Method for texturing and marking surface

By first preparing areas with different roughness on the plastic surface and performing local melting treatment, the texture and printing complexity problems in the prior art are solved, and the surface effects of different textures and light reflectivity are achieved, the production process is simplified and the production process is reduced. cost.

CN119032005APending Publication Date: 2024-11-26KETER HOME & GARDEN PROD LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380031552.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-27
Filing Date
2023-04-19
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The prior art requires expensive equipment and hazardous materials when textured plastic surfaces, and the printing process is complex, making it difficult to effectively achieve surface effects of different reflectivity and tones.

Method used

Texturizing and marking is achieved by first preparing foamed thermoplastic polymer materials with rough surfaces, selectively melting in specific areas, reducing roughness to obtain areas with different textures and light reflectivity, and local heat treatment with heating rollers or plates to achieve texture and marking .

Benefits of technology

The simpler and more cost-effective production of surfaces with different textures and light reflectivity is achieved, capable of simulating the visual effects of natural or artificial materials, and allows direct printing of ink on textured surfaces, improving adhesion and fixation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119032005A_ABST
    Figure CN119032005A_ABST
Patent Text Reader

Abstract

The present disclosure relates to texturing and / or marking surfaces of plastic articles, and more particularly to methods for creating textures and marks on surfaces made of foamed plastic material to achieve different reflectance or different hues by selectively altering the roughness of the surface.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to texturing and / or marking the surface of plastic articles, and more particularly to methods for producing textures and markings on surfaces made of plastic materials to obtain different reflectivities or different hues. Background Art

[0002] The following is a list of references that are believed to be relevant to the background of the presently disclosed subject matter:

[0003] - U.S. Patent Application Publication No. 2007 / 0235414

[0004] - U.S. Patent No. 4,107,247

[0005] Acknowledgment herein of the above references should not be inferred as meaning that these references are in any way relevant to the patentability of the presently disclosed subject matter.

[0006] background

[0007] In order to obtain various aesthetic effects, it is desirable to texture or mark a surface, in particular a surface made of plastic material. By texturing, a surface with different reflectivity, a different touch, a different hue, a defined pattern, etc. can be obtained.

[0008] Texturing of plastic surfaces, such as surfaces made of polypropylene, can be performed with various known techniques, such as engraving, etching, brushing, laser treatment, plasma treatment, corona treatment, etc. These techniques generally involve the removal of material from the surface of the article by different mechanisms, such as ablation, engraving, or by local chemical modification of the surface; these techniques generally require the use of expensive equipment. Other techniques involve printing onto the surface, however, due to the significant differences in surface tension and chemical compatibility between the plastic surface and the printing ink, it is generally necessary to first apply one or more primer compositions to the surface. Such surface printing generally involves hazardous materials, as well as the need for further processing steps and equipment. Summary of the invention

[0009] General Description

[0010] The present disclosure provides a method for obtaining a textured article, i.e., an article having a texture on its surface, which has regions of different textures and light reflectivity. In contrast to known methods in which a smooth surface is first obtained and then textured, in the method of the present disclosure, an article having a rough surface is first produced, and then processed to selectively reduce the roughness in one or more regions, thereby obtaining the desired texture, resulting in regions with different roughness and different light reflectivity. The method of the present disclosure provides a simpler and more cost-effective way to produce an article with a desired textured surface. The method of the present disclosure can also be used to mark a surface with different markings (such as letters, numbers, symbols, etc.).

[0011] By a first aspect of the present disclosure, there is provided a method for texturing a surface made of a thermoplastic polymer material to obtain a textured surface having regions with different roughness levels, the method comprising: providing a foamed surface made of a foamed thermoplastic polymer material, the foamed surface having a first roughness level; melting the foamed thermoplastic material at one or more regions of the foamed surface to reduce the roughness in the one or more regions to a second roughness level, thereby obtaining the textured surface.

[0012] By another aspect of the present disclosure, the present disclosure provides a method for providing an article having a textured surface, wherein the textured surface includes areas of different light reflectivity, the method comprising: providing a foamed surface made of a foamed thermoplastic polymer material to obtain a first light reflectivity of the foamed surface; and melting the foamed thermoplastic material at one or more areas of the foamed surface to reduce the roughness in the one or more areas, thereby obtaining a second light reflectivity of the one or more areas, wherein the second light reflectivity is greater than the first light reflectivity.

[0013] Texturing (or any linguistic variant thereof) is meant to represent the formation of one or more three-dimensional (3D) artifacts on the surface of an object, i.e., artifacts extending from or recessed into the surface. Texturing can be an ordered pattern, graphic, image, etc.; or a random texture, for example simulating natural materials (such as wood, stone, clay, etc.), or simulating artificial materials (such as concrete). In the context of the present disclosure, texturing is also meant to cover various forms of marking the surface, such as by letters, numbers, symbols, graphics, etc.

[0014] The term roughness (or surface roughness or roughness level, used interchangeably herein) is meant to represent a measure of the irregularity of a surface compared to an ideal, smooth form of the surface. In other words, roughness is an average measure of fine surface details such as peaks, protrusions, depressions, valleys, etc. The higher the roughness value, the rougher the surface, meaning that the surface details have a larger or more prominent amplitude.

[0015] The term light reflectance (or light reflectance ratio or reflectivity, used interchangeably herein) means the relative amount of light reflected from a surface. In the context of the present disclosure, light reflectance means the reflectance of light in the visible spectrum. Light reflectance is affected by and is related to surface roughness-the higher the surface roughness, the lower the light reflectance. Smooth surfaces generally cause incident light rays that hit the surface to be reflected in an orderly manner, i.e., where the reflected light rays are parallel to each other (referred to as "regular reflection"). Therefore, the more reflected light reaches the viewer's eyes, the more "glossy" and "darker" the surface color perceived by the viewer is. In contrast, a rougher surface will cause the incident light rays to be reflected at different angles due to the irregularities of the surface (referred to as "diffuse reflection") and therefore be perceived by the viewer as a "lighter", "brighter" or "duller" hue. Light reflectance is also referred to herein interchangeably as specular gloss, as measured according to ASTM D2457 (unless otherwise explicitly stated).

[0016] In articles produced according to the methods of the present disclosure, differences in roughness and / or light reflectance are exploited to provide an article with a textured surface, wherein regions of the surface have different roughnesses, and therefore different light reflectances, which are perceived by a viewer as different color hues.

[0017] According to some embodiments, the method increases the light reflectance of the one or more regions by at least 20 gloss units (GU, as measured according to ASTM D2457). Thus, according to some embodiments, the second light reflectance is at least 20 GU greater than the first light reflectance.

[0018] By some embodiments, the first light reflectivity is at most 5 GU. By some other embodiments, the second light reflectivity is at least 25 GU.

[0019] In the method of the present disclosure, the surface is made of a foamed thermoplastic polymer material, and the foaming results in a surface having a first roughness. The foamed surface is then subjected to a selective heating process, whereby one or more selected areas of the surface are exposed to heating conditions, thereby softening or melting the thermoplastic polymer material in these one or more areas to cause smoothing or a reduction in the roughness level in these areas. Thus, a desired texture or pattern characterized by different roughness levels (or light reflectance) is obtained on the surface.

[0020] Melting refers to a change in the physical state of a thermoplastic polymer material, wherein the thermoplastic polymer material is transformed into a molten state between a solid and a liquid state due to exposure to heat (i.e., due to an increase in temperature without exposure to any solvent). Thus, the method of the present disclosure utilizes the molten state of a thermoplastic polymer material, wherein the thermoplastic polymer material is pliable, in order to locally change its roughness in selected areas of a surface (e.g., reduce the roughness of the surface at its desired area).

[0021] The regions may be of any size and shape, continuous or comprise several non-continuous sub-regions on the surface. The regions may form an ordered pattern or image, or may have a random shape and / or be randomly distributed on the surface.

[0022] By some embodiments, melting is obtained by contacting the foaming surface with at least one textured heating surface, the heating surface having a texture with the second roughness level. In other words, local melting of the foaming surface is induced by contacting the foaming surface with the textured heating surface of the second roughness level, the foaming surface being embossed with the texture of the heating surface at the one or more areas in contact with the textured heating surface.

[0023] By some embodiments, the textured heating surface comprises a pattern having at least two zones with different roughness levels between the at least two zones. According to such embodiments, the textured heating surface may include a first zone having the second roughness level and a second zone having a third roughness level less than the second roughness level. In other words, contact of the foaming surface with the first zone will result in a region having the second roughness level, while contact of the foaming surface with the second zone will result in a region having an even smaller roughness level (i.e., the third roughness level). By another example, the textured heating surface is designed such that each of the one or more zones has a first zone and a second zone having different roughness levels.

[0024] According to some embodiments, the textured heated surface is a heated roller. According to other embodiments, the textured heated surface is a heated plate.

[0025] By some embodiments, the textured heating surface is heated to a temperature of at least about 140° C. By other embodiments, the textured heating surface is heated to a temperature in a range between about 140° C. and about 180° C.

[0026] It should be noted that selective heating / melting may be achieved by other suitable techniques such as laser etching, corona treatment, exposure to an open flame, and the like.

[0027] As mentioned above, the surface is made of a thermoplastic polymer material, which is a polymer material having a melting point and which can be softened or melted by applying heat thereto. The term thermoplastic polymer material is intended to include homopolymers, copolymers, such as block copolymers, graft copolymers, random copolymers and alternating copolymers, and terpolymers, and also includes their derivatives, combinations and blends. The term includes all geometric configurations of this structure, including linear, block, grafted, random, alternating, branched structures and combinations thereof. The term also means a blend or mixture comprising two or more thermoplastic polymers. Non-limiting examples of such thermoplastic polymer materials include polyolefins, polar thermoplastic materials, polystyrene, polyvinyl chloride (PVC), acrylonitrile-butadiene-styrene (ABS), styrene copolymers, polyacrylonitrile, polyacrylates, polyacrylamides, vinyl acetate polymers, vinyl alcohol polymers, cellulosics, thermoplastic elastomers, thermoplastic polyurethanes, polyester-based thermoplastic elastomers, thermoplastic polyesters, polyethylene terephthalate, polybutylene terephthalate, compatible thermoplastic blends, polyacetals, polyethers, polyarylates, polycarbonates, polyamides, polyimides, polybenzimidazoles, aromatic polyhydrazides and polyoxadiazoles, polyphenyl-quinoxalines, polyphenylene sulfides, polyphenylene vinylenes, conductive thermoplastic materials, conductive thermoplastic composites, poly(arylethersulfones), poly(aryletherketones), poly(aryletherketone-co-sulfones), poly(aryletherketoneamides), polytetrafluoroethylene, and mixtures thereof.

[0028] By some embodiments, the thermoplastic polymer material is a composition comprising one or more polyolefins or copolymers thereof.

[0029] By some embodiments, the thermoplastic polymer material is a composition comprising polyethylene, polypropylene, or copolymers or mixtures thereof.

[0030] By some embodiments, the thermoplastic polymer material is a composition comprising polypropylene or a copolymer or mixture thereof.

[0031] The thermoplastic polymer material is foamed to obtain a foamed surface. The term foam (or any linguistic variation thereof) refers to a cellular structure containing pores which are connected to each other and form an interconnected 3-dimensional network.

[0032] According to some embodiments, the foamed thermoplastic polymer material is a closed cell foam.

[0033] By some embodiments, the foamed thermoplastic polymer material is obtained by exothermic foaming. Exothermic foaming is obtained by the decomposition of a chemical reaction or a foaming agent, and is characterized in that gas and energy (mainly in the form of heat) are released during the reaction. Therefore, due to the formation and expansion of gaseous decomposition products, the volume expansion or foaming of the thermoplastic polymer is obtained; when the exothermic reaction produces heat, it is actually self-propagating. In other words, after the initial heating stage of the initiation reaction, once enough heat is released due to the reaction, it is not necessary to provide further external heating and the foaming reaction self-propagates. This makes the utilization of the exothermic foaming agent more cost-effective and reduces the total energy invested in the method.

[0034] According to some embodiments, the thermoplastic polymer material is a composition comprising at least one thermoplastic polymer and at least one exothermic blowing agent. The exothermic foaming stage comprises exposing the composition to conditions allowing exothermic decomposition of the blowing agent to obtain a foamed thermoplastic polymer material.

[0035] According to some embodiments, the conditions under which the exothermic foaming is performed are a temperature ranging between about 170°C and about 220°C.

[0036] According to some embodiments, the exothermic blowing agent may be selected from azodicarbonamide (ADC); 4,4-oxybisbenzenesulfonylhydrazide (OBSH); p-toluenesulfonylhydrazide (TSH); 5-phenyltetrazole (5-PT); p-toluenesulfonylsemicarbazide (PTSS); dinitrosopentamethylenetetramine (DNPT), and any mixture thereof.

[0037] It will be appreciated that the blowing agent may be utilized as such, ie as a pure material, or may be introduced into the thermoplastic polymer material in formulated form, typically as a formulation of carrier particles (which may be made of a thermoplastic polymer) coated or embedded with the blowing agent.

[0038] The thermoplastic polymer material may also include one or more additives, such as functional additives, which are used to impart one or more desired properties to the thermoplastic polymer material. Such functional additives may be, for example, pigments, reinforcing fibers or particles, fillers, UV stabilizers, UV absorbers, plasticizers, antistatic agents, antioxidants, flame retardants, minerals, biocides, etc.

[0039] According to some embodiments, the method further comprises printing one or more layers of printed ink on at least a portion of the textured surface to provide further texturing or to provide one or more additional visual effects. While typical printing on plastic surfaces requires the use of one or more primer layers to increase the adhesion of the printed ink to the polymer surface, the roughness of the textured surface obtained by the method of the present disclosure allows the printed ink to be mechanically fixed or locked into the rough surface structure. Thus, further visual texturing can be obtained by printing one or more layers of ink onto the textured surface.

[0040] Printing may be performed by any suitable technique, such as digital printing, screen printing, flexographic printing, lithographic printing or transfer printing. According to some embodiments, the printing is digital printing.

[0041] According to some embodiments, the textured surface is the surface of an extruded panel.

[0042] By some embodiments, the extruded article is made of, ie, consists entirely of, the foamed thermoplastic polymer material.

[0043] By other embodiments, the extruded panel comprises a core made of a non-foamed thermoplastic material and the foamed surface is made of the foamed thermoplastic polymer material.According to such embodiments, the non-foamed thermoplastic material is a composition comprising polypropylene, polyethylene or copolymers or blends thereof.

[0044] By some other embodiments, the extruded panel includes a core made from a non-polymeric thermoplastic composition, the core at least partially coated with a foamed thermoplastic polymer material.

[0045] According to some embodiments, the extruded article is manufactured by coextruding a core material and the thermoplastic polymer material coating the core material.

[0046] According to some embodiments, the extrusion and / or coextrusion is performed under conditions that allow the foaming during extrusion.

[0047] According to another aspect of the present disclosure, the present disclosure provides a method for obtaining a pattern on a foamed surface, the foamed surface being made of a foamed thermoplastic polymer material and having a first roughness level, the method comprising melting the foamed thermoplastic material at one or more regions of the foamed surface to reduce the roughness in the one or more regions to a second roughness level, thereby obtaining the pattern.

[0048] Another aspect of the present disclosure provides a method for patterning a foamed surface of an article, the foamed surface being made of a foamed thermoplastic polymer material and having a first light reflectivity, the method comprising melting the foamed thermoplastic material at one or more regions of the foamed surface to reduce the roughness in the one or more regions, thereby obtaining a second light reflectivity of the one or more regions, the second light reflectivity being greater than the first light reflectivity.

[0049] By yet another aspect, the present disclosure provides an article having a surface made of a foamed thermoplastic material having a first roughness level and including one or more regions having a second roughness level that is less than the first roughness level, the article being made according to the method disclosed herein.

[0050] As used herein, the term about is meant to encompass deviations of ±10% from the specifically mentioned parameter value (such as temperature, pressure, concentration, etc.).

[0051] Whenever a numerical range is indicated herein, it is meant to include any cited numerical value (fractional or integer) within the indicated range. The phrases range between a first indicated number and a second indicated number and range from a first indicated number to a second indicated number are used interchangeably herein and are meant to include the first indicated number and the second indicated number and all fractions and integers therebetween.

[0052] It should be understood that certain features described in the context of separate embodiments for clarity may also be provided in combination in a single embodiment. Conversely, various features of the invention described in the context of a single embodiment for brevity may also be provided individually or in any suitable subcombination or suitably provided in any other described embodiment of the invention. Certain features described in the context of various embodiments should not be considered essential features of those embodiments unless the embodiment is inoperable without those elements. BRIEF DESCRIPTION OF THE DRAWINGS

[0053] In order to better understand the subject matter disclosed herein and to illustrate how it may be implemented in practice, embodiments will now be described, by way of non-limiting example only, with reference to the accompanying drawings, in which:

[0054] Figure 1A to Figure 1B They are schematic diagrams of regular reflection and diffuse reflection of light from a surface.

[0055] FIG. 2A to FIG. 2B An extrusion molded polypropylene composition panel produced according to an embodiment of the method of the present disclosure is shown, wherein Figure 2A The foamed surface of the panel is shown, and Figure 2B The finished panel is shown after regions of the foamed surface have been melted to obtain a pattern.

[0056] Figure 2C A textured heated roller utilized in a method according to an embodiment of the present disclosure is shown.

[0057] FIG. 3A to FIG. 3B The surface structure of the article produced according to the method of the present disclosure is described ( Figure 3A ) and its close-up ( Figure 3B ).

[0058] Figure 4 An exemplary cross-section of a heated texturing roller utilized in one embodiment of a method according to the present disclosure is illustrated.

[0059] Figure 5 An extrusion molded polypropylene composition panel without a foamed surface is shown, on which surface melting is employed.

[0060] Figure 6 An extruded wood plastic composition (WPC) without a foamed surface is shown, on which high pressure mechanical embossing was applied. DETAILED DESCRIPTION

[0061] As described above, the method of the present disclosure can obtain a textured surface of an article having regions of different roughness and light reflectivity to obtain various visual effects. Figure 1A to Figure 1B As shown, the roughness of a surface affects the hue of the color perceived by the viewer. Regular reflection of light is obtained from a smooth surface, in which incident light rays striking the surface are reflected in a parallel, orderly manner, such as Figure 1A In regular reflection, more of the reflected light reaches the viewer's eye, and therefore the surface color is perceived by the user as "darker" or having a darker hue. Figure 1B As explained in , a rougher surface will cause incident light to be reflected at different angles (diffuse reflection) due to the irregularities of the surface and therefore be perceived by the viewer as a "lighter" or "brighter" hue.

[0062] The methods of the present disclosure can provide surfaces with differences in roughness and / or light reflectance, thereby obtaining an article with a textured or patterned surface, wherein areas of the surface have different roughness and, therefore, different light reflectances, which are perceived by a viewer as different color hues.

[0063] Example 1

[0064] Figure 2A, the surface of a panel made by coextrusion of a foamed thermoplastic polymer material is shown in FIG. 1 , in which, in this specific embodiment, the foamed thermoplastic polymer material is a composition comprising polypropylene as a main component and azodicarbonamide (ADC) as an exothermic foaming agent. The material temperature at the coextruder is 170° C. to 220° C., and before being extruded through the extrusion die, the material is kept in the coextruder for a predetermined period of time to allow the ADC to decompose and form the foamed outer surface of the panel.

[0065] After extrusion, the foamed surface of the panel is conveyed under a textured heated roller, an example of which is shown in Figure 2C As can be seen, the area of ​​the roller, generally designated 102, is textured and results in the transfer of heat to the foamed surface in a controlled manner. The roller is heated to a temperature of about 140°C and, when rolled over the foamed surface of the panel, local melting of the polypropylene is obtained, thereby "smoothing" the surface in these areas and giving them a roughness grade and texture according to that of the area 102. Thus, as Figure 2B As can be seen, panel 100 has areas (generally designated 104) of high roughness level resulting from foaming (perceived by the viewer as having a lighter hue), and areas 106 having a lower roughness level (perceived by the viewer as having a darker hue) due to melting and smoothing imparted by the textured heated roller.

[0066] from Figure 2B It can be clearly seen in FIG. 1 that region 106 is significantly darker than region 104 due to the difference in roughness level.

[0067] The light reflectance from the different regions is measured according to ASTM D2457. In region 104, the light reflectance is at most 5 GU, while in region 106, the light reflectance is at least 25 GU. Although the panel has the same color along its entire surface, this difference in reflectance (caused by the difference in roughness) causes the region 104 with a higher degree of roughness to be perceived as having a "lighter" or "duller" hue, and the region 106 with a lesser degree of roughness to be perceived as having a "darker" or "glosser" hue of the same color.

[0068] from Figure 2B , Figure 3A and Figure 3B As can be clearly seen in the Figures, the method enables careful control of the surface roughness, thereby enabling the extruded panel to be given a desired texture, in this particular example simulating a natural wood panel grain and texture with a high degree of accuracy.

[0069] exist Figure 4A close-up view of the illustrated portion of the roller can be seen in , in which the corresponding profile 200 of the heated texturing roller is illustrated. The zones 202 of the roller have a roughness level less than the roughness of the foamed surface of the panel and protrude from the surface of the roller so that the zones 202 come into contact with the foamed surface of the panel when the roller rolls over the surface. The predetermined texture of the zones 202 also enables control of the heat transfer to the panel surface once contact between the roller and the foamed surface to be textured is obtained, thereby avoiding excessive melting of the foamed surface and hindering the desired texture. When the roller is heated, the thermoplastic polymer material constituting the surface of the panel undergoes local melting and is imparted with the roughness and texture of the zones 202 to obtain regions 106 of less roughness level and darker hue. However, the zones 204 of the roller constitute the gaps between the zones 202 where the roller does not come into contact with the surface of the panel, leaving the original, higher roughness foamed texture untreated, thereby obtaining regions 104 with lighter hues.

[0070] Example 2 - Reference Example

[0071] Figure 5 In FIG. 3 , an extruded panel 300 made of the same polypropylene composition as in Example 1, but without a blowing agent, can be seen. The panel was processed by the heated texturing roller of Example 1 under the same conditions to obtain a textured panel 300. Figure 5 As can be seen in FIG. 1 , there is almost no difference in color tone between the area 302 constituting the original smooth surface of the panel and the area 304 being the area in contact with the heating roller.

[0072] Example 3 - Reference Example

[0073] Figure 6 In FIG. 4 , an injection molded panel 400 made of the same polypropylene composition as in Example 1, but without a blowing agent, can be seen. The panel was mechanically embossed by high pressure and heat. Figure 6 As can be seen in FIG, although a pattern is visible on the surface of the panel, almost no difference in color tone is observed.

Claims

1. A method for texturing a surface made of a thermoplastic polymer material to obtain a textured surface having areas of different roughness, the method comprising: providing a foamed surface made of a foamed thermoplastic polymer material, the foamed surface having a first roughness level; as well as The textured surface is obtained by melting the foamed thermoplastic material at one or more regions of the foamed surface to reduce the roughness in the one or more regions to a second roughness level.

2. The method according to claim 1, wherein the melting is obtained by contacting the foaming surface with at least one textured heating surface, the heating surface having a texture with the second roughness level.

3. The method of claim 2, wherein the textured heating surface is heated to a temperature of at least about 140°C.

4. The method of claim 2 or 3, wherein the textured heating surface comprises a pattern having at least two regions with different levels of roughness between the at least two regions. 5 . The method of claim 4 , wherein the textured heating surface comprises a first region having the second roughness level and a second region having a third roughness level less than the second roughness level.

6. A method according to any one of claims 2 to 5, wherein the textured heated surface is a heated roller.

7. The method according to any one of claims 1 to 6, wherein the thermoplastic polymer material is a composition comprising polypropylene or a copolymer thereof.

8. The method according to any one of claims 1 to 7, wherein the foamed thermoplastic polymer material is obtained by exothermic foaming.

9. The method of claim 8, wherein the thermoplastic polymer material is a composition of one or more thermoplastic polymers and one or more exothermic blowing agents, the exothermic foaming comprising exposing the composition to conditions that allow exothermic decomposition of the exothermic blowing agent to obtain the foamed thermoplastic polymer material.

10. The method according to claim 9, wherein the exothermic blowing agent is selected from azodicarbonamide (ADC); 4,4-oxybisbenzenesulfonylhydrazide (OBSH); p-toluenesulfonylhydrazide (TSH); 5-phenyltetrazole (5-PT); p-toluenesulfonyl semicarbazide (PTSS); dinitroso-pentamethylenetetramine (DNPT), and any mixture thereof.

11. The method of any one of claims 1 to 10, wherein the textured surface is the surface of an extruded article.

12. The method of claim 11, wherein the extruded article is made from the foamed thermoplastic polymer material.

13. The method of claim 11, wherein the extruded article comprises a core made of a non-foamed thermoplastic material and the surface is made of the foamed thermoplastic polymer material.

14. The method of claim 13, wherein the non-foamed thermoplastic material is a composition comprising polypropylene or a copolymer thereof.

15. The method of claim 11, wherein the extruded article comprises a core made from a non-polymeric thermoplastic composition, the core being coated with the foamed thermoplastic polymer material.

16. A method according to any one of claims 13 to 15, wherein the extruded article is produced by coextruding the foamed thermoplastic polymer material onto the core.

17. The method of any one of claims 1 to 16, further comprising digitally printing one or more printing inks on at least one area of ​​the textured surface.

18. A method for providing an article having a textured surface comprising regions of different light reflectivity, the method comprising: providing a foamed surface made of a foamed thermoplastic polymer material to obtain a first light reflectivity of the surface; as well as The foamed thermoplastic material is melted at one or more regions of the foamed surface to reduce the roughness in the one or more regions, thereby obtaining a second light reflectivity of the one or more regions, the second light reflectivity being greater than the first light reflectivity.

19. The method of claim 18, wherein the second light reflectance is at least 20 gloss units greater than the first light reflectance (as measured according to ASTM D2457).

20. The method according to claim 18 or 19, wherein the melting is obtained by contacting the foaming surface with at least one textured heating surface, the heating surface having a texture with the second roughness level.

21. The method of claim 20, wherein the heated surface comprises a pattern having at least two zones with a different level of roughness between the at least two zones.

22. The method of claim 21, wherein the heated surface comprises a first region having the second roughness level and a second region having a third roughness level less than the second roughness level.

23. A method according to any one of claims 18 to 22, wherein the textured heated surface is a heated roller.

24. A method according to any one of claims 18 to 23, wherein the thermoplastic material is a composition comprising polypropylene or a copolymer thereof.

25. The method according to any one of claims 18 to 24, wherein the foamed thermoplastic polymer material is obtained by exothermic foaming.

26. The method of claim 25, wherein the thermoplastic polymer material is a composition of one or more thermoplastic polymers and one or more exothermic blowing agents, the exothermic foaming comprising exposing the composition to conditions that allow exothermic decomposition of the exothermic blowing agent to obtain the foamed thermoplastic polymer material.

27. The method according to any one of claims 18 to 26, wherein the article is obtained by extrusion.

28. A method according to any one of claims 18 to 27, wherein the article is made from the foamed thermoplastic polymer material.

29. The method according to any one of claims 18 to 28, wherein the article comprises a core made of a non-foamed thermoplastic material and the surface is made of the foamed thermoplastic polymer material.

30. The method according to claim 29, wherein the article is obtained by coextrusion.

31. A method for obtaining a pattern on a foamed surface, the foamed surface being made of a foamed thermoplastic polymer material and having a first roughness level, the method comprising: The pattern is obtained by melting the foamed thermoplastic material at one or more regions of the foamed surface to reduce the roughness in the one or more regions to a second roughness level.

32. A method for patterning a foamed surface of an article, the foamed surface being made of a foamed thermoplastic polymer material and having a first light reflectivity, the method comprising: The foamed thermoplastic material is melted at one or more regions of the foamed surface to reduce the roughness in the one or more regions, thereby obtaining a second light reflectivity of the one or more regions, the second light reflectivity being greater than the first light reflectivity.

33. An article having a surface made of a foamed thermoplastic material having a first roughness level and comprising one or more regions having a second roughness level, the second roughness being less than the first roughness level, the article being manufactured according to the method of any one of claims 1 to 32.