Interface doping modification method for metal-semiconductor contact resistor

By performing metal element doping modification at the interface between NiSi and Si, using metal elements with less electronegativity such as Hf, Sc, Ti, and Zr, the contact resistance between the source/drain and channel in small-sized integrated circuits is reduced. The problem of interface contact resistance improvement in the prior art has been solved, and the current driving capability and overall performance of the device have been significantly improved.

CN118983307APending Publication Date: 2024-11-19SHANGHAI JIAOTONG UNIV
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411047158.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-01
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

In small-sized integrated circuits, the contact resistance between the source/drain region and the channel increases significantly due to the shrinking of the metal/semiconductor contact area, becoming the main component of external parasitic resistance. The prior art is difficult to effectively reduce the interface contact resistance, which limits the limitation of the current technology. Improved device performance.

Method used

The metal element doping modification is performed at the interface between NiSi and Si, and metal elements with less electronegativity are selected, such as Hf, Sc, Ti, Zr, Al, and Ta, through sputtering deposition and ion implantation, to form a metal/semiconductor interface Doping reduces Schottky barrier and improves carrier transport efficiency.

Benefits of technology

Effectively reduces the gold semi-contact resistance, maintains the advantages of the NiSi system in small size, enhances the current driving ability of the device, and improves the overall performance. Specifically, the selection of Hf, Sc, Ti, Zr and other elements through theoretical calculations and material screening is significantly Reduced NiSi/Si contact resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118983307A_ABST
    Figure CN118983307A_ABST
Patent Text Reader

Abstract

The invention discloses an interface doping modification method of a metal-semiconductor contact resistor, which comprises the following steps: metal element doping modification is carried out on an interface under metal-semiconductor contact, the metal-semiconductor contact is a NiSi and Si system, the metal element is a metal element with weak electronegativity and is selected from one or more of Hf, Sc, Ti, Zr, Al and Ta, particularly, NiSi is used as a metal layer, Si is used as a semiconductor layer, and the metal layer is used as a metal layer. The preparation method comprises the following steps of: doping metal elements on a contact interface, depositing Ni atoms on a Si substrate by a sputtering deposition method to form a thin film, annealing to form NiSi, and injecting the metal elements into an interface of the NiSi and Si by adopting an ion injection mode to carry out interface doping modification. The advantages of a NiSi system under the small size are kept, the interface contact resistance is further reduced, the current driving capacity of the device is enhanced, the overall performance of the device is improved, and therefore the requirement of a small-size device for the interface contact resistance is met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of gold semiconductor contact resistor modification, and in particular relates to an interface doping modification method of a gold semiconductor contact resistor. Background Art

[0002] With the development of integrated circuits, the size of individual components is getting smaller and smaller, resulting in increasingly serious problems such as leakage and heat dissipation, and a sharp increase in power consumption. In order to alleviate the negative effects of size reduction, emerging device structures such as fin field effect transistors (Fin-FET) and gate-all-around transistors (GAA-FET) can reduce leakage current due to enhanced gate control capabilities, thereby reducing device power consumption and improving device reliability. Even so, when the transistor feature size is below 20nm, the contact resistance between the source / drain region and the channel increases exponentially due to the smaller metal / semiconductor contact area, becoming the main component of the external parasitic resistance. Therefore, how to reduce the contact resistance between the source / drain region and the channel is crucial to improving the performance of small-size devices.

[0003] In the prior art, self-aligned silicide is constructed at the interface between the metal electrode and silicon, which can significantly reduce the interface contact resistance. Among them, TiSi2, as the standard silicide material in the industry, has been widely used in the process. However, TiSi2 is seriously affected by the line width effect, and it is very easy to form clusters during the further reduction of the size, and the stability is poor. In contrast, CoSi2 has become a new silicide alternative material due to its lower resistivity and better interface characteristics, but due to its disadvantages such as high thermal budget and excessive consumption of silicon, the further miniaturization of the device size is limited. Recently, NiSi self-aligned silicide is constructed at the interface between the metal electrode and silicon. Due to its advantages such as low resistivity, low silicon consumption, and not easy to form clusters, it is currently an effective method to improve the interface resistance. However, this method still cannot meet the needs of small-sized devices for interface contact resistance. Therefore, it is urgent to study and explore how to further reduce the contact resistance between the source / drain and the Si channel under the current interface NiSi system. On the one hand, it can maintain the advantages of the NiSi system under small size, and on the other hand, it can further reduce the interface contact resistance and enhance the device current driving capability, thereby improving the overall performance of the device.

[0004] Previous studies have found that interfacial charge transfer can significantly affect the dipole and energy band arrangement of the interface, effectively reducing the Schottky barrier of the gold semiconductor contact, thereby reducing the interfacial contact resistance. Therefore, the interface doping modification method under the gold semiconductor contact has become a problem that needs to be urgently solved in the existing technology. Summary of the invention

[0005] The purpose of the present invention is to provide an interface doping modification method for gold-semiconductor contact resistance, in which the interface of NiSi and Si is modified by doping with metal elements in a system with NiSi as the interface silicide, so as to maintain the advantages of the NiSi system in small size on the one hand, and further reduce the interface contact resistance on the other hand, enhance the current driving capability of the device, and improve the overall performance of the device, thereby meeting the requirements of small-size devices for interface contact resistance.

[0006] To achieve the above object, the present invention adopts the following technical solutions:

[0007] The present invention provides an interface doping modification method for a gold-semiconductor contact resistor, comprising: performing metal element doping modification on the interface of a gold-semiconductor contact resistor under the condition of:

[0008] The gold-semiconductor contact is a NiSi and Si system;

[0009] The metal element is a metal element with weak electronegativity, selected from one or more of Hf, Sc, Ti, Zr, Al, and Ta.

[0010] Preferably, the metal element is selected from one or more of Hf, Sc, Ti and Zr.

[0011] More preferably, the metal element is Hf.

[0012] Preferably, the interface doping modification method of the gold-semiconductor contact resistor uses NiSi as the metal layer and Si as the semiconductor layer, and doping metal elements at the contact interface thereof, comprising:

[0013] (1) Ni atoms are deposited on a Si substrate to form a thin film by sputtering, and then annealed to form NiSi;

[0014] (2) Using ion implantation, metal elements are injected into the interface between NiSi and Si to perform interface doping modification.

[0015] Compared with the prior art, the interface doping metal provided by the present invention reduces the gold / semi contact resistance and has the following advantages:

[0016] Beneficial effects:

[0017] (1) Based on the essential mechanism of interface contact resistance regulation, doping a metal with low electronegativity at the metal / semiconductor interface can provide a portion of electrons to the interface system, reduce the semiconductor band offset caused by the metal layer, lower the interface Schottky barrier, and improve the metal / semiconductor contact interface resistance.

[0018] (2) Using metal elements with low electronegativity as dopants at the gold / semi-contact interface can not only contribute electrons but also effectively increase the carrier transport efficiency of the gold / semi-contact interface while also avoiding process complexity.

[0019] (3) When metal is doped at the metal / semiconductor interface, its formation energy is generally less than zero, and doping at the interface is highly practical.

[0020] (4) The method of reducing the metal / semiconductor contact resistance by interface doping in the present invention selects elements such as Al, Sc, Ti, Zr, Hf and Ta to reduce the metal / semiconductor contact resistivity through theoretical calculation and actual material screening. The metal dopants Hf, Sc, Ti and Zr have a more obvious effect on reducing the metal / semiconductor resistivity. When reducing the contact resistance of the NiSi / Si contact system, the Schottky barrier height is low, thereby showing better contact performance, reducing the band shift generated when the metal / semiconductor is in direct contact, and doping Hf with the lowest electronegativity at the NiSi / Si interface can better reduce the NiSi / Si contact resistance. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 Schematic diagram of interface doping modification of the gold-semiconductor contact resistance in the embodiment; 1 is the metal layer NiSi; 2 is the semiconductor layer Si; 3 is the metal doping element.

[0022] Figure 2 Schematic diagram of comparison of Schottky barrier heights in the method for reducing contact resistance in the embodiment; the ordinate is the Schottky barrier height in eV, wherein the dotted line is the Schottky barrier height in an undoped system. DETAILED DESCRIPTION

[0023] In order to more fully understand and demonstrate the technical solutions, purposes and advantages of the present invention, the technical effects produced by the present invention are further described in detail and completely in conjunction with specific embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, not all. It should be pointed out that for those of ordinary skill in the art, other embodiments obtained without departing from the concept of the present invention all belong to the protection scope of the present invention.

[0024] The calculation method used in the following embodiments is a first-principles calculation based on density functional theory, and the calculation software package used is the PWmat calculation software package, but is not limited to this, and there are also VASP, CASTEP, Gauss, Wien2k, etc. PWmat software is a first-principles calculation software package based on GPU acceleration, and it also provides most elements in the periodic table, and is highly practical.

[0025] Example 1

[0026] In this embodiment, the metal layer is NiSi, the semiconductor layer is Si, and the doping element for providing electrons is Ti. The specific method is as follows:

[0027] The formation energy of Ti doped in NiSi / Si is -1.89eV, indicating that Ti doping in NiSi / Si is feasible. Ni atoms are deposited on a Si substrate to form a thin film by sputtering deposition, and then annealed to form NiSi. Subsequently, Hf is implanted at the interface between NiSi and Si by ion implantation. The Schottky barrier height of Ti doped at the NiSi / Si interface was evaluated, and the barrier height was 0.17eV. The results show that the barrier height is less than the barrier height of intrinsic NiSi / Si, which is 0.36eV.

[0028] In this embodiment, Ti is used as a metal / semiconductor interface doping metal, which can improve the quality of the metal / semiconductor contact interface and reduce the semiconductor band offset caused by the metal layer. In addition, Ti doping at the NiSi / Si interface can significantly reduce its Schottky barrier. The low Schottky barrier height proves that interface doping Ti can significantly reduce the NiSi / Si interface contact resistance.

[0029] Example 2

[0030] In this embodiment, the metal layer is NiSi, the semiconductor layer is Si, and the doping element for providing electrons is Hf. The specific method is as follows:

[0031] The formation energy of Hf doped in NiSi / Si is -2.29eV, indicating that Hf doping in NiSi / Si is feasible. Ni atoms are deposited on a Si substrate to form a thin film by sputtering deposition, and then annealed to form NiSi. Subsequently, Hf is implanted at the interface between NiSi and Si by ion implantation. The Schottky barrier height of Hf doped at the NiSi / Si interface is evaluated, and the barrier height is 0.16eV. The results show that the barrier height is less than the barrier height of intrinsic NiSi / Si, which is 0.36eV.

[0032] In this embodiment, Hf is used as a metal / semiconductor interface doping metal, which can improve the quality of the metal / semiconductor contact interface and reduce the semiconductor band offset caused by the metal layer. In addition, Hf doping at the NiSi / Si interface can significantly reduce its Schottky barrier. The low Schottky barrier height proves that interface doping Hf can significantly reduce the NiSi / Si interface contact resistance.

[0033] Example 3

[0034] In this embodiment, the metal layer is NiSi, the semiconductor layer is Si, and the doping element for providing electrons is Sc. The specific method is as follows:

[0035] The formation energy of Sc doped in NiSi / Si is -2.48eV, indicating that Sc doping in NiSi / Si is feasible. Ni atoms are deposited on a Si substrate to form a thin film by sputtering deposition, and then annealed to form NiSi. Subsequently, Sc is implanted at the interface between NiSi and Si by ion implantation. The Schottky barrier height of Sc doped at the NiSi / Si interface is evaluated, and the barrier height is 0.18eV. The results show that the barrier height is less than the barrier height of intrinsic NiSi / Si, which is 0.36eV.

[0036] In this embodiment, Sc is used as a metal / semiconductor interface doping metal, which can improve the quality of the metal / semiconductor contact interface and reduce the semiconductor band offset caused by the metal layer. In addition, Sc doping at the NiSi / Si interface can significantly reduce its Schottky barrier. The low Schottky barrier height proves that interface doping Sc can significantly reduce the NiSi / Si interface contact resistance.

[0037] Example 4

[0038] In this embodiment, the metal layer is NiSi, the semiconductor layer is Si, and the doping element for providing electrons is Zr. The specific method is as follows:

[0039] The formation energy of Zr doped in NiSi / Si is -2.64eV, indicating that Zr doping in NiSi / Si is feasible. Ni atoms are deposited on a Si substrate to form a thin film by sputtering deposition, and NiSi is formed by annealing. Subsequently, Zr is implanted at the interface between NiSi and Si by ion implantation. The Schottky barrier height of Zr doped at the NiSi / Si interface was evaluated, and the barrier height was 0.12eV. The results show that the barrier height is less than the barrier height of intrinsic NiSi / Si, which is 0.36eV.

[0040] In this embodiment, Zr is used as a metal / semiconductor interface doping metal, which can improve the quality of the metal / semiconductor contact interface and reduce the semiconductor band offset caused by the metal layer. In addition, Zr doping at the NiSi / Si interface can significantly reduce its Schottky barrier. The low Schottky barrier height proves that interface doping with Zr can significantly reduce the NiSi / Si interface contact resistance.

[0041] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A method for modifying the interface of gold semiconductor contact resistance by doping, It is characterized in that include: The interface is modified by metal doping under the gold semi-contact; wherein: The gold-semiconductor contact is a NiSi and Si system; The metal element is a metal element with weak electronegativity, selected from one or more of Hf, Sc, Ti, Zr, Al, and Ta.

2. The interface doping modification method of the gold semiconductor contact resistor according to claim 1, It is characterized in that The metal element is selected from one or more of Hf, Sc, Ti and Zr.

3. The interface doping modification method of the gold semiconductor contact resistor according to claim 1, It is characterized in that The metal element is Hf.

4. The interface doping modification method of the gold-semiconductor contact resistor according to any one of claims 1 to 3, wherein NiSi is used as the metal layer and Si is used as the semiconductor layer, and metal elements are doped at the contact interface. include: (1) Ni atoms are deposited on a Si substrate to form a thin film by sputtering, and then annealed to form NiSi; (2) Using ion implantation, metal elements are injected into the interface between NiSi and Si to perform interface doping modification.

Citation Information

Patent Citations

  • Process for manufacturing a schottky contact on a semiconductor substrate

    US20060183267A1

  • Method for manufacturing a semiconductor device

    US20080116494A1

  • Method of reducing contact resistance

    US20140162442A1

  • Multiple layer interface formation for semiconductor structure

    US20160118468A1