Surface nanocrystallization powder metal cementation device
By designing a surface nanopowder metal seepage device, the transmission mechanism increases the relative velocity between the projectile and the workpiece and the centrifugal force, achieving multi-directional impact, forming nanolayers and inhibiting grain growth, the thermal diffusion of nanomaterials is solved The problem of grain growth during seepage process improves the efficiency of seepage layer generation and the stability of the workpiece surface.
Patent Information
- Application Number
- CN202411157901.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-08-22
AI Technical Summary
Nanomaterials face grain growth problems during thermal diffusion and seepage, resulting in insufficient thermal stability of nanostructures, affecting the formation and performance of the seepage layer.
A surface nano-powder metal seepage device was designed, and the relative speed between the projectile and the workpiece was increased through the transmission mechanism. Gravity and centrifugal force were used to make the projectile throw and fall in the seepage tank, achieving multi-directional impact and forming a nanolayer , and dislocations are generated in the permeable layer to inhibit grain growth.
It effectively solves the problem of grain growth, improves the formation efficiency of nanolayers and the generation speed of seepage, avoids grain coarseness, and ensures the nanostructure stability and performance of the workpiece surface.
Smart Images

Figure CN119040798A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of metal material surface strengthening, in particular to a surface nano-powder metal infiltration device. Background Art
[0002] The defects and microcrystalline nanostructures on the surface of metal materials will accelerate the surface chemical reaction and diffusion process and promote the formation of surface coatings. In the method of preparing coatings using these factors, two steps are usually taken: first, the surface structure is changed by physical methods to form a microcrystalline nanostructure with a large number of defects on the surface; then, the surface coating is formed by the diffusion of active atoms using the surface chemical heat treatment method. Zhang Wei et al. adopted a low-temperature carburizing technology for titanium-aluminum-based intermetallic compound materials in the patent "A low-temperature surface carburizing method for titanium-aluminum-based intermetallic compound materials" (patent publication number: CN102409282A). The specific method is to use conventional methods to nano-treat the surface of the metal material, then perform low-temperature carburizing at 500°C~800°C, and prepare a 4~9um thick carburized layer on the sample surface. However, the nanostructured material itself faces a problem - thermodynamic instability. Because nanomaterials have an extremely high interface volume percentage, the large amount of excess free energy stored in the interface provides an extremely high driving force for grain growth. According to the Gibbs-Thomson equation, the driving force of grain growth is inversely proportional to the grain size. When the grain size is reduced from the micron level of traditional coarse-grained materials to the nanometer level, the driving force of grain growth will be very high. Many nanocrystalline materials have begun to grow grains even at room temperature, and grain growth will cause nanomaterials to lose their unique microstructure and properties, such as diffusion properties. The study shows that the chromium-diffused hot working die steel after nano-pretreatment was chromized at different temperatures. It was found that in the temperature range of 500-600 degrees Celsius, the thickness of the chromized layer increased with the increase of temperature and reached a maximum value at 600 degrees Celsius. This is because the increase in temperature is conducive to the diffusion of elements. From 600 degrees Celsius to 700 degrees Celsius, the depth of the chromium diffusion layer decreased with the increase of temperature. This is mainly because, below 600 degrees Celsius, the non-equilibrium grain boundary of the nanostructure dominates the diffusion of chromium elements, and the diffusion speed is very fast. Above 600 degrees Celsius, with the coarsening of the grains, the diffusion of chromium elements gradually changes from grain boundary diffusion to body diffusion, and the diffusion performance gradually decreases. Above 700 degrees Celsius, the grain coarsening is very serious, mainly dominated by lattice diffusion. It can be seen that nanomaterials always face the problem of grain growth in the process of thermal diffusion, and the thermal stability of the nanostructure surface is the key factor restricting the effect of thermal diffusion.
[0003] In order to solve the grain growth problem faced by nanomaterials during thermal diffusion, the inventor Chen Haifeng disclosed a mechanical energy assisted nano thermal diffusion device in the patent "A mechanical energy assisted nano thermal diffusion device" (publication number: CN202210029534.1), including a diffusion tank, a planetary transmission mechanism and a rotating shaft, characterized in that the diffusion tank consists of a left end cover, a tank body and a right end cover, an inner gear ring and a baffle are provided on the inner surface of the diffusion tank, the left end cover is connected to the input shaft by bolts, and the right end cover is connected to the support shaft by Bolt connection, the input shaft is connected to the motor, a heating plate is arranged between the inner wall of the insulation box and the outer surface of the tank body, the planetary transmission mechanism is composed of planetary gears, planetary pins, planetary carriers and sun gears, the planetary carriers are respectively mounted on the inner sides of the left end cover and the right end cover, the planetary gears are mounted on the planetary carriers through planetary pins, the sun gear is fixed on the rotating shaft, a boss is arranged on the rotating shaft, the workpiece is fixed on the workpiece clamping plate, the infiltrant and the projectile are placed in the tank body, when the infiltration tank rotates, the baffle drives the projectile to fall from a high place, and the impact on the surface of the workpiece generates plastic deformation to form a nano layer. However, the planetary gears, planetary carriers and sun gears of the planetary transmission mechanism in this patent are all movable, and the sun gear can only rotate in the same direction with the planetary gears and the inner gear ring, and the relative speed when the projectile collides with the workpiece is small, and the plastic deformation generated by the impact may not necessarily form a nano layer. Summary of the invention
[0004] The purpose of the present invention is to provide a surface nano-powder metal infiltration device to solve the problem that the relative speed between the projectile and the workpiece is low and the plastic deformation caused by the impact may not necessarily form a nano layer.
[0005] In order to achieve the above-mentioned purpose, the present invention adopts the following technical scheme: a surface nano-powder metal infiltration device, including an infiltration tank, a transmission mechanism and a clamping mechanism, characterized in that the transmission mechanism is composed of a fixed frame, an input shaft, a first bevel gear, a second bevel gear and a third bevel gear, the first bevel gear is fixed on the input shaft, the second bevel gear is installed on the fixed frame and can rotate around the axis, the third bevel gear passes through the fixed frame and is connected to the flange sleeve through the second coupling and can rotate around the input shaft, the input shaft passes through the third bevel gear and is connected to the flange sleeve through the first coupling and the rotating shaft; the infiltration tank is composed of a left end cover, The tank body is composed of a tank body and a right end cover, the inner surface of the tank body is evenly provided with baffles, the left end cover is fixedly connected to the flange sleeve, the right end cover is connected to the support shaft by bolts, the support shaft is installed on the right cover plate of the insulation box through a bearing, a heating plate is arranged between the tank body and the insulation box, a left sealing plate, a right sealing plate and a clamping mechanism are arranged on the rotating shaft inside the tank body, the workpiece is installed on the clamping mechanism, the left sealing plate and the right sealing plate are clearance-matched with the inner surface of the tank body, a projectile and a penetrant are arranged between the left sealing plate and the right sealing plate, the linear velocity of the projectile is 2.5~10m / s, and the radius r of the tank body is related to the linear velocity of the projectile Satisfy the formula , g is the acceleration due to gravity.
[0006] Preferably, the rotating shaft is a spline shaft.
[0007] Preferably, the clamping mechanism is composed of an annular boss, a shaft sleeve, a clamping plate and bolts, and the inner sides of the annular boss and the shaft sleeve are both provided with keyways that cooperate with the rotating shaft.
[0008] Preferably, the modules and the numbers of teeth of the first bevel gear, the second bevel gear and the third bevel gear are respectively equal.
[0009] Preferably, the left end cover and the right end cover are fixed to both ends of the tank body by bolts.
[0010] Preferably, the left cover plate and the right cover plate are fixed to both ends of the insulation box by bolts.
[0011] Preferably, the left sealing plate and the right sealing plate are fixed to the rotating shaft by bolts.
[0012] Preferably, the gaps between the left sealing plate and the right sealing plate and the inner surface of the tank body are smaller than the diameter of the penetrant.
[0013] Preferably, the diameter of the pellet is 2-4 mm.
[0014] Preferably, the angle between the baffle and the inner wall of the tank body is 30°~60°.
[0015] Preferably, the penetrant is composed of pure metal powder or alloy powder, a filler and a catalyst, and the composition ratio of the penetrant is as follows by weight percentage: 50-70% pure metal powder or alloy powder, 20-49% filler, and 1-10% catalyst.
[0016] Preferably, the metal powder is zinc powder, aluminum powder, copper powder, or manganese powder, the alloy powder is chromium-aluminum, iron-zinc, iron-aluminum, or aluminum-rare earth alloy, the filler is aluminum oxide or silicon oxide, the catalyst is chloride or fluoride, and the powder particle size is 100-300 mesh.
[0017] The beneficial effect of the present invention is that the transmission mechanism is composed of a fixed frame, an input shaft, a first bevel gear, a second bevel gear and a third bevel gear. Since the first bevel gear is fixed on the input shaft, the second bevel gear is installed on the fixed frame and can rotate around the axis, the third bevel gear passes through the fixed frame and is connected to the flange sleeve through the second coupling and can rotate around the input shaft, and the input shaft passes through the third bevel gear and is connected to the flange sleeve through the first coupling with the rotating shaft. Therefore, the input shaft drives the first bevel gear to rotate while driving the rotating shaft to rotate, the first bevel gear is meshed with the second bevel gear, and the second bevel gear is meshed with the third bevel gear. According to the meshing principle, the first bevel gear and the third bevel gear have opposite rotation directions, and the third bevel gear is connected to the left end cover of the tank body through the flange sleeve, so that the rotation direction of the tank body is opposite to the rotation direction of the rotating shaft. The projectiles and the penetrant are driven to move by the baffles evenly arranged inside the infiltration tank. When the infiltration tank is rotated to a certain angle, the projectiles and the penetrant are thrown down under the combined action of gravity and centrifugal force, and impact the surface of the workpiece in multiple directions. Since the movement direction of the projectile is opposite to the rotation direction of the workpiece, the relative collision speed between the projectile and the workpiece is increased, solving the problem of insufficient relative collision speed between the projectile and the workpiece in the prior art, which is conducive to plastic deformation on the surface of the workpiece to form a nano layer, forming vacancies required for the diffusion of a large number of elements, and accelerating the formation of the infiltration layer. The difference from pre-nano-sizing followed by thermal diffusion infiltration is that although the recovery of grains and the growth of new alloy phases will occur during the thermal diffusion infiltration process, the collision of the projectiles and the penetrant will also produce dislocations in the new alloy phase, so that the nano-sizing process of the grains and the growth of the new phase proceed simultaneously, effectively solving the grain growth problem faced by the material after nano-sizing pretreatment during the thermal diffusion infiltration process.
[0018] However, if the impact speed of the projectile is too small, it is difficult to produce sufficient plastic deformation on the surface of the workpiece, and the nano-effect cannot be formed on the surface of the workpiece. If the impact speed of the projectile is too large, it is easy to form microcracks and other damages on the surface and sub-surface of the workpiece, affecting the service performance of the workpiece. At present, the commonly used methods of using projectile impact to achieve surface nano-peening include rotation acceleration shot peening, surface mechanical grinding, ultrasonic shot peening and high-energy shot peening. Among them, the diameter of the projectile used for surface mechanical grinding is 1~10mm, the vibration frequency is 50~20 kHz, and the projectile speed is 5~20 m / s. In this application, since the number of teeth and the module of the first bevel gear, the second bevel gear and the third bevel gear in the transmission mechanism are equal, the rotation speed of the projectile and the workpiece are equal, and the movement direction is opposite. Ignoring the influence of the radius of the workpiece installation position, the linear speed of the projectile and the workpiece is equal in size and opposite in direction. Therefore, setting the linear speed of the projectile to 2.5~10m / s can ensure that a nano layer can be produced on the surface of the workpiece after the projectile collides, and will not cause microscopic damage to the surface of the workpiece. In addition, the projectile is affected by gravity and centrifugal force at the same time during the movement. In the vertical position, when the centrifugal force on the projectile is greater than the gravity, the projectile will move in a circle along the inner wall of the tank and will not fall. Only in the vertical position, when the centrifugal force on the projectile is less than the gravity, the projectile will fall under the combined action of gravity and centrifugal force. Therefore, the radius r of the tank is related to the linear velocity of the projectile. Satisfy the formula .
[0019] The rotating shaft adopts a spline shaft, and the clamping mechanism consists of an annular boss, a sleeve, a clamping plate and bolts. The inner side of the annular boss and the sleeve are provided with keyways that match the rotating shaft, which facilitates the rapid installation and positioning of the clamping mechanism on the rotating shaft. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a cross-sectional view of the present invention.
[0021] Figure 2 This is a schematic diagram of the seepage tank body.
[0022] Figure 3 It is a schematic diagram of the transmission mechanism of the present invention.
[0023] Figure 4 This is a schematic diagram of the third bevel gear.
[0024] Figure 5 Schematic diagram of the annular boss.
[0025] Figure 6 Schematic diagram of the shaft sleeve.
[0026] Figure 7 Schematic diagram of the rotation axis.
[0027] Figure 8 Schematic diagram of flange sleeve.
[0028] Markings in the figure: 1-third bevel gear; 2-second coupling; 3-flange sleeve; 4-left end cover; 5-insulation box; 6-tank body; 6a-baffle; 7-clamping plate; 8-bolt; 9-right sealing plate; 10-right end cover; 11-support shaft; 12-bearing; 13-right cover plate; 14-sleeve; 15-bolt; 16-annular boss; 17-rotating shaft; 18-heating plate; 19-projectile; 20-left sealing plate; 21-first coupling; 22-left cover plate; 23-bearing; 24-first bevel gear; 25-input shaft; 26-fixed frame; 27-second bevel gear. DETAILED DESCRIPTION Example 1
[0029] The present invention will be further described below with reference to specific embodiments. Figure 1-Figure 8 , a surface nano-powder metal infiltration device, including an infiltration tank, a transmission mechanism and a clamping mechanism, characterized in that the transmission mechanism is composed of a fixed frame 26, an input shaft 25, a first bevel gear 24, a second bevel gear 27 and a third bevel gear 1, the first bevel gear 24 is fixed on the input shaft 25, the second bevel gear 27 is installed on the fixed frame 26 and can rotate around the axis, the third bevel gear 1 passes through the fixed frame 26 and is connected to the flange sleeve 3 through the second coupling 2, and can rotate around the input shaft 25, the input shaft 25 passes through the third bevel gear 1 and the flange sleeve 3 through the first coupling 21 and is connected to the rotating shaft 17; the infiltration tank is composed of a left end cover 4, a tank body 6 and a right end cover 10, The inner surface of the tank body 6 is evenly provided with baffles 6a, the left end cover 4 is fixedly connected to the flange sleeve 3, the right end cover 10 is connected to the support shaft 11 by bolts, the support shaft 11 is installed on the right cover plate 13 of the heat preservation box through a bearing, a heating plate 18 is arranged between the tank body 6 and the heat preservation box 5, a left sealing plate 20, a right sealing plate 9 and a clamping mechanism are arranged on the rotating shaft 17 inside the tank body 6, the workpiece is installed on the clamping mechanism, the left sealing plate 20 and the right sealing plate 9 are clearance fit with the inner surface of the tank body 6, a projectile 19 and a penetrant are arranged between the left sealing plate 20 and the right sealing plate 9, the linear velocity of the projectile 19 is 2.5m / s, and the radius r of the tank body 6 and the linear velocity V of the projectile 19 satisfy the formula The radius of the tank 6 is taken as 0.65m.
[0030] The rotating shaft 17 is a spline shaft.
[0031] The clamping mechanism is composed of an annular boss 16 , a shaft sleeve 14 , a clamping plate 7 and a bolt 8 . The inner sides of the annular boss 16 and the shaft sleeve 14 are both provided with keyways that cooperate with the rotating shaft 17 .
[0032] The modules and the numbers of teeth of the first bevel gear 24 , the second bevel gear 27 and the third bevel gear 1 are respectively equal.
[0033] The left end cover 4 and the right end cover 10 are fixed to both ends of the tank body 6 by bolts.
[0034] The left cover plate 22 and the right cover plate 13 are fixed to both ends of the heat preservation box 5 by bolts.
[0035] The left sealing plate 20 and the right sealing plate 9 are fixed to the rotating shaft 17 by bolts.
[0036] The gaps between the left sealing plate 20 and the right sealing plate 9 and the inner surface of the tank body 6 are smaller than the diameter of the penetrant.
[0037] The diameter of the projectile is 2 mm.
[0038] The included angle between the baffle 6a and the inner wall of the tank body 6 is 30°.
[0039] The penetrant is composed of pure metal powder, filler and catalyst. The composition ratio of the penetrant is as follows by weight percentage: 40% pure metal powder, 57% filler and 3% catalyst.
[0040] The metal powder is aluminum powder or chromium powder, the filler is aluminum oxide, the catalyst is chloride, and the powder particle size is 100 meshes.
[0041] The working principle is: the motor drives the rotating shaft and the first bevel gear to rotate through the input shaft, the first bevel gear meshes with the second bevel gear, the second bevel gear meshes with the third bevel gear, and the third bevel gear drives the tank body to rotate in the opposite direction. The baffles evenly arranged inside the infiltration tank are used to drive the projectiles and the penetrant to move. When the infiltration tank rotates to a certain angle, the projectiles are thrown down under the combined action of gravity and centrifugal force, impacting the surface of the workpiece, causing it to produce thermoplastic deformation and form a nanolayer. The infiltration tank is filled with a penetrant to achieve simultaneous formation of material surface defects and element diffusion. Example 2
[0042] The present invention will be further described below with reference to specific embodiments. Figure 1-Figure 8A surface nano-powder metal infiltration device, comprising an infiltration tank, a transmission mechanism and a clamping mechanism, characterized in that the transmission mechanism is composed of a fixed frame 26, an input shaft 25, a first bevel gear 24, a second bevel gear 27 and a third bevel gear 1, the first bevel gear 24 is fixed on the input shaft 25, the second bevel gear 27 is installed on the fixed frame 26 and can rotate around the axis, the third bevel gear 1 passes through the fixed frame 26 and is connected to the flange sleeve 3 through the second coupling 2, and can rotate around the input shaft 25, the input shaft 25 passes through the third bevel gear 1 and the flange sleeve 3 through the first coupling 21 and is connected to the rotating shaft 17; the infiltration tank is composed of a left end cover 4, a tank body 6 and a right end cover 10 The inner surface of the tank body 6 is evenly provided with baffles 6a, the left end cover 4 is fixedly connected to the flange sleeve 3, the right end cover 10 is connected to the support shaft 11 by bolts, the support shaft 11 is installed on the right cover plate 13 of the heat preservation box through a bearing, a heating plate 18 is arranged between the tank body 6 and the heat preservation box 5, a left sealing plate 20, a right sealing plate 9 and a clamping mechanism are arranged on the rotating shaft 17 inside the tank body 6, the workpiece is installed on the clamping mechanism, the left sealing plate 20 and the right sealing plate 9 are clearance-matched with the inner surface of the tank body 6, a projectile 19 and a penetrant are arranged between the left sealing plate 20 and the right sealing plate 9, the linear velocity of the projectile 19 is 10m / s, and the radius r of the tank body 6 is proportional to the linear velocity of the projectile 19 Satisfy the formula The radius of the tank 6 is taken as 10.5 m.
[0043] The rotating shaft 17 is a spline shaft.
[0044] The clamping mechanism is composed of an annular boss 16 , a shaft sleeve 14 , a clamping plate 7 and a bolt 8 . The inner sides of the annular boss 16 and the shaft sleeve 14 are both provided with keyways that cooperate with the rotating shaft 17 .
[0045] The modules and the numbers of teeth of the first bevel gear 24 , the second bevel gear 27 and the third bevel gear 1 are respectively equal.
[0046] The left end cover 4 and the right end cover 10 are fixed to both ends of the tank body 6 by bolts.
[0047] The left cover plate 22 and the right cover plate 13 are fixed to both ends of the heat preservation box 5 by bolts.
[0048] The left sealing plate 20 and the right sealing plate 9 are fixed to the rotating shaft 17 by bolts.
[0049] The gaps between the left sealing plate 20 and the right sealing plate 9 and the inner surface of the tank body 6 are smaller than the diameter of the penetrant.
[0050] The diameter of the projectile is 4 mm.
[0051] The included angle between the baffle 6a and the inner wall of the tank body 6 is 60°.
[0052] The penetrant is composed of alloy powder, filler and catalyst. The composition ratio of the penetrant is as follows by weight percentage: alloy powder 75%, filler 20%, catalyst 5%.
[0053] The alloy powder is chromium-aluminum, the filler is alumina, the catalyst is chloride plus rare earth, and the powder particle size is 300 mesh.
[0054] The working principle is: the motor drives the rotating shaft and the first bevel gear to rotate through the input shaft, the first bevel gear meshes with the second bevel gear, the second bevel gear meshes with the third bevel gear, and the third bevel gear drives the tank body to rotate in the opposite direction. The baffles evenly arranged inside the infiltration tank are used to drive the projectiles and the penetrant to move. When the infiltration tank rotates to a certain angle, the projectiles are thrown down under the combined action of gravity and centrifugal force, impacting the surface of the workpiece, causing it to produce thermoplastic deformation and form a nanolayer. The infiltration tank is filled with a penetrant to achieve simultaneous formation of material surface defects and element diffusion.
Claims
1. A surface nano-powder metal infiltration device, comprising an infiltration tank, a transmission mechanism and a clamping mechanism, characterized in that: The transmission mechanism is composed of a fixed frame (26), an input shaft (25), a first bevel gear (24), a second bevel gear (27) and a third bevel gear (1); the first bevel gear (24) is fixed on the input shaft (25); the second bevel gear (27) is mounted on the fixed frame (26) and can rotate around the axis; the third bevel gear (1) passes through the fixed frame (26) and is connected to the flange sleeve (3) through the second coupling (2) and can rotate around the input shaft (25); the input shaft (25) passes through the third bevel gear (1) and is connected to the flange sleeve (3) through the first coupling (21) and is connected to the rotating shaft (17); the seepage tank is composed of a left end cover (4), a tank body (6) and a right end cover (10); baffles (6a) are evenly arranged on the inner surface of the tank body (6) The left end cover (4) is fixedly connected to the flange sleeve (3), the right end cover (10) is connected to the support shaft (11) by bolts, the support shaft (11) is mounted on the right cover plate (13) of the heat preservation box by bearings, a heating plate (18) is arranged between the tank body (6) and the heat preservation box (5), a left sealing plate (20), a right sealing plate (9) and a clamping mechanism are arranged on the rotating shaft (17) inside the tank body (6), the workpiece is mounted on the clamping mechanism, the left sealing plate (20) and the right sealing plate (9) are clearance-fitted with the inner surface of the tank body (6), a projectile (19) and a penetrant are arranged between the left sealing plate (20) and the right sealing plate (9), the linear velocity of the projectile (19) is 2.5-10 m / s, and the radius r of the tank body (6) is proportional to the linear velocity of the projectile (19). Satisfy the formula .
2. A surface nano-powder metallization device according to claim 1, characterized in that: The rotating shaft (17) is a spline shaft.
3. The surface nano-powder metallization device according to claim 1, characterized in that: The clamping mechanism is composed of an annular boss (16), a shaft sleeve (14), a clamping plate (7) and a bolt (8); the inner sides of the annular boss (16) and the shaft sleeve (14) are both provided with keyways that cooperate with the rotating shaft (17).
4. The surface nano-powder metallization device according to claim 1, characterized in that: The modules and the numbers of teeth of the first bevel gear (24), the second bevel gear (27) and the third bevel gear (1) are respectively equal.
5. The surface nano-powder metallization device according to claim 1, characterized in that: The left end cover (4) and the right end cover (10) are fixed to the two ends of the tank body (6) by means of bolts.
6. The surface nano-powder metallization device according to claim 1, characterized in that: The left cover plate (22) and the right cover plate (13) are fixed to both ends of the heat preservation box (5) by means of bolts.
7. The surface nano-powder metallization device according to claim 1, characterized in that: The left sealing plate (20) and the right sealing plate (9) are fixed to the rotating shaft (17) by bolts.
8. The surface nano-powder metallization device according to claim 1, characterized in that: The gaps between the left sealing plate (20) and the right sealing plate (9) and the inner surface of the tank body (6) are smaller than the diameter of the penetrant.
9. The surface nano-powder metallization device according to claim 1, characterized in that: The diameter of the pellet is 2-4 mm.
10. The surface nano-powder metallization device according to claim 1, characterized in that: The included angle between the baffle (6a) and the inner wall of the tank body (6) is 30° to 60°.
11. The surface nano-powder metallization device according to claim 1, characterized in that: The penetrant is composed of pure metal powder or alloy powder, filler and catalyst. The composition ratio of the penetrant is as follows by weight percentage: 50-70% pure metal powder or alloy powder, 20-49% filler and 1-10% catalyst.
12. The surface nano-powder metallization device according to claim 11, characterized in that: The metal powder is zinc powder, aluminum powder, copper powder or manganese powder, the alloy powder is chromium-aluminum, iron-zinc, iron-aluminum or aluminum-rare earth alloy, the filler is aluminum oxide or silicon oxide, the catalyst is chloride or fluoride, and the powder particle size is 100-300 meshes.
Citation Information
Patent Citations
Surface nanocrystallization method capable of accelerating vacuum carburizing rate
CN108179374A
Mechanical energy assisted nanocrystallization thermal diffusion infiltration device
CN114318214A