Direct printing of solid state batteries

By directly printing the electrochemical layer in the frame, the problem of excessive use of adhesives and complex drying processes in the existing electrochemical cell manufacturing is solved, and efficient electrochemical cell manufacturing is achieved, and energy density is improved. Simplicity in manufacturing.

CN118943400APending Publication Date: 2024-11-12FORD GLOBAL TECH LLC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410519713.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-01
Filing Date
2024-04-28
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing electrochemical cell manufacturing methods have problems such as excessive use of adhesives, complex drying processes and inefficiency, especially inefficiency caused by the dangling electrode layer.

Method used

The electrochemical layer is arranged in the frame by direct printing, reducing or without the use of adhesive, and applying and compacting the powder layer through nozzles and presses to form a sealed electrochemical assembly.

Benefits of technology

The energy density of the electrochemical cell and the loading of the active material are improved, the manufacturing process is simplified, the waste is reduced, and the cohesion and adhesion of the electrochemical layer is improved, avoiding the inefficiency problems caused by the overhanging electrode layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118943400A_ABST
    Figure CN118943400A_ABST
Patent Text Reader

Abstract

The present disclosure provides direct printing of solid state batteries. An electrochemical assembly consists of a dry electrochemical powder layer (e.g., an anode layer, a separator layer, a cathode layer, and / or a current collector layer) that is substantially free of solvents and / or binders. Electrochemical assemblies are produced by disposing (e.g., printing / spraying) a dry powder layer directly into a non-conductive frame.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Methods of printing solid-state batteries, and more particularly printing bipolar solid-state battery assemblies, are provided. Background Art

[0002] Recently, a great deal of resources and effort have been invested in developing alternative energy sources. However, many alternative sources require storage of the harnessed energy. Electrochemical cells themselves can be an alternative energy source or the primary technology for storing harnessed energy. Summary of the invention

[0003] A method for manufacturing an electrochemical cell is provided. The method may include: disposing a first electrode powder layer of the electrochemical cell in a frame; disposing a second separator layer of the electrochemical cell in the frame; and disposing a third electrode powder layer of the electrochemical cell in the frame such that the separator layer is disposed between the first electrode layer and the second electrode layer.

[0004] An electrochemical assembly is provided. The electrochemical assembly includes a frame, a first end plate, a first compacted anode powder layer, a first compacted diaphragm powder layer, and a first compacted cathode powder layer, such that the first diaphragm layer is disposed between the first anode layer and the first cathode layer. In one variation, the first end plate is disposed at a first end of the frame, and the second end plate is disposed at a second end of the frame, such that the end plates sandwich the electrochemical layers. In various embodiments, the frame supports the end plates and the various electrochemical layers.

[0005] A system for preparing a battery assembly is also provided. The system includes a conveyor assembly, one or more nozzles, and a press. In one variation, the conveyor assembly is configured to receive a frame of an electrochemical assembly. In an improved embodiment, the nozzle distributes multiple electrochemical powder layers within the frame. The press compacts one or more of the electrochemical powder layers. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] Figure 1 is a schematic cross-sectional view of a system / method for manufacturing an electrochemical assembly.

[0007] Figure 2 is a flow chart of a method for manufacturing an electrochemical cell assembly.

[0008] Figure 3 is a cross-sectional schematic diagram of a method for fabricating an electrochemical assembly using multiple texturing presses.

[0009] Figure 4 is a schematic side view of a carousel assembly used to manufacture an electrochemical assembly.

[0010] Figure 5 is a schematic diagram of a dovetail lock used to assemble an electrochemical assembly.

[0011] Figure 6 is a schematic top view of the electrochemical assembly.

[0012] Figure 7 is a schematic side view in cross section of an embodiment of fabricating an electrochemical assembly. DETAILED DESCRIPTION

[0013] As required, detailed embodiments of the present invention are disclosed herein. However, it should be understood that the disclosed embodiments are merely examples of the present invention that may be embodied in various forms and alternative forms. The accompanying drawings are not necessarily drawn to scale, and therefore some features may be enlarged or minimized to illustrate the details of particular components. Therefore, the specific structural details and functional details disclosed herein are not to be construed as limiting, but only as a representative basis for teaching those skilled in the art to adopt the present invention in various ways.

[0014] In addition, unless otherwise expressly indicated, all numerical quantities in the present disclosure are understood to be modified by the word "about" when describing the broader scope of the present disclosure. Practice within the stated numerical limits is generally preferred. In addition, unless expressly stated to the contrary, percentages, "parts" and ratio values ​​are by weight. The term "polymer" includes "oligomers", "copolymers", "terpolymers" and the like. Describing a group or a class of materials as suitable or preferred for a given purpose implies that any mixture of two or more of the members in the group or class may be suitable or preferred in the same manner. The molecular weight provided for any polymer refers to the number-average molecular weight. The description of a component in chemical terms refers to the component when added to any combination specified in this specification, and once mixed, chemical interactions between the components of the mixture are not necessarily excluded. The first definition of an acronym or other abbreviation applies to all subsequent uses of the same abbreviation in this article, and can be applied to the normal grammatical variations of the abbreviation initially defined with appropriate modifications. Unless there is a clear contrary statement, the measurement result of a property is determined by the same technique as cited before or after for the same property.

[0015] The present disclosure is not limited to the specific embodiments and methods described below, as specific components and / or conditions may be different. Furthermore, the terminology used herein is for the purpose of describing specific embodiments only and is not intended to be limiting in any way.

[0016] The terms "substantially" or "substantially" may be used herein to describe the disclosed or claimed embodiments. The terms "substantially" or "substantially" may modify a value or relative property disclosed or claimed in the present disclosure. In such examples, "substantially" or "substantially" may mean that a value or relative property is within a manufacturing tolerance or is modified within ±0%, 0.1%, 0.5%, 1%, 2%, 3%, 4%, 5%, or 10% of a value or relative property.

[0017] It should also be understood that integer ranges explicitly include all intermediate integers. For example, integer ranges 1 to 10 explicitly include 1, 2, 3, 4, 5, 6, 7, 8, 9 and 10. Similarly, ranges 1 to 100 include 1, 2, 3, 4 ... 97, 98, 99, 100. Similarly, when any range is required, intermediate values ​​that are the difference between the upper and lower limits divided by an increment of 10 may be considered as an alternative upper or lower limit. For example, if the range is 1.1 to 2.1, the following values ​​1.2, 1.3, 1.4, 1.5, 1.6, 1.7, 1.8, 1.9 and 2.0 may be selected as lower or upper limits.

[0018] refer to Figure 1 to Figure 2 , a method 10 for manufacturing an electrochemical assembly using a system 100 is provided. The method 10 includes providing a frame 202 (i.e., step 20), disposing a first electrochemical layer 204 in the frame 202 (i.e., step 40), disposing a second electrochemical layer 206 in the frame 202 (i.e., step 50), and disposing a third electrochemical layer 208 in the frame 202 (i.e., step 60). In an improved solution, a fourth electrochemical layer 210 may be disposed in the frame 202 adjacent to the first electrochemical layer 204 and / or the third electrochemical layer 208 (i.e., step 70).

[0019] In various embodiments, the first layer 204, the second layer 206, the third layer 208, and the fourth layer 210 are all different from each other. One or more of the electrochemical layers 204, 206, 208, and 210 are dry (e.g., powder) layers and / or are free of / substantially free of solvents. For example, solid layers and / or powder layers are used. Conventional systems are not directly arranged in electrochemical frames, and therefore require inactive binder materials and / or unused active areas to accommodate deviations and provide tolerances. Inactive encapsulation and sealing materials further limit the efficiency of conventional electrochemical assemblies. Therefore, direct printing increases the loading and energy density of active materials. The electrochemical assemblies described herein may be free of or substantially free of binders because they are directly arranged in the frame, so that cohesion and / or adhesion may be less than conventional assemblies in which the layers are prepared before or separately and assembled together but can still move relative to each other. Similarly, the layers are directly arranged in the frame to prevent or alleviate deviations, thereby eliminating inefficiencies such as those caused by overhanging electrode layers and improving quality (i.e., direct printing is self-aligned). In a refinement, each layer may have less than 5% by weight binder, or more preferably less than 2.5%, or even more preferably less than 1%.

[0020] Printing the electrochemical layers directly into the electrochemical framework is a much simpler process than conventional manufacturing methods that involve creating liquid solutions and / or slurries and complex drying methods that can be energy intensive and require expensive solvent recovery equipment. There is also less waste because the assembly is built into the desired shape and size defined by the framework.

[0021] In one or more embodiments, the second electrochemical layer 206 is disposed on the first electrochemical layer 204, and the third electrochemical layer 208 is disposed on the second electrochemical layer 206, so that the second electrochemical layer 206 is sandwiched between the first electrochemical layer 204 and the third electrochemical layer 208. The layers can be applied uniformly, for example, with a thickness of up to 150 microns, or more preferably up to 120 microns, or even more preferably up to 50 microns. The cathode layer and / or the anode layer can be applied at a thickness of 10 microns to 150 microns, or more preferably 25 microns to 130 microns, or even more preferably 50 microns to 100 microns. In other embodiments, a thickness of up to 50 microns may be suitable. For example, the separator layer can be 1 micron to 50 microns, or more preferably 5 microns to 45 microns, or even more preferably 10 microns to 30 microns. However, it should be understood that the thickness of each layer and / or stack depends on many variables including chemical properties and / or intended use.

[0022] In one variation, steps 40 to 70 may be repeated one or more times (ie, step 80), for example, multiple times, to form an electrochemical array / stack, such as Figure 6 to Figure 7As shown. For example, deposition of a first anode layer, a first electrolyte / separator layer, a first cathode layer, a first bipolar plate / collector, a second anode layer, a second electrolyte / separator layer, a second cathode layer, and a second bipolar plate / collector layer in frame 202 may be performed. Additional cell assemblies may be included, such as or up to 3, 4, 5, 6, 7, 8, 9, 10, 15, 20, 25, 30, 35, 45, 50, 55, 60, 70, 80, 90, or 100 cells. In one variation, the assembly may include or the process may be repeated at least 5 times, or more preferably at least 10 times, or even more preferably at least 40 times.

[0023] In a refinement, the first end plate 212 and the second end plate 214 can be disposed in the frame 202 (i.e., steps 30 and 90, respectively) such that they form the outermost regions of the electrochemical assembly 100 (i.e., the first end plate 212 and the second end plate 214 sandwich the electrochemical layers from the first end and the second end of the electrochemical assembly 200). In one variation, the first end plate 212 can be disposed in the frame 202 before the electrochemical layers, such that the first electrochemical layer 204 (and / or other layers) can be disposed on the first end plate 212. In one or more embodiments, the first end plate 212 and the second end plate 214 can form a first terminal 216 and a second terminal 218 (i.e., a negative end plate terminal and a positive end plate terminal) to provide power to an external circuit. For example, the first end plate 212 can form a negative terminal, while the second end plate 214 forms a positive terminal. In various embodiments, once the various layers are disposed in the electrochemical assembly 200, the electrochemical assembly is hermetically sealed. In an improved scheme, the electrochemical assembly 200 is sealed so that the external surrounding environment is separated from the internal electrochemical environment to prevent the active material from being exposed to gases such as oxygen or moisture. For example, the frame may include a housing, a support housing and / or cooperate with the housing to facilitate the sealing of the electrochemically active material from the external environment. In an improved scheme, the method / arrangement has a self-sealing effect because the layer is applied and compacted directly into the frame / housing, which can be achieved in a controlled environment. The outer edges of the various layers are compacted against the walls of the frame / housing so that they form a seal, thereby preventing or alleviating exposure to the inner layer once the outer layer is applied to the inner layer (i.e., because the layers are directly arranged in the frame / housing, there is no gap between the frame / housing wall and the layer arranged therein). Sealing via the frame / housing may be easier than conventional sealing mechanisms such as using soft-pack batteries. In yet other embodiments, the electrochemical assembly may be quasi-sealed so that it includes a vent to release gases generated from the electrochemically active components during the life of the assembly. For example, a sealant may be used to seal the assembly in a frame / housing.

[0024] In one or more embodiments, the solid and / or powder layer can be applied without solvent (e.g., substantially without solvent or completely without solvent) by any suitable powder layer application method known in the art, such as powder spraying, powder leveling, powder bed (3D) printing, and / or electrostatic deposition. For example, the anode powder layer 104 (such as the anode electrode powder 105) can be sprayed into the frame 202 by the spray nozzle 118 and disposed on the first end plate 212, such as Figure 1 As shown. In one variation, one or more newly formed solid and / or powder layers may be compacted, such as by one or more presses 120, to form, for example, a denser layer having better adhesion and / or cohesive properties. For example, the first electrochemical layer 204 / electrode anode powder layer 104 may be applied by spraying anode powder 205 in the frame 202. The frame 202 and the partial assembly may then be moved under the press 120 for compaction. In an improved embodiment, the compacted layer may have a relative density of 50% to 100%, or more preferably 80% to 100%, or even more preferably 95% to 100%, for example, as determined by ISO 1183-1:2004 or ASTM D854.

[0025] In an improved solution, each layer can be compacted within the frame 202 after it is applied to the adjacent layer. For example, compaction can occur after one or more steps (e.g., each step, multiple steps, after all layers are applied, or after all steps). Similarly, the electrolyte / separator powder layer 106 can be applied by a spray nozzle 126 spraying the electrolyte / separator powder 107, and the cathode powder layer 108 can be applied by a spray nozzle 128 spraying the cathode powder 209. In an improved solution, the bipolar substrate / collector layer 110 can be applied by a spray nozzle 130 spraying the conductive powder 111, or alternatively, a conductive foil can be inserted.

[0026] It should be understood that any combination of the following: a single nozzle may be used to spray multiple different layers; a single press may be used to compact each layer or assembly; multiple nozzles may spray different layers; and / or multiple presses may be used. The assembly may then be sealed, or the process may be repeated multiple times to form an unsealed electrochemical array / stack 230, which is then sealed with a second end plate 214 to form a sealed electrochemical array / stack 240. It should also be understood that the application of a single layer or multiple layers may be applied through one or more channels / powder application layers, nozzle arrangements (e.g., one nozzle, multiple nozzles, circular nozzles, slit nozzles, nozzle angles, application angles, etc.), and / or flow rates to emphasize and / or mitigate certain electrochemical / mechanical properties depending on the specific chemistry and arrangement to configure it for its intended use.

[0027] In one or more embodiments, the Figure 4 The conveyor and / or carousel / circular box 300 shown. For example, a single nozzle or press can serve the carousel 300. Alternatively, multiple nozzles and / or presses can serve the carousel 300. In a variation, each station 301 to 308 of the carousel 300 can apply different layers and / or presses. In yet another example, each station 301 to 308 of the carousel 300 can accommodate its own frame, which is filled simultaneously by one or more nozzles and one or more presses. The carousel 300 also includes a feed port 310 and a discharge port 312. For example, a nozzle and / or press can be arranged above each station 301 to 308 of the carousel so that when it rotates, the layer is arranged in the frame and / or compacted, that is, the anode station, the diaphragm station, the cathode station and / or the collector station. More or fewer stations can be included. For example, 3 to 10 stations can be included. In one variation, the carousel 300 may be rotated multiple times to prepare an array or stack 200. In a refinement, frames each having a first end plate may be received in the carousel 300 via an infeed 310, and an unsealed array / stack may exit the carousel 300 via an outfeed 312 to be sealed with a second end plate. In some embodiments, the frame 202 may be cylindrical.

[0028] In various embodiments, one or more presses 120 may be textured to impart / imprint unique properties / features to one or more layers of the electrochemical assembly 200, such as Figure 3 As shown. For example, one or more texturing presses 122 can provide one or more textured layers 123 having properties such as increased contact area between the electrode and the separator and a shorter, less tortuous ion transport path to the electrode active material. In one variation, the press 120 can be heated and / or cooled to facilitate densification of the electrochemical layer. In an improved scheme, emptying can be performed before or after compaction to increase density or clear porosity paths of one or more layers.

[0029] In one or more embodiments, the frame 202 structure may include features that allow the individual cells to form a rigid structure. In other words, applying the electrochemical components directly to the frame 202 inherently provides a rigid structure for protection and assembly, which would typically be added via additional steps to form an array or module. In various examples, the frame 202 may feature one or more dovetails, such as Figure 5 As shown, it can be used to hold the electrochemical assembly 200 together and in place within a group of cells. For example, the end plates 212, 214 can be held or locked in place with dovetails.

[0030] Compaction (such as high pressure compaction) can form a unitary body within the frame 202 that expands and / or contracts with little friction with the frame 202. In one or more embodiments, the end plates 212, 214 include an adjustment member 220 that allows expansion and contraction of the electrochemical layer without compromising the airtight seal 222. In a refinement, one or more of the end plates 212, 214 can have an elastically deformable portion, such as an elastic material or a spring, disposed between one or more of the end plates 212 / 214, the frame 202, and / or the electrochemical layer. For example, a spring can be disposed between one or more of the end plates 212, 214 and the electrochemical layer, such as Figure 7 As shown. In an improved solution, a rigid plate (not shown) can be disposed between the outer electrochemical powder layer and the spring so that the powder layer is not deformed or damaged during expansion and contraction, and the pressure is evenly dispersed along the layer. In another example, an elastic member can be disposed along the edge of the end plate 212 / 214, thereby connecting the end plate 212 / 214 to the frame 202. The elastic portion provides flexibility so that it allows the electrochemical component to move within the frame 202 without endangering the airtight seal 222. The adjustment member 220 should also not interfere with the electrical transmission between the stack and the terminal. In an improved solution, the adjustment member 220 can be conductive (e.g., a resistivity of no more than 1Ω·m, or more preferably no more than 10Ω·m to 2 1Ω·m, or even more preferably 10Ω·m to 7 1Ω·m) so that it does not affect the current received by the terminal. In an improved solution, the frame 202 can be coated with a non-conductive coating that reduces friction to promote expansion and / or contraction without damaging the electrochemical cell. In one variation, one or more actuators, such as springs, may also be disposed between one or more of the end plates 212 / 214 and the electrochemical layer to accommodate expansion and contraction.

[0031] In one variation, the first electrochemical layer 104 may be a first electrode layer, the second electrochemical layer 106 may be an electrolyte / separator layer, the third electrochemical layer 108 may be a second electrode layer, and the fourth electrochemical layer 110 may be a bipolar substrate / current collector layer. In a refinement, the first electrode layer is an anode layer or a cathode layer, and the third electrode layer may be the other of the anode layer or the cathode layer. In various embodiments, the electrode layers may be formed from electrode powders. For example, graphite, lithium titanate (LTO, e.g., Li4Ti5O 12), tin-cobalt alloys and / or silicon-carbon composites can be used for the anode. In an improved scheme, powders or powder mixtures of lithium iron phosphate (LFP, such as LiFePO4) and / or metal oxides (such as lithium cobalt oxide (LCO, such as LiCoO2), lithium manganese oxide (LMO, such as LiMn2O4 spinel or Li2MnO3), lithium nickel manganese cobalt oxide (NMC, such as LiNiMnCoO2), lithium nickel cobalt aluminum oxide (NCA, such as LiNiCoAlO2)) and / or other lithium-rich and manganese (LMR) cathode materials can be used for the cathode.

[0032] In one or more embodiments, the electrolyte / separator layer may be a solid electrolyte (SSE), such as an inorganic solid electrolyte (ISE), a solid polymer electrolyte (SPE), and / or a composite polymer electrolyte (CPE). In one variation, a polymer or oxide (e.g., powder, such as poly(ethylene oxide) (PEO), poly(propylene oxide) (PPO), lithium bis(fluorosulfonyl)imide (LiSI), polytrimethyl carbonate (PTMC), poly(acrylonitrile) (PAN), poly(methyl methacrylate) (PMMA), poly[bis(methoxy-ethoxy-ethoxy)phosphazene] (MEEP), and / or poly(vinylidene fluoride) (PVdF)) powder may be used.

[0033] In one or more embodiments, the bipolar substrate / collector layer can be formed of a conductive powder or foil. The bipolar plate / collector promotes electron transport, but prevents lithium ion diffusion. In an improved scheme, the bipolar substrate / collector is electrochemically stable at both the anode and cathode potentials. For example, a metal material such as stainless steel, copper and / or aluminum, or a semi-metallic material may be included. Alloys such as bimetallic alloys, such as Al-Cu, may also be used. In various embodiments, the substrate / collector foil may be coated with Li metal, such as on one side, and may be inserted in a single step.

[0034] In various embodiments, the frame 202 includes electronically insulating / non-conductive areas, such as to prevent or mitigate electrical shorts, or is electronically insulating / non-conductive, and can incorporate additional useful features directly into the electrochemical assembly 200. In a refinement, the frame 202 includes an insulating material / surface that contacts the electrochemically active components. For example, the contact surface can be coated to provide electrical insulation properties. In a refinement, the insulating material should prevent dielectric breakdown or be equivalent to the electrochemical properties of the assembly in dielectric form (e.g., configured to accommodate the size / voltage of the electrochemical assembly to prevent dielectric breakdown). For example, the frame 202 can be made of plastic or ceramic or coated with plastic or ceramic.

[0035] In various embodiments, the frame 202 includes a built-in cooling system, such as by providing a hollow channel for receiving and circulating a fluid (i.e., a cooling circuit / jacket), a fixture for securing the electrochemical assembly 200 to a suitable location (such as for securing the assembly 200 to a vehicle), including a bus connection, and / or including a built-in monitoring assembly and / or its housing. The methods and assemblies described herein may be particularly suitable for bipolar assemblies, however, parallel connections may be added to provide other electrochemical assemblies. For example, switching contacts, parallel connections, and / or bus connections may be formed at the edge of the frame 202.

[0036] Although exemplary embodiments are described above, these embodiments are not intended to describe all possible forms of the present invention. Rather, the words used in the specification are descriptive rather than restrictive terms, and it should be understood that various changes may be made without departing from the spirit and scope of the present invention. In addition, the features of the various embodiments of implementation may be combined to form other embodiments of the present invention.

[0037] According to the present invention, a method for manufacturing an electrochemical cell includes: (a) disposing a first electrode powder layer of the electrochemical cell in a frame; (b) disposing a diaphragm layer of the electrochemical cell in the frame; and (c) disposing a second electrode powder layer of the electrochemical cell in the frame, so that the diaphragm layer is disposed between the first layer and the second layer.

[0038] In one aspect of the invention, the process is substantially free of solvent.

[0039] In one aspect of the invention, a foil current collector layer is disposed in the frame adjacent to the first electrode powder layer and / or the second electrode powder layer.

[0040] In one aspect of the invention, a current collector powder mix is ​​disposed in said frame.

[0041] In one aspect of the invention, the method comprises compacting the layers.

[0042] In one aspect of the invention, compaction is performed after each layer is arranged within the frame.

[0043] In one aspect of the invention, compacting is performed using a texturizing press.

[0044] In one aspect of the invention, steps (a) to (c) are repeated to form an electrochemical stack comprising a plurality of electrochemical cells.

[0045] In one aspect of the invention, steps (a) to (c) are repeated by rotating the frame on a carousel.

[0046] In one aspect of the invention, the method comprises disposing a first end plate at a first end of the frame and disposing a second end plate at a second end of the frame such that the first end plate and the second end plate sandwich the layer.

[0047] In one aspect of the present invention, the first electrode layer is an anode powder mixture or a cathode powder mixture and is disposed on the first end plate, the diaphragm layer is a diaphragm powder and is disposed on the first layer, and the second electrode layer is the other of the anode powder mixture or the cathode powder mixture and is disposed on the diaphragm layer.

[0048] In one aspect of the invention, the powder mixture is powder sprayed.

[0049] According to the present invention, an electrochemical assembly is provided, which has: a frame, which supports a first end plate at a first end and a second end plate at a second end, so that the end plate sandwiches a first compacted anode powder layer, a first compacted diaphragm powder layer and a first compacted cathode powder layer, and the compacted first diaphragm powder layer is arranged between the first anode powder layer and the first cathode powder layer.

[0050] According to one embodiment, a second compacted anode layer, a second compacted separator and a second compacted cathode layer are arranged in the frame.

[0051] According to one embodiment, the layer is substantially free of binder.

[0052] According to one embodiment, the invention also features an alignment member disposed along the first end plate and / or the second end plate to accommodate expansion and contraction of the layers within the frame while maintaining an airtight seal.

[0053] According to one embodiment, the assembly is solvent-free.

[0054] According to the present invention, a system for preparing a battery assembly is provided, which comprises: a conveyor assembly, which is used to receive a frame of an electrochemical assembly; one or more nozzles, which are used to distribute multiple electrochemical powder layers in the frame; and a press, which is used to compact the one or more electrochemical powder layers in the electrochemical powder layer.

[0055] According to one embodiment, the conveyor assembly is a carousel assembly.

[0056] According to one embodiment, the one or more nozzles include a first nozzle for dispensing an anode powder mixture, a second nozzle for dispensing a separator layer, and a third nozzle for dispensing a cathode powder mixture.

Claims

1. A method for manufacturing an electrochemical cell, comprising: (a) placing a first electrode powder layer of an electrochemical cell in a frame; (b) placing a separator layer of the electrochemical cell in the frame; as well as (c) disposing a second electrode powder layer of the electrochemical cell in the frame such that the separator layer is disposed between the first layer and the second layer.

2. The method of claim 1, wherein the method is substantially free of solvent. 3 . The method of claim 1 , wherein a foil current collector layer is disposed in the frame adjacent to the first electrode powder layer and / or the second electrode powder layer. The method of claim 1 , wherein a current collector powder mixture is disposed in the frame.

5. The method of claim 1 further comprising compacting the layer.

6. The method of claim 5, wherein compaction is performed after each layer is arranged in the frame.

7. The method of claim 5, wherein the compacting is performed using a texturizing press.

8. The method of claim 1, wherein steps (a) to (c) are repeated to form an electrochemical stack comprising a plurality of electrochemical cells.

9. The method of claim 8, wherein steps (a) to (c) are repeated by rotating the frame on a carousel.

10. The method of claim 1, further comprising disposing a first end plate at a first end of the frame and a second end plate at a second end of the frame such that the first end plate and the second end plate sandwich the layer.

11. The method of claim 1 , wherein the first electrode layer is an anode powder mixture or a cathode powder mixture and is disposed on the first end plate, the diaphragm layer is a diaphragm powder and is disposed on the first layer, and the second electrode layer is the other of the anode powder mixture or the cathode powder mixture and is disposed on the diaphragm layer.

12. The method of claim 1, wherein the powder mixture is powder sprayed.

13. An electrochemical assembly comprising: A frame supporting a first end plate at a first end and a second end plate at a second end, such that the end plates sandwich a first compacted anode powder layer, a first compacted diaphragm powder layer, and a first compacted cathode powder layer, the compacted first diaphragm powder layer being disposed between the first anode powder layer and the first cathode powder layer.

14. The electrochemical assembly of claim 13, wherein a second compacted anode layer, a second compacted separator, and a second compacted cathode layer are disposed in the frame.

15. The electrochemical assembly of claim 13, wherein the layer is substantially free of binder.