Reduced charging by low negative voltage in FIB systems
By applying a negative bias voltage to the conductive structure when milling non-conductive materials in focus ion beams, repelling secondary electrons back to the sample surface, the problem of positive charge formation in the milling area is solved and the stability and accuracy of the milling process are improved.
Patent Information
- Application Number
- CN202380034348.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-20
- Filing Date
- 2023-04-11
- Publication Date
- 2024-11-22
AI Technical Summary
When milling non-conductive materials in focus ion beam (FIB), adverse positive charges are easily formed, affecting the milling process.
By placing the sample in a vacuum chamber, scanning with a focused ion beam and applying a negative bias to the conductive structure close to the milling area, the trajectory of the secondary electrons is changed and repelled back to the sample surface, thereby maintaining the neutral charge in the milling area. The conductive structure can be a gas injection nozzle, a voltage pin or a nanooperator positioned between 5 microns and 1.5 mm from the milling area.
Effectively reduce or prevent positive charge formation in the milling area, improve the stability and accuracy of the milling process, and is especially suitable for milling of non-conductive materials.
Smart Images

Figure CN119013758A_ABST
Abstract
Description
Technical Field
[0001] This application claims the benefit of U.S. Patent Application No. 17 / 725,023, filed on April 20, 2022, the entire disclosure of which is incorporated herein by reference for all purposes. Background Art
[0002] In the study of electronic materials and processes for fabricating such materials into electronic structures, samples of electronic structures may be used for microscopic examination for the purposes of failure analysis and device verification. For example, a sample such as a silicon wafer including one or more integrated circuits (ICs) or other electronic structures formed on the one or more ICs may be milled and imaged with a focused ion beam (FIB) to study specific characteristics of the circuits or other structures formed on the wafer.
[0003] As an example, a FIB can be used to mill holes or grooves in one or more layers formed on a sample. During this milling process, ions bombard the sample to trigger a series of events that can generate free electrons that escape from the sample surface. When the milled material is a conductive layer, electrons from within the sample can quickly replace the escaping electrons, thereby maintaining a relatively neutral charge in the milled area. However, when the milled material is a non-conductive (i.e., electrically insulating) layer, electrons do not move freely through the material. Therefore, electrons that escape or are otherwise released from the milled area during the milling process of non-semiconductor materials may not be replaced, and the milled area may form a positive charge that may adversely affect the milling process.
[0004] Therefore, there is a need for improved techniques for milling non-conductive materials. Summary of the invention
[0005] Embodiments disclosed herein provide improved techniques and processes to mill areas on a sample to reduce or prevent the formation of positive charges in the milled area, even when the milled material is non-conductive.
[0006] In some embodiments, a method for processing an area of a sample comprises: positioning the sample within a vacuum chamber; generating an ion beam using a focused ion beam (FIB) column; focusing the ion beam on the sample and scanning the focused ion beam across the sample area, thereby generating secondary electrons emitted from the sample surface within the area; and during the scan, applying a negative bias to a conductive structure near the area to change the trajectory of the secondary electrons and repel the secondary electrons back to the sample surface, wherein the conductive structure is one of a gas injection nozzle, a voltage pin, or a nanomanipulator.
[0007] Various implementations of the embodiments described herein may include one or more of the following features. During the milling process, the conductive structure may be positioned at a distance of five millimeters or less from the region. The conductive structure may include a gas injection nozzle located between a column cap of the FIB column and the sample. The gas injection nozzle may be heated when a negative bias is applied to the gas injection nozzle. During scanning, the first end of the gas injection nozzle may be positioned adjacent to the region, and the second end of the gas injection nozzle may extend through a conductive wall of a component of the vacuum chamber and be electrically insulated but thermally coupled to the wall. The conductive structure may include a voltage pin that is operable to move within 100 microns of the region. The sample may include a non-conductive layer formed on an upper surface of the sample, and the focusing step may scan the focused ion beam across the sample region, thereby milling a portion of the non-conductive layer. The sample may include a semiconductor substrate and during scanning, the conductive structure may be between 5 microns and 1.5 millimeters away from the region.
[0008] Some embodiments relate to a non-transitory computer medium storing instructions that, when executed by one or more processors, cause the processors to: position a sample within a vacuum chamber; generate an ion beam using a focused ion beam (FIB) column; focus the ion beam on the sample and scan the focused ion beam across an area of the sample, thereby generating secondary electrons that are ejected from a surface of the sample within the area; and during the scan, apply a negative bias to a conductive structure proximate the area to change the trajectory of the secondary electrons and repel the secondary electrons back to the sample surface, wherein the conductive structure is one of a gas injection nozzle, a voltage pin, or a nanomanipulator.
[0009] Some embodiments relate to a system for milling a sample region according to any of the methods described above or herein. For example, the system may include: a vacuum chamber; a sample support configured to hold a sample within the vacuum chamber during a processing operation; a focused ion beam (FIB) column configured to direct an ion beam into the vacuum chamber toward the sample region during a processing operation; a conductive structure movable to a position such that when the sample is located on the sample support, the conductive structure is adjacent to the sample region, wherein the conductive structure is one of a gas injection nozzle, a voltage pin, or a nanomanipulator; and a voltage source operable to apply a negative bias to the conductive structure.
[0010] In order to better understand the nature and advantages of the present invention, reference should be made to the following description and drawings. However, it should be understood that each of the drawings is provided for illustrative purposes only and is not intended as a definition of the limitations of the scope of the present invention. In addition, as a general rule, and unless otherwise apparent from the description, where the same reference numerals are used for elements in different drawings, the elements are generally the same or at least similar in function or use. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 A simplified diagram of a sample focused ion beam (FIB) evaluation system according to some embodiments of the present invention;
[0012] Figure 2 and Figure 3 is a simplified illustration of a portion of a previously known charged ion column;
[0013] Figure 4 A simplified diagram of a sample focused ion beam (FIB) evaluation system according to some embodiments of the present invention;
[0014] Figure 5 A simplified flow chart illustrating the steps associated with a method of milling a sample according to some embodiments;
[0015] Fig. 6A is a simplified illustration of a portion of a FIB column and a gas nozzle according to some embodiments;
[0016] Figure 6B To simplify the plan view, the figure illustrates Fig. 6A The gas injection nozzle shown in FIG. is located above a portion of a sample being milled;
[0017] Figure 6C is a simplified illustration of a gas injection nozzle positioned above a sample being milled according to some embodiments;
[0018] Figure 7 is a simplified diagram of a gas nozzle connection system according to some embodiments;
[0019] Fig. 8A is a simplified diagram of a sample focused ion beam (FIB) evaluation system according to some embodiments;
[0020] Figure 8B is a simplified diagram of a sample focused ion beam (FIB) evaluation system according to some embodiments;
[0021] Figure 8C is a simplified diagram of a sample focused ion beam (FIB) evaluation system according to some embodiments; and
[0022] Fig. 9 is a simplified illustration of areas on a semiconductor wafer where one or more areas may be milled according to some embodiments. DETAILED DESCRIPTION
[0023] Embodiments disclosed herein provide improved techniques and processes for milling areas on a sample to reduce or prevent the formation of positive charges in the milled area, even when the milled material is non-conductive.
[0024] Exemplary Focused Ion Beam (FIB) Evaluation Tools
[0025] In order to better understand and comprehend this case, first refer to Figure 1 , which is a simplified schematic diagram of a focused ion beam (FIB) evaluation system 100 according to some embodiments of the present invention. Figure 1 As shown in , system 100 may include, among other elements, a focused ion beam (FIB) column, a sample support element 140, and a secondary electron detector 150 (or in some embodiments, a secondary ion detector or a combination of two detectors operating in parallel). FIB column 110 is operable to generate a charged particle beam 120 and direct the particle beam toward a sample 130 (sometimes referred to herein as an "object" or "sample") to mill or otherwise process the sample. The sample (e.g., a semiconductor wafer) may be supported on support element 140 within vacuum chamber 105.
[0026] The FIB column 110 can mill (e.g., drill grooves in the sample 130) the sample 130 to form a cross section by irradiating the sample with a charged particle beam 120, and can also smooth the cross section (if necessary). The FIB milling process typically operates by positioning the sample in a vacuum environment and emitting a focused ion beam toward the sample to etch or mill away material on the sample. In some cases, the vacuum environment can be purged by a background gas of controllable concentration, which is used to help control the etching rate and quality or to help control the deposition of substances. The accelerated ions can be generated by xenon, gallium, or other suitable elements, and are typically accelerated toward the sample by a voltage in the range of 500 volts to 100,000 volts, and more typically falling in the range of 3,000 volts to 30,000 volts. The beam current is typically in the range of from a few picoamps to a few microamps depending on the FIB instrument configuration and application, and the pressure is typically controlled at 10 -10 Up to 10 -5 Between millibars.
[0027] The milling process can be accomplished by, for example, (1) locating a location of interest that should be milled so as to remove a portion of material (e.g., a portion of one or more layers) from the sample, (2) moving the sample (e.g., via mechanical support element 140) so that the sample is located below the field of view of the FIB unit, and (3) milling the sample to remove a desired amount of material in the location of interest. The milling process can include forming grooves (typically with lateral dimensions of a few microns to several hundred microns) in the sample.
[0028] The milling process typically involves scanning a charged particle beam back and forth (e.g., in a raster or other scan pattern) over a particular area of the sample being imaged or milled. One or more lenses (not shown) coupled to the charged particle column may implement a scan pattern as known to those skilled in the art. The scanned area is typically a very small portion of the overall area of the sample. For example, the sample may be a semiconductor wafer having a diameter of 150 mm, 200 mm, or 300 mm, and each area scanned on the wafer (i.e., the milled area) may be a rectangular area having a width and / or length measured in microns or tens of microns. Each iteration (or frame) that the ion beam is scanned over the milled area is typically measured in microseconds and removes a very small amount of material (e.g., as low as 0.01 atomic layers using a low-i probe (e.g., 10 pA) or as many as 1000 atomic layers using a high-i probe (e.g., 1000 nA)) so that the scan pattern is repeated thousands or even millions of times to etch the hole to the desired depth.
[0029] During the milling operation, a charged particle beam 120 generated by the FIB column 110 propagates through a vacuum environment formed within the vacuum chamber 105 before striking the sample 130. The milling process produces byproducts such as molecules, atoms, and ions of the milled material and secondary electrons. For example, when ions strike the sample surface at a relatively high energy level, the ions may begin a collision cascade that transfers momentum and energy from the ions to the sample until the ions stop and implant. The momentum and energy transfer during the collision cascade can result in the dislocation of atoms, the ionization of atoms, and the generation of phonons (heat). The cascade can reach the sample surface, causing atoms with sufficient momentum and energy to be sputtered to escape the solid sample, and producing secondary ions and electrons as a combination of ionization and sputtering that also escape the sample surface. Secondary ions or secondary electrons (at Figure 1 The secondary ions / electrons 125 (illustrated in FIG. 1 ) may be detected by a suitable detector 150. The detected secondary ions or secondary electrons may then be used to analyze the properties of the milled layers and structures.
[0030] Although not in Figure 1As shown in , the FIB evaluation system 100 may include several additional components, including but not limited to one or more gas nozzles for delivering process gases to the chamber 105, vacuum valves and other valves for controlling the pressure within the chamber 105, and one or more lenses for directing the charged particle beam, among other components. The system 100 may also include one or more controllers, processors, or other hardware units, each of which can control the operation of the system 100 by executing computer instructions stored in one or more computer-readable memories, as will be known to those skilled in the art. For example, the computer-readable memory may include solid-state memory (such as random access memory (RAM) and / or read-only memory (ROM), which may be programmable, flash-updatable, and / or the like), a disk drive, an optical storage device, or a similar non-transitory computer-readable storage medium.
[0031] Accumulation of positive charges on the sample
[0032] As described above, when a sample is bombarded with an ion beam during a focused ion beam (FIB) milling process, secondary electrons can be generated that escape from the sample. Figure 2 , which is a simplified schematic diagram of a portion of a FIB column 200 spaced apart from a sample 230. The FIB column 200 may represent Figure 1 For ease of illustration, the FIB column 120 is shown in FIG. Figure 2 Only selected elements of the FIB column 200 are illustrated in FIG. As shown, the FIB column 200 includes a column cap 210 at a distal end of the column.
[0033] During the milling operation, the FIB column 200 generates an ion beam 220 and directs an electron beam so that the electron beam strikes a sample 230. The interaction of the ion beam with the sample 230 generates various secondary electrons, some of which are ejected from the sample, as shown by secondary electrons 240. When the layer being milled within the sample 230 is a non-conductive layer, the ejected secondary electrons are not easily replaced by other electrons within the sample 230. Therefore, a positive charge may be established within a region 250 of the milled sample. As described above, the positive charge may adversely affect the ion beam 220 by, for example, causing the ion beam to deviate from its intended trajectory.
[0034] In some known sample evaluation systems, a negative voltage may be applied to the charged particle column to repel secondary electrons back into the sample and maintain a neutral charge on the sample surface. Figure 3is a simplified schematic diagram of a portion of a charged particle column 300 spaced apart from a sample 330. The charged particle column 300 may include the same or similar components as column 200, and is shown as producing a charged particle beam 320 that is directed through an opening in a column cap 310 toward a sample 330. During a processing operation in which the charged particle beam is directed to impact the sample 330, a negative voltage may be applied to the column cap 310 that is sufficient to repel ejected secondary electrons 340 back toward the sample 330. In this way, the charged particle column 300 may avoid the formation of a strong positive charge on the surface of the sample 330.
[0035] However, in practice, the cap 310 and the detector (e.g., secondary electron detector) are each spaced apart from the upper surface of the sample 330 by a distance X1 of several millimeters or more. For example, in a typical milling operation, the cap 310 may be spaced apart from the sample surface by about 10 to 15 mm, and the secondary electron detector may be spaced apart from one side of the milling area by a similar distance. Figure 3 As shown in , even if a negative voltage is applied to the column cap 310, the relatively large spacing (in the millimeter range) between the column cap 310 and the sample can cause the repelled secondary electrons 340 to return to the sample 330 in a region having a radius of about Y1, which can be several millimeters or more from the region where the ion beam strikes the sample 330. When the ion beam is directed toward the sample with micron-level precision, the repelled electrons may not be able to offset the accumulation of positive charge near the ion beam, which can still produce undesirable effects during the milling process. Additionally, in order to effectively repel electrons from this distance, a relatively strong potential is required, which can interfere with the optical properties of the primary ion beam emitted from the column.
[0036] Applying negative voltage to structures very close to the milling area
[0037] According to some embodiments disclosed herein, a negative bias may be applied to a conductive structure in close proximity to the milled region to repel secondary electrons back to the sample surface in the same general region from which they were ejected from the sample. As used herein, "close proximity" refers to a distance between about 5 microns and less than 5 millimeters. And, in various embodiments, a negative bias is applied to a conductive structure that is 2 millimeters or less from the milled region, between 5 microns and 1.5 millimeters from the milled region, and / or 5 microns to 700 microns from the milled region, which is substantially at least several times closer to the milled region than the column cap (and in many cases a full order of magnitude or closer).
[0038] As described below, in some embodiments, the conductive structure may be one or more of a gas injection nozzle, a voltage pin, a nanomanipulator, and / or any suitable conductive structure that can be positioned very close to the milling region (as defined above) without interfering with the ion beam while a negative bias is applied to the conductive structure.
[0039] 1. Gas injection nozzle
[0040] Reference Figure 4 , Figure 4 4 is a simplified diagram of a focused ion beam (FIB) evaluation system 400 according to some embodiments. System 400 can be similar to system 100 and include a FIB column 410 that can direct an ion beam 420 toward a sample 430 positioned on a sample support 440. System 400 can also include a secondary electron or ion detector 450 that detects secondary electrons or ions 425 generated during a milling operation.
[0041] The FIB evaluation system 400 further includes a gas injection nozzle 460 positioned between the distal end of the FIB column 410 and the sample 430. In some embodiments, the gas injection nozzle 460 can be in a fixed relationship relative to the FIB column 410 in the X-plane and the Y-plane, and can be moved in the Z-plane to allow the nozzle to be very close to the upper surface of the sample 430 (e.g., in some embodiments, close to 300 microns). In some embodiments, the gas injection nozzle 460 may include a hole or channel formed through the gas injection nozzle that allows the ion beam 420 to pass through the gas injection nozzle and collide with the sample 430 at a position directly below the nozzle, as described below with respect to FIG. 6A to FIG. 6C Discussed.
[0042] However, in discussing FIG. 6A to FIG. 6C Before, yes Figure 5 For reference, Figure 5 4 is a simplified flow chart illustrating steps associated with a method 500 of milling a sample according to some embodiments. The method 500 begins by positioning a sample (such as a semiconductor wafer having a non-conductive layer formed on the semiconductor wafer) within a processing chamber of a sample evaluation system (step 410). The processing chamber, which may be, for example, chamber 405, may include a focused ion beam (FIB) column, such as FIB column 410, and a gas injection nozzle, such as nozzle 460. Step 510 may include positioning the sample on a sample support, such as support 440, within a vacuum chamber.
[0043] Next, a negative bias is applied to the gas injection nozzle (step 520) and the FIB column can be activated to generate an ion beam (step 530), which is focused and scanned across the region of interest on the sample (step 540). The ion beam can be passed through a focusing lens ( Figure 4 ) and may be focused and scanned across an area of the substrate ( Figure 4 (not shown in the figure).
[0044] As the ion beam is scanned across the region of interest, a negative bias is applied to the gas injection nozzle. The negative bias should be high enough to repel secondary electrons escaping from the sample surface back into the sample, but the negative bias should not be so high as to affect the trajectory of the ion beam 420, which would adversely affect the milling process. When a negative bias is applied to the gas injection nozzle, and as the ion beam is scanned across the region of interest, secondary electrons ejected from the sample are repelled back into the sample, thereby maintaining a relatively neutral charge in the milling region. Therefore, despite Figure 5 Steps 520 through 550 are described as separate sequential steps, but in practice, steps 520 through 550 may occur simultaneously with one another.
[0045] In some embodiments, the negative bias voltage may be the minimum voltage required to repel a predetermined percentage of secondary electrons. The appropriate value of the negative bias voltage will depend in part on the geometry of the gas injection nozzle, the spacing from the nozzle to the sample, and the predetermined percentage of secondary electrons that will be repelled back into the sample. Therefore, the appropriate negative bias voltage can be determined by simulation or experiment as can be easily determined by a person skilled in the art. In some embodiments, the bias voltage may be between negative 50 volts and negative 1000 volts; and in other embodiments, the bias voltage may be between negative 100 volts and negative 500 volts.
[0046] Although Figure 5 One method is discussed in conjunction with the milling operation of the non-conductive layer, but it should be understood that in other embodiments. Figure 5 Embodiments in which a negative voltage is applied to a gas injection nozzle are discussed, but it will be appreciated that the same or similar techniques may be used in conjunction with other conductive structures described herein for such purposes, including voltage pins, nanomanipulators, and the like.
[0047] Reference Fig. 6A , Fig. 6A for Figure 4 A simplified diagram of the gas injection nozzle 460 is shown in FIG. Figure 6B4 is a simplified plan view illustration of a portion of the gas injection nozzle 460. As shown, the gas injection nozzle 460 includes a channel 615 that extends through the nozzle 460 from the upper surface of the nozzle 460 to the lower surface of the nozzle. The channel 615 can have a circular cross-section and can be centered on the ion beam 420 so that the ion beam strikes the sample 430 (e.g., Figure 6B The gas flows through the channel 615 of the gas injection nozzle 460 before passing through the area 675 shown in FIG. 4 . The nozzle 460 also includes an opening 620 adjacent to the upper surface of the sample 430 at the bottom surface of the nozzle. The gas flowing through the nozzle 460 can be distributed to the surface of the sample 430 via the opening 620. Figure 6B As shown in , the opening 620 can also have a circular cross-section, can surround the channel 615, and can symmetrically surround the area 675 on the sample 430 where the ion beam 420 contacts and mills the sample. In this way, the gas delivered by the nozzle 460 can be delivered directly to the area 675 of the sample 430 being milled.
[0048] like Figure 4 and Fig. 6A , the gas injection nozzle 460 is closer to the sample 430 than the column tip 610 or the secondary ion detector (not shown). For example, the nozzle 460 can be an order of magnitude or more closer to the area on the upper surface of the milled sample 430 than the closest portion of the focused ion beam column to be milled.
[0049] In previously known systems, the substrate support 440 and the gas nozzle 460 are typically electrically grounded. However, some embodiments disclosed herein apply a negative voltage to the gas injection nozzle 460 in a manner similar to that discussed above with respect to the column tip 310 ( Figure 3 ) to repel the secondary electrons generated by the milling operation back into the sample. For illustration, refer to Figure 6C , Figure 6C is a simplified illustration of a portion of a gas injection nozzle 460 positioned above a milled sample 430. Because the gas nozzle 460 is closer to the milling region than the column tip 310 (or column tip 610), applying an appropriate negative voltage level to the gas nozzle 460 will repel the secondary electrons 640 back to a region of the sample having a much smaller radius, and therefore closer to the milling region than the secondary electrons repelled back to the sample 330 by the column tip 310. In some embodiments, the lower surface of the nozzle 460 may be spaced apart from the upper surface of the sample 430 by a distance X2 measured in tens or hundreds of microns. As a non-limiting example, in some milling operations, the lower surface of the nozzle 460 may be spaced apart from the sample surface by approximately 200 to 700 microns.
[0050] like Figure 6BThe design of the gas nozzle 460 shown completely and symmetrically surrounding the milling area, and the very close spacing (in the micron range) between the gas nozzle 460 and the sample can result in the repelled secondary electrons 640 returning to the sample 430 in a region centered on the milling area and having a radius of about Y2 measured in tens of microns rather than millimeters (and thus at least one order of magnitude or two orders of magnitude or more smaller than Y1). Thus, the secondary electrons can be repelled back to an area on the sample that is in the same general vicinity (measured in microns) as the milled area, thus allowing the milled area to maintain a neutral charge even when the milled material is non-conductive.
[0051] 2. Electrically isolate the gas injection nozzle
[0052] In order to charge the gas nozzle 460 with a negative voltage, the nozzle needs to be electrically isolated from the rest of the system 400 which is grounded. Figure 7 is a simplified diagram of a gas nozzle connection system 700 that can electrically decouple a gas nozzle from the rest of the system 400 according to some embodiments. As shown, the nozzle connection system 700 can charge a gas injection nozzle 710, which can represent a gas injection nozzle 460, with its own electrical potential by providing a negative voltage to the gas nozzle 710. Figure 7 , the gas nozzle 710 includes an end 712 that can extend through a wall 720. The gas nozzle 710 and the wall 720 can be made of a conductive material such as a metal. In some embodiments, the wall 720 can be a wall of a vacuum chamber (e.g., chamber 105 or 405) of a FIB evaluation system (such as system 100 or 400). In other embodiments, the wall 720 can be a wall of a gas box that includes various valves and conduits (not shown) to control the flow of one or more gases into the gas nozzle 710, wherein the gas box is positioned within the vacuum chamber (e.g., chamber 105 or 405). In either case, the gas can be delivered through the nozzle 710 pipeline in the direction indicated by arrow 715, and the wall 720 can be electrically grounded.
[0053] An insulated feed line 730 may extend through the wall 720 and be electrically coupled to a thermally conductive electrode 740. When a voltage is applied to the feed line 730, the electrode 740 transmits the applied voltage to the gas nozzle.
[0054] For some applications, it is important to heat the nozzle 460 to avoid material deposition from the gas flowing through the nozzle, which could interfere with gas flow to the milling area or completely block the nozzle. To this end, the gas nozzle 460 can be electrically isolated from the chamber wall and / or other components within the chamber via an electrically insulating but thermally conductive O-ring 750 or similar structure (e.g., an electrically insulating thermally conductive paste). A heater element (not shown) is operably connected to the wall 720 and the gas nozzle 710 to heat both the wall and the nozzle to a sufficient temperature to prevent or otherwise reduce deposition within the gas nozzle. The electrically insulating but thermally conductive O-ring 750 allows heat to be transferred between the two components while allowing the electrical potential of the gas nozzle 710 to be decoupled from the electrical potential of the wall 720.
[0055] 3. Voltage pin / nano-manipulator
[0056] In some embodiments, in addition to or in lieu of applying a negative voltage to a gas injection nozzle or a similar structure positioned very close to the milling area (e.g., less than 1 mm), a voltage pin (e.g., a structure where the sole or primary purpose is to apply a voltage near the area being milled or imaged), a nanomanipulator, or a similar structure may be included in the system that can be moved into a position very close to the area being milled. Fig. 8A and Figure 8B 800a and 800b, respectively, according to some embodiments. Each of the FIB evaluation systems 800a and 800b can be similar to the systems 100 and 400 discussed above and include a FIB column 810 that can direct an ion beam 820 toward a sample 830 positioned on a sample support 840. Systems 800a and 800b can also include a secondary ion detector (on the Fig. 8A or Figure 8B ), and a gas injection nozzle 860, wherein the secondary ion detector detects secondary ions generated during the milling operation, and the gas injection nozzle is positioned to introduce one or more gases into the area being milled.
[0057] like Fig. 8A and Figure 8B As shown in FIG. 8 , system 800a does not include a gas injection nozzle, while system 800b includes a gas nozzle 860 that directs gas from a location away from the milling area to the side of the milling area, in contrast to gas nozzle 460 ( FIG. 1 ) that introduces gas directly above the milling area. Figure 4) relative to the ion beam 820. Each of the systems 800a and 800b further includes a voltage applying structure 850, which can be positioned in close proximity (e.g., less than 1 mm) to the area on the sample 830 that is milled by the ion beam 820. In some embodiments, the voltage applying structure can be positioned less than 100 microns from the milled area, and in some embodiments, the voltage applying structure can be positioned within a few tens of microns from the milled area. In some embodiments, the voltage applying structure 850 can be freely moved within the processing chamber independent of the FIB column and other components, and in some embodiments, the voltage applying structure 850 can be physically connected to the gas injection nozzle and move with the gas injection nozzle.
[0058] The voltage applying structure 850 can be operably coupled to a voltage source and, once properly positioned, can apply a negative voltage near the milling area. In this way, the voltage applying structure 850 can repel secondary electrons that escape from the sample during the milling process back to the sample surface, as described above with respect to Figure 6C Discussed.
[0059] like Figure 8C As shown in , in other embodiments, the voltage application structure 870 may include a conductive ring structure 875 at its tip, the conductive ring structure including an internal opening 880 through which the ion beam can pass. The opening 880 can be very small (e.g., less than 1 mm in diameter), and the structure 875 can be positioned very close to the upper surface of the sample 830 so that when an appropriate negative voltage is applied to the structure 875, the secondary electrons can react with the above-mentioned Figure 6C The gas is repelled back to the surface of the sample 830 in the same manner as described above with respect to the gas nozzle 460.
[0060] Example of sample to be milled
[0061] As described above, embodiments of the present invention may be used to mill or image many different types of samples, including electronic circuits formed on semiconductor structures, solar cells formed on polycrystalline or other substrates, nanostructures formed on various substrates, etc. As a non-limiting example, Fig. 9 is a simplified illustration of an area on a semiconductor wafer that may be milled according to some embodiments. Specifically, Fig. 9Included is a top view of a wafer 900 and two expanded views of a particular portion of the wafer 900. The wafer 900 may be, for example, a 150 mm, 200 mm, or 300 mm semiconductor wafer, and may include a plurality of integrated circuits 905 (52 in the example shown) formed on the wafer 900. The integrated circuits 905 may be in an intermediate stage of manufacture, and the milling techniques described herein may be used to evaluate and analyze one or more regions 910 of the integrated circuit, including two or more sections adjacent to each other that exhibit different milling rates. For example, Fig. 9 Exploded view A of 905 illustrates a plurality of regions 910 of one of integrated circuits 905 that may be evaluated and analyzed according to the techniques described herein. Exploded view B illustrates one of those regions 910 including various electronic structures formed in the regions.
[0062] The embodiments of the present invention can use, for example, Figure 5 The method 500 discussed herein can be used to analyze and evaluate the region 910. The evaluation can be accomplished by scanning the SEM beam back and forth within the region 910 according to a raster pattern, such as in Fig. 9 Scan pattern 920 is shown in a simplified format in the expanded view B of .
[0063] For the purpose of explanation, the above description uses specific nomenclature to provide a thorough understanding of the described embodiments. However, it is obvious to those skilled in the art that specific details are not required to practice the described embodiments. Therefore, for the purpose of illustration and description, the foregoing description of the specific embodiments described herein is presented. The foregoing description is not intended to be exhaustive or to limit the embodiments to the precise form disclosed. In addition, although different embodiments of the present case are disclosed above, the specific details of the specific embodiments can be combined in any appropriate manner without departing from the spirit and scope of the embodiments of the present case. In addition, it is obvious to those skilled in the art that, in view of the above teachings, many modifications and variations are possible.
[0064] Furthermore, any reference in the above specification to a method shall apply mutatis mutandis to a system capable of executing the method and shall apply mutatis mutandis to a computer program product storing instructions which, upon execution, result in the execution of the method. Similarly, any reference in the above specification to a system shall apply mutatis mutandis to a method executable by the system and the system shall apply mutatis mutandis to a computer program product storing instructions executable by the system; and any reference in the specification to a computer program product shall apply mutatis mutandis to a method executable upon execution of the instructions stored in the computer program product and shall apply mutatis mutandis to a system configured to execute the instructions stored in the computer program product.
[0065] Because most of the embodiments shown in the present case can be implemented using electronic components and devices known to those skilled in the art, in order to understand and appreciate the basic concepts of the present case and in order not to confuse or distract from the teachings of the present case, the explanation of the details does not exceed the scope deemed necessary as described above.
[0066] Additional Embodiments
[0067] Any reference to a method in the above specification shall apply mutatis mutandis to a system capable of executing the method and shall apply mutatis mutandis to a computer program product storing instructions which, upon execution, result in the performance of the method. Similarly, any reference to a system in the above specification shall apply mutatis mutandis to a method executable by the system and the system shall apply mutatis mutandis to a computer program product storing instructions executable by the system; and any reference to a computer program product in the specification shall apply mutatis mutandis to a method executable when the instructions stored in the computer program product are executed and shall apply mutatis mutandis to a system configured to execute the instructions stored in the computer program product.
[0068] While most of the illustrated embodiments in the present case can be implemented using electronic components and circuits known to those skilled in the art, the explanation of the details does not exceed the scope deemed necessary above in order to understand and appreciate the basic concepts of the present case and to not confuse or distract from the teachings of the present case.
[0069] For purposes of explanation, the above description uses specific nomenclature to provide a thorough understanding of the described embodiments. However, it will be apparent to one skilled in the art that specific details are not required to practice the described embodiments. For example, although various embodiments are described above with respect to applying a negative voltage to a gas nozzle or voltage application structure during a milling operation, the same concepts can be beneficially applied to imaging operations in which secondary ions are collected while an ion beam is directed toward a substrate. In such operations, when a non-conductive material is exposed to an ion beam during an imaging process, the embodiments described herein can prevent or greatly reduce the accumulation of positive charge in the imaged area by repelling secondary electrons back to the sample.
[0070] Therefore, the foregoing description of the specific embodiments described herein is presented for the purpose of illustration and description. The foregoing description is not intended to be exhaustive or to limit the embodiments to the precise form disclosed. In addition, although different embodiments of the present case are disclosed above, the specific details of the specific embodiments may be combined in any appropriate manner without departing from the spirit and scope of the embodiments of the present case. In addition, it will be apparent to those skilled in the art that many modifications and variations are possible in view of the above teachings.
Claims
1. A method for processing an area of a sample, the method comprising: positioning a sample within a vacuum chamber; An ion beam is generated using a focused ion beam (FIB) column; focusing the ion beam on the sample and scanning the focused ion beam across the region of the sample to generate secondary electrons that can be ejected from a surface of the sample within the region; as well as During the scan, a negative bias is applied to a conductive structure near the region to change the trajectory of the secondary electrons and repel the secondary electrons back to the sample surface, wherein the conductive structure is one of a gas injection nozzle, a voltage pin, or a nanomanipulator.
2. The method of claim 1, wherein during said scanning, said conductive structure is positioned five millimeters or less from said region.
3. The method of claim 1 or 2, wherein the conductive structure comprises a gas injection nozzle located between a column cap of the FIB column and the sample. 4 . The method of claim 3 , further comprising: heating the gas injection nozzle while applying a negative bias to the gas injection nozzle.
5. The method of claim 4, wherein during the scanning step, a first end of the gas injection nozzle is positioned adjacent to the region and a second end of the gas injection nozzle extends through a conductive wall of a component of the vacuum chamber and is electrically insulated from but thermally coupled to the wall.
6. The method of claim 1 or 2, wherein the conductive structure comprises a voltage pin operable to move within 100 microns of the area.
7. A method as described in any one of claims 1 to 6, wherein the sample includes a non-conductive layer formed on an upper surface of the sample, and the focusing step scans the focused ion beam across the area of the sample to mill a portion of the non-conductive layer.
8. The method of any one of claims 1 to 6, wherein the sample comprises a semiconductor substrate and during the scanning, the conductive structure is positioned between 5 micrometers and 1.5 millimeters from the region.
9. A system for processing an area of a sample, the system comprising: Vacuum chamber; a sample support configured to retain a sample within the vacuum chamber during a processing operation; a focused ion beam (FIB) column configured to direct an ion beam into the vacuum chamber toward the region of the sample during the processing operation; a conductive structure movable to a position so that when the sample is positioned on the sample support, the conductive structure is adjacent to the region of the sample, wherein the conductive structure is one of a gas injection nozzle, a voltage pin, or a nanomanipulator; as well as A voltage source is operable to apply a negative bias to the conductive structure.
10. The system of claim 9, wherein the conductive structure is positioned 1.5 millimeters or less from the region of the sample.
11. The system of claim 9, further comprising a processor and a memory coupled to the processor, wherein the memory comprises a plurality of computer-readable instructions, and when the instructions are executed by the processor, the system performs the following operations: positioning a sample within a vacuum chamber; An ion beam is generated using a focused ion beam (FIB) column; focusing the ion beam on the sample and scanning the focused ion beam across the region of the sample to generate secondary electrons that can be ejected from a surface of the sample within the region; as well as During the scan, a negative bias is applied to the conductive structure near the region of the sample to change the trajectory of the secondary electrons and repel the secondary electrons back to the sample surface.
12. The system of claim 9, wherein the conductive structure is a gas injection nozzle.
13. The system of claim 12, further comprising heating the gas injection nozzle while applying a negative bias to the gas injection nozzle.
14. The system of claim 12, wherein during the scanning step, a first end of the gas injection nozzle is positioned adjacent to the region and a second end of the gas injection nozzle extends through a conductive wall of a component of the vacuum chamber and is electrically insulated from but thermally coupled to the wall.
15. A system as described in any one of claims 9 to 14, wherein the sample includes a non-conductive layer formed on an upper surface of the sample, and the focusing step scans the focused ion beam across the area of the sample to mill a portion of the non-conductive layer.
16. A non-transitory computer-readable memory comprising a plurality of computer-readable instructions, which, when executed by one or more processors, cause the processors to perform the following operations: positioning a sample within a vacuum chamber; An ion beam is generated using a focused ion beam (FIB) column; focusing the ion beam on the sample and scanning the focused ion beam across the region of the sample to produce secondary electrons that are ejected from a surface of the sample within the region; as well as During the scan, a negative bias is applied to a conductive structure near the region to change the trajectory of the secondary electrons and repel the secondary electrons back to the sample surface, wherein the conductive structure is one of a gas injection nozzle, a voltage pin, or a nanomanipulator.
17. The non-transitory computer readable memory of claim 16, wherein the computer readable instructions cause the conductive structure to be positioned 1.5 millimeters or less from the region.
18. The non-transitory computer readable memory of claim 16 or 17, wherein the conductive structure comprises a gas injection nozzle located between a cap of the FIB column and the sample.
19. The non-transitory computer readable memory of claim 18, wherein the computer readable instructions further comprise instructions that cause the one or more processors to heat the gas injection nozzle while a negative bias voltage is applied to the gas injection nozzle.
20. The non-transitory computer readable memory of claim 18, wherein a first end of the gas injection nozzle is positioned adjacent to the region, and a second end of the gas injection nozzle extends through a conductive wall of a component of the vacuum chamber and is electrically insulated from but thermally coupled to the wall.