Preparation method of display panel, display panel and display device
The method improves OLED display panel performance by using controlled evaporation angles and substrate movement to enhance electrode overlap with isolation structures, reducing carrier crosstalk and resistance, thus enhancing display quality.
Patent Information
- Application Number
- CN202411200007.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-12-06
AI Technical Summary
Current OLED display products require improvements in performance, particularly in reducing carrier crosstalk and overlapping resistance between electrodes and isolation structures to enhance display quality.
A method involving the use of multiple evaporation chambers with controlled emission angles and substrate movement to form a first electrode layer that overlaps with an isolation structure, reducing carrier crosstalk and improving film formation continuity.
This method enhances the display effect and performance of OLED panels by increasing the overlap area and reducing resistance between electrodes and isolation structures, thereby improving overall display quality without the need for precision masks.
Smart Images

Figure CN119095458A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of display, and in particular to a method for preparing a display panel, a display panel and a display device. Background Art
[0002] Organic Light Emitting Diode (OLED) and flat panel display devices based on technologies such as Light Emitting Diode (LED) have been widely used in various consumer electronic products such as mobile phones, televisions, laptops, desktop computers, etc. due to their advantages such as high image quality, power saving, thin body and wide application range, becoming the mainstream in display devices.
[0003] However, the performance of current OLED display products needs to be improved. Summary of the invention
[0004] The embodiments of the present application provide a method for manufacturing a display panel, a display panel, and a display device, aiming to improve the performance of the display panel.
[0005] A first aspect of the present application provides a method for preparing a display panel, the method comprising:
[0006] An isolation structure is prepared on the substrate, wherein the isolation structure encloses an isolation opening;
[0007] The electrode material in the first evaporation chamber group is evaporated multiple times to one side of the isolation opening in a first direction; the first direction is parallel to the substrate; the first evaporation chamber group includes at least one first evaporation chamber;
[0008] The electrode material in the second evaporation chamber group is evaporated to the other side of the isolation opening in the first direction to form a first electrode layer, wherein the first electrode layer includes a first electrode located in the isolation opening, and the first electrode is electrically connected to the isolation structure; the second evaporation chamber group includes at least one second evaporation chamber, and the emission direction of the electrode material in the second evaporation chamber is different from the emission direction of the electrode material in the first evaporation chamber.
[0009] According to an embodiment of the first aspect of the present application, the first evaporation chamber group includes at least two first evaporation chambers, and in the step of evaporating the electrode material in the first evaporation chamber group multiple times to one side of the isolation opening in the first direction, the method further includes:
[0010] The electrode materials in at least two first evaporation chambers are evaporated into the isolation openings respectively.
[0011] According to any of the aforementioned embodiments of the first aspect of the present application, the emission directions of the electrode materials in at least two first evaporation chambers have different angles with the substrate.
[0012] According to any of the aforementioned embodiments of the first aspect of the present application, the angle between the emission direction of the electrode material in the first evaporation chamber and the substrate is greater than or equal to 30°.
[0013] According to any of the aforementioned embodiments of the first aspect of the present application, in the step of evaporating the electrode material in the first evaporation chamber group multiple times to one side of the isolation opening in the first direction, the method further includes:
[0014] The substrate is moved back and forth along the first direction so that the electrode material in the first evaporation chamber group is evaporated to the isolation opening multiple times; or,
[0015] The first evaporation chamber group is moved back and forth along a first direction, so that the electrode material in the first evaporation chamber group is evaporated to the isolation opening for multiple times.
[0016] According to any of the aforementioned embodiments of the first aspect of the present application, in the step of evaporating the electrode material in the second evaporation chamber group to the other side of the isolation opening in the first direction, the method further includes:
[0017] The electrode material in the second evaporation chamber group is evaporated to the isolation opening for multiple times at the other side of the isolation opening along the first direction.
[0018] According to any of the aforementioned embodiments of the first aspect of the present application, the second evaporation chamber group includes at least two second evaporation chambers, and in the step of evaporating the electrode material in the second evaporation chamber group multiple times to the other side of the isolation opening in the first direction, the method further includes:
[0019] The electrode materials in the at least two second evaporation chambers are evaporated into the isolation openings respectively.
[0020] According to any of the aforementioned embodiments of the first aspect of the present application, the emission directions of the electrode materials in at least two second evaporation chambers have different angles with the substrate.
[0021] According to any of the aforementioned embodiments of the first aspect of the present application, the angle between the emission direction of the electrode material in the second evaporation chamber and the substrate is less than or equal to 150°.
[0022] According to any of the aforementioned embodiments of the first aspect of the present application, in the step of evaporating the electrode material in the second evaporation chamber group multiple times to the other side of the isolation opening in the first direction, the method further includes:
[0023] The substrate is moved back and forth along the first direction so that the electrode material in the second evaporation chamber group is evaporated to the isolation opening multiple times; or,
[0024] The second evaporation chamber group is moved back and forth along the first direction, so that the electrode material in the second evaporation chamber group is evaporated to the isolation opening for multiple times.
[0025] According to any of the aforementioned embodiments of the first aspect of the present application, the evaporation source in the first evaporation chamber and / or the second evaporation chamber is a linear evaporation source, and an extension direction of the linear evaporation source is perpendicular to the first direction and parallel to the substrate.
[0026] According to any of the aforementioned embodiments of the first aspect of the present application, the angle between the emission direction of the electrode material in the first evaporation chamber and the substrate is an acute angle, and the angle between the emission direction of the electrode material in the second evaporation chamber and the substrate is an obtuse angle.
[0027] According to any of the aforementioned embodiments of the first aspect of the present application, the electrode material in the first evaporation chamber and the electrode material in the second evaporation chamber are respectively emitted toward two opposite sides of the isolation opening in the first direction.
[0028] According to any of the aforementioned implementations of the first aspect of the present application, the display panel includes a display area and a binding area, and the display area and the binding area are distributed along a first direction.
[0029] A second aspect of the present application provides another method for preparing a display panel, the method comprising:
[0030] An isolation structure is prepared on the substrate, wherein the isolation structure encloses an isolation opening;
[0031] The electrode material in the first evaporation chamber group is evaporated to the isolation opening multiple times; the first evaporation chamber group includes at least one first evaporation chamber, and the electrode material in the first evaporation chamber is emitted toward one side of the isolation opening in a first direction, and the first direction is parallel to the substrate.
[0032] According to an embodiment of the second aspect of the present application, the first evaporation chamber group includes at least two first evaporation chambers, and in the step of evaporating the electrode material in the first evaporation chamber group to the isolation opening multiple times on one side of the isolation opening along the first direction, the method further includes:
[0033] The electrode materials in at least two first evaporation chambers are evaporated into the isolation openings respectively.
[0034] According to any of the aforementioned embodiments of the second aspect of the present application, the angle between the emission direction of the electrode material in the first evaporation chamber and the substrate is an acute angle.
[0035] According to any of the aforementioned embodiments of the second aspect of the present application, the emission directions of the electrode materials in at least two first evaporation chambers have different angles with the substrate.
[0036] According to any of the aforementioned embodiments of the second aspect of the present application, the angle between the emission direction of the electrode material in the first evaporation chamber and the substrate is greater than or equal to 30°.
[0037] According to any of the aforementioned implementations of the second aspect of the present application,
[0038] The method further comprises: a step of evaporating the electrode material in the first evaporation chamber group into the isolation opening on one side of the isolation opening along the first direction for multiple times.
[0039] The substrate is moved back and forth along the first direction so that the electrode material in the first evaporation chamber group is evaporated to the isolation opening multiple times; or,
[0040] The first evaporation chamber group is moved back and forth along the first direction, so that the electrode material in the first evaporation chamber group is evaporated to the isolation opening multiple times.
[0041] According to a third aspect of the present application, there is provided a display panel, comprising: a substrate; an isolation structure located on the substrate, the isolation structure enclosing a plurality of isolation openings; a light-emitting layer located on the substrate, the light-emitting layer comprising a plurality of light-emitting units located in the isolation openings; a first electrode layer located on a side of the light-emitting layer away from the substrate, the first electrode layer comprising a first electrode located in the isolation openings, and an electrical connection between the first electrode and the isolation structure; the first electrode comprising a central portion and an overlapping portion located on a peripheral side of the central portion, the overlapping portion covering a side wall of the isolation structure, the thickness of at least a portion of the overlapping portion being greater than or equal to twenty percent of the thickness of the central portion.
[0042] According to an implementation of the third aspect of the present application, the thickness of the overlapping portion on the peripheral side of the central portion is greater than or equal to twenty percent of the thickness of the central portion.
[0043] According to any of the aforementioned embodiments of the third aspect of the present application, the first electrode also includes a connecting portion located between the central portion and the overlapping portion, and the thickness of the connecting portion is greater than or equal to the thickness of the overlapping portion; the connecting portion is annular, and the inner edge of the connecting portion is connected to the central portion, and the outer edge of the connecting portion is connected to the overlapping portion.
[0044] According to any of the aforementioned embodiments of the third aspect of the present application, the orthographic projection of the central portion on the substrate coincides with the orthographic projection of the isolation opening on the substrate.
[0045] According to any of the aforementioned embodiments of the third aspect of the present application, the thickness of the connecting portion is greater than or equal to fifty percent of the thickness of the central portion.
[0046] According to any of the aforementioned embodiments of the third aspect of the present application, the isolation structure includes a first layer and a second layer, the second layer is located on the side of the first layer facing away from the substrate, and the orthographic projection of the first layer on the substrate is located within the orthographic projection of the second layer on the substrate.
[0047] According to any of the aforementioned embodiments of the third aspect of the present application, the first layer includes a conductive material.
[0048] According to any of the aforementioned embodiments of the third aspect of the present application, the second layer includes a conductive material or an insulating material.
[0049] According to any of the aforementioned embodiments of the third aspect of the present application, the first layer and the second layer both include metal materials, and the materials of the first layer and the second layer are different.
[0050] According to any of the aforementioned embodiments of the third aspect of the present application, the isolation structure further includes a third layer located on the side of the first layer facing the substrate, and the orthographic projection of the first layer on the substrate is located within the orthographic projection of the third layer on the substrate.
[0051] According to any of the aforementioned embodiments of the third aspect of the present application, at least part of the third layer includes multiple sub-layers.
[0052] An embodiment of a fourth aspect of the present application provides a display device, which includes a display panel of any of the above-mentioned embodiments.
[0053] According to the method for preparing a display panel of an embodiment of the present application, an isolation structure is prepared on a substrate, and the isolation structure encloses an isolation opening to separate the light-emitting layer to form mutually disconnected light-emitting units, thereby reducing the crosstalk of carriers in the light-emitting layer and improving the display effect of the display panel. In addition, the light-emitting units do not need to use a precision mask plate, which can reduce the development and use of precision masks and reduce the preparation cost. The electrode material in the first evaporation chamber group is repeatedly evaporated to one side of the isolation opening along the first direction, and then the electrode material in the second evaporation chamber group is evaporated to the other side of the isolation opening along the first direction, thereby forming a first electrode layer, the first electrode layer includes a first electrode located in the isolation opening, and the first electrodes are electrically connected to each other through the isolation structure to form a whole-surface electrode. The first evaporation chamber group includes at least one first evaporation chamber; the second evaporation chamber group includes at least one second evaporation chamber. The evaporation directions of the first evaporation chamber group and the second evaporation chamber group are opposite, so that the first evaporation chamber group can evaporate the electrode material into one side of the isolation opening along the first direction, and the second evaporation chamber group can evaporate the electrode material into the other side of the isolation opening along the first direction, so that both sides of the first electrode in the first direction can overlap with the isolation structure, thereby improving the overlap performance of the first electrode and the isolation structure. The electrode material in the first evaporation chamber group is evaporated to one side of the isolation opening along the first direction for multiple times, so that the film formation continuity of the first electrode on one side of the isolation opening can be improved, the overlap area of the first electrode and the isolation structure on one side can be increased, and the overlap resistance of the first electrode on one side with the isolation structure can be reduced, thereby improving the display effect and performance of the display panel. BRIEF DESCRIPTION OF THE DRAWINGS
[0054] Other features, objects and advantages of the present application will become more apparent by reading the following detailed description of non-limiting embodiments with reference to the accompanying drawings, in which the same or similar reference numerals represent the same or similar features and the accompanying drawings are not drawn to scale.
[0055] Figure 1It is a schematic flow chart of a method for preparing a display panel provided in an embodiment of the present application;
[0056] Figures 2 to 11 is a diagram of a manufacturing process of a display panel provided in an embodiment of the present application;
[0057] Fig.12 It is a schematic flow chart of another method for preparing a display panel provided in an embodiment of the present application;
[0058] Fig.13 is a partial cross-sectional view of a display panel provided in an embodiment of the present application;
[0059] Fig.14 is a partial cross-sectional view of a display panel provided by another embodiment;
[0060] Fig.15 is a partial cross-sectional view of a display panel provided by yet another embodiment.
[0061] Description of reference numerals:
[0062] 10. Display panel;
[0063] 100. Substrate;
[0064] 200, isolation structure; 210, first layer; 220, second layer; 230, third layer; 240, isolation opening;
[0065] 300, light-emitting layer; 310, light-emitting unit;
[0066] 400, first electrode layer; 410, first electrode; 411, central portion; 412, connecting portion; 413, overlapping portion;
[0067] 500, pixel definition layer; 510, pixel definition portion; 520, pixel opening; 530, second electrode;
[0068] 600, first evaporation chamber group; 610, first evaporation chamber;
[0069] 700, second evaporation chamber group; 710, second evaporation chamber;
[0070] α, first angle; β, second angle; γ, third angle; θ, fourth angle;
[0071] X, first direction. DETAILED DESCRIPTION
[0072] The features and exemplary embodiments of various aspects of the present application will be described in detail below. In order to make the purpose, technical solutions and advantages of the present application clearer, the present application will be further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the specific embodiments described herein are only configured to explain the present application and are not configured to limit the present application. For those skilled in the art, the present application can be implemented without the need for some of these specific details. The following description of the embodiments is only to provide a better understanding of the present application by illustrating the examples of the present application.
[0073] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the statement "include..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.
[0074] It should be understood that when describing the structure of a component, when a layer or a region is referred to as being "on" or "over" another layer or another region, it may mean that it is directly on the other layer or another region, or that other layers or regions are included between it and the other layer or another region. Moreover, if the component is turned over, the layer or a region will be "below" or "beneath" another layer or another region.
[0075] Embodiments of the present application provide a method for manufacturing a display panel, a display panel, and a display device. Embodiments of the method for manufacturing a display panel, a display panel, and a display device are described below in conjunction with the accompanying drawings.
[0076] Embodiments of the present application provide a method for manufacturing a display panel, a display panel, and a display device. The display panel may be an organic light emitting diode (OLED) display panel.
[0077] See also Figures 1 to 11 , Figure 1 It is a schematic flow chart of a method for preparing a display panel provided in an embodiment of the present application; Figures 2 to 11 This is a diagram of a preparation process of a display panel provided in an embodiment of the present application.
[0078] like Figures 1 to 11 As shown, a first aspect of the present application provides a method for preparing a display panel, the method comprising:
[0079] Step S01: preparing an isolation structure on a substrate, wherein the isolation structure encloses an isolation opening;
[0080] Step S02: evaporating the electrode material in the first evaporation chamber group to one side of the isolation opening in the first direction for multiple times; the first evaporation chamber group includes at least one first evaporation chamber;
[0081] Step S03: evaporate the electrode material in the second evaporation chamber group to the other side of the isolation opening in the first direction to form a first electrode layer, wherein the first electrode layer includes a first electrode located in the isolation opening, and the first electrode is electrically connected to the isolation structure; the second evaporation chamber group includes at least one second evaporation chamber, and the emission direction of the electrode material in the second evaporation chamber is different from the emission direction of the electrode material in the first evaporation chamber. In particular, "one side of the isolation opening in the first direction" in step S02 and "the other side of the isolation opening in the first direction" in step S03 are two opposite sides of the isolation opening in the first direction.
[0082] According to the method for preparing the display panel 10 of the embodiment of the present application, the isolation structure 200 is prepared by step S01, and the isolation structure 200 encloses the isolation opening 240 to separate the light-emitting layer 300 to form mutually disconnected light-emitting units 310, thereby reducing the crosstalk of carriers in the light-emitting layer 300, improving the display effect of the display panel 10, and the light-emitting unit 310 does not need to use a precision mask plate, which can reduce the development and use of precision masks and reduce the preparation cost. The electrode material in the first evaporation chamber group 600 is repeatedly evaporated to one side of the isolation opening 240 along the first direction X by step S02. Then, the electrode material in the second evaporation chamber group 700 is evaporated to the other side of the isolation opening 240 along the first direction X by step S03, thereby forming a first electrode layer 400, and the first electrode layer 400 includes a first electrode 410 located in the isolation opening 240, and the first electrodes 410 are electrically connected to each other through the isolation structure 200 to form a whole-surface electrode. The first evaporation chamber group 600 includes at least one first evaporation chamber 610; the second evaporation chamber group 700 includes at least one second evaporation chamber 710, and the evaporation directions of the first evaporation chamber group 600 and the second evaporation chamber group 700 are opposite, so that the first evaporation chamber group 600 can evaporate the electrode material into one side of the isolation opening 240 along the first direction X, and the second evaporation chamber group 700 can evaporate the electrode material into the isolation opening 240 along the other side of the first direction X, so that the first electrode 410 can overlap with the isolation structure 200 on both sides in the first direction X, thereby improving the overlapping performance of the first electrode 410 and the isolation structure 200. By repeatedly evaporating the electrode material in the first evaporation chamber group 600 to one side of the isolation opening 240 along the first direction X, the film formation continuity of the first electrode 410 on one side in the isolation opening 240 can be improved, the overlapping area between the first electrode 410 and one side of the isolation structure 200 can be increased, the overlapping resistance between the first electrode 410 and the isolation structure 200 on one side can be reduced, and the display effect and performance of the display panel 10 can be improved.
[0083] Optionally, the thickness of the electrode material evaporated into the isolation opening 240 by the first evaporation chamber group 600 is the same as or different from the thickness of the electrode material evaporated into the isolation opening 240 by the second evaporation chamber group 700. For example, the thickness of the electrode material evaporated into the isolation opening 240 by the first evaporation chamber group 600 is 50A, and the thickness of the electrode material evaporated into the isolation opening 240 by the second evaporation chamber group 700 is 50A, or the thickness of the electrode material evaporated into the isolation opening 240 by the first evaporation chamber group 600 is 20A, and the thickness of the electrode material evaporated into the isolation opening 240 by the second evaporation chamber group 700 is 80A. It is sufficient to ensure that the total thickness of the first electrode 410 is 100A.
[0084] like Figure 5As shown, in some optional embodiments, the first evaporation chamber group 600 includes at least two first evaporation chambers 610, and in the step of evaporating the electrode material in the first evaporation chamber group 600 to one side of the isolation opening 240 in the first direction X for multiple times, the method further includes:
[0085] The electrode materials in the at least two first evaporation chambers 610 are evaporated into the isolation openings 240 respectively.
[0086] In these optional embodiments, by setting up multiple first evaporation chambers 610 in the first evaporation chamber group 600, multiple first evaporation chambers 610 are used to evaporate the electrode material on one side of the isolation opening 240 along the first direction X, so that the film formation continuity of the first electrode 410 on one side of the isolation opening 240 can be improved, the overlapping area between the first electrode 410 and the one side of the isolation structure 200 is increased, and the overlapping resistance between the first electrode 410 and the isolation structure 200 on one side is reduced, thereby improving the display effect and performance of the display panel 10.
[0087] Optionally, the thickness of the electrode material evaporated into the isolation opening 240 in each first evaporation chamber 610 is the same or different. For example, the first evaporation chamber group 600 includes two first evaporation chambers 610, one of which evaporates into the isolation opening 240 with a thickness of 25A, and the other evaporates into the isolation opening 240 with a thickness of 25A. Alternatively, the thickness of the electrode material evaporated into the isolation opening 240 in one of the two first evaporation chambers 610 is 10A, and the thickness of the electrode material evaporated into the isolation opening 240 in the other is 40A, so as to ensure that the thickness of the electrode material evaporated into the isolation opening 240 of the first evaporation chamber group 600 is 50A.
[0088] Optionally, the first evaporation chamber 610 includes an evaporation source of at least one electrode material, for example, the first evaporation chamber 610 includes an evaporation source of Mg and an evaporation source of Ag. The evaporation source includes a crucible and a nozzle disposed on the crucible, the central axis of the nozzle is the emission direction, and the angle between the central axis and the substrate 100 is the emission range.
[0089] Optionally, the angles between the emission directions of the electrode materials in at least two first evaporation chambers 610 and the substrate 100 are different, so that the evaporation angle of at least one first evaporation chamber 610 changes, thereby improving the continuity of the first electrode 410 on one side of the isolation opening 240, increasing the overlapping area between the first electrode 410 and the isolation structure 200 on one side, reducing the overlapping resistance between the first electrode 410 and the isolation structure 200 on one side, and improving the display effect and performance of the display panel 10.
[0090] like Figure 6As shown, optionally, at least one first evaporation chamber 610 in the first evaporation chamber group 600 is rotated by a first angle α relative to another first evaporation chamber 610, so that the evaporation angle of at least one first evaporation chamber 610 changes, thereby improving the continuity of the first electrode 410 on one side in the isolation opening 240, increasing the overlap area of the first electrode 410 and the isolation structure 200 on one side, reducing the overlap resistance of the first electrode 410 and the isolation structure 200 on one side, and improving the display effect and performance of the display panel 10. And rotating the first evaporation chamber 610 by the first angle α relative to the reference plane 110 can adjust the thickness and overlap range of the first electrode 410 at the overlap position with the isolation structure 200 on one side.
[0091] Optionally, the first rotation angles α of multiple first evaporation chambers 610 in the first evaporation chamber group 600 are different or the same, that is, multiple first evaporation chambers 610 are rotated by a certain angle relative to the same first evaporation chamber 610, so that the evaporation angles of multiple first evaporation chambers 610 are changed, thereby further improving the continuity of the first electrode 410 on one side of the isolation opening 240, increasing the overlap area between the first electrode 410 and one side of the isolation structure 200, reducing the overlap resistance between the first electrode 410 and the isolation structure 200 on one side, and improving the display effect and performance of the display panel 10.
[0092] like Figure 7 As shown, optionally, the angle between the emission direction of the electrode material in the first evaporation chamber 610 and the substrate 100 is a second angle β, and the second angle β is greater than or equal to 30°, for example, it can be 35°, 40°, etc. This setting can improve the problem that after the first evaporation chamber 610 is rotated, it is difficult to evaporate the electrode material to one side of the isolation opening 240, resulting in difficulty in overlapping the first electrode 410 and one side of the isolation structure 200 due to the small angle between the emission direction and the substrate 100.
[0093] In some optional embodiments, in the step of evaporating the electrode material in the first evaporation chamber group 600 multiple times onto one side of the isolation opening 240 in the first direction X, the method further includes:
[0094] The substrate 100 is moved back and forth along the first direction X, so that the electrode material in the first evaporation chamber group 600 is evaporated to the isolation opening 240 for multiple times.
[0095] In these optional embodiments, the first evaporation chamber group 600 is fixed, and the substrate 100 is moved back and forth along the first direction X, so that the substrate 100 can pass through the evaporation range of the first evaporation chamber group 600 twice, so that the electrode material in the first evaporation chamber group 600 is evaporated twice into one side of the isolation opening 240 along the first direction X. For example, the thickness of the electrode material evaporated into the isolation opening 240 by the first evaporation chamber group 600 once is 25A, and after the substrate 100 passes back and forth, the total thickness of the electrode material evaporated into the isolation opening 240 by the first evaporation chamber group 600 twice is 50A.
[0096] In some optional embodiments, in the step of evaporating the electrode material in the first evaporation chamber group 600 multiple times onto one side of the isolation opening 240 in the first direction X, the method further includes:
[0097] The first evaporation chamber set 600 is moved back and forth along the first direction X, so that the electrode material in the first evaporation chamber set 600 is evaporated to the isolation opening 240 for multiple times.
[0098] In these optional embodiments, the substrate 100 is moved into the evaporation range of the first evaporation chamber group 600 and fixed, and the first evaporation chamber group 600 is moved back and forth along the first direction X, so that the substrate 100 can pass through the evaporation range of the first evaporation chamber group 600 twice, thereby achieving the electrode material in the first evaporation chamber group 600 being evaporated twice into one side of the isolation opening 240 along the first direction X.
[0099] In some optional embodiments, in the step of evaporating the electrode material in the second evaporation chamber group 700 to the other side of the isolation opening 240 in the first direction X, the method further includes:
[0100] At the other side of the isolation opening 240 along the first direction X, the electrode material in the second evaporation chamber group 700 is evaporated to the isolation opening 240 for multiple times.
[0101] In these optional embodiments, the electrode material in the second evaporation chamber group 700 is evaporated multiple times to the other side of the isolation opening 240 along the first direction X, which can improve the film formation continuity of the first electrode 410 on the other side of the isolation opening 240, increase the overlapping area between the first electrode 410 and the other side of the isolation structure 200, reduce the overlapping resistance between the first electrode 410 and the isolation structure 200 on the other side, and improve the display effect and performance of the display panel 10.
[0102] like Figure 8 As shown, in some optional embodiments, the second evaporation chamber group 700 includes at least two second evaporation chambers 710, and in the step of evaporating the electrode material in the second evaporation chamber group 700 multiple times to the isolation opening 240 on the other side of the first direction X, the method further includes:
[0103] The electrode materials in the at least two second evaporation chambers 710 are evaporated into the isolation openings 240 respectively.
[0104] In these optional embodiments, by setting up a plurality of second evaporation chambers 710 in the second evaporation chamber group 700, and using the plurality of second evaporation chambers 710 to evaporate the electrode material on the other side of the isolation opening 240 along the first direction X, the film formation continuity of the first electrode 410 on the other side of the isolation opening 240 can be improved, the overlapping area between the first electrode 410 and the other side of the isolation structure 200 is increased, the overlapping resistance between the first electrode 410 and the isolation structure 200 on the other side is reduced, and the display effect and performance of the display panel 10 are improved.
[0105] like Fig. 9 As shown, the first evaporation chamber group 600 includes at least two first evaporation chambers 610 spaced apart from each other, and the second evaporation chamber group 700 includes at least two second evaporation chambers 710 spaced apart from each other. Multiple first evaporation chambers 610 are used to perform multiple evaporation depositions of electrode materials on one side of the isolation opening 240 along the first direction X, which can improve the film formation continuity of the first electrode 410 on one side of the isolation opening 240, increase the overlap area between the first electrode 410 and one side of the isolation structure 200, reduce the overlap resistance between the first electrode 410 and the isolation structure 200 on one side, and improve the display effect and performance of the display panel 10. By using multiple second evaporation chambers 710 to perform multiple evaporation depositions of electrode materials on the other side of the isolation opening 240 along the first direction X, the continuity of the film formation of the first electrode 410 on the other side of the isolation opening 240 can be improved, the overlapping area between the first electrode 410 and the other side of the isolation structure 200 can be increased, the overlapping resistance between the first electrode 410 and the isolation structure 200 on the other side can be reduced, and the display effect and performance of the display panel 10 can be improved.
[0106] Optionally, the thickness of the electrode material evaporated into the isolation opening 240 in each second evaporation chamber 710 is the same or different. For example, the second evaporation chamber group 700 includes two second evaporation chambers 710, one of which evaporates into the isolation opening 240 with a thickness of 25A, and the other evaporates into the isolation opening 240 with a thickness of 25A. Alternatively, the thickness of the electrode material evaporated into the isolation opening 240 in one of the two second evaporation chambers 710 is 10A, and the thickness of the electrode material evaporated into the isolation opening 240 in the other is 40A, so as to ensure that the thickness of the electrode material evaporated into the isolation opening 240 of the second evaporation chamber group 700 is 50A.
[0107] Optionally, the second evaporation chamber 710 includes an evaporation source of at least one electrode material. For example, the second evaporation chamber 710 includes an evaporation source of Mg and an evaporation source of Ag.
[0108] Optionally, the emission directions of the electrode materials in at least two second evaporation chambers 710 have different angles with the substrate 100, so that the evaporation angle of at least one second evaporation chamber 710 changes, thereby improving the continuity of the first electrode 410 on the other side of the isolation opening 240, increasing the overlapping area between the first electrode 410 and one side of the isolation structure 200, reducing the overlapping resistance between the first electrode 410 and the isolation structure 200 on one side, and improving the display effect and performance of the display panel 10.
[0109] like Fig.10 As shown, optionally, at least one second evaporation chamber 710 in the second evaporation chamber group 700 is rotated by a third angle γ relative to another second evaporation chamber 710, so that the evaporation angle of at least one second evaporation chamber 710 changes, thereby improving the continuity of the second electrode on the other side of the isolation opening 240, increasing the overlap area of the second electrode and the other side of the isolation structure 200, reducing the overlap resistance of the second electrode and the isolation structure 200 on the other side, and improving the display effect and performance of the display panel 10. And rotating the second evaporation chamber 710 by the third angle γ relative to the reference plane 110 can adjust the thickness and overlap range of the first electrode 410 at the overlap position with the isolation structure 200 on the other side.
[0110] Optionally, the third angles γ at which the multiple second evaporation chambers 710 in the second evaporation chamber group 700 rotate are different or the same, that is, the multiple second evaporation chambers 710 are rotated by a certain angle relative to another second evaporation chamber 710, so that the evaporation angles of the multiple second evaporation chambers 710 are changed, thereby further improving the continuity of the second electrode on the other side of the isolation opening 240, increasing the overlapping area between the second electrode and the other side of the isolation structure 200, reducing the overlapping resistance between the second electrode and the isolation structure 200 on the other side, and improving the display effect and performance of the display panel 10.
[0111] like Fig.11 As shown, optionally, the angle between the emission direction of the electrode material in the second evaporation chamber 710 and the substrate 100 is a fourth angle θ, and the fourth angle θ is less than or equal to 150°, for example, it can be 120°, 145°, etc. Such a setting can improve the problem that after the first evaporation chamber 610 is rotated, it is difficult to evaporate the electrode material to one side of the isolation opening 240, resulting in difficulty in overlapping the first electrode 410 and one side of the isolation structure 200 due to the large angle between the emission direction and the substrate 100.
[0112] In some optional embodiments, in the step of evaporating the electrode material in the second evaporation chamber group 700 multiple times to the isolation opening 240 on the other side of the first direction X, the method further includes:
[0113] The substrate 100 is moved back and forth along the first direction X, so that the electrode material in the second evaporation chamber group 700 is evaporated to the isolation opening 240 for multiple times.
[0114] In these optional embodiments, the second evaporation chamber group 700 is fixed, and the substrate 100 is moved back and forth along the first direction X, so that the substrate 100 can pass through the evaporation range of the second evaporation chamber group 700 twice, so that the electrode material in the second evaporation chamber group 700 is evaporated twice into the other side of the isolation opening 240 along the first direction X. For example, the thickness of the electrode material evaporated into the isolation opening 240 by the second evaporation chamber group 700 once is 25A, and after the substrate 100 passes back and forth, the total thickness of the electrode material evaporated into the isolation opening 240 by the second evaporation chamber group 700 twice is 50A.
[0115] In some optional embodiments, in the step of evaporating the electrode material in the second evaporation chamber group 700 multiple times to the isolation opening 240 on the other side of the first direction X, the method further includes:
[0116] The second evaporation chamber set 700 is moved back and forth along the first direction X, so that the electrode material in the second evaporation chamber set 700 is evaporated to the isolation opening 240 for multiple times.
[0117] In these optional embodiments, the substrate 100 is moved into the evaporation range of the second evaporation chamber group 700 and fixed, and the second evaporation chamber group 700 is moved back and forth along the first direction X, so that the substrate 100 can pass through the evaporation range of the second evaporation chamber group 700 twice, thereby achieving the electrode material in the second evaporation chamber group 700 being evaporated twice into the other side of the isolation opening 240 along the first direction X.
[0118] Optionally, the angle between the emission direction of the electrode material in the first evaporation chamber 610 and the substrate 100 is an acute angle, and the angle between the emission direction of the electrode material in the second evaporation chamber 710 and the substrate 10 is an obtuse angle, that is, the evaporation directions of the first evaporation chamber group 600 and the second evaporation chamber group 700 are opposite, so that the first evaporation chamber group 600 can evaporate the electrode material into one side of the isolation opening 240 along the first direction X, and the second evaporation chamber group 700 can evaporate the electrode material into the isolation opening 240 along the other side of the first direction X, so that the first electrode 410 can overlap with the isolation structure 200 on both sides in the first direction X, thereby improving the overlapping performance of the first electrode 410 and the isolation structure 200.
[0119] Optionally, the electrode material in the first evaporation chamber 610 and the electrode material in the second evaporation chamber 710 are emitted toward two opposite sides of the isolation opening 240 in the first direction X, respectively.
[0120] Optionally, the display panel 10 includes a display area and a binding area, and the display area and the binding area are distributed along the first direction.
[0121] See also Fig.12 , Fig.12 It is a schematic flow chart of another method for preparing a display panel provided in an embodiment of the present application.
[0122] like Fig.12 As shown, a second aspect of the present application provides a method for preparing a display panel 10, the method comprising:
[0123] Step S1: preparing an isolation structure on a substrate, wherein the isolation structure encloses an isolation opening;
[0124] Step S2: evaporating the electrode material in the first evaporation chamber group to the isolation opening multiple times; the first evaporation chamber group includes at least one first evaporation chamber, and the electrode material in the first evaporation chamber is emitted toward one side of the isolation opening in a first direction, and the first direction is parallel to the substrate.
[0125] According to the method for preparing the display panel 10 of the embodiment of the present application, the isolation structure 200 is prepared by step S01, and the isolation structure 200 encloses the isolation opening 240 to separate the light-emitting layer 300 to form mutually disconnected light-emitting units 310, thereby reducing the crosstalk of carriers in the light-emitting layer 300, improving the display effect of the display panel 10, and the light-emitting unit 310 does not need to use a precision mask plate to prepare the light-emitting unit 310, which can reduce the development and use of the precision mask plate and reduce the preparation cost. The electrode material in the first evaporation chamber group 600 is repeatedly evaporated to one side of the isolation opening 240 along the first direction X. The electrode material in the first evaporation chamber group 600 is repeatedly evaporated to one side of the isolation opening 240 along the first direction X, which can improve the film formation continuity of the first electrode 410 on one side of the isolation opening 240, increase the overlap area of the first electrode 410 and one side of the isolation structure 200, reduce the overlap resistance of the first electrode 410 on one side with the isolation structure 200, and improve the display effect and performance of the display panel 10. Optionally, the angle between the emission direction of the electrode material in the first evaporation chamber 710 and the substrate 100 is an acute angle, so as to facilitate multiple evaporation of the electrode material in the first evaporation chamber group 600 to one side of the isolation opening 240 along the first direction X.
[0126] A third aspect of the present application provides another method for preparing a display panel 10, the method comprising:
[0127] An isolation structure 200 is prepared on the substrate 100, and the isolation structure 200 encloses an isolation opening 240;
[0128] The electrode material in the first evaporation chamber group 600 is evaporated to the isolation opening 240 at one side of the isolation opening 240 along the first direction X;
[0129] The electrode material in the second evaporation chamber group 700 is evaporated to the isolation opening 240 multiple times on the other side of the isolation opening 240 along the first direction X to form a first electrode layer 400 . The first electrode layer 400 includes a first electrode 410 located in the isolation opening 240 . The first electrode 410 is electrically connected to the isolation structure 200 .
[0130] According to the method for preparing the display panel 10 of the embodiment of the present application, the isolation structure 200 encloses and forms an isolation opening 240 to separate the light-emitting layer 300 to form mutually disconnected light-emitting units 310, thereby reducing the crosstalk of carriers in the light-emitting layer 300, improving the display effect of the display panel 10, and the light-emitting unit 310 does not need to be prepared using a precision mask plate, which can reduce the development and use of precision masks and reduce the preparation cost. The electrode material in the first evaporation chamber group 600 is evaporated to one side of the isolation opening 240 along the first direction X. Then, the electrode material in the second evaporation chamber group 700 is evaporated multiple times to the other side of the isolation opening 240 along the first direction X, thereby forming a first electrode layer 400, the first electrode layer 400 includes a first electrode 410 located in the isolation opening 240, and the first electrodes 410 are electrically connected to each other through the isolation structure 200 to form a whole-surface electrode. By repeatedly evaporating the electrode material in the second evaporation chamber group 700 to the other side of the isolation opening 240 along the first direction X, the film formation continuity of the first electrode 410 on the other side of the isolation opening 240 can be improved, the overlapping area between the first electrode 410 and the other side of the isolation structure 200 can be increased, the overlapping resistance between the first electrode 410 and the isolation structure 200 on the other side can be reduced, and the display effect and performance of the display panel 10 can be improved.
[0131] See also Fig.13 , Fig.13 It is a partial cross-sectional view of a display panel provided in an embodiment of the present application.
[0132] like Fig.13As shown, the third aspect of the present application provides a display panel 10, which includes: a substrate 100; an isolation structure 200, which is located on the substrate 100, and the isolation structure 200 encloses a plurality of isolation openings 240; a light-emitting layer 300, which is located on the substrate 100, and the light-emitting layer 300 includes a plurality of light-emitting units 310 located in the isolation openings 240; a first electrode layer 400, which is located on the side of the light-emitting layer 300 away from the substrate 100, and the first electrode layer 400 includes a first electrode 410 located in the isolation opening 240, and the first electrode 410 is electrically connected to the isolation structure 200; the first electrode 410 includes a central portion 411 and an overlapping portion 413 located on the peripheral side of the central portion 411, the overlapping portion 413 covers the side wall of the isolation structure 200, and the thickness of at least part of the overlapping portion 413 is greater than or equal to 20 percent of the thickness of the central portion 411.
[0133] According to the display panel 10 of the embodiment of the present application, the display panel 10 includes a substrate 100, an isolation structure 200, a light-emitting layer 300 and a first electrode layer 400. The isolation structure 200 is arranged on the substrate 100 and encloses a plurality of isolation openings 240. When preparing the light-emitting layer 300, the light-emitting layer 300 has a large drop at the edge of the isolation structure 200. The light-emitting layer 300 is difficult to connect at the edge of the isolation structure 200, and thus breaks. The light-emitting layer 300 breaks to form mutually disconnected light-emitting units 310. There is no need to use a precision mask plate to prepare the light-emitting unit 310, which can reduce the development and use of precision masks and reduce the preparation cost. The first electrode 410 serves as the electrode of the light-emitting unit 310, and is electrically connected to the isolation structure 200 to form a full-surface electrode to ensure the normal light emission of the light-emitting unit 310. The overlapping portion 413 of the first electrode 410 overlaps the side wall of the isolation structure 200 to achieve electrical connection between the first electrode 410 and the isolation structure 200. The thickness of at least part of the overlapping portion 413 is greater than or equal to twenty percent of the thickness of the central portion 411. This can improve the problem of poor overlapping performance between the overlapping portion 413 and the isolation structure 200 due to the overlapping portion 413 being too thin, ensure the overlapping effect of at least part of the overlapping portion 413 and the isolation structure 200, and improve the performance of the display panel 10.
[0134] In some optional embodiments, the thickness of the overlapping portion 413 on the peripheral side of the central portion 411 is greater than or equal to 20 percent of the thickness of the central portion 411 .
[0135] In these optional embodiments, the thickness of the overlapping portion 413 on the peripheral side of the center portion 411 is greater than or equal to twenty percent of the thickness of the center portion 411, which can improve the problem of poor overlapping performance between the overlapping portion 413 and the isolation structure 200 due to the low thickness of the overlapping portion 413, ensure the overlapping effect of the overlapping portion 413 on the peripheral side of the center portion 411 and the isolation structure 200, and further improve the performance of the display panel 10.
[0136] In some optional embodiments, the first electrode 410 also includes a connecting portion 412 located between the central portion 411 and the overlapping portion 413, and the thickness of the connecting portion 412 is greater than or equal to the thickness of the overlapping portion 413; the connecting portion 412 is annular, and the inner edge of the connecting portion 412 is connected to the central portion 411, and the outer edge of the connecting portion 412 is connected to the overlapping portion 413.
[0137] In these optional embodiments, during the evaporation process of the first electrode 410, due to process reasons, the thickness of the first electrode 410 gradually decreases in the direction from the central portion 411 toward the peripheral side, so the thickness of the connecting portion 412 is greater than or equal to the thickness of the overlapping portion 413. The connecting portion 412 has a greater thickness, which can ensure that the first electrode 410 has a lower voltage drop and improve the performance of the first electrode 410.
[0138] Optionally, the orthographic projection of the central portion 411 on the substrate 100 coincides with the orthographic projection of the isolation opening 240 on the substrate 100 , and the central portion 411 covers the light emitting unit 310 to drive the light emitting unit 310 to emit light.
[0139] In some optional embodiments, the thickness of the connecting portion 412 is greater than or equal to fifty percent of the thickness of the central portion 411 .
[0140] In these optional embodiments, the thickness of the connection portion 412 is greater than or equal to fifty percent of the thickness of the central portion 411, which can improve the problem that the thickness of the overlapping portion 413 extending from the connection portion 412 toward the isolation structure 200 is too low, and the overlapping performance of the overlapping portion 413 and the isolation structure 200 is poor, thereby ensuring the overlapping effect of the overlapping portion 413 and the isolation structure 200, and further improving the performance of the display panel 10. It can also ensure that the connection portion 412 and the overlapping portion 413 have a large thickness, improve the continuity of the film layer of the connection portion 412 and the overlapping portion 413, reduce the resistance of the connection portion 412 and the overlapping portion 413, and thus reduce the power consumption of the first electrode 410.
[0141] In some optional embodiments, the isolation structure 200 includes a first layer 210 and a second layer 220 , wherein the second layer 220 is located on a side of the first layer 210 facing away from the substrate 100 , and the orthographic projection of the first layer 210 on the substrate 100 is located within the orthographic projection of the second layer 220 on the substrate 100 .
[0142] In these optional embodiments, the first layer 210 and the second layer 220 are stacked to form the isolation structure 200, the orthographic projection of the first layer 210 disposed close to the substrate 100 on the substrate 100 is located within the orthographic projection of the second layer 220 on the substrate 100, the orthographic projection area of the second layer 220 is larger than the orthographic projection area of the first layer 210, and the second layer 220 covers the top surface of the first layer 210, and at this time, the first layer 210 is recessed relative to the second layer 220 in a direction away from the isolation opening 240. When preparing the light-emitting layer 300, the light-emitting layer 300 has a large drop at the edge of the isolation structure 200, and the first layer 210 is recessed relative to the second layer 220, and the light-emitting layer 300 is difficult to connect at the edge of the isolation structure 200, so it breaks, and the light-emitting layer 300 breaks to form mutually disconnected light-emitting units 310, and the preparation of the light-emitting units 310 does not require the use of a precision mask plate, which can reduce the development and use of precision masks and reduce the preparation cost.
[0143] Optionally, the first layer 210 includes a conductive material, and the first layer 210 is connected to the first electrode 410 to achieve electrical connection between the isolation structure 200 and the first electrode 410 .
[0144] In some optional embodiments, the second layer 220 includes a conductive material or an insulating material.
[0145] In these optional embodiments, the second layer 220 includes a conductive material, for example, the second layer 220 includes a non-metallic conductive material or a metallic conductive material. When the second layer 220 is a non-metallic conductive material or an insulating material, the second layer 220 is difficult to be etched during wet etching of the first layer 210 using an etching solution, so that the first layer 210 is more easily concavely arranged relative to the second layer 220.
[0146] In some optional embodiments, both the first layer 210 and the second layer 220 include metal materials, and the materials of the first layer 210 and the second layer 220 are different.
[0147] In these optional embodiments, when both the first layer 210 and the second layer 220 are made of metal materials, the first layer 210 may be wet-etched with an etching solution, and the etching rate of the second layer 220 may be set to be lower than the etching rate of the first layer 210 by setting the etching solution. Since the etching rate of the first layer 210 is relatively high, when the etching solution is used for wet etching, even if the second layer 220 is etched to a certain extent, the first layer 210 is etched faster, so that the first layer 210 is set concave relative to the second layer 220.
[0148] See also Fig.14 , Fig.14 FIG. 1 is a partial cross-sectional view of a display panel 10 provided in another embodiment.
[0149] like Fig.14 As shown, in some optional embodiments, the isolation structure 200 further includes a third layer 230 located on the side of the first layer 210 facing the substrate 100, and the orthographic projection of the first layer 210 on the substrate 100 is located within the orthographic projection of the third layer 230 on the substrate 100. Among them, the patents CN118251982A, 202410864269.8, PCT / CN2024 / 098407, PCT / CN2024 / 102783, PCT / CN2024 / 098217, PCT / CN2024 / 099419, and PCT / CN2024 / 099072 record the relevant contents of the isolation structure 200 for reference.
[0150] In these optional embodiments, in order to obtain the first layer 210 with a concave setting, the first layer 210 has a faster etching rate than the second layer 220 and the third layer 230 during the etching process, thereby forming the concave first layer 210. Since the etching rate of the first layer 210 is faster, the waste generated by etching is more likely to enter other positions of the display panel 10, thereby causing adverse effects. After the third layer 230 is set, the first layer 210 can be well attached to the third layer 230, and the generated etching waste falls on the third layer 230, which is easy to clean.
[0151] See also Fig.15 , Fig.15 is a partial cross-sectional view of a display panel provided by yet another embodiment.
[0152] like Fig.15 As shown, in some optional embodiments, at least a portion of the third layer 230 includes multiple sub-layers.
[0153] In these optional embodiments, regardless of whether the third layer 230 includes one sub-layer or multiple sub-layers, when the thickness of the overlapping portion 413 is greater than or equal to twenty percent of the thickness of the central portion 411, the overlapping effect between the overlapping portion 413 and the isolation structure 200 can be improved. Therefore, the present application is applicable to scenarios with different isolation structures 200.
[0154] Optionally, the overlapping portion 413 covers the third layer 230 so that the overlapping portion 413 is electrically connected to the third layer 230, thereby achieving overlapping electrical connection between the overlapping portion 413 and the isolation structure 200, and the overlapping portion 413 covering the third layer 230 can ensure that the overlapping portion 413 and the isolation structure 200 have a good overlapping effect.
[0155] Optionally, the overlapping portion 413 covers the third layer 230 and at least a portion of the first layer 210 to increase the overlapping area between the overlapping portion 413 and the isolation structure 200 , thereby improving the overlapping effect between the overlapping portion 413 and the isolation structure 200 .
[0156] Optionally, the number of sub-layers of the third layer 230 of the isolation structure 200 around at least some of the light-emitting units 310 of different colors is different. Since the thicknesses of the light-emitting units 310 of different colors are different, when the number of sub-layers of the corresponding third layer 230 is set differently, the thickness of the corresponding third layer 230 is also different. For example, the number of sub-layers of the third layer 230 of the isolation structure 200 around the light-emitting unit 310 with greater thickness is greater, and the thickness of the third layer 230 is greater. When the first electrode 410 is subsequently prepared, the first electrodes 410 corresponding to the light-emitting units 310 of different colors can be well overlapped with the third layer 230, thereby improving the overlap effect of the overall first electrode 410 and the isolation structure 200. The light-emitting unit 310 corresponds to the first electrode 410, which means that the light-emitting unit 310 and the first electrode 410 are located in the same isolation opening 240.
[0157] Optionally, the display panel 10 further includes a pixel definition layer 500, which is located between the substrate 100 and the light-emitting layer 300. The pixel definition portion 510 of the pixel definition layer 500 encloses a pixel opening 520 to set the light-emitting unit 310 and realize normal light emission of the light-emitting unit 310. The pixel definition portion 510 defines the setting area of each light-emitting unit 310 to reduce the cross-color defect between each light-emitting unit 310.
[0158] Optionally, the display panel 10 further includes a second electrode 530, the second electrode 530 is located between the substrate 100 and the pixel definition layer 500, and the second electrode 530 is exposed by the pixel opening 520. One of the second electrode 530 and the first electrode 410 serves as the anode of the light-emitting unit 310, and the other serves as the cathode of the light-emitting unit 310. The embodiment of the present application takes the second electrode 530 as the anode of the light-emitting unit 310 and the first electrode 410 as the cathode of the light-emitting unit 310 as an example. Patents with application numbers 202310707209.0 and 202311346196.5 record the relevant contents of the cathode for reference.
[0159] Optionally, the light emitting layer 300 includes an electron injection layer (EIL), an electron transport layer (ETL), a light emitting material layer, a hole injection layer (HIL) and a hole transport layer (HTL).
[0160] According to the embodiments described above, these embodiments do not describe all the details in detail, nor do they limit the invention to the specific embodiments described. Obviously, many modifications and changes can be made based on the above description. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present application, so that those skilled in the art can make good use of the present application and the modifications based on the present application. The present application is limited only by the claims and their full scope and equivalents.
Claims
1. A method for preparing a display panel, characterized in that: The method comprises: Preparing an isolation structure on a substrate, wherein the isolation structure encloses an isolation opening; The electrode material in the first evaporation chamber group is evaporated multiple times to one side of the isolation opening in a first direction; the first direction is parallel to the substrate; the first evaporation chamber group includes at least one first evaporation chamber; The electrode material in the second evaporation chamber group is evaporated to the other side of the isolation opening in the first direction to form a first electrode layer, wherein the first electrode layer includes a first electrode located in the isolation opening, and the first electrode is electrically connected to the isolation structure; the second evaporation chamber group includes at least one second evaporation chamber, and the emission direction of the electrode material in the second evaporation chamber is different from the emission direction of the electrode material in the first evaporation chamber.
2. The preparation method according to claim 1, characterized in that: The first evaporation chamber group includes at least two first evaporation chambers, and in the step of evaporating the electrode material in the first evaporation chamber group to one side of the isolation opening in the first direction for multiple times, the method further includes: The electrode materials in at least two of the first evaporation chambers are evaporated into the isolation openings respectively.
3. The preparation method according to claim 2, characterized in that: The exit directions of the electrode materials in at least two of the first evaporation chambers have different angles with the substrate; Preferably, the angle between the emission direction of the electrode material in the first evaporation chamber and the substrate is greater than or equal to 30°.
4. The preparation method according to claim 1, characterized in that: In the step of evaporating the electrode material in the first evaporation chamber group to one side of the isolation opening in the first direction for multiple times, the method further includes: The substrate is moved back and forth along the first direction so that the electrode material in the first evaporation chamber group is evaporated to the isolation opening multiple times; or, The first evaporation chamber group is moved back and forth along the first direction, so that the electrode material in the first evaporation chamber group is evaporated to the isolation opening for multiple times.
5. The preparation method according to claim 1, characterized in that: In the step of evaporating the electrode material in the second evaporation chamber group to the other side of the isolation opening in the first direction, the method further includes: The electrode material in the second evaporation chamber group is evaporated multiple times to the isolation opening at the other side of the isolation opening along the first direction.
6. The preparation method according to claim 5, characterized in that: The second evaporation chamber group includes at least two second evaporation chambers, and in the step of evaporating the electrode material in the second evaporation chamber group to the other side of the isolation opening in the first direction for multiple times, the method further includes: The electrode materials in at least two of the second evaporation chambers are evaporated into the isolation openings respectively.
7. The preparation method according to claim 6, characterized in that: The emission directions of the electrode materials in at least two of the second evaporation chambers have different angles with the substrate; Preferably, the angle between the emission direction of the electrode material in the second evaporation chamber and the substrate is less than or equal to 150°.
8. The preparation method according to claim 5, characterized in that: In the step of evaporating the electrode material in the second evaporation chamber group multiple times to the other side of the isolation opening in the first direction, the method further includes: The substrate is moved back and forth along the first direction so that the electrode material in the second evaporation chamber group is evaporated to the isolation opening multiple times; or, The second evaporation chamber group is moved back and forth along the first direction, so that the electrode material in the second evaporation chamber group is evaporated to the isolation opening for multiple times.
9. The preparation method according to claim 1, characterized in that: The evaporation source in the first evaporation chamber and / or the second evaporation chamber is a linear evaporation source, and an extension direction of the linear evaporation source is perpendicular to the first direction and parallel to the substrate; Preferably, the angle between the emission direction of the electrode material in the first evaporation chamber and the substrate is an acute angle, and the angle between the emission direction of the electrode material in the second evaporation chamber and the substrate is an obtuse angle; Preferably, the electrode material in the first evaporation chamber and the electrode material in the second evaporation chamber are respectively emitted toward two opposite sides of the isolation opening in the first direction; Preferably, the display panel comprises a display area and a binding area, and the display area and the binding area are distributed along the first direction.
10. A method for preparing a display panel, characterized in that: The method comprises: Preparing an isolation structure on a substrate, wherein the isolation structure encloses an isolation opening; The electrode material in the first evaporation chamber group is evaporated to the isolation opening multiple times; the first evaporation chamber group includes at least one first evaporation chamber, and the electrode material in the first evaporation chamber is emitted toward one side of the isolation opening in a first direction, and the first direction is parallel to the substrate.
11. The preparation method according to claim 10, characterized in that: The first evaporation chamber group includes at least two first evaporation chambers. In the step of evaporating the electrode material in the first evaporation chamber group to the isolation opening multiple times, the method further includes: Evaporating the electrode materials in at least two of the first evaporation chambers into the isolation openings respectively; Preferably, the angle between the emission direction of the electrode material in the first evaporation chamber and the substrate is an acute angle.
12. The preparation method according to claim 11, characterized in that: The exit directions of the electrode materials in at least two of the first evaporation chambers have different angles with the substrate; Preferably, the angle between the emission direction of the electrode material in the first evaporation chamber and the substrate is greater than or equal to 30°.
13. The preparation method according to claim 10, characterized in that: In the step of evaporating the electrode material in the first evaporation chamber group to the isolation openings multiple times, the method further includes: The substrate is moved back and forth along the first direction so that the electrode material in the first evaporation chamber group is evaporated to the isolation opening multiple times; or, The first evaporation chamber group is moved back and forth along the first direction, so that the electrode material in the first evaporation chamber group is evaporated to the isolation opening for multiple times.
14. A display panel, characterized in that: include: substrate; An isolation structure, located on the substrate, the isolation structure encloses a plurality of isolation openings; A light-emitting layer, located on the substrate, the light-emitting layer comprising a plurality of light-emitting units located in the isolation openings; A first electrode layer, located on a side of the light-emitting layer away from the substrate, the first electrode layer comprising a first electrode located in the isolation opening, the first electrode being electrically connected to the isolation structure; The first electrode includes a central portion and an overlapping portion located around the central portion, the overlapping portion covers the side wall of the isolation structure, and the thickness of at least part of the overlapping portion is greater than or equal to 20 percent of the thickness of the central portion.
15. The display panel according to claim 14, characterized in that: The first electrode further includes a connecting portion located between the central portion and the overlapping portion, wherein a thickness of the connecting portion is greater than or equal to a thickness of the overlapping portion; Preferably, the connecting portion is annular, the inner edge of the connecting portion is connected to the central portion, and the outer edge of the connecting portion is connected to the overlapping portion; Preferably, the orthographic projection of the central portion on the substrate coincides with the orthographic projection of the isolation opening on the substrate.
16. The display panel according to claim 14, characterized in that: The thickness of the connecting portion is greater than or equal to fifty percent of the thickness of the central portion.
17. The display panel according to claim 14, characterized in that: The isolation structure includes a first layer and a second layer, wherein the second layer is located on a side of the first layer facing away from the substrate, and an orthographic projection of the first layer on the substrate is located within an orthographic projection of the second layer on the substrate.
18. The display panel according to claim 17, characterized in that: The first layer includes a conductive material; Preferably, the second layer comprises a conductive material or an insulating material; Preferably, both the first layer and the second layer include metal materials, and the materials of the first layer and the second layer are different.
19. The display panel according to claim 17, characterized in that: The isolation structure further includes a third layer located on a side of the first layer facing the substrate, and an orthographic projection of the first layer on the substrate is located within an orthographic projection of the third layer on the substrate; Preferably, at least part of the third layer comprises a plurality of sub-layers.
20. A display device, characterized in that: A display panel comprising any one of claims 14-19.