Multi-layer composite artificial board and preparation method thereof

By using a combined structure of shaving base plate, glued layer, multi-layer board and shaving roof plate in multi-layer composite artificial board, combined with the design of prefabricated holes and four-claw nuts, the problems of easy damage to the solid wood veneer layer and insufficient structural strength are solved, and the solid wood veneer layer is achieved. Stable and powerful wood effect reduces maintenance costs.

CN118990707APending Publication Date: 2024-11-22ZOY HOME FURNISHING CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411246692.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-06
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The existing solid wood veneer is prone to damage, fall off, and has insufficient structural strength. The high price of eucalyptus boards leads to stability and strength problems in use of multi-layer boards.

Method used

Using a multi-layer composite structure consisting of a shaving base plate, a lower glue layer, a multi-layer board, an upper glue layer and a shaving roof board, the design of prefabricated holes and four-claw nuts increases structural stability and strength, and spray transparent spray on the particle board The membrane resin reinforces the nut to form a stable wooden effect.

Benefits of technology

The stability of the woody effect of the particleboard surface and the structural strength of the multi-layer board are achieved, avoiding the problems of easy damage and falling, while reducing maintenance costs and broadening the scope of application.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118990707A_ABST
    Figure CN118990707A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of artificial boards, and particularly relates to a multi-layer composite artificial board and a preparation method thereof. The invention provides a multi-layer composite artificial board which structurally comprises a wood shaving bottom board, a lower cementing layer, a multi-layer board, an upper cementing layer and a wood shaving top board which are sequentially arranged from bottom to top, so that 1, the surface wood effect provided by the wood shaving bottom board and the wood shaving top board is stable enough; 2, the structural strength and the supporting strength which are mainly provided by the multi-layer plate are sufficient; in addition, the invention further provides a preparation method of the artificial board, and the preparation method is further used for effectively arranging a bottom prefabricated hole, a top prefabricated hole, a post-forming open hole and a four-claw nut.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of artificial boards, and in particular relates to a multi-layer composite artificial board and a preparation method thereof. Background Art

[0002] Common artificial boards are generally multi-layered, with the layers connected by glue. The above-mentioned "layers" can be, for example, density boards, particle boards, multi-layer boards, solid wood boards, and veneer boards. When density boards, particle boards, and multi-layer boards are produced, various types of glue mentioned above are also used.

[0003] On the other hand, the outstanding advantages of the particleboard mentioned above are: the particle details are exposed and the wood feels strong, but its structural strength is average, while the main advantage of the multilayer board is that the structural strength is large and can provide sufficient support strength. As for the density board mentioned above, its structural strength is between the particleboard and the multilayer board, while the solid wood board and veneer board mentioned above are made of raw wood without glue. The main disadvantage of the former is the high price, and the main disadvantage of the latter is that the maintenance cost and difficulty are relatively high.

[0004] For example, a Chinese utility model patent with authorization announcement number CN213682545U and authorization announcement date 2021.07.13 discloses a multi-layer board material, including a density board layer, a first connecting adhesive layer is connected to the top of the density board layer, a particle board layer is arranged on the top of the first connecting adhesive layer, a second connecting adhesive layer is connected to the top of the particle board layer, a eucalyptus board layer is arranged on the top of the second connecting adhesive layer, and a solid wood veneer layer is fixed on the top of the eucalyptus board layer.

[0005] The general advantages of the multi-layer board in this utility model patent are: the solid wood veneer layer has the texture and feel of natural real wood.

[0006] However, in actual use, the multilayer board still has at least the following two shortcomings, which are also the technical problems to be solved by the present invention, namely: First, the thickness of the existing common solid wood veneer layer is generally about 0.4mm, so it is easy to break and fall off; Second, the structural strength of the multi-layer board is mainly provided by density board, particle board and eucalyptus board. Among them, the structural strength of eucalyptus board is not as good as that of multi-layer board, and the price of eucalyptus board is higher. The structural strength of the former two is even worse than that of multi-layer board.

[0007] Therefore, in summary, there is an urgent need for a multi-layer composite artificial board with exposed and stable wood effect and relatively large overall structural strength for use in furniture, construction and other fields. Summary of the invention

[0008] The present invention provides a multi-layer composite artificial board, the structure of which includes a shavings bottom plate, a lower glue layer, a multi-layer board, an upper glue layer, and a shavings top plate which are arranged in sequence from bottom to top, so that: 1. the surface wood effect provided by the shavings bottom plate and the shavings top plate is sufficiently stable; 2. the structural strength and supporting strength mainly provided by the multi-layer board are sufficient.

[0009] In addition, the present invention also provides a method for preparing the above-mentioned artificial board, which is further used to effectively set the bottom prefabricated holes, the top prefabricated holes, the post-forming openings, and the four-claw nuts.

[0010] The technical solution adopted by the present invention to solve the above problems is: a multi-layer composite artificial board, the structure of which includes a wood chip bottom plate, a lower glue layer, a multi-layer board, an upper glue layer, and a wood chip top plate arranged in sequence from bottom to top.

[0011] A further preferred technical solution is that the thickness of the artificial board is 12.0-14.0 mm, and the thickness of the shavings top board is greater than that of the shavings bottom board.

[0012] A further preferred technical solution is that: the wood chip bottom plate is also provided with a bottom prefabricated hole, the wood chip top plate is also provided with a top prefabricated hole, the multilayer board is also provided with a post-forming opening, and the top prefabricated hole is provided with a four-claw nut that is plugged into the post-forming opening and the bottom prefabricated hole.

[0013] A further preferred technical solution is that the diameter of the bottom prefabricated hole is equal to the post-molding opening and smaller than the top prefabricated hole, and the positioning claws of the four-claw nut are arranged on the wood chip top plate.

[0014] A further preferred technical solution is that a top coating layer is further provided on the upper surface of the shavings top plate, and a bottom coating layer is further provided on the lower surface of the shavings bottom plate.

[0015] A further preferred technical solution is that a coating resin block is provided between the top prefabricated hole and the four-claw nut, which is connected to the top coating layer and is used to reinforce the four-claw nut.

[0016] A further preferred technical solution is that: the thickness of the top coating layer and the bottom coating layer is ≤1.0 mm; and the distance between the upper surface of the top coating layer and the upper end surface of the four-claw nut is ≤0.2 mm.

[0017] A method for preparing a multi-layer composite artificial board comprises the following steps in sequence: S1, opening the bottom prefabricated hole on the shaving bottom plate, and opening the top prefabricated hole on the shaving top plate; S2, firstly apply glue on both surfaces of the multilayer board, then press the wood chip bottom board and wood chip top board respectively, and finally solidify to form the lower glue layer and the upper glue layer; S3, inserting and then turning on a drill bit in the top prefabricated hole until the drill bit penetrates the lower adhesive layer, thereby finally forming the post-molding opening; S4. Insert and install the four-claw nut in the prefabricated hole on the top until the positioning claws of the four-claw nut are inserted into the wood chip top plate.

[0018] A further preferred technical solution is to include the following steps in sequence after S4: S5, spraying transparent coating resin on the upper surface of the shavings top plate and the lower surface of the shavings bottom plate respectively, and finally forming the top coating layer and the bottom coating layer.

[0019] A further preferred technical solution is that in S3, the signal of the drill bit penetrating the lower adhesive layer is a sudden decrease in the reaction force on the drill bit, at which time the lower annular edge of the annular surface of the drill bit coincides with the upper annular edge of the bottom prefabricated hole. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 It is a structural schematic diagram of the present invention.

[0021] Figure 2 It is a schematic diagram of the appearance characteristics of the wood chip bottom plate in the present invention.

[0022] Figure 3 It is a schematic diagram of the layered structure of the multilayer board in the present invention.

[0023] Figure 4 It is a schematic diagram of a distribution method of the four-claw nut in the present invention.

[0024] Figure 5 Schematic diagrams of two usage modes of the connecting bolts in the present invention.

[0025] Figure 6 It is a schematic diagram of the position of the four-claw nut in the present invention.

[0026] Figure 7 It is a schematic diagram of the molding state of the lower glue layer and the upper glue layer in the present invention.

[0027] Figure 8 It is a schematic diagram of the insertion and use of the drill bit in the present invention.

[0028] Fig. 9 It is a schematic diagram of the end position of the drill bit insertion action in the present invention.

[0029] Fig.10 Schematic diagram of the installation method of the four-claw nut in the present invention, Fig.11 Schematic diagram of the positions of the top coating layer and the bottom coating layer in the present invention.

[0030] Fig.12 Schematic diagram of the position and shape of the coating resin block in the present invention.

[0031] Fig.13 This is a schematic diagram of the first shape of the bottom coating layer in the present invention.

[0032] Fig.14 This is a schematic diagram of the second shape of the bottom coating layer in the present invention. In the figure, the meanings of the symbols are as follows: Drill bit a, bolt b, hardware c, furniture frame board d; Wood chip bottom plate 1, lower glue layer 2, multilayer board 3, upper glue layer 4, wood chip top plate 5, bottom prefabricated hole 6, top prefabricated hole 7, post-forming opening 8, four-claw nut 9, top coating layer 10, bottom coating layer 11, coating resin block 12; The annular surface has an annular edge a-1 at the lower end, an annular edge 6-1 at the upper end, and wood shavings 1-1. DETAILED DESCRIPTION

[0033] The following descriptions are merely preferred embodiments of the present invention and are not intended to limit the scope of the present invention.

[0034] As attached Figure 1-14 As shown, a multi-layer composite artificial board has a structure comprising a wood chip bottom plate 1, a lower glue layer 2, a multi-layer board 3, an upper glue layer 4, and a wood chip top plate 5 which are arranged in sequence from bottom to top.

[0035] In this embodiment, the particle board bottom plate 1 and the particle board top plate 5 are both common particle board products, such as wood particle board, bamboo particle board, etc. The material of the lower glue layer 2 and the upper glue layer 4 can be selected from the following ranges, for example: trialdehyde glue, MDI glue, soybean glue, and AB glue.

[0036] In addition, the multilayer board 3 is a multilayer solid wood board, which is formed by gluing three or more layers of single boards and heating and pressing. Both the particle board and the multilayer board 3 can be commercially available products.

[0037] At this point, the artificial board can achieve sufficient structural strength and supporting strength through the multilayer board 3, and can obtain a relatively beautiful and natural wooden feel through the particle boards on both sides.

[0038] The thickness of the particle board 1 and the particle board 5 is much greater than the common veneer layer. Specifically, the particle board is at least 2.0 mm thick, while the common veneer layer is at most 0.5 mm thick. Therefore, the particle board 1 and the particle board 5 have relatively high glue bonding stability and their own structural strength, and the particle board is not easy to fall or break.

[0039] The thickness of the artificial board is 12.0-14.0 mm, and the thickness of the shavings top board 5 is greater than that of the shavings bottom board 1 .

[0040] In this embodiment, when the thickness of the artificial board is 12.0 mm, the thicknesses of the wood chip bottom board 1, the lower glue layer 2, the multilayer board 3, the upper glue layer 4 and the wood chip top board 5 are 2 mm, 1 mm, 5 mm, 1 mm and 3 mm, respectively. When the thickness of the artificial board is 14.0 mm, the above dimensions are 3 mm, 1 mm, 5 mm, 1 mm and 4 mm, respectively.

[0041] The reason why the thickness of the wood chip top plate 5 is greater than that of the wood chip bottom plate 1 is as follows.

[0042] When the artificial board is installed vertically, the shavings top plate 5 faces outwards and faces the user, and when it is installed horizontally, the shavings top plate 5 faces upwards and is then connected to other structures, such as the cushions of a sofa. Therefore, compared to the shavings bottom plate 1, the display of wood feeling and the installation of hardware generally occur on the shavings top plate 5, so it requires greater structural strength, that is, a relatively large thickness.

[0043] The shavings bottom plate 1 is also provided with a bottom prefabricated hole 6, the shavings top plate 5 is also provided with a top prefabricated hole 7, the multilayer board 3 is also provided with a post-forming opening 8, and the top prefabricated hole 7 is provided with a four-claw nut 9 for plugging the post-forming opening 8 and the bottom prefabricated hole 6.

[0044] In this embodiment, the bottom prefabricated hole 6 and the top prefabricated hole 7 are prefabricated and excavated respectively, and then the lower adhesive layer 2 and the upper adhesive layer 4 are coated and cured, and finally the post-molded opening 8 is excavated and formed. The reasons for this molding method are mainly the following two points: First, if the lower adhesive layer 2 and the upper adhesive layer 4 are solidified first, and the above three openings are excavated and formed at one time, the problem faced is that the density and hardness performance of the particle board and the multilayer board 3 are quite different, and the punching operation needs to deal with the material change phenomenon from the particle top board 5 to the multilayer board 3, and then from the multilayer board 3 to the particle bottom board 1 from top to bottom. This makes it relatively difficult to achieve a precise punching effect in the punching operation. The through hole formed at one time is prone to various harmful problems such as tilting, burrs, and misalignment, which is not conducive to the structural stability of the artificial board itself and the subsequent hardware installation stability at the through hole; Second, if the bottom prefabricated hole 6, the top prefabricated hole 7 and the post-molding opening 8 are all prefabricated separately, when the lower adhesive layer 2 and the upper adhesive layer 4 are coated and cured, a large amount of glue will enter the post-molding opening 8, blocking it and preventing the subsequently installed bolts, which is very inconvenient.

[0045] In summary, the bottom prefabricated hole 6 and the top prefabricated hole 7 are prefabricated, and the post-molding opening 8 is opened after the lower adhesive layer 2 and the upper adhesive layer 4 are solidified, which is more conducive to the production and use of the artificial board.

[0046] The aperture of the bottom prefabricated hole 6 is equal to that of the post-molding opening 8 and smaller than that of the top prefabricated hole 7 , and the positioning claws of the four-claw nut 9 are arranged on the wood chip top plate 5 .

[0047] In this embodiment, for example, the diameters of the bottom prefabricated hole 6 and the post-molding opening 8 are 6 mm, and the diameter of the top prefabricated hole 7 is 8 mm. The reasons for the size difference are mainly the following two: First, when the post-forming opening 8 is excavated, the end point of the drill bit a is the bottom prefabricated hole 6, so the rod of the drill bit a will not enter the bottom prefabricated hole 6, and the rod will not cause harmful phenomena such as hole expansion and scratching to the bottom prefabricated hole 6, and the aperture of the bottom prefabricated hole 6 does not need to be larger than the post-forming opening 8; Second, when the post-forming opening 8 is being excavated, the rod of the drill bit a is always located in the top prefabricated hole 7. If the top prefabricated hole 7 and the post-forming opening 8 being opened have the same aperture, the drill bit a itself cannot completely avoid swinging, and is prone to scratching and colliding on the top prefabricated hole 7, which is very disadvantageous for the shavings top plate 5 with relatively low structural strength, and is likely to cause cracks to appear on the shavings top plate 5 starting from the top prefabricated hole 7.

[0048] Correspondingly, when the bottom prefabricated holes 6 and the top prefabricated holes 7 are respectively formed on the shaving bottom plate 1 and the shaving top plate 5, special attention should be paid to selecting a high-quality drill bit with a relatively short length and relatively high rigidity.

[0049] On the other hand, the existing common four-claw nut 9 has a structure composed of a nut body and a positioning claw. The positioning claw is arranged on the shavings top plate 5, so that the four-claw nut 9 can be stably installed. This is also one of the reasons why the thickness of the shavings top plate 5 needs to be relatively large, greater than the shavings bottom plate 1.

[0050] Among them, the central axes of the bottom prefabricated hole 6, the top prefabricated hole 7 and the post-forming opening 8 coincide with each other. When installing, the four-claw nut 9 passes through the top prefabricated hole 7, the post-forming opening 8 and the bottom prefabricated hole 6 in sequence, and the nut body of the four-claw nut 9 does not protrude outside the bottom prefabricated hole 6, so that the artificial board can fully fit the above-mentioned furniture frame board d.

[0051] Finally, the four-claw nut 9 may also be relatively short, and its nut body may not enter the bottom prefabricated hole 6, as long as it is ensured that the four-claw nut 9 can be stably screwed to its corresponding bolt.

[0052] A top coating layer 10 is further provided on the upper surface of the shavings top plate 5 , and a bottom coating layer 11 is further provided on the lower surface of the shavings bottom plate 1 .

[0053] In this embodiment, the materials of the top coating layer 10 and the bottom coating layer 11 can be selected from the following ranges, for example: polylactic acid, surlyn resin, polymethyl methacrylate, and polycarbonate.

[0054] The common characteristics of the above types of resins are: First, the material is transparent, which can protect the particleboard while revealing the wood feel of the particle structure; Second, it is suitable for lamination molding process.

[0055] A coating resin block 12 is also provided between the top prefabricated hole 7 and the four-claw nut 9 and is connected to the top coating layer 10 and is used to reinforce the four-claw nut 9 .

[0056] In this embodiment, the diameter of the top prefabricated hole 7 is larger than the size of the post-molded opening 8, so that an annular gap is formed between the top prefabricated hole 7 and the outer ring surface of the nut body of the four-claw nut 9.

[0057] At this time, the resin material corresponding to the top coating layer 10 is cast into the gap, so that the coating resin block 12 can bond and reinforce the four-claw nut 9, further enhancing the installation stability of the four-claw nut 9 on the main body of the artificial board. It should be noted that most of the commonly used multilayer boards 3 have a relatively high nail holding force and can stably clamp the four-claw nut 9, while the nail holding force performance of various types of particle boards varies.

[0058] Therefore, due to the use of the coated resin block 12, the particleboard top board 5 can be made of various types of particleboards, for example, with relatively poor nail holding force but more outstanding other properties, which can greatly broaden its scope of application, which is very practical.

[0059] Generally, the outer diameter of the nut body of the four-claw nut 9 is within 0.1 mm larger than the aperture of the post-molded opening 8, thereby achieving a sufficient and appropriate interference fit and a stable plug-in effect.

[0060] The thickness of the top coating layer 10 and the bottom coating layer 11 is ≤1.0 mm; the distance between the upper surface of the top coating layer 10 and the upper end surface of the four-claw nut 9 is ≤0.2 mm.

[0061] In this embodiment, when the top coating layer 10 is being formed by coating, a small amount of resin material thereof will enter into the four-claw nut 9 or form a sealing film on the four-claw nut 9 .

[0062] Similarly, when the bottom coating layer 11 is being formed by coating, a small amount of resin material thereof will enter into the four-claw nut 9 , or enter into the bottom prefabricated hole 6 without touching the four-claw nut 9 .

[0063] Therefore, no matter which case, for the bolts adapted by the four-claw nut 9, they need to penetrate the accidental gathering and accumulation of the resin. The bolts can be of pointed type. For specific conditions, please refer to the attached Fig.12 , 13 、14.

[0064] A method for preparing a multi-layer composite artificial board comprises the following steps in sequence: S1, opening the bottom prefabricated hole 6 on the shaving bottom plate 1, and opening the top prefabricated hole 7 on the shaving top plate 5; S2, firstly apply glue on both surfaces of the multilayer board 3, then press the wood chip bottom board 1 and the wood chip top board 5 respectively, and finally solidify to form the lower glue layer 2 and the upper glue layer 4; S3, inserting and then turning on a drill bit a in the top prefabricated hole 7 until the drill bit a penetrates the lower adhesive layer 2, thereby finally forming the post-molding opening 8; S4, insert and install the four-claw nut 9 into the top prefabricated hole 7 until the positioning claws of the four-claw nut 9 are inserted into the shavings top plate 5.

[0065] In S3 of this embodiment, the drill bit a will penetrate the upper adhesive layer 4 and the lower adhesive layer 2 in sequence, and these two resin layers will not cause substantial and significant impact on the drilling operation of the drill bit a.

[0066] After S4, the following steps are sequentially included: S5, spraying transparent coating resin on the upper surface of the shavings top plate 5 and the lower surface of the shavings bottom plate 1 respectively, and finally forming the top coating layer 10 and the bottom coating layer 11.

[0067] In S5 of this embodiment, the top coating layer 10 needs to use a resin with relatively low viscosity and provide sufficient casting time to ensure that the coating resin block 12 is fully filled to form a complete tubular block.

[0068] In S3, the signal that the drill bit a penetrates the lower adhesive layer 2 is that the reaction force on the drill bit suddenly decreases, and at this time, the lower annular edge of the annular surface of the drill bit a coincides with the upper annular edge of the bottom prefabricated hole 6.

[0069] As attached Fig. 9 As shown, this corresponds to the end state of the excavation operation of the drill bit a. Since the thickness and hardness of the lower adhesive layer 2 are relatively small, the time required for its drilling and excavation can be ignored.

[0070] Therefore, the drilling operation can be stopped after the rod of the drill bit a completely passes through the multilayer board 3. The latest stopping time of the drilling operation is when the annular edge a-1 at the lower end of the annular surface abuts against the annular edge 6-1, ensuring that the shavings bottom board 1 will not be rubbed or hit by the drill bit a.

[0071] The embodiments of the present invention are described in detail above in conjunction with the accompanying drawings, but the present invention is not limited to the above embodiments. Various modifications can be made within the knowledge of ordinary technicians in the technical field without departing from the purpose of the present invention. These are all non-creative modifications and are protected by patent law as long as they are within the scope of the claims of the present invention.

Claims

1. A multi-layer composite artificial board, characterized in that: The structure comprises a wood shavings bottom plate (1), a lower glue layer (2), a multilayer board (3), an upper glue layer (4), and a wood shavings top plate (5) which are arranged in sequence from bottom to top.

2. The multi-layer composite artificial board according to claim 1, characterized in that: The thickness of the artificial board is 12.0-14.0 mm, and the thickness of the wood chip top board (5) is greater than that of the wood chip bottom board (1).

3. The multi-layer composite artificial board according to claim 1, characterized in that: The wood chip bottom plate (1) is also provided with a bottom prefabricated hole (6), the wood chip top plate (5) is also provided with a top prefabricated hole (7), the multilayer board (3) is also provided with a post-forming opening (8), and the top prefabricated hole (7) is provided with a four-claw nut (9) for plugging into the post-forming opening (8) and the bottom prefabricated hole (6).

4. The multi-layer composite artificial board according to claim 3, characterized in that: The diameter of the bottom prefabricated hole (6) is equal to that of the post-molding opening (8) and smaller than that of the top prefabricated hole (7), and the positioning claws of the four-claw nut (9) are arranged on the wood chip top plate (5).

5. The multi-layer composite artificial board according to claim 4, characterized in that: A top coating layer (10) is also provided on the upper surface of the shavings top plate (5), and a bottom coating layer (11) is also provided on the lower surface of the shavings bottom plate (1).

6. The multi-layer composite artificial board according to claim 5, characterized in that: A coating resin block (12) is also provided between the top prefabricated hole (7) and the four-claw nut (9) and is connected to the top coating layer (10) and is used to reinforce the four-claw nut (9).

7. The multi-layer composite artificial board according to claim 5, characterized in that: The thickness of the top coating layer (10) and the bottom coating layer (11) is ≤1.0 mm; and the distance between the upper surface of the top coating layer (10) and the upper end surface of the four-claw nut (9) is ≤0.2 mm.

8. The method for preparing a multi-layer composite artificial board according to claim 5, characterized in that The following steps are included in sequence: S1, opening the bottom prefabricated hole (6) on the wood chip bottom plate (1), and opening the top prefabricated hole (7) on the wood chip top plate (5); S2, firstly coating glue on both surfaces of the multilayer board (3), then respectively pressing the wood chip bottom board (1) and the wood chip top board (5), and finally curing them to form the lower glue layer (2) and the upper glue layer (4); S3, inserting and then turning on a drill bit (a) in the top prefabricated hole (7) until the drill bit (a) penetrates the lower adhesive layer (2), thereby finally forming the post-molding opening (8); S4, inserting and installing the four-claw nut (9) into the top prefabricated hole (7) until the positioning claws of the four-claw nut (9) are inserted into the wood chip top plate (5).

9. The method for preparing a multi-layer composite artificial board according to claim 8, characterized in that S4 then includes the following steps in sequence: S5, spraying transparent coating resin on the upper surface of the shavings top plate (5) and the lower surface of the shavings bottom plate (1) respectively, and finally forming the top coating layer (10) and the bottom coating layer (11).

10. The method for preparing a multi-layer composite artificial board according to claim 8, characterized in that: In S3, the signal indicating that the drill bit (a) penetrates the lower adhesive layer (2) is that the reaction force on the drill bit suddenly decreases, and at this time, the lower annular edge of the annular surface of the drill bit (a) coincides with the upper annular edge of the bottom prefabricated hole (6).

Citation Information

Patent Citations

  • Mute flame-retardant door or window and a manufacturing method thereof

    CN109519092A

  • Manufacturing method of heat preservation and decoration integrated plate

    CN114412111A

  • Preparation method of antibacterial enhanced wood shaving veneer plywood

    CN116749287A

  • Sandwich composite board

    CN206426577U

  • Cellular board

    CN212684893U