A welding repair device and method for fractured external teeth of slewing bearings
By using a motor-driven bevel gear transmission system and a clamping mechanism for automated cleaning and polishing, combined with direct connection of electrode blocks to the welding machine, the problems of long cleaning time and high cost in the repair of fractured external teeth of slewing bearings are solved, achieving efficient and low-cost repair results.
Patent Information
- Application Number
- CN202510441595.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2025-04-09
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2045-04-09
AI Technical Summary
In the existing process of repairing fractured external teeth of slewing bearings, the cleaning work is time-consuming and labor-intensive, and traditional welding methods are costly and have long maintenance cycles.
The system employs a motor-driven bevel gear transmission system, combined with a clamping mechanism and a brush roller, to achieve automated cleaning and polishing of the slewing bearing. It also allows for direct welding via an electrode block connected to a welding machine, simplifying the circuitry and shortening the maintenance cycle.
It reduced the labor intensity of staff, shortened the maintenance cycle, improved welding precision and efficiency, and reduced costs.
Smart Images

Figure CN120170406B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of slewing bearing external tooth repair technology, specifically to a welding repair device and method for fractured external teeth of slewing bearings. Background Technology
[0002] Slewing bearings are important components in construction machinery and are widely used in the slewing platforms of equipment such as cranes and excavators. However, in actual use, due to improper installation, poor lubrication, long-term overload, or improper operation, the external gears of slewing bearings are prone to breakage. The traditional repair method is to replace the external gears, but this method is costly. Therefore, welding repair is often used to reduce costs.
[0003] In the existing technology, before welding, repair personnel need to clean the surface of the broken external teeth to remove impurities such as oil and rust, so as to provide a clean surface for welding. Intact external teeth also need to be cleaned, which is convenient for measurement and comparison during subsequent grinding and for the discovery of new defects. However, excessive time is spent on cleaning, which not only increases the labor cost of the staff, but also prolongs the maintenance cycle and causes inconvenience to the normal operation of the equipment.
[0004] Therefore, it is urgent to improve the welding repair device for fractured external teeth of slewing bearings in order to solve the above-mentioned problems. Summary of the Invention
[0005] The purpose of this invention is to provide a device and method for welding and repairing fractured outer teeth of a slewing bearing. The motor can drive bevel gear one and bevel gear two to rotate synchronously through an active bevel gear. Bevel gear one drives the turntable to rotate, and the clamping mechanism can fix the slewing bearing. Bevel gear two drives the brush roller and water pump to work, thereby making the slewing bearing and the brush roller rotate synchronously, quickly cleaning the fractured outer teeth and the original teeth. This not only reduces the labor intensity of the workers, but also allows the outer teeth to be polished by the brush roller after welding, thus greatly shortening the maintenance cycle.
[0006] To achieve the above objectives, the main technical solutions adopted by the present invention include: A welding repair device for fractured external teeth of a slewing bearing includes a welding lathe and a turntable rotatably mounted on the welding lathe. A clamping mechanism is fixedly installed inside the turntable. A welding station is provided on one side of the welding lathe corresponding to the turntable. A reserved groove is provided on the side of the welding lathe away from the welding station. A brush roller is rotatably mounted above the reserved groove. A motor is fixedly installed on the bottom side of the welding lathe, and a drive rod is fixedly installed on the output end of the motor. Two active bevel gears are fixedly installed on the drive rod. A bevel gear rod one is fixedly connected to the bottom end of the turntable. The bevel gear rod one meshes with the active bevel gear on the right side. A bevel gear rod two is meshed on the active bevel gear on the left side. The shaft of the bevel gear rod two passes through the welding lathe and extends to the top of the welding lathe. A water tank is fixedly installed on the upper end of the welding lathe, and a water pump is fixedly installed on one side of the water tank. The shaft of the second bevel gear extends into the interior of the water pump, and a water pipe is fixedly connected to the output end of the water pump, extending above the turntable.
[0007] Preferably, a right-angle fixing plate is fixedly installed on the bottom side of the welding lathe, the motor is fixedly installed on the welding lathe, the shaft of the second bevel gear passes through the right-angle fixing plate and the welding lathe and extends to the top of the welding lathe, a bearing seat is fixedly installed on the side of the drive rod away from the right-angle fixing plate, and the drive rod passes through the right-angle fixing plate and the bearing seat and extends to the outside of the bearing seat.
[0008] Preferably, the clamping mechanism includes a cylinder, which is fixedly installed inside the turntable. A square push block is fixedly installed at the output end of the cylinder, and four push rods are rotatably arranged around the square push block. The upper side of the turntable is provided with a cross groove, and four sliders are slidably arranged inside the cross groove. A hinge is fixedly provided on the side of the slider near the clamping mechanism. The end of the push rod away from the cylinder is rotatably connected to the slider through the hinge.
[0009] Preferably, a clamping plate is fixedly installed at the upper end of the slider, and the clamping plate is slidably disposed on the upper side of the turntable via the slider.
[0010] Preferably, an electrode block is fixedly installed on the side of the clamping plate away from the clamping mechanism, and one end of the electrode block is electrically connected to the outside via a wire.
[0011] Preferably, a waste liquid guide channel is fixedly installed on the bottom side of the reserved groove by bolts, and the end of the waste liquid guide channel away from the welding station extends to the side of the welding lathe.
[0012] Preferably, the welding lathe has upright lugs fixedly installed on the upper sides of both ends of the reserved groove, and the brush roller passes through the upright lugs and extends to both sides of the upright lugs.
[0013] Preferably, an input bevel gear is fixedly installed at one end of the brush roller, and a driven bevel gear is rotatably provided on the welding lathe corresponding to the position of the input bevel gear, and the input bevel gear meshes with the driven bevel gear.
[0014] Preferably, a sprocket is fixedly mounted on the bottom side of the driven bevel gear, and a chain is fixedly mounted on the outer side of the sprocket. During the rotation of the bevel gear rod, the driven bevel gear is driven to rotate through the chain.
[0015] A method for welding repair of fractured external teeth of a slewing bearing includes the following steps: Fixing: Use a turntable and clamping mechanism to fix the broken tooth to be repaired. At the same time, build an insulated shed around the broken tooth to ensure that the ambient temperature within 1 m around the broken tooth is stable and not lower than 5℃, and is not affected by strong winds. Cleaning: Start the motor and drive the bevel gear through the bevel gear rod 2 and the driven bevel gear to rotate the bevel gear to clean the surface of the broken outer tooth. At the same time, use kerosene to clean the oil stains on the surface of the broken tooth. Clean at least the broken tooth and one tooth on each side to ensure that the surface is clean and free of impurities. Grinding: Use an angle grinder to remove broken teeth, cracks, and fissures, grind out a bevel and polish to a metallic luster; Preheating: Use a preheating device to preheat the broken outer tooth, dry and heat the broken tooth location and the three teeth on each side to 150°C, lay heat-insulating and fireproof cotton on the left and right teeth, and preheat the transition layer welding rod MX-2 and the overlay welding rod MX-3 at the same time. Transition layer welding: Rotate the broken external tooth to the corresponding position of the welding station, start the welding machine, and the output end of the welding machine is electrically connected to the slewing bearing through the electrode block. Then, the welding rod contacts the broken external tooth to form a circuit for welding repair. This process uses MX-2 flux-coated welding rods with a diameter of 2 mm and a ZX7-400 DC welding machine with reverse polarity, a peak current of 100A, linear electrode movement, and low heat input. Weld until it is well fused with the base material, with a layer height of 3 mm to reduce melting of the base material. Weld the entire welding rod in one go to prevent cracking. After air cooling to below 100℃, knock off the flux coating, check the welding quality, and weld the next welding rod only after visually passing the inspection. Continue until all broken sections are welded to the full layer height. After completion, cover with asbestos cloth for insulation and slow cooling to 50℃. Welding of the overlay layer: After the transition layer is welded, the overlay layer is welded to a height exceeding the normal tooth surface using MX-3 welding rods with a diameter of 3.5 mm, which facilitates grinding. The welding method is the same as that of the transition layer. The interlayer temperature is controlled within 50℃. After the welding is completed, the temperature is kept warm and slowly cooled to 20℃. Grinding: The welded external teeth are ground using a grinding device to achieve the same size and shape as the original teeth; Polishing: Start the motor to drive the turntable and brush roller to rotate synchronously. The brush roller circulates and polishes the welded outer teeth and other original teeth to achieve a refurbished effect. At the same time, use an angle grinder to repair the welded teeth for rough processing. Use plaster to make plaster models of the two adjacent continuous teeth. Spray colorant on the plaster models. Grind the plaster mold with the repaired welded teeth. Use a sanding wheel to polish the protruding parts until the entire broken tooth fits well with the plaster mold. Check the tooth flank clearance of the large and small gears. The difference between the clearance between the repaired tooth and the small gear and the clearance between the ordinary tooth and the small gear is between 0.00-0.2 mm. Flaw detection verification: After grinding, ultrasonic and penetrant testing is used with a 100% flaw detection rate. Level II is qualified. The internal and surface quality of the weld overlay is inspected. The second flaw detection is carried out after the first flaw detection is qualified and the cumulative operation time is 24 hours. Penetrant testing is used to check the surface quality and whether there are any new cracks. Level II is qualified.
[0016] The present invention has at least the following beneficial effects: 1. The motor of this invention can drive bevel gear one and bevel gear two to rotate synchronously through active bevel gear transmission. Bevel gear one drives the turntable to rotate, and the clamping mechanism can fix the slewing support. Bevel gear two drives the brush roller and water pump to work, thereby making the slewing support and the brush roller rotate synchronously, quickly cleaning the broken outer teeth and original teeth. This not only reduces the labor intensity of the workers, but also allows the outer teeth to be polished by the brush roller after welding, thus greatly shortening the maintenance cycle.
[0017] 2. In this invention, the cylinder drives the square push block to slide downwards. The square push block drives one end of the four push rods to slide downwards. The end of the push rod away from the square push block slides inside the cross groove through the hinge drive of the slider, thereby pushing the clamping plate to slide around and contact the inner wall of the slewing bearing. On the one hand, it can fix the position of the slewing bearing, and on the other hand, it can make the center of the slewing bearing correspond to the center of the turntable, which is beneficial to the subsequent cleaning and polishing process and can also improve the welding accuracy.
[0018] 3. During the fixing process of the slewing bearing, the clamping plate contacts the inner wall of the slewing bearing. Therefore, the slewing bearing can be electrically connected to the welding machine through the electrode block and the wire. When the welding machine is started, the slewing bearing is energized. At this time, the maintenance personnel can directly use the welding rod to contact the slewing bearing to form a complete conductive circuit. It is not necessary to close the circuit through the external cable, which is more secure and convenient and helps to improve the speed of welding repair.
[0019] 4. During the rotation of the bevel gear rod of the present invention, the driven bevel gear can be rotated through chain transmission. The bevel gear meshes with the input bevel gear, thereby driving the brush roller to rotate and polish the outer teeth of the slewing bearing. On the one hand, it can reduce the use of the drive mechanism, and on the other hand, it can make the brush roller and the slewing bearing rotate synchronously. At the same time, the water pump draws out the coolant in the water tank and pours it through the water pipe to the position where the outer teeth of the slewing bearing contact the brush roller, which improves the polishing accuracy and simplifies the control logic. Attached Figure Description
[0020] The accompanying drawings, which are included to provide a further understanding of this application and form part of this application, illustrate exemplary embodiments and are used to explain this application, but do not constitute an undue limitation of this application. In the drawings: Figure 1 This is a three-dimensional structural schematic diagram provided for the present invention; Figure 2 This is a front view diagram provided for the present invention; Figure 3 The driving rod structure diagram provided by the present invention; Figure 4 An exploded view of the clamping mechanism provided by the present invention; Figure 5 This invention provides a sectional elevation view of the water tank; Figure 6 The circuit diagram of the welding machine provided for this invention; Figure 7 A schematic diagram of the waste liquid diversion channel structure provided by the present invention. Figure 8 This is a schematic diagram of the chain structure provided by the present invention.
[0021] In the diagram, 1. Welding lathe; 101. Right-angle fixing plate; 102. Bearing seat; 103. Vertical lug; 104. Driven bevel gear; 105. Sprocket; 106. Chain; 2. Turntable; 201. Cross slide; 202. Slider; 203. Hinge; 204. Clamping plate; 205. Electrode block; 3. Clamping mechanism; 301. Cylinder; 302. Square push block; 303. Push rod; 4. Welding station; 5. Reserved slot; 6. Brush roller; 601. Input bevel gear; 7. Motor; 8. Drive rod; 9. Drive bevel gear; 10. Bevel gear rod one; 11. Bevel gear rod two; 12. Water tank; 13. Water pump; 14. Water pipe; 15. Waste liquid guide channel. Detailed Implementation
[0022] The following will describe in detail the implementation of this application with reference to the accompanying drawings and embodiments, so that the implementation process of how this application uses technical means to solve technical problems and achieve technical effects can be fully understood and implemented accordingly.
[0023] like Figures 1-8As shown, the slewing bearing external tooth fracture welding repair device provided in this embodiment includes a welding lathe 1 and a turntable 2 rotatably mounted on the welding lathe 1. A clamping mechanism 3 is fixedly installed inside the turntable 2. A welding station 4 is opened on one side of the welding lathe 1 corresponding to the turntable 2. A reserved groove 5 is opened on the side of the welding lathe 1 away from the welding station 4. A brush roller 6 is rotatably mounted above the reserved groove 5. The welding station 4 is used for maintenance personnel to install and disassemble the slewing bearing. Its side can be used to place a welding machine and a preheating device. The reserved groove 5 and the welding station are distributed on both sides of the turntable 2, which can ensure the cleanliness of the welding station 4. A motor 7 is fixedly installed on the bottom side of the welding lathe 1. A drive rod 8 is fixedly installed on the output end of the motor 7. Two active bevel gears 9 are fixedly installed on the drive rod 8. A bevel gear rod 10 is fixedly connected to the bottom end of the turntable 2. The bevel gear rod 10 meshes with the active bevel gear 9 on the right side. A bevel gear rod 21 is meshed on the active bevel gear 9 on the left side. The shaft of the bevel gear rod 21 passes through the welding lathe 1 and extends to the top of the welding lathe 1. A water tank 12 is fixedly installed at the top end of the welding lathe 1. A water pump 13 is fixedly installed on one side of the water tank 12. The shaft of the bevel gear rod 21 extends into the water pump 13. A water pipe 14 is fixedly connected to the output end of the water pump 13 and extends to the top of the turntable 2. Among them, the motor 7 is used to drive the bevel gear 10 and bevel gear 2 11 to rotate synchronously through the active bevel gear 9. The bevel gear 10 drives the turntable 2 to rotate. The clamping mechanism 3 can fix the slewing support. The bevel gear 2 11 drives the brush roller 6 and the water pump 13 to work, thereby making the slewing support and the brush roller 6 rotate synchronously, quickly cleaning the broken outer teeth and original teeth. Moreover, after welding, the outer teeth can be polished by the brush roller 6, which reduces the labor intensity of the workers and shortens the maintenance cycle. Specifically, the brushes on the brush roller 6 are replaceable. The inside of the brush roller 6 is a worm gear that can mesh with the external teeth of the slewing bearing. During the polishing process, the bevel gear rod 11 can drive the water pump 13 to work. The water pump 13 draws out the coolant from the water tank and pours it through the water pipe 14 onto the position where the external teeth of the slewing bearing contact the brush roller 6 to cool it down. This helps to reduce wear and thus greatly extends the service life of the brush roller 6.
[0024] Furthermore, such as Figures 1-8 As shown, a right-angle fixing plate 101 is fixedly installed on the bottom side of the welding lathe 1, and the motor 7 is fixedly installed on the welding lathe 1. The shaft of the bevel gear 11 passes through the right-angle fixing plate 101 and the welding lathe 1 and extends to the top of the welding lathe 1. A bearing seat 102 is fixedly installed on the side of the drive rod 8 away from the right-angle fixing plate 101. The drive rod 8 passes through the right-angle fixing plate 101 and the bearing seat 102 and extends to the outside of the bearing seat 102. The bearing seat 102 can provide support for the drive rod 8 and reduce the friction of the drive rod 8 during rotation or reciprocating motion. The welding lathe 1 has a stand ear 103 fixedly installed on the upper side of both ends of the reserved slot 5. The brush roller 6 passes through the stand ear 103 and extends to both sides of the stand ear 103. This through-type structural design allows the drive rod 8 and the brush roller 6 to establish a connection between different working parts. The right angle fixing plate 101 plays the role of fixing the position of the bevel gear rod 11, ensuring the stability of the bevel gear rod 11 during the working process.
[0025] Furthermore, such as Figures 1-8 As shown, the clamping mechanism 3 includes a cylinder 301, which is fixedly installed inside the turntable 2. A square push block 302 is fixedly installed at the output end of the cylinder 301. Four push rods 303 are rotatably arranged around the square push block 302. A cross slide groove 201 is opened on the upper side of the turntable 2. Four sliders 202 are slidably arranged inside the cross slide groove 201. A hinge 203 is fixedly installed on the side of the slider 202 near the clamping mechanism 3. The end of the push rod 303 away from the cylinder 301 is rotatably connected to the slider 202 through the hinge 203. A clamping plate 204 is fixedly installed on the upper end of the slider 202. The clamping plate 204 is slidably arranged on the upper side of the turntable 2 through the slider 202. When fixing the slewing bearing: The maintenance personnel first place the slewing bearing on the turntable 2, and then start the cylinder 301 to drive the square push block 302 to slide downward. The square push block 302 drives one end of the four push rods 303 to slide downward. The end of the push rod 303 away from the square push block 302 drives the slider 202 to slide inside the cross groove 201 through the hinge 203, thereby pushing the clamping plate 204 to slide around and contact the inner wall of the slewing bearing. On the one hand, this can fix the position of the slewing bearing, and on the other hand, it can make the center of the slewing bearing correspond to the center of the turntable 2, which is beneficial to the subsequent cleaning and polishing process and can also improve the welding accuracy.
[0026] In addition, such as Figure 4 and Figure 6 As shown, an electrode block 205 is fixedly installed on the side of the clamping plate 204 away from the clamping mechanism 3, and one end of the electrode block 205 is electrically connected to the outside through a wire. When welding slewing bearings: During the fixing process, the clamping plate 204 contacts the inner wall of the slewing bearing. Therefore, the slewing bearing can be electrically connected to the welding machine through the electrode block 205 and the wire. When the welding machine is started, the slewing bearing is energized. At this time, the maintenance personnel can directly use the welding rod to contact the slewing bearing to form a complete conductive circuit. It is not necessary to close the circuit through an external cable, which is more secure and convenient and helps to improve the speed of welding repair.
[0027] Furthermore, such as Figure 1 and Figure 7As shown, a waste liquid guide channel 15 is bolted to the bottom side of the reserved tank 5. The end of the waste liquid guide channel 15 away from the welding station 4 extends to the side of the welding lathe 1. During the welding process, various waste liquids are generated, such as flux residue, coolant, and cleaning fluid used in the welding process. The waste liquid guide channel 15 installed on the bottom side of the reserved tank 5 can effectively collect these waste liquids. The bolt fixing ensures that the waste liquid guide channel 15 is tightly connected to the reserved tank 5, preventing waste liquid leakage. To solve the problem of the linkage between the bevel gear rod 11 and the brush roller 6: like Figure 1 As shown, an input bevel gear 601 is fixedly installed at one end of the brush roller 6. A driven bevel gear 104 is rotatably installed on the welding lathe 1 corresponding to the position of the input bevel gear 601. The input bevel gear 601 meshes with the driven bevel gear 104. A sprocket 105 is fixedly installed on the bottom side of the driven bevel gear 104. A chain 106 is fixedly installed on the outer side of the sprocket 105. During the rotation of the bevel gear rod 11, the driven bevel gear 104 is driven to rotate through the chain 106. During the rotation of the bevel gear 11, the driven bevel gear 104 can be driven to rotate via the chain 106. The driven bevel gear 104 meshes with the input bevel gear 601, thereby driving the brush roller 6 to rotate and polish the outer teeth of the slewing bearing. On the one hand, this reduces the use of the drive mechanism, and on the other hand, it allows the brush roller 6 to rotate synchronously with the slewing bearing. At the same time, the water pump 13 extracts the coolant from the water tank and pours it through the water pipe 14 onto the contact position between the outer teeth of the slewing bearing and the brush roller 6, improving the polishing accuracy while simplifying the control logic.
[0028] like Figures 1-8 As shown in this embodiment, the method for welding and repairing fractured external teeth of a slewing bearing includes the following steps: Fixing: Use turntable 2 and clamping mechanism 3 to fix the broken tooth to be repaired. At the same time, build an insulation shed around the broken tooth location to ensure that the ambient temperature within 1 m around the broken tooth location is stable, not lower than 5℃, and is not affected by strong winds. Cleaning: Start motor 7 drives bevel gear 601 to rotate through bevel gear rod 11 and driven bevel gear 104 to clean the broken outer tooth surface. At the same time, use kerosene to clean the oil stains on the broken tooth area. Clean at least the broken tooth and one tooth on each side to ensure the surface is clean and free of impurities. Grinding: Use an angle grinder to remove broken teeth, cracks, and fissures, grind out a bevel and polish to a metallic luster; Preheating: Use a preheating device to preheat the broken outer tooth, dry and heat the broken tooth location and the three teeth on each side to 150°C, lay heat-insulating and fireproof cotton on the left and right teeth, and preheat the transition layer welding rod MX-2 and the overlay welding rod MX-3 at the same time. Transition layer welding: Rotate the broken external tooth to the position corresponding to welding station 4, start the welding machine, and the output end of the welding machine is electrically connected to the slewing bearing through electrode block 205. Then, the welding rod contacts the broken external tooth to form a circuit for welding repair. This process uses MX-2 flux-coated welding rods with a diameter of 2 mm and a ZX7-400 DC welding machine with reverse polarity, peak current of 100 A, linear electrode movement, and low heat input. Weld until it is well fused with the base material, with a layer height of 3 mm to reduce melting of the base material. Weld the entire welding rod in one go to prevent cracking. After air cooling to below 100℃, knock off the flux coating, check the welding quality, and weld the next welding rod after visual inspection. Continue until all broken sections are welded to the full layer height. After completion, cover with asbestos cloth for insulation and slow cooling to 50℃. Welding of the overlay layer: After the transition layer is welded, the overlay layer is welded to a height exceeding the normal tooth surface using MX-3 welding rods with a diameter of 3.5 mm, which facilitates grinding. The welding method is the same as that of the transition layer. The interlayer temperature is controlled within 50℃. After the welding is completed, the temperature is kept warm and slowly cooled to 20℃. Grinding: The welded external teeth are ground using a grinding device to achieve the same size and shape as the original teeth; Polishing: Start the motor 7 to drive the turntable 2 and brush roller 6 to rotate synchronously. The brush roller 6 performs cyclic polishing on the welded outer teeth and other original teeth to achieve a refurbishment effect. At the same time, use an angle grinder to repair the welded teeth for rough processing. Use plaster to make plaster models of the two adjacent continuous teeth. Spray colorant on the plaster models. Grind the plaster mold with the repaired welded teeth. Use a sanding wheel to polish the protruding parts until the entire broken tooth fits well with the plaster mold. Check the tooth flank clearance of the large and small gears. The difference between the clearance between the repaired tooth and the small gear and the clearance between the ordinary tooth and the small gear is between 0.00-0.2 mm. Flaw detection verification: After grinding, ultrasonic and penetrant testing is used with a 100% flaw detection rate. Level II is qualified. The internal and surface quality of the weld overlay is inspected. The second flaw detection is carried out after the first flaw detection is qualified and the cumulative operation time is 24 hours. Penetrant testing is used to check the surface quality and whether there are any new cracks. Level II is qualified.
[0029] The above are merely preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
Claims
1. A welding repair device for fractured external gears of a slewing bearing, comprising a welding lathe (1) and a turntable (2) rotatably mounted on the welding lathe (1), characterized in that: The turntable (2) is fixedly installed with a clamping mechanism (3). The welding lathe (1) has a welding station (4) on one side of the turntable (2). The welding lathe (1) has a reserved groove (5) on the side away from the welding station (4). A brush roller (6) is rotatably arranged above the reserved groove (5). A motor (7) is fixedly installed on the bottom side of the welding lathe (1). A drive rod (8) is fixedly installed on the output end of the motor (7). Two active bevel gears (9) are fixedly installed on the drive rod (8). A bevel gear rod one (10) is fixedly connected to the bottom end of the turntable (2). The bevel gear rod one (10) meshes with the active bevel gear (9) on the right side. A bevel gear rod two (11) meshes with the active bevel gear (9) on the left side. The shaft of the bevel gear rod two (11) passes through the welding lathe (1) and extends to the top of the welding lathe (1). A water tank (12) is fixedly installed on the upper end of the welding lathe (1), and a water pump (13) is fixedly installed on one side of the water tank (12). The shaft of the bevel gear rod (11) extends into the interior of the water pump (13). A water pipe (14) is fixedly connected to the output end of the water pump (13), and the water pipe (14) extends above the turntable (2). The clamping mechanism (3) includes a cylinder (301), which is fixedly installed inside the turntable (2). A square push block (302) is fixedly installed at the output end of the cylinder (301), and four push rods (303) are rotatably arranged around the square push block (302). The turntable (2) has a cross groove (201) on its upper side. Four sliders (202) are slidably arranged inside the cross groove (201). A hinge (203) is fixedly arranged on the side of the slider (202) near the clamping mechanism (3). The end of the push rod (303) away from the cylinder (301) is rotatably connected to the slider (202) through the hinge (203). A clamping plate (204) is fixedly installed at the upper end of the slider (202), and the clamping plate (204) is slidably disposed on the upper side of the turntable (2) through the slider (202); An electrode block (205) is fixedly installed on the side of the clamping plate (204) away from the clamping mechanism (3), and one end of the electrode block (205) is electrically connected to the outside through a wire. An input bevel gear (601) is fixedly installed at one end of the brush roller (6), and a driven bevel gear (104) is rotatably provided on the welding lathe (1) corresponding to the position of the input bevel gear (601). The input bevel gear (601) meshes with the driven bevel gear (104). A sprocket (105) is fixedly installed on the bottom side of the driven bevel gear (104), and a chain (106) is fixedly installed on the outer side of the sprocket (105). During the rotation of the bevel gear rod (11), the driven bevel gear (104) is driven to rotate through the chain (106).
2. The slewing bearing external tooth fracture welding repair device according to claim 1, characterized in that: A right-angle fixing plate (101) is fixedly installed on the bottom side of the welding lathe (1). The motor (7) is fixedly installed on the welding lathe (1). The shaft of the bevel gear rod (11) passes through the right-angle fixing plate (101) and the welding lathe (1) and extends to the top of the welding lathe (1). A bearing seat (102) is fixedly installed on the side of the drive rod (8) away from the right-angle fixing plate (101). The drive rod (8) passes through the right-angle fixing plate (101) and the bearing seat (102) and extends to the outside of the bearing seat (102).
3. The slewing bearing external tooth fracture welding repair device according to claim 1, characterized in that: Waste liquid guide channel (15) is fixedly installed on the bottom side of the reserved groove (5) by bolts, and the end of the waste liquid guide channel (15) away from the welding station (4) extends to the side of the welding lathe (1).
4. The slewing bearing external tooth fracture welding repair device according to claim 1, characterized in that: The welding lathe (1) has a stand-up lug (103) fixedly installed on the upper side of both ends of the reserved groove (5), and the brush roller (6) passes through the stand-up lug (103) and extends to both sides of the stand-up lug (103).
5. A method for welding and repairing fractured external teeth of a slewing bearing, using the welding and repair device for fractured external teeth of a slewing bearing as described in claim 4, characterized in that: Includes the following steps: Fixing: Use a turntable (2) and a clamping mechanism (3) to fix the broken tooth to be repaired. At the same time, build an insulation shed around the broken tooth to ensure that the ambient temperature within 1 m around the broken tooth is stable, not lower than 5℃, and not affected by strong winds. Cleaning: Start the motor (7) and drive the input bevel gear (601) to rotate through the bevel gear rod (11) and the driven bevel gear (104) to clean the surface of the broken outer tooth. At the same time, use kerosene to clean the oil stains on the surface of the broken tooth. Clean at least the broken tooth and one tooth on each side to ensure that the surface is clean and free of impurities. Grinding: Use an angle grinder to remove broken teeth, cracks, and fissures, grind out a bevel and polish to a metallic luster; Preheating: Use a preheating device to preheat the broken outer tooth, dry and heat the broken tooth location and the three teeth on each side to 150°C, lay heat-insulating and fireproof cotton on the left and right teeth, and preheat the transition layer welding rod MX-2 and the overlay welding rod MX-3 at the same time. Transition layer welding: Rotate the broken outer tooth to the position corresponding to the welding station (4), start the welding machine, the output end of the welding machine is electrically connected to the slewing bearing through the electrode block (205), and then the welding rod contacts the broken outer tooth to form a circuit for welding repair. This process uses MX-2 flux-coated welding rod with a diameter of 2 mm, and the welding machine uses ZX7-400 DC welding machine, reverse connection, peak current 100 A, straight rod movement, small heat input welding, and good fusion with the base material. The layer height is 3 mm to reduce the melting of the base material. Weld the entire welding rod at once to prevent cracks from forming. After air cooling to below 100℃, knock off the coating, check the welding quality, and weld the next welding rod after visual inspection until all the broken stubs are welded to the full layer height. After completion, cover with asbestos cloth for heat preservation and slow cooling to 50℃. Welding of the overlay layer: After the transition layer is welded, the overlay layer is welded to a height exceeding the normal tooth surface using MX-3 welding rods with a diameter of 3.5 mm, which facilitates grinding. The welding method is the same as that of the transition layer. The interlayer temperature is controlled within 50℃. After the welding is completed, the temperature is kept warm and slowly cooled to 20℃. Grinding: The welded external teeth are ground using a grinding device to achieve the same size and shape as the original teeth; Polishing: Start the motor (7) to drive the turntable (2) and the brush roller (6) to rotate synchronously. The brush roller (6) performs cyclic polishing on the welded outer teeth and other original teeth to achieve the effect of renovation. At the same time, use an angle grinder to repair the welded teeth and perform rough processing. Use plaster to make plaster models of the two adjacent continuous teeth. Spray colorant on the plaster model. Grind the plaster mold with the repaired welded teeth. Use a sanding wheel to polish the protruding parts until the entire broken tooth fits well with the plaster mold. Check the tooth side clearance of the large and small gears. The difference between the clearance between the repaired tooth and the small gear and the clearance between the ordinary tooth and the small gear is between 0.00-0.2 mm. Flaw detection verification: After grinding, ultrasonic and penetrant testing is used with a 100% flaw detection rate. Level II is qualified. The internal and surface quality of the weld overlay is inspected. The second flaw detection is carried out after the first flaw detection is qualified and the cumulative operation time is 24 hours. Penetrant testing is used to check the surface quality and whether there are any new cracks. Level II is qualified.
Citation Information
Patent Citations
Slewing bearing cleaning device
CN119035134A
Gear-machining surface grinding device
WO2022252293A1