Resistive random access memory, resistive random element, resistive random layer and preparation method thereof

By forming a resistive layer by first etching and then deposition, the problem of R height restriction and side wall damage in the resistive memory is solved, and the effect of reducing R height and side wall loss is achieved, reducing the risk of failure.

CN118984644APending Publication Date: 2024-11-19XIAMEN IND TECH RES INST CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411014549.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

During the preparation of the resistive memory, the R height restriction and sidewall damage caused by metal oxide film etching increases the risk of failure.

Method used

Using the method of etching first and then deposition, grooves are formed by multiple photomask etching and filling the dielectric film, and then flattening and depositing the transition metal oxide film, reducing the height of R and reducing side wall losses.

Benefits of technology

The height and volume of R are effectively reduced, the risk of failure is reduced, and the sidewall loss is reduced by etching first and then deposition method is reduced, thereby improving the uniformity and density of the pit profile.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118984644A_ABST
    Figure CN118984644A_ABST
Patent Text Reader

Abstract

The invention discloses a resistive random access memory, a resistive random element, a resistive random layer and a preparation method thereof, and the method comprises the steps: carrying out the etching of a bottom electrode through a first photomask, so as to form a first groove; thirdly, depositing a dielectric thin film on the etched bottom electrode to cover the bottom electrode, and flattening the dielectric thin film by adopting a second photomask; then, etching the flattened dielectric thin film by adopting a third photomask to form a second groove; and finally, depositing a transition metal oxide thin film on the etched dielectric thin film to cover the dielectric thin film, and planarizing the transition metal oxide thin film to obtain a resistive layer, therefore, the structural height of the resistive random access element is reduced through two-time dielectric film deposition treatment, so that the size and distance limitation of the resistive random access element can be reduced, and the failure risk is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of storage technology, and in particular to a method for preparing a resistive switching layer, a resistive switching layer, a resistive switching element and a resistive switching memory. Background Art

[0002] In the related art, the resistive random access memory (RRAM) has a 1T1R structure, where T refers to a transistor and R refers to ReRAM. In the process of preparing the resistive random access memory layer, a metal oxide film is usually deposited on the bottom electrode first, and then the deposited metal oxide film is etched to form a 1T1R structure. Figure 1 The morphology shown in the figure; this method results in the height of R being limited, that is, the size and gap of R are limited, thereby increasing the risk of failure; furthermore, after the transition metal oxide film is etched, side wall damage is inevitable. Summary of the invention

[0003] The present invention aims to solve at least one of the technical problems in the above-mentioned technology to a certain extent. To this end, one object of the present invention is to provide a method for preparing a resistive switching layer, which can reduce the height of R, thereby avoiding the risk of failure, and at the same time reduce the sidewall loss caused by etching by etching first and then deposition.

[0004] The second objective of the present invention is to provide a resistive switching layer.

[0005] The third objective of the present invention is to provide a resistive switching element.

[0006] A fourth objective of the present invention is to provide a resistive random access memory.

[0007] To achieve the above-mentioned purpose, a method for preparing a resistive layer is proposed in an embodiment of the first aspect of the present invention, comprising the following steps: etching a bottom electrode using a first photomask to form a first groove; depositing a dielectric film on the etched bottom electrode to cover the bottom electrode, and flattening the dielectric film using a second photomask; etching the flattened dielectric film using a third photomask to form a second groove; depositing a transition metal oxide film on the etched dielectric film to cover the dielectric film, and flattening the transition metal oxide film to obtain a resistive layer.

[0008] According to the method for preparing the resistive switching layer of an embodiment of the present invention, first, a bottom electrode is etched using a first photomask to form a first groove; then, a dielectric film is deposited on the etched bottom electrode to cover the bottom electrode, and a second photomask is used to flatten the dielectric film; then, a third photomask is used to etch the flattened dielectric film to form a second groove; finally, a transition metal oxide film is deposited on the etched dielectric film to cover the dielectric film, and the transition metal oxide film is flattened to obtain the resistive switching layer; thereby avoiding the risk of failure, and reducing the side wall loss caused by etching by etching first and then depositing.

[0009] In addition, the method for preparing the resistive switching layer according to the above embodiment of the present invention may also have the following additional technical features:

[0010] Optionally, the transition metal oxide film is planarized by etching, wherein the concentration, flow rate and pressure of the etching gas are adjusted and monitored during etching to improve the uniformity of the pit profile.

[0011] Optionally, the transition metal oxide film is planarized by chemical mechanical polishing, wherein the chemical reaction activity and surface tension during the polishing process are changed by adjusting the pH value and adding different chemical reagents to improve the uniformity of the pit profile.

[0012] Optionally, the deposition method is plasma enhanced chemical vapor deposition.

[0013] Optionally, the dielectric film serves as a stop layer for the chemical mechanical polishing or etching.

[0014] Optionally, the dielectric film includes any one of silicon oxide, silicon nitride or silicon oxynitride.

[0015] In order to achieve the above object, a second aspect of the present invention provides a resistive switching layer, which is manufactured by the above-mentioned manufacturing method.

[0016] According to the resistive switching layer of the embodiment of the present invention, the height of R can be reduced by the above-mentioned preparation method, thereby reducing the volume and distance of R. At the same time, the side wall loss caused by etching can be reduced by etching first and then deposition.

[0017] To achieve the above objectives, a third aspect of the present invention provides a resistive switching element, comprising a bottom electrode, a top electrode, and a resistive switching layer and an oxygen storage layer arranged between the bottom electrode and the top electrode, wherein the resistive switching layer is manufactured using the above-mentioned preparation method.

[0018] To achieve the above-mentioned object, a fourth aspect of the present invention provides a resistive random access memory, comprising a plurality of resistive random access elements as described above, wherein the plurality of resistive random access elements are arranged in an array. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a structural schematic diagram of an existing resistive switching element;

[0020] Figure 2 A schematic diagram of a process for preparing a resistive switching layer according to an embodiment of the present invention;

[0021] Figure 3 A schematic diagram of a process for preparing a resistive switching layer according to an embodiment of the present invention;

[0022] Figure 4 FIG. 4 is a schematic diagram of a process for preparing a resistive switching layer according to another embodiment of the present invention. DETAILED DESCRIPTION

[0023] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention.

[0024] In order to better understand the above technical solution, exemplary embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. Although exemplary embodiments of the present invention are shown in the accompanying drawings, it should be understood that the present invention can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided to enable a more thorough understanding of the present invention and to fully convey the scope of the present invention to those skilled in the art.

[0025] In order to better understand the above technical solution, the above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0026] The following describes a method for preparing a resistive switching layer, a resistive switching layer, a resistive switching element, and a resistive switching memory according to embodiments of the present invention with reference to the accompanying drawings.

[0027] Figure 2 FIG. 1 is a schematic diagram of a process for preparing a resistive switching layer according to an embodiment of the present invention; Figure 2 As shown, the method for preparing the resistive switching layer includes the following steps:

[0028] S101, etching the bottom electrode using a first photomask to form a first groove.

[0029] That is, etching is performed on the bottom electrode prepared by using a first photomask so that a first groove is formed on the bottom electrode, wherein the bottom electrode prepared by the present invention is as follows: Figure 3 or Figure 4 As shown in (a).

[0030] As an example, Figure 3 or Figure 4 As shown in (b), an R mask is used to etch the bottom electrode to form a first groove.

[0031] S102, depositing a dielectric film on the etched bottom electrode to cover the bottom electrode, and using a second photomask to planarize the dielectric film.

[0032] As an example, Figure 3 or Figure 4 As shown in (c), a dielectric film (Si) is deposited on the etched bottom electrode using plasma enhanced chemical vapor deposition (PECVD). 3 N 4 ), so that the dielectric film fills the first groove and covers the bottom electrode, and then the dielectric film is flattened by using an Etch back mask. Figure 3 or Figure 4 As shown in (d), at this time, the aspect ratio of R is 6:10, and the aspect ratio of the PECVD dielectric film filling is greater than 1, so there is no risk of hole formation.

[0033] It should be noted that the dielectric film is first filled and then etched, so that voids are less likely to exist. After the transition metal oxide film is filled, there is no risk of failure due to void short circuit.

[0034] S103, using a third photomask to etch the flattened dielectric film to form a second groove. Figure 3 or Figure 4 As shown in (e), a mask is used to etch out a hole with a width of 21nm and a height of 5nm (the opening size of the 28nm process is about 20-30nm), leaving 10-20nm overlap on the left and right, so the R size can be 41nm*41nm~61nm*61nm.

[0035] S104, depositing a transition metal oxide film on the etched dielectric film to cover the dielectric film, and planarizing the transition metal oxide film to obtain a resistive switching layer.

[0036] It should be noted that the deposition of transition metal oxide thin films (Transition metal oxide, TMO

[0037] ) after Figure 3 or Figure 4 As shown in (f), the transition metal oxide film may be HfO, and this application does not make any specific limitation to this.

[0038] As an embodiment, the transition metal oxide film is planarized by etching, wherein the concentration, flow rate and pressure of the etching gas are adjusted and monitored during etching to improve the uniformity of the pit profile.

[0039] It should be noted that the planarization process is Figure 3 As shown in (g1) and (h1), pits exist after the deposition of the transition metal oxide film, and the pits can be effectively concentrated in the conductive filaments (CF) formed between the electrodes. In order to ensure the uniformity of the pit profile, cleaning and treatment processes are performed before etching to ensure that there are no impurities. At the same time, the photoresist filling selectivity ratio is utilized. When controlling the etching conditions, the concentration, flow rate and pressure of the etching gas are adjusted and monitored to improve the uniformity of the pit profile. After etching, cleaning is performed to obtain the resistive layer.

[0040] As another embodiment, a transition metal oxide film is planarized by chemical mechanical polishing, wherein the chemical reaction activity and surface tension during polishing are changed by adjusting the pH value and adding different chemical reagents to improve the uniformity of the pit profile.

[0041] It should be noted that the planarization process is Figure 4 As shown in (g2) and (h2), pits exist after the deposition of the transition metal oxide film, and the pits can be effectively concentrated on the conductive filaments formed between the electrodes. In order to ensure the uniformity of the pit profile, chemical mechanical polishing (CMP) is used to flatten the transition metal oxide film, wherein the chemical reaction activity and surface tension in the polishing process are changed by adjusting the pH value and adding different chemical reagents during polishing to improve the uniformity of the pit profile. During intermittent processing, an air gap is introduced in the contact between the polishing pad and the silicon wafer surface to reduce the wear of the CMP polishing pad, and the CMP process is monitored in real time. After polishing, the interface is cleaned with an acidic cleaning agent to obtain a resistive layer, wherein the dielectric film serves as a stop layer for CMP.

[0042] like Figure 3 or Figure 4 As shown in (i) and (j), an oxygen storage layer can be deposited on the resistive layer in an existing manner, and a top electrode can be deposited on the oxygen storage layer to obtain a resistive unit, wherein Dielectric film 1 can be used as an air gap, and Dielectric film 2 is a dielectric film including but not limited to insulating materials such as silicon oxide, silicon nitride or silicon oxynitride, which can be used as an etching stop layer.

[0043] Therefore, the present application can reduce the critical size and gap of R by reducing the height of R without increasing the process steps, and avoid the formation of voids, thereby achieving the effect of increasing density and reducing the area of ​​CF; specifically, the existing Rsize 90*90, space 85, Area = 90 + 85 / 28 × 90 + 85 / 28 = 39F 2 , this application can achieve R size 41*41, space 50, Area = 41 + 50 / 28 × 41 + 50 / 28 = 10.5F 2 (The opening size of the 28nm process is about 20-30nm, with an overlap of 10-20nm). In addition, by etching first and then filling, the sidewall loss caused by etching can be reduced, thereby reducing the risk of ILR (Initial Low Resistance). ILR means that there are more defects in components when the initial resistance value is low.

[0044] In summary, according to the method for preparing the resistive switching layer of an embodiment of the present invention, first, a bottom electrode is etched using a first photomask to form a first groove; then, a dielectric film is deposited on the etched bottom electrode to cover the bottom electrode, and a second photomask is used to planarize the dielectric film; then, a third photomask is used to etch the planarized dielectric film to form a second groove; finally, a transition metal oxide film is deposited on the etched dielectric film to cover the dielectric film, and the transition metal oxide film is planarized to obtain the resistive switching layer; thereby avoiding the risk of failure, and at the same time, the side wall loss caused by etching is reduced by etching first and then depositing.

[0045] In order to realize the above embodiment, the embodiment of the present invention provides a resistive switching layer, which is manufactured by the above manufacturing method.

[0046] According to the resistive switching layer of the embodiment of the present invention, the height of R can be reduced by using the above-mentioned preparation method, thereby avoiding the risk of failure. At the same time, the side wall loss caused by etching can be reduced by etching first and then depositing.

[0047] To implement the above embodiment, the present invention provides a resistive switching element, including a bottom electrode, a top electrode, and a resistive switching layer and an oxygen storage layer disposed between the bottom electrode and the top electrode, wherein the resistive switching layer is manufactured by the above manufacturing method.

[0048] In order to implement the above embodiment, an embodiment of the present invention provides a resistive random access memory, comprising a plurality of resistive random access elements as described above, wherein the plurality of resistive random access elements are arranged in an array.

[0049] Those skilled in the art will appreciate that embodiments of the present invention may be provided as methods, systems, or computer program products. Therefore, the present invention may take the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Moreover, the present invention may take the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program code.

[0050] The present invention is described with reference to flowcharts and / or block diagrams of methods, devices (systems), and computer program products according to embodiments of the present invention. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as the combination of processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to produce a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.

[0051] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture comprising an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.

[0052] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1 A step that specifies a function in one or more boxes.

[0053] It should be noted that in the claims, any reference signs placed between brackets shall not be construed as limiting the claims. The word "comprising" does not exclude the presence of components or steps not listed in the claim. The word "a" or "an" preceding a component does not exclude the presence of a plurality of such components. The invention may be implemented by means of hardware comprising several different components and by means of a suitably programmed computer. In a unit claim enumerating several means, several of these means may be embodied by the same item of hardware. The use of the words first, second, and third etc. does not indicate any order. These words may be interpreted as names.

[0054] Although the preferred embodiments of the present invention have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present invention.

[0055] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.

[0056] In the description of the present invention, it should be understood that the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0057] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0058] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0059] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms should not be understood as necessarily referring to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, unless they are contradictory.

[0060] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may change, modify, replace and vary the above embodiments within the scope of the present invention.

Claims

1. A method for preparing a resistive switching layer, characterized in that: The following steps are involved: Using a first photomask to etch the bottom electrode to form a first groove; Depositing a dielectric film on the etched bottom electrode to cover the bottom electrode, and flattening the dielectric film using a second photomask; Using a third photomask to etch the flattened dielectric film to form a second groove; A transition metal oxide film is deposited on the etched dielectric film to cover the dielectric film, and the transition metal oxide film is planarized to obtain a resistive switching layer.

2. The method for preparing a resistive switching layer according to claim 1, characterized in that: The transition metal oxide film is planarized by etching, wherein the concentration, flow rate and pressure of the etching gas are adjusted and monitored during etching to improve the uniformity of the pit profile.

3. The method for preparing a resistive switching layer according to claim 1, characterized in that: The transition metal oxide film is planarized by chemical mechanical polishing, wherein the chemical reaction activity and surface tension in the polishing process are changed by adjusting the pH value and adding different chemical reagents during polishing to improve the uniformity of the pit profile.

4. The method for preparing the resistive switching layer according to claim 3, characterized in that: The dielectric film serves as a stop layer for the chemical mechanical polishing or etching.

5. The method for preparing a resistive switching layer according to claim 1, characterized in that: The deposition method is plasma enhanced chemical vapor deposition.

6. The method for preparing a resistive switching layer according to claim 1, characterized in that: The dielectric film includes any one of silicon oxide, silicon nitride or silicon oxynitride.

7. A resistive switching layer, characterized in that: The method is prepared according to any one of claims 1 to 6.

8. A resistive switching element, characterized in that: It comprises a bottom electrode, a top electrode, and a resistive switching layer and an oxygen storage layer arranged between the bottom electrode and the top electrode, wherein the resistive switching layer is made by the preparation method according to any one of claims 1 to 6.

9. A resistive random access memory, characterized in that: It comprises a plurality of resistive switching elements as claimed in claim 8, wherein the plurality of resistive switching elements are arranged in an array.