquid crystal display device are proposed.
[0027] In the first aspect, a method for manufacturing a CF with an ultra-narrow line width, such as Figure 4 , Figure 4 The first schematic diagram of the method for manufacturing a CF with ultra-narrow line width in the present invention comprises: Step 100: clean the white glass substrate and then apply glue to obtain a first CF substrate, and pre-cure the first CF substrate to obtain a second CF substrate.
[0028] Due to the characteristics of CF negative photoresist, after OVEN (main curing 230℃ / 30min), the line width structure of the negative photoresist is in a positive trapezoidal shape, and the tape angle 10 (slope angle) is small (e.g. Figure 1 ), if the slope angle 10 on both sides of the line width is small, a layer of BM glue (black photoresist) will be formed on the surface of the glass substrate. Figure 1 , Figure 1Schematic diagram of the line width of black photoresist in the prior art; it will affect the transmittance of the area.
[0029] In a preferred embodiment, Figure 5 , Figure 5 It is a second schematic diagram of the method for manufacturing a CF with an ultra-narrow line width in the present invention; step 100 includes: step 110, UV cleaning the white glass substrate; step 120, DI water washing the white glass substrate after UV cleaning, and then coating it with photoresist.
[0030] In a preferred embodiment, Figure 6 , Figure 6 This is the third schematic diagram of the method for producing a CF with an ultra-narrow line width in the present invention; step 110 includes: step 111, placing a white glass substrate on a transmission table of a UV cleaning device; step 112, using ultraviolet rays emitted by a UV light source of the UV cleaning device to irradiate the surface of the white substrate to decompose organic matter and perform UV cleaning.
[0031] In the embodiment of the present application, the overall production process is: Input white glass substrate - UV cleaning - DI water washing - glue coating - pre-curing - exposure - development - UV curing - main curing (OVEN process) - output the final CF substrate.
[0032] In an application scenario of this embodiment, dust on the surface of a white glass substrate is removed by UV cleaning. Particles, etc. If there are many pollutants on the substrate, a longer UV cleaning time needs to be set. Adjust the transmission speed of the substrate in the UV cleaning equipment to ensure that the substrate can be evenly irradiated with UV. Too fast a transmission speed may result in incomplete cleaning of some areas, while too slow a transmission speed will affect the cleaning efficiency. If the UV cleaning equipment generates ozone to assist in cleaning, the concentration of ozone needs to be controlled. It is usually more appropriate to control the ozone concentration within the range of 100-130ppm. Too much or too little ozone may affect the cleaning effect. Place the prepared white glass substrate on the transmission device of the UV cleaning equipment to ensure that the substrate can pass through the UV irradiation area smoothly. Start the UV cleaning equipment, and the ultraviolet rays emitted by the UV light source begin to irradiate the surface of the substrate. The energy of ultraviolet rays can directly open and cut the covalent bonds in organic molecules, activate the organic molecules, and decompose them into ions, free atoms, excited molecules, etc.; at the same time, the oxygen molecules in the air will produce ozone and atomic oxygen after absorbing ultraviolet light of a specific wavelength. Atomic oxygen has a strong oxidizing effect and reacts with the activated organic molecules to generate volatile gases (such as CO2, CO, H2O, NO, etc.) that escape from the surface of the object, thereby achieving the purpose of cleaning.
[0033] Step 200: Expose and develop the second CF substrate in sequence to obtain a third CF substrate.
[0034] In some preferred embodiments, Figure 7 , Figure 7 It is the fourth schematic diagram of the method for manufacturing a CF with an ultra-narrow line width in the present invention; step 200 includes: step 210, manufacturing a mask plate, and placing the mask plate and the second CF substrate into an exposure machine for exposure; step 220, placing the exposed second CF substrate into a developer for development treatment.
[0035] In some preferred embodiments, Figure 8 , Figure 8 This is the fifth schematic diagram of the method for producing a CF with an ultra-narrow line width in the present invention; step 210 includes: step 211, producing a mask plate according to the CF substrate pattern, and designing a light-transmitting area and a light-shielding area corresponding to the pattern on the mask plate; step 212, accurately aligning the mask plate with the second CF substrate, and then placing it in an exposure machine for exposure.
[0036] In an application scenario of this embodiment, a layer of negative photoresist is evenly coated on the cleaned substrate. The coating method can be spin coating, scraping coating, spraying, etc. to ensure that the thickness of the photosensitive adhesive layer is uniform. After the photosensitive adhesive is coated, the substrate needs to be dried to remove the solvent in the photosensitive adhesive and solidify the photosensitive adhesive layer. The drying temperature and time must be strictly controlled. Too high a temperature or too long a time may cause the performance of the photosensitive adhesive layer to change, affecting the exposure effect.
[0037] In an application scenario of the present embodiment, a corresponding mask is made according to the pattern and color information required by the second CF substrate. There are light-transmitting areas and light-shielding areas on the mask. The light-transmitting areas correspond to the parts that need to be exposed, and the light-shielding areas are used to block light. The mask is accurately aligned with the second CF substrate coated with photosensitive adhesive to ensure that the pattern on the mask is accurately aligned with the corresponding position on the substrate. The accuracy of the alignment directly affects the accuracy and quality of the pattern on the second CF substrate, and automatic alignment equipment or optical alignment systems are usually used for alignment operations. The aligned mask and the second CF substrate are placed in an exposure machine, and the photosensitive adhesive layer is exposed using light of a specific wavelength and intensity. The exposure time and intensity need to be adjusted according to the characteristics of the photosensitive adhesive and the process requirements to ensure that the photosensitive adhesive layer can form a clear pattern after exposure.
[0038] Step 300: Evenly irradiate UV light on the third CF substrate to perform UV curing to obtain a fourth CF substrate.
[0039] In some preferred embodiments, Fig. 9 , Fig. 9The sixth schematic diagram of the method for manufacturing ultra-narrow line width CF of the present invention; step 300 includes: step 310, coating the pattern of the third CF substrate with UV glue; step 320, placing the third CF substrate coated with UV glue into a UV curing device for UV curing, such as Figure 2 and Figure 3 , Figure 2 is a schematic diagram of the UV curing process in the present invention, Figure 3 Schematic diagram of the line width of the black photoresist in the present invention.
[0040] In some preferred embodiments, Fig.10 , Fig.10 This is the seventh schematic diagram of the method for manufacturing a CF with an ultra-narrow line width in the present invention; step 310 includes step 311, uniformly coating UV glue on the pattern of the third CF substrate; step 312, performing a leveling treatment on the third CF substrate coated with UV glue.
[0041] In an application scenario of this embodiment, the selected UV glue or UV paint is evenly coated on the third CF substrate. The coating method can be selected according to the specific situation, such as spraying, spin coating, scraping, etc. The coating thickness should be uniform to avoid being too thick or too thin. After the UV material is applied, it needs to be leveled on the substrate to eliminate bubbles and flow marks in the coating and improve the flatness and uniformity of the coating.
[0042] In some preferred embodiments, Fig.11 , Fig.11 This is the eighth schematic diagram of the method for producing CF with ultra-narrow line width in the present invention; step 320 includes: step 321, positioning the third CF substrate after being placed in the UV curing device; step 322, evenly irradiating the UV light source on the UV glue pattern for UV curing.
[0043] In an application scenario of this embodiment, the third CF substrate coated with UV material is placed in a UV curing device and positioned to ensure that the UV light source can accurately irradiate the coating. The wavelength of the UV light source is generally between 200-400nm. The curing time is usually between a few seconds and a few minutes, and the intensity is generally between tens and hundreds of milliwatts per square centimeter. If the curing time is too short or the intensity is too low, the coating may not be completely cured; if the curing time is too long or the intensity is too high, the substrate or coating may be damaged. During the curing process, ensure that the UV light source can evenly irradiate all parts of the coating to avoid incomplete local curing or over-curing. Uniform irradiation can be achieved by adjusting the position, angle, and number of UV light sources.
[0044] Step 400, leveling the fourth CF substrate, and then placing the fourth CF substrate in a preheated oven for primary curing to obtain a final CF substrate. After the negative photoresist of the CF substrate is exposed and developed by UV light, a surface curing reaction occurs again, so that the line width pattern maintains its original state after exposure and development, so that when the negative photoresist material is baked in a high-temperature device for primary curing, it is no longer prone to deformation or collapse, so that there is no BM glue residue at the bottom of the line width, and the slope angle becomes larger, thereby achieving the product requirement of narrowing the line width based on the original process equipment.
[0045] In some preferred embodiments, Fig.12 , Fig.12 The ninth schematic diagram of the method for manufacturing ultra-narrow line width CF in the present invention. Step 400 includes: step 410, adjusting the position and spacing of the fourth CF substrate in the oven so that the pattern of the fourth CF substrate is fully solidified; step 420, taking out the solidified fourth CF substrate and cooling it to obtain the final CF substrate.
[0046] In an application scenario of the present embodiment, the fourth CF substrate is placed in a preheated oven and cured according to the set curing process parameters. When placing the substrate, pay attention to the placement and spacing of the substrate to ensure that the hot air in the oven can circulate evenly so that all parts of the substrate can be fully cured. Set the temperature curve of the oven. During the curing process, pay close attention to the temperature changes in the oven to ensure that the temperature always remains within the set range. If the temperature is too high, it may cause decomposition, discoloration and other problems in the coating material; if the temperature is too low, the curing may be incomplete, affecting the performance of the coating.
[0047] In a second aspect, a liquid crystal display device is provided, comprising a CF substrate manufactured by the ultra-narrow linewidth CF manufacturing method of the first aspect.
[0048] The present invention implements a method for manufacturing a CF with an ultra-narrow line width and a liquid crystal display device. After the negative photoresist on the CF substrate is exposed and developed by UV light, a surface curing reaction occurs again, so that the line width pattern maintains its original state after exposure and development. When the main curing is performed and the negative photoresist material is baked in a high-temperature device, it is no longer prone to deformation or collapse, so that there is no BM glue residue at the bottom of the line width, the slope angle becomes larger, and the product requirement of narrowing the line width is achieved based on the original process equipment.
[0049] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for manufacturing a CF with an ultra-narrow line width, comprising: Step 100, cleaning the white glass substrate and then applying glue to obtain a first CF substrate, and pre-curing the first CF substrate to obtain a second CF substrate; Step 200, sequentially performing exposure processing and development processing on the second CF substrate to obtain a third CF substrate; Step 300, irradiating UV light uniformly on the third CF substrate to perform UV curing to obtain a fourth CF substrate; Step 400: perform leveling treatment on the fourth CF substrate, and then place the fourth CF substrate into a preheated oven for primary curing to obtain a final CF substrate.
2. The method for manufacturing a CF with an ultra-narrow line width according to claim 1, characterized in that: The step 100 comprises: Step 110, performing UV cleaning on the white glass substrate; Step 120 , the white glass substrate after UV cleaning is washed with DI water, and then coated with photoresist.
3. The method for manufacturing a CF with an ultra-narrow line width according to claim 2, characterized in that: The step 110 includes: Step 111, placing the white glass substrate on a transmission table of a UV cleaning device; Step 112: Use ultraviolet rays emitted by the UV light source of the UV cleaning equipment to irradiate the surface of the white glass substrate to decompose organic matter and perform UV cleaning.
4. The method for manufacturing a CF with an ultra-narrow line width according to claim 3, characterized in that: The step 200 comprises: Step 210: making a mask plate, and placing the mask plate and the second CF substrate into an exposure machine for exposure; Step 220: placing the exposed second CF substrate into a developer for development.
5. The method for manufacturing a CF with an ultra-narrow line width according to claim 4, characterized in that: The step 210 includes: Step 211, manufacturing a mask plate according to the CF substrate pattern, and designing a light-transmitting area and a light-shielding area corresponding to the pattern on the mask plate; Step 212: accurately align the mask plate and the second CF substrate, and then place them in an exposure machine for exposure.
6. The method for manufacturing a CF with an ultra-narrow line width according to claim 5, characterized in that: The step 300 includes: Step 310, coating the pattern of the third CF substrate with UV glue; Step 320: Place the third CF substrate coated with UV glue into a UV curing device for UV curing.
7. The method for manufacturing a CF with an ultra-narrow line width according to claim 6, characterized in that: The step 310 includes: Step 311, uniformly coating the UV glue on the pattern of the third CF substrate; Step 312: performing a leveling process on the third CF substrate coated with UV glue.
8. The method for manufacturing a CF with an ultra-narrow line width according to claim 7, characterized in that: The step 320 includes: Step 321, positioning the third CF substrate after being placed in the UV curing device; Step 322: Evenly irradiate the UV light source onto the UV glue pattern to perform UV curing.
9. The method for manufacturing a CF with an ultra-narrow line width according to claim 8, characterized in that: The step 400 includes: Step 410, adjusting the position and spacing of the fourth CF substrate in the oven so that the pattern of the fourth CF substrate is fully cured; Step 420: The solidified fourth CF substrate is taken out and cooled to obtain the final CF substrate.
10. A liquid crystal display device, characterized in that: It comprises a CF substrate manufactured by the ultra-narrow linewidth CF manufacturing method described in any one of claims 1-9.