Battery monomer, battery and electric device
Patent Information
- Application Number
- CN202280094277.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-29
- Publication Date
- 2024-11-08
AI Technical Summary
During the use of a battery cell, dendrites are prone to grow in the bending area of the electrode assembly, causing internal short circuits and affecting the safety of the battery.
The battery cell design includes an insulating layer and an adhesive layer. The insulating layer is bonded to the bending area of the electrode assembly through the adhesive layer to provide buffering and barrier effects, reduce the growth rate of dendrites, and extend the service life of the battery.
It effectively reduces the growth rate of dendrites, extends the service life of the battery, and improves the safety and stability of the battery.
Smart Images

Figure CN118922981A_ABST
Abstract
Description
Battery cells, batteries and electrical devices Technical Field
[0001] The present application relates to the field of battery technology, and in particular to a battery cell, a battery, and an electrical device. Background Art
[0002] The electrode assembly is the component in a battery cell where electrochemical reactions occur. The electrode assembly includes a positive electrode sheet, a negative electrode sheet, and a separator that separates the positive and negative electrode sheets. The positive electrode sheet, separator, and negative electrode sheet can be wound to form a rolled electrode assembly, so that the electrode assembly has a main body area and a bending area provided on the end side of the main body area. However, during the use of the battery cell, the bending area of the electrode assembly is prone to metal precipitation, and over time, dendrites are prone to grow in the bending area. Dendrites can easily cause internal short circuits in the battery cell, affecting the safety of the battery cell. Technical issues
[0003] The embodiments of the present application provide a battery cell, a battery, and an electrical device to solve the problem that during the use of the battery cell, the electrode assembly is prone to grow dendrites in the bending area, causing an internal short circuit in the battery cell and affecting the safety of the battery cell. Technical Solutions
[0004] The technical solution adopted in the embodiment of this application is:
[0005] In a first aspect, a battery cell is provided, the battery cell comprising at least one electrode assembly, the electrode assembly comprising a positive electrode sheet, a negative electrode sheet, a separator, an insulating layer, and a glue layer;
[0006] The positive electrode sheet, the separator and the negative electrode sheet are stacked and wound, and the electrode assembly has a bending area;
[0007] At least a portion of the insulating layer and at least a portion of the adhesive layer are arranged in the bending area, and the insulating layer is bonded to the positive electrode sheet or the negative electrode sheet through the adhesive layer; in the thickness direction of the insulating layer, the projected area of the adhesive layer is smaller than the projected area of the insulating layer.
[0008] The battery cell provided in the embodiment of the present application can firmly and reliably adhere the insulating layer to the bent portion of any circle of the positive electrode sheet or the negative electrode sheet through the adhesive layer, so that the insulating layer can be permanently and reliably stabilized in the bent area during the use of the battery cell, which can effectively reduce the risk of displacement and detachment of the insulating layer, thereby ensuring that the insulating layer can be permanently, stably and reliably effective at a specific position during the use of the battery cell. In addition, by making the projected area of the adhesive layer in the thickness direction of the insulating layer smaller than the projected area of the insulating layer in the thickness direction, the negative impact of the adhesive layer on the extension and deformation properties of the insulating layer is effectively reduced during the winding and pre-pressing of the electrode assembly and during the use of the battery cell, thereby facilitating the insulating layer to extend and deform adaptively with the electrode sheet, facilitating the insulating layer to be permanently and reliably effective during the use of the battery cell, effectively reducing the risk of tearing defects in the insulating layer during the use of the battery cell, and correspondingly ensuring and extending the service life of the insulating layer.
[0009] The battery cell provided in the embodiment of the present application can also form a buffering effect on the bending stress borne by the bent part of the electrode piece through the insulating layer provided in the bending area during the winding and pre-pressing of the electrode assembly and during the use of the battery cell, thereby effectively reducing the risk of tearing defects in the bent part of the electrode piece leading to a reduction in active material, effectively reducing the risk of metal precipitation in the bending area of the electrode assembly due to the reduction of active material, and effectively alleviating the growth rate of dendrites, thereby correspondingly extending the service life of the battery cell and correspondingly improving the safety of the battery cell. Moreover, even if dendrites grow in the bending area of the electrode assembly with prolonged use, the insulating layer with insulating properties can form an insulating barrier to the dendrites growing toward it, preventing the dendrites from directly contacting the conductive positive and negative pole pieces, and even hindering and delaying the growth of the dendrites, thereby effectively delaying the occurrence of the phenomenon of "dendrites directly causing internal short circuits in the battery cells", and effectively delaying the occurrence of the phenomenon of "dendrites heating up due to short circuits and melting the diaphragms around the dendrites, causing direct contact and short circuit between the positive and negative pole pieces where the diaphragms melt", which can correspondingly extend the service life of the battery cells and improve the safety of the battery cells.
[0010] In some embodiments, the adhesive layer includes a plurality of adhesives, and at least a portion of the adhesives is distributed in the edge region of the insulating layer.
[0011] By adopting the above solution, multiple colloids, especially those placed near the edges of the insulating layer, can be used to securely and reliably bond the insulating layer, especially the edges of the insulating layer, to the bent portion of any positive or negative electrode. This allows the insulating layer to be permanently and reliably positioned and effective. Furthermore, while ensuring the adhesive layer's effectiveness in securing the insulating layer, the number of colloids installed and the area they occupy can be reduced, effectively reducing the adhesive layer's negative impact on the insulating layer's elongation and deformation properties. This allows the insulating layer to adapt to the elongation and deformation of the electrode, thus ensuring the effectiveness and service life of the insulating layer.
[0012] In some embodiments, the colloid is a strip-shaped colloid, and a plurality of colloids are arranged at intervals along the width direction of the insulating layer, or a plurality of colloids are arranged at intervals along the length direction of the insulating layer.
[0013] By adopting the above solution, multiple colloids can be optimally arranged on one side of the insulating layer, particularly allowing the two colloids furthest apart to be positioned near the two edges of the insulating layer. This ensures that each strip of colloid can firmly and reliably adhere the insulating layer, particularly the two edges of the insulating layer, to the bent portion of any coil of the electrode, thereby ensuring that the insulating layer can be securely and reliably positioned and function effectively. Furthermore, while optimizing the layout of each strip of colloid to ensure the tightening effect on the insulating layer, the number of colloids installed and the area they occupy can be effectively reduced, effectively reducing the negative impact of the adhesive layer on the elongation and deformation properties of the insulating layer. This allows the insulating layer to adapt to the extension and deformation of the electrode, thereby ensuring the effectiveness and service life of the insulating layer. Furthermore, as the insulating layer adapts to the extension and deformation of the electrode, the multiple strips of colloid can be spaced apart and deformed accordingly, ensuring that the adhesive layer can secure the insulating layer reliably and durably.
[0014] In some embodiments, the colloid is a block-shaped colloid, and at least a portion of the colloid is distributed at corners of the insulating layer.
[0015] By adopting the above scheme, multiple block-shaped colloids, especially those distributed at the corners of the insulating layer, can be used to securely and reliably bond the insulating layer, especially the corners and edges of the insulating layer, to the bent portion of any coil of the electrode. This allows the insulating layer to be permanently and reliably positioned and effective. Furthermore, because the colloids are block-shaped and multiple block-shaped colloids can be optimally arranged on one side of the insulating layer, the number of colloids installed and the area occupied can be effectively reduced while ensuring the adhesive layer's effectiveness in securing the insulating layer. This effectively reduces the negative impact of the adhesive layer on the insulating layer's elongation and deformation properties, allowing the insulating layer to adapt to the extension and deformation of the electrode, thereby ensuring the effectiveness and service life of the insulating layer. Furthermore, while the insulating layer adapts to the extension and deformation of the electrode, the multiple block-shaped colloids can be spaced apart adaptively with the insulating layer, ensuring the adhesive layer's overall effectiveness in securing the insulating layer is long-lasting and effective.
[0016] In some embodiments, the adhesive layer is a hot melt adhesive that is resistant to electrolyte.
[0017] By adopting this solution, a hot melt adhesive with fast, strong, and stable bonding properties can be used to form an adhesive layer, allowing the insulating layer to be firmly bonded to the bent portion of the electrode conveniently, quickly, and reliably. Furthermore, the hot melt adhesive's electrolyte resistance ensures that the adhesive layer maintains a long-lasting and effective fastening effect on the insulating layer during the battery's life.
[0018] In some embodiments, in the thickness direction of the insulating layer, the ratio of the projected area of the adhesive layer to the projected area of the insulating layer is 20% to 50%.
[0019] By adopting the above scheme, during the winding and pre-pressing of the electrode assembly and during the use of the battery cell, the area ratio of the glue layer relative to the insulating layer can be effectively reduced on the basis of ensuring the fastening effect of the glue layer on the insulating layer, thereby effectively reducing the negative impact of the glue layer on the extension and deformation properties of the insulating layer, thereby facilitating the insulating layer to extend and deform adaptively with the pole piece, facilitating the insulating layer to perform its function durably and reliably during the use of the battery cell, effectively reducing the risk of tearing defects in the insulating layer during the use of the battery cell, and effectively ensuring and extending the service life of the insulating layer.
[0020] In some embodiments, the thickness of the adhesive layer is 2 micrometers (um) to 8 um.
[0021] By adopting the above solution, the thickness of the adhesive layer can be effectively reduced while ensuring the fastening effect of the adhesive layer on the insulating layer, thereby helping to ensure and improve the energy density of the electrode assembly and the battery cell.
[0022] In some embodiments, in the bending region, at least one insulating layer is bonded to the inner side of the innermost positive electrode plate through an adhesive layer.
[0023] By adopting the above scheme, on the one hand, when "metal precipitation occurs at the bent part of the innermost circle of the negative electrode sheet, and dendrites grow from the defects of the bent part of the diaphragm over time", the growing dendrites can be insulated and blocked by an insulating layer provided on the inner side of the bent part of the innermost circle of the positive electrode sheet to prevent the dendrites from directly contacting the conductive positive electrode sheet and the negative electrode sheet. This can effectively delay the occurrence of "dendrites directly causing internal short circuits in the battery cells" between the innermost circle of the positive electrode sheet and the innermost circle of the negative electrode sheet where metal precipitation is easily generated, and effectively delay the occurrence of "dendrites heating up due to short circuits and melting the diaphragm around the dendrites, causing direct contact and short circuits between the positive electrode sheet and the negative electrode sheet where the diaphragm melts", thereby correspondingly extending the service life of the battery cells and improving the safety of the battery cells.
[0024] On the other hand, during the winding and pre-pressing of the electrode assembly and during the use of the battery cell, the insulating layer provided inside the bent portion of the innermost positive electrode tab can buffer the compressive stress experienced by the bent portion of the innermost positive electrode tab, thereby reducing the risk of tearing defects in the bent portion of the innermost positive electrode tab, which could lead to a reduction in active material. It can even buffer the tensile stress experienced by the bent portion of the innermost negative electrode tab, thereby reducing the risk of tearing defects in the bent portion of the innermost negative electrode tab, which could lead to a reduction in active material. This effectively reduces the risk of metal precipitation exacerbated by the reduction in active material, and effectively mitigates the growth rate of dendrites between the innermost positive and negative electrode tabs, thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0025] In some embodiments, in the bending region, at least one insulating layer is bonded to the outer side of the innermost positive electrode plate through an adhesive layer.
[0026] By adopting the above solution, during the winding and pre-pressing of the electrode assembly and during the use of the battery cell, the insulating layer provided on the outer side of the bent portion of the innermost positive electrode tab can buffer the tensile stress experienced by the bent portion of the innermost positive electrode tab, thereby reducing the risk of tearing defects in the bent portion of the innermost positive electrode tab, which could lead to a reduction in active material. Furthermore, the compressive stress experienced by the bent portion of the second innermost negative electrode tab can be buffered, thereby reducing the risk of tearing defects in the bent portion of the second innermost negative electrode tab, which could lead to a reduction in active material. This effectively reduces the risk of metal precipitation exacerbated by the reduction in active material, and effectively mitigates the growth rate of dendrites between the innermost positive electrode tab and the second innermost negative electrode tab, thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0027] By adopting the above solution, during the use of the battery cell, the insulating layer provided on the outside of the bent portion of the innermost positive electrode tab can be used to insulate and block dendrites growing toward it, thereby preventing the dendrites from directly contacting and conducting the innermost positive electrode tab and the next innermost negative electrode tab. This effectively delays the occurrence of "dendrites directly causing internal short circuits in the battery cell" between the innermost positive electrode tab and the next innermost negative electrode tab, and effectively delays the occurrence of "dendrites heating up due to short circuits and melting the diaphragm around the dendrites, causing direct contact and short circuits between the positive and negative electrode tabs where the diaphragm melts", thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0028] In some embodiments, two insulating layers are provided in the bending region, one of which is bonded to the inner side of the innermost positive electrode plate through an adhesive layer, and the other insulating layer is bonded to the outer side of the innermost positive electrode plate through an adhesive layer.
[0029] By adopting the above solution, the bending zone can effectively delay the risk of short circuits through two insulating layers in the "innermost positive electrode sheet and the innermost negative electrode sheet" and "innermost positive electrode sheet and the second innermost negative electrode sheet" where metal precipitation is prone to occur and the metal precipitation is relatively serious. It can also effectively alleviate the compression stress and tensile stress in the bent portion of the innermost positive electrode sheet, which is subject to greater bending stress and prone to tearing defects, thereby reducing the risk of bending and tearing, thereby effectively extending the service life of the battery cell and effectively improving the safety of the battery cell. While maximizing the effectiveness of the insulating layer, by adopting the above solution, the number of insulating layers set can also be reduced, thereby ensuring and improving the energy density of the electrode assembly and battery cell.
[0030] In some embodiments, the electrode assembly has a main body region and a bending region arranged on the end side of the main body region; the insulating layer has a bent section bent in the bending region, and an extension section connected to the end of the bent section and arranged in the main body region.
[0031] By adopting the above-mentioned scheme, the setting area of the insulating layer can be extended accordingly, and the preset position of the insulating layer on the continuous positive electrode sheet or the continuous negative electrode sheet has a wider tolerance range, thereby effectively ensuring that when the electrode assembly is wound, the insulating layer can retain the bent section clamped between the bent part of the electrode sheet and the diaphragm, and can adapt to the extended section extending to the main area according to the position tolerance, thereby effectively reducing the accuracy requirements for the preset position of the insulating layer on the continuous positive electrode sheet or the continuous negative electrode sheet, and can effectively ensure and improve the production yield of the electrode assembly.
[0032] In some embodiments, the insulating layer is provided with a plurality of holes.
[0033] By adopting this solution, during the charge and discharge process of the battery cell, active ions can freely penetrate the pores of the insulating layer and the separator to move between the positive and negative electrode plates. This effectively ensures that the provision of the insulating layer does not significantly affect the charge and discharge process of the battery cell, effectively ensuring the charge and discharge performance of the battery cell.
[0034] In some embodiments, an absolute value of a difference between the porosity of the insulating layer and the porosity of the separator is less than or equal to 25%.
[0035] By adopting the above solution, the porosity of the insulating layer can be made almost the same as that of the diaphragm. Based on this, active ions can freely and normally penetrate the insulating layer and the diaphragm, thereby effectively ensuring that the setting of the insulating layer will not have a significant impact on the charging and discharging process of the battery cell, and effectively ensuring the charging and discharging performance of the battery cell.
[0036] In some embodiments, an absolute value of a difference between the porosity of the insulating layer and the porosity of the separator is less than or equal to 10%.
[0037] By adopting the above solution, the porosity of the insulating layer can be set to be similar to the porosity of the diaphragm, so that the active ions can freely and normally penetrate the insulating layer and the diaphragm, thereby effectively ensuring that the setting of the insulating layer will not have a significant impact on the charging and discharging process of the battery cell, and effectively ensuring the charging and discharging performance of the battery cell.
[0038] In some embodiments, the insulating layer is a polyolefin separator.
[0039] By adopting the above scheme, an insulating layer can be made of a polyolefin diaphragm such as a polypropylene diaphragm to ensure that the porosity of the insulating layer is similar to or even the same as the porosity of the diaphragm, thereby ensuring that active ions can freely and normally penetrate the insulating layer and the diaphragm, effectively ensuring that the setting of the insulating layer will not have a significant impact on the charging and discharging process of the battery cell, and effectively ensuring the charging and discharging performance of the battery cell.
[0040] In some embodiments, the porosity of the insulating layer is 40% to 50%.
[0041] By adopting this solution, on the one hand, the insulation layer can be guaranteed to have moderate air permeability, ensuring that active ions can freely and normally penetrate the insulation layer. On the other hand, when the adhesive layer is applied to the side of the insulation layer, the amount of glue that penetrates into the pores of the insulation layer is small, while a large amount of glue remains on the surface of the insulation layer. This ensures the adhesive strength of the adhesive layer, ensures that the insulation layer can be reliably fixed to the electrode through the adhesive layer, and reduces the effect of the adhesive layer on blocking the pores of the insulation layer, ensuring that active ions can freely and normally penetrate the insulation layer, thereby ensuring electrical conductivity.
[0042] In some embodiments, the diameter of the pores of the insulating layer is A, the thickness of the insulating layer is B, and 24≤B / A≤400.
[0043] By adopting this solution, the thickness B of the insulating layer and the pore diameter A of the insulating layer can be adjusted to a moderate value. This, on the one hand, makes it difficult for dendrites to pierce or pass through the insulating layer, thereby ensuring the insulating layer's dendrite-blocking effect. On the other hand, it allows active ions to easily and quickly move through the insulating layer, thereby reducing the risk of active ion precipitation due to difficulty in moving. This effectively extends the service life of the battery cell and improves its safety.
[0044] In some embodiments, the pores of the insulating layer have a pore diameter A of 0.05 um to 0.5 um.
[0045] By adopting the above solution, on the one hand, the air permeability of the insulating layer can be guaranteed to be moderate, and the active ions can be guaranteed to be able to freely and normally penetrate the pores of the insulating layer. On the other hand, it can be guaranteed that when the glue layer is coated on the side of the insulating layer, the amount of glue that penetrates into the pores of the insulating layer is small, while the amount of glue left on the surface of the insulating layer is large, thereby ensuring the adhesion of the glue layer, ensuring that the insulating layer can be reliably fixed to the electrode through the glue layer, and reducing the blocking effect of the glue layer on the pores of the insulating layer, ensuring that active ions can freely and normally penetrate the insulating layer, and ensuring electrical conductivity. On the one hand, during the use of the battery cell, the insulating layer can be guaranteed to have a barrier effect on dendrites growing from defects in the diaphragm, and reduce the risk of dendrites growing from the pores of the insulating layer, thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0046] In some embodiments, the thickness B of the insulating layer is 12 um to 20 um.
[0047] By adopting the above scheme, the thickness B of the insulating layer can be ensured to be moderate, so as to reduce the influence of the insulating layer on the energy density of the battery cell and the penetration rate of active ions through the insulating layer on the basis of ensuring that the insulating layer can form a better insulating barrier effect on the dendrites growing toward it, thereby ensuring the electrical conductivity and the charging and discharging performance of the battery cell, extending the service life of the battery cell accordingly, and improving the safety of the battery cell accordingly.
[0048] In some embodiments, the adhesive layer avoids the hole in the thickness direction of the insulating layer.
[0049] By adopting the above scheme, the blocking effect of the glue layer on the pores of the insulating layer can be reduced to a great extent on the basis of ensuring the fastening effect of the glue layer on the insulating layer, thereby facilitating the free penetration of active ions through the pores of the insulating layer and the diaphragm during the charging and discharging process of the battery cell, and realizing the movement between the positive electrode sheet and the negative electrode sheet, thereby effectively reducing the influence of the setting of the insulating layer on the charging and discharging process of the battery cell, and effectively ensuring the charging and discharging performance of the battery cell.
[0050] In some embodiments, the tensile strength of the insulating layer in the width direction thereof is greater than or equal to 1000 kilograms force per square centimeter (kgf / cm 2 ).
[0051] By adopting the above-mentioned solution, it can be ensured that the insulating layer has sufficient tensile strength in its width direction, which can effectively reduce the risk of fracture and cracking defects of the insulating layer under the action of tension, thereby ensuring and improving the insulating barrier effect of the insulating layer on dendrites growing from the defects of the diaphragm, and effectively reducing the risk of dendrites continuing to grow along the fracture and cracking defects of the insulating layer, thereby correspondingly extending the service life of the battery cell and correspondingly improving the safety of the battery cell.
[0052] In some embodiments, the elongation of the insulating layer in the width direction thereof is greater than or equal to 10%.
[0053] By adopting the above solution, it can be ensured that the insulating layer has sufficient elongation in its width direction to ensure that the insulating layer can adaptively extend and deform with the electrode assembly, thereby ensuring that the effective range of the insulating layer can cover the corresponding area of the electrode piece, and ensuring that the insulating layer can form a reliable insulation barrier effect on the dendrites growing from the defects of the diaphragm.
[0054] In some embodiments, the shrinkage rate of the insulating layer at 105 degrees Celsius (° C.) is 0-3%.
[0055] By adopting the above solution, it can be ensured that the insulating layer will shrink less in size due to the internal temperature of the battery cell during the use of the battery cell, thereby ensuring that the effective range of the insulating layer can cover the corresponding area of the electrode and ensuring that the insulating layer can form a reliable insulating barrier effect on the dendrites growing from the defects of the diaphragm.
[0056] In a second aspect, a battery is provided, which includes the battery cell provided in the embodiments of the present application.
[0057] By adopting the above solution, the battery can ensure and extend the battery life and ensure and improve the battery safety by applying the battery cells provided in the embodiments of the present application.
[0058] In a third aspect, an electrical device is provided, which includes the battery or battery cell provided in an embodiment of the present application.
[0059] By adopting the above solution, the electrical device can ensure and extend the service life of the electrical device and ensure and improve the safety of the electrical device by applying the battery or battery cell provided in the embodiment of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0060] In order to clearly illustrate the technical solutions in the embodiments of the present application, the following briefly introduces the drawings required for use in the embodiments of the present application or the exemplary technical description. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0061] FIG1 is a schematic structural diagram of a vehicle provided in an embodiment of the present application;
[0062] FIG2 is an exploded schematic diagram of a battery provided in an embodiment of the present application;
[0063] FIG3 is an exploded schematic diagram of a battery cell provided in an embodiment of the present application;
[0064] FIG4 is a schematic cross-sectional view of a battery cell provided in an embodiment of the present application;
[0065] FIG5 is a schematic structural diagram of an electrode assembly provided in an embodiment of the present application;
[0066] FIG6 is a partial schematic diagram of the electrode assembly provided in FIG5 ;
[0067] FIG7 is a second partial schematic diagram of the electrode assembly provided in FIG5 ;
[0068] FIG8 is a schematic diagram of the structure of an insulating layer and an adhesive layer provided in one embodiment of the present application, wherein a plurality of strip-shaped adhesives are arranged at intervals along the width direction of the insulating layer;
[0069] FIG9 is a schematic diagram of the structure of an insulating layer and an adhesive layer provided in another embodiment of the present application, wherein a plurality of strip-shaped adhesives are spaced apart along the length direction of the insulating layer;
[0070] FIG10 is a schematic structural diagram of an insulating layer and an adhesive layer provided in another embodiment of the present application, wherein at least part of the block-shaped colloid is distributed at each corner of the insulating layer.
[0071] Among them, the reference numerals in the figures are:
[0072] 1-battery, 2-controller, 3-motor; 100-battery unit, 200-box, 201-first part, 202-second part;
[0073] 10-electrode assembly, 11-positive electrode sheet, 111-positive electrode tab, 112-innermost positive electrode sheet, 12-negative electrode sheet, 121-negative electrode tab, 122-innermost negative electrode sheet, 123-next inner negative electrode sheet, 13-diaphragm, 14-insulating layer, 141-bending section, 142-extension section, 15-glue layer, 151-colloid, 16-main body, 17-bending area; 20-electrolyte; 30-shell, 40-end cover, 50-electrode terminal. Modes for Carrying Out the Invention
[0074] In order to make the technical problems, technical solutions and beneficial effects to be solved by this application clear and understandable, the present application is described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain this application and are not intended to limit this application.
[0075] In the description of this application, it should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the accompanying drawings, and are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on this application.
[0076] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features being referred to. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of such features. Throughout the description of this application, "plurality" means two or more, unless otherwise specifically defined.
[0077] In this application, unless otherwise expressly specified or limited, terms such as "mounted," "connected," "connect," and "fixed" should be understood in a broad sense. For example, they may refer to fixed connections, detachable connections, or integration; mechanical connections or electrical connections; direct connections or indirect connections through an intermediate medium; and internal connections between two components or interactions between two components. Those skilled in the art will understand the specific meanings of these terms in this application based on specific circumstances.
[0078] A battery cell is the smallest unit for storing and outputting electrical energy. A battery cell typically contains at least one electrode assembly. The electrode assembly is the component within the battery cell where electrochemical reactions occur. The electrode assembly includes a positive electrode sheet, a negative electrode sheet, and a separator that separates the positive and negative electrode sheets. The positive electrode sheet, separator, and negative electrode sheet can be wound to form a rolled electrode assembly, such that the electrode assembly has a main body region and a bending region disposed at the end of the main body region. When the battery cell is charged, the positive electrode sheet generates active ions. The active ions provided by the positive electrode sheet can penetrate the pores of the separator to move to the negative electrode sheet and embed into the negative active material of the negative electrode sheet. Conversely, when the battery cell is discharged, the active ions embedded in the negative active material of the negative electrode sheet are released. The active ions released from the negative electrode sheet can penetrate the pores of the separator to move to the positive electrode sheet and embed into the positive active material of the positive electrode sheet.
[0079] However, the applicant found that:
[0080] 1. In the bending zone, since the positive electrode tabs of any circle are located outside the negative electrode tabs of the same circle, the curvature radius of the positive electrode tabs of any circle will be relatively larger than the curvature radius of the negative electrode tabs of the same circle. For example, since the positive electrode tabs of the innermost circle are located outside the negative electrode tabs of the innermost circle, the curvature radius of the positive electrode tabs of the innermost circle will be relatively larger than the curvature radius of the negative electrode tabs of the innermost circle. Based on this, in the bending zone, the area of the positive electrode tabs of any circle will be relatively larger than the area of the negative electrode tabs of the same circle. As a result, during the charging process of the battery cell, the positive electrode tabs with larger areas and relatively more positive active materials will generate more active ions, but the negative electrode tabs with smaller areas and relatively less negative active materials have insufficient space for active ions to embed, resulting in the precipitation of active ions that cannot be embedded in the negative active materials, resulting in metal precipitation.
[0081] 2. During the process of winding the positive electrode sheet, separator, and negative electrode sheet to form a rolled electrode assembly, the bent portions of the positive and negative electrode sheets (i.e., the portions of the electrode sheets corresponding to the bent areas) will bend and bend, and the radius of curvature will decrease as the inner circles become smaller, causing the positive active material in the bent portion of the positive electrode sheet to partially fall off (i.e., powdering). The negative active material in the bent portion of the negative electrode sheet will also experience powdering. Furthermore, since the radius of curvature of the negative electrode sheet in any circle is relatively smaller than the radius of curvature of the positive electrode sheet in the same circle, the powdering of the bent portion of the negative electrode sheet during bending will be relatively severe. The powdering phenomenon will reduce the content of active material on the electrode sheet, resulting in a decrease in the number of sites available for active ions to embed in the negative electrode sheet with reduced negative active material during the charging process of the battery cell, thereby increasing the number of active ions that cannot be embedded in the negative active material and exacerbating the metal precipitation phenomenon.
[0082] 3. During the winding and pre-pressing of the electrode assembly, as well as during the use of the battery cells, the bent portions of the positive and negative electrode sheets are subjected to greater forces due to bending. The smaller the radius of curvature, the greater the forces applied. This can lead to tearing defects in the bent portions of the positive and negative electrode sheets. If tearing defects occur, the active material at the torn portion will fall off. This can also prevent the active material from being embedded during the charge and discharge process of the battery cells, increasing the amount of active ions released and exacerbating metal precipitation.
[0083] Based on this, the applicant discovered that during the use of the battery cell, metal precipitation is prone to occur in the bending area of the electrode assembly. The continuous diaphragm may have defects such as large pore size and damage in local areas, resulting in the precipitation of active ions that easily grow dendrites at the defects of the diaphragm in the bending area as the battery cell is used for a longer time. As the dendrites grow, they easily contact and conduct the positive and negative pole pieces, causing a short circuit inside the battery cell, thereby affecting the safety of the battery cell. During the short circuit, the dendrites will generate heat and melt the diaphragm part on the side of the dendrite, causing the diaphragm defects to expand, resulting in direct contact and short circuit between the positive and negative pole pieces at the place where the diaphragm melts, thereby aggravating the short circuit phenomenon and seriously affecting the safety of the battery cell.
[0084] Therefore, some embodiments of the present application provide a battery cell, which can firmly and reliably bond the insulating layer to the bent part of any circle of the positive electrode sheet or the negative electrode sheet through the adhesive layer, so that during the winding and pre-pressing of the electrode assembly, as well as during the use of the battery cell, the insulating layer provided in the bending area can form a buffering effect on the bending stress borne by the bent part of the electrode sheet, thereby effectively reducing the risk of tearing defects in the bent part of the electrode sheet leading to a reduction in active material, effectively reducing the risk of metal precipitation in the bending area of the electrode assembly due to the reduction of active material, and effectively alleviating the growth rate of dendrites, thereby correspondingly extending the service life of the battery cell and correspondingly improving the safety of the battery cell. Moreover, even if dendrites grow in the bending area of the electrode assembly with prolonged use, the battery cell can form an insulating barrier to the dendrites growing toward it through an insulating layer with insulating properties, preventing the dendrites from directly contacting the conductive positive electrode and negative electrode sheets, and even hindering and delaying the growth of the dendrites, thereby effectively delaying the occurrence of the phenomenon of "dendrites directly causing internal short circuits in the battery cell", and effectively delaying the occurrence of the phenomenon of "dendrites heating up due to short circuits and melting the diaphragm around the dendrites, causing direct contact and short circuit between the positive electrode sheet and the negative electrode sheet at the place where the diaphragm melts", which can correspondingly extend the service life of the battery cell and improve the safety of the battery cell.
[0085] The battery cells disclosed in the embodiments of the present application can be used independently or in combination with other battery cells to form modular batteries that can provide higher voltage and capacity, such as battery modules, battery modules or battery packs. The battery cells and batteries disclosed in the embodiments of the present application can be used in electrical devices that use battery cells and batteries as power sources, or in various energy storage systems that use battery cells and batteries as energy storage elements. The electrical devices may be, but are not limited to, vehicles, mobile phones, portable devices, laptops, ships, spacecraft, electric toys and power tools, etc. Vehicles may be fuel vehicles, gas vehicles or new energy vehicles, and new energy vehicles may be pure electric vehicles, hybrid vehicles or extended-range vehicles, etc. Spacecraft include airplanes, rockets, space shuttles and spacecraft, etc. Electric toys include fixed or mobile electric toys, such as game consoles, electric car toys, electric ship toys and electric airplane toys, etc. Power tools include metal cutting power tools, grinding power tools, assembly power tools and railway power tools, such as electric drills, electric grinders, electric wrenches, electric screwdrivers, electric hammers, impact drills, concrete vibrators and electric planers, etc.
[0086] In order to illustrate the technical solution provided by the present application, the following is a detailed description with reference to specific drawings and embodiments, taking "the electrical device being a vehicle" as an example.
[0087] Please refer to Figure 1, which is a schematic structural diagram of a vehicle provided in some embodiments of the present application. The vehicle can be a fuel vehicle, a gas vehicle or a new energy vehicle. The new energy vehicle can be a pure electric vehicle, a hybrid vehicle or an extended-range vehicle, etc. A battery 1 is provided inside the vehicle, and the battery 1 can be provided at the bottom, head or tail of the vehicle. The battery 1 is used to power the vehicle. For example, the battery 1 can be used as an operating power source for the vehicle. The vehicle may also include a controller 2 and a motor 3. The controller 2 is used to control the battery 1 to power the motor 3, for example, for starting, navigating and operating power requirements during driving of the vehicle.
[0088] In some embodiments of the present application, the battery 1 can serve not only as the operating power source of the vehicle, but also as the driving power source of the vehicle, replacing or partially replacing fuel or natural gas to provide driving power for the vehicle.
[0089] Please refer to Figure 2, which is an exploded schematic diagram of a battery 1 provided in some embodiments of the present application. The battery 1 includes a battery cell 100 and a housing 200, with the battery cell 100 housed within the housing 200. The housing 200 is used to provide a storage space for the battery cell 100 and can have various structures. In some embodiments, the housing 200 can include a first portion 201 and a second portion 202, which overlap with each other and together define a storage space for the battery cell 100. The second portion 202 can be a hollow structure with one end open, and the first portion 201 can be a plate-like structure, with the first portion 201 overlapping the open side of the second portion 202, so that the first portion 201 and the second portion 202 jointly define a storage space. Alternatively, the first portion 201 and the second portion 202 can each be a hollow structure with one end open, with the open side of the first portion 201 overlapping the open side of the second portion 202. Of course, the box body 200 formed by the first part 201 and the second part 202 can be in various shapes, such as a cylinder, a cuboid, etc.
[0090] In the battery 1 , there may be multiple battery cells 100 , and the multiple battery cells 100 may be connected in series, in parallel, or in mixed connection. Mixed connection means that the multiple battery cells 100 are connected in both series and in parallel.
[0091] Specifically, the battery unit 100 can be a battery cell. Multiple battery cells can be directly connected in series, in parallel, or in a mixed manner, and then the battery cell structure can be housed in the housing 200. The battery cell can be a lithium-ion secondary battery, a lithium-ion primary battery, a lithium-sulfur battery, a sodium-lithium-ion battery, a sodium-ion battery, or a magnesium-ion battery, etc.; the battery cell can be cylindrical, flat, rectangular, or in other shapes, etc.; the battery cell can be packaged in different ways to form a cylindrical battery cell, a square battery cell, or a soft-pack battery cell, etc.; this application does not impose any restrictions on this.
[0092] Alternatively, the battery unit 100 may be a battery module or battery assembly. Multiple battery cells may be connected in series, parallel, or in series to form a modular structure, i.e., a battery module or battery assembly. Multiple battery modules or battery assembly may then be connected in series, parallel, or in series to form a single unit, which is then housed within the housing 200.
[0093] Of course, the battery 1 may also include other structures. For example, the battery 1 may also include a busbar component (not shown in the figure) for achieving electrical connection between the multiple battery cells 100 .
[0094] Of course, in some embodiments, the battery 1 may not include the box body 200 , but rather a plurality of battery cells may be electrically connected and formed into a whole through necessary fixing structures and then assembled into an electrical device.
[0095] Please refer to Figures 3 and 4, which are schematic diagrams of the battery cell structure provided in some embodiments of the present application. A battery cell is the smallest unit that stores and outputs electrical energy. A battery cell includes components such as an electrode assembly 10, an electrolyte 20, a housing 30, and an end cap 40.
[0096] The end cap 40 is a component that covers the opening of the housing 30 to isolate the internal environment of the battery cell from the external environment. In some embodiments, the shape of the end cap 40 can be adapted to match the shape of the housing 30 to fit the housing 30. In some embodiments, the end cap 40 can be made of a material with a certain degree of hardness and strength. This prevents deformation when subjected to compression or collision, thereby enhancing the structural strength and safety of the battery cell. Of course, this embodiment does not limit the material of the end cap 40; the end cap 40 can be made of copper, iron, aluminum, stainless steel, aluminum alloy, plastic, and other materials. In some embodiments, the end cap 40 may be provided with functional components such as electrode terminals 50. The electrode terminals 50 can be used to electrically connect to the electrode assembly 10 for inputting or outputting electrical energy. In some embodiments, the end cap 40 may also be provided with a pressure relief mechanism (not shown) to release internal pressure when the internal pressure or temperature of the battery cell reaches a threshold. In some embodiments, an insulating member (not shown) may be provided inside the end cap 40 to isolate the electrical connection components within the housing 30 from the end cap 40 to reduce the risk of short circuits. Alternatively, the insulating member may be made of plastic, rubber, or the like.
[0097] The housing 30 is a component that cooperates with the end cap 40 to form the internal environment of the battery cell. The internal environment formed by the housing 30 and the end cap 40 can be used to accommodate components such as the electrode assembly 10 and the electrolyte 20. In some embodiments, the housing 30 and the end cap 40 can be separate components. An opening can be provided in the housing 30, and the end cap 40 is placed over the opening to form the internal environment of the battery cell. In some embodiments, the end cap 40 and the housing 30 can also be integrated. Specifically, the end cap 40 and the housing 30 can form a common connection surface before other components are inserted into the housing. When the interior of the housing 30 needs to be enclosed, the end cap 40 is placed over the housing 30. The housing 30 can be of various shapes and sizes, such as a rectangular parallelepiped, a cylinder, a hexagonal prism, etc. Specifically, the shape of the housing 30 can be determined based on the specific shape and size of the electrode assembly 10. The housing 30 can be made of a variety of materials, such as copper, iron, aluminum, stainless steel, aluminum alloy, plastic, etc., and this embodiment of the present application is not intended to be limiting.
[0098] The electrode assembly 10 is a component in the battery cell where electrochemical reactions occur. The housing 30 may include one or more electrode assemblies 10. Referring to Figure 5, the electrode assembly 10 includes a positive electrode sheet 11, a negative electrode sheet 12, and a separator 13. The separator 13 separates the positive electrode sheet 11 from the negative electrode sheet 12. The positive electrode sheet 11, the negative electrode sheet 12, and the separator 13 separating the positive electrode sheet 11 from the negative electrode sheet 12 can be processed by winding to form a roll structure. The electrode assembly 10 in a roll structure has a main body area 16 and a bending area 17 arranged on the end side of the main body area 16. Among them, the parts of the positive electrode sheet 11 and the negative electrode sheet 12 that do not have active materials each constitute a pole ear, which is the current transmission end of the electrode assembly 10, used to connect to the electrode terminal 50 and transmit current. The tab of the positive electrode sheet 11 is the positive electrode tab 111 , and the tab of the negative electrode sheet 12 is the negative electrode tab 121 . The positive electrode tab 111 and the negative electrode tab 121 can be located together on one side of the main body area 16 or respectively on two opposite sides of the main body area 16 .
[0099] The electrolyte 20 is the liquid that soaks the electrode assembly 10. When the battery cell is charging, the positive electrode plate 11 generates active ions. These active ions can penetrate the pores of the separator 13, travel through the electrolyte 20 to the negative electrode plate 12, and become embedded in the negative active material of the negative electrode plate 12. Conversely, when the battery cell is discharging, the active ions embedded in the negative active material of the negative electrode plate 12 are released. The released active ions can penetrate the pores of the separator 13, travel through the electrolyte 20 to the positive electrode plate 11, and become embedded in the positive active material of the positive electrode plate 11.
[0100] Referring to Figures 4, 5, 6, and 7, some embodiments of the present application provide a battery cell, which includes at least one electrode assembly 10. The electrode assembly 10 includes a positive electrode sheet 11, a negative electrode sheet 12, a separator 13, an insulating layer 14, and a glue layer 15. The positive electrode sheet 11, the separator 13, and the negative electrode sheet 12 are stacked and wound, and the electrode assembly 10 has a bending area 17. At least a portion of the insulating layer 14 and at least a portion of the glue layer 15 are arranged in the bending area 17, and the insulating layer 14 is bonded to the positive electrode sheet 11 or the negative electrode sheet 12 through the glue layer 15. In the thickness direction of the insulating layer 14, the projected area of the glue layer 15 is smaller than the projected area of the insulating layer 14.
[0101] It should be noted that the electrode assembly 10 is a component in a battery cell where electrochemical reactions occur. One or more electrode assemblies 10 may be disposed inside a battery cell.
[0102] In the electrode assembly 10, the positive electrode sheet 11 is a continuous positive electrode sheet 11, the negative electrode sheet 12 is a continuous negative electrode sheet 12, and the separator 13 is a continuous separator 13. Two continuous separators 13 are provided. Before winding, one continuous separator 13 is provided between the continuous positive electrode sheet 11 and the continuous negative electrode sheet 12, and the other continuous separator 13 is provided on the side of the continuous negative electrode sheet 12 away from the continuous positive electrode sheet 11, or on the side of the continuous positive electrode sheet 11 away from the continuous negative electrode sheet 12. Based on this, when the positive electrode sheet 11, the separator 13 and the negative electrode sheet 12 are wound and pre-pressed to form a rolled structure, the two continuous separators 13 can separate the positive electrode sheet 11 and the negative electrode sheet 12 to prevent the positive electrode sheet 11 and the negative electrode sheet 12 from direct contact and causing a short circuit. Among them, the separator 13 has a number of pores that allow active ions to penetrate freely.
[0103] As shown in FIG5 , the rolled electrode assembly 10 has a main body region 16 and a bending region 17. The main body region 16 is located relatively centrally within the rolled structure, while the bending region 17 is located at the end of the rolled structure and is bent. There may be one or more bending regions 17.
[0104] It should also be noted that in the electrode assembly 10, the insulating layer 14 can be provided in one bending region 17, or in multiple bending regions 17. In a bending region 17 provided with an insulating layer 14, one or more insulating layers 14 can be provided. Referring also to FIG8 , the length direction a of the insulating layer 14 corresponds to the extension direction of the electrode sheet and is also the winding direction of the electrode sheet; the width direction b of the insulating layer 14 corresponds to the width direction of the electrode sheet; and the thickness direction of the insulating layer 14 is perpendicular to its length and width directions and also corresponds to the thickness direction of the electrode sheet.
[0105] The insulating layer 14 is provided with an adhesive layer 15 along one side of its thickness. The insulating layer 14 can be bonded to the inside or outside of the bent portion of any circle of the positive electrode tab 11 through the adhesive layer 15. In this case, the insulating layer 14 is located between the bent portion of the positive electrode tab 11 and the separator 13. The insulating layer 14 can also be bonded to the inside or outside of the bent portion of any circle of the negative electrode tab 12 through the adhesive layer 15. In this case, the insulating layer 14 is located between the bent portion of the negative electrode tab 12 and the separator 13.
[0106] Specifically, before winding, the insulating layer 14 can be bonded to a specific position of the continuous positive electrode sheet 11 or the continuous negative electrode sheet 12 via the adhesive layer 15 to stabilize the relative position and state of the insulating layer 14 with respect to the electrode sheet. Based on this, during the winding process of the electrode assembly 10, it can be ensured that the insulating layer 14 and the adhesive layer 15 can be wound along with the continuous positive electrode sheet 11 or the continuous negative electrode sheet 12 in a stable position and state relative to the electrode sheet, and wound to the bending region 17. This allows for convenient and quick installation of the insulating layer 14 and the adhesive layer 15, convenient and quick formation of the electrode assembly 10, and effectively ensures and improves the production efficiency and production yield of the electrode assembly 10.
[0107] The adhesive layer 15 and the insulating layer 14 are both resistant to electrolyte, meaning they are not easily dissolved in the electrolyte 20. Consequently, when the electrode assembly 10 and the electrolyte 20 are encapsulated within the battery cell, and during the battery cell's use, the insulating layer 14 is reliably bonded and fixed to the electrode via the adhesive layer 15, firmly stabilizing their relative position and state. This effectively reduces the risk of displacement or detachment of the insulating layer 14, ensuring that the insulating layer 14 can function durably, stably, and reliably in its specific position during the battery cell's use.
[0108] Among them, the insulating layer 14 has excellent insulation properties. Based on this, when the insulating layer 14 is set at the bent portion of any circle of the positive electrode plate 11, even during the charging process of the battery cell, active ions are analyzed from the bent portion of the negative electrode plate 12, and as the battery cell is used for a longer time, dendrites grow from the defects in the bent portion of the diaphragm 13. By setting the insulating layer 14 at the bent portion of any circle of the positive electrode plate 11, the growing dendrites can be insulated and blocked, preventing the dendrites from directly contacting and conducting the positive electrode plate 11 and the negative electrode plate 12, and even to a certain extent hindering and slowing the growth rate of the dendrites. This can effectively delay the occurrence of the phenomenon of "dendrites directly causing internal short circuits in the battery cell", and can effectively delay the occurrence of the phenomenon of "dendrites heating up due to short circuits and melting the diaphragm 13 on the side of the dendrites, causing the positive electrode plate 11 and the negative electrode plate 12 to directly contact and short circuit at the melted diaphragm 13", thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0109] Similarly, when the insulating layer 14 is provided on the bent portion of any circle of the negative electrode sheet 12, even when the active ions are released from the bent portion of the negative electrode sheet 12 during the charging process of the battery cell, the insulating layer 14 provided on the bent portion of any circle of the negative electrode sheet 12 can also shield and protect the bent portion of the diaphragm 13. This can effectively delay the occurrence of the phenomenon of "the released active ions breaking through the insulating layer 14 and growing dendrites from the defects in the bent portion of the diaphragm 13", effectively delay the occurrence of the phenomenon of "the dendrites directly causing a short circuit inside the battery cell", and effectively delay the occurrence of the phenomenon of "the dendrites heating up due to the short circuit and melting the diaphragm 13 on the side of the dendrites, causing the positive electrode sheet 11 part and the negative electrode sheet 12 part where the diaphragm 13 melts directly to short circuit", thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0110] The insulating layer 14 has excellent buffering properties. Therefore, during the winding and pre-pressing of the electrode assembly 10 and during the use of the battery cell, the insulating layer 14 can buffer the large bending stresses borne by the bent portion of the electrode sheet. This effectively reduces the risk of tearing defects in the bent portion of the electrode sheet, leading to a reduction in active material, and the risk of metal precipitation in the bent region 17 of the electrode assembly 10 due to a reduction in active material. It can also effectively slow the growth rate of dendrites, thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0111] In the thickness direction of the insulating layer 14, the projected area of the adhesive layer 15 is smaller than the projected area of the insulating layer 14. That is, the adhesive layer 15 is applied to a portion of the side surface of the insulating layer 14. Based on this, during the winding and pre-pressing of the electrode assembly 10 and during the use of the battery cell, the adhesive layer 15 can stabilize the position and state of the insulating layer 14 relative to the electrode sheet, effectively reducing the negative impact of the adhesive layer 15 on the extension and deformation properties of the insulating layer 14. This allows the insulating layer 14 to extend and deform adaptively with the electrode sheet, allowing the insulating layer 14 to function durably and reliably during the use of the battery cell, effectively reducing the risk of tearing defects in the insulating layer 14 during the use of the battery cell, and effectively ensuring and extending the service life of the insulating layer 14.
[0112] In summary, the battery cell provided in the embodiment of the present application can firmly and reliably bond the insulating layer 14 to the bent part of any circle of the positive electrode plate 11 or the negative electrode plate 12 through the adhesive layer 15, so that the insulating layer 14 can be durably and reliably stabilized in the bending area 17 during the use of the battery cell, which can effectively reduce the risk of displacement and falling off of the insulating layer 14, thereby ensuring that the insulating layer 14 can durably, stably and reliably perform its function in a specific position during the use of the battery cell. Furthermore, by making the projected area of the adhesive layer 15 in the thickness direction of the insulating layer 14 smaller than the projected area of the insulating layer 14 in its thickness direction, the negative impact of the adhesive layer 15 on the elongation and deformation properties of the insulating layer 14 can be effectively reduced during the winding and pre-pressing of the electrode assembly 10 and during the use of the battery cell. This allows the insulating layer 14 to extend and deform adaptively with the pole piece, allowing the insulating layer 14 to function durably and reliably during the use of the battery cell, effectively reducing the risk of tearing defects in the insulating layer 14 during the use of the battery cell, and correspondingly ensuring and extending the service life of the insulating layer 14.
[0113] On this basis, the battery cell provided in the embodiment of the present application can also form a buffering effect on the bending stress borne by the bent part of the electrode piece through the insulating layer 14 provided in the bending area 17 during the winding and pre-pressing of the electrode assembly 10 and during the use of the battery cell, thereby effectively reducing the risk of tearing defects in the bent part of the electrode piece leading to a reduction in active material, and effectively reducing the risk of metal precipitation in the bending area 17 of the electrode assembly 10 due to the reduction of active material, and effectively alleviating the growth rate of dendrites, thereby correspondingly extending the service life of the battery cell and correspondingly improving the safety of the battery cell. Moreover, even if dendrites grow in the bending area 17 of the electrode assembly 10 as the usage time increases, the insulating layer 14 with insulating properties can form an insulating barrier to the dendrites growing toward it, thereby preventing the dendrites from directly contacting the conductive positive electrode plate 11 and the negative electrode plate 12, and even hindering and delaying the growth of the dendrites, thereby effectively delaying the occurrence of the phenomenon of "dendrites directly causing internal short circuits in the battery cell", and effectively delaying the occurrence of the phenomenon of "dendrites heating up due to short circuits and melting the diaphragm 13 on the side of the dendrites, causing direct contact and short circuit between the positive electrode plate 11 part and the negative electrode plate 12 part where the diaphragm 13 melts", which can correspondingly extend the service life of the battery cell and improve the safety of the battery cell.
[0114] Please refer to FIG. 6 , FIG. 7 , and FIG. 8 . In some embodiments of the present application, the adhesive layer 15 includes a plurality of adhesives 151 , and at least a portion of the adhesives 151 is distributed in the edge region of the insulating layer 14 .
[0115] It should be noted that, based on the setting that "in the thickness direction of the insulating layer 14, the projected area of the adhesive layer 15 is smaller than the projected area of the insulating layer 14", this embodiment divides the adhesive layer 15 into multiple colloids 151, and any two colloids 151 can be set in abutment with each other or can be set at intervals, and this embodiment does not impose any restrictions on this.
[0116] The insulating layer 14 has multiple edges along one side of its thickness direction. For example, when the insulating layer 14 is a rectangular parallelepiped, the insulating layer 14 has four edges along one side of its thickness direction.
[0117] At least some of the colloids 151 are distributed along the edge of the insulating layer 14, that is, at least some of the colloids 151 are disposed near the edge of the insulating layer 14. For example, one colloid 151 may be disposed near one edge of the insulating layer 14. For another example, four colloids 151 may be disposed near four edges of the insulating layer 14.
[0118] By adopting the above solution, the insulating layer 14, especially the edge of the insulating layer 14, can be firmly and reliably bonded to the bent portion of any positive electrode sheet 11 or negative electrode sheet 12 through multiple colloids 151, especially the colloids 151 disposed near the edge of the insulating layer 14. This allows the insulating layer 14 to be permanently and reliably positioned and function effectively. Furthermore, while ensuring the adhesive layer 15's ability to secure the insulating layer 14, the number of colloids 151 disposed and the area they occupy can be reduced, effectively reducing the negative impact of the adhesive layer 15 on the elongation and deformation properties of the insulating layer 14. This allows the insulating layer 14 to adapt to the elongation and deformation of the electrode sheet, thereby ensuring the effectiveness and service life of the insulating layer 14.
[0119] Please refer to FIG. 6 , FIG. 7 , and FIG. 8 . In some embodiments of the present application, the colloid 151 is a strip-shaped colloid 151 , and a plurality of colloids 151 are spaced apart along the width direction b of the insulating layer 14 .
[0120] It should be noted that the colloid 151 is a strip-shaped colloid 151, that is, the colloid 151 is arranged in a strip-shaped extension. Multiple colloids 151 are arranged at intervals along the width direction b of the insulating layer 14, that is, multiple colloids 151 are arranged in sequence along the width direction b of the insulating layer 14. The extension direction of the colloid 151 intersects with the width direction b of the insulating layer 14. For example, the extension direction of the colloid 151 can be parallel to the length direction a of the insulating layer 14.
[0121] By adopting the above solution, multiple strips of colloid 151 can be arranged in sequence along the width direction b of the insulating layer 14, allowing for an optimized layout of the multiple colloids 151 on one side of the insulating layer 14. In particular, the two colloids 151 that are farthest apart along the width direction b of the insulating layer 14 can be positioned close to the two side edges of the insulating layer 14. This ensures that each strip of colloid 151 can firmly and reliably bond the insulating layer 14, especially the two side edges of the insulating layer 14, to the bent portion of any electrode, thereby ensuring that the insulating layer 14 can be permanently and reliably positioned and function effectively. Furthermore, while optimizing the layout of each strip of colloid 151 to ensure the tightening effect of the insulating layer 14, the number of colloids 151 installed and the area they occupy can be effectively reduced, thereby effectively reducing the negative impact of the adhesive layer 15 on the elongation and deformation properties of the insulating layer 14. This allows the insulating layer 14 to extend and deform adaptively with the electrode, thereby ensuring the effectiveness and service life of the insulating layer 14. On the one hand, while the insulating layer 14 is extending and deforming adaptively with the pole piece, the plurality of strip-shaped colloids 151 can be spaced apart and extended and deformed adaptively with the insulating layer 14 , thereby ensuring that the adhesive layer 15 can permanently and reliably fasten the insulating layer 14 .
[0122] Please refer to FIG. 6 , FIG. 7 , and FIG. 9 . In some embodiments of the present application, the colloid 151 is a strip-shaped colloid 151 , and a plurality of colloids 151 are spaced apart along the length direction a of the insulating layer 14 .
[0123] It should be noted that the colloid 151 is a strip-shaped colloid 151, that is, the colloid 151 is arranged in a strip-shaped extension. Multiple colloids 151 are arranged at intervals along the longitudinal direction a of the insulating layer 14, that is, multiple colloids 151 are arranged in sequence along the longitudinal direction a of the insulating layer 14. The extension direction of the colloid 151 intersects the longitudinal direction a of the insulating layer 14. For example, the extension direction of the colloid 151 can be parallel to the width direction b of the insulating layer 14.
[0124] By adopting the above solution, multiple strips of colloid 151 can be arranged in sequence along the length direction a of the insulating layer 14, allowing for an optimized layout of the multiple colloids 151 on one side of the insulating layer 14. In particular, the two colloids 151 that are farthest apart along the length direction a of the insulating layer 14 can be positioned close to the two side edges of the insulating layer 14. This ensures, on the one hand, that each strip of colloid 151 can firmly and reliably adhere the insulating layer 14, particularly the two side edges of the insulating layer 14, to the bent portion of any coil of the electrode, thereby ensuring that the insulating layer 14 can be permanently and reliably positioned and function effectively. On the other hand, while optimizing the layout of each strip of colloid 151 to ensure the tightening effect of the insulating layer 14, the number of colloids 151 installed and the area they occupy can be effectively reduced, thereby effectively reducing the negative impact of the adhesive layer 15 on the elongation and deformation properties of the insulating layer 14. This facilitates the insulating layer 14 to extend and deform adaptively with the electrode, thereby ensuring the effectiveness and service life of the insulating layer 14. On the one hand, while the insulating layer 14 is extending and deforming adaptively with the pole piece, the plurality of strip-shaped colloids 151 can be spaced apart and extended and deformed adaptively with the insulating layer 14 , thereby ensuring that the adhesive layer 15 can permanently and reliably fasten the insulating layer 14 .
[0125] Please refer to FIG. 6 , FIG. 7 , and FIG. 10 . In some embodiments of the present application, the colloid 151 is a block-shaped colloid 151 , and at least a portion of the colloid 151 is distributed at each corner of the insulating layer 14 .
[0126] It should be noted that the colloid 151 is a block-shaped colloid 151 , for example, a circular block-shaped colloid 151 , or a rectangular block-shaped colloid 151 .
[0127] The insulating layer 14 has a plurality of corners on one side along the thickness direction. For example, when the insulating layer 14 is a rectangular parallelepiped, the insulating layer 14 has four corners on one side along the thickness direction.
[0128] At least some of the multiple block-shaped colloids 151 are distributed at the corners of the insulating layer 14. For example, if the insulating layer 14 has four corners along one side in the thickness direction, four or more block-shaped colloids 151 may be respectively disposed at the four corners of the insulating layer 14. The block-shaped colloids 151 distributed at the corners of the insulating layer 14 may be disposed close to the edge of the insulating layer 14.
[0129] By adopting the above scheme, the insulating layer 14, especially the corners and edges of the insulating layer 14, can be firmly and reliably bonded to the bent portion of any coil of the electrode through multiple block-shaped colloids 151, especially the block-shaped colloids 151 distributed at the corners of the insulating layer 14, so that the insulating layer 14 can be permanently and reliably stabilized and function effectively. In addition, because the colloids 151 are block-shaped and multiple block-shaped colloids 151 can be optimally arranged on one side of the insulating layer 14, it is beneficial to effectively reduce the number of colloids 151 and the area occupied by them while ensuring the fastening effect of the adhesive layer 15 on the insulating layer 14, thereby effectively reducing the negative impact of the adhesive layer 15 on the extension and deformation performance of the insulating layer 14, thereby facilitating the insulating layer 14 to extend and deform adaptively with the electrode, which is beneficial to ensuring the effectiveness and service life of the insulating layer 14. Furthermore, while the insulating layer 14 is extending and deforming adaptively with the pole piece, the plurality of block-shaped colloids 151 can be spaced apart adaptively with the insulating layer 14 , thereby ensuring that the overall fastening effect of the adhesive layer 15 on the insulating layer 14 is long-lasting and effective.
[0130] Please refer to FIG. 4 , FIG. 6 , and FIG. 7 . In some embodiments of the present application, the adhesive layer 15 is a hot melt adhesive that is resistant to the electrolyte 20 .
[0131] It should be noted that hot melt adhesive is a plastic adhesive that is solid at room temperature and can quickly bond after being heated and melted. Hot melt adhesive has the characteristics of fast bonding, strong bonding, stable performance, and low cost.
[0132] By adopting this solution, adhesive layer 15 can be formed using a hot melt adhesive that exhibits rapid, strong, and stable bonding properties, thereby conveniently, quickly, and reliably bonding insulating layer 14 to the bent portion of the electrode. Furthermore, the hot melt adhesive's resistance to electrolyte 20 ensures that adhesive layer 15 maintains a long-lasting and effective fastening effect on insulating layer 14 during the battery's lifetime.
[0133] Referring to FIG. 6 , FIG. 7 , and FIG. 8 , in some embodiments of the present application, in the thickness direction of the insulating layer 14 , the ratio of the projected area of the adhesive layer 15 to the projected area of the insulating layer 14 is 20%-50%.
[0134] It should be noted that, in the thickness direction of the insulating layer 14, the projected area of the adhesive layer 15 is smaller than the projected area of the insulating layer 14. By dividing the projected area of the adhesive layer 15 by the projected area of the insulating layer 14, the ratio of the projected area of the adhesive layer 15 to the projected area of the insulating layer 14 can be obtained. This ratio is 20% to 50%, for example, 25%.
[0135] By adopting the above-mentioned scheme, during the winding and pre-pressing of the electrode assembly 10 and during the use of the battery cell, the area ratio of the glue layer 15 relative to the insulating layer 14 can be effectively reduced on the basis of ensuring the fastening effect of the glue layer 15 on the insulating layer 14, thereby effectively reducing the negative impact of the glue layer 15 on the extension and deformation performance of the insulating layer 14, thereby facilitating the insulating layer 14 to extend and deform adaptively with the pole piece, facilitating the insulating layer 14 to perform its function durably and reliably during the use of the battery cell, effectively reducing the risk of tearing defects in the insulating layer 14 during the use of the battery cell, and effectively ensuring and extending the service life of the insulating layer 14.
[0136] Please refer to FIG. 6 , FIG. 7 , and FIG. 8 . In some embodiments of the present application, the thickness of the adhesive layer 15 is 2 um to 8 um.
[0137] It should be noted that the thickness of the adhesive layer 15 refers to the dimension of the adhesive layer 15 along the thickness direction thereof, that is, the dimension of the adhesive layer 15 along the thickness direction of the insulating layer 14 .
[0138] By adopting the above solution, the thickness of the adhesive layer 15 can be effectively reduced while ensuring the fastening effect of the adhesive layer 15 on the insulating layer 14, thereby facilitating the protection and improvement of the energy density of the electrode assembly 10 and the battery cell.
[0139] Please refer to FIG. 5 , FIG. 6 , and FIG. 7 . In some embodiments of the present application, in the bending region 17 , at least one insulating layer 14 is bonded to the inner side of the innermost positive electrode plate 112 through an adhesive layer 15 .
[0140] It should be noted that in the electrode assembly 10, an insulating layer 14 may be provided in one bending region 17, or in multiple bending regions 17. In the bending regions 17 provided with insulating layers 14, at least one insulating layer 14 is bonded to the inner side of the bent portion of the innermost positive electrode tab 112 via an adhesive layer 15.
[0141] Because the radius of curvature decreases toward the innermost circle, the bent portion of the innermost positive electrode tab 112 and the bent portion of the innermost negative electrode tab 122 are subject to greater bending stress and are more susceptible to powder loss, resulting in metal deposition between the bent portion of the innermost positive electrode tab 112 and the bent portion of the innermost negative electrode tab 122. Furthermore, because the bent portion of the innermost positive electrode tab 112 is relatively outward of the bent portion of the innermost negative electrode tab 122, metal deposition is likely to occur from the bent portion of the innermost negative electrode tab 122 during battery cell charging.
[0142] Therefore, by adopting the above scheme, on the one hand, when "metal precipitation occurs at the bent portion of the innermost circle negative electrode sheet 122, and dendrites grow from the defects of the bent portion of the diaphragm 13 over time", the growing dendrites can be insulated and blocked by the insulating layer 14 arranged on the inner side of the bent portion of the innermost circle positive electrode sheet 112 to prevent the dendrites from directly contacting the conductive positive electrode sheet 11 and the negative electrode sheet 12. This can effectively delay the occurrence of the phenomenon of "dendrites directly causing internal short circuits in the battery cell" between the innermost circle positive electrode sheet 112 and the innermost circle negative electrode sheet 122 where metal precipitation is easily generated, and effectively delay the occurrence of the phenomenon of "dendrites heating up due to short circuits and melting the diaphragm 13 on the side of the dendrites, causing direct contact and short circuit between the positive electrode sheet 11 and the negative electrode sheet 12 where the diaphragm 13 melts", thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0143] On the other hand, during the winding and pre-pressing of the electrode assembly 10 and during the use of the battery cell, the insulating layer 14 disposed inside the bent portion of the innermost positive electrode tab 112 can buffer the compressive stress borne by the bent portion of the innermost positive electrode tab 112, thereby reducing the risk of tearing defects in the bent portion of the innermost positive electrode tab 112, which leads to a reduction in active material. It can even buffer the tensile stress borne by the bent portion of the innermost negative electrode tab 122, thereby reducing the risk of tearing defects in the bent portion of the innermost negative electrode tab 122, which leads to a reduction in active material. This can effectively reduce the risk of metal precipitation due to the reduction in active material, and can effectively alleviate the growth rate of dendrites between the innermost positive electrode tab 112 and the innermost negative electrode tab 122, thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0144] Please refer to FIG. 5 , FIG. 6 , and FIG. 7 . In some embodiments of the present application, in the bending region 17 , at least one insulating layer 14 is bonded to the outer side of the innermost positive electrode plate 112 through an adhesive layer 15 .
[0145] It should be noted that in the electrode assembly 10, an insulating layer 14 may be provided in one bending region 17, or in multiple bending regions 17. In the bending regions 17 provided with insulating layers 14, at least one insulating layer 14 is bonded to the outer side of the bent portion of the innermost positive electrode tab 112 via an adhesive layer 15.
[0146] Because the bent portion of the innermost positive electrode tab 112 is subject to significant bending stress, the above-described solution allows the insulating layer 14 disposed outside the bent portion of the innermost positive electrode tab 112 to buffer the tensile stress experienced by the bent portion of the innermost positive electrode tab 112 during winding and pre-pressing of the electrode assembly 10 and during battery cell use, thereby reducing the risk of tearing defects in the bent portion of the innermost positive electrode tab 112, leading to a reduction in active material. Furthermore, the insulating layer 14 can buffer the compressive stress experienced by the bent portion of the second innermost negative electrode tab 123, thereby reducing the risk of tearing defects in the bent portion of the second innermost negative electrode tab 123, leading to a reduction in active material. This effectively reduces the risk of metal precipitation exacerbated by active material reduction and mitigates the growth rate of dendrites between the innermost positive electrode tab 112 and the second innermost negative electrode tab 123, thereby correspondingly extending the battery cell's service life and improving its safety.
[0147] The second innermost negative electrode sheet 123 is located outside the innermost positive electrode sheet 112. When the battery cell is charging, the active ions provided by the outer surface of the innermost positive electrode sheet 112 can move to the second innermost negative electrode sheet 123 and be embedded in the negative active material of the second innermost negative electrode sheet 123.
[0148] Therefore, by adopting the above solution, during the use of the battery cell, the insulating layer 14 provided on the outside of the bent portion of the innermost positive electrode tab 112 can be used to insulate and block the dendrites growing toward it, thereby preventing the dendrites from directly contacting and conducting the innermost positive electrode tab 112 and the second innermost negative electrode tab 123. This can effectively delay the occurrence of the phenomenon of "dendrites directly causing internal short circuits in the battery cell" between the innermost positive electrode tab 112 and the second innermost negative electrode tab 123, and effectively delay the occurrence of the phenomenon of "dendrites generating heat due to short circuits and melting the diaphragm 13 on the side of the dendrites, causing direct contact and short circuit between the positive electrode tab 11 and the negative electrode tab 12 where the diaphragm 13 melts", thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0149] Please refer to Figures 5, 6, and 7. In some embodiments of the present application, the bending area 17 is provided with two insulating layers 14, one of which is bonded to the inner side of the innermost positive electrode plate 112 through the adhesive layer 15, and the other insulating layer 14 is bonded to the outer side of the innermost positive electrode plate 112 through the adhesive layer 15.
[0150] It should be noted that in the electrode assembly 10, an insulating layer 14 may be provided in one bending region 17, or in multiple bending regions 17. In the bending region 17 provided with the insulating layer 14, an insulating layer 14 is provided on the inner side and the outer side of the bent portion of the innermost positive electrode tab 112, respectively. The insulating layer 14 is bonded to the tab via an adhesive layer 15.
[0151] By adopting the above solution, the bending zone 17 can effectively delay the risk of short circuits through the two insulating layers 14 in the "innermost positive electrode sheet 112 and the innermost negative electrode sheet 122" and "innermost positive electrode sheet 112 and the second innermost negative electrode sheet 123" where metal precipitation is likely to occur and the metal precipitation is relatively serious. It can also effectively relieve the compression stress and tensile stress at the bent portion of the innermost positive electrode sheet 112, which is subject to greater bending stress and is prone to tearing defects, thereby reducing the risk of bending and tearing, thereby effectively extending the service life of the battery cell and effectively improving the safety of the battery cell. While maximizing the effectiveness of the insulating layer 14, by adopting the above solution, the number of insulating layers 14 provided can also be reduced, thereby ensuring and improving the energy density of the electrode assembly 10 and the battery cell.
[0152] 5 , 6 , and 7 , in some embodiments of the present application, the electrode assembly 10 includes a main body region 16 and a bending region 17 disposed at an end of the main body region 16 . The insulating layer 14 includes a bent section 141 bent at the bending region 17 , and an extension section 142 connected to an end of the bent section 141 and disposed at the main body region 16 .
[0153] It should be noted that, as shown in Figure 5, the electrode assembly 10 with a rolled structure has a main area 16 and a bending area 17. The main area 16 is a relatively straight part of the rolled structure that is relatively located in the middle, while the bending area 17 is a bent part of the rolled structure that is located at the end side of the main area 16.
[0154] The insulating layer 14 has a curved section 141, which is disposed in the bend region 17, that is, on the inside or outside of the bent portion of the electrode. The insulating layer 14 has one or two extension sections 142. When one extension section 142 is provided, the extension section 142 extends from one end of the curved section 141 and is disposed in the main body region 16. When two extension sections 142 are provided, the two extension sections 142 extend from opposite ends of the curved section 141 and are both disposed in the main body region 16. The extension lengths of the two extension sections 142 can be the same or different.
[0155] Since the insulating layer 14 is bonded to the preset position of the continuous positive electrode sheet 11 or the continuous negative electrode sheet 12 through the adhesive layer 15 before winding, by adopting the above scheme, the setting area of the insulating layer 14 can be extended accordingly, and the preset position of the insulating layer 14 on the continuous positive electrode sheet 11 or the continuous negative electrode sheet 12 has a wider tolerance range, thereby effectively ensuring that when the electrode assembly 10 is wound, the insulating layer 14 can retain the bent section 141 clamped between the bent part of the electrode sheet and the diaphragm 13, and the extended section 142 that can extend to the main area 16 according to the position tolerance, thereby effectively reducing the accuracy requirements for the preset position of the insulating layer 14 on the continuous positive electrode sheet 11 or the continuous negative electrode sheet 12, and effectively ensuring and improving the production yield of the electrode assembly 10.
[0156] Please refer to FIG. 6 , FIG. 7 , and FIG. 8 . In some embodiments of the present application, the insulating layer 14 is provided with a plurality of holes.
[0157] It should be noted that the insulating layer 14 has multiple pores. Because the projected area of the adhesive layer 15 in the thickness direction of the insulating layer 14 is smaller than the projected area of the insulating layer 14 in the thickness direction, at least some of the multiple pores in the insulating layer 14 are not blocked by the adhesive layer 15. The pores not blocked by the adhesive layer 15 allow active ions to freely penetrate.
[0158] By adopting the above solution, during the charge and discharge process of the battery cell, active ions can freely penetrate the pores of the insulating layer 14 and the separator 13, and move between the positive electrode plate 11 and the negative electrode plate 12. This effectively ensures that the provision of the insulating layer 14 does not significantly affect the charge and discharge process of the battery cell, and effectively guarantees the charge and discharge performance of the battery cell.
[0159] Please refer to FIG. 5 , FIG. 6 , and FIG. 7 . In some embodiments of the present application, the absolute value of the difference between the porosity of the insulating layer 14 and the porosity of the diaphragm 13 is less than or equal to 25%.
[0160] It should be noted that in this embodiment, the porosity can be determined by the gas replacement method. Specifically, it can be determined by referring to GB / T 24586-2009 through the following steps: the insulating layer 14 or the diaphragm 13 is immersed in ethyl methyl carbonate (EMC) for cleaning, then filled into a specific device and measured using the gas replacement method. The porosity of the insulating layer 14 is the percentage of the pore volume in the insulating layer 14 to the total volume of the insulating layer 14, and the porosity of the diaphragm 13 is the percentage of the pore volume in the diaphragm 13 to the total volume of the diaphragm 13. Specifically, porosity = (V-V0) / V×100%, where V0 is the true volume and V is the apparent volume.
[0161] It should also be noted that the porosity of the insulating layer 14 can be greater than the porosity of the diaphragm 13, and the difference between the porosity of the insulating layer 14 and the porosity of the diaphragm 13 is less than or equal to 25%. For example, if the porosity of the insulating layer 14 is 50% and the porosity of the diaphragm 13 is 35%, the difference between the porosity of the insulating layer 14 and the porosity of the diaphragm 13 is 15%. For another example, if the porosity of the insulating layer 14 is 40% and the porosity of the diaphragm 13 is 35%, the difference between the porosity of the insulating layer 14 and the porosity of the diaphragm 13 is 5%.
[0162] The porosity of the insulating layer 14 may also be smaller than the porosity of the diaphragm 13 , and the difference between the porosity of the diaphragm 13 and the porosity of the insulating layer 14 is less than or equal to 25%.
[0163] By adopting the above solution, the porosity of the insulating layer 14 can be made not much different from the porosity of the diaphragm 13. Based on this, active ions can freely and normally penetrate the insulating layer 14 and the diaphragm 13, thereby effectively ensuring that the setting of the insulating layer 14 will not have a significant impact on the charging and discharging process of the battery cell, and effectively ensuring the charging and discharging performance of the battery cell.
[0164] Please refer to FIG. 5 , FIG. 6 , and FIG. 7 . In some embodiments of the present application, the absolute value of the difference between the porosity of the insulating layer 14 and the porosity of the diaphragm 13 is less than or equal to 10%.
[0165] By adopting the above solution, the porosity of the insulating layer 14 can be set to be similar to the porosity of the diaphragm 13. In this way, the active ions can freely and normally penetrate the insulating layer 14 and the diaphragm 13, and move between the positive electrode sheet 11 and the negative electrode sheet 12, thereby effectively ensuring that the setting of the insulating layer 14 will not have a significant impact on the charging and discharging process of the battery cell, and effectively ensuring the charging and discharging performance of the battery cell.
[0166] Please refer to FIG. 5 , FIG. 6 , and FIG. 7 . In some embodiments of the present application, the insulating layer 14 is a polyolefin membrane, such as a polypropylene (PP) membrane.
[0167] By adopting the above scheme, the insulating layer 14 can be made of a polyolefin diaphragm such as a polypropylene diaphragm to ensure that the porosity of the insulating layer 14 is similar to or even the same as the porosity of the diaphragm 13, thereby ensuring that active ions can freely and normally penetrate the insulating layer 14 and the diaphragm 13, and effectively ensuring that the setting of the insulating layer 14 will not have a significant impact on the charging and discharging process of the battery cell, thereby effectively ensuring the charging and discharging performance of the battery cell.
[0168] Please refer to FIG. 6 , FIG. 7 , and FIG. 8 . In some embodiments of the present application, the porosity of the insulating layer 14 is 40% to 50%.
[0169] It should be noted that, in theory, the greater the porosity of the insulating layer 14, the better the air permeability. However, as the porosity of the insulating layer 14 increases, when the same mass of adhesive layer 15 is applied to the side of the insulating layer 14, the amount of glue that penetrates into the pores of the insulating layer 14 will increase, and the amount of glue remaining on the surface of the insulating layer 14 will decrease, resulting in a decrease in the air permeability of the insulating layer 14 and the adhesion of the adhesive layer 15. This will lead to a decrease in the fixing effect between the insulating layer 14 and the electrode, resulting in a decrease in the penetration rate of active ions and electrical conductivity.
[0170] Therefore, by adopting the above solution, on the one hand, the air permeability of the insulating layer 14 can be ensured to be moderate, and the active ions can be guaranteed to freely and normally penetrate the insulating layer 14. On the other hand, it can ensure that when the adhesive layer 15 is applied to the side of the insulating layer 14, a small amount of glue penetrates into the pores of the insulating layer 14, while a large amount of glue remains on the surface of the insulating layer 14. This ensures the adhesion of the adhesive layer 15, ensures that the insulating layer 14 can be reliably fixed to the electrode via the adhesive layer 15, and reduces the blocking effect of the adhesive layer 15 on the pores of the insulating layer 14. It ensures that the active ions can freely and normally penetrate the insulating layer 14, and thus ensures the electrical conductivity.
[0171] Please refer to FIG. 6 , FIG. 7 , and FIG. 8 . In some embodiments of the present application, the pore diameter of the holes in the insulating layer 14 is A, the thickness of the insulating layer 14 is B, and 24≤B / A≤400.
[0172] It should be noted that the insulating layer 14 has a plurality of pores, and the pore diameter A of the insulating layer 14 refers to the radial size of each pore of the insulating layer 14 .
[0173] It is understandable that the aperture A of each hole in the insulating layer 14 may be exactly the same or different. The aperture may refer to the aperture when the apertures of the holes are the same, or the aperture of any part of the holes when the apertures of the holes are not exactly the same.
[0174] It is understood that the shape of each hole in the insulating layer 14 can be circular or other shapes such as rectangular. When the hole is circular, the hole diameter A refers to the hole diameter; when the hole is rectangular or other shapes, the hole diameter A refers to the size of the hole in the radial direction perpendicular to the central axis.
[0175] It should also be noted that the thickness B of the insulating layer 14 refers to the dimension of the insulating layer 14 along the thickness direction a thereof.
[0176] B / A refers to the ratio of the thickness B of the insulating layer 14 to the pore diameter A of the pores of the insulating layer 14 when the units are the same.
[0177] When B / A is less than 24, the thickness B of the insulating layer 14 will be too small, and the aperture A of the pores in the insulating layer 14 will be too large. In this case, dendrites will more easily pierce the insulating layer 14 or pass through the insulating layer 14, and the insulating layer 14 will not have a barrier effect.
[0178] When B / A is greater than 400, the thickness B of the insulating layer 14 will be too large, and the pore size A of the insulating layer 14 will be too small. At this time, the path for the active ions to shuttle through the insulating layer 14 will be too long. Moreover, because the pore size A of the insulating layer 14 is too small, the active ions have difficulty in shuttling, which may easily cause more active ions to precipitate.
[0179] Therefore, by adopting the above solution, the thickness B of the insulating layer 14 and the pore diameter A of the insulating layer 14 can be both moderate. Based on this, on the one hand, it is difficult for dendrites to pierce or pass through the insulating layer 14, thereby ensuring the insulating layer 14's dendrite barrier effect; on the other hand, it allows active ions to easily shuttle through the insulating layer 14 and the shuttle path is short, thereby reducing the risk of active ion precipitation due to shuttle difficulties. As a result, the service life of the battery cell can be effectively extended, and the safety of the battery cell can be effectively improved.
[0180] Please refer to FIG. 6 , FIG. 7 , and FIG. 8 . In some embodiments of the present application, the pores of the insulating layer 14 have a diameter of 0.05 um to 0.5 um.
[0181] It should be noted that, in theory, the larger the pore size of the insulating layer 14, the better the air permeability. However, as the pore size of the insulating layer 14 increases, when the same mass of glue layer 15 is applied to the side of the insulating layer 14, the amount of glue that penetrates into the pores of the insulating layer 14 will increase, and the amount of glue remaining on the surface of the insulating layer 14 will decrease, causing the air permeability of the insulating layer 14 and the adhesion of the glue layer 15 to deteriorate, thereby causing the fixing effect between the insulating layer 14 and the electrode to deteriorate, resulting in poor penetration and conductivity of active ions. In addition, as the pore size of the insulating layer 14 increases, during the use of the battery cell, the insulating layer 14 will have a poor barrier effect on dendrites growing from defects in the diaphragm 13, and there may even be a risk of dendrites growing from the pores of the insulating layer 14.
[0182] Therefore, by adopting the above solution, on the one hand, the air permeability of the insulating layer 14 can be ensured to be moderate, and the active ions can be ensured to freely and normally penetrate the pores of the insulating layer 14. On the other hand, it can be ensured that when the glue layer 15 is applied to the side of the insulating layer 14, the amount of glue that penetrates into the pores of the insulating layer 14 is small, while the amount of glue remaining on the surface of the insulating layer 14 is large, thereby ensuring the adhesion of the glue layer 15, ensuring that the insulating layer 14 can be reliably fixed to the electrode via the glue layer 15, and reducing the blocking effect of the glue layer 15 on the pores of the insulating layer 14, ensuring that active ions can freely and normally penetrate the insulating layer 14, and ensuring electrical conductivity. On the other hand, during the use of the battery cell, the insulating layer 14 can be guaranteed to have a blocking effect on dendrites growing from defects in the diaphragm 13, and reduce the risk of dendrites growing from the pores of the insulating layer 14, thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0183] Please refer to FIG. 6 , FIG. 7 , and FIG. 8 . In some embodiments of the present application, the thickness of the insulating layer 14 is 12 um to 20 um.
[0184] It should be noted that, in theory, the thicker the insulating layer 14, the better its insulation barrier effect on dendrites. However, as the thickness of the insulating layer 14 increases, the energy density of the battery cell decreases, and the penetration rate of active ions through the insulating layer 14 decreases, resulting in poor electrical conductivity and even exacerbated metal precipitation.
[0185] Therefore, by adopting the above-mentioned scheme, the thickness of the insulating layer 14 can be ensured to be moderate, so as to reduce the influence of the insulating layer 14 on the energy density of the battery cell and the penetration rate of active ions through the insulating layer 14 on the basis of ensuring that the insulating layer 14 can form a better insulating barrier effect on the dendrites growing toward it, thereby ensuring the electrical conductivity, ensuring the charging and discharging performance of the battery cell, extending the service life of the battery cell accordingly, and improving the safety of the battery cell accordingly.
[0186] Please refer to FIG. 6 , FIG. 7 , and FIG. 8 . In some embodiments of the present application, the adhesive layer 15 avoids the hole in the thickness direction of the insulating layer 14 .
[0187] It should be noted that, based on the setting that "in the thickness direction of the insulating layer 14, the projected area of the adhesive layer 15 is smaller than the projected area of the insulating layer 14", this embodiment can set the adhesive layer 15 to avoid the holes in the insulating layer 14 to prevent the adhesive layer 15 from blocking the holes in the insulating layer 14.
[0188] By adopting the above solution, the blocking effect of the glue layer 15 on the pores of the insulating layer 14 can be reduced to a great extent while ensuring the fastening effect of the glue layer 15 on the insulating layer 14. This allows the active ions to freely penetrate the pores of the insulating layer 14 and the diaphragm 13 during the charging and discharging process of the battery cell, thereby moving between the positive electrode sheet 11 and the negative electrode sheet 12. This effectively reduces the influence of the setting of the insulating layer 14 on the charging and discharging process of the battery cell, and effectively ensures the charging and discharging performance of the battery cell.
[0189] Please refer to FIG6, FIG7, and FIG8. In some embodiments of the present application, the tensile strength of the insulating layer 14 in the width direction b is greater than or equal to 1000 kgf / cm 2 .
[0190] It should be noted that the length direction a of the insulating layer 14 corresponds to the extension direction of the electrode sheet, which is also the winding direction of the electrode sheet. The width direction b of the insulating layer 14 corresponds to the width direction of the electrode sheet. The tensile strength of the insulating layer 14 along the width direction b can be measured by applying a tensile force to the insulating layer 14 along the width direction b until the insulating layer 14 can no longer withstand the tensile force and breaks. The tensile strength of the insulating layer 14 along the width direction b reflects the insulating layer 14's ability to resist damage in the width direction b when subjected to a tensile force.
[0191] Because the insulating layer 14 is disposed in the bend region 17, the insulating layer 14 is subjected to a certain amount of tension during the winding and pre-pressing of the electrode assembly 10, as well as during the use of the battery cell. Based on this, by adopting the above solution, it is possible to ensure that the insulating layer 14 has sufficient tensile strength in its width direction b, effectively reducing the risk of fracture or cracking defects in the insulating layer 14 under the action of tension, thereby ensuring and improving the insulating barrier effect of the insulating layer 14 on dendrites growing from defects in the separator 13, and effectively reducing the risk of dendrites continuing to grow along fracture or cracking defects in the insulating layer 14, thereby correspondingly extending the service life of the battery cell and improving the safety of the battery cell.
[0192] It should be noted that when the insulating layer 14 has sufficient tensile strength in its width direction b, the tensile strength of the insulating layer 14 in its extension direction can basically meet the requirements. Therefore, this embodiment does not specifically limit the tensile strength of the insulating layer 14 in its extension direction.
[0193] Please refer to FIG. 6 , FIG. 7 , and FIG. 8 . In some embodiments of the present application, the elongation of the insulating layer 14 in the width direction b thereof is greater than or equal to 10%.
[0194] It should be noted that by applying a tensile force along the width direction b to the insulating layer 14 until the insulating layer 14 can no longer withstand the tensile force and is broken, the percentage of the tensile deformation portion of the insulating layer 14 in its width direction b to the original length is the elongation of the insulating layer 14 in its width direction b.
[0195] Because the electrode assembly 10 may expand and deform during battery cell use, the insulating layer 14 disposed in the bending region 17 of the electrode assembly 10 must exhibit a certain degree of elongation and deformation. Therefore, the above-described solution ensures that the insulating layer 14 has sufficient elongation in its width direction b, ensuring that the insulating layer 14 can adaptively extend and deform along with the electrode assembly 10. This ensures that the insulating layer 14's effective range covers the corresponding area of the electrode sheet and can reliably insulate against dendrites growing from defects in the separator 13.
[0196] Please refer to FIG. 6 , FIG. 7 , and FIG. 8 . In some embodiments of the present application, the shrinkage rate of the insulating layer 14 at 105° C. is 0-3%.
[0197] It should be noted that the shrinkage rate of the insulating layer 14 at 105° C. can be obtained by comparing the shrinkage of the “dimensions of the insulating layer 14 at 105° C.” with the shrinkage of the “dimensions of the insulating layer 14 at room temperature”.
[0198] During the use of a battery cell, as the internal temperature of the battery cell increases, the insulating layer 14 may shrink and deform. If the shrinkage is too large, the effective range of the insulating layer 14 may not cover the corresponding area of the entire electrode. Based on this, by adopting the above solution, the degree of dimensional shrinkage of the insulating layer 14 caused by the internal temperature of the battery cell can be minimized during the use of the battery cell, thereby ensuring that the effective range of the insulating layer 14 can cover the corresponding area of the electrode, and ensuring that the insulating layer 14 can form a reliable insulation barrier effect on dendrites growing from defects in the diaphragm 13.
[0199] Please refer to FIG. 2 . Some embodiments of the present application further provide a battery 1 . The battery 1 includes a battery cell provided in an embodiment of the present application.
[0200] By adopting the above solution, the battery 1 can ensure and extend the service life of the battery 1 and ensure and improve the safety of the battery 1 by applying the battery cells provided in the embodiments of the present application.
[0201] Please refer to FIG1 . Some embodiments of the present application further provide an electrical device, which includes a battery 1 or a battery cell provided in an embodiment of the present application.
[0202] By adopting the above solution, the electrical device can ensure and extend the service life of the electrical device and ensure and improve the safety of the electrical device by applying the battery 1 or battery cell provided in the embodiment of the present application.
[0203] The above are merely optional embodiments of the present application and are not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present application should be included within the scope of the claims of the present application.
Claims
1. A battery cell, wherein: The battery cell comprises at least one electrode assembly, wherein the electrode assembly comprises a positive electrode sheet, a negative electrode sheet, a separator, an insulating layer and a glue layer; The positive electrode sheet, the separator and the negative electrode sheet are stacked and wound, and the electrode assembly has a bending area; At least a portion of the insulating layer and at least a portion of the adhesive layer are provided in the bending region, and the insulating layer is bonded to the positive electrode sheet or the negative electrode sheet through the adhesive layer; In the thickness direction of the insulating layer, the projected area of the adhesive layer is smaller than the projected area of the insulating layer.
2. The battery cell according to claim 1, wherein: The glue layer includes a plurality of glues, and at least part of the glues are distributed in the edge area of the insulating layer.
3. The battery cell according to claim 2, wherein: The colloid is a strip-shaped colloid, and a plurality of the colloids are arranged at intervals along the width direction of the insulating layer, or a plurality of the colloids are arranged at intervals along the length direction of the insulating layer.
4. The battery cell according to claim 2, wherein: The colloid is a block-shaped colloid, and at least a portion of the colloid is distributed at each corner of the insulating layer.
5. The battery cell according to any one of claims 1 to 4, wherein: The adhesive layer is a hot melt adhesive that is resistant to electrolyte.
6. The battery cell according to any one of claims 1 to 4, wherein: In the thickness direction of the insulating layer, the ratio of the projected area of the adhesive layer to the projected area of the insulating layer is 20% to 50%.
7. The battery cell according to any one of claims 1 to 4, wherein: The thickness of the adhesive layer is 2 um to 8 um.
8. The battery cell according to any one of claims 1 to 7, wherein: In the bending region, at least one of the insulating layers is bonded to the inner side of the innermost circle of the positive electrode plate through the adhesive layer.
9. The battery cell according to any one of claims 1 to 7, wherein: In the bending region, at least one of the insulating layers is bonded to the outer side of the innermost circle of the positive electrode plate through the adhesive layer.
10. The battery cell according to any one of claims 1 to 7, wherein: The bending area is provided with two insulating layers, one of which is bonded to the inner side of the innermost circle of the positive electrode sheet through the adhesive layer, and the other insulating layer is bonded to the outer side of the innermost circle of the positive electrode sheet through the adhesive layer.
11. The battery cell according to any one of claims 1 to 10, wherein: The electrode assembly has a main body area and a bending area arranged at the end side of the main body area; the insulating layer has a bending section bent in the bending area, and an extension section connected to the end of the bending section and arranged in the main body area.
12. The battery cell according to any one of claims 1 to 11, wherein: The insulating layer is provided with a plurality of holes.
13. The battery cell according to claim 12, wherein: An absolute value of a difference between a porosity of the insulating layer and a porosity of the diaphragm is less than or equal to 25%.
14. The battery cell according to claim 13, wherein: An absolute value of a difference between a porosity of the insulating layer and a porosity of the diaphragm is less than or equal to 10%.
15. The battery cell according to claim 12, wherein: The insulating layer is a polyolefin diaphragm.
16. The battery cell according to claim 12, wherein: The porosity of the insulating layer is 40% to 50%.
17. The battery cell according to claim 12, wherein: The pore diameter of the insulating layer is A, the thickness of the insulating layer is B, and 24≤B / A≤400.
18. The battery cell according to claim 17, wherein: The pore diameter A of the pores in the insulating layer is 0.05 um to 0.5 um.
19. The battery cell according to claim 17, wherein: The thickness B of the insulating layer is 12 um to 20 um.
20. The battery cell according to any one of claims 12 to 19, wherein: In the thickness direction of the insulating layer, the adhesive layer avoids the hole.
21. The battery cell according to any one of claims 1 to 20, wherein: The tensile strength of the insulating layer in its width direction is greater than or equal to 1000 kgf / cm 2 .
22. The battery cell according to any one of claims 1 to 20, wherein: The elongation of the insulating layer in the width direction thereof is greater than or equal to 10%.
23. The battery cell according to any one of claims 1 to 20, wherein: The shrinkage rate of the insulating layer at 105° C. is 0-3%.
24. A battery, wherein: The battery comprises the battery cell according to any one of claims 1 to 23.
25. An electrical device, wherein: The electrical device comprises the battery according to claim 24, or the battery cell according to any one of claims 1 to 23.