Preparation method of anti-dazzle acrylic adhesive
Through real-time observation and intermittent monitoring of the fluidity of the adhesive, the problem of difficult to control the thickening process of the adhesive is solved, and the precise viscosity adjustment and optimization of the adhesive is achieved, and the fluidity and adhesion of the adhesive is improved.
Patent Information
- Application Number
- CN202411264848.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-10
- Publication Date
- 2024-11-22
AI Technical Summary
During the adhesive preparation process, the thickening process of the adhesive cannot be visually observed by controlling the stirring progress by controlling the time, resulting in difficulty in viscosity control.
Using real-time observation of the fluidity of the adhesive, adjust the viscosity and add solvent and thickener by sampling every 20 minutes in the first two hours and after sampling every 10 minutes, the monitoring mechanism and cleaning mechanism are used to achieve batch viscosity monitoring. , accurately control the reaction rate.
Accurate control of the viscosity of the adhesive is achieved, ensuring that the adhesive reaches an ideal state, optimizing the fluidity and adhesion of the adhesive, avoiding the generation of bubbles, and improving the use effect.
Smart Images

Figure CN118995088A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of adhesive preparation, in particular to a method for preparing an anti-glare acrylic adhesive. Background Art
[0002] Acrylic adhesives are a type of adhesive with unique properties and a wide range of applications. According to the form and application characteristics of the adhesive, it can be divided into solvent-based, emulsion-based, reactive, pressure-sensitive, instant-drying, anaerobic, photosensitive and hot-melt types. One of the advantages of acrylic adhesives is their high viscosity. They have good adhesion and excellent initial viscosity, and can form sufficiently strong bonding in a short time.
[0003] At the same time, during the preparation of acrylic adhesives, special attention should be paid to the operation time, because most structural adhesives are applied or dispensed by static mixing, and chemical reactions begin to occur after mixing, causing the glue to thicken and solidify. During the preparation of adhesives, only controlling the stirring progress of the adhesive by controlling the time cannot more intuitively observe the thickening process of the adhesive. Summary of the invention
[0004] The invention discloses a method for preparing an anti-glare acrylic adhesive, aiming to solve the technical problem that in the adhesive preparation process, the stirring progress of the adhesive is controlled only by controlling the time, and the thickening process of the adhesive cannot be observed more intuitively.
[0005] In order to achieve the above object, the present invention adopts the following technical solutions:
[0006] A method for preparing an anti-glare acrylic adhesive comprises the following specific steps:
[0007] S1: Raw material preparation;
[0008] S2: placing in a reactor: placing the prepared raw materials in a reactor for mixing, mixing with a cross-linking agent, an auxiliary agent and a solvent, and polymerizing the monomers to form a high molecular polymer;
[0009] S3: Real-time observation of the fluidity of the adhesive: The adhesive is placed in a mixing kettle. During the stirring and mixing process of the adhesive, samples are taken every 20 minutes in the first two hours to observe the viscosity of the adhesive by observing the fluidity of the adhesive. After two hours, samples are taken every 10 minutes to observe the mixed viscosity of the adhesive in the reactor in real time.
[0010] S4: Adjust viscosity: Add solvent and thickener according to the real-time observation results to adjust the viscosity of the polymer;
[0011] S5: filtering the synthesized adhesive and placing it into a container for storage;
[0012] The auxiliary agents in S3 include inhibitors, surfactants, diluents and stabilizers. The inhibitor is a nitro compound, the surfactant is an acrylate active agent, the diluent is an active diluent, and the ratio of the inhibitor, stabilizer and surfactant is 1:3:10:1. The auxiliary agents account for 10%-12% of the acrylic adhesive.
[0013] By adding inhibitors, surfactants and diluents to the additives, only stabilizers are added to general acrylic adhesives, and the viscosity of the adhesive is reduced by diluents. On the basis of general adhesive concentration, the fluidity of the adhesive can be optimized, thereby facilitating the spreading of the adhesive on the surface of the substrate. At the same time, the addition of inhibitors can form a protective film on the surface of the glue to prevent air penetration. The use of auxiliary surfactants optimizes the polarity of the acrylic adhesive. While enhancing the adhesion to the substrate, it also assists with the inhibitor to avoid the formation of bubbles on the glue surface, thereby optimizing the use effect of the glue.
[0014] In a preferred embodiment, the mixing kettle includes a stirring kettle body, a monitoring mechanism arranged on one side of the stirring kettle body, a cleaning mechanism, a flow rate monitor facing the monitoring mechanism and a base frame fixed to the bottom end of the flow rate monitor; the monitoring mechanism includes a second through pipe, a solenoid valve arranged on the second through pipe, a first water pump, a linear observation area arranged on the second through pipe, a recovery tank arranged at the bottom end of the second through pipe, a third through pipe connected to the inner wall of one side of the recovery tank, a second water pump connected to the third through pipe and a back plate arranged between the linear observation area and the third through pipe; the cleaning mechanism includes a second diversion pipe connected to the inner wall of one side of the linear observation area, a high-pressure nozzle connected to the second diversion pipe and a high-pressure water pump connected to the high-pressure nozzle.
[0015] By providing a monitoring mechanism and a cleaning mechanism, during the adhesive preparation process, the first water pump intermittently adsorbs the adhesive in the middle of the stirring tank body, and the adhesive flows into the linear observation area. The falling speed of the adhesive is monitored in real time by a flow rate monitor to analyze and calculate the viscosity of the adhesive. The sample after suction falls into the recovery tank through the second through pipe, and enters the stirring tank body again from the top of the stirring tank body through the second water pump and the third through pipe, thereby avoiding the loss of raw materials. Afterwards, with the flushing of the cleaning mechanism to ensure the clarity of the observation area, intermittent viscosity monitoring can be achieved through the cleaning mechanism and the monitoring mechanism, so that the reaction rate of the adhesive can be accurately controlled to ensure that the adhesive reaches an ideal state.
[0016] In a preferred embodiment, a suction head is provided at the input end of the second through pipe, a support shaft is provided in the stirring kettle body, and upper and lower groups of stirring plates are equidistantly provided on the outer circumference of the support shaft, a gap is provided between the upper and lower groups of stirring plates, and the suction head is provided in the gap, and the bottom end of the suction head is movably fitted on the top end of the stirring plate, a guiding slope is provided at the bottom end of the recovery tank, and a discharge port is provided through one side of the recovery tank, and the discharge port is connected to one end of the third through pipe.
[0017] By providing a suction head, the bottom end of the suction head will be continuously cleaned during the rotation of the stirring plate. Therefore, due to the flow and heating of the colloid in the stirring kettle and the cleaning effect of the stirring plate, it can be ensured that the suction head will not be blocked by the adhesive, thereby ensuring smooth sample transportation.
[0018] In a preferred solution, the second shunt pipe is fixed at the bottom end of the linear observation area in an oblique upward manner, the high-pressure nozzle and the high-pressure water pump are connected by a first through pipe, the other side of the second through pipe is fixedly connected to the first shunt pipe in an oblique downward manner, and the first shunt pipe is located at the top of the linear observation area, a waste storage tank is provided at the bottom end of the first shunt pipe, the outer wall of the second through pipe is fixedly connected to the first support plate, and the first support plate is located below the second shunt pipe, a hydraulic rod is fixedly connected to the first support plate, the bottom end of the second through pipe is movably sleeved with an outer sleeve, and the outer wall of one side of the outer sleeve is fixedly connected with the second support plate, the top of the second support plate is connected to the output end of the hydraulic rod, the top of the recovery tank is movably connected to the waste storage tank, and the two ends of the waste storage tank are respectively fixedly connected to hangers, the hangers are movably clamped at the top of the recovery tank, and one side of one of the hangers is fixedly connected to a slider, one side of the recovery tank is fixedly connected to a linear guide rail, and the slider moves on the linear guide rail.
[0019] A cleaning mechanism is provided. In the cleaning mechanism, when cleaning is carried out inside the tube, the cleaning liquid passes through the linear observation area and is discharged from the first diversion pipe when the solenoid valve is closed. At the beginning of cleaning, the cleaning liquid will also be diverted and flow out to the waste storage tank along the bottom end of the second through tube to clean the tail of the second through tube. As the water level in the waste storage tank rises, the outer sleeve is blocked, thereby suppressing the diversion of the cleaning liquid, thereby ensuring the flow rate of the cleaning liquid in the linear observation area, and further ensuring the overall cleaning effect of the second through tube.
[0020] As can be seen from the above, a method for preparing an anti-glare acrylic adhesive, the mixing kettle includes a stirring kettle body, a monitoring mechanism arranged on one side of the stirring kettle body, a cleaning mechanism, a flow rate monitor facing the monitoring mechanism and a bottom frame fixed to the bottom of the flow rate monitor; the monitoring mechanism includes a second through pipe, a solenoid valve arranged on the second through pipe, a first water pump, a linear observation area arranged on the second through pipe, a recovery tank arranged at the bottom of the second through pipe, a third through pipe connected to the inner wall of one side of the recovery tank, a second water pump connected to the third through pipe and a back plate arranged between the linear observation area and the third through pipe; the cleaning mechanism includes a second shunt pipe connected to the inner wall of one side of the linear observation area, a high-pressure nozzle connected to the second shunt pipe and a high-pressure water pump connected to the high-pressure nozzle. The method for preparing an anti-glare acrylic adhesive provided by the present invention has the technical effect of realizing intermittent viscosity monitoring, accurately controlling the reaction rate of the adhesive, and ensuring that the adhesive reaches an ideal state. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 The present invention provides a schematic diagram of the overall structure of a mixing kettle for preparing an anti-glare acrylic adhesive.
[0022] Figure 2 The present invention provides a schematic diagram of the internal structure of a mixing kettle for preparing an anti-glare acrylic adhesive.
[0023] Figure 3 The present invention provides a schematic diagram of the disassembled structure of a mixing kettle tube body in a method for preparing an anti-glare acrylic adhesive.
[0024] Figure 4 The present invention provides a schematic diagram of a disassembled cleaning mechanism of a mixing kettle portion of a method for preparing an anti-glare acrylic adhesive.
[0025] Figure 5 The present invention provides a specific flow chart of a method for preparing an anti-glare acrylic adhesive.
[0026] In the figure: 1. cleaning mechanism; 2. monitoring mechanism; 3. stirring kettle body; 4. flow rate monitor; 5. bottom frame; 6. support shaft; 7. stirring plate; 101. first diversion pipe; 102. waste storage tank body; 103. waste storage tank; 104. high-pressure water pump; 105. hydraulic rod; 106. first support plate; 107. second diversion pipe; 108. outer sleeve; 109. second support plate; 110. high-pressure nozzle; 111. first through pipe; 112. linear guide rail; 113. bracket; 114. slider; 201. suction head; 202. second through pipe; 203. solenoid valve; 204. first water pump; 205. linear observation area; 206. second water pump; 207. third through pipe; 208. recovery tank; 209. guiding slope; 210. discharge port; 211. back plate. DETAILED DESCRIPTION
[0027] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.
[0028] The invention discloses a method for preparing an anti-glare acrylic adhesive, which is mainly used in the scenario of adhesive preparation.
[0029] Reference Figure 5 , a method for preparing an anti-glare acrylic adhesive, comprising the following specific steps:
[0030] S1: Raw material preparation;
[0031] S2: placing in a reactor: placing the prepared raw materials in a reactor for mixing, mixing with a cross-linking agent, an auxiliary agent and a solvent, and polymerizing the monomers to form a high molecular polymer;
[0032] S3: Real-time observation of the fluidity of the adhesive: The adhesive is placed in a mixing kettle. During the stirring and mixing process of the adhesive, samples are taken every 20 minutes in the first two hours to observe the viscosity of the adhesive by observing the fluidity of the adhesive. After two hours, samples are taken every 10 minutes to observe the mixed viscosity of the adhesive in the reactor in real time.
[0033] S4: Adjust viscosity: Add solvent and thickener according to the real-time observation results to adjust the viscosity of the polymer;
[0034] S5: filtering the synthesized adhesive and placing it into a container for storage;
[0035] The additives in S3 include inhibitors, surfactants, diluents and stabilizers. The inhibitor is a nitro compound, the surfactant is an acrylate active agent, the diluent is an active diluent, and the ratio of the inhibitor, stabilizer and surfactant is 1:3:10:1. The additives account for 10%-12% of the acrylic adhesive. Generally, only stabilizers are added to acrylic adhesives, and the viscosity of the adhesive is reduced by diluents. On the basis of the general adhesive concentration, the fluidity of the adhesive can be optimized, thereby facilitating the laying of the adhesive on the surface of the substrate. At the same time, the addition of inhibitors can form a protective film on the glue surface to prevent air penetration. The use of auxiliary surfactants optimizes the polarity of the acrylic adhesive. While enhancing the adhesion to the substrate, it also assists with the inhibitor to avoid the generation of bubbles on the glue surface, thereby optimizing the use effect of the glue.
[0036] Reference Figure 1-Figure 4 In a preferred embodiment, the mixing kettle comprises a stirring kettle body 3, a monitoring mechanism 2 arranged on one side of the stirring kettle body 3, a cleaning mechanism 1, a flow rate monitor 4 facing the monitoring mechanism 2, and a bottom frame 5 fixed to the bottom end of the flow rate monitor 4;
[0037] The monitoring mechanism 2 includes a second through pipe 202, a solenoid valve 203 disposed on the second through pipe 202, a first water pump 204, a linear observation area 205 disposed on the second through pipe 202, a recovery tank 208 disposed at the bottom end of the second through pipe 202, a third through pipe 207 connected to the inner wall of one side of the recovery tank 208, a second water pump 206 connected to the third through pipe 207, and a back plate 211 disposed between the linear observation area 205 and the third through pipe 207;
[0038] The cleaning mechanism 1 includes a second shunt pipe 107 connected to the inner wall of one side of the linear observation area 205, a high-pressure nozzle 110 connected to the second shunt pipe 107, and a high-pressure water pump 104 connected to the high-pressure nozzle 110. During the adhesive preparation process, the first water pump 204 intermittently adsorbs the adhesive located in the middle of the stirring tank body 3, and flows into the linear observation area 205, and a single background is established through the back plate 211. Then, the falling speed of the adhesive is monitored in real time by the flow rate monitor 4 to analyze and calculate the viscosity of the adhesive, and the sample after suction It falls into the recovery tank 208 through the second through pipe 202, and enters the stirring tank body 3 again from the top of the stirring tank body 3 through the second water pump 206 and the third through pipe 207, thereby avoiding the loss of raw materials. Later, in the cleaning mechanism 1, the high-pressure water pump 104 sucks the cleaning liquid and sprays it into the second through pipe 202 through the high-pressure nozzle 110, so that the second through pipe 202 can be automatically cleaned in the intermittent process. Therefore, intermittent viscosity monitoring can be achieved through the cleaning mechanism 1 and the monitoring mechanism 2, so that the reaction rate of the adhesive can be accurately controlled to ensure that the adhesive reaches an ideal state.
[0039] Reference Figure 2 In a preferred embodiment, a suction head 201 is provided at the input end of the second through-tube 202, a support shaft 6 is provided in the stirring kettle body 3, and upper and lower groups of stirring plates 7 are equidistantly provided on the outer circumference of the support shaft 6, a gap is provided between the upper and lower groups of stirring plates 7, and the suction head 201 is provided in the gap, and the bottom end of the suction head 201 is movably fitted to the top end of the stirring plate 7, and the suction end diameter of the second through-tube 202 is enlarged by the suction head 201, and based on the bottom end of the suction head 201 being fitted to the top end of the stirring plate 7, the bottom end of the suction head 201 is continuously cleaned during the rotation of the stirring plate 7, thereby, under the flow and heating of the colloid in the stirring kettle body 3 and the cleaning action of the stirring plate 7, it can be ensured that the suction head 201 will not be blocked by the adhesive, thereby ensuring smooth sample transportation.
[0040] Reference Figure 4 In a preferred embodiment, a guiding slope 209 is provided at the bottom end of the recovery groove 208 , and a discharge port 210 is provided through one side of the recovery groove 208 , and the discharge port 210 is connected to one end of the third through pipe 207 .
[0041] Reference Figure 3 In a preferred embodiment, the second diverter pipe 107 is fixed obliquely upward at the bottom end of the linear observation area 205, the high-pressure nozzle 110 and the high-pressure water pump 104 are connected via a first through pipe 111, and the other side of the second through pipe 202 is fixedly connected obliquely downward with the first diverter pipe 101, and the first diverter pipe 101 is located at the top of the linear observation area 205.
[0042] Reference Figure 3 In a preferred embodiment, a waste storage tank 102 is provided at the bottom end of the first diversion pipe 101, a first support plate 106 is fixedly connected to the outer wall of the second through pipe 202, and the first support plate 106 is located below the second diversion pipe 107, and a hydraulic rod 105 is fixedly connected to the first support plate 106.
[0043] Reference Figure 3 In a preferred embodiment, the bottom end of the second through pipe 202 is movably connected to the outer sleeve 108, and the outer wall of one side of the outer sleeve 108 is fixedly connected to the second support plate 109, and the top end of the second support plate 109 is connected to the output end of the hydraulic rod 105.
[0044] Reference Figure 4In a preferred embodiment, the top of the recovery tank 208 is movably connected to the waste storage tank 103, and the two ends of the waste storage tank 103 are respectively fixedly connected to the hangers 113, the hangers 113 are movably connected to the top of the recovery tank 208, and one side of one of the hangers 113 is fixedly connected to a slider 114, one side of the recovery tank 208 is fixedly connected to a linear guide 112, and the slider 114 moves on the linear guide 112. In the cleaning mechanism 1, before the high-pressure nozzle 110 sprays the cleaning liquid into the second diverter pipe 107, the slider 114 moves on the linear guide 112 to drive the waste storage tank 103 to move to the bottom end of the second through pipe 202, and under the action of the hydraulic rod 105, the outer sleeve is driven 108 moves downward along the outer wall of the second through tube 202, extends the length of the second through tube 202, and extends into the waste storage tank 103. Therefore, when cleaning the tube, the cleaning liquid passes through the linear observation area 205 and is discharged from the first diversion tube 101 when the solenoid valve 203 is closed. At the beginning of cleaning, the cleaning liquid will also be diverted and flow out to the waste storage tank 103 along the bottom end of the second through tube 202 to clean the tail of the second through tube 202. As the water level of the waste storage tank 103 rises, the outer sleeve 108 is blocked, thereby suppressing the diversion of the cleaning liquid, thereby ensuring the flow rate of the cleaning liquid in the linear observation area 205, and further ensuring the overall cleaning effect of the second through tube 202.
[0045] Working principle: During the adhesive preparation process, the adhesive located in the middle of the stirring tank body 3 is intermittently adsorbed by the first water pump 204, and flows into the linear observation area 205, and a single background is established through the back plate 211. Then, the falling speed of the adhesive is monitored in real time by the flow rate monitor 4 to analyze and calculate the viscosity of the adhesive. The sample after suction falls into the recovery tank 208 through the second through pipe 202, and enters the stirring tank body 3 again from the top of the stirring tank body 3 through the second water pump 206 and the third through pipe 207, thereby avoiding the loss of raw materials. Then, in the cleaning mechanism 1, the high-pressure water pump 104 sucks the cleaning liquid and sprays it into the second through pipe 202 by the high-pressure nozzle 110, so that the second through pipe 202 can be automatically cleaned in the intermittent process. Therefore, intermittent viscosity monitoring can be realized through the cleaning mechanism 1 and the monitoring mechanism 2, so that the reaction rate of the adhesive can be accurately controlled to ensure that the adhesive reaches an ideal state. At the same time, in the cleaning mechanism 1, Before the high-pressure nozzle 110 sprays the cleaning liquid into the second shunt pipe 107, the slider 114 moves on the linear guide rail 112 to drive the waste storage tank 103 to move to the bottom end of the second through pipe 202, and under the action of the hydraulic rod 105, the outer sleeve 108 is driven to move downward along the outer wall of the second through pipe 202, extending the length of the second through pipe 202 and extending it into the waste storage tank 103. Therefore, when cleaning the inside of the pipe, the cleaning liquid is closed when the solenoid valve 203 is closed. The cleaning liquid passes through the linear observation area 205 and is discharged from the first diversion pipe 101. When cleaning just starts, the cleaning liquid will also be diverted and flow out along the bottom end of the second through pipe 202 to the waste storage tank 103 to clean the tail of the second through pipe 202. As the water level of the waste storage tank 103 rises, the outer sleeve 108 is blocked, thereby suppressing the diversion of the cleaning liquid, thereby ensuring the flow rate of the cleaning liquid in the linear observation area 205, and further ensuring the overall cleaning effect of the second through pipe 202.
[0046] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A method for preparing an anti-glare acrylic adhesive, characterized in that: The specific steps include: S1: Raw material preparation; S2: placing in a reactor: placing the prepared raw materials in a reactor for mixing, mixing with a cross-linking agent, an auxiliary agent and a solvent, and polymerizing the monomers to form a high molecular polymer; S3: Real-time observation of the fluidity of the adhesive: The adhesive is placed in a mixing kettle. During the stirring and mixing process of the adhesive, samples are taken every 20 minutes in the first two hours to observe the viscosity of the adhesive by observing the fluidity of the adhesive. After two hours, samples are taken every 10 minutes to observe the mixed viscosity of the adhesive in the reactor in real time. S4: Adjust viscosity: Add solvent and thickener according to the real-time observation results to adjust the viscosity of the polymer; S5: filtering the synthesized adhesive and placing it in a container for storage; The auxiliary agents in S3 include inhibitors, surfactants, diluents and stabilizers. The inhibitor is a nitro compound, the surfactant is an acrylate active agent, the diluent is an active diluent, and the ratio of the inhibitor, stabilizer and surfactant is 1:3:10:
1. The auxiliary agents account for 10%-12% of the acrylic adhesive.
2. The method for preparing an anti-glare acrylic adhesive according to claim 2, characterized in that: The mixing kettle comprises a stirring kettle body (3), a monitoring mechanism (2) arranged on one side of the stirring kettle body (3), a cleaning mechanism (1), a flow rate monitor (4) facing the monitoring mechanism (2), and a bottom frame (5) fixed to the bottom end of the flow rate monitor (4); The monitoring mechanism (2) comprises a second through pipe (202), a solenoid valve (203) arranged on the second through pipe (202), a first water pump (204), a linear observation area (205) arranged on the second through pipe (202), a recovery tank (208) arranged at the bottom end of the second through pipe (202), a third through pipe (207) connected to an inner wall of one side of the recovery tank (208), a second water pump (206) connected to the third through pipe (207), and a back plate (211) arranged between the linear observation area (205) and the third through pipe (207); The cleaning mechanism (1) comprises a second shunt pipe (107) connected to an inner wall of one side of the linear observation area (205), a high-pressure nozzle (110) connected to the inside of the second shunt pipe (107), and a high-pressure water pump (104) connected to the high-pressure nozzle (110).
3. The method for preparing an anti-glare acrylic adhesive according to claim 2, characterized in that: A suction head (201) is provided at the input end of the second through pipe (202), a support shaft (6) is provided in the stirring kettle body (3), and upper and lower groups of stirring plates (7) are equidistantly provided on the outer circumference of the support shaft (6), a gap is provided between the upper and lower groups of stirring plates (7), and the suction head (201) is provided in the gap, and the bottom end of the suction head (201) is movably fitted to the top end of the stirring plate (7).
4. The method for preparing an anti-glare acrylic adhesive according to claim 2, characterized in that: A guiding slope (209) is provided at the bottom end of the recovery groove (208), and a discharge port (210) is provided through one side of the recovery groove (208), and the discharge port (210) is connected to one end of the third through pipe (207).
5. The method for preparing an anti-glare acrylic adhesive according to claim 2, characterized in that: The second shunt pipe (107) is fixed at the bottom end of the linear observation area (205) in an oblique upward direction, the high-pressure nozzle (110) and the high-pressure water pump (104) are connected via a first through pipe (111), and the other side of the second through pipe (202) is fixedly connected to the first shunt pipe (101) in an oblique downward direction, and the first shunt pipe (101) is located at the top end of the linear observation area (205).
6. The method for preparing an anti-glare acrylic adhesive according to claim 5, characterized in that: A waste storage tank (102) is provided at the bottom end of the first diversion pipe (101), a first support plate (106) is fixedly connected to the outer wall of the second through pipe (202), and the first support plate (106) is located below the second diversion pipe (107), and a hydraulic rod (105) is fixedly connected to the first support plate (106).
7. The method for preparing an anti-glare acrylic adhesive according to claim 6, characterized in that: The bottom end of the second through pipe (202) is movably sleeved with an outer sleeve (108), and a second support plate (109) is fixedly connected to an outer wall of one side of the outer sleeve (108), and the top end of the second support plate (109) is connected to the output end of the hydraulic rod (105).
8. The method for preparing an anti-glare acrylic adhesive according to claim 7, characterized in that: The top of the recovery trough (208) is movably connected to a waste storage trough (103), and both ends of the waste storage trough (103) are respectively fixedly connected to hanging brackets (113), the hanging brackets (113) are movably connected to the top of the recovery trough (208), and one side of one of the hanging brackets (113) is fixedly connected to a sliding block (114), and one side of the recovery trough (208) is fixedly connected to a linear guide rail (112), and the sliding block (114) moves on the linear guide rail (112).