Preparation method of optical fiber immunosensor based on chemiluminescence and application of optical fiber immunosensor in detection of silk fibroin
Through a chemiluminescence-based fiber immune sensor, the catalytic reaction of Au/Pt@CuO/Cu2O-labeled secondary antibody combined with the luminol luminescent group combined with hydrogen peroxide was achieved, and ultra-sensitive quantitative detection of silk fibroin in ancient silk artifacts was achieved. It solves the problem of archaeological on-site inspection, provides fast and convenient detection methods and realizes real-time information transmission.
Patent Information
- Application Number
- CN202411285166.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-11-15
AI Technical Summary
Traditional detection methods are difficult to effectively detect silk fibroin in ancient silk relics at archaeological sites, and there are problems of low sensitivity and insufficient specificity.
Using a chemiluminescence-based fiber immunosensor, the luminol luminescent group coupled to the surface of the fiber through Au/Pt@CuO/Cu2O labeled secondary antibody, combined with hydrogen peroxide catalytic reaction, realizes ultra-sensitive quantitative detection of silk fibroin , and connect it to the mobile phone through Bluetooth to achieve real-time information transmission.
It realizes fast, convenient and ultra-sensitive quantitative detection at the archaeological site, avoids the dependence of large-scale detection instruments, improves detection efficiency and accuracy, and can transmit detection data in real time.
Smart Images

Figure CN118961684A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of immunosensors, and more specifically relates to a preparation method of a chemiluminescence-based optical fiber immunosensor and an application thereof in detecting silk fibroin. Background Art
[0002] Silk has a long history in China and represents the splendid civilization of ancient China. In ancient times, silk was often used as burial objects to highlight the identity and status of the tomb owner. Therefore, the excavation of silk cultural relics at the archaeological site is of great significance to the exploration of ancient Chinese silk culture and ancient civilization. However, since tombs are often buried deep in the soil and are very old, silk cultural relics will be eroded by water, inorganic salts, acids, alkalis, microorganisms and other substances, degraded into small molecules, amino acids, peptide chains, and many unearthed silk cultural relics are fragmented or even dissolved in the soil, making them difficult to distinguish with the naked eye. Moreover, the unearthed cultural relic samples contain a large amount of impurities, which will have a great impact on the test results. Traditional detection methods such as (direct observation method, mass spectrometry) are difficult to obtain effective information. Therefore, the archaeological site urgently needs a highly sensitive, highly specific and on-site detection method for silk cultural relic detection.
[0003] Fibroin is a protein unique to silk. It can be detected to distinguish it from other impurities in cultural relics. There are many types of immunosensors that can be used to detect proteins. The principle is to amplify the immune binding signal based on the specific binding of antigens and antibodies, thereby achieving sensitive detection of silk fibroin. Although these sensors have very high sensitivity, they require the use of large instruments and equipment, and need to be tested and analyzed in the laboratory for several days, so they cannot be used at archaeological sites. This hinders the development of archaeological work. Summary of the invention
[0004] The present invention aims to provide a preparation method of a chemiluminescent optical fiber immunosensor and its application in detecting silk fibroin. Based on the extraction of silk fibroin from silk, Au / Pt@CuO / Cu2O is first prepared, and the product is coupled with a secondary antibody for labeling antibodies. A silane coupling agent is then used to fix a primary antibody and a luminescent group luminol on the surface of an optical fiber. The primary antibody is combined with the silk fibroin in the sample to be tested to produce an immune conjugate, which is then reacted with a secondary antibody labeled with Au / Pt@CuO / Cu2O. The silk fibroin is used as an antigen to capture the secondary antibody to form a double antibody sandwich immune complex. The optical fiber chemiluminescent immunosensor is then immersed in a triggering solution of hydrogen peroxide. At this time, Au / Pt@CuO / Cu2O catalyzes hydrogen peroxide to decompose single oxygen oxidized luminol, thereby emitting fluorescence. The light signal enters the photon counter through the total reflection of the optical fiber, so that the detection device generates a reading, and realizes ultra-sensitive quantitative detection of silk cultural relic samples. Since no large-scale detection instruments are required, this method can be applied to detection at archaeological sites, and can be connected to smart devices such as mobile phones via Bluetooth to achieve real-time information transmission.
[0005] In order to achieve the above object, the present invention is implemented by the following technical scheme: a method for preparing a chemiluminescence-based optical fiber immunosensor, the optical fiber immunosensor comprising a secondary antibody labeled with Au / Pt@CuO / Cu2O and an optical fiber probe, and the preparation method comprises the following steps:
[0006] Step 1: Preparation of Au / Pt@CuO / Cu2O labeled secondary antibody;
[0007] (1) Adding an Au NPs dispersion to a solution containing HAuCl4·4H2O and HCl, then adding an AgNO3 solution and an ascorbic acid solution, and then dispersing in water to obtain an Au NPs solution; mixing the Au NPs solution, NaI solution, hexadecyltrimethylammonium bromide solution, AgNO3 solution and ascorbic acid solution, and stirring at 70°C for 0.5-2h; then adding a K2PtCl6 solution, stirring at 70°C for 4h, and then centrifuging to obtain Au / PtNPs;
[0008] (2) PVP powder was added to Cu(NO3)2 solution, and then Au / Pt NPs solution and N2H4·H2O solution were added, and the mixture was stirred for 40-60 min, centrifuged, and washed to obtain Au / Pt@CuO / Cu2O powder;
[0009] (3) Au / Pt@CuO / Cu2O powder was dispersed in an ethanol aqueous solution, the pH was adjusted to 5-5.5, 3-aminopropyltriethoxysilane solution was added, and after ultrasonic dispersion, the solution was heated in a water bath and heated and stirred at 75°C for 1 hour; after the reaction was completed, the reactants were filtered and washed, and the obtained reactants were dispersed in an ethanol aqueous solution, the mixed solution was mixed with PBS buffer, and glutaraldehyde solution was added, and incubated at 25°C for 2 hours; then dispersed in a solution containing EDC and NHS, incubated at room temperature for 1 hour, and then Ab2 solution was added and incubated for 24 hours, and then the Au / Pt@CuO / Cu2O labeled secondary antibody was separated by centrifugation;
[0010] The electrons between Au / Pt and CuO / Cu2O have a lower binding energy (Bes), so they are more active in catalyzing H2O2. The absorption energy of Au / Pt@CuO / Cu2O for H2O2 is negative, so H2O2 is more easily absorbed on Au / Pt@Cu2O. Specifically, copper-based catalysts can form free radicals in the luminescent reaction due to their high reaction rate and low redox potential. Their catalytic activity and stability can be effectively improved by constructing heterostructures. By constructing a heterostructure of CuO / Cu2O, the catalytic activity and stability of Cu2O can be effectively improved. The partial conversion of Cu2O can inhibit the corrosion of Cu2O in strong alkali. In the corrosion in strong alkaline solution, CuO has a high adsorption force due to its high isoelectric point. In addition, the core-shell structure formed by the precious metals (Au, Ag and Pt) provides a uniform reaction environment to promote the catalytic reaction in the core@shell structure. Au in the core-shell structure enhances the absorption capacity of H2O2 on Pt-O-Cu. The presence of Pt on the Au / Pt surface can induce the transfer of excess electrons on the gold atom to the adjacent platinum atom. In the Au / Pt nanoparticles, the electron transfer of gold (En = 2.54) to platinum (En = 2.8) can enhance the active sites on the catalyst. Moreover, the OO bond in H2O2 is easily broken by Pt-O-Cu. Therefore, it shows higher catalytic activity to catalyze H2O2 to generate OH - and O 2- Free radicals.
[0011] Step 2: Preparation of optical fiber probe;
[0012] (a) The sheath layer of the optical fiber probe is removed with a knife at a position 0.5 cm from the end to form the sensing area. The sensing area is immersed in hydrofluoric acid to remove the cladding of the optical fiber, and then washed and dried.
[0013] (b) immersing the sensing area of the optical fiber probe in a mixed solution of γ-glycidyloxypropyltrimethoxysilane and ethanol for 1-3 hours, taking it out and immersing it in a primary antibody solution, and incubating it at room temperature for 1 hour;
[0014] (c) After taking out, immerse in luminol solution and incubate for 2 h, then immerse in BSA solution to block nonspecific binding sites, wash and refrigerate for later use.
[0015] Further preferably, in step (1), the added volume ratio of the Au NPs dispersion, the solution containing HAuCl4·4H2O and HCl, the AgNO3 solution and the ascorbic acid solution is 15:50-60:1-2:15-18:7-9; the concentration of the AuNPs solution is 2-5mM; in the solution containing HAuCl4·4H2O and HCl, the concentration of HAuCl4·4H2O is 7-8mM, and the concentration of HCl is 1-1.2M; the concentration of the AgNO3 solution is 5-6mM; and the concentration of the ascorbic acid solution is 0.05-0.2mM.
[0016] Further preferably, in step (1), the added volume ratio of the Au NPs solution, NaI solution, hexadecyltrimethylammonium bromide solution, AgNO3 solution, ascorbic acid solution and K2PtCl6 solution is 5mL: 100-200μL: 20-25mL: 20-50μL: 450-550μL: 900μL; the concentration of the Au NPs solution is 5-6mM; the concentration of the NaI solution is 10mM; the concentration of the hexadecyltrimethylammonium bromide solution is 50mM; the concentration of the AgNO3 solution is 5mM; the concentration of the ascorbic acid solution is 0.1M; and the concentration of the K2PtCl6 solution is 5mM.
[0017] Further preferably, in step (2), the ratio of the added amounts of the PVP powder, Cu(NO3)2 solution, Au / PtNPs solution and N2H4·H2O solution is 1g:5-20mL:1mL:15-20μL; the average molecular weight of the PVP is 50000-60000; the concentration of the Cu(NO3)2 solution is 0.01M; the concentration of the Au / Pt NPs solution is 50-70mM; and the mass concentration of the N2H4·H2O solution is 80%.
[0018] Further preferably, in step (3), the volume ratio of ethanol to water in the ethanol-water solution is 1:1; the ratio of the added amounts of the Au / Pt@CuO / Cu2O powder, the ethanol-water solution and the 3-aminopropyltriethoxysilane solution is 0.01-0.03 g:10 mL:0.6 mL; the ratio of the added amounts of the reactant to the ethanol-water solution is 0.02-0.05 g:10 mL; the ratio of the added amounts of the mixed solution, PBS buffer, glutaraldehyde solution, the solution containing EDC and NHS, and Ab2 solution is 0.1 mL:1-2 mL:1-2 mL:1 mL:10 μL; the pH of the PBS buffer is 7.4; the mass concentration of the glutaraldehyde solution is 1%; in the solution containing EDC and NHS, the concentration of EDC is 20 mg / mL, and the concentration of NHS is 10 mg / mL; the concentration of the Ab2 solution is 1-2 mg / mL, and the secondary antibody is a rabbit anti-silk fibroin antibody.
[0019] Further preferably, in step (b), the mixed solution of γ-glycidyloxypropyltrimethoxysilane solution and ethanol has a mixing volume ratio of 1:1, the mass concentration of γ-glycidyloxypropyltrimethoxysilane solution is 2%, and the ethanol is anhydrous ethanol; the concentration of the primary antibody solution is 0.05-0.2 mg / mL, and the primary antibody is a mouse anti-silk fibroin antibody.
[0020] Further preferably, in step (c), the concentration of the luminol solution is 10-15 mg / mL; and the mass concentration of the BSA solution is 1-2%.
[0021] The second technical solution of the present invention: an application of the optical fiber immunosensor prepared by the above preparation method in detecting silk fibroin, comprising the following steps: connecting the optical fiber probe to the data transmission module, immersing the sensing area end of the optical fiber probe in a silk fibroin solution for incubation, adding a secondary antibody solution labeled with Au / Pt@CuO / Cu2O for incubation, and finally adding a hydrogen peroxide solution as a trigger; receiving the detection data on the computer side and recording it.
[0022] Luminol is a chemical fluorescent molecule that can emit blue light after oxidation, so it is widely used in criminal investigation, chemical tracing, bioengineering and other fields. The principle is that some enzymes such as horseradish peroxidase HRP and some metal compounds such as iron in blood can catalyze the decomposition of hydrogen peroxide, turning hydrogen peroxide into water and single oxygen, among which single oxygen can oxidize luminol, so that luminol emits blue fluorescence. Using this principle, a chemical immunosensor can be designed for the detection of silk fibroin. Luminol and anti-silk fibroin antibodies are fixed on the sensor surface, the sample solution to be tested is dripped on the sensor, and then combined with a secondary antibody labeled with a catalytic luminescent substance, the sensor is placed in a hydrogen peroxide solution, and a luminescent signal will be generated on the sensor surface, and the luminescent signal is collected using a portable photon counter.
[0023] As the concentration of silk fibroin increases, the luminescence intensity of luminol will also show an increasing trend. Through the change of luminescence intensity, the qualitative and quantitative analysis of silk cultural relics can be achieved. By adding a Bluetooth or WIFI module inside the sensor, it can also be connected to smart devices such as mobile phones to achieve real-time information transmission, remote monitoring and other intelligent operations. Data can be received and recorded on the computer. The connection between geographic location and big data in the form of a mobile terminal can better solve the problem of scientifically restoring the ancient silk transmission route and is more conducive to exploring the origin of silk.
[0024] Compared with the prior art, the present invention has the following advantages:
[0025] (1) The present invention is based on the extraction of silk protein from silk cultural relics. First, Au / Pt@CuO / Cu2O is prepared, and the product is coupled with a secondary antibody for labeling antibodies. Then, a primary antibody and a luminescent group luminol are fixed on the surface of an optical fiber using a silane coupling agent. The primary antibody combines with the silk protein in the sample to be tested to produce an immune conjugate, which then reacts with the secondary antibody labeled with Au / Pt@CuO / Cu2O. The silk protein captures the secondary antibody as an antigen to form a double antibody sandwich immune complex. Then, the optical fiber chemiluminescent immunosensor is immersed in a 30% hydrogen peroxide trigger solution. At this time, Au / Pt@CuO / Cu2O catalyzes hydrogen peroxide to decompose single oxygen oxidized luminol, thereby emitting fluorescence. The light signal enters the photon counter through the total reflection of the optical fiber, so that the detection device generates a reading, thereby realizing ultra-sensitive quantitative detection of silk cultural relic samples. Since no large-scale detection instruments are required, this method can be applied to detection at archaeological sites, and can be connected to smart devices such as mobile phones via Bluetooth to achieve real-time information transmission.
[0026] (2) Among many sensors, the fiber optic chemiluminescence sensor used for temporary on-site detection has the advantages of being fast, convenient, and having a sensitive detection limit compared to other types of sensors. Since it does not require large-scale precision detection equipment and has a simple operation method, it is expected to be used for the detection of silk artifacts at archaeological sites. It also has high sensitivity. Compared with enzyme-linked immunosorbent assay, chemiluminescence immunosensor has a great advantage.
[0027] (3) Within the range visible to the naked eye, as the concentration of silk fibroin increases, the light signal emitted by the solution also shows a deepening trend. Therefore, as the content of silk fibroin in silk cultural relics increases, the luminescence signal obtained by the photon counter becomes stronger, thereby achieving ultra-sensitive quantitative detection of silk cultural relic samples. The link between geographic location and big data through mobile phones can better solve the problem of scientifically restoring the ancient silk transmission route and is more conducive to exploring the origin of silk. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1CL response curves of silk fibroin at different concentrations in Example 1;
[0029] Figure 2 is the calibration curve of silk fibroin concentration in Example 1;
[0030] Figure 3 is the ELISA response curve;
[0031] Figure 4 is the ELISA calibration curve;
[0032] Figure 5 CL response curves of silk fibroin at different concentrations in Example 2;
[0033] Figure 6 is the silk fibroin concentration calibration curve in Example 2;
[0034] Figure 7 CL response curves of silk fibroin at different concentrations in Example 3;
[0035] Figure 8 is the calibration curve of silk fibroin concentration in Example 3;
[0036] Fig. 9 CL response curves of silk fibroin at different concentrations in Comparative Example 1;
[0037] Fig.10 is the calibration curve of silk fibroin concentration in Comparative Example 1;
[0038] Fig.11 CL response curves of silk fibroin at different concentrations in Comparative Example 2;
[0039] Fig.12 is the calibration curve of silk fibroin concentration in Comparative Example 2;
[0040] Fig.13 CL response curves of silk fibroin at different concentrations in Comparative Example 3;
[0041] Fig.14 is the calibration curve of silk fibroin concentration in Comparative Example 3;
[0042] Fig.15 CL response curves of silk fibroin at different concentrations in Comparative Example 4;
[0043] Fig.16 is the calibration curve of silk fibroin concentration in Comparative Example 4;
[0044] Fig.17 CL response curves of silk fibroin at different concentrations in Comparative Example 5;
[0045] Fig.18 This is the calibration curve of silk fibroin concentration in Comparative Example 5. DETAILED DESCRIPTION
[0046] Various exemplary embodiments of the present invention will now be described in detail. This detailed description should not be considered as limiting the present invention, but should be understood as a more detailed description of certain aspects, features, and embodiments of the present invention.
[0047] Extraction of silk fibroin: Take 10g of silk sample, 21.3g of anhydrous calcium chloride, 27.6mL of deionized water, and 22.4mL of ethanol and mix them evenly in a small beaker. Boil the mixture for 60 minutes and filter it. The resulting salt solution is transferred to a cellulose membrane with a molecular cutoff of 8000 Daltons for dialysis. The water is changed every 8 hours to fully remove the salt ions in the solution. After dialysis for 3 days, pour out the remaining silk fibroin solution in the bag, freeze-dry it in a vacuum freeze dryer, and finally grind the obtained silk fibroin into powder, dissolve it with phosphate buffer (pH 7.4), and put it in a clean glass vial for use.
[0048] In addition, the solutions in the examples and comparative examples are all aqueous solutions of substances unless otherwise specified. The molar concentration calculation formula of AuNPs dispersion and Au / PtNPs (60mM) solution is: the amount of substance calculated by weighing Au NPs / Au / Pt NPs / the volume of dispersion (water).
[0049] Example 1
[0050] Step 1: Preparation of Au / Pt@CuO / Cu2O labeled secondary antibody;
[0051] (1) 300 mL of 1 mM HAuCl4 solution was added to a three-necked flask, heated and stirred for 4 min, and then 10 mL of 0.1 M sodium citrate solution was added and heated and stirred until boiling, and then a purple-red solution was obtained, and then the solution was centrifuged at a speed of 6000 r / min for separation. After removing the supernatant, the precipitate was washed with deionized water and centrifuged again, and the operation was repeated three times to completely remove the reactants. The obtained precipitate was freeze-dried to obtain Au NPs.
[0052] (2) Add 15 mL of AuNPs (5 mM) dispersion into 50 mL of a solution containing HAuCl4·4H2O (7.5 mM) and 1.5 mL of HCl (1 M), then add 15 mL of AgNO3 (5 mM) solution and 7.5 mL of ascorbic acid (0.1 M) solution, stir for 30 s, and then disperse in 10 mL of deionized water to obtain an Au NPs solution. Then, 5 mL of AuNPs (45 mM) solution, 100 μL of NaI (10 mM) solution, 20 mL of CTAB (50 mM) solution, 30 μL of AgNO3 (5 mM) solution and 480 μL of ascorbic acid (0.1 M) solution were stirred at 70 ° C for 1 h, 900 μL of K2PtCl6 (5 mM) solution was added, and stirred at 70 ° C for 4 h. The solution was added into a centrifuge tube and Au / PtNPs were obtained according to the operation in step 1. The obtained Au / PtNPs were dispersed in 1 mL of water to obtain an Au / Pt NPs solution.
[0053] (3) At 30°C, 1 g of PVP (polyvinyl pyrrolidone, average molecular weight 58,000) powder was added to 10 mL of 0.01 M Cu(NO3)2 solution. Then, 1 mL of Au / Pt NPs (60 mM) solution and 20 μL of N2H4·H2O solution (80 wt%) were added. After stirring for 45 min, the mixture was washed with water and ethanol to obtain Au / Pt@CuO / Cu2O powder.
[0054] (4) 0.01g Au / Pt@CuO / Cu2O powder was dispersed in 10mL ethanol aqueous solution (V:V=1:1), the pH was adjusted to 5, 0.6mL 3-aminopropyltriethoxysilane solution (7.5%) was added, ultrasonic dispersion was used for 20min, and stirring was carried out in a water bath at 75℃ for 1h. After filtering and washing, the obtained reactant was dispersed in 10mL ethanol aqueous solution (V:V=1:1), 0.1mL of the obtained mixture was mixed with 1mL PBS (0.01M, pH 7.4), 1mL glutaraldehyde solution (1wt%) was added, and incubated at 25℃ for 2h. Then, it was dispersed in 1mL solution containing EDC (20mg / mL) and NHS (10mg / mL), incubated at room temperature for 1h, 10μLAb2 solution (1mg / mL) was added and incubated for 24h, and then the Au / Pt@CuO / Cu2O labeled secondary antibody was separated by centrifugation. The Au / Pt@CuO / Cu2O labeled secondary antibody was dispersed in 1 mL PBS (pH 7.4, 0.01 M) and set aside. The resulting solution concentration was 1.5 mg / mL.
[0055] Step 2: Preparation of optical fiber probe;
[0056] (a) The length of the optical fiber probe is 15 cm. The sheath layer is removed with a knife at 0.5 cm from the end as the sensing area. The sensing area is immersed in a 24% hydrofluoric acid solution for 10 minutes to remove the fiber cladding. Then it is washed three times with 0.1M NaOH solution and then washed three times with distilled water. The washed optical fiber probe is dried in a nitrogen stream.
[0057] (b) The sensing area was immersed in a KH-560-ethanol (V:V=1:1, the concentration of KH-560 in the KH-560 solution was 2 wt%) solution for 3 h. The sensing area was then immersed in a 50 μg / mL primary antibody solution and incubated at room temperature for 1 h.
[0058] (c) The sensing area was immersed in a 10 mg / mL luminol solution and incubated for 2 h. Then, it was immersed in a 1% BSA solution to block nonspecific binding sites. After being thoroughly washed with a PBS buffer solution (pH 7.4), the prepared optical fiber probe was kept in a refrigerator at 4°C for later use.
[0059] (d) Assembly of the fiber optic immunosensor platform: Connect the output signal end of the fiber optic probe to the fiber optic collimator, which is then connected to the photon counter to ensure that the luminescent signal is transmitted to the photon counter for detection. Add a data transmission module and a Bluetooth module to the photon counter, and turn on the Bluetooth function of smart devices such as mobile phones to connect to the device.
[0060] Step 3: Detection of silk fibroin;
[0061] Take 10mL of silk fibroin solution with concentrations of (10pg / mL, 100pg / mL, 1ng / mL, 10ng / mL, 100ng / mL, 500ng / mL, 1μg / mL) in a light-proof glass vial. Insert the fiber optic probe (sensing area end) and incubate for 2 hours to allow the silk fibroin and immune antibody to fully combine. Add Au / Pt@CuO / Cu2O labeled secondary antibody solution (1.5mg / mL) and incubate for 2 hours, and finally add a 30% mass concentration of hydrogen peroxide solution as a trigger. The data can be received and recorded on the computer.
[0062] The results are as follows Figure 1 and 2 As shown in the figure, the prepared optical fiber chemiluminescence sensor for quantitative detection of silk fibroin in silk was -1 ~10 2 In the range of pg / mL, a good linear relationship was achieved between the silk fibroin concentration and the luminescence intensity, and the calibration equation was y=139.9x+1184.47(R 2=0.9945) (where y is the chemiluminescence intensity and x is the silk fibroin concentration (ng / mL)). The limit of detection (LOD) was defined by the 3σ / M value (where the standard deviation (SD) of blank samples similar to the treated silk fibroin samples is recorded as σ, n=10, and M is the slope of the calibration curve in the low concentration linear range) and was determined to be 28.1 pg / mL. Figure 3 and 4 As shown, compared with the gold standard ELISA experiment, the sensitivity is three orders of magnitude higher and has a wider detection range, indicating that the immunosensor has excellent detection performance and achieves rapid detection in archaeological samples.
[0063] Example 2
[0064] The only difference from Example 1 is that in step (3) of preparing the secondary antibody labeled with Au / Pt@CuO / Cu2O:
[0065] (3) At 30°C, 1 g of PVP (polyvinyl pyrrolidone, average molecular weight 58,000) powder was added to 15 mL of 0.01 M Cu(NO3)2 solution. Then, 1 mL of 60 mM Au / PtNPs solution and 15 μL of N2H4·H2O solution (80 wt%) were added. After stirring for 45 min, the mixture was washed with water and ethanol to obtain Au / Pt@CuO / Cu2O powder.
[0066] like Figure 5 and 6 The results show that the prepared optical fiber chemiluminescence sensor for quantitative detection of silk fibroin in silk is -1 ~10 2 In the range of pg / mL, a good linear relationship was achieved between the silk fibroin concentration and the luminescence intensity, and the calibration equation was y=127.441x+1204.17(R 2 =0.989)(where Y is the chemiluminescence intensity and X is the silk protein concentration (ng / mL)). The limit of detection (LOD) was defined by the 3σ / M value (where the standard deviation (SD) of the blank sample similar to the treated silk protein sample is recorded as σ, n=10, and M is the slope of the calibration curve in the low concentration linear range) and was determined to be 30.6pg / mL. Compared with the gold standard ELISA experiment, the sensitivity is three orders of magnitude higher and has a wider detection range, indicating that the immunosensor has excellent detection performance and achieves rapid detection in archaeological samples.
[0067] Example 3
[0068] The only difference from Example 1 is that in step (2) of preparing the secondary antibody labeled with Au / Pt@CuO / Cu2O:
[0069] (2) 15 mL of Au NPs (3 mM) dispersion was added to 50 mL of a solution containing HAuCl4·4H2O (8 mM) and 1.5 mL of HCl (1 M), and then 15 mL of AgNO3 (5 mM) solution and 7.5 mL of ascorbic acid (0.1 M) solution were added, stirred for 30 s, and then dispersed in 10 mL of deionized water to obtain an Au NPs solution. Then 5 mL of Au NPs (44.5 mM) solution, 100 μL of NaI (10 mM) solution, 20 mL of CTAB (50 mM) solution, 30 μL of AgNO3 (5 mM) solution, and 480 μL of ascorbic acid (0.1 M) solution were stirred at 70 °C for 1 h. Then, 900 μL of K2PtCl6 (5 mM) solution was added and stirred at 70°C for 4 h. The solution was added into a centrifuge tube and Au / PtNPs were obtained according to the operation in step 1. The obtained Au / PtNPs were dispersed in 1 mL of water.
[0070] like Figure 7 and 8 The results show that the prepared optical fiber chemiluminescence sensor for quantitative detection of silk fibroin in silk is -1 ~10 2 In the range of pg / mL, a good linear relationship was achieved between the silk fibroin concentration and the luminescence intensity, and the calibration equation was y=197.990x+1175.86(R 2 =0.996)(where Y is the chemiluminescence intensity and X is the silk protein concentration (ng / mL)). The limit of detection (LOD) was defined by the 3σ / M value (where the standard deviation (SD) of the blank sample similar to the treated silk protein sample is recorded as σ, n=10, and M is the slope of the calibration curve in the low concentration linear range) and was determined to be 19.8 pg / mL. Compared with the gold standard ELISA experiment, the sensitivity is three orders of magnitude higher and has a wider detection range, indicating that the immunosensor has excellent detection performance and achieves rapid detection in archaeological samples.
[0071] Comparative Example 1
[0072] The only difference from Example 1 is that the preparation of the secondary antibody labeled with Au / Pt@CuO / Cu2O is changed to the preparation of the secondary antibody labeled with Au@CuO / Cu2O.
[0073] (2) 15 mL of AuNPs (5 mM) was added to 50 mL of a solution containing HAuCl4·4H2O (7.5 mM) and 1.5 mL of HCl (1 M), and then 15 mL of AgNO3 (5 mM) solution and 7.5 mL of ascorbic acid (0.1 M) solution were added, stirred for 30 s, and then dispersed in 10 mL of deionized water to obtain an Au NPs solution.
[0074] (3) At 30°C, 1 g of PVP (polyvinyl pyrrolidone, average molecular weight 58,000) powder was added to 10 mL of 0.01 M Cu(NO3)2 solution. Then, 1 mL of Au NPs (60 mM) solution and 20 μL of N2H4·H2O solution (80 wt%) were added. After stirring for 45 min, the mixture was washed with water and ethanol to obtain Au@CuO / Cu2O powder.
[0075] like Fig. 9 and 10 The results show that the catalytic performance of Au@CuO / Cu2O powder without Pt NPs is far inferior to that of Au / Pt@CuO / Cu2O. The prepared fiber optic chemiluminescence sensor for quantitative detection of silk fibroin in silk was -1 ~10 2 In the pg / mL range, the calibration equation is y = 18.36x + 374.15 (R 2 =0.783)(where Y is the chemiluminescence intensity and X is the silk protein concentration (ng / mL)). The limit of detection (LOD) was defined by the 3σ / M value (where the standard deviation (SD) of the blank sample similar to the treated silk protein sample is recorded as σ, n=10, and M is the slope of the calibration curve in the low concentration linear range) and was determined to be 2.12 ng / mL. Due to the lack of composite Pt NPs, Pt-O-Cu cannot be formed to break the OO bond in H2O2, resulting in a decrease in its catalytic performance.
[0076] Comparative Example 2
[0077] The only difference from Example 1 is that the preparation of the secondary antibody labeled with Au / Pt@CuO / Cu2O is changed to the preparation of the secondary antibody labeled with Au / Pt@CuO.
[0078] (3) At 30°C, 1 g of PVP (polyvinyl pyrrolidone, average molecular weight 58,000) powder was added to 10 mL of 0.01 M Cu(NO3)2 solution. Then, 1 mL of Au / Pt NPs (60 mM) solution and 20 μL of N2H4·H2O solution (80 wt%) were added. After stirring for 45 min, oxygen was introduced for 1 h to completely oxidize Cu2O to CuO. The Au / Pt@CuO powder was washed with water and ethanol to obtain Au / Pt@CuO powder.
[0079] like Fig.11 and 12 As shown in the figure, the results show that the ability of Au / Pt@CuO labeled secondary antibody to catalyze the decomposition of hydrogen peroxide is reduced due to the lack of Cu2O, resulting in a decrease in the sensitivity of the sensor. The prepared optical fiber chemiluminescence sensor for quantitative detection of silk fibroin in silk was -1 ~10 2In the pg / mL range, the calibration equation is y = 36.98x + 281.87 (R 2 =0.86)(where Y is the chemiluminescence intensity and X is the silk protein concentration (ng / mL)). The detection limit (LOD) was defined by the 3σ / M value (where the standard deviation (SD) of the blank sample similar to the treated silk protein sample is recorded as σ, n=10, and M is the slope of the calibration curve in the low concentration linear range) and was determined to be 1.05 ng / mL. Due to the lack of the heterogeneous structure formed by Cu2O and CuO, the catalytic activity and stability are reduced. This leads to a decrease in the sensitivity of the sensor.
[0080] Comparative Example 3
[0081] The only difference from Example 1 is that in the preparation of the secondary antibody labeled with Au / Pt@CuO / Cu2O, the preparation ratio of CuO / Cu2O is different (too much N2H4·H2O solution is added).
[0082] (3) At 30°C, 1 g of PVP (polyvinyl pyrrolidone, average molecular weight 58,000) powder was added to 10 mL of 0.01 M Cu(NO3)2 solution. Then, 1 mL of Au / Pt NPs (60 mM) solution and 100 μL of N2H4·H2O solution (80 wt%) were added. After stirring for 45 min, the mixture was washed with water and ethanol to obtain Au / Pt@CuO / Cu2O powder.
[0083] like Fig.13 and 14 As shown in the figure, the results show that the addition of excessive N2H4·H2O leads to an imbalance in the ratio of CuO / Cu2O, and the ability of the Au / Pt@CuO / Cu2O labeled secondary antibody to catalyze the decomposition of hydrogen peroxide is reduced, resulting in a decrease in the sensitivity of the sensor. The prepared optical fiber chemiluminescence sensor for quantitative detection of silk fibroin in silk is -1 ~10 2 In the pg / mL range, the calibration equation is y = 116.18x + 1045.58 (R 2 =0.967)(where Y is the chemiluminescence intensity and X is the silk protein concentration (ng / mL)). The detection limit (LOD) was defined by the 3σ / M value (where the standard deviation (SD) of the blank sample similar to the treated silk protein sample is recorded as σ, n=10, and M is the slope of the calibration curve in the low concentration linear range) and was determined to be 43pg / mL. Too little CuO destroyed the heterogeneous structure formed by Cu2O and CuO, and the catalytic activity and stability decreased. This resulted in a decrease in the sensitivity of the sensor.
[0084] Comparative Example 4
[0085] The only difference from Example 1 is that the incubation time of steps (b) and (c) in the preparation process of the optical fiber probe is too short and too low.
[0086] (b) The sensing area was immersed in a KH-560-ethanol (V:V=1:1, the concentration of KH-560 in the KH-560 solution was 2 wt%) solution for 1 h. Then the sensing area was immersed in a 50 μg / mL primary antibody solution and incubated at room temperature for 0.5 h.
[0087] (c) The sensing area was immersed in a 10 mg / mL luminol solution and incubated for 1 hour. Then, it was immersed in a 1% BSA solution to block nonspecific binding sites. After being thoroughly washed with PBS buffer (pH 7.4), the prepared optical fiber probe was kept in a refrigerator at 4°C for later use.
[0088] like Fig.15 and 16 As shown in the figure, the results show that the short incubation time in processes (b) and (c) leads to a reduction in the primary antibody and luminol loading on the sensor, a reduction in the antibody fixing the antigen and a reduction in the luminescent substance, which leads to a decrease in the luminescence intensity and a decrease in the sensitivity of the sensor. -1 ~10 2 In the pg / mL range, the calibration equation is y = 73.12x + 429.24 (R 2 =0.927)(where Y is the chemiluminescence intensity and X is the silk fibroin concentration (ng / mL)). The limit of detection (LOD) was defined by the 3σ / M value (where the standard deviation (SD) of blank samples similar to the treated silk fibroin samples was recorded as σ, n=10, and M was the slope of the calibration curve in the low concentration linear range) and was determined to be 64 pg / mL.
[0089] Comparative Example 5
[0090] The only difference from Example 1 is that the concentration of hydrogen peroxide solution used in the detection process of the silk fibroin solution is too low.
[0091] Step 3: Detection of silk fibroin;
[0092] Take 10mL of silk fibroin solution with concentrations of (10pg / mL, 100pg / mL, 1ng / mL, 10ng / mL, 100ng / mL, 500ng / mL, 1μg / mL) in a light-proof glass vial. Insert the fiber optic probe (sensing area end) and incubate for 2 hours to allow the silk fibroin and immune antibody to fully combine. Add Au / Pt@CuO / Cu2O labeled secondary antibody solution (1.5mg / mL) and incubate for 2 hours, and finally add a 10% mass concentration of hydrogen peroxide solution as a trigger. The data can be received and recorded on the computer.
[0093] like Fig.17 and 18 As shown in the figure, the results show that as a reactant in the luminol-catalyzed luminescence reaction, a too low concentration of hydrogen peroxide will lead to a slow reaction process, resulting in a decrease in the obtained luminescence intensity, thereby reducing the sensitivity of the sensor. The prepared optical fiber chemiluminescence sensor for quantitative detection of silk fibroin in silk is 10 -1 ~10 2 In the pg / mL range, the calibration equation is y = 89.95x + 591.78 (R 2 =0.980) (where Y is the chemiluminescence intensity and X is the silk fibroin concentration (ng / mL)). The limit of detection (LOD) was defined by the 3σ / M value (where the standard deviation (SD) of blank samples similar to the treated silk fibroin samples was recorded as σ, n=10, and M was the slope of the calibration curve in the low concentration linear range) and was determined to be 55 pg / mL.
[0094] The lowest concentration of silk fibroin that can be detected by the optical fiber immunosensor prepared in the above-mentioned embodiments and comparative examples is shown in Table 1 below.
[0095] Table 1
[0096]
[0097] The above embodiments of the present invention are merely examples for illustrating the present invention, and are not intended to limit the embodiments of the present invention. For those skilled in the art, other different forms of changes and modifications can be made based on the above description. It is impossible to list all the embodiments here. Any obvious changes or modifications derived from the technical solution of the present invention are still within the scope of protection of the present invention.
Claims
1. A method for preparing a chemiluminescent optical fiber immunosensor, characterized in that: The optical fiber immunosensor comprises a secondary antibody labeled with Au / Pt@CuO / Cu2O and an optical fiber probe, and the preparation method thereof comprises the following steps: Step 1: Preparation of Au / Pt@CuO / Cu2O labeled secondary antibody; (1) adding the Au NPs dispersion into a solution containing HAuCl4·4H2O and HCl, then adding an AgNO3 solution and an ascorbic acid solution, and then dispersing the mixture in water to obtain an Au NPs solution; The Au NPs solution, NaI solution, hexadecyltrimethylammonium bromide solution, AgNO3 solution and ascorbic acid solution were mixed and stirred at 70°C for 0.5-2h; then K2PtCl6 solution was added and stirred at 70°C for 4h, followed by centrifugation to obtain Au / PtNPs; (2) PVP powder was added to Cu(NO3)2 solution, and then Au / Pt NPs solution and N2H4·H2O solution were added, and the mixture was stirred for 40-60 min, centrifuged, and washed to obtain Au / Pt@CuO / Cu2O powder; (3) Au / Pt@CuO / Cu2O powder was dispersed in an ethanol aqueous solution, the pH was adjusted to 5-5.5, 3-aminopropyltriethoxysilane solution was added, and after ultrasonic dispersion, the solution was heated in a water bath and heated and stirred at 75°C for 1 hour; after the reaction was completed, the reactants were filtered and washed, and the obtained reactants were dispersed in an ethanol aqueous solution, the mixed solution was mixed with PBS buffer, and glutaraldehyde solution was added, and incubated at 25°C for 2 hours; then dispersed in a solution containing EDC and NHS, incubated at room temperature for 1 hour, and then Ab2 solution was added and incubated for 24 hours, and then the Au / Pt@CuO / Cu2O labeled secondary antibody was separated by centrifugation; Step 2: Preparation of optical fiber probe; (a) The sheath layer of the optical fiber probe is removed with a knife at a position 0.5 cm from the end to form the sensing area. The sensing area is immersed in hydrofluoric acid to remove the cladding of the optical fiber, and then washed and dried. (b) immersing the sensing area of the optical fiber probe in a mixed solution of γ-glycidyloxypropyltrimethoxysilane and ethanol for 1-3 hours, taking it out and immersing it in a primary antibody solution, and incubating it at room temperature for 1 hour; (c) After taking out, immerse in luminol solution and incubate for 2 h, then immerse in BSA solution to block nonspecific binding sites, wash and refrigerate for later use.
2. The method for preparing the chemiluminescence-based optical fiber immunosensor according to claim 1, characterized in that: In step (1), the added volume ratio of the Au NPs dispersion, the solution containing HAuCl4·4H2O and HCl, the AgNO3 solution and the ascorbic acid solution is 15:50-60:1-2:15-18:7-9; the added volume ratio of the AuNPs solution, NaI solution, hexadecyltrimethylammonium bromide solution, AgNO3 solution, ascorbic acid solution and K2PtCl6 solution is 5mL:100-200μL:20-25mL:20-50μL:450-550μL:900μL.
3. The method for preparing the chemiluminescence-based optical fiber immunosensor according to claim 1 or 2, characterized in that: In step (1), the concentration of the Au NPs dispersion is 5-6 mM; in the solution containing HAuCl4·4H2O and HCl, the concentration of HAuCl4·4H2O is 7-8 mM, and the concentration of HCl is 1-1.2 M; and the concentration of the K2PtCl6 solution is 2-5 mM.
4. The method for preparing the chemiluminescence-based optical fiber immunosensor according to claim 1, characterized in that: In step (2), the ratio of the added amounts of the PVP powder, Cu(NO3)2 solution, Au / PtNPs solution and N2H4·H2O is 1 g: 5-20 mL: 1 mL: 15-20 μL.
5. The method for preparing the chemiluminescence-based optical fiber immunosensor according to claim 1 or 4, characterized in that: In step (2), the average molecular weight of the PVP is 50000-60000; the concentration of the Au / PtNPs solution is 50-70mM; and the concentration of the Cu(NO3)2 solution is 0.01M.
6. The method for preparing the chemiluminescence-based optical fiber immunosensor according to claim 1, characterized in that: In step (3), the volume ratio of ethanol to water in the ethanol-water solution is 1:1; the added amount ratio of the Au / Pt@CuO / Cu2O powder, the ethanol-water solution and the 3-aminopropyltriethoxysilane solution is 0.01-0.03 g:10 mL:0.6 mL; and the added amount ratio of the reactant to the ethanol-water solution is 0.02-0.05 g:10 mL.
7. The method for preparing the chemiluminescence-based optical fiber immunosensor according to claim 1 or 6, characterized in that: In step (3), the ratio of the added amounts of the mixed solution, PBS buffer, glutaraldehyde solution, solution containing EDC and NHS, and Ab2 solution is 0.1 mL: 1-2 mL: 1-2 mL: 1 mL: 10 μL; in the solution containing EDC and NHS, the concentration of EDC is 20 mg / mL, and the concentration of NHS is 10 mg / mL; the concentration of Ab2 solution is 1-2 mg / mL, and the secondary antibody is rabbit anti-silk fibroin monoclonal antibody.
8. The method for preparing the chemiluminescence-based optical fiber immunosensor according to claim 1, characterized in that: In step (b), the mixed solution of γ-glycidyloxypropyltrimethoxysilane solution and ethanol has a mixing volume ratio of 1:1; the concentration of the primary antibody solution is 0.05-0.2 mg / mL, and the primary antibody is a mouse anti-silk fibroin monoclonal antibody.
9. The method for preparing the chemiluminescence-based optical fiber immunosensor according to claim 1 or 8, characterized in that: In step (c), the concentration of the luminol solution is 10-15 mg / mL; the mass concentration of the BSA solution is 1-2%.
10. An application of the optical fiber immunosensor prepared by the preparation method according to any one of claims 1 to 9 in detecting silk fibroin, characterized in that: The method comprises the following steps: connecting the optical fiber probe to the data transmission module, immersing the sensing area end of the optical fiber probe in a silk protein solution for incubation, adding a secondary antibody solution labeled with Au / Pt@CuO / Cu2O for incubation, and finally adding a hydrogen peroxide solution as a trigger; receiving the detection data on the computer side and recording it.
Citation Information
Cited By
Preparation method and application of self-supporting electrochemical immunosensor based on Au-modified Cu2O / CuO heterostructure
CN119534829A