Electrochemical cell, electrochemical cell device, module, and module housing device
By covering the conductive oxide film on the metal surface of the fuel cell stack, the release of chromium is suppressed, and the problem of degradation of power generation performance at high temperatures is solved, and the power generation performance and oxidation resistance are improved.
Patent Information
- Application Number
- CN202380027702.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-18
- Filing Date
- 2023-03-17
- Publication Date
- 2024-11-08
Smart Images

Figure CN118922969A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to an electrochemical cell, an electrochemical cell device, a module, and a module receiving device. Background Art
[0002] In recent years, various fuel cell stack devices including a plurality of fuel cells have been proposed as next-generation energy sources. A fuel cell is an electrochemical cell that can generate electricity using a fuel gas such as a hydrogen-containing gas and an oxygen-containing gas such as air.
[0003] Prior Art Literature
[0004] Patent Literature
[0005] Patent Document 1: Japanese Patent Application Publication No. 2015-162357 Summary of the invention
[0006] An electrochemical cell according to one embodiment of the present invention comprises a component part, a metal body and an oxide covering material. The metal body contains chromium and is electrically connected to the component part. The oxide covering material covers the metal body and is exposed to an oxidizing atmosphere. The oxide covering material suppresses the release of chromium into the oxidizing atmosphere. The oxide covering material has at least a first conductive covering material.
[0007] Furthermore, the electrochemical cell device of the present disclosure includes a cell stack including the electrochemical cells described above.
[0008] Furthermore, the module of the present disclosure includes the electrochemical cell device described above and a storage container for storing the electrochemical cell device.
[0009] Furthermore, the module storage device of the present disclosure includes the above-mentioned module; auxiliary equipment for operating the module; and an outer casing for storing the module and the auxiliary equipment. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1A It is a cross-sectional view showing an example of the electrochemical cell according to the first embodiment.
[0011] Figure 1B It is a side view of an example of the electrochemical cell according to the first embodiment as viewed from the air electrode side.
[0012] Figure 2A It is a perspective view showing an example of the cell stack device according to the first embodiment.
[0013] Figure 2B for Figure 2A A cross-sectional view along line XX is shown.
[0014] Figure 2CIt is a top view showing an example of the cell stack device according to the first embodiment.
[0015] Figure 3 It is a perspective view showing the appearance of an example of the module according to the first embodiment.
[0016] Figure 4 It is an exploded perspective view schematically showing an example of the module housing device according to the first embodiment.
[0017] Figure 5 It is a cross-sectional view showing an example of an electrochemical cell according to the second embodiment.
[0018] Figure 6 It is a cross-sectional view showing an example of an electrochemical cell according to the third embodiment.
[0019] Figure 7 It is a cross-sectional view showing an example of an electrochemical cell according to a fourth embodiment.
[0020] Figure 8 It is a cross-sectional view showing an example of an electrochemical cell according to a fifth embodiment.
[0021] Fig. 9 It is a cross-sectional view showing an example of an electrochemical cell according to the sixth embodiment. DETAILED DESCRIPTION
[0022] The above-described fuel cell stack device has room for improvement in terms of enhancing power generation performance.
[0023] Therefore, it is desirable to provide an electrochemical cell, an electrochemical cell device, a module, and a module housing device that can improve performance.
[0024] Hereinafter, embodiments of the electrochemical cell, electrochemical cell device, module, and module housing device disclosed in the present application will be described in detail with reference to the accompanying drawings. The present invention is not limited to the embodiments described below.
[0025] In addition, it should be noted that the drawings are schematic, and the relationship between the dimensions of the elements, the ratio of the elements, etc. may be different from the actual ones. Furthermore, the drawings may also include different parts in the relationship between the dimensions, the ratio, etc.
[0026] [First embodiment]
[0027] <Structure of single cell>
[0028] First, refer to Figure 1A , Figure 1BAs the electrochemical cell involved in the first embodiment, a solid oxide fuel cell is used as an example for explanation. The electrochemical cell device may also include a cell stack having a plurality of electrochemical cells. The electrochemical cell device having a plurality of electrochemical cells is simply referred to as a cell stack device.
[0029] Figure 1A It is a cross-sectional view showing an example of the electrochemical cell according to the first embodiment. Figure 1B FIG. 1 is a side view of an example of the electrochemical cell according to the first embodiment as viewed from the air electrode side. Figure 1A , Figure 1B Part of each structure of the unit cell 1 is shown in an enlarged manner. Hereinafter, an electrochemical unit cell may be simply referred to as a unit cell.
[0030] like Figure 1A As shown, the unit cell 1 includes a metal body 2, an element portion 4, and a sealing material 8. The element portion 4 includes a fuel electrode 5, a solid electrolyte layer 6, and an air electrode 7.
[0031] The metal body 2 has a first surface 201 and a second surface 202 facing each other in the thickness direction T, and a third surface 203 and a fourth surface 204 connecting the first surface 201 and the second surface 202 .
[0032] In addition, the metal body 2 has a gas flow path 2a and an opening 2b. The gas flow path 2a is located between the first surface 201 and the second surface 202, and is a space extending in the length direction L. The opening 2b is a through hole whose first end is open at the first surface 201 and whose second end is connected to the gas flow path 2a. The fuel gas flowing in the gas flow path 2a is supplied to the fuel electrode 5 of the element part 4 through the opening 2b. The diameter of the opening 2b can also be set to 0.1 mm to 0.5 mm, in particular 0.3 mm to 0.4 mm, for example. The opening ratio in the area where the opening 2b is formed can also be set to 10% or more, for example.
[0033] The metal body 2 is a member made of metal containing chromium. In addition, the metal body 2 has electrical conductivity. The metal body 2 is, for example, stainless steel such as ferrite stainless steel and austenite stainless steel with high heat resistance. The metal body 2 may also be, for example, a nickel-chromium alloy or an iron-chromium alloy. The metal body 2 may also contain metal oxides. The metal body 2 may also have a structure in which a plurality of plates such as a plate having a first surface 201 and a plate having a second surface 202 are stacked and the ends are welded.
[0034] The element portion 4 is located on the first surface 201 side of the metal body 2. The element portion 4 is provided so as to face the first surface 201. The element portion 4 is fixed to the metal body 2 via the adhesive material 3 and is supported by the metal body 2.
[0035] The element part 4 has a fuel electrode 5, a solid electrolyte layer 6 and an air electrode 7. The material of the fuel electrode 5 can use generally known materials. The fuel electrode 5 can also use porous conductive ceramics such as calcium oxide, magnesium oxide or ZrO2 in which rare earth element oxides are solid-dissolved, and ceramics including Ni and / or NiO. The rare earth element oxide may also contain a plurality of rare earth elements selected from Sc, Y, La, Nd, Sm, Gd, Dy and Yb. Sometimes calcium oxide, magnesium oxide or ZrO2 in which rare earth element oxides are solid-dissolved is called stabilized zirconia. Stabilized zirconia may also contain partially stabilized zirconia. The fuel electrode 5 contains metal particles. Sometimes the electrode containing metal particles is called the first electrode.
[0036] The solid electrolyte layer 6 is an electrolyte that transfers ions between the fuel electrode 5 and the air electrode 7. The solid electrolyte layer 6 has a gas barrier property, and thus the fuel gas and the oxygen-containing gas are unlikely to leak.
[0037] The material of the solid electrolyte layer 6 may be, for example, ZrO2 in which 3 mol% to 15 mol% of rare earth element oxides are solid-dissolved. The rare earth element oxides may also contain, for example, one or more rare earth elements selected from Sc, Y, La, Nd, Sm, Gd, Dy and Yb. The solid electrolyte layer 6 may also contain, for example, ZrO2 in which Yb, Sc or Gd are solid-dissolved, CeO2 in which La, Nd or Yb are solid-dissolved, BaZrO3 in which Sc or Yb are solid-dissolved, or BaCeO3 in which Sc or Yb are solid-dissolved.
[0038] The air electrode 7 has gas permeability. The open porosity of the air electrode 7 may be, for example, in the range of 20% to 50%, particularly 30% to 50%. The open porosity of the air electrode 7 is sometimes referred to as the void ratio of the air electrode 7 .
[0039] The material of the air electrode 7 is not particularly limited as long as it is a material generally used for air electrodes. The material of the air electrode 7 may be, for example, a conductive ceramic such as a so-called ABO3 type perovskite oxide.
[0040] The material of the air electrode 7 may be, for example, a composite oxide in which Sr (strontium) and La (lanthanum) coexist at the A site. Examples of such a composite oxide include La x Sr 1-x Co y Fe 1-y O3, La x Sr 1-x MnO3, La x Sr 1-x FeO3, La x Sr 1-xCoO3 etc. In addition, 0 < x < 1 and 0 < y < 1. Sometimes, the air electrode 7 is referred to as the second electrode relative to the first electrode containing metal particles.
[0041] In addition, the element part 4 may also have an intermediate layer located between the solid electrolyte layer 6 and the air electrode 7. When the element part 4 has an intermediate layer, the intermediate layer has, for example, the function of a diffusion inhibition layer. If Sr (strontium) contained in the air electrode 7 diffuses into the solid electrolyte layer 6, a resistance layer of SrZrO3 is formed in the relevant solid electrolyte layer 6. By making it difficult for Sr to diffuse into the intermediate layer, it is difficult to form SrZrO3.
[0042] The material of the intermediate layer is not particularly limited as long as it is a material that generally hardly causes diffusion of elements between the air electrode 7 and the solid electrolyte layer 6. The material of the intermediate layer may also contain, for example, cerium oxide (CeO2) in which rare earth elements excluding Ce (cerium) are solid-solved. As the relevant rare earth elements, for example, Gd (gadolinium), Sm (samarium), etc. can also be used.
[0043] The sealing material 8 is located at the end face of the fuel electrode 5. The sealing material 8 has gas barrier properties and is provided to cover the periphery of the fuel electrode 5 to seal the flow of fuel gas between the fuel electrode 5 and the outside. The sealing material 8 may also have, for example, a porosity of 5% or less. By the sealing material 8 having a porosity of 5% or less, it is difficult for fuel gas to flow between the fuel electrode 5 and the outside. The porosity of the sealing material 8 may also be set as, for example, the average value of the porosities in at least any 3 cross-sections of the sealing material 8. As Figure 1A 、 Figure 1B shown, the sealing material 8 may also be located at the end faces of the fuel electrode 5 and the solid electrolyte layer 6.
[0044] The sealing material 8 has electrical insulation properties. Hereinafter, sometimes the electrical insulation properties are only referred to as insulation properties. As the sealing material 8, for example, oxides with low conductivity such as glass can be used. Here, having insulation properties, or having low conductivity means that the conductivity is 1 / 10 or less of that of the solid electrolyte layer 6. The conductivity of the sealing material 8 may also be, for example, 0.2 S / m or less at room temperature (25°C), especially 0.002 S / m or less. The material of the sealing material 8 is, for example, amorphous glass, etc., and may also be crystallized glass. As the crystallized glass, for example, any one of materials such as SiO2-CaO system, MgO-B2O3 system, La203-B203-MgO system, La2O3-B203-ZnO system, SiO2-CaO-ZnO system, etc. can be used, and especially a material of SiO2-MgO system can also be used.
[0045] In addition, the single cell 1 may also have a bonding material 3 located between the metal body 2 and the element portion 4. The bonding material 3 is located between the first surface 201 of the metal body 2 and the fuel electrode 5, and bonds the metal body 2 and the element portion 4. The bonding material 3 has, for example, electrical conductivity. The bonding material 3 may also have, for example, gas permeability. The single cell 1 also has a film containing, for example, chromium oxide (Cr2O3) located between the first surface 201 of the metal body 2 and the bonding material 3.
[0046] The binding material 3 may also include inorganic oxides such as conductive particles such as Ni, TiO2, rare earth element oxides (Y2O3, CeO2, etc.), transition metal oxides (Fe2O3, CuO, etc.). In addition, the binding material 3 may also be arranged to be in contact with the first surface 201 where the opening 2b is not provided. In addition, the fuel electrode 5 may also be fixed to the metal body 2 without the binding material 3.
[0047] However, the first to fourth surfaces 201 to 204 of the metal body 2 that are not in contact with the adhesive 3 or the element portion 4 are exposed to the external space. The external space is the space where the air electrode 7 of the cell 1 is exposed and is filled with oxygen-containing gas. That is, the external space is an oxidizing atmosphere.
[0048] When the cell 1 is used in the above environment, the chromium (Cr) contained in the metal body 2 is released in an oxidizing atmosphere and attached to the element portion 4 during high-temperature operation, which may reduce the power generation performance.
[0049] Therefore, the cell 1 according to the present embodiment further includes an oxide film 9. The oxide film 9 covers the metal body 2 and is exposed in the oxidizing atmosphere. Since the oxide film 9 suppresses the release of chromium from the metal body 2 into the oxidizing atmosphere, the power generation performance of the cell 1 is improved. In addition, since the oxide film 9 makes it difficult for chromium to be released from the metal body 2 into the oxidizing atmosphere, the oxidation resistance and aging resistance of the metal body 2 are improved. The oxide film 9 may be a film that makes it difficult to increase the size of the film including chromium oxide (Cr2O3) located on the surface of the metal body 2.
[0050] The oxide film 9 may also include, for example, a conductive first film 31. The first film 31 is an example of a first covering material. The first film 31 may also have a conductivity of 0.005 S / cm or more. The first film 31 may also include a transition metal oxide, such as manganese (Mn). The first film 31 may also include, for example, a composite oxide including Mn. The composite oxide including Mn may also have a spinel structure. The first film 31 may also include, for example, CoMn2O4, MnCo2O4, Mn 1.5 Co 1.5O4, ZnMnCoO4, etc. In the spinel-type composite oxide containing Mn and Co and / or Zn as described above, the composition ratio of Mn, Co and / or Zn can be arbitrarily selected. As a result, the internal resistance of the element portion 4 is reduced compared to the case without the first film 31, thereby improving the power generation performance of the single cell 1. In addition, the first film 31 may also contain, for example, trace amounts of Cr2O3, Al2O3, ZrO2, etc. The composite oxide containing Mn may also contain, for example, Al, Zr, etc.
[0051] The above-mentioned single cell 1 is obtained as follows. A laminated body in which a molded sheet of, for example, a fuel electrode 5 and a molded sheet of a solid electrolyte layer 6 are laminated and sintered, and a metal body 2 having a first film 31 (or a molded film of the first film 31) is prepared. The surface of the fuel electrode 5 of the laminated body is bonded to the first surface 201 having the opening 2b of the metal body 2 via the adhesive material 3. Thereafter, an intermediate layer and an air electrode 7 are formed on the solid electrolyte layer 6, and a sealing material 8 is further provided on the side of the element part 4, thereby obtaining the single cell 1. The sealing material 8 may be located only on the side of the fuel electrode 5 in the element part 4. The sealing material 8 may be located on at least a portion of the side of the solid electrolyte layer 6, and further on at least a portion of the surface of the solid electrolyte layer 6. The sealing material 8 may be located on the adhesive material 3, or may be located on at least a portion of the first film 31. The first film 31 may not be arranged on the first surface 201 having the opening 2b of the metal body 2.
[0052] The stacked body of the fuel electrode 5 and the solid electrolyte layer 6 can also be produced, for example, as follows. A mixture of Ni or NiO powder, stabilized zirconium oxide powder, an organic solvent, and a binder is sheet-formed to obtain a sheet-formed body of the fuel electrode 5. A mixture of stabilized zirconium oxide powder, an organic solvent, and a binder is sheet-formed on the sheet-formed body of the fuel electrode 5 to obtain a stacked body. The obtained stacked body is sintered to obtain a stacked body of the fuel electrode 5 and the solid electrolyte layer 6.
[0053] The first film 31 can also be formed as follows. A paste in which a powder of a composite oxide containing, for example, Mn, a solvent, and a binder are mixed is applied to the surface of the metal body 2 that does not have the opening 2b, and dried to form a molded film of the first film 31. Furthermore, a composite body is obtained by bonding the surface of the fuel electrode 5 of the stack to the surface of the metal body 2 having the opening 2b using a bonding material 3, and the composite body is sintered at, for example, 900°C to 1200°C to obtain a joint body of the metal body 2 and the stack having the first film 31. Furthermore, a molded body of an intermediate layer is formed on the surface of the solid electrolyte layer 6 of the joint body, and the intermediate layer is formed by sintering at, for example, 1000°C to 1200°C. Furthermore, a molded body of the air electrode 7 is formed on the intermediate layer, and the air electrode 7 is formed by sintering at, for example, 1000°C to 1200°C, thereby obtaining a single cell 1.
[0054] In addition, the fuel electrode 5, the solid electrolyte layer 6, the intermediate layer, and the air electrode 7 may be directly formed in sequence on the first surface 201 having the opening 2b of the metal body 2 having the first film 31 or the molded film of the first film 31. In addition, a laminated sheet, such as the element portion 4, may be prepared in advance, bonded to the first surface 201 having the opening 2b of the metal body 2, and then sintered.
[0055] The sealing material 8 can be formed by applying the above-mentioned glass powder paste to a predetermined location, drying it, and then performing a heat treatment at, for example, 800° C. to 900° C.
[0056] <Structure of Single Cell Stack Device>
[0057] Next, refer to Figure 2A to Figure 2C A cell stack device according to the present embodiment using the above-described cell 1 will be described. Figure 2A is a perspective view showing an example of a cell stack device according to the first embodiment. Figure 2B for Figure 2A The cross-sectional view of line XX is shown. Figure 2C It is a top view showing an example of the cell stack device according to the first embodiment.
[0058] like Figure 2A As shown in the figure, the cell stack device 10 includes: Figure 1A ) a single cell stack 11 having a plurality of single cells 1 arranged (stacked) on a surface; and a fixing member 12.
[0059] The fixing member 12 includes a fixing material 13 and a support member 14. The support member 14 supports the single cell 1. The fixing material 13 fixes the single cell 1 to the support member 14. In addition, the support member 14 includes a support body 15 and a gas tank 16. The support body 15 and the gas tank 16 as the support member 14 are made of metal and have conductivity.
[0060] like Figure 2B As shown, the support body 15 has an insertion hole 15a into which the lower end portions of the plurality of cells 1 are inserted. The lower end portions of the plurality of cells 1 and the inner wall of the insertion hole 15a are joined by a fixing material 13 .
[0061] The gas tank 16 has an opening for supplying reaction gas to the plurality of cells 1 through the insertion hole 15a and a groove 16a around the opening. The end of the outer periphery of the support 15 is joined to the gas tank 16 by the joining material 21 filled in the groove 16a of the gas tank 16.
[0062] exist Figure 2A In the example shown, the fuel gas is stored in the internal space 22 formed by the support body 15 as the support member 14 and the gas tank 16. The gas flow pipe 20 is connected to the gas tank 16. The fuel gas is supplied to the gas tank 16 through the gas flow pipe 20, and is supplied from the gas tank 16 to the gas flow path 2a (see Figure 1A The fuel gas supplied to the gas tank 16 is supplied by the reformer 102 (see Figure 3 )generate.
[0063] The hydrogen-rich fuel gas can be produced by steam reforming a raw fuel, etc. When the fuel gas is produced by steam reforming, the fuel gas contains water vapor.
[0064] exist Figure 2A In the example shown, there are two rows of single cell stacks 11, two supports 15, and a gas tank 16. The two rows of single cell stacks 11 each have a plurality of single cells 1. Each single cell stack 11 is fixed to each support 15. The gas tank 16 has two through holes on the upper surface. Each support 15 is arranged in each through hole. The internal space 22 is formed by one gas tank 16 and two supports 15.
[0065] The shape of the insertion hole 15a is, for example, an elliptical shape when viewed from the top surface. The length of the insertion hole 15a, for example, in the arrangement direction of the battery cells 1, that is, in the thickness direction T, is greater than the distance between the two end current collecting members 17 located at both ends of the battery stack 11. The width of the insertion hole 15a is, for example, greater than the width direction W of the battery cells 1 (see Figure 1A ) is long.
[0066] like Figure 2BAs shown, the joint between the inner wall of the insertion hole 15a and the lower end of the single cell 1 is filled with the fixing material 13 and cured. As a result, the inner wall of the insertion hole 15a and the lower ends of the plurality of single cells 1 are respectively joined and fixed, and the lower ends of the single cells 1 are joined and fixed to each other. The gas flow path 2a of each single cell 1 communicates with the internal space 22 of the support member 14 at the lower end.
[0067] A material with low conductivity such as glass can be used for the fixing material 13 and the bonding material 21. As specific materials of the fixing material 13 and the bonding material 21, amorphous glass and the like can be used, and in particular, crystallized glass and the like can be used.
[0068] As crystallized glass, any of the materials such as SiO2-CaO system, MgO-B2O3 system, La203-B203-MgO system, La203-B203-ZnO system, SiO2-CaO-ZnO system, etc. can be used, especially SiO2-MgO system materials.
[0069] In addition, if Figure 2B As shown, a conductive member 18 is interposed between adjacent cells 1 among the plurality of cells 1. The conductive member 18 electrically connects one adjacent cell 1 to another adjacent cell 1 in series. More specifically, the conductive member 18 connects the fuel electrode 5 of one cell 1 to the air electrode 7 of another cell 1.
[0070] In addition, if Figure 2B As shown, the end current collecting member 17 is electrically connected to the outermost single cell 1 in the arrangement direction of the plurality of single cells 1. The end current collecting member 17 is connected to a conductive portion 19 protruding outside the single cell stack 11. The conductive portion 19 collects electricity generated by the single cell 1 and leads it to the outside. In addition, Figure 2A In the figure, the end current collecting member 17 is omitted.
[0071] In addition, if Figure 2C As shown, the cell stack device 10 may be a single battery in which two cell stacks 11A and 11B are connected in series. In this case, the conductive portion 19 of the cell stack device 10 may include a positive terminal 19A, a negative terminal 19B, and a connection terminal 19C.
[0072] The positive terminal 19A is the positive electrode when the electric power generated by the cell stack 11 is output to the outside, and is electrically connected to the end current collecting member 17 on the positive electrode side of the cell stack 11A. The negative terminal 19B is the negative electrode when the electric power generated by the cell stack 11 is output to the outside, and is electrically connected to the end current collecting member 17 on the negative electrode side of the cell stack 11B.
[0073] The connection terminal 19C electrically connects the end current collecting member 17 on the negative electrode side in the cell stack 11A and the end current collecting member 17 on the positive electrode side in the cell stack 11B.
[0074] <Module>
[0075] Next, use Figure 3 A module according to an embodiment of the present disclosure using the above-described cell stack device 10 will be described. Figure 3 It is a perspective view showing the appearance of the module according to the first embodiment. Figure 3 The figure shows a state in which the front surface and the rear surface as a part of the storage container 101 are removed and the single cell stack device 10 of the fuel cell stored inside is taken out to the rear.
[0076] like Figure 3 As shown, the module 100 includes a storage container 101 and a cell stack device 10 stored in the storage container 101. Moreover, a reformer 102 is arranged above the cell stack device 10.
[0077] The related reformer 102 reforms the raw fuel such as natural gas and kerosene to generate fuel gas and supplies it to the single cell 1. The raw fuel is supplied to the reformer 102 via the raw fuel supply pipe 103. In addition, the reformer 102 may also include a gasification unit 102a for gasifying water and a reforming unit 102b. The reforming unit 102b includes a reforming catalyst (not shown) to reform the raw fuel into fuel gas. The reformer 102 as described above can perform steam reforming as a highly efficient reforming reaction.
[0078] The fuel gas generated by the reformer 102 is supplied to the gas flow path 2a of the cell 1 through the gas flow pipe 20, the gas tank 16, and the support member 14 (see Figure 1A ).
[0079] In the module 100 having the above-described structure, the temperature inside the module 100 during normal power generation is about 500° C. to 1000° C. as the gas is combusted and the unit cells 1 generate power.
[0080] The module 100 described above can be configured by accommodating the cell stack device 10 having the cells 1 with improved power generation performance as described above, thereby achieving the module 100 with improved power generation performance.
[0081] <Module Storage Device>
[0082] Figure 4 1 is an exploded perspective view showing an example of a module storage device according to the first embodiment. The module storage device 110 according to this embodiment includes an outer casing 111, Figure 3The module 100 shown in the figure and the auxiliary equipment not shown in the figure. The auxiliary equipment operates the module 100. The module 100 and the auxiliary equipment are accommodated in the outer packaging shell 111. In addition, Figure 4 Part of the structure is omitted.
[0083] Figure 4 The outer packaging shell 111 of the module storage device 110 shown has pillars 112 and an outer packaging plate 113. The partition plate 114 divides the outer packaging shell 111 in the up and down directions. The space above the partition plate 114 in the outer packaging shell 111 is a module storage chamber 115 for storing the module 100, and the space below the partition plate 114 in the outer packaging shell 111 is an auxiliary equipment storage chamber 116 for storing auxiliary equipment of the operating module 100. In addition, Figure 4 In the figure, the auxiliary equipment housed in the auxiliary equipment housing chamber 116 is omitted.
[0084] The partition plate 114 has an air flow port 117 for passing air from the auxiliary equipment storage room 116 to the module storage room 115. The outer plate 113 constituting the module storage room 115 has an exhaust port 118 for exhausting air from the module storage room 115.
[0085] In the module housing device 110 described above, as described above, by equipping the module 100 with improved power generation performance in the module housing chamber 115 , it is possible to achieve the module housing device 110 with improved power generation performance.
[0086] [Second embodiment]
[0087] Figure 5 1 is a cross-sectional view showing an example of an electrochemical cell according to the second embodiment. The cell 1 according to the present embodiment is different from the cell 1 according to the first embodiment in that the first film 31 is away from the adhesive material 3. Since the first film 31 is away from the adhesive material 3, it is difficult to generate O between the first film 31 and the adhesive material 3. 2 -The so-called reverse diffusion in which ions such as the above-mentioned move, thereby improving the power generation performance of the single cell 1.
[0088] The cell 1 according to the present embodiment is obtained as follows. For example, the surface of the fuel electrode 5 of the stacked body described in the first embodiment is bonded to the first surface 201 having the opening 2b of the metal body 2 via the adhesive material 3. At this time, the stacked body is arranged so that the first film 31 formed on the metal body 2 and the fuel electrode 5 of the stacked body are separated. Thereafter, the intermediate layer and the air electrode 7 are formed on the solid electrolyte layer 6, and the sealing material 8 is further provided on the side of the element part 4, thereby obtaining the cell 1 according to the present embodiment.
[0089] The sealing material 8 may also be located in the gap between the first film 31 and the bonding material 3. Thus, since the release of chromium from the first surface 201 of the metal body 2 exposed to the oxidizing atmosphere is suppressed, for example, the aging resistance of the metal body 2 can be improved. The sealing material 8 is an example of a second covering material located between the metal body 2 and the element portion 4.
[0090] In addition, the second film 32 may also be located between the metal body 2 and the sealing material 8. The second film 32 may also include, for example, C r2 O3. In addition, the second film 32 does not contain any of the first covering material and the second covering material.
[0091] [Third Embodiment]
[0092] Figure 6 is a cross-sectional view showing an example of an electrochemical cell according to the third embodiment. Figure 5 The cell 1 shown is different in that it has a sealing material 28 instead of the sealing material 8. The sealing material 28 has gas barrier properties. The sealing material 28 may have a porosity of, for example, 5% or less. The sealing material 28 has a porosity of 5% or less, so that the fuel gas is difficult to flow between the fuel electrode 5 and the outside. The porosity of the sealing material 28 may also be set to, for example, the average value of the porosity in at least three arbitrary cross sections of the sealing material 28.
[0093] The single cell 1 involved in the present embodiment is obtained as follows. For example, the surface of the fuel electrode 5 of the stack described in the first embodiment is joined to the first surface 201 having the opening 2b of the metal body 2 via the adhesive material 3. At this time, the stack is configured so that the first film 31 formed on the metal body 2 and the fuel electrode 5 of the stack are separated. Thereafter, an intermediate layer is formed on the solid electrolyte layer 6, and a sealing material 28 is further provided on the side of the stack. After the sealing material 28 is provided, the air electrode 7 is formed on the intermediate layer, thereby obtaining the single cell 1 involved in the present embodiment. The intermediate layer can also be formed by a gas phase method such as vacuum evaporation.
[0094] The sealing material 28 may also include insulating oxides such as forsterite, which have higher heat resistance than the sealing material 8. Therefore, the sealing material 28 is not limited to suppressing the release of chromium from the first surface 201 of the metal body 2 during the operation of the single cell 1, for example, but also during the manufacture of the single cell 1, thereby further improving the power generation performance of the single cell 1. Compared with the sealing material 8, the sealing material 28 is less likely to dissolve in high-temperature water vapor, evaporate components, etc., and is therefore less likely to leak gas and reduce electrode performance. In particular, forsterite has a thermal expansion coefficient close to that of the metal / alloy used as the material of the metal body 2 and / or close to that of the element part 4, and can improve the thermal shock resistance of the single cell 1. In addition, forsterite is also resistant to high-temperature water vapor due to the glass used in the sealing material 8. 2 - etc., the ion conductivity is reduced, and it is more difficult to produce reverse diffusion. Forsterite has, for example, 1×10 12 Electrical resistivity above Ω·m.
[0095] [Fourth Embodiment]
[0096] Figure 7 is a cross-sectional view showing an example of an electrochemical cell according to a fourth embodiment. Figure 1A The cell 1 shown is different in the following points: the sealing material 8 is arranged from the first surface 211 of the metal body 2 to surround the third surface 203 and the fourth surface 204 to the second surface 212 where the oxide film 9 is located. The metal body 2 is covered by the oxide film 9 and the sealing material 8 exposed to the oxidizing atmosphere, and the metal body 2 itself is not exposed to the oxide atmosphere. As a result, the chromium (Cr) contained in the metal body 2 is difficult to be released into the oxidizing atmosphere during high-temperature operation. Therefore, according to this embodiment, the power generation performance of the cell 1 can be improved. The oxide film 9 involved in this embodiment is, for example, the first film 31. In addition, the cell 1 may also have, for example, a second film 32 between the oxide film 9 and the metal body 2.
[0097] [Fifth and Sixth Embodiments]
[0098] Figure 8 It is a cross-sectional view showing an example of an electrochemical cell according to a fifth embodiment. Fig. 9 It is a cross-sectional view showing an example of an electrochemical cell according to the sixth embodiment.
[0099] like Figure 8 As shown in FIG. 1 , the single cell 1 may also include a substantially cylindrical metal body 2. Fig. 9 As shown in FIG. 1 , the cell 1 may also include a flat metal body 2. The flat metal body 2 includes: a first surface 211 and a second surface 212 located opposite to each other in the thickness direction T; Figure 1B ) is formed on the gas flow path 2a extending on the metal body 2. In this way, regardless of the shape of the metal body 2, the portion exposed to the oxidizing atmosphere is covered with the oxide film 9 and the sealing material 8, thereby improving the power generation performance of the single cell 1. The oxide film 9 involved in this embodiment is, for example, the first film 31. In addition, the single cell 1 may also have, for example, a second film 32 between the oxide film 9 and the metal body 2.
[0100] [Other embodiments]
[0101] exist Figure 7 to Figure 9 In the illustrated single cell 1 , the sealing material 8 is shown as being provided, but the sealing material 28 may be provided instead of the sealing material 8 .
[0102] In addition, in each of the above-mentioned embodiments, a fuel cell, a fuel cell stack device, a fuel cell module, and a fuel cell device are shown as an example of an "electrochemical cell", "electrochemical cell device", "module", and "module housing device", but other examples may be an electrolysis cell, an electrolysis cell stack device, an electrolysis module, and an electrolysis device. The electrolysis cell has a first electrode, a solid electrolyte layer, and a second electrode, and decomposes water vapor into hydrogen and oxygen or decomposes carbon dioxide into carbon monoxide and oxygen by supplying electricity. In addition, in each of the above-mentioned embodiments, an oxide ion conductor or a hydrogen ion conductor is shown as an example of an electrolyte material for an electrochemical cell, but it may also be a water oxide ion conductor. According to the electrolysis cell, electrolysis cell stack device, electrolysis module, and electrolysis device as described above, the electrolysis performance can be improved.
[0103] As mentioned above, although this disclosure was demonstrated in detail, this disclosure is not limited to the said embodiment, Various changes, improvements, etc. are possible within the range which does not deviate from the summary of this disclosure.
[0104] As described above, the electrochemical cell (cell 1) according to the embodiment includes the element portion 4, the metal body 2, and the oxide covering material. The metal body 2 contains chromium and supports the element portion 4. The oxide covering material covers the surface of the metal body 2 and is exposed in the oxidizing atmosphere. The oxide covering material suppresses the release of chromium into the oxidizing atmosphere. The oxide covering material has at least a conductive first covering material (first film 31). Thus, the performance of the cell 1 can be improved.
[0105] Furthermore, the electrochemical cell device (cell stack device 10 ) according to the embodiment includes the cell stack 11 including electrochemical cells. This can improve the performance of the cell stack device 10 .
[0106] Furthermore, the module 100 according to the embodiment includes the electrochemical cell device described above and the storage container 101 for storing the electrochemical cell device. This can improve the performance of the module 100.
[0107] Furthermore, the module storage device 110 according to the embodiment includes the above-mentioned module 100, auxiliary equipment for operating the module 100, and an outer casing for storing the module 100 and the auxiliary equipment. Thus, the performance of the module storage device 110 can be improved.
[0108] The embodiments disclosed this time should be considered as illustrative and not restrictive in all aspects. In fact, the above embodiments can be implemented in various ways. In addition, the above embodiments can also be omitted, replaced, and changed in various ways without departing from the attached claims and their main purpose.
[0109] -Explanation of symbols-
[0110] 1 single battery
[0111] 2 Metal body
[0112] 4 Components
[0113] 8 Sealing material
[0114] 9 Oxide film
[0115] 10 Single Cell Stack Device
[0116] 11 Single Cell Stack
[0117] 31 First membrane
[0118] 32 Second membrane
[0119] 100 modules
[0120] 110 Module containment device.
Claims
1. An electrochemical cell comprising: Components Department; a metal body, including chromium, electrically connected to the element portion; and an oxide covering material covering the metal body, exposing it to an oxidizing atmosphere, and inhibiting the release of chromium into the oxidizing atmosphere, The oxide covering material includes at least a first covering material having electrical conductivity.
2. The electrochemical cell according to claim 1, wherein: The oxide covering material further includes an insulating second covering material.
3. The electrochemical cell according to claim 2, wherein: The second covering material is located between the element portion and the first covering material.
4. The electrochemical cell according to claim 2 or 3, wherein: The element unit includes a first electrode, a solid electrolyte layer, and a second electrode. The electrical conductivity of the second covering material is 1 / 10 or less of the electrical conductivity of the solid electrolyte layer.
5. The electrochemical cell according to any one of claims 2 to 4, wherein: The second covering material has a porosity of 10% or less.
6. The electrochemical cell according to any one of claims 2 to 4, wherein: The second covering material includes forsterite.
7. The electrochemical cell according to any one of claims 1 to 6, wherein: The first capping material includes manganese.
8. An electrochemical cell device, wherein: The electrochemical cell device comprises a cell stack, and the cell stack includes the electrochemical cell according to any one of claims 1 to 7.
9. A module comprising: The electrochemical cell device of claim 8; and The storage container stores the electrochemical cell device.
10. A module storage device, comprising: The module of claim 9; and Auxiliary equipment for operating the module; and The outer packaging shell accommodates the module and the auxiliary equipment.