Multi-point shape-adjusting spinning forming numerical simulation research method
The numerical simulation method for multi-point shape adjustment spinning forming addresses the inefficiencies of existing methods by using a bilinear hardening model and Coulomb friction theory, enabling accurate and efficient simulation of deformation processes and thinning rate prediction.
Patent Information
- Application Number
- CN202410981454.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-22
- Publication Date
- 2024-12-06
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing finite element simulation methods for multi-point shape adjustment spinning forming are complex, inefficient, and struggle to accurately reflect the actual deformation process due to complex boundary and contact conditions, leading to lengthy calculation times.
A numerical simulation research method involving finite element modeling on the Hypermesh platform, using a bilinear hardening elastic-plastic model, setting material parameters, defining load and motion modes, applying Coulomb friction theory, and meshing with mass scaling factors to accelerate calculations while ensuring accuracy.
The method provides a reliable and efficient simulation of stress-strain distribution, allowing for optimization of material flow and parameter settings, and accurately predicts the influence of shape adjustment units on thinning rates and deformation processes.
Smart Images

Figure CN119089725A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of multi-point shape adjustment, and in particular to a numerical simulation research method for multi-point shape adjustment spinning forming. Background Art
[0002] Multi-point shaping spinning technology is a complex elastic and plastic deformation process involving geometric shapes, physical properties and boundary conditions. Although the elastic-plastic finite element method is somewhat complex in operation to simulate this forming technology, it can quickly demonstrate the spinning process in an economical and efficient way. With the rapid development of computer technology and the significant improvement of software and hardware performance in recent years, the application of finite element technology in the shaping processing industry has received widespread attention, and its application scope is also continuously expanding;
[0003] Since the spinning process is a complex nonlinear large deformation process, it is difficult for finite element simulation to fully and accurately reflect the actual deformation process. In addition, due to the relatively complex boundary conditions and contact conditions, the calculation time is particularly long. Therefore, we propose a numerical simulation research method for multi-point shape adjustment spinning forming. Summary of the invention
[0004] The purpose of the present invention is to provide a numerical simulation research method for multi-point shape adjustment spinning forming to solve the problems raised in the above-mentioned background technology.
[0005] In order to solve the above technical problems, the present invention adopts the following technical solutions:
[0006] A multi-point shaping spinning forming numerical simulation research method includes the following steps:
[0007] S1, establish finite element model: on the Hypermesh finite element platform, based on the 3D geometric model built by SolidWorks, import and build a finite element model including the double-rotating wheel, core mold, polyurethane cover layer and blank;
[0008] S2, set material model and parameters: use bilinear hardening elastic-plastic model to set material density, elastic modulus, Poisson's ratio, yield stress and shear modulus parameters;
[0009] S3, set the load and motion mode: set the core mold to rotate and move upward in a uniform linear motion, and the roller to rotate and translate along the edge of the blank, so as to cooperate with the core mold to extrude and deform the blank; set friction and contact: based on the Coulomb friction theory, set the friction coefficients between the core mold and the blank, the core mold and polyurethane, the polyurethane and the blank, and the blank and the roller, and select a suitable friction model;
[0010] S4, Meshing and Calculation Acceleration: Meshing the model and applying mass scaling factors to accelerate the calculation process; Reliability Verification: Reliability verification of the established finite element model is performed using the energy method;
[0011] S5, analysis of stress-strain field distribution: simulate and analyze the stress-strain field distribution of the formed part, as well as the influence of the number of shape adjustment units arranged in each circle on the spinning forming.
[0012] Preferably, the method further includes the step of evaluating the adjustment effect of the shape adjustment unit: analyzing the stress, strain and thinning rate after the shape adjustment unit is adjusted up or down, so as to provide a basis for subsequent material flow and parameter optimization.
[0013] Preferably, the establishment of the model in step S1 also includes simplifying the blank model, including cutting off a small area of the blank in contact with the tail top, so as to reduce the number of grids and improve calculation efficiency.
[0014] Preferably, in step S2, the specific parameters of the material model include a density of 7850 g / cm 3 , elastic modulus is 200GPa, Poisson's ratio is 0.27, yield stress is 300MPa, and shear modulus is 760MPa.
[0015] Preferably, in step S3, the rotation speed of the rotating wheel is set to 8 r / s, the feed rate is set to 0.5 mm / r, and the rotation speed of the core mold is set to 5 r / s.
[0016] Preferably, in step S3, the friction coefficient between the polyurethane and the blank is set to 0.03, and the friction coefficient between the rotating wheel and the blank is set to 0.1.
[0017] Preferably, the Coulomb friction theory assumes that there is a proportional relationship between the friction force between objects and the vertical pressure of the contact surface, and the expression is:
[0018] τ=μσn
[0019] or
[0020] Ff=μFN
[0021] Where:
[0022] τ and Ff are friction stresses; σn and FN are pressures in the normal direction of the contact surface.
[0023] Preferably, in step S5, high-quality grids are used for meshing to ensure calculation accuracy, and a quality scaling factor of 1000 is applied to accelerate the calculation process.
[0024] It can be seen without a doubt that the above-mentioned technical solution of the present application can definitely solve the technical problem to be solved by the present application.
[0025] At the same time, through the above technical solutions, the present invention has at least the following beneficial effects:
[0026] The present invention analyzes the stress-strain distribution of the formed part after the shape-adjusting unit is lowered, and explores the influence of the lowering of the shape-adjusting unit on the thinning rate. It is concluded that when the shape-adjusting unit needs to be lowered, the first circle of the shape-adjusting unit can be slightly raised to prevent the steady rotation stage from moving backward. At the same time, the thinning rate when the rotating wheel contacts the first circle for processing can be closer to the preset value. According to the simulation results, the influence of the height of the shape-adjusting unit on the thinning rate is explored. It is concluded that when the nth circle needs to be raised, the n-1th circle can also be slightly raised to be closer to the preset value. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying any creative work.
[0028] Figure 1 It is a schematic diagram of the finite element simulation process of the present invention;
[0029] Figure 2 The finite element model components and assembly drawings of the present invention;
[0030] Figure 3 is a blank grid diagram of the present invention;
[0031] Figure 4 It is the kinetic internal energy ratio diagram of the present invention;
[0032] Figure 5 It is the equivalent stress distribution cloud diagram of the present invention;
[0033] Figure 6 It is the equivalent strain distribution cloud diagram of the present invention;
[0034] Figure 7 It is a stress distribution cloud diagram of the blank under the b-type core mold of the present invention;
[0035] Figure 8 The stress curve distribution of the two core molds of the present invention;
[0036] Fig. 9 is the thinning rate of the two core molds of the present invention;
[0037] Fig.10 The flexible core mold of the present invention is lowered for the first circle;
[0038] Fig.11 This is the equivalent stress diagram of the first circle of the present invention;
[0039] Fig.12 This is an equivalent stress curve diagram of the first circle of the present invention;
[0040] Fig.13 The equivalent stress diagram of the first and second turns of the present invention is lowered;
[0041] Fig.14 It is a stress curve diagram of two lowering schemes of the present invention;
[0042] Fig.15 The equivalent stress diagram of the first, second and third turns of the present invention is lowered;
[0043] Fig.16 It is a stress curve diagram of three lowering schemes of the present invention;
[0044] Fig.17 The strain cloud diagrams of three different lowering schemes of the shape adjustment unit of the present invention;
[0045] Fig.18 It is a graph of thinning rate of three different lowering schemes of the shape adjustment unit of the present invention;
[0046] Fig.19 The stress diagrams of the shape adjustment unit of the present invention at three different height adjustments;
[0047] Fig. 20 It is the stress curve diagram of three height adjustment schemes of the present invention;
[0048] Fig.21 The strain cloud diagrams of three different height adjustment schemes of the shape adjustment unit of the present invention;
[0049] Fig. 22 It is the thinning rate curve diagram of three height adjustment schemes of the present invention. DETAILED DESCRIPTION
[0050] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0051] Example
[0052] Reference Figure 1-22 , a multi-point shaping spinning forming numerical simulation research method, comprising the following steps:
[0053] S1, establish finite element model: on the Hypermesh finite element platform, based on the 3D geometric model built by SolidWorks, import and build a finite element model including the double-rotating wheel, core mold, polyurethane cover layer and blank;
[0054] S2, set material model and parameters: use bilinear hardening elastic-plastic model to set material density, elastic modulus, Poisson's ratio, yield stress and shear modulus parameters;
[0055] S3, set the load and motion mode: set the core mold to rotate and move upward in a uniform linear motion, and the roller to rotate and translate along the edge of the blank, so as to cooperate with the core mold to extrude and deform the blank; set friction and contact: based on the Coulomb friction theory, set the friction coefficients between the core mold and the blank, the core mold and polyurethane, the polyurethane and the blank, and the blank and the roller, and select a suitable friction model;
[0056] S4, Meshing and Calculation Acceleration: Meshing the model and applying mass scaling factors to accelerate the calculation process; Reliability Verification: Reliability verification of the established finite element model is performed using the energy method;
[0057] S5, analysis of stress-strain field distribution: simulate and analyze the stress-strain field distribution of the formed part, as well as the influence of the number of shape adjustment units arranged in each circle on the spinning forming.
[0058] It also includes the step of evaluating the adjustment effect of the shape adjustment unit: analyzing the stress, strain and thinning rate after the shape adjustment unit is adjusted up or down, providing a basis for subsequent material flow and parameter optimization.
[0059] The establishment of the model in step S1 also includes simplifying the blank model, including cutting off a small area of the blank in contact with the tail top, so as to reduce the number of grids and improve the calculation efficiency.
[0060] In step S2, the specific parameters of the material model include a density of 7850 g / cm 3 , elastic modulus is 200GPa, Poisson's ratio is 0.27, yield stress is 300MPa, and shear modulus is 760MPa.
[0061] In step S3, the rotation speed of the rotating wheel is set to 8 r / s, the feed rate is set to 0.5 mm / r, and the rotation speed of the core mold is set to 5 r / s.
[0062] In step S3, the friction coefficient between the polyurethane and the blank is set to 0.03, and the friction coefficient between the roller and the blank is set to 0.1.
[0063] The Coulomb friction theory assumes that there is a proportional relationship between the friction force between objects and the vertical pressure of the contact surface, which is expressed as:
[0064] τ=μσn
[0065] or
[0066] Ff=μFN
[0067] Where:
[0068] τ and Ff are friction stresses; σn and FN are pressures in the normal direction of the contact surface.
[0069] In step S5, high-quality grids are used for meshing to ensure calculation accuracy, and a quality scaling factor of 1000 is applied to speed up the calculation process.
[0070] 1. Establishment of multi-point shaping spinning finite element model
[0071] It is very important to build an accurate finite element analysis model, which should cover the following key points: simplification and assumption, model establishment, material property setting, contact mode definition, meshing, etc. Figure 1 The complete finite element simulation process is demonstrated.
[0072] 2. Model Simplification and Assumptions
[0073] Since the spinning process is a complex nonlinear large deformation process, it is difficult for finite element simulation to fully and accurately reflect the actual deformation process. In addition, due to the relatively complex boundary conditions and contact conditions, the calculation time is particularly long. In this study, the following simplifications and assumptions are made. These assumptions and simplifications can improve the calculation efficiency while maintaining the simulation accuracy, so that the research can proceed smoothly.
[0074] (1) When establishing the billet model, a small area of the billet in contact with the tail top is cut off to reduce the number of grids and improve the calculation efficiency.
[0075] (2) The entire spinning process is completed at room temperature, so the influence of temperature is not considered.
[0076] (3) When defining the contact, it is assumed that the axial sliding friction and circumferential rolling friction between the wheel and the blank can be uniformly represented by Coulomb friction.
[0077] (4) When defining the constraints, the “tie” method is used to connect the blank directly to the core mold, eliminating the need to model the tail top separately, while keeping the movement of the blank completely synchronized with the core mold.
[0078] (5) In actual production, the shape adjustment unit needs to be connected to the core mold through threads and reinforced with glass glue. In order to save calculation time, the shape adjustment unit and the core mold are modeled as one in the simulation process.
[0079] (6) Since the present invention covers the surface of the shape adjustment unit with polyurethane to smooth the gap and improve the surface quality, the cutting angle of the shape adjustment unit on the blank will not be too large, and the selected shape adjustment unit is a hemisphere. However, when adjusting its shape, the height needs to be lowered or raised. Since the shape adjustment unit is connected to the core mold by threads, in order to facilitate modeling, the threaded parts are all replaced by the shape adjustment unit.
[0080] (7) To speed up the calculation, a mass scaling factor of 1000 was used in the model, which is one of the common methods to speed up the calculation, especially when the influence of strain rate is not considered.
[0081] 3. Model Building
[0082] The double rotating wheels have the characteristic of stable rotation, so the present invention adopts the method of symmetrically distributing the two rotating wheels, creates a corresponding three-dimensional geometric model in the SolidWorks modeling software, and imports the constructed parts into the Hypermesh finite element analysis software.
[0083] The present invention first takes 3 circles of shape adjustment units, whose diameter is 2mm, and the distribution position of the shape adjustment units along the generatrix is 0.03mm. In addition, the two wheels are defined as rigid bodies, and the polyurethane covered on the surface of the core mold is defined as an elastic body, and the blank is a deformable body. The various components after definition and the assembly model are as follows Figure 2 shown.
[0084] 4. Material model and load settings
[0085] (1) Material model
[0086] The present invention uses a bilinear hardening elastoplastic model, also known as an ideal linear hardening elastoplastic model, which is a commonly used classic simplified material model. The equivalent stress and equivalent strain of the formed part are analyzed. Its mechanical parameters are shown in Table 1 below.
[0087] Table 1 Material parameters
[0088]
[0089] (2) Load application
[0090] The spinning method of the multi-point shaping spinning model in the present invention is that the core mold rotates and moves upward in a uniform linear motion toward the blank to replace the movement of the two rollers along the generatrix of the conical core mold. The two rollers rotate and translate along the edge direction of the blank (xy plane). In this motion mode, the core mold is used to extrude and deform the blank to complete the conical strong spinning. The rotation speed of the roller is set to 8r / s, and the rotation speed of the core mold is set to 5r / s according to the feed rate of 0.5mm / r.
[0091] Friction and contact settings
[0092] In the spinning process, there is friction between the core mold and the blank, the core mold and polyurethane, the polyurethane and the blank, and the blank and the two spinning wheels. The friction coefficient between polyurethane and the blank is 0.03, and the friction coefficient between the spinning wheel and the blank is 0.1. At the same time, choosing a suitable friction model is crucial for the reliability of the spinning process. This study is based on the Coulomb friction theory to explain the friction phenomenon of the contact surface of objects. The theory assumes that there is a proportional relationship between the friction force between objects and the vertical pressure on the contact surface, and its expression is:
[0093] τ=μσn(1)
[0094] or
[0095] Ff=μFN(2)
[0096] Where:
[0097] τ, Ff—friction stress; σn, FN—pressure in the normal direction of the contact surface.
[0098] The contact characteristics in the spinning process are extremely complex. The workpiece will be locally deformed under the pressure and shear force of the spinning wheel. As the spinning wheel gradually advances, the contact position between the workpiece and the mold also changes accordingly. In order to simplify the model, the tie constraint in Hypermesh is used to ensure that the degrees of freedom of the blank and the core mold are consistent.
[0099] Table 2 shows the three contact pairs and the constraints between the core mold and the blank, and between the core mold and the polyurethane are tie constraints, and the contact type is face-to-face. Specifically, both the roller 1 and the roller 2 are in contact with the blank, and the polyurethane is also in contact with the blank. In addition, the contact part from the center of the blank to the top of the core mold, as well as the contact area between the polyurethane and the core mold, are fixed by tie constraints. When establishing the contact pair, in order to avoid the occurrence of interlayer penetration, the primary contact surface should be set to a surface with high rigidity or hardness, and the secondary contact surface should be designed as a deformable material.
[0100] Table 2 Contact pairs and tie constraints
[0101]
[0102] 5. Grid Division
[0103] The multi-point spinning curved surface forming process mainly studies the forming performance of sheet metal, and it is necessary to analyze factors affecting stress, plastic deformation, thickness, etc. In order to speed up the calculation, the blank is set as a deformable shell unit, the polyurethane is set as a solid unit, and the other parts are set as rigid shell units.
[0104] Theoretically, the more meshes are divided, the greater the model mesh density is, and the more accurate the result is. However, after exceeding a certain value, not only is the accuracy not greatly improved, but the time cost is also increased. Finite element analysis aims to restore mathematical models to actual engineering models. Meshing affects the calculation results and scale, so it is necessary to adopt appropriate mesh types and division techniques. In the present invention, when dividing the mesh of the blank in Hypermesh finite element software, a hybrid method of using quadrilaterals as the main and triangles as the auxiliary is used for mesh division, and the mesh size is selected as 0.05mm. Figure 3 The figure shows the mesh diagram of the billet. After the billet is meshed, the number of nodes is 10703 and the number of meshes is 10590.
[0105] 6. Model Validation
[0106] This study uses a dynamic display algorithm to analyze the spinning process. In order to improve the calculation efficiency, a mass magnification factor is introduced in the process. To ensure the accuracy of the analysis model, the energy balance principle is used to verify the stability of the obtained model. By plotting the ratio of kinetic energy to internal energy over time, when this ratio is far less than 5%, it means that the model follows the quasi-static conditions, thereby verifying the reliability of the results.
[0107] like Figure 4 As shown, it is a graph showing the change of the kinetic energy to internal energy ratio. It can be seen that during the spinning process, the ratio is less than 1%, so the constructed model meets the quasi-static simulation conditions.
[0108] 7. Material deformation characteristics analysis
[0109] The present invention mainly analyzes the stress and strain distribution law of conical parts spinning, and the main specific model parameters are shown in Table 3.
[0110] Table 3 Model parameters
[0111]
[0112] 8. Equivalent stress distribution analysis
[0113] Figure 5This is a cloud diagram of the equivalent stress distribution during the forming process. From the figure, it can be seen intuitively that the position where the maximum equivalent stress appears is always the contact position between the blank and the rotating wheel, and the rotating wheel rotates and performs circumferential linear motion. Therefore, as the rotating wheel feeds, its maximum stress position also begins to change downward, and the minimum equivalent stress is always maintained at the position where the blank is clamped by the tail top and the core mold. And during the entire spinning process, the equivalent stress of the conical part gradually distributes in a ring shape from the center to the outside as the spinning begins, and is relatively symmetrically distributed with the two rotating wheels as the symmetry planes. The equivalent stress values along the circumference of the blank are relatively uniform. The maximum stress value has been fluctuating within a certain range. This is because polyurethane is an elastomer. When the rotating wheel is processed to the highest point of the shape adjustment unit, the corresponding contact position of the rotating wheel and the shape adjustment unit becomes smaller, and the thickness of the blank will change, so the stress will increase. When it is processed to other positions, the stress will decrease, so the stress value will fluctuate. From Figure 5 (a) shows that as the multi-point shaping spinning is carried out, the axial part of the processed area shows a significant increase in stress. This phenomenon is mainly attributed to the stretching and bending effect of the spinning wheel on the metal in the pre-processing area. Gradually, when the spinning enters the steady spinning stage, the stress level in the formed area shows a relatively small change, and the maximum stress value near the contact point with the spinning wheel is maintained in a stable range. In all the figures, another notable phenomenon is that two relatively high stress areas appear in the unformed area below the axial direction and behind the circumference of the spinning wheel. This happens because the core mold and the tail top simultaneously fix the blank for rotation, while the spinning wheel performs a feeding action, thereby producing a crushing effect on the flange.
[0114] IX. Equivalent strain distribution analysis
[0115] During the spinning process of the multi-point shape-adjusting conical parts, the deformation process of the workpiece is divided into four main stages. After the spinning is completed, the inner surface of the conical part is closely attached to the outer surface of the polyurethane. Figure 6The equivalent strain distribution characteristics of the multi-point shape-adjusting spinning cone in four different forming stages are shown. It can be clearly seen from the image that the equivalent plastic strain is relatively stable during the entire spinning process of the cone, and is distributed in an annular layer from the center of the blank to the outside, and each layer is uniform, and the equivalent plastic strain value gradually increases, indicating that the design of the model, contact conditions, boundary conditions and other settings are all reasonable. Among them, the maximum equivalent strain is mainly concentrated in the area where the workpiece and the spinning wheel are in direct contact, specifically in the circumferential position. The main factor of this phenomenon is that the spinning wheel always pushes forward along the generatrix direction of the core mold during the forming process to produce an extrusion effect on the workpiece. In the area of contact behind the spinning wheel, the workpiece material is jointly affected by the lateral cutting force and the longitudinal bending force. It can be observed from the four figures that the equivalent plastic strain generated in the shearing area is significantly lower than that in the bending area. This comparison result shows that the degree of deformation in the bending process is higher than the shear deformation, thereby proving the suitability of the selected spinning wheel edge radius.
[0116] 10. Influence of shape adjustment unit arrangement on forming results
[0117] In the previous modeling, 2mm shaping units were designed and evenly distributed on the core mold. The number was selected according to the number of the core mold that covers one circle. The number of the first circle was 52, the second circle was 57, and the third circle was 62. Therefore, the present invention continues to use finite element analysis software to perform numerical simulation on the multi-point shaping spinning cone process, taking the number of the first circle of shaping units as 51, the second circle as 56, and the third circle as 61, in order to find out the influence of the shaping units on the forming results. For the convenience of description, the first core mold is named as a-type core mold, and the second core mold is named as b-type core mold.
[0118] Figure 7 The Mi Se stress distribution cloud diagram of the forming result of the b-type core mold in the conical part spinning model. It can be seen from the figure that when the b-type core mold is used, the stress distribution, maximum stress position, minimum stress position, etc. are almost the same as those of the a-type core mold. During the spinning process, the maximum stresses in the previous a-type core mold in several stages were 563MPa, 688MPa, 720MPa, and 580MPa, respectively, and its stress value changed greatly compared with the a-type core mold.
[0119] from Figure 8From the analysis of the change of equivalent stress, it can be seen that the equivalent plastic strain of the b-type core mold during the spinning process is also quite close to that of the a-type. The stress increases at the beginning of spinning, and the stress fluctuates during the processing. This is because the corresponding positions of the rotating wheel and the adjusting core mold have changed, and the overall stability is relatively stable. However, in the 25%-50% and 75%-100% stages of the forming stage, the maximum stress value of the b-type core mold increases suddenly. This is because the number of adjusting units is reduced, and the corresponding contact position between the rotating wheel and the core mold is reduced, causing the blank to accumulate, and then with the feeding of the rotating wheel, the stress value increases suddenly. Due to the occurrence of this phenomenon, the thinning rate to determine whether the structure is reasonable is analyzed next.
[0120] The allowable deviation range of the blank during the conical part spinning process is -10% to 5%. Fig. 9 It can be seen that the deviation rate of the thinning rate of the a-type core mold is within the allowable range, which shows the rationality of the model design. However, the deviation rate of the b-type core mold in the 25%-50% and 75%-100% spinning forming stages is greater than the maximum value of 25% in the allowable range. Therefore, the structure is unreasonable, so the influence of the number of shape adjustment units on the blank forming is no longer considered.
[0121] 11. Analysis and influence of lowering the profile unit on forming
[0122] The previous study investigated the effect of the number of shape adjustment units in each circle on the forming process. Next, the effect of the height change of the shape adjustment unit on the thinning rate was studied. Since the thickness of the blank is 0.6mm and the preset thinning rate is 20%, the height of the shape adjustment unit can only be lowered by 0.12mm at most. In summary, the shape adjustment unit is fine-tuned without changing the blank thickness and the positioning of the rotary wheel, and its influence on the stress, strain distribution and thinning rate is analyzed. First, the effect of lowering the shape adjustment unit by 0.01mm on the forming result is explored.
[0123] Stress analysis after the shape adjustment unit is lowered
[0124] (1) Analysis of stress after reducing the first circle
[0125] First, the first circle of the shape adjustment unit is lowered by 0.01 mm. The schematic diagram and three-dimensional model of the flexible core mold after the lowering are as follows: Fig.10 As shown in the figure, the distance between the line segment AB parallel to the first circle of shape adjustment units and the rigid conical core mold is the height to which the shape adjustment units are lowered.
[0126] The same finite model modeling settings as before were used to numerically simulate the spinning process, and the following results were obtained: Fig.11The results are shown. It can be seen intuitively from the figure that the position where the maximum equivalent stress appears is still the same as the position of the initial model, which is always at the contact position between the blank and the rotating wheel, and the minimum equivalent stress is also always maintained at the position where the blank is clamped by the tail top and the core mold. And during the entire spinning process, the equivalent stress of the conical part gradually distributes in a ring shape from the center to the outside as the spinning begins, and is relatively symmetrically distributed with the two rotating wheels as the symmetry planes. The equivalent stress values along the circumference of the blank are relatively uniform. At the beginning of forming, that is, it first contacts with the shaping unit after the first circle is lowered. Because the thinning rate is small, its stress value is also relatively small. Then it gradually contacts with the second circle, and the equivalent stress value gradually increases, which is in line with the forming law after lowering the shaping unit.
[0127] Fig.12 The equivalent stress curve is shown in Figure 1. As the spinning process progresses, the equivalent stress value increases and is relatively stable. Since the adjustment spacing of the shaping unit is small, the stress value changes relatively little, but it is greater than the previous forming stage from the 50% forming stage to the 100% forming stage.
[0128] (2) Analysis of stress after two turns of adjustment: The same as the operation setting of adjusting the shape adjustment unit by one turn, the shape adjustment unit of the first two turns is adjusted down by 0.1 mm respectively, and the following is obtained: Fig.13 The stress distribution diagram is shown.
[0129] It can be seen from the figure that when the shape adjustment unit is lowered by the first circle, the distribution law is the same as when it is lowered by the first and second circles, and the positions of the maximum stress value and the minimum stress value are the same. And when the rotating wheel gradually contacts the second circle to the third circle, the equivalent stress value gradually increases.
[0130] According to the two different adjustments of the shaping unit, the stress curve of the forming process is compared. Fig.14 As shown in the figure, it can be seen that the change trend of the major diameter is the same, both of which increase to a certain value first and then decrease. The stress values when the lowered part is spun are smaller than when the height of the shaping unit does not change, but the whole forming process is relatively stable without much fluctuation and change.
[0131] (3) Analysis of stress after three turns of reduction
[0132] Since the present invention sets three circles of shape adjustment units, the influence of the changes of the three circles of shape adjustment units on the stress is analyzed. The model is changed according to the above settings, and then finite element simulation is performed to obtain the following: Fig.15 The stress distribution cloud diagram is shown. It can be seen from the figure that the positions where the maximum and minimum stress values appear are always the same, and the stress distribution is relatively uniform during the entire spinning process.
[0133] from Fig.16It can be seen from the three stress curves shown that when the shape-adjusting unit is lowered by two circles and three circles, the stress values are almost the same. The reason is that the height change of the shape-adjusting unit itself is not large, and the number of circles lowered is also close.
[0134] However, from the careful observation of the figure, it can be seen that when the three circles of the shaping unit are all lowered, the stress value is relatively more stable. After analyzing the stress of the above three shaping unit lowering schemes, no defects appeared in the formed parts and flange parts, which shows the rationality of forming after the shaping unit height adjustment and the feasibility of this scheme.
[0135] Strain analysis after the shape adjustment unit is lowered
[0136] like Fig.17 As shown in the figure, the strain cloud diagrams of the three shaping units after being adjusted down are shown. It can be seen from the figure that the equivalent plastic strain of the three different adjustment schemes of the shaping unit is relatively stable during the spinning forming process, and is gradually distributed in layers from the center of the blank to the outside, and each layer is annular and uniform, which shows the rationality of the shaping scheme.
[0137] As can be seen in Figure (a), after the first circle shaping unit is lowered, the strain at the second and third circles is larger, and the steady spinning stage is pushed back. As can be seen in Figure (b), the strain distribution is obviously more uniform than the first shaping scheme. As can be seen from Figure (c), the overall strain change is relatively more uniform, because the flexible core mold does not change from the beginning to the end of the spinning process, and the thinning rate of the blank remains unchanged during the whole process, so that the strain range is small and uniform.
[0138] The influence of lowering the shape adjustment unit on the thinning rate
[0139] In order to better explore the influence of the shaping unit lowering on the wall thickness of the spinning part during the whole process of multi-point shaping spinning, the present invention selects the thinning rate index and obtains the following results based on the above numerical simulation results: Fig.18The thinning rate curve is shown in the figure. It can be seen from the figure that the thinning rates of the three different lowering schemes of the shape adjustment unit are similar and the variation range is not large. When the shape adjustment unit is lowered, its maximum thinning rate and minimum thinning rate are both within the allowable range of the deviation rate, which shows the rationality of the design. The first 25% forming stage is the covered polyurethane, so its thinning rate does not fluctuate much and keeps increasing. Then it is fed to the 40% stage, that is, the highest point of the first circle of the shape adjustment unit participates in the processing. In this process, the thinning rate fluctuates between 12% and 14%, and there is a certain small gap from the standard thinning rate of 18.3% of the adjusted height. The 40% to 70% forming stage is the position from the highest point of the first circle of the shape adjustment unit to the highest point of the second circle, and finally the spinning forming stage from the highest point of the second circle of the shape adjustment unit to the third circle of the shape adjustment unit. From the whole figure, it can be seen that the stable spinning stage of multi-point shape adjustment spinning moves backward as the shape adjustment unit is lowered, and the final stable spinning stage is when it starts to contact with the second circle of the shape adjustment unit. In actual use, since the first circle position of the shaping unit is close to the rounded corner position, the thinning rate change is not significant when only the first circle of the shaping unit is adjusted. If the second and third circles need to be lowered, the original position of the first circle of the shaping unit can be appropriately raised to obtain a formed part that is closer to the preset thinning rate value. At the same time, there will be no backward shift in the steady rotation stage, and the positive deviation phenomenon in this stage will also be improved accordingly.
[0140] Analysis and influence of height adjustment and shape adjustment unit on forming
[0141] The present invention explores the influence of the shape adjustment unit on the stress, strain and thinning rate of the formed part after the shape adjustment unit is adjusted by 0.01 mm.
[0142] Stress analysis after the height adjustment of the shaping unit requires corresponding adjustments to the height of the shaping unit on the flexible core mold of the model and the polyurethane covering it. The height of the first circle, the first and second circles, and the first, second and third circles are adjusted respectively. The equivalent stress distribution cloud diagram after the height adjustment is as follows Fig.19 shown.
[0143] From the figure, we can see that the positions of the maximum equivalent stress and minimum stress of the three different height adjustment of the shaping unit remain unchanged, and all appear in the contact between the blank and the rotating wheel and the clamping part of the tail top. The equivalent stress distribution of (a), (b), and (a) in the figure is relatively uniform, and is also symmetrically distributed with the two rotating wheels as the symmetry plane. From the above analysis, it can be seen that when the shaping unit is adjusted
[0144] The formed parts obtained after the unit height adjustment are reasonable and conform to the forming law. Fig. 20It can be seen that when the shaping unit is raised, the stress value fluctuation range is larger than when it is lowered. The reason is that when the shaping unit is raised, the distance between the rotating wheel and the shaping unit on the core mold becomes smaller. Overall, the stress value changes of the three shaping schemes are relatively close, without much fluctuation. When only the first circle is raised, the stress values in the later stage are smaller than those of the other two shaping schemes. Among the three shaping schemes, the stress value change range of the second and third ones is relatively smaller.
[0145] Strain analysis after height adjustment of the shape adjustment unit
[0146] like Fig.21 Shown are the strain cloud diagrams after three different height adjustments of the shape adjustment unit. It can be seen from the figure that the equivalent plastic strain in the spinning forming process of the three different height adjustment schemes of the shape adjustment unit is relatively stable and the distribution is relatively uniform, which illustrates the rationality of the height adjustment scheme of the shape adjustment unit.
[0147] In Figure (a), only the first circle of shape adjustment units were adjusted, and the shape adjustment units were close to the fillet, so the strain did not change much during the process. In Figure (b), the position with a larger strain value appeared at the position of the second circle of shape adjustment units. From Figure (c), it can be seen that compared with the second adjustment scheme, the range of large strain changes has increased. This is because compared with the second scheme, the third circle was also adjusted higher, which is in line with the forming law.
[0148] The influence of height adjustment of the shaping unit on the thinning rate
[0149] Also taking the thinning rate as an indicator, according to the above numerical simulation results, we get Fig. 22 The thinning rate curve is shown.
[0150] It can be seen from the figure that the thinning rates of the three height adjustment schemes are all within the allowable range of the deviation rate, which shows the rationality of the structural design. When the shape adjustment unit is raised by the first circle, the rotary wheel feeds to the highest point of the first circle shape adjustment unit, corresponding to the third peak in the figure, it can be seen from the figure that the three height adjustment schemes all have peaks here, and then the thinning rate decreases due to the lower contact position corresponding to the shape adjustment unit, until the contact area with the second circle, that is, the 40% to 70% forming stage, the thinning rate is relatively stable and decreases, and finally the thinning rate increases slightly when it contacts the third circle. When the first and second circles are raised, the whole process is close to the preset value. When it contacts the third circle, the thinning rate gradually approaches 20% because the height of the third circle shape adjustment unit is not adjusted. When the first, second, and third circles of the shape adjustment unit are raised respectively, the value in the first stage is closer to the preset thinning rate value, and the value in the latter stage decreases, forming a negative deviation. According to the obtained rules, if the nth circle needs to be adjusted higher in actual use, the n-1th circle can also be slightly adjusted higher to be closer to the preset value.
[0151] Based on the above, it can be seen that through the above settings, this application can certainly achieve the following technical effects:
[0152] The present invention analyzes the stress-strain distribution of the formed part after the shape-adjusting unit is lowered, and explores the influence of the lowering of the shape-adjusting unit on the thinning rate. It is concluded that when the shape-adjusting unit needs to be lowered, the first circle of the shape-adjusting unit can be slightly raised to prevent the steady rotation stage from moving backward. At the same time, the thinning rate when the rotating wheel contacts the first circle for processing can be closer to the preset value. According to the simulation results, the influence of the height of the shape-adjusting unit on the thinning rate is explored. It is concluded that when the nth circle needs to be raised, the n-1th circle can also be slightly raised to be closer to the preset value.
[0153] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection, an electrical connection, or communication with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0154] Obviously, the embodiments described above are only some embodiments of the present invention, rather than all embodiments. The preferred embodiments of the present invention are given in the accompanying drawings, but they do not limit the patent scope of the present invention. The present invention can be implemented in many different forms. On the contrary, the purpose of providing these embodiments is to make the understanding of the disclosure of the present invention more thorough and comprehensive. Although the present invention has been described in detail with reference to the aforementioned embodiments, for those skilled in the art, it is still possible to modify the technical solutions recorded in the aforementioned specific embodiments, or to perform equivalent replacements for some of the technical features therein. Any equivalent structure made using the contents of the specification and drawings of the present invention, directly or indirectly used in other related technical fields, is also within the scope of patent protection of the present invention.
Claims
1. A numerical simulation research method for multi-point shaping spinning, characterized in that: The following steps are involved: S1, establish finite element model: on the Hypermesh finite element platform, based on the three-dimensional geometric model built by SolidWorks, import and build a finite element model including the double-rotating wheel, core mold, polyurethane cover layer and blank; S2, set material model and parameters: use bilinear hardening elastic-plastic model to set material density, elastic modulus, Poisson's ratio, yield stress and shear modulus parameters; S3, set the load and motion mode: set the core mold to rotate and move upward in a uniform linear motion, and the roller to rotate and translate along the edge of the blank, so as to cooperate with the core mold to extrude and deform the blank; set friction and contact: based on the Coulomb friction theory, set the friction coefficients between the core mold and the blank, the core mold and polyurethane, the polyurethane and the blank, and the blank and the roller, and select a suitable friction model; S4, Meshing and Computational Acceleration: Meshing the model and applying mass scaling factors to accelerate the computational process; Reliability verification: The reliability of the established finite element model is verified by the energy method; S5, analysis of stress-strain field distribution: simulate and analyze the stress-strain field distribution of the formed part, as well as the influence of the number of shape adjustment units arranged in each circle on the spinning forming.
2. A multi-point shape adjustment spinning forming numerical simulation research method according to claim 1, characterized in that: It also includes the step of evaluating the adjustment effect of the shape adjustment unit: analyzing the stress, strain and thinning rate after the shape adjustment unit is adjusted up or down, providing a basis for subsequent material flow and parameter optimization.
3. The method for numerical simulation of multi-point shape adjustment spinning forming according to claim 1 is characterized in that: The establishment of the model in step S1 also includes simplifying the blank model, including cutting off a small area of the blank in contact with the tail top, so as to reduce the number of grids and improve the calculation efficiency.
4. The method for numerical simulation of multi-point shape adjustment spinning forming according to claim 1 is characterized in that: In step S2, the specific parameters of the material model include a density of 7850 g / cm 3 , elastic modulus is 200GPa, Poisson's ratio is 0.27, yield stress is 300MPa, and shear modulus is 760MPa.
5. A multi-point shape adjustment spinning forming numerical simulation research method according to claim 4, characterized in that: In step S3, the rotation speed of the rotating wheel is set to 8 r / s, the feed rate is set to 0.5 mm / r, and the rotation speed of the core mold is set to 5 r / s.
6. The method for numerical simulation of multi-point shape adjustment spinning forming according to claim 4 is characterized in that: In step S3, the friction coefficient between the polyurethane and the blank is set to 0.03, and the friction coefficient between the roller and the blank is set to 0.
1.
7. The method for numerical simulation of multi-point shape adjustment spinning forming according to claim 1 is characterized in that: The Coulomb friction theory assumes that there is a proportional relationship between the friction force between objects and the vertical pressure of the contact surface, which is expressed as: τ=μσn or Ff=μFN Where: τ and Ff are friction stresses; σn and FN are pressures in the normal direction of the contact surface.
8. The method for numerical simulation of multi-point shape adjustment spinning forming according to claim 1 is characterized in that: In step S5, high-quality grids are used for meshing to ensure calculation accuracy, and a quality scaling factor of 1000 is applied to speed up the calculation process.
Citation Information
Cited By
Assembly deformation stress cooperative control-oriented aircraft rigid-flexible hybrid structure multi-level analysis method
CN120893252A