Wiring board
By designing obtuse angle protrusions and thickened through-hole conductors at the openings of the through-hole conductors, the stress concentration problem caused by expansion of the resin filler is solved, and the electrical reliability of the wiring substrate is improved.
Patent Information
- Application Number
- CN202380029526.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-30
- Filing Date
- 2023-03-30
- Publication Date
- 2024-11-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Under high temperature conditions, the expansion of the resin filler causes stress concentration of the through-hole conductor, resulting in cracks or stripping of the connecting plate, resulting in poor electrical reliability of the wiring substrate.
A wiring substrate structure is designed, wherein the through-hole conductor has a protrusion extending inwardly at the opening of the through-hole, and has an obtuse angle with the filling resin, reducing stress concentration and thickening the through-hole conductor to improve strength.
It effectively reduces the occurrence of cracks in the through-hole conductors, improves the electrical reliability of the wiring substrate, and ensures that good electrical performance can be maintained under high temperature conditions.
Smart Images

Figure CN118975416A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a wiring substrate. Background Art
[0002] Conventionally, in wiring substrates, there are cases where through-holes are filled with through-hole conductors and cases where through-hole conductors are formed only on the inner wall surface of the through-hole and the remaining portion is filled with resin. For example, in a wiring substrate described in Patent Document 1, a conductor film is located on the inner wall surface of the through-hole, and a filler formed of resin is located on the remaining portion.
[0003] In the case where the conductor film is located on the inner wall surface of the through hole and the filler formed of resin is located on the remaining part as in the wiring substrate described in Patent Document 1, for example, under high temperature conditions, the filler formed of resin expands and stress is concentrated on the corner of the through hole. If the stress is concentrated in this way, cracks will be generated in the through hole conductor or the through hole land will be peeled off. As a result, the electrical reliability of the wiring substrate will deteriorate.
[0004] Prior Art Literature
[0005] Patent Literature
[0006] Patent Document 1: Japanese Patent Application Publication No. 2021-27167 Summary of the invention
[0007] -Methods for solving problems-
[0008] The wiring substrate involved in the present disclosure includes: an insulating layer having a first surface and a second surface located on the side opposite to the first surface; a through hole having openings on the first surface and the second surface of the insulating layer; a through-hole conductor configured from the periphery of the opening of the first surface to the periphery of the opening of the second surface via the inner wall surface of the through-hole; and a filling resin located in an area surrounded by the through-hole conductor and having two surfaces, a first surface on the first surface side and a second surface on the second surface side. The through-hole conductor includes a first through-hole conductor. The first through-hole conductor has a protrusion extending toward the inside of the through-hole at the opening of at least one side of the through-hole. When viewed in section, the angle formed by the portion of the protrusion adjacent to the filling resin and at least the first surface or the second surface of the filling resin is an obtuse angle. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 It is a cross-sectional view showing a wiring substrate according to one embodiment of the present disclosure.
[0010] Figure 2 It is used to illustrate Figure 1 An enlarged illustration of region X is shown.
[0011] Figure 3 It is used to illustrate Figure 1 An enlarged illustration of region Y is shown.
[0012] Figure 4 It is used to form Figure 1 An explanatory diagram of the process in area X is shown.
[0013] Figure 5 It is used to form Figure 1 An explanatory diagram of the process in area X is shown. DETAILED DESCRIPTION
[0014] In the conventional wiring substrate described in Patent Document 1, when the conductor film is located on the inner wall surface of the through hole and the filler formed by the resin is located in the remaining part, for example, under high temperature conditions, the filler formed by the resin expands and the stress is concentrated on the corner of the through hole. If the stress is concentrated in this way, cracks will be generated in the through hole conductor or the through hole connection land will be peeled off. As a result, the electrical reliability of the wiring substrate deteriorates. Therefore, a wiring substrate with excellent electrical reliability and reduced cracks in the through hole conductor is required.
[0015] The wiring board according to the present disclosure has the structure described in the section of means for solving the problems, thereby reducing cracks generated in through-hole conductors and having excellent electrical reliability.
[0016] based on Figures 1 to 3 A wiring board according to an embodiment of the present disclosure will be described. Figure 1 1 is a cross-sectional view showing a wiring board 1 according to an embodiment of the present disclosure. The wiring board 1 according to the first embodiment includes a core insulating layer 2 , a build-up layer 3 , and a solder resist 6 .
[0017] The core insulating layer 2 is not particularly limited as long as it is a material having insulating properties. Examples of insulating materials include epoxy resins, bismaleimide-triazine resins, polyimide resins, polyphenylene ether resins, and the like. Two or more of these resins may be mixed and used. The thickness of the core insulating layer 2 is not particularly limited, and is, for example, 800 μm or more and 1400 μm or less.
[0018] The core insulating layer 2 may include a reinforcing material. Examples of the reinforcing material include insulating fabrics such as glass fiber, glass nonwoven fabric, aramid nonwoven fabric, aramid fiber, and polyester fiber. Two or more reinforcing materials may be used in combination. Furthermore, inorganic insulating fillers such as silica, barium sulfate, talc, clay, glass, calcium carbonate, and titanium oxide may be dispersed in the core insulating layer 2. Two or more inorganic insulating fillers may be used in combination.
[0019] The build-up layer 3 is located on the first surface and the second surface of the core insulating layer 2. The first surface and the second surface refer to the upper surface and the lower surface. Figure 1In the embodiment, for convenience, the first surface is set as the upper surface and the second surface is set as the lower surface. The build-up layer 3 has a structure in which the conductor layer 4 and the build-up layer insulating layer 5 are alternately stacked. The conductor layer 4 included in the build-up layer 3 is formed of a conductor such as copper foil or copper plating. The thickness of the conductor layer 4 is not particularly limited, for example, it is greater than 15 μm and less than 30 μm.
[0020] The build-up insulating layer 5 included in the build-up layer 3 is the same as the core insulating layer 2, and is not particularly limited as long as it is a material with insulating properties. Examples of insulating materials include epoxy resins, bismaleimide-triazine resins, polyimide resins, polyphenylene ether resins, and other resins. Two or more of these resins may be mixed and used. When there are two or more build-up insulating layers 5 in the build-up layer 3, each build-up insulating layer 5 may be formed of the same resin or different resins. The build-up insulating layer 5 and the core insulating layer 2 included in the build-up layer 3 may be the same resin or different resins.
[0021] Furthermore, the build-up insulating layer 5 included in the build-up layer 3 may also contain a reinforcing material, similarly to the core insulating layer 2. Examples of the reinforcing material include insulating fabrics such as glass fiber, glass nonwoven fabric, aramid nonwoven fabric, aramid fiber, and polyester fiber. Two or more reinforcing materials may be used in combination. Furthermore, in the build-up insulating layer 5, inorganic insulating fillers such as silica, barium sulfate, talc, clay, glass, calcium carbonate, and titanium oxide may be dispersed, similarly to the core insulating layer 2. Two or more inorganic insulating fillers may be used in combination.
[0022] The thickness of the build-up insulating layer 5 included in the build-up layer 3 is not particularly limited, and is, for example, 25 μm to 60 μm. When there are two or more build-up insulating layers 5 in the build-up layer 3, the respective build-up insulating layers 5 may have the same thickness or different thicknesses.
[0023] The build-up insulating layer 5 included in the build-up layer 3 has a via conductor for electrically connecting the layers. The via conductor is located in a via hole that penetrates the upper and lower surfaces of the build-up insulating layer 5 included in the build-up layer 3. The via conductor is formed of a conductor such as a metal plating layer such as a copper plating layer. The via conductor is connected to the conductor layer 4 located on the upper and lower surfaces of the build-up insulating layer 5 included in the build-up layer 3. The via conductor can be filled in the via hole, or it can be located only on the inner wall surface of the via hole.
[0024] The solder resist 6 is located on a part of both surfaces of the wiring board 1 according to the first embodiment. The solder resist 6 is formed of, for example, an acrylic modified epoxy resin. The solder resist 6 has a function of protecting, for example, solder from adhering to the conductor layer 4 when mounting electronic components.
[0025] The core insulating layer 2 has a first through-hole conductor 21 and a second through-hole conductor 22 in order to electrically connect the first surface and the second surface (upper and lower surfaces) of the core insulating layer 2. The first through-hole conductor 21 and the second through-hole conductor 22 are located in through-holes 2a and 2b that penetrate the upper and lower surfaces of the core insulating layer 2. The first through-hole conductor 21 and the second through-hole conductor 22 are, for example, cylindrical in the through-holes 2a and 2b, and are formed of a conductor such as a metal (for example, copper), and are connected to the conductor layer 4 located on the upper and lower surfaces of the core insulating layer 2.
[0026] For example, Figure 1 As shown, the first through-hole conductor 21 located in the through-hole 2a is located in the first region 11. The first region 11 is a region having a first occupancy ratio in which the ratio of the opening area of the through-hole 2a to the unit area is relatively high. The first occupancy ratio can be read, for example, from an enlarged photograph of the surface of the core insulating layer 2 at a position of 1 mm 2 The number of through holes 2a in the inner wall is multiplied by the opening area (mm) of each through hole 2a. 2 In the first region 11, the opening area of the through hole 2a is calculated by 2 For example, 0.07 mm 2 above.
[0027] The first through-hole conductor 21 is arranged from the opening periphery of the first surface of the core insulating layer 2 to the opening periphery of the second surface via the inner wall surface of the through-hole 2a. Figure 2 As shown in FIG. 1 , the first through-hole conductor 21 has a protrusion 211 extending toward the inside of the through-hole 2a at at least one opening of the through-hole 2a. Figure 2 In the embodiment, there are protrusions 211 in the two openings of the through hole 2a. Figure 2 It is used to illustrate Figure 1 An enlarged illustration of region X is shown.
[0028] The first through-hole conductor 21 is not filled in the through-hole 2a. In the through-hole 2a, the portion other than the first through-hole conductor 21 is filled with a filling resin 21a. The filling resin 21a is in a columnar shape with the uppermost surface (end surface) located on the first surface side of the core insulating layer 2 as the first surface F1 and the lowermost surface (end surface) located on the second surface side as the second surface F2. Examples of the filling resin 21a include resins such as epoxy resins, bismaleimide-triazine resins, polyimide resins, and polyphenylene ether resins.
[0029] The width of at least one of the first surface F1 and the second surface F2 of the filling resin 21a may be not less than 40% and not more than 90% of the width of the through hole 2a. Figure 2As shown in FIG. 1 , when the width of at least one of the first surface F1 and the second surface F2 of the filling resin 21a is set to W1 and the width of the through hole 2a is set to W2, the length of the width W1 may be 40% or more and 90% or less of the length of the width W2. If the width of at least one of the first surface F1 and the second surface F2 of the filling resin 21a is within such a range, the thickness of the first through-hole conductor 21 near the opening of the through hole 2a can be ensured while maintaining the ease of filling of the filling resin 21a, thereby achieving improved strength.
[0030] like Figure 2 As shown, when the through hole 2a is cross-sectioned, the angle θ formed by the portion P1 of the protrusion 211 adjacent to the filling resin 21a and the first surface F1 of the filling resin 21a is an obtuse angle. The angle θ is not limited as long as it is an obtuse angle, and can be, for example, greater than 100° and less than 160°. There are four angles θ in a cross-section of the through hole 2a, and they do not need to be all the same angle. The angles of the angle θ can be different as long as they are obtuse angles. The "section" of the cross-section refers to the section in the depth direction of the through hole 2a (the thickness direction of the core insulation layer 2).
[0031] In the first region 11 where the through holes 2a are densely present, as shown in FIG. Figure 1 As shown, the via conductors located in the insulating layer 5 for the build-up layer tend to be stacked. By stacking the via conductors in this way, stress is easily applied to the through-hole land located in the lower layer, and cracks are easily generated. By making the angle θ an obtuse angle, the stress can be dispersed near the opening of the through hole 2a. Therefore, the peeling of the through-hole land can be reduced. Furthermore, near the opening of the through hole 2a, the first through-hole conductor 21 is thicker, so it is difficult to crack even if stress is applied. If the angle θ is greater than 100° and less than 160°, these effects can be further exerted.
[0032] The through-hole connection pad is a connection pad conductor that is part of the conductor layer 4, and is arranged on the surface of the filling resin 21a located on the first surface side (the first surface F1 of the filling resin 21a) and the surface of the filling resin 21a located on the second surface side (the second surface F2 of the filling resin 21a), and the surface of the through-hole conductor (first through-hole conductor 21) located on the first surface and the second surface of the core insulation layer 2.
[0033] In the core insulating layer 2, not only the first through-hole conductor 21 but also the second through-hole conductor 22 may be present. The second through-hole conductor 22 is located in the through-hole 2b of the core insulating layer 2. Figure 1 As shown, the through hole 2b is located in the second region 12, for example. The second region 12 is a region having a second occupancy ratio in which the ratio of the opening area of the through hole 2b per unit area is lower than the first occupancy ratio. In the second region 12, the opening area of the through hole 2b is 1 mm2 per 1 mm2 of the surface of the core insulating layer 2.2 For example, 0.05 mm 2 The second occupancy can be read, for example, from a magnified photograph of the surface of the core insulating layer 2 at a position of 1 mm 2 The number of through holes 2b in the hole 2 is multiplied by the opening area (mm) of each through hole 2b. 2 ) to calculate.
[0034] The second through-hole conductor 22 is also arranged from the opening periphery of the first surface of the core insulating layer 2 to the opening periphery of the second surface via the inner wall surface of the through-hole 2b, similarly to the first through-hole conductor 21. Figure 3 As shown, the second through-hole conductor 22 does not have the protruding portion 211 that the first through-hole conductor 21 has. Figure 3 It is used to illustrate Figure 1 An enlarged illustration of region Y is shown.
[0035] The second through-hole conductor 22 is also not filled in the through-hole 2b like the first through-hole conductor 21, and the remaining portion in the through-hole 2b is filled with a filling resin 22a. The filling resin 22a is the same as the filling resin 21a, and a detailed description thereof is omitted.
[0036] The second through-hole conductor 22 does not have the protrusion 211. That is, the width of the first surface side (first surface F1) and the second surface side (second surface F2) of the filling resin 22a surrounded by the second through-hole conductor 22 is wider than the width of the first surface F1 and the second surface F2 of the filling resin 21a surrounded by the first through-hole conductor 21, corresponding to the absence of the protrusion 211. In the second region 12 where the through-holes 2b are sparse, as shown in FIG. Figure 1 As shown, the via conductors located in the build-up insulating layer 5 are rarely stacked. Therefore, stress is less likely to be applied to the via lands located in the lower layer. Therefore, the protrusion 211 is not provided, and the filling resin 22a has a structure with excellent filling properties.
[0037] The thickness L2 of the second through-hole conductor 22 located on the inner wall of the through-hole 2b may be thicker than the thickness L1 of the first through-hole conductor 21 located on the inner wall of the through-hole 2a. Specifically, the first through-hole conductor 21 located on the inner wall of the through-hole 2a may have a thickness L1 of, for example, 10 μm or more and 40 μm or less. The second through-hole conductor 22 located on the inner wall of the through-hole 2b may have a thickness L2 of, for example, 10 μm or more and 40 μm or less. Within these ranges, the thickness L2 of the second through-hole conductor 22 may be thicker than the thickness L1 of the first through-hole conductor 21. The thickness of the conductor located on the inner wall may be set to, for example, the average value of the values obtained by measuring the thickness of the conductor at three points in the vertical direction from the inner wall of the through-hole.
[0038] By increasing the thickness of the conductor located on the inner wall of the through hole 2b in the second through-hole conductor 22, the rigidity of the wiring substrate 1 can be improved. As a result, the warping of the wiring substrate 1 can be reduced. Furthermore, the wiring in the second region 12 tends to be longer than that in the first region 11, and the on-resistance increases. By increasing the thickness of the conductor located on the inner wall of the through hole 2b in the second through-hole conductor 22, the on-resistance can be reduced.
[0039] about Figure 2 The metal layer 23a, the seed layer 23b, the seed layer 4a, and the electrolytic plated metal layer 4b described in 3 are also described when describing the process of forming the region X described later.
[0040] In the wiring substrate 1 according to one embodiment, the first through-hole conductor 21 is formed in the through-hole 2a, and the method of filling the filling resin 21a is not limited, for example, by Figure 4 as well as Figure 5 The process shown is formed. Figure 4 as well as Figure 5 It is used to form Figure 1 An explanatory diagram of the process in area X is shown.
[0041] First, if Figure 4 As shown in A, a double-sided metal-clad laminate is prepared in which a metal layer 23a such as copper is laminated on both sides of the core insulating layer 2. The thickness of the metal layer 23a is, for example, 2 μm to 20 μm. The core insulating layer 2 is as described above, and detailed description thereof is omitted.
[0042] Then, if Figure 4 As shown in B, a through hole 2a is formed in the double-sided metal-clad laminate. The method for forming the through hole 2a is not limited, and it can be formed using a drill, etc. At this time, the opening corner of the through hole 2a can be formed to be substantially right angles like a general through hole.
[0043] After forming the through hole 2a, a desmear treatment is performed to remove the resin and other residues. Figure 4 As shown in FIG. 3C , the inner wall surface of the through hole 2 a and the surface of the metal layer 23 a are subjected to electroless plating to form a seed layer 23 b made of a metal such as copper.
[0044] Then, if Figure 4 As shown in D, electrolytic plating is performed to form a first through-hole conductor 21 on the surface of the seed layer 23b. Since the current density is concentrated at the opening corner of the through-hole 2a, the first through-hole conductor 21 is formed thicker and protrudes toward the inside of the through-hole 2a. Figure 4 As shown in FIG. E, the through hole 2a is filled with a filling resin 21a. The filling resin 21a is as described above, and a detailed description thereof is omitted.
[0045] Then, if Figure 4 As shown in F, both surfaces are ground until the angle θ between the thick corner portion (the portion eventually corresponding to the protrusion 211) of the first through-hole conductor 21 and the surface (end face) of the filling resin 21a becomes an obtuse angle. The grinding method is not limited, and examples thereof include a polishing grinder, a belt grinder, and the like.
[0046] After grinding, Figure 5 As shown in A of FIG. 1 , a resist 7 is formed at a portion where a through hole land is formed. As the resist 7, for example, a dry film resist is used. Next, as shown in FIG. Figure 5 As shown in B, etching is performed to remove the metal layer 23a not covered by the resist 7, and then the resist 7 is removed.
[0047] After removing the metal layer 23a and the resist 7, as shown in FIG. Figure 5 As shown in FIG. C, the surface of the exposed core insulating layer 2 is subjected to electroless plating to form a seed layer 4a using a metal such as copper. The seed layer 4a is also formed in the portion covered by the resist 7. The seed layer 4a is the same as the seed layer 23b described above.
[0048] Then, if Figure 5 As shown in D, a resist 7 is formed outside the portion where the through hole land is formed. After the resist 7 is formed, electrolytic plating is performed to form an electrolytic plated metal layer 4b with a metal such as copper. Figure 5 As shown in FIG. 8E, etching is performed to remove the resist 7 and the seed layer 4a covered by the resist 7, thereby forming a through-hole land (conductor layer 4).
[0049] Through this process, the Figure 1 The area X is shown. Figure 1 The region Y shown is also formed by the same steps as the above process. Specifically, the second through-hole conductor 22 formed thickly at the opening corner of the through-hole 2b where the current density is concentrated is removed by grinding, or the plating conditions are adjusted so that the second through-hole conductor 22 is not formed thickly and only needs to be filled with the filling resin 22a.
[0050] The wiring substrate of the present disclosure is not limited to the wiring substrate 1 involved in the above-mentioned embodiment. In the wiring substrate 1 involved in the above-mentioned embodiment, the first through-hole conductor 21 is located in the first region 11, and the second through-hole conductor 22 is located in the second region 12. However, the wiring substrate of the present disclosure may not have the second through-hole conductor, and the first through-hole conductor may be located in the second region. Furthermore, the first through-hole conductor and the second through-hole conductor may be mixed in the first region and the second region.
[0051] -Explanation of symbols-
[0052] 1 Wiring substrate
[0053] 11First Area
[0054] 12 Second Area
[0055] 2Insulation layer for fiber core
[0056] 2a, 2b through holes
[0057] 21 first through-hole conductor
[0058] 211 salient
[0059] 21 a Filling resin
[0060] 22 Second through-hole conductor
[0061] 22a Filling resin
[0062] 23a Metal layer
[0063] 23b Seed layer
[0064] 3 layers
[0065] 4 conductor layers
[0066] 4a Seed layer
[0067] 4b Electrolytically plated metal layer
[0068] 5. Insulation layer for build-up
[0069] 6. Solder Resist
[0070] 7. Resist
[0071] F1 first surface
[0072] F2 second surface
[0073] P1: A portion of the protruding portion adjacent to the filling resin.
Claims
1. A wiring substrate comprising: An insulating layer having a first surface and a second surface located on a side opposite to the first surface; a through hole having openings on the first surface and the second surface of the insulating layer; a through-hole conductor arranged from the periphery of the opening of the first surface to the periphery of the opening of the second surface via the inner wall surface of the through-hole; and The filling resin is located in a region surrounded by the through-hole conductor and has two surfaces, a first surface on the first surface side and a second surface on the second surface side. The through-hole conductors include a first through-hole conductor, The first through-hole conductor has a protrusion extending toward the inside of the through-hole at the opening of at least one of the through-holes. In cross-sectional view, an angle formed between a portion of the protrusion adjacent to the filling resin and at least the first surface or the second surface of the filling resin is an obtuse angle.
2. The wiring substrate according to claim 1, wherein: The land conductor is arranged on the surface of the through-hole conductor located on the first surface, the first surface of the filling resin located on the first surface side, the surface of the through-hole conductor located on the second surface, and the second surface of the filling resin located on the second surface side.
3. The wiring substrate according to claim 1 or 2, wherein: The first angle is greater than or equal to 100° and less than or equal to 160°.
4. The wiring substrate according to any one of claims 1 to 3, wherein: A width of at least one of the first surface and the second surface of the filling resin surrounded by the first through-hole conductor is not less than 40% and not more than 90% of a width of the through-hole.
5. The wiring substrate according to any one of claims 1 to 4, wherein: The insulating layer includes a first region where the ratio of the opening area of the through hole to the unit area is a first occupancy rate and a second region where the ratio of the opening area of the through hole to the unit area is a second occupancy rate, the second occupancy rate is smaller than the first occupancy rate, The first through-hole conductor is located in the first region.
6. The wiring substrate according to claim 5, wherein: The through-hole conductor further includes a second through-hole conductor, The thickness of the conductor located on the inner wall of the through hole in the second through-hole conductor is thicker than the thickness of the conductor located on the inner wall of the through hole in the first through-hole conductor. The second through-hole conductor is located in the second region.
7. The wiring substrate according to claim 6, wherein: Widths of the first surface and the second surface of the filling resin surrounded by the second through-hole conductor are larger than widths of the first surface and the second surface of the filling resin surrounded by the first through-hole conductor.
Citation Information
Patent Citations
Wiring board
JP2021027167A